A circuit board and a laser radar

By designing a double-layer solder resist ink layer on the lidar circuit board, using high-content inorganic filler materials and inorganic light-absorbing materials, and optimizing the material composition and surface structure, the problem of light straying was solved, and the detection performance of lidar was improved.

CN123164643APending Publication Date: 2026-11-24SUTENG INNOVATION TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510669817.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-22
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

The high reflectivity of the solder resist ink layer on existing lidar printed circuit boards leads to severe optical stray light problems, affecting the detection performance of high-precision lidar.

Method used

A double-layer solder resist ink layer structure is adopted. The second solder resist ink layer contains a high proportion of inorganic filler and inorganic light-absorbing material. By optimizing the material composition and surface structure, the reflectivity is reduced.

Benefits of technology

It significantly reduces the light reflectivity of the circuit board surface, effectively solves the problem of light straying, and improves the detection performance of lidar.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123164643A_ABST
    Figure CN123164643A_ABST
Patent Text Reader

Abstract

This invention discloses a circuit board and a lidar. The circuit board includes a substrate, a conductive pattern layer, a first solder resist ink layer, and a second solder resist ink layer. The conductive pattern layer is located between the substrate and the first solder resist ink layer, and the first solder resist ink layer is located between the conductive pattern layer and the second solder resist ink layer. The reflectivity of the second solder resist ink layer is lower than that of the first solder resist ink layer. By employing a double-layer solder resist ink layer structure, and using a second solder resist ink layer with a high content of inorganic filler material or inorganic light-absorbing material, this invention optimizes the material composition and surface structure, achieving high-efficiency light absorption and low-reflection characteristics. This significantly reduces the light reflectivity of the circuit board surface and effectively solves the problem of internal light straying in lidar.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to the field of circuit board manufacturing, and in particular to a circuit board and a lidar. Background Technology

[0002] In lidar systems, over 80% of the surface area of ​​the printed circuit board (PCB) is covered by a solder resist layer. The high surface reflectivity of the solder resist layer exacerbates the stray light problem within the lidar system. Current technologies typically use matte ink instead of glossy ink to reduce diffuse reflection, and black ink instead of green ink to increase light absorption, thereby reducing the PCB's surface reflectivity.

[0003] However, the effect of using matte black ink instead of green ink in suppressing stray light is limited. Due to limitations in the content and composition of its filler materials, matte black solder resist ink has a smooth surface and low roughness, resulting in still relatively high surface reflectivity. It can only reduce light reflectivity by about 20%, which is insufficient to effectively suppress stray light inside the lidar system. This fails to meet the requirements of lidar systems for reducing internal optical strays, especially in high-precision lidar applications where optical strays will severely affect the detection performance of the lidar. Summary of the Invention

[0004] The main technical problem solved by the embodiments of the present invention is to provide a circuit board and its lidar, which can solve at least some of the defects existing in the printed circuit boards of lidar.

[0005] In a first aspect, embodiments of the present invention provide a circuit board, including a substrate, a conductive pattern layer, a first solder resist ink layer, and a second solder resist ink layer; the conductive pattern layer is located between the substrate and the first solder resist ink layer, the first solder resist ink layer is located between the conductive pattern layer and the second solder resist ink layer, and the reflectivity of the second solder resist ink layer is less than the reflectivity of the first solder resist ink layer.

[0006] In some embodiments, the second solder resist ink layer includes a resin matrix and an inorganic filler material, wherein the inorganic filler material in the second solder resist ink layer accounts for more than or equal to 70% by weight; the inorganic filler material in the second solder resist ink layer includes a first inorganic filler material and a second inorganic filler material, wherein the first inorganic filler material accounts for more than or equal to 50% by weight and the second inorganic filler material accounts for more than or equal to 10% by weight.

[0007] In some embodiments, the first inorganic filler material is silica particles, and the average particle size of the silica particles is greater than 0.3 micrometers and less than 10 micrometers. When the particle size is less than 0.3 micrometers or greater than 10 micrometers, the specific surface area will decrease, which is not conducive to reducing light reflectivity. The second solder resist ink layer adopts a densely arranged inorganic filler material structure, wherein the first inorganic filler material (silica particles) and the second inorganic filler material form a tightly packed microstructure, which effectively increases the surface roughness and light absorption path.

