Method for manufacturing wiring circuit board and manufacturing system for wiring circuit board

By removing the passivation coating on the surface of the stainless steel substrate before etching, and using a combination of first and second etching solutions, the etching accuracy problem caused by uneven passivation coating thickness was solved, achieving high-precision etching and manufacturing of the substrate.

CN123164664APending Publication Date: 2026-11-24NITTO DENKO CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202610656310.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-21
Filing Date
2026-05-13
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

The etching precision of stainless steel substrates in the prior art is insufficient, especially the reduction in the dimensional accuracy of the substrate after etching due to uneven passivation coating thickness.

Method used

Before etching, a pretreatment process is performed to remove the passivation coating on the substrate surface using a first etching solution, followed by etching using a second etching solution to ensure precise etching of the substrate.

Benefits of technology

The etching precision of the stainless steel substrate has been improved, ensuring the dimensional accuracy of the metal support layer, terminals and openings, and achieving higher manufacturing precision.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123164664A_ABST
    Figure CN123164664A_ABST
Patent Text Reader

Abstract

This invention relates to a method for manufacturing a wiring circuit board and a system for manufacturing a wiring circuit board. The method for manufacturing a wiring circuit board of this invention includes a laminate formation step, a pretreatment step, and an etching step. In the laminate formation step, a laminate is formed on a stainless steel substrate. The laminate has a circuit pattern, a first insulating layer disposed between a metal support layer and the circuit pattern, and a second insulating layer covering the circuit pattern. In the pretreatment step, after the laminate formation step, the substrate is treated with a first etching solution. In the etching step, after the pretreatment step, the substrate is etched using a second etching solution. The first etching solution can dissolve a passivation coating on the surface of the substrate, and the second etching solution can dissolve iron in the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to a method for manufacturing a wiring circuit board and a system for manufacturing a wiring circuit board. Background Technology

[0002] Previously, it was known that a method was used to sequentially form a base insulating layer, a conductor layer and a cover insulating layer on a suspension substrate containing a metal such as stainless steel, and then etch the suspension substrate into a given shape to obtain a suspension substrate with circuitry (for example, see Patent Document 1 below).

[0003] Existing technical documents Patent documents Patent Document 1: Japanese Patent Application Publication No. 2005-217250 Summary of the Invention

[0004] The technical problem that the invention aims to solve In manufacturing methods such as those described in Patent Document 1, it is required to further improve the etching precision.

[0005] This disclosure provides a method and system for manufacturing a wiring circuit board that can improve the etching accuracy of a stainless steel substrate.

[0006] Technical solutions for solving technical problems This disclosure [1] includes a method for manufacturing a wiring circuit board, comprising the following steps: a laminate formation step, wherein a laminate is formed on a stainless steel substrate, the laminate having a circuit pattern, a first insulating layer disposed between the substrate and the circuit pattern, and a second insulating layer covering the circuit pattern; a pretreatment step, wherein, after the laminate formation step, the substrate is treated with a first etchant; and an etching step, wherein, after the pretreatment step, the substrate is etched with a second etchant, wherein, in the pretreatment step, the first etchant is capable of dissolving a passivation coating on the surface of the substrate, and in the etching step, the second etchant is capable of dissolving iron in the substrate.

[0007] According to this method, the substrate can be etched after the passivation coating on the substrate surface is removed in the pretreatment process.

[0008] Therefore, it can suppress the reduction in dimensional accuracy (etching accuracy) of the substrate after etching due to uneven thickness of the passivation coating.

[0009] As a result, the etching precision of the substrate can be improved.

[0010] This disclosure [2] includes a method for manufacturing a wiring circuit board according to [1] above, wherein the wiring circuit board has a metal support layer made from the substrate in the etching process and the laminate disposed on the metal support layer.

