Circuit board etching method and circuit board

By using partitioned design and graphic layout to regulate the flow of etching solution, the problem of uneven etching of inner layers of printed circuit boards was solved, achieving uniform etching rate and high yield of circuit boards.

CN123164665APending Publication Date: 2026-11-24GUANGDONG AMBER CIRCUIT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611334478.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-31
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In the prior art, the problem of uneven etching caused by uneven copper thickness and pattern density on the same side of the inner layer of the printed circuit board includes defects such as line width deviation, short circuit or open circuit, and side etching.

Method used

By using a zoned design, stress cold spots and stress hot spots are identified, and stress aggregation patterns and stress release patterns are laid out respectively. By using a flow-gathering layer and a flow guide to regulate the flow of the etching solution during the etching process, uniformity of the etching rate is achieved.

Benefits of technology

It significantly improves the etching uniformity and product yield of circuit boards, avoids circuit defects, and simplifies the process flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123164665A_ABST
    Figure CN123164665A_ABST
Patent Text Reader

Abstract

This invention discloses a circuit board etching method and a circuit board. The circuit board etching method includes: partitioning the inner layer board surface into a grid and calculating the etching stress index to identify stress cold spot areas and stress hot spot areas; a first pattern transfer to form a stress aggregation pattern in the stress cold spot areas; electroplating to form a current-collecting layer at the stress aggregation pattern; a second pattern transfer to form a stress release pattern in the stress hot spot areas and a perimeter pattern at the edge of the current-collecting layer; a first etching to form a guide portion and a connecting portion; a third pattern transfer to form an etching area; circuit etching to form the main circuit and a first and second breakable neck; and cleaning and waste removal by using ultrasonic vibration to break the breakable neck, causing the guide portion and the current-collecting layer to detach from the main circuit. To address the etching rate differences caused by uneven copper thickness and pattern density distribution, the current-collecting layer accelerates the etching of cold spot areas, while the guide portion slows down the etching of hot spot areas, achieving global etching uniformity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of printed circuit board manufacturing technology, and particularly to a circuit board etching method, and a circuit board manufactured using the circuit board etching method. Background Technology In the process of printed circuit board manufacturing, the etching process of the inner layer board is a key process for forming circuit patterns. The design of the inner layer board is becoming increasingly complex. On the same board surface, there are often multiple pattern structures such as large areas of copper foil, dense fine lines, and isolated thick lines, resulting in significant differences in the copper thickness distribution and pattern density distribution in different areas of the same surface.

[0002] In existing technologies, when the copper thickness distribution on the same side of the inner layer board is uneven, areas with thicker copper are prone to under-etching due to the longer etching time required, resulting in problems such as excessively large linewidths, short circuits, or residual copper. Conversely, areas with thinner copper are prone to over-etching due to the faster etching speed, resulting in problems such as insufficiently large linewidths and open circuits.

[0003] Furthermore, when the pattern density distribution on the same surface is uneven, high-density areas are prone to under-etching due to difficulties in chemical exchange, while low-density areas are prone to over-etching due to sufficient chemical supply.

[0004] In addition, areas with abrupt changes in local pattern density, such as isolated thick lines or the junction of large areas of copper foil and dense thin lines, can suffer from severe lateral etching due to uneven flow of the chemical solution, affecting the accuracy and reliability of the circuit. Summary of the Invention

[0005] This invention aims to at least solve one of the technical problems existing in the prior art. To this end, this invention proposes a circuit board etching method that can lay out different auxiliary patterns in stress cold spot areas and stress hot spot areas according to the stress distribution on the surface of the inner layer board. The etching rate in the stress cold spot areas is accelerated by the current-collecting layer, and the etching rate in the stress hot spot areas is slowed down by the current-guiding part, thereby achieving global etching uniformity on the same surface.

[0006] The present invention also proposes a circuit board manufactured using the above-described circuit board etching method.

[0007] The circuit board etching method according to the present invention is used to etch an inner layer board with a copper-clad layer on its surface, the inner layer board including an etching area, and includes the following steps: The inner layer board is divided into multiple grids by a partitioned design. Copper thickness distribution data and pattern density distribution data of the inner layer board surface are obtained. Based on the copper thickness distribution data and the pattern density distribution data, the etching stress index of each grid is calculated. The grid with an etching stress index less than a first preset threshold is identified as a stress cold spot area, and the grid with an etching stress index greater than a second preset threshold is identified as a stress hot spot area. In the first pattern transfer, after the partition design, the copper-clad layer surface is exposed and developed to form a plating pattern, the plating pattern including a stress-polymerization pattern, the stress-polymerization pattern being arranged in the stress cold spot region and located in the etching area; Electroplating: After the first pattern transfer, the inner layer board is electroplated to form a current-accumulating layer on the copper-clad layer surface corresponding to the stress-polymerization pattern, and then the plating pattern is removed. The second pattern transfer involves forming a first etched pattern on the surface of the copper-clad layer after electroplating through exposure and development. The first etched pattern includes a stress relief pattern and an edge pattern. The stress relief pattern is located in the stress hot spot area and in the etched area, and the edge pattern is arranged at the edge of the current-collecting layer. First etching: After the second pattern transfer, the inner layer plate is etched to form a guide section through the stress relief pattern and a connecting section through the edge pattern; The third pattern transfer occurs after the second pattern transfer, whereby the surface of the copper-clad layer is exposed and developed to form a second etched pattern, the second etched pattern including etched areas. The inner layer board is etched after the third pattern transfer to form the main circuit on the surface of the inner layer board. The current guide portion is etched to form a first breakable neck, and the connection portion is etched to form a second breakable neck. After the circuit etching, the inner layer board is cleaned by passing a cleaning solution to remove the etching solution. The cleaning solution is configured to be connected to an ultrasonic vibrator, which can drive the first and second fragile necks to break, thereby driving the flow guide and the current-collecting layer to detach from the main circuit.