[0008] In some embodiments, 10% of the silica particles have a particle size less than or equal to 1 micrometer, and 90% of the silica particles have a particle size less than or equal to 7 micrometers. By controlling the particle size distribution, it is ensured that the silica particles can form an uneven structure on the surface of the solder resist ink layer, causing light to undergo multiple reflections and absorptions on the surface of the second solder resist ink layer or after entering the second solder resist ink layer, thereby reducing the overall reflectivity.

[0009] In some embodiments, the second inorganic filler material is one or more of barium sulfate, insulating carbon black, and insulating carbon nanotubes, wherein 90% of the particles in the particle size distribution of the second inorganic filler material have a particle size less than or equal to 2 micrometers. The second inorganic filler material mainly fills the gaps between the first inorganic filler material, further improving the light absorption efficiency. Its particle size is controlled within a small range, which is beneficial for forming a uniform and compact microstructure.

[0010] In some embodiments, the second solder resist ink layer includes a resin matrix, an inorganic filler, and an inorganic light-absorbing material; the inorganic light-absorbing material in the second solder resist ink layer accounts for more than 25% by weight, and the inorganic filler material in the second solder resist ink layer accounts for less than 5% by weight. By controlling the high content of the inorganic light-absorbing material, the light absorption capacity of the solder resist ink layer can be significantly enhanced, and the light reflectivity can be reduced.

[0011] In some embodiments, the inorganic filler material comprises one or more combinations of silica particles and barium sulfate, and the inorganic light-absorbing material comprises one or more combinations of insulating carbon black and insulating carbon nanotubes. Both insulating carbon black and insulating carbon nanotubes in the inorganic light-absorbing material exhibit excellent light absorption properties. Choosing insulating materials rather than conductive materials ensures that the electrical insulation performance of the circuit board is not affected.

[0012] In some embodiments, the total thickness of the first solder resist ink layer and the second solder resist ink layer is between 15 and 45 micrometers.

[0013] In some embodiments, the thickness of the first solder resist ink layer is 10 to 40 micrometers, and the thickness of the second solder resist ink layer is 5 to 30 micrometers.

[0014] In a second aspect, embodiments of the present invention provide a lidar, including a receiving unit, a transmitting unit, and a circuit board as described in the first aspect.

[0015] The beneficial effects of the embodiments of the present invention are as follows: Unlike the prior art, the embodiments of the present invention adopt a double-layer solder resist ink layer structure. The second solder resist ink layer adopts a high content inorganic filler material or inorganic light-absorbing material. By optimizing the material composition and surface structure, high efficiency light absorption and low reflection characteristics are achieved, which can significantly reduce the light reflectivity of the circuit board surface and effectively solve the problem of light straying inside the lidar. Attached Figure Description

[0016] One or more embodiments are illustrated by way of example with reference to the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements having the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.

[0017] Figure 1 This is a schematic diagram of the structure of a circuit board provided in an embodiment of this application;

[0018] Figure 2 It shows Figure 1 The circuit board shown is composed of a first solder resist ink layer and a second solder resist ink layer.

[0019] Figure 3 This is a schematic diagram of another circuit board structure provided in an embodiment of this application;

[0020] Figure 4 It shows Figure 3 The circuit board shown is composed of a first solder resist ink layer and a second solder resist ink layer.

[0021] Figure 5 This is a schematic diagram of another circuit board structure provided in the embodiments of this application;

[0022] Figure 6 It shows Figure 5 The circuit board shown has a second solder resist layer. Detailed Implementation

[0023] To facilitate understanding of this application, a more detailed description is provided below with reference to the accompanying drawings and specific embodiments. It should be noted that when an element is described as being "fixed to" another element, it can be directly on the other element, or one or more intermediate elements may exist between them. When an element is described as being "connected" to another element, it can be directly connected to the other element, or one or more intermediate elements may exist between them. The terms "upper," "lower," "inner," "outer," "bottom," etc., used in this specification indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application. Furthermore, the terms "first," "second," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0024] Unless otherwise defined, all technical and scientific terms used in this specification have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used in this specification is for the purpose of describing particular embodiments only and is not intended to limit the scope of this application. The term "and / or" as used in this specification includes any and all combinations of one or more of the associated listed items.

[0025] Furthermore, the technical features involved in the different embodiments of this application described below can be combined with each other as long as they do not conflict with each other.