[0011] This disclosure [3] includes a method for manufacturing a wiring circuit board as described in [2] above, wherein the method for manufacturing the wiring circuit board includes, after the lamination forming process, a shape processing process for adjusting the shape of the metal support layer, the shape processing process including the pretreatment process and the etching process.

[0012] This method can improve the dimensional accuracy of the metal support layer.

[0013] This disclosure [4] includes a method for manufacturing a wiring circuit board according to any one of [1] to [3] above, wherein the method for manufacturing the wiring circuit board includes, after the laminate formation process, a terminal formation process for forming terminals from the substrate, the terminal formation process including the pretreatment process and the etching process.

[0014] This method enables improvements in the dimensional accuracy of terminals made from substrates.

[0015] This disclosure [5] includes a method for manufacturing a wiring circuit board according to any one of [1] to [4] above, wherein the method for manufacturing the wiring circuit board includes, after the laminate formation process, an opening formation process for forming an opening in the substrate, the opening formation process including the pretreatment process and the etching process.

[0016] This method can improve the dimensional accuracy of the opening.

[0017] This disclosure [6] includes a wiring circuit board manufacturing system, which is a manufacturing system that can be used in the wiring circuit board manufacturing method of any one of [1] to [5] above, and includes: a pretreatment apparatus for performing the pretreatment process, and an etching apparatus for performing the etching process.

[0018] Based on this structure, a pretreatment device is provided for carrying out pretreatment processes.

[0019] Therefore, it is possible to etch the substrate after removing the passivation coating on the substrate surface using a pretreatment device.

[0020] As a result, the etching precision of the substrate can be improved.

[0021] This disclosure [7] includes a manufacturing system for the wiring circuit board of the above [6], wherein the pretreatment device is disposed on the upstream side of the travel direction of the etching device in a continuous production line.

[0022] Invention Effects According to the manufacturing method and system for the wiring circuit board disclosed herein, it is possible to improve the etching precision of stainless steel substrates. Attached Figure Description

[0023] Figure 1 This is a cross-sectional view of the wiring circuit board.

[0024] Figures 2A to 2C It means Figure 1 The diagram shows a method for manufacturing a wiring circuit board. Figure 2A This indicates the first insulating layer formation process. Figure 2B This indicates the process of forming the circuit pattern. Figure 2C This indicates the process of forming the second insulating layer.

[0025] Figure 3A and Figure 3B It continues Figure 2C A diagram illustrating the manufacturing method of a wiring circuit board. Figure 3A Indicates the pretreatment process. Figure 3B This indicates the etching process.

[0026] Figure 4 This is a block diagram representing the manufacturing system of a wiring circuit board.

[0027] Figures 5A-5C This is a process diagram illustrating the terminal forming process in the manufacturing method of the wiring circuit board of modified example (1). Figure 5A Indicates the etching process. Figure 5B Indicates the plating process. Figure 5C This indicates the heating process.

[0028] Figure 6A and Figure 6B This is an explanatory diagram used to illustrate a modified example of a wiring circuit board. Figure 6A This indicates a structure with a conductor layer between the metal support layer and the first insulating layer. Figure 6B This indicates a structure having a second circuit pattern and a third insulating layer on the second insulating layer. Detailed Implementation

[0029] 1. Wiring circuit board Reference Figure 1 The wiring circuit board 1 will be described. It should be noted that the wiring circuit board 1 can be a flexible wiring circuit board or a suspended board with circuitry.

[0030] The wiring circuit board 1 has a metal support layer 2 and a laminate 10.

[0031] (1) Metal support layer Metal support layer 2, support layer stack 10. Metal support layer 2 is made of a stainless steel substrate. Metal support layer 2 may be made solely of a stainless steel substrate.

[0032] (2) Layered body The laminate 10 is disposed on the metal support layer 2 in the thickness direction of the metal support layer 2. The laminate 10 has a first insulating layer 3, a circuit pattern 4, and a second insulating layer 5.

