A cavity slot wall plane gold finger printed board and a manufacturing method thereof
By employing slot hole design and pulse electroplating full-fill hole and step-by-step controlled-depth milling process on the cavity wall, the standardization and reliability issues of gold finger processing on the cavity wall are solved, realizing low-cost and high-yield mass production, which is suitable for high-end packaging scenarios such as SiC power modules and high-power power supply modules for AI servers.
Patent Information
- Application Number
- CN202611527092.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-29
- Publication Date
- 2026-11-24
AI Technical Summary
Existing technologies cannot process standardized planar gold finger structures on the cavity groove wall, resulting in high equipment investment costs, poor spring adaptability, insufficient long-term contact reliability, low batch production yield, and difficulty in meeting the needs of large-scale production.
By adopting a slot design and pulse electroplating full-fill hole and step-by-step controlled-depth milling process, after processing and filling the inner layer slot with copper, controlled-depth milling exposes the straight long side, forming a regular rectangular pure metal plane gold finger contact. The entire process is completed by combining conventional PCB equipment, avoiding the need for special sidewall exposure equipment.
It has achieved low-cost, high-yield, and standardized mass production of cavity groove wall planar gold fingers, improved contact area and contact resistance stability, reduced production costs and equipment investment, and is suitable for a variety of high-end application scenarios.
Smart Images

Figure CN123164652A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of printed circuit board manufacturing technology, and particularly relates to a discrete planar slot wall gold finger structure and supporting manufacturing process for a printed circuit board with a built-in sunken cavity. It is mainly used in semiconductor packaging scenarios with stringent requirements for reliability and miniaturization, such as SiC silicon carbide power modules, AI server high-power power supply modules, high-speed optical communication packaging substrates, and cavity spring contact test carrier boards. Background Technology
[0002] With the rapid development of semiconductor devices towards higher power, higher integration, and thinner designs, recessed cavity printed circuit boards (PCBs) are being widely adopted. Embedding bare chips and power components within the PCB cavity significantly reduces packaging parasitic parameters and compresses the overall module assembly size. To achieve stable electrical interconnection between the cavity-embedded components and external circuits, gold finger contacts are machined on the vertical inner wall of the cavity, relying on spring-loaded contact points to ensure long-term stable power and signal conduction.
[0003] Currently, the industry mainly uses two mainstream solutions for machining cavity groove walls with gold fingers: Option 1: After the cavity is integrally formed, the entire board is copper plated, and the side wall circuit pattern is completed in conjunction with liquid photoresist spraying equipment and multi-axis tilting laser direct imaging (LDI) equipment. Option 2: Electroplating fills the through-hole circular hole. After forming, the substrate on one side is removed by controlled-depth milling along the center line of the through hole, exposing the semi-circular sidewall to form an arc-shaped groove wall conductive contact.
[0004] Neither of the two existing processes mentioned above can simultaneously meet the production and usage requirements of mass production, universal spring matching, and long-term reliable contact. The specific shortcomings are as follows: (1) Liquid photoresist spraying + multi-axis tilting LDI exposure process; The entire production line requires the purchase of specialized liquid photosensitive photoresist spraying equipment and multi-angle tilting laser exposure equipment, resulting in extremely high equipment purchase and maintenance costs. The entire process is complex, with frequent defects such as uneven ink coating thickness on the cavity sidewalls, false exposure edges, and residual development, leading to a low production yield. It is not suitable for large-scale mass production and faces significant challenges in industry adoption.
[0005] (2) Milling process for filling circular through holes in half; The contact points after milling are semi-cylindrical arc-shaped curved surfaces, which are incompatible with the industry standard flat gold finger structure and cannot be matched with the standardized springs on the market. The contact points only have local point contact, resulting in local pressure concentration. Long-term repeated pressing will quickly wear down the surface gold plating, causing the contact resistance to drift continuously, and the electrical reliability of the product is insufficient in the long term.
[0006] In addition, in existing stepped groove gold finger solutions, the gold fingers are usually set at the bottom of the stepped groove or at the plug position on the board edge, rather than on the vertical sidewall of the cavity. This makes it difficult to meet the application requirements of electrical interconnection between built-in components and external circuits on the sidewall of the cavity. Even if a few solutions attempt to make gold fingers on the sidewall of the cavity, they mostly rely on special equipment such as sidewall exposure, resulting in high process complexity and cost.
[0007] In summary, there is an urgent need in this field for a discrete gold finger processing technology for cavity groove walls that does not require high-end specialized equipment, has a standard planar contact structure, is compatible with universal springs, has excellent mass production capabilities, and provides stable and reliable long-term contact. Summary of the Invention
[0008] To overcome the problems of high equipment investment costs, non-standard contact structure, poor spring adaptability, insufficient long-term contact reliability, low yield in mass production, and high failure risk in existing technologies, the present invention discloses a cavity groove wall planar gold finger printed circuit board and its manufacturing method.
[0009] To achieve the above objectives, the present invention adopts the following technical solution: a cavity groove wall planar gold finger printing plate, the cavity groove wall planar gold finger printing plate comprising: A multilayer composite substrate body, wherein the substrate body has a recessed recessed cavity; The vertical inner wall of the cavity is independently spaced with multiple sets of planar gold finger contacts; The planar gold finger contact is formed by electroplating a slot through the thickness of the inner layer board, and then removing the outer substrate of the slot through controlled depth milling to expose the straight long side of the slot. The contact is a regular rectangular pure metal plane. The slot has rounded corners at both ends and is filled with a dense, non-porous electroplated copper layer. The surface of the planar gold finger contact is uniformly plated with a protective gold layer; The straight long side of the slot is arranged parallel to the sidewall of the cavity, and the length direction of the straight long side extends along the depth direction of the cavity; the contact surface of the planar gold finger contact is coplanar with the sidewall of the cavity.
[0010] Furthermore, the slot width is ≥0.6mm, and an insulating substrate isolation strip of ≥0.15mm is reserved between the sidewalls of adjacent slots. The multiple sets of planar gold finger contacts are electrically isolated by the insulating substrate isolation strip. The multiple sets of planar gold finger contacts are arranged at equal intervals along the horizontal direction of the cavity sidewall, and the center distance between adjacent planar gold finger contacts is 0.8mm~2.0mm.
[0011] Furthermore, the milling depth of the cavity is 1.0mm~2.0mm, the remaining substrate thickness at the bottom of the cavity is ≥0.4mm; the fillet radius at both ends of the slot is ≥0.3mm; the thickness of the protective gold layer is 0.5μm~1.0μm; the protective gold layer is a hard gold plating layer, and the hardness of the hard gold plating layer is 130HV~250HV.
[0012] Furthermore, the multilayer composite substrate body adopts a high-temperature resistant FR4 substrate with a Tg≥170℃, which is suitable for harsh working conditions such as high and low temperature cycling and high power heating. The interlayer prepreg of the multilayer composite substrate body is a high Tg halogen-free prepreg, wherein the high Tg halogen-free prepreg has a Tg ≥ 180℃ and a Z-axis CTE ≤ 50ppm / ℃.
[0013] Furthermore, a process clearance gap is reserved between the bottom of the slot and the substrate of the cavity bottom; the width of the process clearance gap is 0.1mm~0.3mm, which is used to avoid damage to the bottom copper layer circuit during milling.
