piezoelectric device
By designing a gradually decreasing thickness section of the base in the piezoelectric device and optimizing the adhesive structure, the problems of deteriorated electrical properties and reduced adhesive strength caused by the flow of conductive adhesive were solved, thereby improving impact resistance and electrical properties.
Patent Information
- Application Number
- CN202610677419.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-23
- Filing Date
- 2026-05-18
- Publication Date
- 2026-11-24
AI Technical Summary
In piezoelectric devices, as miniaturization progresses, the bonding area of conductive adhesives becomes narrower, resulting in reduced bonding strength. Furthermore, conductive adhesives tend to flow into vibration areas, causing deterioration in electrical properties and short circuits between excitation electrodes.
The base design incorporates a thickness reduction section at the end of the piezoelectric vibrator that decreases in thickness towards the center, preventing the conductive adhesive from flowing. The optimized bonding structure between the base, the piezoelectric vibrator, and the container enhances the bonding strength and impact resistance.
It effectively prevents conductive adhesive from flowing to the center side of the piezoelectric vibrator, avoiding deterioration of electrical characteristics and short circuits between excitation electrodes, thus improving the impact resistance and electrical characteristics of piezoelectric equipment.
Smart Images

Figure CN123163548A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a piezoelectric device having a structure in which a piezoelectric vibrator is connected to a container via a pedestal. Background Technology
[0002] As piezoelectric devices, there exist piezoelectric vibrators, piezoelectric oscillators, and other piezoelectric devices that use piezoelectric vibrating plates that perform thickness shear vibration. These piezoelectric devices typically have a structure in which a piezoelectric vibrating plate, which is rectangular in shape when viewed from above, is fixed to a container at two points on one of its short sides by a conductive adhesive, a so-called cantilever support structure.
[0003] In piezoelectric devices using piezoelectric vibrators that perform thickness shear vibration, if conductive adhesive reaches the vibration area of the piezoelectric vibrator, it can cause problems such as deterioration of the electrical characteristics of the piezoelectric device and short circuits between the excitation electrodes. To avoid this, a structure is provided to prevent the conductive adhesive from flowing (e.g., Patent Document 1, Patent Document 2).
[0004] On the other hand, the demand for high-performance piezoelectric devices is increasing. As a technical means to meet this demand, a method has been proposed to connect a piezoelectric vibrator to a container via a pedestal. It is claimed that the electrical characteristics of the piezoelectric device can be improved because the pedestal can mitigate stresses from the container (Patent Document 3).
[0005] [Existing Technical Documents]
[0006] [Patent Literature]
[0007] [Patent Document 1] Japanese Patent Application Publication No. 2000-31773
[0008] [Patent Document 2] Japanese Patent Application Publication No. 2013-85298
[0009] [Patent Document 3] Japanese Patent Application Publication No. 2010-135890 Summary of the Invention
[0010] [The problem the invention aims to solve]
[0011] In piezoelectric devices using a base, the shape of the base is also important to prevent conductive adhesive from flowing towards the vibration area. This importance increases as piezoelectric devices become smaller, both the base and the piezoelectric vibrator become smaller. However, while Patent Document 3 describes the relationship between the bonding positions of the base, the piezoelectric vibrator, and the container, and the use of lead wire bonding as a wiring method, it neither describes nor suggests a preferred structure for preventing the conductive adhesive from flowing from the base itself. Furthermore, as piezoelectric devices become smaller, the bonding area based on conductive adhesive also narrows, making countermeasures against reduced adhesive strength due to impacts such as drops important.
[0012] This application has been made in view of this aspect, and therefore the object of this application is to provide a novel piezoelectric device having a structure in which a piezoelectric vibrator is connected to a container via a pedestal, the piezoelectric device having a pedestal that is preferred in preventing the flow of conductive adhesive and also preferred in improving impact resistance.
[0013] [Technical means to solve the problem]
[0014] To achieve this objective, according to the present invention, a piezoelectric device includes: a piezoelectric vibrating plate, which is quadrilateral in shape when viewed from above; a container for mounting the piezoelectric vibrating plate; a pedestal disposed between the piezoelectric vibrating plate and the container at a predetermined portion along a first side; a first conductive adhesive for bonding the piezoelectric vibrating plate and the pedestal; and a second conductive adhesive for bonding the pedestal and the container. The piezoelectric device is characterized in that...
[0015] The end of the piezoelectric vibrating plate on the center side of the platform in a second direction orthogonal to the first side includes a thickness reduction section whose thickness decreases toward the center side.
[0016] In implementing this invention, the thickness reduction portion only needs to have an inclined surface that slopes from at least the piezoelectric vibrating plate side of the two main surfaces of the pedestal toward the center side (see Figure 4(A)). However, the thickness reduction portion may also have inclined surfaces that slope from the two opposing main surfaces of the pedestal toward the center side respectively (see Figures 1(A) to 1(C), Figures 2(A) to 2(C)).
[0017] Furthermore, the thickness reduction portion can take various forms, such as: a structure comprising an inclined surface inclined at a constant angle toward the center (Figs. 1(A) to 1(C), 2(A) to 2(C), 4(A)); a structure comprising an inclined surface inclined at multiple different angles toward the center (Fig. 4(B)); a structure comprising a curved surface with a constant curvature or multiple curvatures (Fig. 4(C)); a structure comprising a substantially vertical step and the aforementioned exemplified inclined surface or curved surface connected thereto and decreasing in thickness toward the center (Fig. 4(D)); or a structure comprising a thickness reduction portion at each end of the second direction decreasing outward along the second direction (Fig. 4(E)), etc. In the case where there are thickness reduction portions at each end of the second direction, it is permissible regardless of whether the inclined surfaces at each end are closed (Fig. 4(E)).