[0026] In lidar systems, over 80% of the PCB surface is covered by a solder resist layer. The high surface reflectivity of this solder resist layer exacerbates stray light issues within the lidar system. Current technologies typically use matte ink instead of glossy ink to reduce diffuse reflection and black ink instead of green ink to increase light absorption, thereby reducing the PCB's surface reflectivity. However, the effect of using matte black ink to suppress stray light is limited. Due to limitations in its filler content and composition, matte black solder resist has a smooth surface and low roughness, resulting in still relatively high surface reflectivity. It can only reduce light reflectivity by about 20%, which is insufficient to effectively suppress stray light within the lidar system. This fails to meet the requirements of lidar systems for reducing internal stray light, especially in high-precision lidar applications, where stray light issues will severely impact the lidar's detection performance.

[0027] To address the above problems, in one embodiment, such as Figure 1As shown, this application provides a circuit board. The circuit board includes a substrate 100, a first solder resist layer 300, and a second solder resist layer 400. The circuit board also includes a plurality of exposed conductive elements 220 and a conductive pattern layer 210. The surface of the conductive pattern layer 210 is covered by the solder resist layer. The conductive pattern layer 210 is located between the substrate 100 and the first solder resist layer 300, and the first solder resist layer 300 is located between the conductive pattern layer 210 and the second solder resist layer 400. The reflectivity of the second solder resist layer 400 is less than that of the first solder resist layer 300.

[0028] In some embodiments, the substrate 100 may be made of conventional printed circuit board substrates such as FR-4 (epoxy glass cloth laminate), high-frequency laminate (such as composite materials containing polytetrafluoroethylene), ceramic substrate, metal substrate, and flexible substrate materials (such as polyimide, polyester). Exposed conductive elements 220 include exposed copper contacts or wire structures formed by exposed copper areas. The conductive pattern layer 210 is typically formed by etching copper foil and is used to achieve electrical connections in the circuit.

[0029] In some embodiments, the first solder resist ink layer 300 is a conventional solder resist ink layer, primarily used to protect the conductive pattern layer from oxidation, damage, or contamination. The solder resist ink layer also provides electrical insulation properties. A conventional solder resist ink layer refers to a protective layer formed from standard solder resist ink materials widely used in the manufacturing process of printed circuit boards (PCBs). A conventional solder resist ink layer mainly consists of a resin matrix (typically epoxy resin, polyurethane resin, acrylic resin, or mixtures thereof), flame retardants, photoinitiators, curing agents, inorganic fillers, and colorants. The resin matrix forms the skeleton of the solder resist ink layer, directly affecting adhesion, chemical resistance, and mechanical strength. Inorganic fillers are generally used to adjust the viscosity, hardness, and thermal stability of the ink, including one or more combinations of materials such as silica, alumina, barium sulfate, talc, or insulating carbon black.

[0030] It is worth noting that conventional solder resist ink layers have limitations in optical performance, especially in applications such as lidar that are particularly sensitive to light straying. While traditional black solder resist ink has a higher absorbance than green ink, it still retains a relatively high reflectivity. Therefore, a second solder resist ink layer 400 is added. In one embodiment, such as... Figure 2As shown, the second solder resist ink layer 400 includes a resin matrix, an inorganic filler, and an inorganic light-absorbing material. The resin matrix serves as a binder and forms a film, and can be epoxy resin or other resin materials suitable for printed circuit boards. The inorganic light-absorbing material in the second solder resist ink layer 400 accounts for more than 25% by weight, while the inorganic filler material accounts for less than 5% by weight. By controlling the high content of the inorganic light-absorbing material, the light absorption capacity of the solder resist ink layer can be significantly enhanced, and the light reflectivity can be reduced.

[0031] Inorganic filler materials can include one or more combinations of silica particles and barium sulfate, while inorganic light-absorbing materials can include one or more combinations of insulating carbon black and insulating carbon nanotubes. A weight percentage (greater than 30%) of inorganic light-absorbing materials results in a total carbon content in the ink exceeding 90% (by weight), effectively improving light absorption. For example, it exhibits over 90% absorption for light at a wavelength of 940 nm (corresponding to the wavelength of the emitted laser in a lidar system). Both insulating carbon black and insulating carbon nanotubes in the inorganic light-absorbing materials possess excellent light absorption properties. Choosing insulating materials rather than conductive materials ensures that the electrical insulation performance of the circuit board remains unaffected.