[0014] Another object of the present invention is to provide a method for manufacturing the gold finger printed circuit board of the cavity groove wall, the method comprising the following steps: S1, Inner layer CNC machining of slot long holes: CNC milling to machine through-type long slot holes, the slot holes are arranged parallel to the side wall of the subsequent forming cavity with straight long sides, and the two ends of the slot are machined with rounded corners to eliminate stress concentration; S2, Slot Pulse Electroplating Full Filling: The process involves sequentially removing drilling debris and chemical copper plating activation. Then, a pulse reverse electroplating process is used to completely fill the slot holes with copper plating. After electroplating, the board surface is ground and leveled. X-ray non-destructive testing and metallographic section sampling are used to control the quality of the copper layer in the slot holes, ensuring that the copper layer in the slot is dense without excessive voids and that there are no depressions or defects at the slot opening. S3, Multilayer substrate hot pressing: The prepreg (PP) and the outer conductive copper foil are laminated. The multilayer substrate is pressed by a stepped heating hot pressing process to ensure that the interfaces of each layer are tightly bonded and to avoid the risk of thermal delamination. The stepped heating hot pressing process includes: In the first heating stage, the temperature is increased to 120-140℃ at a rate of 1.0-2.0℃ / min and held for 20-40min. In the second heating stage, the temperature is increased to 180-200℃ at a rate of 0.5-1.5℃ / min and held for 60-120min. Then, the temperature is decreased to room temperature at a rate of 1.0-3.0℃ / min. S4, Outer Layer Conventional Pattern Transfer: Through dry film lamination, standard vertical LDI exposure, development, etching, and film removal, the outer layer conductive circuitry is formed without the need for special tilting exposure equipment for the sidewalls. S5, Step-by-Step Deep Milling to Form the Cavity: The sunken cavity is machined using a multi-blade layered milling process, precisely controlling the milling depth to the design dimensions; the local insulating substrate within the cavity contour area and on the side of the slot facing the cavity is removed by milling, so that the straight long side of the slot is fully exposed on the vertical inner wall of the cavity, forming a standard rectangular planar metal contact. S6, Cavity Plasma Surface Treatment: Plasma cleaning removes milling dust and debris from the inside of the cavity, and simultaneously deburrs and micro-roughens the sidewalls of the flat gold fingers to improve the adhesion and surface uniformity of the subsequent gold plating layer. S7, Selective gold plating of contacts: Selective electroplating of gold on the gold finger area of the cavity sidewall plane to form a uniform, dense and wear-resistant gold plating layer; S8, Post-processing and Inspection: After removing the anti-plating dry film from the board surface, and completing the full appearance inspection and metallographic section sampling verification of the plating and structure, the solder resist printing, character production, and shape cutting and finishing are carried out in sequence to finally obtain the finished cavity groove wall plane gold finger printing board.
[0015] Furthermore, the slot width is ≥0.6mm, an insulating substrate isolation strip of ≥0.15mm is reserved between the side walls of adjacent slots, and the slot wall roughness Ra is controlled to ≤1.5μm; the alignment tolerance of the controlled depth milling is controlled within ±25μm to ensure the machining accuracy of the contact size; The multi-blade layered milling process includes two stages: rough milling and finish milling. The single cutting depth in the rough milling stage is 0.3~0.6mm, and the single cutting depth in the finish milling stage is 0.05~0.15mm. After being formed in steps S5 to S7, the planar gold finger contacts are used to repeatedly press and engage with standard spring contacts to achieve electrical conduction. Regarding the wear durability of the gold plating layer under this press-fitting engagement, the wear cycle life of the gold plating layer of the planar gold finger contacts is characterized by the following wear prediction model:
[0016] In the formula, The number of spring clip crimping cycles that the gold plating layer can withstand. The wear resistance constant of the gold plating layer. To protect the thickness of the gold layer, The coefficient of friction at the interface between the gold layer and the spring sheet is denoted as . This refers to the normal contact pressure applied by the spring sheet to the planar contact point. The crimping frequency is the number of times per unit time.
[0017] Furthermore, in step S2, the slot is fully filled using a pulsed reverse electroplating process instead of a copper paste plugging process, with a pure copper layer plated as the filling medium for the slot. The pulsed reverse electroplating process uses an acidic copper plating solution containing a leveling agent, an inhibitor, and an accelerator, with Cl in the plating solution. - The concentration is 40~80ppm.
[0018] To address the thermal expansion mismatch between the electroplated pure copper layer inside the slot and the surrounding substrate under service conditions, the thermal cycling interlayer stress at the interface between the copper-filled layer in the slot and the surrounding substrate is... The value is determined by the difference in the coefficient of thermal expansion between the electroplated pure copper layer and the substrate, and by the operating temperature cycle amplitude, and satisfies the following:
[0019] If the interlayer stress during thermal cycling is less than the interlayer bonding strength threshold at the interface between the prepreg and the copper layer, then:
[0020] In the formula, This refers to the interlayer stress caused by thermal cycling at the interface between the copper filler layer of the slot and the surrounding substrate due to the difference in the coefficients of thermal expansion. The elastic modulus of the electroplated pure copper layer. The coefficient of linear expansion of the electroplated pure copper layer is... is the equivalent linear expansion coefficient of the multilayer composite substrate. This represents the operating temperature cycle amplitude. This represents the interlayer bonding strength threshold at the interface between the prepreg and the copper layer.
[0021] Furthermore, in step S5, the rectangular planar metal contact formed by exposing the straight long side of the slot hole through controlled depth milling is a regular planar structure with a flatness of ≤0.05mm and a coplanarity tolerance of ≤±0.03mm between the contact sidewall and the cavity sidewall. Compared with the arc-shaped curved surface contact of the same size, it has a contact area gain. The contact area gain of the planar gold finger contact compared to the arc-shaped curved surface contact of the same size satisfies the following geometric relationship:
[0022]
[0023] In the formula, This represents the increase in contact area between a planar contact and a curved contact. For the contact width, Let be the radius of curvature of the arc-shaped curved surface contact point. The maximum offset arch height between the vertex of the curved surface and the plane. This represents the actual contact area of the planar contact point. This represents the theoretical contact area of the curved surface contacts of the same width.
[0024] Furthermore, in step S7, selective gold plating uses a 15-50 μm thick anti-plating dry film to cover the non-gold finger area, exposing only the gold finger contact area on the sidewall of the cavity for electroplating, forming a uniform and dense gold plating layer on the surface of the gold finger contact, wherein the surface roughness Ra of the gold plating layer is ≤0.10 μm. The regular rectangular pure metal planar structure ensures that the actual contact area when the planar gold finger contacts are pressed against the standard spring contact is larger than that of an arc-shaped curved surface contact of the same size, thereby reducing the total contact resistance. The following relationship must be satisfied:
[0025] In the formula, This is the total contact resistance. The volume resistivity of the gold plating layer. This is the equivalent conduction path length of the current within the planar contact. This represents the actual contact area of the planar contact point. It represents the surface contact resistance at the interface between the gold layer and the spring.
[0026] Combining all the above technical solutions, the beneficial effects of this invention are as follows: First, this invention abandons the traditional arc-shaped contact solution and special sidewall exposure equipment. Relying on conventional PCB mass production equipment, it processes cavity groove wall planar contacts that are consistent with the standard board edge gold finger structure, fundamentally solving the problems of curved surface point contact plating wear and contact resistance drift, and realizing low-cost, high-yield, standardized, and highly reliable mass production of cavity discrete planar gold fingers.
[0027] Secondly, compared with the prior art, the present invention has the following substantial improvements and technical advantages: 1. Achieve a standardized planar contact structure for the gold fingers on the cavity groove wall.