[0033] (2-1) First insulating layer A first insulating layer 3 is disposed on one side of the metal support layer 2 in the thickness direction. The first insulating layer 3 is disposed on one surface of the metal support layer 2 in the thickness direction. The first insulating layer 3 is disposed between the metal support layer 2 and the circuit pattern 4 in the thickness direction. The first insulating layer 3 insulates the metal support layer 2 from the circuit pattern 4. The first insulating layer 3 comprises a resin. Examples of resins include polyimide, maleimide, epoxy resin, polybenzoxazole, and polyester.

[0034] (2-2) Circuit diagram The circuit pattern 4 is disposed on one side of the first insulating layer 3 in the thickness direction. The circuit pattern 4 is disposed on one surface of the first insulating layer 3 in the thickness direction. The circuit pattern 4 is disposed on the side of the first insulating layer 3 opposite to the metal support layer 2 in the thickness direction. The circuit pattern 4 contains metal. Examples of metals include copper, silver, gold, iron, aluminum, chromium, and their alloys. The circuit pattern 4 preferably contains copper. The shape of the circuit pattern 4 is not limited. The circuit pattern 4, for example, has a plurality of wirings 41 and a plurality of terminals (not shown). The wirings 41 can be signal wirings for transmitting electrical signals or power wirings for transmitting current from a power source.

[0035] (2-3) Second insulating layer The second insulating layer 5 is disposed on the first insulating layer 3 in the thickness direction. The second insulating layer 5 covers the circuit pattern 4. Specifically, the second insulating layer 5 covers at least a portion of the wiring 41. The second insulating layer 5 does not cover at least a portion of the terminals. The second insulating layer 5 comprises a resin. Examples of resins include polyimide, maleimide, epoxy resin, polybenzoxazole, and polyester.

[0036] 2. Manufacturing method of wiring circuit board Next, the manufacturing method of the wiring circuit board 1 will be described.

[0037] The manufacturing method of the wiring circuit board 1 includes a laminate formation process (see reference). Figures 2A to 2C ) and external processing procedures (refer to Figure 3A and Figure 3B ).

[0038] (1) Laminated body formation process In the laminate formation process, a laminate 10 is formed on a stainless steel substrate M. The laminate formation process includes a first insulating layer formation process (see reference). Figure 2A ), Circuit pattern formation process (refer to Figure 2B ) and the second insulating layer formation process (refer to Figure 2C ).

[0039] (1-1) First insulating layer formation process like Figure 2A As shown, in the first insulating layer forming process, a first insulating layer 3 is formed on one side surface of a stainless steel substrate M.

[0040] Specifically, in the first insulating layer formation step, firstly, a solution of photosensitive resin (varnish) is coated onto a substrate M, forming a photosensitive resin coating film on the substrate M. Next, the photosensitive resin coating film is dried by heating (first heating step). Then, the dried coating film is exposed to light and then heated (second heating step). The heating temperature in the second heating step is higher than the heating temperature in the first heating step. Next, the exposed coating film is developed and then heated (third heating step). Thus, the first insulating layer 3 is formed. The heating temperature in the third heating step is higher than the heating temperature in the second heating step.

[0041] Here, by heating the substrate M in each heating process (first heating process to third heating process), the passivation coating P on the surface of the substrate M grows unevenly. Therefore, the thickness of the passivation coating P may become uneven.

[0042] (1-2) Circuit pattern formation process Next, as Figure 2B As shown, in the circuit pattern forming process, a circuit pattern 4 is formed on the first insulating layer 3.

[0043] In detail, firstly, a seed layer is formed on one side surface of the first insulating layer 3 and one side surface of the substrate M in the thickness direction. The seed layer is formed, for example, by sputtering. Examples of materials for the seed layer include chromium, copper, nickel, titanium, and alloys thereof.

[0044] Next, the seed layer is coated with a plating resist.