[0008] The circuit board etching method according to the present invention has at least the following beneficial effects: By dividing the same surface of the inner layer board into multiple grids through partitioning design, and calculating the etching stress index based on copper thickness distribution data and pattern density distribution data, stress cold spot regions and stress hot spot regions can be accurately identified. When there are differences in copper thickness in different regions of the surface, regions with thicker copper become stress cold spot regions due to slower etching rates, while regions with thinner copper become stress hot spot regions due to faster etching rates. When there are differences in pattern density in different regions of the surface, high-density regions become stress cold spot regions due to difficulties in chemical exchange, while low-density regions become stress hot spot regions due to sufficient chemical supply. To address this, stress aggregation patterns are arranged in the stress cold spot regions and a current-aggregating layer is formed through electroplating. This current-aggregating layer, acting as a raised sacrificial layer, can disturb the chemical flow and accelerate localization during etching. The etching process involves exchanging etching solutions to improve the etching rate in cold spots, preventing short circuits or residual copper due to insufficient etching. Simultaneously, stress-relieving patterns are created in stress hotspot areas, and flow guides are formed through etching. These flow guides direct the etching solution flow and disperse locally high-concentration solutions, reducing the etching rate in hotspot areas and preventing under-etching of linewidths or open circuits. Furthermore, the flow guides and current-collecting layers are connected to the main circuitry via first and second fragile necks, respectively. During etching, the fragile necks are partially etched, forming weak structures. In subsequent cleaning and waste removal steps, ultrasonic vibration causes the fragile necks to break, automatically detaching the flow guides and current-collecting layers from the main circuitry without additional removal steps. This simplifies the process, enabling intelligent and differentiated control of the etching process, significantly improving the etching uniformity and product yield of the circuit board.

[0009] According to some embodiments of the present invention, in the partition design of the circuit board etching method, the grid is a square grid, and the side length of the square grid is 3 to 5 times the minimum linewidth of the inner layer board surface; the copper thickness distribution data is obtained by an eddy current thickness gauge, and the graphic density distribution data is obtained by superimposing the circuit design diagram of the inner layer board with the grid and calculating the proportion of copper foil area in each grid.

[0010] According to some embodiments of the circuit board etching method of the present invention, in the partition design, the etching stress index is calculated from at least one of the following: copper thickness difference coefficient, pattern density difference coefficient, local pattern density gradient coefficient, and etching difficulty coefficient within the grid.

[0011] According to some embodiments of the present invention, the etch stress index is H, and the etch method includes a first boundary value A, a second boundary value B and a third boundary value C, and a second preset threshold value < A < B < C. When the second preset threshold of the etching stress index within the grid is <H < A, the stress relief pattern includes stress relief lines. The line width of the stress relief lines is the same as the line width of the signal lines of the inner layer board. The spacing of the stress relief lines is greater than twice the spacing of the signal lines of the inner layer board. The stress relief lines are used to increase the pattern density to balance the etching rate. When the etching stress index A < H < B within the grid, the stress relief pattern includes a circular stress equalization block. The diameter of the circular stress equalization block is 1.5 to 2 times the width of the signal line of the inner layer board. The circular stress equalization block is used to consume etching solution during the etching process to slow down the etching rate. When the etching stress index B < H < C within the grid, the stress relief pattern includes a dumbbell-shaped guide channel. The dumbbell-shaped guide channel includes two ends and a middle part. The width of the ends is greater than the width of the middle part. The dumbbell-shaped guide channel is connected to the main line through the middle part. The dumbbell-shaped guide channel is used to guide the flow of etching solution during the etching process to equalize the concentration of the etching solution. When the etching stress index C < H within the grid, the stress relief pattern includes a snowflake-shaped stress equalization block. The snowflake-shaped stress equalization block includes a center point and multiple arms radiating outward from the center point. The end of the arm opposite to the center point is connected to the main line. The snowflake-shaped stress equalization block is used to equalize the flow of etching solution from multiple directions during the line etching process to eliminate turbulence.

[0012] According to some embodiments of the present invention, in the circuit board etching method, the material of the current-collecting layer is nickel or tin, and the thickness of the current-collecting layer is proportional to the etching stress index of the stress cold spot region.

[0013] According to some embodiments of the present invention, the etch stress index is H, and the etch method includes a fourth boundary value D, a fifth boundary value E and a sixth boundary value F, wherein D < E < F < a first preset threshold. When the etching stress index within the grid satisfies H < D, the stress aggregation pattern is elongated, the electroplated current aggregation layer is a flow guide fin, the length direction of the flow guide fin is parallel to the spraying direction of the etching solution, the height of the flow guide fin is 1 to 2 times the thickness of the copper cladding layer, and the flow guide fin is used to guide the etching solution to the stress cold spot region to improve the chemical exchange rate. When the etching stress index within the grid satisfies D < H < E, the stress aggregation pattern is cylindrical, and the electroplated current aggregation layer is a turbulence column group. The turbulence column group includes multiple cylindrical protrusions distributed in an array. The diameter of the cylindrical protrusions is 2 to 3 times the thickness of the copper cladding layer, and the spacing between adjacent cylindrical protrusions is 1.5 to 2 times the diameter of the cylindrical protrusions. The turbulence column group is used to generate turbulence in the etching solution to improve the etching rate. When the etching stress index within the grid satisfies E < H < F, the stress aggregation pattern is trapezoidal, the electroplated current aggregation layer is a current aggregation protrusion, the height of the current aggregation protrusion is 2 to 3 times the thickness of the copper cladding layer, the bottom diameter of the current aggregation protrusion is 3 to 5 times the thickness of the copper cladding layer, and the current aggregation protrusion is used to accumulate chemicals during the etching process to accelerate etching. When the etching stress index within the grid satisfies F < H < first preset threshold, the stress aggregation pattern is a composite column and trapezoid shape, and the electroplated current aggregation layer is a composite current aggregation structure. The composite current aggregation structure includes a central current aggregation boss and a group of turbulence pillars arranged around the current aggregation boss. The turbulence pillars are located around the current aggregation boss. The composite current aggregation structure is used to jointly achieve chemical aggregation and turbulence disturbance during the etching process.