[0018] Furthermore, in implementing this invention, the piezoelectric vibrator can be any type of vibrator that performs thickness shear vibration, such as an AT-cut crystal vibrator, a so-called double-rotation crystal vibrator represented by SC cutting, a piezoelectric vibrator made of piezoelectric ceramic, or a piezoelectric vibrator using piezoelectric crystals such as lithium niobate. However, an AT-cut crystal vibrator is particularly preferred as a piezoelectric vibrator. This is because, compared to other piezoelectric vibrators, crystal oscillators and crystal transducers using AT-cut crystal vibrators have high precision and excellent mass production capabilities, thus offering high industrial applicability.
[0019] Furthermore, in implementing this invention, the piezoelectric vibrator can be configured as an AT-cut crystal vibrator that is rectangular in shape when viewed from above. Depending on whether the long side of the crystal vibrator is along the X-axis of the crystal (so-called an X-length crystal vibrator) or whether the long side of the crystal vibrator is along the Z'-axis (so-called a Z'-length crystal vibrator), the crystal pedestal can be configured as an AT-cut crystal wafer or a Z-plate crystal wafer. The crystal vibrator and the crystal pedestal are arranged so that their crystal axes are parallel to each other (see Figures 5(A) and 5(B)). Here, the Z'-axis refers to the axis that deviates from the true Z-axis of the crystal based on the cutting angle of the AT-cut crystal wafer.
[0020] Furthermore, when the piezoelectric vibrator is an AT-cut crystal vibrator with a rectangular shape when viewed from above, and the pedestal is made of crystal, the pedestal is preferably made with a thickness selected from the range of 30 μm to 60 μm. Details will be described later.
[0021] Furthermore, although the piezoelectric device described in this invention will be detailed in one of the embodiments, it can be a piezoelectric vibration device including a piezoelectric vibrating plate, a container, and a pedestal; a piezoelectric oscillator including a piezoelectric vibrating plate, a container, the pedestal, and an oscillation circuit for the piezoelectric vibrating plate; or a so-called built-in temperature sensor type piezoelectric vibration device including a piezoelectric vibrating plate, a container, the pedestal, and a temperature sensor (e.g., a thermistor). Moreover, the built-in temperature sensor type piezoelectric vibration device can be a so-called single-chamber structure built-in temperature sensor type piezoelectric vibration device in which the piezoelectric vibrating plate and the temperature sensor are installed in one chamber; or a so-called H-shaped built-in temperature sensor type piezoelectric vibration device in which the first chamber for installing the piezoelectric vibrating plate and the second chamber for installing the temperature sensor are connected to each other on the bottom surface and the cross-section cut along the thickness direction presents an H-shape.
[0022] [The effects of the invention]
[0023] The piezoelectric device of the present invention includes a base with a thickness reduction portion where the thickness of the piezoelectric vibrating plate at its center side decreases towards the center side. Therefore, in the thickness reduction portion, the distance between the piezoelectric vibrating plate and the base widens towards the center side of the piezoelectric vibrating plate.
[0024] Therefore, if a first conductive adhesive is applied to the upper surface of the pedestal and a piezoelectric vibrator is placed thereon, although the first conductive adhesive flows towards the center of the piezoelectric vibrator between the pedestal and the piezoelectric vibrator, the gap between the pedestal and the piezoelectric vibrator widens due to the presence of a thickness reduction section, making it difficult for the first conductive adhesive to flow towards the center of the piezoelectric vibrator. Furthermore, the thickness of the first conductive adhesive increases at the thickness reduction section (see Figure 2(B)). Therefore, since the first conductive adhesive is difficult to flow towards the center of the piezoelectric vibrator, deterioration of the electrical characteristics of the piezoelectric device and short circuits between the excitation electrodes can be prevented. In addition, since the thickness of the first conductive adhesive near the thickness reduction section increases, the piezoelectric vibrator becomes correspondingly difficult to peel off from the pedestal, thereby improving impact resistance. As the first conductive adhesive is mainly a silicone-based adhesive, for silicone-based conductive adhesives, a thicker thickness to a certain extent provides a better elastic effect and exhibits an improved impact resistance effect; in this respect, the thickness reduction section of the present invention is also useful.
[0025] Therefore, according to the present invention, a novel piezoelectric device having a base that is preferred in preventing the flow of conductive adhesive and also preferred in improving impact resistance can be provided. Attached Figure Description
[0026] Figures 1(A) to 1(C) are diagrams used to illustrate the crystal oscillator 10 of the piezoelectric device as a first embodiment.
[0027] Figures 2(A) to 2(C) are used to illustrate the features of the base of the present invention and comparative examples.
[0028] Figure 3 This is a diagram illustrating a preferred embodiment of the base of the present invention.
[0029] Figures 4(A) to 4(E) are diagrams illustrating modified examples of the base of the present invention.
[0030] Figures 5(A) and 5(B) are diagrams illustrating preferred examples when using a crystal pedestal as a pedestal.
[0031] Figure 6 This is a diagram used to illustrate the relationship between the thickness of the crystal substrate and stress mitigation.
[0032] Figure 7 This is a diagram used to illustrate the crystal oscillator 30 of the second embodiment.
[0033] Figure 8 This is a diagram used to illustrate the crystal oscillator 40 of the third embodiment.
[0034] Figure 9 This is a diagram used to illustrate the crystal oscillator 50 of the fourth embodiment.