[0045] Next, the resist is exposed and developed. Thus, the resist in the areas where circuit pattern 4 is formed is removed, exposing the seed layer in those areas. On the other hand, the resist in the areas where circuit pattern 4 is not formed is retained.

[0046] Next, circuit pattern 4 is formed on the exposed seed layer by electroplating. After electroplating, the resist is stripped. Then, the seed layer exposed due to the stripping of the resist is removed by etching.

[0047] Thus, a circuit pattern 4 is formed on the first insulating layer 3.

[0048] (1-3) Second insulation layer formation process Next, as Figure 2C As shown, in the second insulating layer forming process, the same operation as in the first insulating layer forming process is performed to form the second insulating layer 5 on the first insulating layer 3.

[0049] Specifically, in the second insulating layer formation process, firstly, a solution of photosensitive resin (varnish) is coated onto the substrate M, the first insulating layer 3, and the circuit pattern 4, and the formed coating is dried by heating (fourth heating step). Next, the dried coating is exposed and then heated (fifth heating step). The heating temperature in the fifth heating step is higher than that in the fourth heating step. Next, the exposed coating is developed and then heated (sixth heating step). Thus, the second insulating layer 5 is formed. The heating temperature in the sixth heating step is higher than that in the fifth heating step.

[0050] In each heating step (fourth to sixth heating steps) of the second insulating layer formation process, similarly to each heating step (first to third heating steps) of the first insulating layer formation process, the passivation coating P grows unevenly by heating the substrate M. Therefore, the unevenness of the thickness of the passivation coating P may be further increased.

[0051] (2) External processing procedures Next, the shape processing step is performed after the laminate formation step. In the shape processing step, the shape of the metal support layer 2 is adjusted. The shape processing step includes a pretreatment step (see...). Figure 3A ) and etching process (refer to Figure 3B That is, the manufacturing method of the wiring circuit board 1 includes a pretreatment process and an etching process.

[0052] (2-1) Pretreatment process like Figure 3A As shown, the pretreatment process is performed after the laminate formation process and before the etching process. In the pretreatment process, the substrate M is treated with a first etching solution. In the pretreatment process, the first etching solution can dissolve the passivation coating P on the surface of the substrate M. Thus, the passivation coating P is removed. The first etching solution preferably does not dissolve iron.

[0053] Examples of first etching solutions include cerium ammonium nitrate solution, aqueous sodium hydroxide solution, potassium permanganate solution, and sodium metasilicate solution.

[0054] After the pretreatment process, for example, the substrate M is washed with water to remove the first etching solution adhering to the substrate M.

[0055] (2-2) Etching process Next, as Figure 3B As shown, the etching process is performed after the laminate formation process and after the pretreatment process. In the etching process, the substrate M is etched using a second etching solution. In this embodiment, the aforementioned metal support layer 2 is fabricated in the etching process.

[0056] In detail, during the etching process, a photoresist is formed on one side surface of the substrate M in the thickness direction and on the other side surface of the substrate M in the thickness direction. The photoresist covers the non-etched portions of the substrate M and exposes the portions of the substrate M to be etched.

[0057] It should be noted that, in order to form the photoresist, dry film photoresist is pasted on one side surface of the substrate M in the thickness direction and on the other side surface of the substrate M in the thickness direction, and the dry film photoresist is exposed and developed.

[0058] Next, a second etching solution is used to etch the portion of the substrate M exposed from the resist (a part of the substrate M).

[0059] In the etching process, the second etching solution can dissolve the iron in the substrate M. Examples of the second etching solution include aqueous solutions of ferric chloride, copper chloride, and sulfuric acid / hydrogen peroxide.

[0060] After the etching process, the metal support layer 2 and the substrate M are cleaned, for example, with water to remove the second etching solution adhering to the metal support layer 2 and the substrate M. After cleaning, the resist is stripped off.

[0061] Thus, the wiring circuit board 1 described above is obtained.