[0014] The circuit board etching method according to some embodiments of the present invention, In the initial etching, a first neck is formed between the guide portion and the main line, and a second neck is formed between the connection portion and the main line. The width of the first neck and the second neck is 1 / 2 to 2 / 3 of the linewidth of the main line. After the line is etched, the first neck forms the first fragile neck, and the second neck forms the second fragile neck after the line is etched. The width of the first fragile neck and the second fragile neck is 1 / 5 to 1 / 3 of the line width of the main line.

[0015] According to some embodiments of the present invention, in the initial etching, the etching depth of the inner layer board is 30% to 50% of the thickness of the copper cladding layer to form the first neck and the second neck.

[0016] According to some embodiments of the circuit board etching method of the present invention, in the cleaning and waste removal process, the frequency of the ultrasonic vibrator is 20kHz to 40kHz and the power density is 0.5W / cm² to 2W / cm². The first fragile neck and the second fragile neck break sequentially or simultaneously under the action of ultrasonic waves. After the breakage, the guide portion and the current-gathering layer fall off from the main circuit and are carried away from the surface of the inner layer board by the cleaning fluid.

[0017] The circuit board according to the present invention is manufactured using the circuit board etching method described in the present invention.

[0018] The circuit board according to the present invention has at least the following beneficial effects: the linewidth uniformity of the main circuit of the circuit board is significantly improved, and the lateral etching amount at the edge of the circuit is consistent, effectively avoiding circuit defects caused by local over-etching or under-etching.

[0019] Additional aspects and advantages of the invention will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. Attached Figure Description

[0020] The above and / or additional aspects and advantages of the present invention will become apparent and readily understood from the description of the embodiments taken in conjunction with the following drawings, in which: Figure 1 This is a flowchart of a circuit board etching method according to an embodiment of the present invention.

[0021] Explanation of icon numbers: Partition design S100; First pattern transfer S200; Electroplating S300; Second pattern transfer S400; First etching S500; Third pattern transfer S600; Circuit etching S700; Cleaning and waste removal S800; Detailed Implementation Embodiments of the present invention are described in detail below. Examples of these embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and should not be construed as limiting the present invention.

[0022] In the description of this invention, it should be understood that the orientation descriptions, such as up, down, front, back, left, right, etc., are based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limiting this invention.

[0023] In the description of this invention, "several" means one or more, "more than" means two or more, "greater than," "less than," and "exceeding" are understood to exclude the stated number, while "above," "below," and "within" are understood to include the stated number. The use of "first" and "second" in the description is merely for distinguishing technical features and should not be construed as indicating or implying relative importance, or implicitly indicating the number of indicated technical features, or implicitly indicating the order of the indicated technical features.

[0024] In the description of this invention, unless otherwise explicitly defined, terms such as "set up," "install," and "connect" should be interpreted broadly, and those skilled in the art can reasonably determine the specific meaning of the above terms in this invention in conjunction with the specific content of the technical solution.

[0025] In the description of this invention, the terms "one embodiment," "some embodiments," "illustrative embodiment," "example," "specific example," or "some examples," etc., refer to specific features, structures, materials, or characteristics described in connection with that embodiment or example, which are included in at least one embodiment or example of the invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.

[0026] Therefore, such as Figure 1 As shown, the circuit board etching method proposed in this invention includes the following steps executed sequentially: partition design S100, first pattern transfer S200, electroplating S300, second pattern transfer S400, initial etching S500, third pattern transfer S600, circuit etching S700, and cleaning and waste removal S800.

[0027] Specifically, in the partition design S100, the surface of the inner layer board is divided into multiple grids, and the copper thickness distribution data and pattern density distribution data of the inner layer board surface are obtained. Based on the copper thickness distribution data and pattern density distribution data, the etching stress index of each grid is calculated. Grids with an etching stress index less than a first preset threshold are identified as stress cold spot areas, and grids with an etching stress index greater than a second preset threshold are identified as stress hot spot areas.

[0028] It is easy to understand that by using the partitioned design S100, the problem of different etching rates caused by uneven copper thickness and pattern density distribution on the same surface of the inner layer board can be transformed into a quantifiable stress index, providing a basis for subsequent differentiated control.

[0029] Furthermore, in the first pattern transfer S200, a plating pattern is formed on the surface of the copper-clad layer by exposure and development. The plating pattern includes a stress-polymerized pattern, which is arranged in the stress cold spot region and located in the etching region.

[0030] It should be noted that stress-polymerized patterns are patterns formed after photolithography development. Their shapes include strips, columns, trapezoids, or composite shapes, and the specific shape is determined according to the etching stress index level of the stress cold spot area.

[0031] In electroplating S300, the inner layer board after the first pattern transfer S200 is electroplated to form a current-accumulating layer on the copper-clad layer surface corresponding to the stress-polymerization pattern, and then the plating pattern is removed. The current-accumulating layer is a raised solid structure that grows in the opening area corresponding to the stress-polymerization pattern during the electroplating process. Its shape corresponds to the stress-polymerization pattern. As a sacrificial layer for the protrusion, it can disturb the flow of the etching solution during subsequent etching, accelerate local etching solution exchange, and thus improve the etching rate of the cold spot area.