[0035] Explanation of icon numbers
[0036] 10: Implemented forms of crystal oscillators (piezoelectric devices, crystal oscillators)
[0037] 11: AT-cut crystal oscillators (piezoelectric oscillators, crystal oscillators)
[0038] 11a: Excitation electrode
[0039] 11b: The first side of the crystal vibrator (first side)
[0040] 11c: Outgoing wiring
[0041] 13: Container
[0042] 13a: First recess (recess)
[0043] 13b: Second recess (recess)
[0044] 13c: Bonding pad (solder pad)
[0045] 13d: Pad
[0046] 13e: External connection terminal
[0047] 13f: Metallic conductor
[0048] 13x: Main body part
[0049] 13y: Ring-shaped component
[0050] 15, 15p, 15q, 15r: pedestal
[0051] 15a: First wiring pattern (wiring pattern)
[0052] 15b: Second wiring pattern
[0053] 15c: Third wiring pattern
[0054] 15d: Rear section
[0055] 15x: Incision area
[0056] 15z, 15z1, 15z2, 15z3, 15z4, 15z5, 15z6: Thickness gradually decreasing section
[0057] 17: Temperature sensor (thermometer)
[0058] 19: Cover component
[0059] 21a: Conductive adhesive (first conductive adhesive)
[0060] 21b: Conductive adhesive (secondary conductive adhesive)
[0061] 21c: Conductive adhesive
[0062] 25: Pedestal (pedestal) of comparative example
[0063] 30: Crystal oscillator of the embodiment (crystal oscillator of the second embodiment, crystal oscillator)
[0064] 40: Crystal oscillator of the third embodiment (crystal oscillator, crystal oscillator)
[0065] 50: Crystal oscillator of the embodiment (crystal oscillator of the fourth embodiment, crystal oscillator)
[0066] 51: Semiconductor chip
[0067] a, b: Inclined surfaces
[0068] D: Steps
[0069] g1, g2: Interval
[0070] S1: Back dimension
[0071] T: Thickness
[0072] X, Y, Y', Z, Z': Axis
[0073] θ1, θ2: Angles Detailed Implementation
[0074] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. Furthermore, the drawings used in the description are only schematic representations to the extent that the present invention can be understood. Also, in the drawings used in the description, sometimes the same reference numerals are used to indicate the same components, and their descriptions are omitted. Moreover, the structural examples, components, etc., described below are only preferred examples within the scope of the present invention. Therefore, the present invention is not limited to the embodiments described below.
[0075] 1. First Implementation Form
[0076] 1-1. Structural Description
[0077] The first embodiment of the piezoelectric device is an example of applying the present invention to a single-chamber crystal oscillator with a built-in temperature sensor. Referring to this, see Figures 1(A) to 1(C) and Figures 2(A) to 2(C). Figure 3 Hereinafter, Figure 1(A) is a top view of the crystal oscillator 10, Figure 1(B) is a cross-sectional view along line PP in Figure 1(A), and Figure 1(C) is a bottom view. Furthermore, Figure 2(A) is a partially enlarged perspective view showing the portion including the pedestal 15 in Figures 1(A) to 1(C), Figure 2(B) is a side view illustrating the effect of the pedestal 15 of the present invention, and Figure 2(C) is a side view illustrating the problems with the pedestal of the comparative example. Furthermore, Figure 3 These are plan views, rear views (perspective views), and side views illustrating a preferred wiring example mounted on the pedestal. Additionally, in Figure 1(A), illustrations of the crystal oscillator 11, cover member 19, conductive adhesive 21a, conductive adhesive 21b, etc., shown in Figure 1(B) are omitted.
[0078] The crystal oscillator 10 includes a crystal oscillator 11, a container 13, a base 15, a temperature sensor 17, and a cover component 19. The following is a detailed description of each component.
[0079] The crystal oscillator 11 is an AT-cut crystal oscillator that is quadrilateral in plan view and rectangular in plan view in this case. The crystal oscillator 11 includes excitation electrodes 11a on the main surface of the back of the watch, and further includes lead wires 11c in the region from each excitation electrode 11a toward the first short side 11b, which is the first side of the crystal oscillator 11 (see Figure 2(A) in particular).
[0080] The container 13 is used to mount the crystal oscillator 11 and the temperature sensor 17. In this example, it includes: a ceramic body 13x having a recess 13b for mounting the temperature sensor 17 (hereinafter also referred to as the second recess 13b); and a metal annular member 13y serving as a sidewall, which is connected to the body 13x by means of, for example, brazing, to form a first recess 13a for accommodating the crystal oscillator 11, which has a quadrilateral planar shape and an area wider than the second recess 13b.
[0081] The second recess 13b of the container 13 is offset to one side relative to the first recess 13a. Two pads 13c for connecting the crystal oscillator 11 are provided along a predetermined direction on the step created around the second recess 13b of the ceramic body 13x due to the offset of the second recess 13b. Specifically, the two pads 13c are positioned apart from each other in a direction parallel to the first short side 11b of the crystal oscillator 11. Furthermore, two pads 13d for connecting the temperature sensor 17 are provided on the bottom surface of the second recess 13b, and an external connection terminal 13e is provided on the back of the container 13. The two pads 13c and two pads 13d are connected to the external connection terminal 13e via through-hole wiring (not shown). Additionally, a metal conductor 13f is provided at an appropriate position in the ceramic body 13x, which connects the metal annular member 13y to a ground terminal in the external connection terminal 13e. Electromagnetic shielding can be improved by using the cover member 19, the metal ring member 13y, and the metal conductor 13f.
[0082] The platform 15 has a generally rectangular shape, with a width equal to the short side of the crystal oscillator 11 and a length that does not reach the excitation electrode 11a of the crystal oscillator 11. Furthermore, at the end of the platform 15 on the center side of the crystal oscillator 11 in a direction orthogonal to the first short side 11b of the crystal oscillator 11, there is a thickness reduction portion 15z whose thickness decreases toward the center side (see Figures 2(A) and 2(B) in particular).
[0083] Furthermore, in the first embodiment, the thickness reduction section 15z is an inclined surface at the end of the crystal oscillator 11 on the center side of the pedestal 15, with its thickness inclined at a constant angle towards the center side. In this case, the inclined surface exists on both the front and back of the pedestal 15, and forms inclined surfaces that are interconnected (closed) near the approximate center in the thickness direction of the pedestal 15. The angle θ between the interconnected surfaces is not limited to this, and can be, for example, approximately 90 to 120 degrees. The detailed function and effect of the thickness reduction section 15z will be described later.