[0062] 3. Manufacturing system for wiring circuit boards Next, the manufacturing system 100 for the wiring circuit board 1 that can be used in the above-described manufacturing method of the wiring circuit board 1 will be described.

[0063] like Figure 4 As shown, the manufacturing system 100 may include a continuous production line L. The manufacturing system 100 may also include multiple production lines L. The production line L includes a pretreatment unit 101, an etching unit 102, and a cleaning unit 103. That is, the manufacturing system 100 includes a pretreatment unit 101, an etching unit 102, and a cleaning unit 103.

[0064] It should be noted that production line L can perform the above-mentioned pretreatment and etching processes in a roller-to-roll manner, or it can perform the above-mentioned pretreatment and etching processes on multiple sheets conveyed along the travel direction.

[0065] Alternatively, production line L may also be provided upstream of pretreatment device 101 in the direction of travel of production line L, with devices for the first insulating layer forming process (e.g., coating device, exposure device, developing device, heating device), devices for the circuit pattern forming process (e.g., plating tank), and devices for the second insulating layer forming process (e.g., coating device, exposure device, developing device, heating device).

[0066] The pretreatment apparatus 101 performs the pretreatment process described above. The pretreatment apparatus 101 is positioned upstream of the etching apparatus 102 in the travel direction of the production line L. The pretreatment apparatus 101 is capable of spraying a first etching solution onto the substrate M. The pretreatment apparatus 101, for example, has a tank and multiple spray nozzles. The tank contains the first etching solution. The multiple spray nozzles spray the first etching solution supplied from the tank toward the substrate M. Preferably, the pretreatment apparatus 101 sprays the first etching solution onto the substrate M from both sides in the thickness direction. Alternatively, the pretreatment apparatus 101 may not be capable of spraying the first etching solution. The pretreatment apparatus 101 may also have a solution tank for storing the first etching solution, and be capable of immersing the substrate M in the first etching solution within the solution tank.

[0067] It should be noted that the production line L may also have a cleaning device using water as a cleaning solution between the pretreatment device 101 and the etching device 102 in the direction of travel of the production line L.

[0068] The etching apparatus 102 is disposed downstream of the pretreatment apparatus 101 in the travel direction of the production line L. The etching apparatus 102 performs the etching process described above. The etching apparatus 102 is capable of spraying a second etching solution onto the substrate M. The etching apparatus 102 has, for example, a tank and a plurality of spray nozzles. The tank contains the second etching solution. The plurality of spray nozzles spray the second etching solution supplied from the tank toward the substrate M. Preferably, the etching apparatus 102 sprays the second etching solution onto the substrate M from both sides in the thickness direction.

[0069] The cleaning device 103 is disposed downstream of the etching device 102 in the travel direction of the production line L. The cleaning device 103 cleans the substrate M after the etching process described above. The cleaning device 103 includes, for example, a tank and multiple spray nozzles. The tank contains a cleaning solution. Examples of cleaning solutions include water and acid. Each of the multiple spray nozzles sprays the cleaning solution supplied from the tank toward the substrate M.

[0070] It should be noted that production line L may also have multiple cleaning devices 103 using different cleaning solutions downstream of etching device 102 in the direction of travel of production line L. For example, production line L may also have a first cleaning device 103 using acid as the cleaning solution and a second cleaning device 103 using water as the cleaning solution downstream of etching device 102 in the direction of travel of production line L. Examples of acids used in the first cleaning device 103 include sulfuric acid, hydrochloric acid, and nitric acid. The second cleaning device 103 is disposed downstream of the first cleaning device 103 in the direction of travel of production line L.

[0071] Alternatively, production line L may also have a resist stripping device and a drying device for stripping the resist on the downstream side of the cleaning device 103 in the direction of travel of production line L.