[0032] In the second pattern transfer S400, the copper-clad layer surface is exposed and developed to form a first etch pattern. The first etch pattern includes a stress relief pattern and a border pattern. The stress relief pattern is arranged in the stress hot spot area and located in the etch area, and the border pattern is arranged at the edge of the current-collecting layer.

[0033] Furthermore, in the initial etching S500, the inner layer board after the second pattern transfer S400 is etched to form a guide section through stress-relieving patterns and a connecting section through edge patterns. It is understood that the guide section can guide the flow of the etching solution during subsequent etching processes, dispersing locally high-concentration solutions and thus reducing the etching rate in hot spots.

[0034] In the third pattern transfer S600, a second etch pattern is formed on the surface of the copper-clad layer by exposure and development. The second etch pattern includes etched areas.

[0035] Furthermore, in the circuit etching S700, the inner layer board after the third pattern transfer S600 is etched to form the main circuit on the surface of the inner layer board, and the current guide is partially etched to form the first fragile neck, and the connection part is partially etched to form the second fragile neck.

[0036] Finally, in the cleaning and waste removal S800, after the line etching S700, the inner layer board is passed through a cleaning solution to clean the residual etching solution. The cleaning solution is configured to be connected to an ultrasonic vibrator, which can drive the first and second fragile necks to break, thereby driving the guide section and the current-collecting layer to detach from the main line.

[0037] The design of the first and second fragile necks allows the flow guide and flow-gathering layer to automatically detach during the cleaning and waste removal process of S800, eliminating the need for additional removal steps.

[0038] In some embodiments of this application, in the partition design S100, the grid is a square grid, and the side length of the square grid is 3 to 5 times the minimum line width of the inner layer plate surface.

[0039] In another implementation, the mesh division in the partitioning design S100 can adopt an adaptive mesh division method, that is, using a smaller mesh size in areas with drastic changes in copper thickness or pattern density, and a larger mesh size in areas with gradual changes, so as to reduce the amount of computation while ensuring accuracy. In yet another implementation, the mesh can also adopt a rectangular mesh or a hexagonal mesh to adapt to the characteristics of different circuit layouts.

[0040] Optionally, the copper thickness distribution data is obtained by using an eddy current thickness gauge, and the graphic density distribution data is obtained by superimposing the circuit design diagram of the inner layer board with the grid and calculating the proportion of copper foil area in each grid. By reasonably setting the grid size and using an eddy current thickness gauge, both zoning accuracy and detection efficiency can be taken into account.

[0041] In another embodiment, copper thickness distribution data can also be obtained using an X-ray thickness gauge or a backscattered electron detector to suit inner layer boards of different materials and thicknesses. In yet another embodiment, pattern density distribution data can be directly extracted using computer-aided design software, or obtained from the actual board surface pattern distribution information using an optical scanner, thereby improving the flexibility of data acquisition.

[0042] Specifically, in the partitioned design S100, the etching stress index is calculated from at least one of the following: copper thickness difference coefficient within the grid, pattern density difference coefficient, local pattern density gradient coefficient, and etching difficulty coefficient.

[0043] The copper thickness difference coefficient reflects the degree of non-uniformity in copper thickness distribution within the grid, and its calculation formula is as follows: C _cu = |T _top - T _bottom | / T _avg × k _1 Among them, T _top T represents the copper thickness of the mesh on the upper surface. _bottom T represents the copper thickness of the mesh on the lower surface. _avg The average copper thickness of the grid on both the top and bottom surfaces is T. _avg = (T _top + T _bottom ) / 2, k _1 This is the weighting coefficient for copper thickness difference, with a value ranging from 0.5 to 2.0.

[0044] The graphic density difference coefficient reflects the variation in graphic density within the grid, and its calculation formula is as follows: C _den = |D _top - D _bottom | / D _avg × k _2+ α × |D _local - D _global | / D _global Among them, D _top and D _bottom These are the graphic densities of the grid on the top and bottom surfaces, respectively, D. _avg The average graphic density of the grid on both the top and bottom surfaces is D. _avg = (D _top + D _bottom ) / 2,D _local D represents the graphic density of the grid. _global k represents the average graphic density of the entire board surface. _2 α is the graphic density difference weighting coefficient, with a value ranging from 0.3 to 1.5, and α is the local deviation adjustment coefficient, with a value ranging from 0.2 to 1.0.

[0045] The local graphic density gradient coefficient reflects the degree of drastic change in graphic density between adjacent meshes, and its calculation formula is as follows: C _grad = 1 / n × Σ _i =1^n (|D _center - D _neighbor ,i| / D _center ) × k _3 Among them, D _center D is the graphic density of the central grid. _neighbor ,i is the graph density of the i-th adjacent grid, n is the number of adjacent grids, usually 4 or 8, k _3 This is the gradient weight coefficient, with a value ranging from 0.5 to 2.0.

[0046] The etching difficulty coefficient reflects the difficulty of etching the circuit pattern within the mesh, and its calculation formula is as follows: C _etch = (W _ref / W _min )^k _4 + (S _ref / S _min )^k _5 Among them, W _min S is the minimum line width within this grid. _min W represents the minimum spacing within the grid. _ref and S _ref For reference line width and reference spacing, typically 100 μm, k _4 and k _5 This is the difficulty index coefficient, with a value ranging from 0.5 to 1.5.

[0047] By combining these coefficients, the etching stress level of each grid can be assessed more accurately.

[0048] In one implementation, the etching stress index H can be calculated using a weighted summation method.

[0049] Right now: H = β _1 × C _cu + β _2 × C _den + β _3 × C _grad + β _4 × C _etch , Where β_1 to β_4 are the weighting factors for each coefficient, satisfying β _1 + β _2 + β _3 + β _4 = 1, with default recommended weight values ​​of 0.3, 0.3, 0.2, and 0.2 respectively.