[0028] Relying on the rectangular planar contacts formed by the straight long side of the slot, the traditional curved surface point contact solution is completely abandoned; the contact shape and size are completely consistent with the industry's common board edge gold finger standard, and can be directly adapted to existing standardized spring contact assembly; the planar contact has a larger effective conduction area and more uniformly distributed contact pressure, which greatly reduces the wear rate of the gold plating layer, suppresses contact resistance drift under long-term operation, and significantly improves the stability of electrical connection.
[0029] 2. The process is highly versatile, significantly reducing mass production costs and barriers to entry.
[0030] The entire process uses only industry-standard PCB equipment, eliminating the need to purchase expensive specialized equipment such as liquid photoresist spraying and multi-axis tilting LDI. The entire process has a wide tolerance range, and the yield rate of mass production is stable and controllable, enabling large-scale manufacturing and significantly reducing equipment investment and overall production and processing costs.
[0031] 3. Flexible structural design, adaptable to a variety of high-end application scenarios.
[0032] By adjusting the length and width parameters of the slot, the contact area of the gold finger can be flexibly changed, taking into account both the requirements of precise interconnection of small signals and conduction of high-power current; it is compatible with various high-end packaged products with sunken cavities such as SiC power modules, high-speed optical modules, AI high-power power modules, and RF test carrier boards.
[0033] Third, the positive effects of this invention are also reflected in the following important aspects: 1. This invention can achieve large-scale mass production directly using existing general-purpose equipment in PCB factories, without the need for additional investment in expensive dedicated exposure equipment. The equipment investment for a single production line can be reduced by several million yuan, significantly reducing the manufacturing cost of cavity gold finger printed circuit boards.
[0034] With SiC power modules and AI server power modules as typical application scenarios, the number of cavity gold finger contacts in a single module is expected to reach dozens to hundreds. This invention achieves full compatibility between the contact structure and industry standard springs, so that downstream module assembly does not require customized springs, which greatly reduces the system-level assembly cost. It is expected to promote the large-scale commercial application of cavity embedded packaging technology in high-power and high-frequency scenarios, and has broad market application prospects.
[0035] 2. Currently, the processing solutions for gold fingers on cavity groove walls in the industry all have obvious technical defects. The liquid photoresist spraying solution relies on expensive special equipment and has a low yield rate. The circular through-hole half-milling solution can only obtain arc-shaped curved surface contacts and cannot be adapted to standard springs. Neither of them can simultaneously meet the dual requirements of "low-cost mass production" and "standardized planar contact structure".
[0036] This invention is the first to systematically integrate slot long slot design with pulse electroplating full-fill hole and step-by-step controlled-depth milling process. It utilizes the naturally straight long side of the slot to directly form the standard planar gold finger of the cavity sidewall, creating a new path for cavity slot wall gold finger processing technology that is different from the existing arc-shaped contact solution and dedicated sidewall exposure solution, filling the technical gap in mass manufacturing standard planar gold fingers of cavity sidewall on conventional PCB production lines.
[0037] 3. There has long been a desire in this field to form planar gold finger contacts on the sidewalls of the cavity that match standard spring contacts, but this has not yet been achieved. Existing technical solutions are limited by the precision of the sidewall exposure equipment and the defects of the arc-shaped milling structure, making it impossible to achieve low-cost, high-yield mass production while ensuring the standardization of the contact structure. The industry has generally attempted to alleviate the problem by upgrading the precision of the sidewall exposure equipment and optimizing the coating thickness of the arc-shaped contacts, but none of these methods have fundamentally overcome the technical bottleneck of "compatibility between planar contacts and conventional equipment."
[0038] This invention breaks away from the traditional technical thinking of "performing graphic processing inside the cavity" and creatively moves the graphic processing of gold fingers to the inner slot groove processing stage. Through the reverse process path of "first processing the slot groove on the periphery and completing the copper filling, and then controlling the depth of milling to expose the straight long edge", the standard planar contact points on the side wall of the cavity can be mass-produced with conventional equipment, fundamentally solving the above-mentioned technical problem that has not been successfully solved for a long time.
[0039] 4. A common technical bias in this field is that fabricating high-quality gold fingers on the vertical sidewalls of a cavity requires specialized sidewall patterning equipment such as liquid photoresist spraying or multi-axis tilting LDI exposure; otherwise, it is impossible to form fine circuit patterns on non-planar vertical sidewalls. Based on this bias, industry R&D investment has long focused on improving the accuracy of sidewall exposure equipment and specialized photosensitive materials, neglecting the possibility of circumventing the sidewall exposure requirement through structural design and process innovation.
[0040] This invention breaks through the traditional technical path of "must perform patterning on the sidewall after cavity forming" by reverse processing approach of prefabricating slots and exposing them after controlled-depth milling. It proves that standard planar gold fingers of cavity slot walls can be mass-produced on conventional PCB production lines without the need for special exposure equipment for sidewalls, effectively overcoming the above-mentioned technical biases. Attached Figure Description
[0041] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with the disclosure of this invention and, together with the description, serve to explain the principles of the disclosure of this invention. Figure 1 This is a three-dimensional cross-sectional view of the gold finger printed circuit board with a cavity groove wall provided in an embodiment of the present invention; Figure 2 This is a cross-sectional view of the controlled-depth milling forming cavity and exposed planar gold finger contact points provided in an embodiment of the present invention; Figure 3(a) is a schematic diagram of the long slot structure design provided in an embodiment of the present invention; Figure 3(b) is a schematic diagram of the etched circuit pattern provided in an embodiment of the present invention; Figure 3(c) is a schematic diagram of the gold finger formed by controlled depth milling according to an embodiment of the present invention; In the diagram: 1. Cavity; 2. Copper layer; 3. Prepreg; 4. Sidewall gold fingers; 5. Gold plating layer. Detailed Implementation
[0042] To make the above-mentioned objects, features, and advantages of the present invention more apparent and understandable, specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings. Many specific details are set forth in the following description to provide a thorough understanding of the present invention. However, the present invention can be practiced in many other ways different from those described herein, and those skilled in the art can make similar modifications without departing from the spirit of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.
[0043] The innovation of this invention lies in: (1) Product structure innovation: Standard planar contacts are formed by utilizing the naturally straight long side of the slot. A through-type long slot is used in combination with a pulse reverse electroplating full-filling process. The two ends of the slot are set with transition rounded corners and the bottom of the slot is reserved for process avoidance gaps. The insulating substrate on the outside of the slot is removed by multi-blade step-by-step precise depth control milling. The straight long side of the slot is fully exposed along the depth direction of the cavity to the vertical inner side wall of the cavity. The contact surface is coplanar with the side wall of the cavity, forming an integrated, dense and regular rectangular pure metal planar gold finger contact, which is different from the existing arc-shaped curved surface protrusion structure and stepped slot bottom gold finger solution.
[0044] (2) Process path innovation: Avoiding the need for dedicated sidewall exposure equipment by using reverse timing. The gold finger patterning step is moved from the sidewall processing stage after cavity forming to the inner layer slot processing stage. Through the reverse process path of "processing the slot first and filling it with copper, and then controlling the depth of milling to expose the straight long edge", the entire process does not require high-end dedicated equipment such as liquid photoresist spraying and multi-axis tilting LDI sidewall exposure. The entire process can be completed using only industry-standard PCB production line equipment, which greatly reduces the production line investment threshold and production cost.