[0072] 4. Effects (1) According to the manufacturing method of the wiring circuit board, such as Figure 3A As shown, in the laminate formation process (refer to...) Figures 2A to 2C In the subsequent shape processing steps, during the etching process (see...) Figure 3B The preceding step includes a pretreatment process where the substrate is treated with a first etching solution. The first etching solution can dissolve the passivation coating P on the surface of the substrate M. The second etching solution can dissolve the iron in the substrate M.

[0073] Therefore, the substrate M can be etched after the passivation coating P on the surface of the substrate M is removed in the pretreatment process.

[0074] Therefore, it is possible to suppress the reduction in dimensional accuracy (etching accuracy) of the metal support layer 2 (etched substrate M) caused by the uneven thickness of the passivation coating P.

[0075] As a result, the dimensional accuracy of the metal support layer (in other words, the etching accuracy of the substrate M) can be improved.

[0076] (2) According to the wiring circuit board manufacturing system 100, such as Figure 4 As shown, a pretreatment apparatus 101 is provided for performing pretreatment processes.

[0077] Therefore, the substrate M can be etched after the passivation coating P on the surface of the substrate M is removed using the pretreatment device 101.

[0078] As a result, the etching precision of the substrate M can be improved.

[0079] 5. Variations The following describes a variation. In the variation, the same symbols are used to mark the same components as in the above-described embodiment, and their descriptions are omitted.

[0080] (1) The heating process of the substrate M (heating process) is not limited to the heating process in the laminate formation process (specifically, each heating process in the first insulating layer formation process and each heating process in the second insulating layer formation process).

[0081] For example, the manufacturing method of the wiring circuit board can also be carried out in the laminate formation process (see reference). Figures 2A to 2C After that, and the pretreatment process (refer to...) Figure 3A (Previously included) Figures 5A-5C The terminal forming process involves forming a terminal 200 from a substrate M as shown. During this terminal forming process, the substrate M is heated.

[0082] In detail, the terminal forming process includes an etching process (see...). Figure 5A ), plating process (refer to Figure 5B ) and heating process (refer to Figure 5C ).

[0083] like Figure 5A As shown, in the etching process, resist R1 is formed on one surface of the substrate M in the thickness direction and on the other surface of the substrate M in the thickness direction, and then the substrate M is etched. As a result, a terminal 200 is formed on the other side of the first insulating layer 3 in the thickness direction. It should be noted that the first insulating layer 3 has a through-hole (not shown). The circuit pattern 4 is connected to the terminal 200 through the through-hole (not shown). The etching uses the second etching solution described above. The resist R1 is removed after the etching process.

[0084] Next, as Figure 5B As shown, in the plating process, a plating resist R2 is formed on one side surface of the substrate M in the thickness direction and on the other side surface of the substrate M in the thickness direction. Then, a plating layer 201 is formed on the surface of the terminal 200. The plating layer 201 is, for example, a gold plating layer. The plating resist R2 is peeled off after the plating process.

[0085] Next, as Figure 5C As shown, the plating layer 201 is heated during the heating process. Heating improves the adhesion between the plating layer 201 and the terminal 200.

[0086] Then, after the terminal forming process, a pretreatment process is performed in the same manner as in the above embodiment (see...). Figure 3A ) and etching process (refer to Figure 3B ).

[0087] According to this modified example, the heating process in the terminal forming process (refer to...) Figure 5C In this process, the substrate M is also heated together with the coating layer 201. Therefore, the non-uniformity of the passivation coating P thickness may be further amplified.

[0088] In this regard, similar to the above-described implementation, a pretreatment process is performed after the terminal forming process and before the etching process to remove the passivation coating P.

[0089] Therefore, in this modified example, the etching accuracy of the substrate M can also be improved.

[0090] (2) The terminal forming process of variation (1) may include the pretreatment process described above before the etching process. Specifically, in the terminal forming process, before forming the resist R1, the substrate M is treated with a first etching solution to remove the passivation coating P. Then, in the etching process, as described above, the resist R1 is formed, and the substrate M is etched using a second etching solution.