[0050] In another implementation, the etching stress index H can also be calculated using a product method, i.e.: H = C _cu ^a × C _den ^b × C _grad ^c × C _etch ^d, Where a, b, c, and d are the exponential factors of each coefficient, which can be adjusted according to actual process requirements.

[0051] In another implementation, the calculation of the etching stress index can also take into account factors such as the angle between the extension direction of the lines in the grid and the direction of the etchant spray, and the corner density of the lines in the grid, so as to more comprehensively evaluate the etching stress.

[0052] In some embodiments of this application, the etching stress index is H, and the circuit board etching method includes a first boundary value A, a second boundary value B, and a third boundary value C, wherein a second preset threshold < A < B < C.

[0053] When the etching stress index within the grid meets the second preset threshold <H <A, the stress relief pattern includes stress relief lines. The line width of the stress relief lines is the same as the line width of the signal lines of the inner layer board, and the spacing of the stress relief lines is greater than twice the spacing of the signal lines of the inner layer board. The stress relief lines are used to increase the pattern density to balance the etching rate.

[0054] When the etching stress index within the mesh satisfies A < H < B, the stress relief pattern includes circular stress equalization blocks. The diameter of the circular stress equalization blocks is 1.5 to 2 times the linewidth of the signal lines on the inner layer board. The circular stress equalization blocks are used to consume the etching solution during the etching process to slow down the etching rate.

[0055] When the etching stress index within the mesh satisfies B < H < C, the stress relief pattern includes a dumbbell-shaped channel. The dumbbell-shaped channel includes two ends and a middle section. The width of the ends is greater than the width of the middle section. The dumbbell-shaped channel is connected to the main line through the middle section. The dumbbell-shaped channel is used to guide the flow of etching solution during the etching process to equalize the concentration of the etching solution.

[0056] When the etching stress index within the mesh satisfies C < H, the stress relief pattern includes a snowflake-shaped stress equalization block. The snowflake-shaped stress equalization block includes a center point and multiple arms radiating outward from the center point. The end of the arm opposite to the center point is connected to the main line. The snowflake-shaped stress equalization block is used to equalize the flow of etching solution from multiple directions to eliminate turbulence during the etching of the S700 line.

[0057] By setting different stress release graphs and corresponding stress index ranges, differentiated control measures can be taken for stress hotspot areas of different degrees.

[0058] In some applications, stress relief lines can also be designed with a wavy or serrated shape to increase their contact area with the solution and further improve the equalization effect.

[0059] In other applications, circular stress equalization blocks can also be designed in elliptical or polygonal shapes to accommodate different circuit layout orientations.

[0060] In some applications, the ratio of the end to the middle of the dumbbell-shaped channel can be adjusted according to the actual etching stress index. The higher the stress index, the greater the width ratio of the end to the middle.

[0061] In some further applications, the number of arms of the snowflake-shaped stress equalization block can be adjusted according to the stress index. The higher the stress index, the more arms there are, for example, it can be set to 6 or 8 arms.

[0062] In some embodiments of this application, the material of the current-collecting layer is nickel or tin, and the thickness of the current-collecting layer is proportional to the etching stress index of the stress cold spot region. Specifically, when the etching stress index of the stress cold spot region is lower, that is, when the etching rate is slower, the thickness of the current-collecting layer is thinner; when the etching stress index of the stress cold spot region is higher, that is, when it is close to the first preset threshold, the thickness of the current-collecting layer is thicker.

[0063] By making the thickness of the flow-forming layer proportional to the stress index, differentiated chemical disturbance effects can be provided for cold spot areas of varying degrees.

[0064] In some embodiments of this application, the etching stress index is H, and the circuit board etching method includes a fourth boundary value D, a fifth boundary value E, and a sixth boundary value F, wherein D < E < F < a first preset threshold.

[0065] When the etching stress index within the grid satisfies H < D, the stress aggregation pattern is elongated, and the electroplated aggregation layer is a flow guide fin. Specifically, the length direction of the flow guide fin is parallel to the spraying direction of the etching solution, and the height of the flow guide fin is 1 to 2 times the thickness of the copper cladding layer. The flow guide fin is used to guide the etching solution to the stress cold spot area to improve the chemical exchange rate.

[0066] In some applications, the number of guide fins can be set to multiple and arranged in parallel along the spray direction to form a guide fin array to enhance the guiding effect.

[0067] It should be noted that during the electroplating process, the coating in the elongated stress polymerization pattern grows within the elongated opening to form an elongated protruding structure, namely a flow guide fin. The flow guide fin extends along the spray direction and can guide the chemical solution to flow along the length direction, introducing the chemical solution into the cold spot area.

[0068] When the etching stress index within the mesh satisfies D < H < E, the stress aggregation pattern is cylindrical, and the electroplated current aggregation layer is a turbulence column group. Specifically, the turbulence column group includes multiple cylindrical protrusions distributed in an array. The diameter of the cylindrical protrusions is 2 to 3 times the thickness of the copper cladding layer, and the spacing between adjacent cylindrical protrusions is 1.5 to 2 times the diameter of the cylindrical protrusions. The turbulence column group is used to generate turbulence in the etching solution to improve the etching rate.

[0069] In some applications, the cylindrical protrusions in the turbulence column group can also be arranged in a hexagonal or rhomboid pattern to generate turbulence effects in different directions.

[0070] It should be noted that the columnar stress-aggregation pattern consists of multiple independent circular or near-circular openings. During the electroplating process, a cylindrical protrusion grows within each columnar opening, forming a group of turbulent columns. These columnar protrusions can disrupt the flow lines of the chemical solution, generate local turbulence, and enhance chemical exchange.

[0071] When the etching stress index within the grid satisfies E < H < F, the stress aggregation pattern is trapezoidal, and the electroplated current aggregation layer is a current aggregation bump. Specifically, the height of the current aggregation bump is 2 to 3 times the thickness of the copper cladding layer, and the bottom diameter of the current aggregation bump is 3 to 5 times the thickness of the copper cladding layer. The current aggregation bump is used to accumulate the etching solution during the etching process to accelerate etching.