[0032] The first solder resist ink layer 300 serves as a base layer, primarily providing electrical protection and insulation. Its material composition and thickness ensure good adhesion to the copper surface and substrate. Using the first solder resist ink layer 300 as a base layer has multiple technical necessities and advantages. The second solder resist ink layer 400, as a functional layer, primarily provides optical absorption, reducing reflectivity. The second solder resist ink layer 400 contains a high proportion (greater than 30%) of inorganic light-absorbing materials. When the content of these materials increases to a carbon content exceeding 90%, it significantly affects the adhesion between the solder resist ink and the substrate. The compatibility between solder resist ink layers is better than the compatibility between solder resist ink layers and the substrate. The adhesion between the second solder resist ink layer 400 and the first solder resist ink layer 300 is greater than the adhesion between the second solder resist ink layer 400 and the substrate 100. Using the first solder resist ink layer 300 as an intermediate transition layer ensures good adhesion between the overall structure and the substrate.

[0033] In practical applications, the first solder resist ink layer 300 is usually coated onto the conductive pattern layer 210 by screen printing and then prepared by pre-curing, exposure, development and curing processes; subsequently, the second solder resist ink layer 400 is coated onto the first solder resist ink layer 300 by a similar process to form a double-layer solder resist ink structure.

[0034] Unlike existing technologies, the circuit board structure provided in this invention, through the design of a double-layer solder resist ink structure, effectively enhances the absorption capacity of the solder resist ink layer for laser, significantly reducing the surface reflectivity of the circuit board from over 50% to less than 5%, effectively reducing optical stray light, effectively solving the optical stray light problem in lidar, and helping to improve the detection performance of lidar.

[0035] In one embodiment, such as Figure 3 The diagram shows another circuit board structure. The circuit board includes a substrate 100, a first solder resist layer 300, and a second solder resist layer 400. The circuit board also includes multiple exposed conductive elements 220 and a conductive pattern layer 210. The surface of the conductive pattern layer 210 is covered by the solder resist layer. The conductive pattern layer 210 is located between the substrate 100 and the first solder resist layer 300, and the first solder resist layer 300 is located between the conductive pattern layer 210 and the second solder resist layer 400. The reflectivity of the second solder resist layer 400 is less than that of the first solder resist layer 300.

[0036] Different from Figure 1 The circuit board shown. Figure 3 The circuit board shown in the exhibition achieved a honeycomb surface structure by adjusting the material ratio and microstructure design, which significantly improved the surface roughness of the solder resist ink layer and effectively reduced the surface emissivity of the circuit board.

[0037] In one embodiment, such as Figure 4 As shown, the second solder resist ink layer 400 includes a resin matrix and an inorganic filler material. The resin matrix can be a polymer material such as epoxy resin or photosensitive resin, used to provide the film-forming properties and structural support of the ink. The inorganic filler material in the second solder resist ink layer 400 accounts for more than or equal to 70% by weight, which is much higher than the content of no more than 40% inorganic filler material in conventional PCB solder resist ink layers.

[0038] In one embodiment, the inorganic filler material in the second solder resist ink layer 400 includes a first inorganic filler material and a second inorganic filler material. The weight percentage of the first inorganic filler material is greater than or equal to 50%, and the weight percentage of the second inorganic filler material is greater than or equal to 10%. By controlling the ratio of the two different inorganic filler materials, an uneven structure, such as a honeycomb structure, is formed on the surface of the second solder resist ink layer, which effectively enhances the light scattering and absorption capabilities of the solder resist ink layer.

[0039] In some embodiments, the first inorganic filler material is silica particles, which are spherical or near-spherical or other shapes, possessing good chemical stability and transparency, and can significantly increase the specific surface area of ​​the solder resist ink layer. The average particle size of the silica particles is greater than 0.3 micrometers and less than 10 micrometers. When the particle size is less than 0.3 micrometers or greater than 10 micrometers, the specific surface area will decrease, which is not conducive to reducing light reflectivity. Figure 4 The second solder resist ink layer 400 shown in the image adopts a densely arranged inorganic filler material structure, in which the first inorganic filler material (silica particles) and the second inorganic filler material form a tightly packed microstructure, which effectively increases the surface roughness and light absorption path.