[0045] (3) Quantitative design for reliability: The matching process combination and quantitative criteria ensure long-term stability. The matching process adopts step-by-step controlled milling (rough and finish staged cutting, alignment tolerance ±25μm), plasma sidewall pretreatment (O2+CF4 mixed atmosphere for deburring and micro-roughening), stepped heating hot pressing (two-stage temperature control curve), plasma sidewall pretreatment, and pulsed hole filling electroplating (acidic copper plating solution Cl). - A combination of processes (concentration 40~80ppm) was used to improve defects such as milling tearing at the tank wall contacts, delamination due to interlayer thermal cycling, and uneven coating thickness; a criterion for interlayer stress matching during thermal cycling was established. This improves the reliability of the tank wall structure under high and low temperature cycling conditions from "empirical estimation" to "quantitative design"; the flatness of the molded flat contact is ≤0.05mm, the coplanarity is ≤±0.03mm, and the surface roughness Ra of the gold plating layer is ≤0.10μm. It can be directly matched with general standard springs, with a larger contact area, more uniform pressure distribution, and significantly improved durability and reliability compared to traditional arc-shaped contacts.
[0046] (4) Material system synergy: Synergistic selection of high-temperature resistant substrate and low-CTE prepreg 3 (PP). The substrate adopts a high-temperature resistant FR4 substrate with Tg≥170℃, and the interlayer prepreg 3 is a high-Tg halogen-free material with Tg≥180℃ and Z-axis CTE≤50ppm / ℃, which is matched with the thermal stress criterion. Together, they form a dual material and mechanical protection system for the integrity of the contact structure under high and low temperature cyclic conditions.
[0047] Example 1, as Figure 1 and Figure 2 As shown, the cavity groove wall planar gold finger printed circuit board provided in this embodiment of the invention includes: A multilayer composite substrate body, wherein the substrate body has a recessed recessed cavity 1; The vertical inner wall of the cavity 1 is independently spaced with multiple sets of planar gold finger contacts; The planar gold finger contact is formed by electroplating a slot through the thickness of the inner layer board, and then removing the outer substrate of the slot through controlled depth milling to expose the straight long side of the slot. The contact is a regular rectangular pure metal plane. The slot has rounded corners at both ends, and the slot is filled with a dense electroplated copper layer 2 (electroplated hole-filling copper layer) without voids. The surface of the planar gold finger contact point is uniformly plated with a protective gold layer 5; The straight long side of the slot is arranged parallel to the side wall of the cavity 1, and the length direction of the straight long side extends along the depth direction of the cavity 1; the contact surface of the planar gold finger contact is coplanar with the side wall of the cavity 1.
[0048] Furthermore, the slot width is ≥0.6mm, and an insulating substrate isolation strip of ≥0.15mm is reserved between the sidewalls of adjacent slots. The multiple sets of planar gold finger contacts are electrically isolated by the insulating substrate isolation strip. The multiple sets of planar gold finger contacts are arranged at equal intervals along the horizontal direction of the sidewall of the cavity 1, and the center distance between adjacent planar gold finger contacts is 0.8mm~2.0mm.
[0049] Furthermore, the milling depth of the cavity 1 is 1.0mm~2.0mm, the remaining substrate thickness at the bottom of the cavity 1 is ≥0.4mm; the transition fillet radius at both ends of the slot is ≥0.3mm; the thickness of the protective gold layer is 0.5μm~1.0μm; the protective gold layer is a hard gold plating layer, and the hardness of the hard gold plating layer is 130HV~250HV.
[0050] Furthermore, the multilayer composite substrate body adopts a high-temperature resistant FR4 substrate with a Tg≥170℃, which is suitable for harsh working conditions such as high and low temperature cycling and high power heating. The interlayer prepreg 3 of the multilayer composite substrate body is a high Tg halogen-free prepreg 3, wherein the high Tg halogen-free prepreg has a Tg ≥ 180℃ and a Z-axis CTE ≤ 50ppm / ℃.
[0051] Furthermore, a process clearance gap is reserved between the bottom of the slot and the substrate of the cavity bottom; the width of the process clearance gap is 0.1mm~0.3mm, which is used to avoid damage to the bottom copper layer 2 circuit during milling.
[0052] It should be noted that, Figure 1 and Figure 2 In the same figures, the same reference numerals indicate the same component. Figure 1 In the middle, there is cavity 1, copper layer 2 (including inner circuit copper layer and slot hole filling copper layer), prepreg 3, and sidewall gold fingers 4. Figure 2 In the middle, there is a copper plating layer 2 for filling the slot, a prepreg 3, and a gold plating layer 5. Figure 2 The 5 in the middle is to distinguish it from Figure 1 The newly added structure.
[0053] Example 2, the manufacturing method of the cavity groove wall planar gold finger printed circuit board provided in this embodiment of the invention specifically includes the following steps: S1, Inner layer CNC machining of slot long holes: CNC milling is used to machine through-type elongated slot holes. The straight long side of the slot hole is arranged parallel to the side wall of the subsequent forming cavity 1. The two ends of the slot are machined with rounded corners to eliminate stress concentration. The slot width is ≥0.6mm, and an insulating substrate isolation strip of ≥0.15mm is reserved between the side walls of adjacent slot holes. The roughness Ra of the slot wall is controlled to be ≤1.5μm; preferably, the roughness Ra of the slot wall is controlled to be ≤0.8μm. The long slot hole structure design is shown in Figure 3(a).
[0054] S2, Slot Pulse Electroplating Full-Filling: The process involves sequentially removing drilling debris and chemical copper plating activation. A pulse reverse electroplating process is then used to completely fill the slots with copper. After electroplating, the board surface is ground and leveled. X-ray non-destructive testing and metallographic section sampling are used to control the quality of the copper layer 2 within the slots, ensuring that the copper layer 2 is dense, free of excessive voids, and that the slot openings are free of depressions. Pure copper layer 2 is used as the filling medium for the slots, employing an acidic copper plating solution containing leveling agents, inhibitors, and accelerators.
[0055] Preferably, the process parameters for the pulsed reverse electroplating are: forward pulse current density 1.5~2.5A / dm³. 2 Reverse pulse current density: 3.0~5.0 A / dm³ 2 The forward pulse conduction time is 10-30 ms, the reverse pulse conduction time is 1-3 ms, the duty cycle is 30%-70%, the electroplating temperature is 20-30℃, and the electroplating time is 60-180 min. The acidic copper plating solution contains 180-240 g / L copper sulfate pentahydrate, 40-80 g / L sulfuric acid, 40-80 ppm chloride ions, 5-15 mL / L leveling agent, 100-300 ppm inhibitor, and 0.5-2.0 ppm accelerator. After electroplating, a ceramic brush wheel is used to grind and level the board surface at a pressure of 1.0-2.5 kgf / cm². 2 Remove 5-15 μm of excess copper layer 2 from the board surface to ensure uniform copper layer 2 thickness. Only after X-ray non-destructive testing confirms that the copper layer 2 within the slot is fully filled and free of voids larger than 50 μm in diameter can the next step be performed.
[0056] It should be noted that, since the slot is a through-type long strip structure with a slot width ≥ 0.6 mm and penetrates the inner layer board thickness (typical board thickness 1.0~3.0 mm), the filling volume is much larger than that of conventional blind holes. Therefore, the electroplating time should be appropriately extended to 60~180 min to ensure that the copper layer 2 in the slot is completely filled without voids.