[0084] In addition, such as Figure 3As shown, the pedestal 15 includes a first wiring pattern 15a on its first surface for connection to the crystal oscillator 11, specifically for connection to the lead wire 11c; a second wiring pattern 15b on its second surface opposite to the first surface for connection to the container, specifically for connection to the two pads 13c; and a third wiring pattern 15c on its sidewall connecting the first wiring pattern 15a and the second wiring pattern 15b. Furthermore, the third wiring pattern 15c is disposed on the sidewall of the pedestal 15 located on the central side of the crystal oscillator 11. By disposing of the third wiring pattern 15c on the sidewall of the pedestal 15 located on the central side of the crystal oscillator 11, a short circuit between the third wiring pattern 15c and the metal annular member 13y can be avoided even when the pedestal 15 contacts the metal annular member 13y.
[0085] Furthermore, in this embodiment, the first wiring pattern 15a and the second wiring pattern 15b each include a recessed portion 15d on the side of the at least metal annular member 13y of the base 15, receding from the edge of the base 15 towards the center. The recessed dimension S1 of the recessed portion 15d is only required to be such that even if the base 15 contacts the metal annular member 13y, it can prevent the first wiring pattern 15a or the second wiring pattern 15b from contacting (short-circuiting) the metal annular member 13y. If the recessed dimension S1 is too large, the area of the wiring pattern becomes smaller, which is not preferable. Although not limited to this, the recessed dimension S1 can be, for example, about 30 μm to 50 μm.
[0086] Furthermore, in this embodiment, the pedestal 15 includes a notch 15x at the corner opposite to the center side of the crystal oscillator 11. The shape of the notch 15x can be any shape, such as a C-face chamfer or an R-face chamfer. Having the notch 15x is preferable because it allows the pedestal 15 to be positioned close to the wall edge of the container 13.
[0087] The material of the base 15 is arbitrary, but it is preferably a material with a coefficient of thermal expansion that is the same as or close to that of the crystal oscillator 11. More preferably, it is a crystal base with the same cutting angle as the crystal oscillator 11. This will be explained later with reference to Figures 5(A) and 5(B).
[0088] In this case, the temperature sensor 17 is made of a thermistor, and the cover member 19 is made of any member corresponding to the sealing method, such as a sheet of material with a specified coating made of Kova alloy.
[0089] Furthermore, the crystal oscillator 10 includes a base 15 between a predetermined portion along the first short side 11b of the crystal oscillator 11 (i.e., the area where the lead wires 11c are provided) and the area of the container 13 where two pads 13c are provided. The crystal oscillator 11 and the base 15 are bonded together by a first conductive adhesive 21a, and the base 15 and the container 13 are bonded together by a second conductive adhesive 21b. More specifically, the crystal oscillator 10 has a structure in which the two bonding pads 13c (corresponding to an example of the predetermined portion along the first side as described in this invention), the first conductive adhesive 21a, the base 15, the second conductive adhesive 21b, and one end of the crystal oscillator 11 overlap in the vertical direction. The cover member 19 is connected to the metal annular member 13y by, for example, seam welding. In addition, the first conductive adhesive 21a and the second conductive adhesive 21b are preferably silicone-based conductive adhesives. The first conductive adhesive 21a and the second conductive adhesive 21b may be made of the same material or different materials, but are typically made of the same material.
[0090] Furthermore, the thermistor 17 is connected to two pads 13d within the second recess 13b via, for example, a conductive adhesive 21c. Additionally, in the illustrated example, the temperature sensor is mounted within the recess with its long side parallel to the long side of the container. However, the orientation of the temperature sensor is not limited to this; for example, it can also be mounted with its long side parallel to the short side of the container.
[0091] In the case of this crystal oscillator 10, since the oscillation frequency of the crystal oscillator is corrected on the chipset side based on the temperature information detected by the temperature sensor 17, the target frequency can be obtained with higher accuracy. Furthermore, since the pedestal 15 of the present invention is included, the following effects are achieved.
[0092] 1-2. Function and effect of pedestal 15
[0093] Next, the effect of the pedestal 15 will be explained with reference to Figures 2(A) to 2(C). In the case of the crystal oscillator 10 including the pedestal 15 of the present invention, as shown in Figure 2(B), in the region of the thickness reduction portion 15z, the spacing between the crystal oscillator 11 and the pedestal 15 widens towards the center side of the piezoelectric oscillator (right-hand direction in Figure 2(B)). That is, as shown in Figure 2(B), the spacing between the crystal oscillator 11 and the pedestal 15 is g1 in the part without the thickness reduction portion 15z, and in contrast, in the part with the thickness reduction portion 15z, the spacing gradually widens from g1 to g2 (g2 > g1). Therefore, if a first conductive adhesive 21a is applied to the upper surface of the base 15 and the crystal oscillator 11 is placed thereon, although the first conductive adhesive 21a flows towards the center of the crystal oscillator 11 between the base 15 and the crystal oscillator 11, the presence of a thickness reduction portion 15z widens the gap between the base and the piezoelectric oscillator, making it difficult for it to flow towards the center of the crystal oscillator 11. Instead, the thickness of the first conductive adhesive 21a increases at the thickness reduction portion 15z (g2 in FIG. 2(B)). Therefore, since the first conductive adhesive 21a is difficult to flow towards the center of the crystal oscillator 11, the deterioration of the electrical characteristics of the crystal oscillator 10 and short circuits between the excitation electrodes can be prevented. Furthermore, since the thickness of the first conductive adhesive 21a near the thickness reduction portion 15z increases, the crystal oscillator 11 becomes correspondingly difficult to peel off from the base 15, thereby improving impact resistance. Regarding impact resistance, the following is particularly important when a silicone-based adhesive is used as the first conductive adhesive 21a. For silicone-based conductive adhesives, the thicker the adhesive, the more elastic it can achieve and the better it can exhibit improved impact resistance, thus making it easier to improve impact resistance.