[0040] In some embodiments, the particle size distribution of the silica particles is precisely controlled, with a D10 particle size of 1 micrometer and a D90 particle size of 7 micrometers. The D10 and D90 particle sizes in the particle size distribution are two key parameters describing the population size distribution of particles, representing the 10% and 90% quantiles of the cumulative distribution, respectively. The D10 particle size indicates that 10% of the particles in the particle size distribution have a particle size less than or equal to this value. For example, if the D10 particle size of the silica particles is 1 micrometer, it means that 10% of the particles in the sample have a particle size less than or equal to 1 micrometer, while 90% of the particles have a particle size greater than 1 micrometer. The D90 particle size indicates that 90% of the particles in the cumulative particle size distribution have a particle size less than or equal to this value. For example, a D90 particle size of 7 micrometers means that 90% of the particles in the sample have a particle size less than or equal to 7 micrometers, and only 10% of the particles have a particle size greater than 7 micrometers.

[0041] By controlling the particle size distribution, it is ensured that the silica particles can form an uneven structure on the surface of the second solder resist ink layer. This causes light to undergo multiple reflections and absorptions on or after entering the second solder resist ink layer, thereby reducing the overall reflectivity. The second inorganic filler material is one or more combinations of barium sulfate, insulating carbon black, and insulating carbon nanotubes, wherein the D90 particle size of the second inorganic filler material is 2 micrometers. The second inorganic filler material mainly fills the gaps between the first inorganic filler material, further improving the light absorption efficiency. Its particle size is controlled within a small range, which is beneficial for forming a uniform and compact microstructure.

[0042] In the embodiments of this application, both insulating carbon black and insulating carbon nanotubes possess excellent light absorption properties, while barium sulfate can enhance the durability and anti-aging properties of the material. A reasonable combination of multiple materials can achieve effective absorption of light of different wavelengths.

[0043] In practical applications, the inorganic filler content of the second solder resist ink layer 400, exceeding 70%, ensures that the surface is essentially covered by the filler material, while the resin content is relatively low, thus forming... Figure 3 and Figure 4The microstructure shown is as follows. The tiny gaps and fine surface irregularities formed between the filler material particles constitute a "honeycomb" surface or an irregular surface containing other irregularities, which effectively increases the scattering and absorption paths of light on the surface.

[0044] To further explain, the inorganic filler content of conventional PCB solder resist inks is typically no more than 40%, and their surfaces are mainly covered by resin, resulting in smooth surfaces, low roughness, and high surface reflectivity. In contrast, this embodiment alters the surface microstructure of the solder resist ink layer by adjusting the material ratio, achieving a transformation from "smooth surface" to "rough surface," effectively reducing light reflectivity and improving light absorption efficiency.

[0045] In one embodiment, the preparation process is briefly described as follows: First, a first inorganic filler material (silica particles) and a second inorganic filler material (such as insulating carbon black) are mixed in a predetermined ratio, and then thoroughly stirred with a resin matrix to produce a solder resist ink with a high inorganic filler content. Subsequently, the second solder resist ink layer 400 is coated onto the surface of the first solder resist ink layer 300 using a screen printing process. After pre-curing, exposure, development, and curing, a surface layer with a special microstructure is formed. Actual measurements have verified that the circuit board structure in this embodiment can reduce the light reflectivity from over 50% of the traditional structure to less than 5%, reducing light straying by more than 90%, and significantly improving the detection performance and ranging accuracy of the lidar.

[0046] In summary, this embodiment introduces a high content of inorganic filler material into the second solder resist ink layer 400, and in particular, precisely controls the ratio and particle size distribution of the first inorganic filler material (silicon dioxide particles) and the second inorganic filler material, forming a special microscopic surface structure that achieves efficient light absorption and provides an ideal circuit board solution for photosensitive applications such as lidar.

[0047] In one embodiment, the inorganic filler material of the second solder resist ink layer 400 includes barium sulfate, silica particles, insulating carbon black, and insulating carbon nanotubes. Barium sulfate serves as an interstitial filler. Silica particles are used to form an irregular structure on the surface of the second solder resist ink layer 400, increasing surface roughness. Insulating carbon black and insulating carbon nanotubes, as inorganic light-absorbing materials, effectively enhance the light absorption capacity of the second solder resist ink layer 400, especially the wavelength of the laser emitted by the lidar, such as 905 nm or 940 nm.