[0057] To address the thermal expansion mismatch between the electroplated pure copper layer 2 inside the slot and the surrounding substrate under service conditions, the interlayer stress at the interface between the copper filling layer 2 in the slot and the surrounding substrate is reduced due to thermal cycling. The coefficient of thermal expansion between the electroplated pure copper layer 2 and the substrate is determined by the difference in thermal expansion coefficients and the operating temperature cycle amplitude, and satisfies the following:
[0058] If the interlayer stress during thermal cycling is less than the interlayer bonding strength threshold at the interface between the prepreg 3 and the copper layer 2, then:
[0059] In the formula, The interlayer stress caused by thermal cycling at the interface between the copper filler layer 2 of the slot and the surrounding substrate due to the difference in the coefficient of thermal expansion. The elastic modulus of the electroplated pure copper layer 2 is given by [reference to a specific parameter]. The coefficient of linear expansion of the electroplated pure copper layer 2 is given. is the equivalent linear expansion coefficient of the multilayer composite substrate. This represents the operating temperature cycle amplitude. The threshold value for interlayer bonding strength at the interface between the prepreg 3 and the copper layer 2.
[0060] S3, Multilayer substrate hot pressing: The prepreg 3 (PP) and the outer conductive copper foil are laminated together. The multilayer substrate is pressed using a stepped heating hot pressing process to ensure a tight bond between the interfaces of each layer and avoid the risk of thermal delamination.
[0061] The stepped heating hot pressing process includes: In the first heating stage, the temperature is increased to 120-140℃ at a rate of 1.0-2.0℃ / min and held for 20-40 minutes. In the second heating stage, the temperature is increased to 180-200℃ at a rate of 0.5-1.5℃ / min and held for 60-120 minutes. After that, the temperature is decreased to room temperature at a rate of 1.0-3.0℃ / min.
[0062] S4, Outer Layer Conventional Pattern Transfer: The outer layer conductive circuitry is formed through a circuit process involving dry film lamination, standard vertical LDI exposure, development, etching, and film stripping, without the need for dedicated tilting exposure equipment for the sidewalls. The etched circuitry pattern is shown in Figure 3(b).
[0063] S5, Step-by-step controlled-depth milling to form cavity 1: The sunken cavity 1 is machined using a multi-blade layered milling process, precisely controlling the milling depth to the design dimension; the local insulating substrate within the contour area of cavity 1 and on the side of the slot facing cavity 1 is removed by milling, so that the straight long side of the slot is completely exposed on the vertical inner wall of cavity 1, forming a standard rectangular planar metal contact; the alignment reference for the controlled-depth milling adopts a preset positioning target in the plate, and the alignment tolerance is controlled within ±25μm to ensure the machining accuracy of the contact size. The plane of the gold finger formed by controlled-depth milling is shown in Figure 3(c).
[0064] Preferably, the controlled depth milling uses a flat-end mill or a fish-scale milling cutter with a diameter of 0.8~2.0mm, a milling cutter speed of 30000~60000rpm, and a feed rate of 200~600mm / min. In the rough milling stage, a milling cutter with a diameter of 1.2~2.0mm is used, with a single cutting depth of 0.3~0.6mm and a feed rate of 400~600mm / min; in the finish milling stage, a milling cutter with a diameter of 0.8~1.2mm is used, with a single cutting depth of 0.05~0.15mm, a feed rate of 200~400mm / min, and a finish milling allowance of 0.05~0.10mm. During the milling process, compressed air or coolant is used for cooling and chip removal, with a compressed air pressure of 0.4~0.6MPa.
[0065] The rectangular planar metal contact is formed by exposing the straight long side of the slot hole through controlled depth milling. The surface of the rectangular planar metal contact is a regular planar structure with a flatness of ≤0.05mm. The coplanarity tolerance between the sidewall of the contact and the sidewall of cavity 1 is ≤±0.03mm. Compared with the arc-shaped curved surface contact of the same size, it has a contact area gain. The contact area gain of the planar gold finger contact compared to the arc-shaped curved surface contact of the same size satisfies the following geometric relationship:
[0066]
[0067] In the formula, This represents the increase in contact area between a planar contact and a curved contact. For the contact width, Let be the radius of curvature of the arc-shaped curved surface contact point. The maximum offset arch height between the vertex of the curved surface and the plane. This represents the actual contact area of the planar contact point. This represents the theoretical contact area of the curved surface contacts of the same width.
[0068] S6, Plasma surface treatment of cavity 1: Plasma cleaning removes dust and debris from the inside of cavity 1, and simultaneously deburrs and roughens the surface of the flat gold finger sidewall to improve the adhesion and surface uniformity of the subsequent gold plating layer 5.
[0069] Preferably, the plasma surface treatment uses a radio frequency plasma treatment device with a radio frequency power of 500~1500W, a vacuum degree of 10~50Pa in the cavity 1, a treatment temperature of 40~60℃, and a treatment time of 5~15min; the plasma treatment atmosphere is a mixture of oxygen and carbon tetrafluoride, with an oxygen flow rate of 100~300sccm, a carbon tetrafluoride flow rate of 30~100sccm, and a volume ratio of oxygen to carbon tetrafluoride of 3:1~5:1; after plasma treatment, the water contact angle of the sidewall of the cavity 1 is ≤30°, and the surface roughness Ra is controlled at 0.3~0.8μm.
[0070] S7, Selective gold plating of contacts: Selective electroplating of gold on the gold finger area of the side wall of cavity 1 to form a uniform, dense and wear-resistant gold plating layer 5; Selective electroplating of gold uses a dry film with a thickness of 15~50μm to cover the non-gold finger area, the thickness of the dry film is preferably 25~40μm, only exposing the gold finger contact area of the side wall of cavity 1 for electroplating, forming a uniform and dense gold plating layer 5 on the surface of the gold finger contact, the surface roughness Ra of the gold plating layer 5 is ≤0.10μm.
[0071] The regular rectangular pure metal planar structure ensures that the actual contact area when the planar gold finger contacts are pressed against the standard spring contact is larger than that of an arc-shaped curved surface contact of the same size, thereby reducing the total contact resistance. The following relationship must be satisfied:
[0072] In the formula, Total contact resistance; The volume resistivity of the gold plating layer; The equivalent conduction path length of the current within the planar contact; This represents the actual contact area of the planar contact point. The surface contact resistance (i.e., film resistance) at the interface between the gold layer and the spring sheet is derived from the following physical sources: the extremely thin oxide film on the surface of the gold layer, the adsorbed contamination layer, and the interfacial barrier effect caused by the micro-roughness of the surface.
[0073] According to Holm's electrical contact theory, the total contact resistance Due to the shrinkage resistance With film resistance It consists of two parts, namely Among them, the shrinkage resistance The film resistance is Additionally, the aforementioned The four-terminal method (Kelvin test) was used to determine the following: a normal pressure of 1.0~3.0N was applied between the standard spring (beryllium copper alloy, gold-plated surface) and the flat gold finger contact, with an ambient temperature of 20~25℃ and a relative humidity of 40%~60%. It decreases with increasing normal contact pressure of the spring and increases with increasing surface roughness Ra of the gold plating layer 5. Within the parameter range of this invention (normal contact pressure)... The pressure is 10~50MPa, and the surface roughness Ra of the gold plating layer 5 is ≤0.10μm. The typical value range is 0.5~5.0mΩ.