[0094] In contrast, as shown in FIG2(C), in the case of a pedestal 25 on a single flat plate without a thickness reduction section 15z, i.e., in the comparative example, the first conductive adhesive 21a easily reaches the center side of the crystal oscillator 11. Furthermore, due to the lack of a thickness reduction section, the first conductive adhesive 21a has low accumulation properties, making it difficult to increase the thickness. Therefore, in the comparative example, the effects described in the present invention cannot be obtained.
[0095] 1-3. Modifications of the pedestal
[0096] In the first embodiment, the thickness reduction section 15z is an inclined surface at the end of the crystal vibrator 11 on the center side of the pedestal 15, with the thickness inclined towards the center side at a constant angle. Furthermore, the thickness reduction section has an inclined surface on each of the two opposing main surfaces of the pedestal. However, the structure of the thickness reduction section is not limited to the above example and various modifications can be made. Several modified examples will be described below with reference to Figures 4(A) to 4(E). Also, in the pedestals shown in Figures 4(A) to 4(E), similarly to those in Figures 1(A) to 1(C) and Figures 2(A) to 2(C), the transverse direction of the paper is parallel to the X-axis of the crystal, and the direction perpendicular to the paper is parallel to the Z' axis of the crystal.
[0097] Figure 4(A) shows an example of a base 15 where an inclined surface extends from one of the main surfaces of the base 15, forming the thickness reduction section 15z1 of the present invention. For the purposes of the invention, the thickness reduction section only needs to be on the side of the base where the crystal oscillator is bonded; therefore, Figure 4(A) corresponds to the example described therein. However, since the thickness reduction section is only on the side of the base where the crystal oscillator is bonded, it is preferable to provide the thickness reduction section on both sides of the base 15, as care must be taken not to mix up the front and back of the base when mounting it in a container. These examples are shown below.
[0098] The pedestal 15 shown in Figure 4(B) is an example of a pedestal with a gradually decreasing thickness 15z2 formed at the end of the pedestal by a plurality of tilt angles, and in the example, tilt surfaces a and b with different tilt angles.
[0099] The pedestal 15 shown in Figure 4(C) is an example of a thickness reduction section 15z3 composed of a surface with constant curvature or multiple curvatures.
[0100] The pedestal 15 shown in Figure 4(D) is an example of a thickness-reducing section 15z4 consisting of a substantially vertical step D and an inclined or curved surface illustrated in Figures 4(B) and 4(C) above, which is connected thereto and has a reduced thickness.
[0101] The pedestal 15 shown in Figure 4(E) is an example in which the thickness reduction portion is included at both ends of the pedestal 15 along the X-axis of the crystal. Specifically, it is an example in which the thickness reduction portion 15z5 is included at one end and the thickness reduction portion 15z6 is included at the other end.
[0102] For the purpose of application, the thickness reduction section only needs to be located at the end of the crystal oscillator on the center side of the stage, but it can also be provided at both ends of the stage as shown in Figure 4(E). In this case, for example, when mounting the stage on a container, the degree of freedom of orientation is increased. In addition, the stage shown in Figure 4(E) with thickness reduction sections at both ends is also convenient in this respect because it can be easily manufactured from an AT-cut crystal wafer using photolithography and wet etching techniques. The thickness reduction sections 15z5 and 15z6 can be the same shape or different shapes. However, when the stage is formed from an AT-cut crystal wafer using photolithography and wet etching techniques, the thickness reduction sections 15z5 and 15z6 become different shapes due to the anisotropy of the crystallization axis of the crystal relative to the wet etching solution. Specifically, if the angle of the closed portion of the thickness reduction section located on the positive X-axis side of the crystal is defined as θ1 (refer to Figure 4(D)), and the angle of the closed portion of the thickness reduction section located on the negative X-axis side of the crystal is defined as θ2, then θ1 > θ2. Furthermore, θ1 is typically around 110 degrees, specifically around 105 to 115 degrees, and θ2 is typically around 64 degrees, specifically around 60 to 70 degrees. It can be said that both the thickness reduction section 15z5 and the thickness reduction section 15z6 are preferred shapes in terms of preventing the flow of the first conductive adhesive and increasing the thickness. Regarding the arrangement direction of the stage, whether the θ1 side or the θ2 side is the center side of the crystal oscillator can be selected according to the design, for example, based on how to set the effect of preventing the conductive adhesive from flowing and the thickness of the adhesive.
[0103] 1-4. Preferred examples of using crystal pedestals as pedestals
[0104] 1-4-1. Preferred Configuration Example
[0105] The pedestal 15 is preferably made of a crystal sheet with the same cutting angle as the crystal oscillator 11, and preferably the two are arranged in such a way that the crystal axis of the crystal oscillator 11 is parallel to the crystal axis of the crystal pedestal 15. This is because, since the difference in the coefficients of thermal expansion between the pedestal and the crystal oscillator becomes closer, the characteristic degradation caused by the difference in coefficients of thermal expansion can be mitigated. The preferred pedestal and the arrangement example for the crystal oscillator will be described below with reference to Figures 5(A) and 5(B).
[0106] Figure 5(A) illustrates the pedestal when the AT-cut crystal oscillator 11 is connected to the pedestal 15 at two locations along the X-axis of the crystal. Specifically, it illustrates a preferred pedestal where the crystal oscillator 11 has its long side along the Z'-axis and its short side along the X-axis, with cantilever support provided on the short side. Here, the Z'-axis represents the deviation from the true Z-axis of the crystal based on the AT-cutting angle.
[0107] In this case, the pedestal can take two structures. One is a pedestal 15p made of AT-cut crystal wafers, as shown in the lower left of Figure 5(A), which includes wiring patterns 15a at two locations along the X-axis of the crystal. The other is a pedestal 15q made of Z-cut crystal wafers, as shown in the lower right of Figure 5(A), which also includes wiring patterns 15a at two locations along the X-axis of the crystal.