[0072] In some applications, the flow-gathering boss can also be designed in a conical or parabolic shape to change the flow characteristics of the drug flow.

[0073] It should be noted that the trapezoidal stress polymerization pattern is a trapezoidal opening that is narrow at the top and wide at the bottom. During the electroplating process, the coating grows in the trapezoidal opening to form a boss structure that is small at the top and large at the bottom, namely a flow-gathering boss. This shape allows the chemical solution to accumulate around the boss, forming a local high-concentration area and accelerating etching.

[0074] When the etching stress index within the mesh satisfies F < H < the first preset threshold, the stress aggregation pattern is a composite column and trapezoid shape, and the electroplated aggregation layer is a composite aggregation structure. Specifically, the composite aggregation structure includes a central aggregation boss and a group of turbulence pillars arranged around the aggregation boss. The turbulence pillars are located around the aggregation boss. The composite aggregation structure is used to jointly achieve chemical aggregation and turbulence disturbance during the etching process.

[0075] It should be noted that the composite columnar and trapezoidal stress aggregation pattern refers to a grid that simultaneously contains a trapezoidal opening at the center and multiple columnar openings surrounding the trapezoidal opening. During the electroplating process, a central flow-gathering protrusion grows within the trapezoidal opening, while a surrounding group of turbulent columns grows within the columnar opening. The two work together, with the central flow-gathering protrusion responsible for collecting the chemical solution and the surrounding turbulent columns responsible for generating turbulence, resulting in a composite control effect.

[0076] In some applications, the number and density of turbulence-generating columns in a composite flow-gathering structure can be adjusted according to the size of the flow-gathering protrusions and the stress index.

[0077] It should be noted that the first and second preset thresholds can be determined experimentally. Specifically, multiple etching tests are conducted for different types of inner layer boards, and the etching effects under different etching stress indices are recorded to determine the optimal threshold. Alternatively, the first and second preset thresholds can be dynamically adjusted based on historical production data to adapt to the actual characteristics of the current batch of inner layer boards.

[0078] In some embodiments of this application, during the initial etching S500, a first neck is formed between the current guide portion and the main line, and a second neck is formed between the connection portion and the main line. The width of the first neck and the second neck is 1 / 2 to 2 / 3 of the line width of the main line.

[0079] After the S700 line is etched, a first neck is formed into a first breakable neck, and a second neck is formed into a second breakable neck. The width of the first breakable neck and the second breakable neck is 1 / 5 to 1 / 3 of the line width of the main line.

[0080] By setting the neck width appropriately, the neck maintains sufficient strength to withstand subsequent processes after the initial etching of S500, while forming a sufficiently weak and brittle neck after the line etching of S700, ensuring reliable breakage during the cleaning and waste removal process of S800.

[0081] In some embodiments of this application, in the initial etching S500, the etching depth of the inner layer board is 30% to 50% of the copper cladding thickness to form a first neck and a second neck. Thus, by controlling the depth of the initial etching S500, the shape and size of the neck can be precisely controlled, laying the foundation for the subsequent formation of the fragile neck.

[0082] In some embodiments of this application, during the cleaning and waste removal process S800, the frequency of the ultrasonic vibrator is 20kHz to 40kHz, and the power density is 0.5W / cm² to 2W / cm². The first and second fragile necks break sequentially or simultaneously under the action of the ultrasonic waves. After breakage, the guide portion and the current-gathering layer detach from the main circuit and are carried away from the surface of the inner layer plate by the cleaning fluid. It is understood that by reasonably setting the ultrasonic parameters, reliable breakage of the fragile necks can be ensured while avoiding damage to the main circuit.

[0083] In one embodiment, the initial etching S500 can be performed using a horizontal spray etching method, where the etching depth can be precisely controlled by adjusting the spray pressure, flow rate, and conveying speed. Alternatively, the initial etching S500 can also be performed using an immersion etching method, which is suitable for application scenarios where the etching depth requirement is particularly precise.

[0084] In summary, the following is an example of a complete embodiment.

[0085] The inner layer has a copper cladding thickness of 12μm, a signal line width of 50μm, a signal line spacing of 50μm, and a minimum line width of 30μm.

[0086] To address this, the S100 partition design uses a square grid with a side length of 120μm, which is four times the minimum linewidth, and a copper thickness variation coefficient C. _cu In the calculation, k _1 Set to 1.0. Graphic density difference coefficient C _den In the calculation, k _2 We set 0.8 and α to 0.5. Local graphic density gradient coefficient C _grad In the calculation, n is 8, k _3 Set to 1.0. Etching difficulty coefficient C _etch In the calculation, W _ref Take 100μm, S _ref Take 100μm, k _4 Take 1.0, k _5 The value is set to 1.0. The etching stress exponent H is calculated using a weighted summation method, β._1 Take 0.3, β _2 Take 0.3, β _3 Take 0.2, β _4 Take 0.2.

[0087] The first preset threshold is 0.3, and the second preset threshold is 0.6. That is, within the same plane, when the etching stress index H of the mesh is less than 0.3, the mesh is identified as a stress cold spot region; when H is greater than 0.6, it is identified as a stress hot spot region; when 0.3 ≤ H ≤ 0.6, the mesh is a normal region and no auxiliary graphic layout is required.