[0074] After being formed in steps S5 to S7, the planar gold finger contact is used to repeatedly press and engage with a standard spring to achieve electrical conduction. Regarding the wear durability of the gold plating layer 5 under this press-fitting engagement, the wear cycle life of the gold plating layer 5 of the planar gold finger contact is characterized by the following wear prediction model:
[0075] In the formula, The number of spring clip crimping cycles that the gold plating layer can withstand; The wear resistance constant of the gold plating layer represents the volumetric wear rate of the gold plating layer under unit normal contact pressure and unit sliding distance, with dimensions in mm. 3 / (N·m) or equivalent dimension, The smaller the value, the better the wear resistance of the gold plating layer; To protect the thickness of the gold layer; The dynamic friction coefficient at the interface between the gold layer and the spring sheet; This refers to the normal contact pressure applied by the spring to the planar contact point; The crimping frequency is the number of times per unit time.
[0076] The theoretical basis of this wear prediction model is Archard's law of wear ( When this invention is applied to the gold finger-spring pressing scenario, the following engineering simplifications are made in sequence: the sliding distance of a single pressing is related to the spring travel and the coefficient of friction. Relatedly, the cumulative total sliding distance is proportional to the number of cycles. Normal load manifests as contact pressure. The product of the contact area and the wear resistance constant is incorporated into the wear resistance constant when the contact size is fixed. When the hardness is constant, the wear resistance life is directly proportional to the thickness of the gold plating layer. By combining and rearranging the above relationships, we obtain the simplified model. This model has been successfully applied in the field of predicting the wear life of electrical contact devices. This invention further extends it to the quantitative evaluation of the crimping cycle life of gold fingers on the cavity wall plane of cavity 1.
[0077] Preferably, the wear resistance constant of the gold plating layer The wear test was performed using a ball-disc friction and wear tester (refer to ASTM G99 standard or GB / T 12444 standard): The gold-plated sample 5 was fixed on a rotating disk and subjected to unidirectional sliding friction using a ball pin of the same material as the standard spring. A normal load F and a sliding distance L were applied. The wear volume of the gold plating was measured by X-ray fluorescence or a surface profilometer. ,but The test conditions were: normal load 1.0~3.0N, sliding speed 10~30mm / s, sliding distance ≥100m, ambient temperature 20~25℃, and relative humidity 40%~60%. For the hard gold plating (hardness 130~250HV) of this invention, the wear resistance constant... The typical value range is 1.0 × 10. -5 ~5.0×10 -4 mm 3 / (N·m).
[0078] S8, Post-processing and Inspection: After removing the anti-plating dry film from the board surface, and completing the full appearance inspection and metallographic section sampling verification of the plating and structure, the solder resist printing, character production, and shape cutting and finishing are carried out in sequence to finally obtain the finished cavity 1 groove wall plane gold finger printing board.
[0079] Preferably, the selection of the substrate material and the prepreg 3 is synergistic with the slot structure and hot-pressing process parameters: the high Tg FR4 substrate (Tg≥170℃) and the low CTE prepreg 3 (Z-axis CTE≤50ppm / ℃) can be fully cured and form a tight interlayer bond under stepped temperature hot pressing (maximum temperature 180~200℃), and the interlayer bond strength threshold is [not specified]. ≥150MPa; Value and pure copper plating layer 2 in Slot hole ≈110GPa, ≈17ppm / ℃) and substrate ( ≈10~14ppm / ℃) in the typical operating temperature range (-40℃~+125℃, Interlaminar stress generated at 165℃ Approximately 80~130MPa is matched, satisfying The reliability criterion is established. Based on this, to further quantify the safety margin of this criterion, a safety margin coefficient is defined. Based on the aforementioned material and process parameters, η≥1.15~1.88 indicates that the interlayer bonding strength has sufficient redundancy for thermal cycling stress, thereby ensuring that the tank wall contacts do not experience interlayer delamination failure under high and low temperature cycling conditions.
[0080] Comparative Example 1: DC electroplating for hole filling; A DC electroplating filling process was used to replace the pulse reverse electroplating full-filling process in step S2, with the remaining steps being the same as in Example 2, to obtain Comparative Sample 1. During the slot filling process of the DC electroplated filling sample, due to the uneven distribution of DC electroplating current, the plating growth rate at the slot inlet was significantly faster than that in the center area of the slot, which easily led to the formation of "clamp" defects or voids inside the slot. The density of the copper layer 2 inside the tank was lower than that of the pulse electroplated sample, and X-ray detection showed that the proportion of voids with a diameter >50μm was significantly higher than that in Example 2. After high and low temperature cycling tests, the probability of microcracks appearing at the contact interface of the tank wall was higher than that in Example 2.
[0081] DC plating uses a relatively stable and continuous DC current to deposit copper, making it easier for the current to concentrate at PCB edges, sharp corners, and areas with large exposed areas. For through-hole structures with large opening areas, such as slots, DC plating struggles to achieve a uniform copper layer distribution inside the slot, easily resulting in a "dog bone effect" (excessively thick plating at the entrance and insufficient plating in the center), leading to incomplete filling.
[0082] In contrast, pulse reverse electroplating, by periodically changing the current direction and current density, utilizes the "deposition-dissolution" self-leveling effect of the reverse pulse, combined with the synergistic adsorption of additives, to effectively improve the uniformity of current distribution inside the slot, thereby achieving dense, void-free filling of the copper layer 2 inside the slot.
[0083] Comparative Example 2: A circular through hole is filled and then milled in half; A circular through hole (with a diameter equal to the width of the slot) was used to replace the long slot hole. After electroplating to fill the hole, the substrate on one side was removed by controlled-depth milling along the center line of the through hole to expose the semi-circular sidewall as an arc-shaped contact point. The remaining steps were the same as in Example 2, and comparative sample 2 was obtained.
[0084] The contact of the comparative sample 2 is a semi-cylindrical arc-shaped curved surface structure. Contact resistance testing showed that the initial contact resistance of the arc-shaped curved surface contact was ≥10mΩ, significantly higher than that of the planar contact in Example 2 (≤5mΩ). After 500 pressing cycles, the contact resistance change rate of the arc-shaped curved surface contact was ≥30%, while that of Example 2 was ≤10%. Abrasion resistance testing of the gold plating layer 5 showed that the arc-shaped contact's gold plating layer 5 could only withstand 1 / 5 to 1 / 2 of the number of abrasion cycles compared to the planar contact.
[0085] The curved contact point after milling a half-circular through-hole is incompatible with the industry standard planar gold finger structure and cannot be matched with standardized springs on the market. The contact point only achieves local point contact (theoretical contact area). Much smaller than a planar contact point Localized pressure concentration caused rapid wear of the gold plating layer 5, resulting in continuous drift in contact resistance. In Example 2, the planar contact is formed by straight long sides through slot holes. The overall contact is a regular rectangular pure metal plane, resulting in a larger contact area and more uniform pressure distribution when pressed against a standard spring. Its wear resistance and contact stability are significantly better than those of the curved surface contact.
[0086] Comparative Example 3: Copper paste plugging process; In contrast, a copper paste plugging process was used to replace the pulse reverse electroplating full-filling process in step S2, with the remaining steps the same as in Example 2, to obtain Comparative Sample 3. Comparative Sample 3 underwent the same metallographic section analysis and high / low temperature cycling tests. The results showed that after the copper paste plugging sample was milled open in the slot wall, the internal resin pores were exposed, making it easy for the process chemicals to penetrate and leave residual corrosion at the interface. After 50 high / low temperature cycles (-40℃ to +125℃), the difference in thermal expansion coefficients between the copper paste and the pure copper layer 2 on the slot wall was significant, making it prone to interfacial micro-cracks and interlayer delamination. After 100 cycles, conductive copper powder detached, and the resistance to repeated friction and fatigue deteriorated, with the contact resistance increasing to more than three times the initial value. This made it only suitable for static welding conduction scenarios where repeated pressing of the spring contact was not required, and could not meet the high-reliability dynamic contact requirements of this invention. In contrast, the pulse electroplating full-filling sample of Example 2 maintained good interfacial bonding and stable contact resistance even after 500 high / low temperature cycles.