[0091] By implementing a pretreatment process in the terminal forming process, the dimensional accuracy of the terminal 200 can be improved.

[0092] (3) The manufacturing method of the wiring circuit board can also be carried out in the laminate formation process (see Figures 2A to 2C The process then includes an opening forming step, which involves forming an opening in the substrate M. This opening forming step is performed, for example, when it is desired to provide an opening in the metal support layer 2. Similar to the shape processing step and terminal forming step described above, the pretreatment step described above may also be performed in the opening forming step before the etching step. That is, the opening forming step may also include a pretreatment step and an etching step.

[0093] In detail, during the opening formation process, before forming the resist, the substrate M is treated with a first etchant to remove the passivation coating P. Then, in the etching process, the resist is formed, and the substrate M is etched using a second etchant.

[0094] By implementing a pretreatment process in the opening formation process, the dimensional accuracy of the opening can be improved.

[0095] (4) The layer structure of the laminate 10 is not limited to the embodiments described above. For example, such as Figure 6A As shown, a conductor layer 301 may be provided between the metal support layer 2 and the first insulating layer 3. Additionally, for example, as... Figure 6B As shown, it may have a second circuit pattern 401 disposed on the second insulating layer 5 and a third insulating layer 402 disposed on the second insulating layer 5 and covering the second circuit pattern 401.

[0096] (5) Modifications (1) to (4) can be combined with each other. For example, after the laminate formation process, the opening formation process, the terminal formation process and the shape processing process are performed in sequence to manufacture a wiring circuit board 1 with openings and terminals 200.

[0097] Example The following examples and comparative examples are shown to further illustrate this disclosure. It should be noted that this disclosure is not limited to any particular example or comparative example. In addition, the specific values ​​of the proportions (including proportions), physical property values, parameters, etc. used in the following description can replace the corresponding upper limits (defined as "below" or "less than") or lower limits (defined as "above" or "more than") of the proportions (including proportions), physical property values, parameters, etc., described in the "Detailed Description" above.

[0098] <Example> First, a solution of photosensitive polyimide (varnish) is applied to a stainless steel substrate, forming a photosensitive polyimide coating. Next, the photosensitive polyimide coating is dried by heating (first heating step). Then, the dried coating is exposed to light and then heated (second heating step). Next, the exposed coating is developed and then heated (third heating step). This forms a first insulating layer on the substrate (see the first insulating layer formation step). Figure 2A ).

[0099] Next, a chromium-containing seed layer is formed on the surfaces of the first insulating layer and the substrate by sputtering. Then, the seed layer is coated with a resist. Next, the resist is exposed and developed. Through development, the resist in the areas where the circuit pattern is to be formed is removed, exposing the seed layer in those areas. Then, the circuit pattern is formed on the exposed seed layer by electrolytic plating (for the circuit pattern formation process, refer to...). Figure 2B ).

[0100] Next, the resist is stripped, and the seed layer exposed by the stripping of the resist is removed by etching.

[0101] Next, a solution of photosensitive polyimide (varnish) is applied to the substrate, the first insulating layer, and the circuit pattern, and the resulting coating is dried by heating (fourth heating step). Next, the dried coating is exposed and then heated (fifth heating step). Next, the exposed coating is developed and then heated (sixth heating step). Thus, the second insulating layer 5 is formed (for the second insulating layer formation process, refer to...). Figure 2C ).

[0102] Next, the first etching solution (cerium ammonium nitrate solution, liquid temperature: 40°C) is sprayed onto the substrate for 40 seconds (pretreatment step, refer to...). Figure 3A ).

[0103] Next, resist is formed on both sides of the substrate, and a second etching solution (ferric chloride aqueous solution, liquid temperature: 50℃) is sprayed for 120 seconds to etch the substrate (etching process, refer to...). Figure 3B ).

[0104] After the etching process, the substrate is washed with water, and then the resist is stripped off.