[0048] In some embodiments, considering structural integrity and manufacturing process compatibility, the total thickness of the first solder resist ink layer 300 and the second solder resist ink layer 400 is controlled within the range of 15 to 45 micrometers. In one embodiment, the thickness of the first solder resist ink layer 300 is 10 to 40 micrometers, and the thickness of the second solder resist ink layer 400 is 5 to 30 micrometers.

[0049] In one embodiment, such as Figure 5 As shown, another schematic diagram of a circuit board structure is provided. The circuit board includes a substrate 100, exposed conductive elements 220, a conductive pattern layer 210, and a third solder resist ink layer 500, wherein the third solder resist ink layer 500 is in direct contact with the substrate 100 to form a single-layer high light absorption structure. Figure 5 In the demonstrated structure, the third solder resist ink layer 500 employs a design with a high content of inorganic light-absorbing material, directly covering the substrate 100 to form a highly efficient light absorption layer. This structure is suitable for specific applications with lower requirements for circuit protection but extremely high requirements for optical absorption. For example... Figure 6 As shown, the third solder resist ink layer 500 includes a resin matrix, a first inorganic filler material, and a second inorganic filler material. Unlike the previous embodiments, the third solder resist ink layer 500 in this embodiment is in direct contact with the substrate 100, without the need for a first solder resist ink layer as a transition layer, thereby simplifying the circuit board manufacturing process.

[0050] Figure 6 The third solder resist ink layer 500 shown employs a densely packed inorganic filler material structure. The first and second inorganic fillers form a tightly packed microstructure, effectively increasing surface roughness and light absorption paths. The total content of inorganic fillers in the third solder resist ink layer 500 can reach over 70% (by weight), with the first inorganic filler accounting for over 50% and the second inorganic filler accounting for over 10%. This high filler content ensures that the surface is primarily composed of filler material particles, rather than being completely covered by resin, thus creating a rough surface structure and significantly reducing light reflectivity.

[0051] In this embodiment, the first inorganic filler material can be spherical silica particles, and the second inorganic filler material can be one or more combinations of barium sulfate, insulating carbon black, or insulating carbon nanotubes. The average particle size of the silica particles is greater than 0.3 micrometers and less than 10 micrometers. The particle size distribution of the silica particles is precisely controlled, with a D10 particle size of less than 1 micrometer and a D90 particle size of less than 7 micrometers. The D90 particle size of the second inorganic filler material is less than 2 micrometers. The second inorganic filler material mainly fills the gaps between the first inorganic filler material, further improving the light absorption efficiency. Its particle size is controlled within a small range, which is beneficial for forming a uniform and compact microstructure.

[0052] The third solder resist ink layer 500 in this embodiment can be used directly as a single functional layer without the need for an additional solder resist layer, simplifying the manufacturing process while maintaining excellent optical performance. However, in applications with high circuit protection requirements, adding an additional solder resist protective layer can still be considered.

[0053] In one embodiment, the type, particle size, and ratio of the first and second inorganic filler materials can be adjusted according to specific needs to optimize optical performance. For example, for applications requiring the absorption of specific wavelengths of light, targeted absorption effects can be achieved by adjusting the composition of the filler materials.

[0054] To further explain, in this embodiment, the third solder resist ink layer 500 can be directly coated onto the surface of the substrate 100 using processes such as screen printing, coating, or spraying. After pre-curing, exposure, and thermal curing, a light-absorbing layer with a special microstructure is formed. Compared to traditional multilayer structures, the single-layer structure of this embodiment simplifies the manufacturing process and reduces production costs.

[0055] For those skilled in the art, it will be understood that the single-layer high-fill material structure of this embodiment is particularly suitable for scenarios with extremely high requirements for optical performance and relatively low requirements for electrical protection, such as non-critical circuit areas or dedicated light absorption areas in lidar systems.

[0056] In some embodiments of this application, the single-layer high-fill material structure of this embodiment can be combined with the double-layer structure of the aforementioned embodiment according to actual application needs, and different structural designs can be adopted in different areas of the same circuit board to meet the diverse needs of complex applications.