[0108] Regarding the crystal oscillator 11 and the mounting base 15p or 15q, the mounting base 15p or 15q is bonded to the pad 13c (see Figure 2(A) etc.) with the X-axis of the crystals parallel to each other, and the crystal oscillator 11 is bonded to the mounting base 15p or 15q. However, the parallel X-axis of the crystals can be in the same direction (as shown in Figure 5(A)) or in the opposite direction, i.e., the mounting bases are arranged in reverse order in Figure 5(A).
[0109] Figure 5(B) is an explanatory diagram of the pedestal 15r in which the crystal oscillator 11 is connected to the pedestal 15r at two locations along the Z' axis of the crystal. That is, it is an explanation of a preferred pedestal when the crystal oscillator 11 has its long side along the X-axis of the crystal and its short side along the Z' axis, and the short side is cantilevered. In this case, the pedestal 15r is an example in which the Z' axis of the crystal is included in the plane and the crystal oscillator 11 can be connected to the pedestal 11 at two locations along the Z' axis.
[0110] Regarding the crystal oscillator 11 and the base 15r, the base is bonded to the bonding pads and the crystal oscillator 11 is bonded to the base in a positional relationship where the Z' axes of the two crystals are parallel. However, the positional relationship where the Z' axes of the two crystals are parallel can be either when the X-axis directions of the two crystals are the same (as shown in Figure 5(B)) or when the X-axis directions of the two crystals are opposite, i.e., the case where the bases are arranged in reverse order in Figure 5(B).
[0111] 1-4-2. Effects of setting it as the preferred configuration
[0112] Next, the effects of using the crystal oscillator 11 and the base 15 with the preferred configuration of the crystallization axis as described above will be explained.
[0113] The inventors of this application have fabricated multiple crystal oscillators 10 (exemplary examples) as described in Figures 1(A) to 1(C) and Figures 5(A) and 5(B), as well as crystal oscillators without a mounting base, i.e., crystal oscillators formed by directly bonding a crystal oscillator 11 to one end of an adhesive pad 13c using a silicone conductive adhesive (comparative example). Both the exemplary and comparative examples were fabricated using a so-called 1612-size ceramic package. In both examples and comparative examples, the AT-cut crystal oscillators used for the experiments were rectangular in top view with their long side along the X-axis of the crystal, a so-called X-length crystal oscillator, and were sized to fit within a 1612-size ceramic package. The oscillation frequency was 76.8 MHz (the thickness of the crystal oscillator was approximately 22 μm), and they had specified excitation electrodes. The specific dimensions of the crystal oscillators used were: X dimension approximately 0.75 mm, Z' dimension approximately 0.51 mm. Furthermore, the platform used in the embodiment is an AT-cut crystal wafer with an X dimension of 1.0 mm, a Z' dimension of 0.8 mm, and a thickness of 40 μm. Here, the so-called 1612-size ceramic package refers to a package with a long side dimension of approximately 1.6 mm and a short side dimension of approximately 1.2 mm, and its internal structure is as illustrated in Figures 1(A) to 1(C).
[0114] Next, the hysteresis characteristics of the frequency-temperature characteristics of the samples in these examples and comparative examples were measured. Here, the hysteresis characteristics of the frequency-temperature characteristics refer to the difference between the frequency-temperature characteristics of the crystal oscillator during heating and cooling when the temperature of the crystal oscillator with a built-in temperature sensor is raised from t1 degrees to tn (tn > t1) degrees and then immediately dropped back to t1 degrees. Although the figures are omitted, the measurements were performed using a temperature control device, a frequency measuring device, and a temperature measuring device. The temperature control device includes a substrate with a Peltier element and a temperature control unit that controls the temperature of the Peltier element.
[0115] Specifically, the samples of the embodiments and comparative examples were connected to a substrate having a Peltier element. A frequency measuring device was connected to the external connection terminal of this sample (the terminal connected to the crystal oscillator 11 in 13e of FIG. 1(C)), and a temperature measuring device was connected to the terminal connected to the temperature sensor 17.
[0116] Next, using a temperature control device, the temperature of the Peltier element is increased from t1 degrees to tn (tn > t1) degrees at specified temperature intervals and under specified heating conditions, and then immediately cooled back to t1 degrees under the same temperature change conditions as during the heating. The actual temperatures of the crystal oscillator 10 during the heating and cooling processes are measured using a temperature sensor 17 and a temperature measuring device, and the frequency of the crystal oscillator 11 is measured using a frequency measuring device. Based on these measurements, the frequency-temperature characteristics during heating and cooling are extracted.
[0117] Next, the frequency difference between the frequency-temperature characteristics during heating and cooling at the same temperature is calculated, which is the frequency hysteresis information. The average value of the frequency difference is then calculated for each evaluation sample.
[0118] Furthermore, using these average values, the average, maximum, and minimum values of the frequency differences of the sample group of the embodiments and the average, maximum, and minimum values of the frequency differences of the sample group of the comparative examples were determined. These results are shown in Table 1. Additionally, the frequency difference is expressed in ppm, which is the ratio obtained by dividing the frequency difference by the oscillation frequency. According to Table 1, regarding the frequency difference during heating and cooling as defined above, when comparing the average values, the average value of the embodiments is 0.06 / 0.026 ≈ 0.23 compared to the comparative examples, approximately one-fifth smaller. Regarding the maximum value, the average value of the embodiments is 0.09 / 0.96 ≈ 0.09 compared to the comparative examples, also approximately one-eleventh smaller.
[0119] [Table 1]
[0120]
[0121] Unit: ppm
[0122] 1-4-3. The material of the pedestal and the crystallization axis of the pedestal
[0123] Furthermore, as another evaluation, the following evaluation based on the finite element method was performed. Four analytical models were created, which were finite element method models simulating the crystal oscillator 10 illustrated in Figures 1(A) to 1(C). The crystallographic axis conditions of the crystal, the material of the pedestal, and the crystallographic axis conditions were set with respect to the orientation of the two bonding points of the AT-cut crystal oscillator as shown in Table 2 below. The von Mises stress generated at the center point of the crystal oscillator in each analytical model was calculated when the temperature of each analytical model was varied from 25°C to 105°C. The results are shown in Table 2.