[0088] For stress hotspot regions, the first boundary value A is 0.65, the second boundary value B is 0.75, and the third boundary value C is 0.85. When the etching stress index H of the mesh satisfies 0.6 < H < 0.65, the stress release pattern is a stress release line with a line width of 50 μm and a spacing of 120 μm; when H satisfies 0.65 < H < 0.75, the stress release pattern is a circular stress equalization block with a diameter of 85 μm; when H satisfies 0.75 < H < 0.85, the stress release pattern is a dumbbell-shaped guide channel with an end width of 80 μm and a middle width of 40 μm; when H > 0.85, the stress release pattern is a snowflake-shaped stress equalization block with a center point diameter of 30 μm, 6 arms, and an arm width of 20 μm.

[0089] For the stress cold spot region, the fourth boundary value D is 0.05, the fifth boundary value E is 0.10, and the sixth boundary value F is 0.20. When the etching stress index H of the mesh satisfies H < 0.05, the stress aggregation pattern is elongated, and the electroplated current-gathering layer is a flow-guiding fin with a height of 15 μm, a length of 500 μm, and a width of 30 μm, arranged parallel to each other along the spray direction with a spacing of 100 μm; when H satisfies 0.05 < H < 0.10, the stress aggregation pattern is cylindrical, and the electroplated current-gathering layer is a group of turbulence pillars with a diameter of 30 μm and a spacing of 50 μm between adjacent cylindrical protrusions, arranged in an array with a row spacing and column spacing of 50 μm; when H satisfies 0.10 < H < 0.05, the stress aggregation pattern is cylindrical, and the electroplated current-gathering layer is a group of turbulence pillars with a diameter of 30 μm and a spacing of 50 μm between adjacent cylindrical protrusions, arranged in an array with a row spacing and column spacing of 50 μm. When H is 0.20, the stress aggregation pattern is trapezoidal, and the electroplated current-aggregating layer is a current-aggregating boss with a height of 30 μm, a bottom diameter of 45 μm, and a top diameter of 25 μm. When H satisfies 0.20 < H < 0.30, the stress aggregation pattern is a composite of columnar and trapezoidal shapes, and the electroplated current-aggregating layer is a composite current-aggregating structure. The height of the central current-aggregating boss is 30 μm, the bottom diameter is 45 μm, and the top diameter is 25 μm. The turbulence column group surrounding the current-aggregating boss consists of 8 cylindrical protrusions with a diameter of 25 μm and a distance of 60 μm from the center point of the current-aggregating boss.

[0090] The current-collecting layer is made of nickel and is electroplated using DC current with a current density of 2A / dm² and an electroplating time of 8 minutes to achieve the target thickness. In the initial etching of S500, the etching depth is 40% of the copper layer thickness, i.e., 4.8μm. The width of the first and second necks is 60% of the main line width, i.e., 30μm.

[0091] After the S700 line etching, the width of the first and second fragile necks is 25% of the main line width, i.e., 12.5 μm. During the cleaning and waste removal process S800, the ultrasonic vibrator frequency is 28 kHz, the power density is 1.0 W / cm², the cleaning fluid temperature is 45 °C, and the transmission speed is 2 m / min. The first and second fragile necks break under the action of ultrasonic waves, and the guide section and the current-collecting layer detach from the main line and are discharged with the cleaning fluid.

[0092] The circuit board according to embodiments of the present invention is manufactured using the circuit board etching method described in any of the above embodiments. By processing the circuit board using the above method, the uniformity of the main line width in each region of the same surface of the circuit board is significantly improved, and the consistency of the lateral etching amount at the line edges is good, effectively avoiding line defects caused by local over-etching or under-etching.

[0093] Meanwhile, as auxiliary structures such as the current-gathering layer and the current-guiding section play a regulatory role in the stress cold point area and the stress hot point area respectively during the etching process, the linewidth uniformity of the main circuit of the circuit board is significantly improved, and the side etching amount of the circuit edge is consistent, effectively avoiding circuit defects caused by local over-etching or under-etching.

[0094] Other configurations and operations of the circuit board according to embodiments of the present invention are known to those skilled in the art and will not be described in detail here.

[0095] The embodiments of the present invention have been described in detail above with reference to the accompanying drawings. However, the present invention is not limited to the above embodiments. Within the scope of knowledge possessed by those skilled in the art, various changes can be made without departing from the spirit of the present invention.

Claims

1. A method for etching a circuit board, for etching processing of an inner layer board having a copper-clad layer on a surface, the inner layer board including an etching area, characterized by, Includes the following steps: The inner layer board is divided into multiple grids on its surface. Copper thickness distribution data and pattern density distribution data of the inner layer board surface are obtained. Based on the copper thickness distribution data and the pattern density distribution data, the etching stress index of each grid is calculated. The grid with an etching stress index less than a first preset threshold is identified as a stress cold spot area, and the grid with an etching stress index greater than a second preset threshold is identified as a stress hot spot area. In the first pattern transfer, after the partition design, the copper-clad layer surface is exposed and developed to form a plating pattern, the plating pattern including a stress-polymerization pattern, the stress-polymerization pattern being arranged in the stress cold spot region and located in the etching area; Electroplating: After the first pattern transfer, the inner layer board is electroplated to form a current-accumulating layer on the copper-clad layer surface corresponding to the stress-polymerization pattern, and then the plating pattern is removed. The second pattern transfer involves forming a first etched pattern on the surface of the copper-clad layer after electroplating through exposure and development. The first etched pattern includes a stress relief pattern and an edge pattern. The stress relief pattern is located in the stress hot spot area and in the etched area, and the edge pattern is arranged at the edge of the current-collecting layer. First etching: After the second pattern transfer, the inner layer plate is etched to form a guide section through the stress relief pattern and a connecting section through the edge pattern; The third pattern transfer occurs after the second pattern transfer, whereby the surface of the copper-clad layer is exposed and developed to form a second etched pattern, the second etched pattern including etched areas. The inner layer board is etched after the third pattern transfer to form the main circuit on the surface of the inner layer board. The current guide portion is etched to form a first breakable neck, and the connection portion is etched to form a second breakable neck. After the circuit etching, the inner layer board is cleaned by passing a cleaning solution to remove the etching solution. The cleaning solution is configured to be connected to an ultrasonic vibrator, which can drive the first and second fragile necks to break, thereby driving the flow guide and the current-collecting layer to detach from the main circuit.