[0087] The following is a comprehensive cost comparison of Comparative Example 1, Comparative Example 2, and the technical solution of this invention, based on a production line with an annual output of 100,000 cavity-type gold finger printed circuit boards: (1) Equipment investment comparison: The liquid photoresist spraying + multi-axis tilt LDI exposure solution requires additional purchase of special spraying equipment and tilt exposure equipment, which increases the equipment investment of a single production line by about RMB 2 million to RMB 5 million; the circular through hole half milling solution does not require special exposure equipment, but the arc-shaped contact structure leads to a significant loss of yield in subsequent processes; the solution of this invention only uses industry-standard PCB equipment (conventional CNC milling machine, vertical electroplating line, standard LDI exposure machine, etc.), and does not require any special side wall processing equipment, so the equipment investment is the lowest among the three.
[0088] (2) Comparison of overall manufacturing costs: After small-batch trial production verification (trial production batch n=3, 100 pieces per batch), the overall yield of the gold finger process on the cavity 1 wall of the present invention reached 92%~95%, which is significantly higher than the 70%~80% of the liquid photoresist spraying solution (the main defects are uneven ink coating on the side wall, false edges after exposure, and residual development) and the 75%~85% of the circular through-hole half-milling solution (the main defects are out-of-tolerance milling dimensions of the arc contact and uneven coating thickness). Based on the overall yield, the effective cost per piece of the present invention is reduced by about 30%~50% compared with the liquid photoresist spraying solution and by about 15%~25% compared with the circular through-hole half-milling solution.
[0089] (3) Mass production efficiency comparison: The entire process of the present invention is fully compatible with conventional PCB production lines, without the need for additional equipment debugging and process development cycles, and can be directly relied on existing production lines to achieve rapid mass production introduction; while the liquid photoresist spraying solution requires the construction of a new dedicated production line or large-scale transformation of the existing production line, which extends the mass production introduction cycle by 3 to 6 months.
[0090] In the above embodiments, the descriptions of each embodiment have different focuses. For parts that are not described in detail or recorded in a certain embodiment, please refer to the relevant descriptions of other embodiments.
[0091] To further demonstrate the positive effects of the above embodiments, the present invention conducts the following tests on the gold finger printing plate of the cavity 1 groove wall plane prepared according to Embodiment 1 and Embodiment 2: (1) Metallographic section analysis: Metallographic sections were prepared along the contact points on the wall of cavity 1. The filling density, thickness uniformity, and interface bonding of the electroplated copper layer 2 in the slot were observed under a 200-500x optical microscope. The test standard referred to IPC-6012 "Qualification and Performance Specifications of Rigid Printed Circuit Boards", which requires that the electroplated copper layer 2 be free of visible voids, delamination, and cracks, and that the thickness deviation not exceed ±20% of the nominal thickness.
[0092] (2) Contact resistance test: The contact resistance of the flat gold finger contact and the standard spring contact after crimping was measured using the four-terminal method (Kelvin test). The test current was 100mA~1A, the normal pressure of the spring contact was 1.0~3.0N, and the number of crimping cycles was 0~500. The change curve of contact resistance with the number of crimping cycles was recorded. The contact resistance change of the same size arc-shaped curved surface contact under the same test conditions was compared.
[0093] (3) High and low temperature cycling test: Temperature cycling test was conducted according to JESD22-A104 standard, with a temperature range of -40℃ to +125℃, a holding time of 15 min, a transition time of ≤1 min, and 100 to 1000 cycles. After the test, metallographic sections were prepared to observe the delamination and cracking at the interface between the copper filling layer 2 in the slot and the substrate, and to verify the results. The effectiveness of the thermal stress matching criterion.
[0094] (4) Abrasion resistance test of gold plating layer 5: The reciprocating friction test of the spring sheet is adopted, with normal pressure of 1.0~3.0N, friction stroke of 2~5mm, and friction frequency of 10~30 times / min. The number of frictions when the gold plating layer 5 exposes the underlying copper is recorded and compared with the number of abrasion resistances of the arc-shaped curved gold plating layer 5 of the same thickness.
[0095] Test results show that the electroplated copper layer 2 inside the slot is dense and free of voids, with a copper filling rate ≥98%; the initial contact resistance of the planar gold finger contacts is ≤5mΩ, and the contact resistance change rate after 500 pressing cycles is ≤10%, which is superior to the arc-shaped curved surface contacts of the same size (initial contact resistance ≥10mΩ, change rate after 500 pressing cycles ≥30%); after 500 high and low temperature cycles, the contact interface shows no delamination or cracks, verifying that... The reliability of the thermal stress criterion; the wear resistance of the gold-plated layer 5 on the flat contact is 2 to 5 times that of the arc contact.
[0096] The above description is only a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any modifications, equivalent substitutions and improvements made by those skilled in the art within the scope of the technology disclosed in the present invention and within the spirit and principles of the present invention should be covered within the scope of protection of the present invention.
Claims
1. A gold finger printing plate with a cavity groove wall, characterized in that, The cavity groove wall planar gold finger printing plate includes: A multilayer composite substrate body, wherein the substrate body has a recessed recessed cavity (1). The vertical inner wall of the cavity (1) is independently spaced with multiple sets of planar gold finger contacts; The planar gold finger contact is formed by electroplating a slot through the thickness of the inner layer board, and then removing the outer substrate of the slot through controlled depth milling to expose the straight long side of the slot. The contact is a regular rectangular pure metal plane. The slot has rounded corners at both ends, and the slot is filled with a dense electroplated copper layer without voids (2). The surface of the planar gold finger contact is uniformly plated with a protective gold layer; The straight long side of the slot is arranged parallel to the side wall of the cavity (1), and the length direction of the straight long side extends along the depth direction of the cavity (1); the contact surface of the planar gold finger contact is coplanar with the side wall of the cavity (1).
2. The gold finger printing plate on the cavity groove wall according to claim 1, characterized in that, The slot width is ≥0.6mm, and an insulating substrate isolation strip of ≥0.15mm is reserved between the sidewalls of adjacent slots. The multiple sets of planar gold finger contacts are electrically isolated by the insulating substrate isolation strip. The multiple sets of planar gold finger contacts are arranged at equal intervals along the horizontal direction of the side wall of the cavity (1), and the center distance between adjacent planar gold finger contacts is 0.8mm~2.0mm.
3. The gold finger printing plate on the cavity groove wall according to claim 1, characterized in that, The milling depth of the cavity (1) is 1.0mm~2.0mm, the remaining substrate thickness at the bottom of the cavity (1) is ≥0.4mm; the radius of the transition fillet at both ends of the slot is ≥0.3mm; the thickness of the protective gold layer is 0.5μm~1.0μm; the protective gold layer is a hard gold plating layer, and the hardness of the hard gold plating layer is 130HV~250HV.