[0124] [Table 2]
[0125]
[0126] As shown in Table 2, the stress generated at the center of the crystal oscillator due to the temperature change is approximately 366 kPa to 386 kPa in analytical models 1 and 2, while it is approximately 10 kPa in analytical models 3 and 4, which is about one-thirty-seventh of that. It can be seen that if a crystal pedestal with an appropriate axial relationship is used relative to the crystallographic axis corresponding to the line segment connecting the two bonding points of the crystal oscillator, i.e., a crystal pedestal with a crystallographic axis suitable for this crystallographic axis, the stress can be reduced.
[0127] Therefore, based on the results in Table 1 and Table 2, it can be seen that appropriately selecting AT-cut crystal pedestals or Z-cut crystal pedestals as pedestals, considering the bonding direction of the two points of the AT-cut crystal oscillator, is effective in reducing the thermal stress of the bonding structure of the crystal oscillator.
[0128] 1-4-4. Discussion on the Thickness of Crystal Mounts
[0129] Regarding the preferred thickness of the pedestal when using a crystal pedestal, the inventors of this application have conducted in-depth research and found that there is a preferred thickness.
[0130] That is, as another evaluation based on the finite element method, the influence of the thickness of the crystal stage on the stress in the crystal oscillator was investigated. Specifically, a large number of analytical models were fabricated. These models had the same basic structure as analytical models 3 and 4 in Table 2, but with a frequency of 153.6 MHz, and a model with the same basic structure as analytical model 4, but with a frequency of 52 MHz. The thickness T of the AT-cut crystal stage was varied in 10 μm increments between 10 μm and 80 μm. Furthermore, the von Mises stress generated at the center point of the crystal oscillator in each model was calculated when the temperature of each analytical model was varied from 25°C to 105°C. Figure 6 The graph shows the results, with the horizontal axis representing the platform thickness and the vertical axis representing the stress values (relative values).
[0131] according to Figure 6 It is evident that in all analytical models, if the pedestal thickness exceeds 20 μm, the stress decreases sharply. Furthermore, in all models, the stress reaches a minimum near a pedestal thickness of 30 μm, and remains relatively low with a slight increase until a thickness of approximately 60 μm. Beyond 60 μm, a saturation or slight decrease tendency is observed. The tendency for the stress to be minimal within the 30 μm–60 μm range is more pronounced in the 76.8 MHz and 153.6 MHz models than in the 52 MHz model. However, it can be said that even with different frequencies, the tendency for the stress to be minimal within the 30 μm–60 μm range, as seen in analytical models 3 and 4, is the same regardless of whether the crystal oscillator is X-length or Z'-length, or whether the pedestal is an AT-cut crystal plate or a Z-plate. Increasing the pedestal thickness leads to an increase in the thickness of the crystal oscillator itself and increases the cost of the pedestal, thus making it less desirable. Taking all these factors into account, it can be said that the thickness of the crystal platform can be selected between 30 μm and 60 μm.
[0132] Considering the above aspects, when taking into account the thickness of the base, the present invention is preferably applied to oscillation frequencies of 50 MHz or higher, including 50 MHz, 76 MHz, and 153 MHz bands. Furthermore, the smaller the container, the smaller the piezoelectric vibrator, and thus the influence of stress becomes significant. Therefore, the present invention is preferably applied to the so-called 1210 type, which includes the aforementioned 1612 type and has a long side of approximately 1.2 mm and a short side of approximately 1.0 mm, the so-called 1008 type, which has a long side of approximately 1.0 mm and a short side of approximately 0.8 mm, and smaller types, in terms of container dimensions.
[0133] 2. Second Implementation Form
[0134] Next, the second embodiment will be described. The difference between the second embodiment and the first embodiment is that the invention is applied to an H-shaped crystal oscillator with a built-in temperature sensor. Figure 7 This is an explanatory diagram, which is a cross-sectional view of the crystal oscillator 30 of the second embodiment, corresponding to the cross-sectional view in FIG1(B).
[0135] The first chamber, in which the crystal oscillator 11 is mounted, and the second chamber, in which the temperature sensor 17 is mounted, are stacked back-to-back, with the first chamber being airtight. Inside the first chamber, the pedestal 15 and the crystal oscillator 11 of the present invention are mounted in the same manner as in the first embodiment.
[0136] 3. Third Implementation Form
[0137] Next, the third implementation form will be explained. Figure 8 This is an explanatory diagram, which is a cross-sectional view of the crystal oscillator 40 of the third embodiment, corresponding to the cross-sectional view in Figure 1(B).
[0138] The first and second embodiments described above are examples of applying the present invention to a crystal oscillator with a built-in temperature sensor, but the crystal oscillator 40 in the third embodiment is an example of applying the present invention to a single crystal oscillator without a built-in temperature sensor.
[0139] The pedestal 15 and the crystal oscillator 11 of the present invention are mounted in the recess 13a containing the crystal oscillator 11 in the same manner as in the first embodiment.
[0140] 4. Fourth Implementation Form
[0141] Next, the fourth implementation form will be explained. Figure 9 This is an explanatory diagram, which is a cross-sectional view of the crystal oscillator 50 of the fourth embodiment, corresponding to the cross-sectional view in Figure 1(B).
[0142] The fourth embodiment of the crystal oscillator 50 is a crystal oscillator that includes a semiconductor chip 51 containing an oscillation circuit that causes the crystal vibrating plate 11 to oscillate within the recess 13a.