2. The circuit board etching method according to claim 1, characterized by: In the partition design, the grid is a square grid, and the side length of the square grid is 3 to 5 times the minimum linewidth of the inner layer board surface; the copper thickness distribution data is obtained by an eddy current thickness gauge, and the graphic density distribution data is obtained by superimposing the circuit design diagram of the inner layer board with the grid and calculating the proportion of copper foil area in each grid.

3. The circuit board etching method of claim 1, wherein: In the partitioned design, the etching stress index is calculated from at least one of the following: copper thickness difference coefficient, pattern density difference coefficient, local pattern density gradient coefficient, and etching difficulty coefficient within the grid.

4. The circuit board etching method according to claim 3, wherein: The etching stress index is H, and the circuit board etching method includes a first boundary value A, a second boundary value B and a third boundary value C, and a second preset threshold < A < B < C. When the second preset threshold of the etching stress index within the grid is <H < A, the stress relief pattern includes stress relief lines. The line width of the stress relief lines is the same as the line width of the signal lines of the inner layer board. The spacing of the stress relief lines is greater than twice the spacing of the signal lines of the inner layer board. The stress relief lines are used to increase the pattern density to balance the etching rate. When the etching stress index A < H < B within the grid, the stress relief pattern includes a circular stress equalization block. The diameter of the circular stress equalization block is 1.5 to 2 times the width of the signal line of the inner layer board. The circular stress equalization block is used to consume etching solution during the etching process to slow down the etching rate. When the etching stress index B < H < C within the grid, the stress relief pattern includes a dumbbell-shaped guide channel. The dumbbell-shaped guide channel includes two ends and a middle part. The width of the ends is greater than the width of the middle part. The dumbbell-shaped guide channel is connected to the main line through the middle part. The dumbbell-shaped guide channel is used to guide the flow of etching solution during the etching process to equalize the concentration of the etching solution. When the etching stress index C < H within the grid, the stress relief pattern includes a snowflake-shaped stress equalization block. The snowflake-shaped stress equalization block includes a center point and multiple arms radiating outward from the center point. The end of the arm opposite to the center point is connected to the main line. The snowflake-shaped stress equalization block is used to equalize the flow of etching solution from multiple directions during the line etching process to eliminate turbulence.

5. The circuit board etching method of claim 3, wherein: The material of the current-collecting layer is nickel or tin, and the thickness of the current-collecting layer is proportional to the etching stress index of the stress cold spot region.

6. The circuit board etching method of claim 5, wherein: The etching stress index is H, and the circuit board etching method includes a fourth boundary value D, a fifth boundary value E and a sixth boundary value F, wherein D < E < F < a first preset threshold. When the etching stress index within the grid satisfies H < D, the stress aggregation pattern is elongated, the electroplated current aggregation layer is a flow guide fin, the length direction of the flow guide fin is parallel to the spraying direction of the etching solution, the height of the flow guide fin is 1 to 2 times the thickness of the copper cladding layer, and the flow guide fin is used to guide the etching solution to the stress cold spot region to improve the chemical exchange rate. When the etching stress index within the grid satisfies D < H < E, the stress aggregation pattern is cylindrical, and the electroplated current aggregation layer is a turbulence column group. The turbulence column group includes multiple cylindrical protrusions distributed in an array. The diameter of the cylindrical protrusions is 2 to 3 times the thickness of the copper cladding layer, and the spacing between adjacent cylindrical protrusions is 1.5 to 2 times the diameter of the cylindrical protrusions. The turbulence column group is used to generate turbulence in the etching solution to improve the etching rate. When the etching stress index within the grid satisfies E < H < F, the stress aggregation pattern is trapezoidal, the electroplated current aggregation layer is a current aggregation protrusion, the height of the current aggregation protrusion is 2 to 3 times the thickness of the copper cladding layer, the bottom diameter of the current aggregation protrusion is 3 to 5 times the thickness of the copper cladding layer, and the current aggregation protrusion is used to accumulate chemicals during the etching process to accelerate etching. When the etching stress index within the grid satisfies F < H < first preset threshold, the stress aggregation pattern is a composite column and trapezoid shape, and the electroplated current aggregation layer is a composite current aggregation structure. The composite current aggregation structure includes a central current aggregation boss and a group of turbulence pillars arranged around the current aggregation boss. The turbulence pillars are located around the current aggregation boss. The composite current aggregation structure is used to jointly achieve chemical aggregation and turbulence disturbance during the etching process.

7. The circuit board etching method according to claim 1, characterized in that: In the initial etching, a first neck is formed between the guide portion and the main line, and a second neck is formed between the connection portion and the main line. The width of the first neck and the second neck is 1 / 2 to 2 / 3 of the linewidth of the main line. After the line is etched, the first neck forms the first fragile neck, and the second neck forms the second fragile neck after the line is etched. The width of the first fragile neck and the second fragile neck is 1 / 5 to 1 / 3 of the line width of the main line.

8. The circuit board etching method according to claim 7, characterized in that: In the initial etching, the inner layer is etched to a depth of 30% to 50% of the copper cladding thickness to form the first neck and the second neck.

9. The circuit board etching method according to claim 1, characterized in that: During the cleaning and waste removal process, the frequency of the ultrasonic vibrator is 20kHz to 40kHz, and the power density is 0.5W / cm² to 2W / cm². The first and second fragile necks break sequentially or simultaneously under the action of ultrasonic waves. After the breakage, the guide part and the flow-gathering layer fall off from the main circuit and are carried away from the surface of the inner layer plate by the cleaning fluid.