4. The gold finger printing plate on the cavity groove wall according to claim 1, characterized in that, The multilayer composite substrate body is made of high-temperature resistant FR4 substrate with Tg≥170℃. The interlayer prepreg (3) of the multilayer composite substrate body adopts a high Tg halogen-free prepreg, wherein the high Tg halogen-free prepreg has a Tg ≥ 180℃ and a Z-axis CTE ≤ 50ppm / ℃.
5. The gold finger printing plate for the cavity groove wall according to claim 1, characterized in that, A process clearance is reserved between the bottom of the slot and the substrate of the cavity (1) bottom; the width of the process clearance is 0.1mm~0.3mm, which is used to avoid damage to the bottom copper layer (2) circuit during milling.
6. A method for manufacturing a gold finger printed circuit board with a cavity groove wall as described in any one of claims 1 to 5, characterized in that, This method Includes the following steps: S1, inner layer CNC machining of slot long holes: CNC milling to process through-type long slot holes, the straight long side of the slot hole is arranged parallel to the side wall of the subsequent forming cavity (1), and the two ends of the slot are machined with rounded corners; S2, Slot Pulse Electroplating Full Filling: The drilling sludge removal and chemical copper plating activation treatments are performed in sequence. The Slot holes are completely filled with copper plating using pulse reverse electroplating technology. After electroplating, the board surface is ground and leveled. X-Ray non-destructive testing and metallographic section sampling are used to control the quality of the copper layer (2) in the Slot holes to ensure that the copper layer (2) in the Slot is dense without excessive voids and the slot opening is free of depression defects. S3, multilayer substrate hot pressing: the prepreg (3) and the outer conductive copper foil are stacked, and the multilayer substrate is pressed by a stepped heating hot pressing process; The stepped heating hot pressing process includes: In the first heating stage, the temperature is increased to 120-140℃ at a rate of 1.0-2.0℃ / min and held for 20-40min. In the second heating stage, the temperature is increased to 180-200℃ at a rate of 0.5-1.5℃ / min and held for 60-120min. Then, the temperature is decreased to room temperature at a rate of 1.0-3.0℃ / min. S4, Outer layer conventional pattern transfer: The outer layer conductive circuit is formed through a circuit process of dry film lamination, standard vertical LDI exposure, development, etching, and film removal; S5, step-by-step deep milling to form cavity (1): the sunken cavity (1) is processed by multi-blade layer milling process. The local insulating substrate within the contour range of cavity (1) and the side of the slot facing cavity (1) is removed by milling, so that the straight long side of the slot is fully exposed on the vertical inner wall of cavity (1) to form rectangular planar metal contacts. S6, Cavity (1) Plasma surface treatment: Plasma cleaning of the inside of cavity (1) and simultaneous surface treatment of the sidewall of the planar gold finger; S7, selective gold plating of contacts: selectively electroplating gold on the gold finger area of the side wall plane of the cavity (1) to form a gold plating layer (5). S8, Post-process finishing and inspection: Remove the anti-plating dry film from the board surface, and after passing the inspection, perform solder resist printing, character production, and shape cutting finishing in sequence to obtain the finished cavity (1) slot wall plane gold finger printing board.
7. The method for manufacturing the gold finger printed circuit board on the cavity groove wall according to claim 6, characterized in that, The slot width is ≥0.6mm, and an insulating substrate isolation strip of ≥0.15mm is reserved between the sidewalls of adjacent slots. The roughness Ra of the slot wall is controlled to ≤1.5μm. The alignment tolerance of the controlled depth milling is controlled within ±25μm. The multi-blade layered milling process includes two stages: rough milling and finish milling. The single cutting depth in the rough milling stage is 0.3~0.6mm, and the single cutting depth in the finish milling stage is 0.05~0.15mm. After being formed in steps S5 to S7, the planar gold finger contact is used to repeatedly press and engage with a standard spring to achieve electrical conduction. Regarding the wear durability of the gold plating layer (5) under this press-fitting engagement, the wear cycle life of the gold plating layer (5) of the planar gold finger contact is characterized by the following wear prediction model: In the formula, The number of spring clip crimping cycles that the gold plating layer can withstand. The wear resistance constant of the gold plating layer. To protect the thickness of the gold layer, The coefficient of friction at the interface between the gold layer and the spring sheet is denoted as . This refers to the normal contact pressure applied by the spring sheet to the planar contact point. The crimping frequency is the number of times per unit time.
8. The method for manufacturing the gold finger printed circuit board on the cavity groove wall according to claim 6, characterized in that, In step S2, the slot is fully filled using a pulse reverse electroplating process instead of a copper paste plugging process, with a pure copper layer (2) plated as the filling medium for the slot. The pulse reverse electroplating process uses an acidic copper plating solution containing a leveling agent, an inhibitor, and an accelerator, with Cl in the plating solution. - The concentration is 40~80 ppm; Thermal cycling interlayer stress at the interface between the slot filler copper layer (2) and the surrounding substrate The coefficient of thermal expansion between the electroplated pure copper layer (2) and the substrate and the operating temperature cycle amplitude are determined, and the following conditions are met: If the interlayer stress during thermal cycling is less than the interlayer bonding strength threshold between the prepreg (3) and the copper layer, then: In the formula, This refers to the interlayer stress caused by thermal cycling at the interface between the copper filler layer of the slot and the surrounding substrate due to the difference in the coefficients of thermal expansion. The elastic modulus of the electroplated pure copper layer. The coefficient of linear expansion of the electroplated pure copper layer is... is the equivalent linear expansion coefficient of the multilayer composite substrate. This represents the operating temperature cycle amplitude. This represents the interlayer bonding strength threshold at the interface between the prepreg and the copper layer.
9. The method for manufacturing the gold finger printed circuit board on the cavity groove wall according to claim 6, characterized in that, In step S5, the rectangular planar metal contact formed by the straight long side of the slot hole is exposed by controlled depth milling. The surface of the rectangular planar metal contact is a regular planar structure with a flatness of ≤0.05mm. The coplanarity tolerance between the sidewall of the contact and the sidewall of the cavity (1) is ≤±0.03mm. Compared with the arc-shaped curved surface contact of the same size, it has a contact area gain. The contact area gain of the planar gold finger contact compared to the arc-shaped curved surface contact of the same size satisfies the following geometric relationship: In the formula, This represents the increase in contact area between a planar contact and a curved contact. For the contact width, Let be the radius of curvature of the arc-shaped curved surface contact point. The maximum offset arch height between the vertex of the curved surface and the plane. This represents the actual contact area of the planar contact point. This represents the theoretical contact area of the curved surface contacts of the same width.
10. The method for manufacturing the gold finger printed circuit board on the cavity groove wall according to claim 6, characterized in that, In step S7, selective electroplating of gold is performed by covering the non-gold finger area with an anti-plating dry film with a thickness of 15~50μm, exposing only the gold finger contact area on the side wall of the cavity (1) for electroplating, forming a uniform and dense gold plating layer (5) on the surface of the gold finger contact, wherein the surface roughness Ra of the gold plating layer (5) is ≤0.10μm; The regular rectangular pure metal planar structure ensures that the actual contact area when the planar gold finger contacts are pressed against the standard spring contact is larger than that of an arc-shaped curved surface contact of the same size, thereby reducing the total contact resistance. The following relationship must be satisfied: In the formula, This is the total contact resistance. The volume resistivity of the gold plating layer. This is the equivalent conduction path length of the current within the planar contact. This represents the actual contact area of the planar contact point. It represents the surface contact resistance at the interface between the gold layer and the spring.