[0105] Through the above operations, the wiring circuit board is obtained.

[0106] The width of the metal support layer of the obtained wiring circuit board was measured, and the measured value was calculated relative to the design value (636). μ The standard deviation (σ) is 0.474 m. μ m.

[0107] <Comparative Example> Without performing any pretreatment steps, the wiring circuit board is obtained by operating in the same manner as in the embodiment. The width of the metal support layer of the obtained wiring circuit board is measured, and the measured value is calculated relative to the design value (636). μ The standard deviation (σ) is 0.697 m. μ m.

[0108] It should be noted that the above-described invention is provided as an illustrative embodiment of the present invention, but this is merely illustrative and should not be interpreted as limiting. It will be apparent to those skilled in the art that variations of the present invention are included within the scope of the patent claims.

[0109] Industrial availability The method and system for manufacturing wiring circuit boards disclosed herein can be used in the manufacture of wiring circuit boards.

[0110] Explanation of reference numerals in the attached figures 1. Wiring circuit board 2 Metal support layer 3 First Insulation Layer 4. Circuit diagram 5 Second Insulation Layer 10-layer stack 100 Manufacturing System 101 Pretreatment Unit 102 Etching apparatus L production line M substrate P passivation coating.

Claims

1. A method for manufacturing a wiring circuit board, characterized in that, The process includes the following steps: A laminate forming process, wherein a laminate is formed on a stainless steel substrate, the laminate having a circuit pattern, a first insulating layer disposed between the substrate and the circuit pattern, and a second insulating layer covering the circuit pattern; A pretreatment step, wherein, after the laminate formation step, the substrate is treated with a first etching solution; and The etching process includes etching the substrate using a second etching solution after the pretreatment process. In the pretreatment step, the first etching solution can dissolve the passivation coating on the surface of the substrate. In the etching process, the second etching solution can dissolve the iron in the substrate.

2. The method for manufacturing a wiring circuit board according to claim 1, wherein, The wiring circuit board has: The metal support layer made from the substrate in the etching process; and The laminate disposed on the metal support layer.

3. The method for manufacturing a wiring circuit board according to claim 2, wherein, The method for manufacturing the wiring circuit substrate includes, after the laminate formation process: The external shaping process includes adjusting the shape of the metal support layer. The shape processing steps include the pretreatment step and the etching step.

4. The method for manufacturing a wiring circuit board according to claim 1, wherein, The method for manufacturing the wiring circuit substrate includes, after the laminate formation process: Terminal forming process, wherein terminals are formed from the substrate. The terminal forming process includes the pretreatment process and the etching process.

5. The method for manufacturing a wiring circuit board according to claim 4, wherein, The terminal forming process also includes a heating process.

6. The method for manufacturing a wiring circuit board according to claim 1, wherein, The method for manufacturing the wiring circuit substrate includes, after the laminate formation process: An opening-forming process, wherein an opening is formed on the substrate. The opening formation process includes the pretreatment process and the etching process.

7. The method for manufacturing a wiring circuit board according to claim 1, wherein, The first etching solution is an etching solution that does not dissolve iron, or an etching solution selected from cerium ammonium nitrate solution, sodium hydroxide aqueous solution, potassium permanganate solution and sodium metasilicate solution.

8. A manufacturing system for a wiring circuit board, characterized in that, It is a manufacturing system that can be used in the manufacturing method of the wiring circuit board according to any one of claims 1 to 7, and comprises: A pretreatment apparatus that performs the pretreatment process; and An etching apparatus that performs the etching process.

9. The manufacturing system for a wiring circuit board according to claim 8, wherein, The pretreatment device is located upstream of the etching device in the direction of travel in a continuous production line.

10. The manufacturing system for a wiring circuit board according to claim 8 or 9, wherein, A cleaning device using water as a cleaning solution is provided between the pretreatment device and the etching device.

Citation Information