Claims
1. A piezoelectric device, comprising: The piezoelectric vibrating plate, when viewed from above, has a quadrilateral shape; Container for mounting the piezoelectric vibrating plate; A base is disposed between the piezoelectric vibrating sheet and the container at a predetermined portion along the first side of the piezoelectric vibrating sheet; a first conductive adhesive is used to bond the piezoelectric vibrating sheet and the base. And a second conductive adhesive, for bonding the base and the container. The end of the platform on the center side of the piezoelectric vibrating sheet in a second direction orthogonal to the first side includes a thickness reduction portion whose thickness decreases toward the center side.
2. The piezoelectric device according to claim 1, characterized in that, The thickness-reducing portion includes an inclined surface that slopes toward the center side at a constant angle.
3. The piezoelectric device according to claim 1, characterized in that, The thickness-reducing section includes inclined surfaces that are inclined toward the center side at multiple different inclination angles.
4. The piezoelectric device according to claim 1, characterized in that, The thickness-reducing portion includes a surface that is inclined toward the central side with a constant curvature or multiple curvatures.
5. The piezoelectric device according to claim 1, characterized in that, The thickness-reducing section includes a substantially vertical step and an inclined or curved surface connected thereto, whose thickness decreases toward the central side.
6. The piezoelectric device according to claim 1, characterized in that, The pedestal includes at both ends of a gradually decreasing thickness portion that decreases outward along the second direction.
7. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is an AT-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the X-axis of the crystal of the crystal oscillator is parallel to the X-axis of the crystal of the pedestal.
8. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is a Z-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the X-axis of the crystal of the crystal oscillator is parallel to the X-axis of the crystal of the pedestal.
9. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is an AT-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the Z' axis of the crystal of the crystal oscillator is parallel to the Z' axis of the crystal of the pedestal, wherein the Z' axis refers to the axis that deviates from the true Z-axis of the crystal according to the cutting orientation of the AT cut.
10. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is an AT-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the X-axis of the crystal of the crystal oscillator is parallel to the X-axis of the crystal of the pedestal. The thickness of the base is selected from the range of 30 μm to 60 μm.
11. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is a Z-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the X-axis of the crystal of the crystal oscillator is parallel to the X-axis of the crystal of the pedestal. The thickness of the base is selected from the range of 30 μm to 60 μm.
12. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is an AT-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the Z' axis of the crystal of the crystal oscillator is parallel to the Z' axis of the crystal of the pedestal. The thickness of the pedestal is selected from the range of 30 μm to 60 μm, where the Z' axis refers to the axis that deviates from the true Z-axis of the crystal according to the cutting orientation of the AT cut.
13. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is an AT-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the X-axis of the crystal of the crystal oscillator is parallel to the X-axis of the crystal of the pedestal. Along the designated portion of the first side, the first conductive adhesive, the base, the second conductive adhesive, and the crystal oscillator overlap in the vertical direction. The first conductive adhesive and the second conductive adhesive are both silicone-based conductive adhesives. The thickness of the base is selected from the range of 30 μm to 60 μm.
14. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is an AT-cut crystal wafer with a thickness decreasing towards the outside along the X-axis of the crystal and closing at both ends. When the angle of the closed portion of the thickness reduction section on the positive X-axis side of the crystal is defined as θ1, and the angle of the closed portion of the thickness reduction section on the negative X-axis side of the crystal is defined as θ2, then θ1 > θ2. The crystal oscillator and the pedestal are arranged such that the Z' axis of the crystal of the crystal oscillator is parallel to the Z' axis of the crystal of the pedestal. Along the designated portion of the first side, the first conductive adhesive, the base, the second conductive adhesive, and the crystal oscillator overlap in the vertical direction. The first conductive adhesive and the second conductive adhesive are both silicone-based conductive adhesives. The thickness of the pedestal is selected from the range of 30 μm to 60 μm, where the Z' axis refers to the axis that deviates from the true Z-axis of the crystal according to the cutting orientation of the AT cut.
15. The piezoelectric device according to claim 1, characterized in that, The piezoelectric vibrator is an AT-cut crystal vibrator, and the platform is an AT-cut crystal wafer. The crystal oscillator and the pedestal are arranged such that the X-axis of the crystal of the crystal oscillator is parallel to the X-axis of the crystal of the pedestal, or the Z' axis of the crystal of the crystal oscillator is parallel to the Z' axis of the crystal of the pedestal. The first conductive adhesive and the second conductive adhesive are both silicone-based conductive adhesives. The thickness of the base is selected from the range of 30 μm to 60 μm. In the piezoelectric device, the container is rectangular in shape when viewed from above. The container has the following dimensions: the long side is 1.6 mm and the short side is 1.2 mm; the long side is 1.2 mm and the short side is 1.0 mm; the long side is 1.0 mm and the short side is 0.8 mm; or smaller. The Z' axis refers to the axis that deviates from the true Z-axis of the crystal according to the cutting orientation of the AT cut.
16. The piezoelectric device according to any one of claims 1 to 15, characterized in that, The piezoelectric device is a piezoelectric vibrator comprising the piezoelectric vibrator, the base, a container for mounting the piezoelectric vibrator and the base, and a cover member for sealing the container.
17. The piezoelectric device according to any one of claims 1 to 15, characterized in that, The piezoelectric device is a piezoelectric oscillator comprising the piezoelectric vibrating plate, the base, a semiconductor chip containing the oscillation circuit of the piezoelectric vibrating plate, a container for mounting the piezoelectric vibrating plate, the base and the semiconductor chip, and a cover member for sealing the container.
18. The piezoelectric device according to any one of claims 1 to 15, characterized in that, The piezoelectric device is an H-shaped piezoelectric device with a built-in temperature sensor, comprising: a first chamber for mounting a piezoelectric vibrating plate; a second chamber, the bottom surface of which is connected to the first chamber and used for mounting a temperature sensor; a base and the piezoelectric vibrating plate, mounted in the first chamber; and the temperature sensor, mounted in the second chamber.
Citation Information
Patent Citations
Crystal vibrator of surface mount type
JP2000031773A
Crystal device
JP2010135890A
Element for crystal oscillator, crystal oscillator, and electronic component
JP2013085298A