[0057] In summary, this embodiment achieves highly efficient light absorption through the design of a special single-layer high-fill material structure, providing a simplified and efficient solution for specific application scenarios. This structure not only boasts advantages such as simple manufacturing processes and relatively low cost, but also maintains excellent optical absorption performance, making it another effective way to optimize the optical performance of circuit boards.

[0058] In one embodiment, a lidar is provided. The lidar includes a receiving unit, a transmitting unit, and a circuit board as described in any of the foregoing embodiments.

[0059] Specifically, the transmitting unit of a lidar system is used to transmit laser signals, and the receiving unit is used to receive the reflected laser signals. The circuit board is used to support and connect the electronic components of the transmitting and receiving units, forming a complete lidar system.

[0060] In some embodiments, the circuit board is a transmitting circuit board with a transmitting unit or a transmitting chip mounted on it. Alternatively, the circuit board is a receiving circuit board with a receiving unit or a receiving chip mounted on it. Or, both the transmitting and receiving units are mounted on the same circuit board, meaning the transmitting and receiving components of the lidar share a single circuit board. The use of a circuit board with low surface reflectivity can effectively solve the problem of optical stray light within the lidar, thereby improving the lidar's detection performance.

[0061] LiDAR can be applied to autonomous vehicles, robots, drones, surveying equipment, and other fields. In these applications, the system has high requirements for ranging accuracy and detection reliability. The use of low-reflectivity circuit boards greatly improves the performance of LiDAR in complex environments.

[0062] The above embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit it. Under the concept of this application, the technical features of the above embodiments or different embodiments can also be combined, the steps can be implemented in any order, and there are many other variations of different aspects of this application as described above. For the sake of brevity, they are not provided in detail. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. These modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.

Claims

1. A circuit board, characterized in that, It includes a substrate, a conductive pattern layer, a first solder resist ink layer, and a second solder resist ink layer. The conductive pattern layer is located between the substrate and the first solder resist ink layer, the first solder resist ink layer is located between the conductive pattern layer and the second solder resist ink layer, and the reflectivity of the second solder resist ink layer is less than that of the first solder resist ink layer.

2. The circuit board according to claim 1, characterized in that, The second solder resist ink layer includes a resin matrix and an inorganic filler material, wherein the inorganic filler material in the second solder resist ink layer accounts for more than or equal to 70% by weight; The inorganic filler material in the second solder resist ink layer includes a first inorganic filler material and a second inorganic filler material, wherein the weight percentage of the first inorganic filler material is greater than or equal to 50%, and the weight percentage of the second inorganic filler material is greater than or equal to 10%.

3. The circuit board according to claim 2, characterized in that, The first inorganic filler material is silica particles, and the average particle size of the silica particles is greater than 0.3 micrometers and less than 10 micrometers.

4. The circuit board according to claim 3, characterized in that, The particle size distribution of the silica particles shows that 10% of the particles have a diameter less than or equal to 1 micrometer, and 90% of the particles have a diameter less than or equal to 7 micrometers.

5. The circuit board according to claim 2, characterized in that, The second inorganic filler material is one or more of barium sulfate, insulating carbon black and insulating carbon nanotubes, wherein 90% of the particles in the particle size distribution of the second inorganic filler material have a particle size of less than or equal to 2 micrometers.

6. The circuit board according to claim 1, characterized in that, The second solder resist ink layer includes a resin matrix, an inorganic filler, and an inorganic light-absorbing material; The inorganic light-absorbing material in the second solder resist ink layer accounts for more than 25% by weight, and the inorganic filler material in the second solder resist ink layer accounts for less than 5% by weight.

7. The circuit board according to claim 6, characterized in that, The inorganic filler material includes one or more combinations of silica particles and barium sulfate, and the inorganic light-absorbing material includes one or more combinations of insulating carbon black and insulating carbon nanotubes.

8. The circuit board according to claim 1, characterized in that, The total thickness of the first solder resist ink layer and the second solder resist ink layer is between 15 and 45 micrometers.

9. The circuit board according to claim 8, characterized in that, The thickness of the first solder resist ink layer is 10 to 40 micrometers, and the thickness of the second solder resist ink layer is 5 to 30 micrometers.

10. A lidar, characterized in that, It includes a receiving unit, a transmitting unit, and a circuit board as described in any one of claims 1 to 9.