Preparation method of thick copper printed circuit board applied to new energy battery management system
By employing a step-by-step process, including filling circuit gaps with prepreg, drilling and electroplating, and laminating with non-prepreg, the problems of residual adhesive in vias and insufficient adhesive filling in circuit gaps on thick copper printed circuit boards are solved, improving product reliability and yield. This technology is suitable for new energy battery management systems.
Patent Information
- Application Number
- CN202611461972.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-20
- Publication Date
- 2026-11-24
AI Technical Summary
Existing technologies cannot simultaneously solve the problems of residual adhesive in vias and insufficient adhesive filling in line gaps under high voltage and high current conditions on thick copper printed circuit boards, resulting in insufficient product reliability and yield.
The process is carried out in steps. First, the prepreg is used to fill the gaps in the circuit under conventional lamination parameters. Then, drilling and electroplating are performed. Finally, a non-prepreg is used for lamination to ensure that there is no residual adhesive in the vias and that the gaps in the circuit are filled.
It achieves high reliability and high yield of thick copper printed circuit boards, avoids copper foil deformation and abnormal via resistance, and is suitable for fields such as new energy battery management systems.
Smart Images

Figure CN123164673A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of printed circuit board manufacturing technology, and specifically to a method for preparing thick copper printed circuit boards used in new energy battery management systems. Background Technology
[0002] Battery management system (BMS) circuit boards for new energy applications are mostly used in high-voltage, high-current conditions, requiring extremely high reliability of via continuity and cleanliness of via walls. BMS circuit boards typically employ thick copper structures to meet high current-carrying capacity requirements, and their manufacturing process faces a series of unique technical challenges.
[0003] Prepreg (PP) used in printed circuit board lamination processes can be broadly classified into two categories based on resin flowability: flowable prepreg and non-flowable prepreg. Flowable prepreg exhibits high resin flowability under high-temperature lamination conditions, effectively filling gaps between circuits. However, resin easily overflows into vias, causing residual resin blockage. Subsequent chemical desmearing processes struggle to completely remove this residue, leading to quality issues such as abnormal via resistance, poor conductivity, and burn-in vias. Therefore, high-reliability BMS circuit boards tend to use non-flowable prepreg for lamination to eliminate via residual resin defects from the outset.
[0004] However, non-flowing prepreg resin has extremely poor flowability. In thick copper PCB structures, the thick copper layer exerts a strong compressive force on the prepreg material. Conventional lamination processes cannot achieve sufficient resin filling in the gaps and edges of the thick copper, frequently resulting in defects such as insufficient resin at copper edges, voids in circuit gaps, and exposed fiberglass. Existing improvement methods mainly include increasing lamination temperature and pressure or replacing with high-flowing prepreg material, but both methods have significant limitations: excessively increasing lamination parameters can easily lead to secondary defects such as copper foil deformation, substrate carbonization, and over-baking of the board; replacing with flowable prepreg will result in residual resin in vias. Therefore, existing technologies cannot simultaneously meet the structural accuracy, electrical insulation performance, and production yield requirements of thick copper BMS circuit boards, exhibiting significant technical shortcomings. Summary of the Invention
[0005] In view of the above-mentioned defects and deficiencies in the prior art, the present invention provides a method for manufacturing thick copper printed circuit boards for use in new energy battery management systems, aiming to solve the two major technical problems of insufficient glue filling between thick copper lines and residual glue in vias, thereby improving product yield and reliability.
[0006] To achieve the above objectives, the present invention provides a method for fabricating a thick copper printed circuit board for use in a new energy battery management system, comprising the following steps: S1. Select a thick copper double-sided board, which includes an FR4 substrate and a first base copper layer and a second base copper layer symmetrically disposed on both sides of the FR4 substrate, wherein the thickness of the first base copper layer and the second base copper layer is 2oz to 6oz.
[0007] S2. After applying photosensitive dry film to both sides of the thick copper double-sided board, exposure, development, acid etching and film removal are performed. The first base copper layer is exposed to preserve the copper surface, and the circuit pattern is etched on the second base copper layer.
[0008] S3. A prepreg and a copper foil layer are sequentially bonded to the surface of the second base copper layer and then pressed at high temperature to allow the prepreg to fill the line spacing of the second base copper layer and cure. The prepreg has a flowability of more than 2.0 mm, a resin content of 65% to 75%, a pressing temperature of 170 to 200°C, a pressing pressure of 280 to 450 psi, and a pressing time of 60 to 120 minutes.
[0009] S4. Mechanical drilling and chemical degumming are performed on the products after high-temperature pressing. The chemical degumming process uses potassium permanganate degumming or plasma degumming.
[0010] S5. Electroplated copper is deposited on the hole wall, the first base copper layer and the copper foil layer of the product obtained in step S4 to make the interlayer of the first base copper layer, the second base copper layer and the copper foil layer conductive. The electroplating current density is 1.5 to 3.0 A / dm² and the thickness of the electroplated copper layer is 20 to 35 μm.
[0011] S6. Repeat the film application, exposure, development, etching and film removal operations of step S2 to process the circuit pattern on the first base copper layer, with only the copper-plated hole areas remaining in the copper foil layer.
[0012] S7. Set the milling machine's drilling depth to the thickness from the copper foil layer to the second base copper layer, and mill away the copper foil layer and the corresponding exposed metal hole area. The control accuracy of the milling machine's drilling depth is ±0.05mm.
[0013] S8. After the product obtained in step S7 has cured, a non-flowing prepreg and a bare board FR4 are sequentially bonded to one side of the curing prepreg, and then pressed and fixed by a high-temperature press to obtain the final thick copper printed circuit board. The non-flowing prepreg has a flowability of 0.2-0.5 mm, a resin content of 55%-65%, a lamination temperature of 180-210°C, a lamination pressure of 300-450 psi, and a lamination time of 90-150 minutes.
[0014] Compared with existing technologies, this invention breaks down the lamination process into specific sequences of prepreg lamination for filling circuits, drilling and electroplating, controlled-depth milling, and non-prepreg lamination. This restructures the process sequence instead of relying on traditional single-parameter optimization or material replacement. On one hand, the good flowability of the prepreg under conventional lamination parameters ensures sufficient filling of gaps in thick copper circuits, effectively avoiding secondary defects such as copper foil deformation, substrate carbonization, and over-baking of the board caused by excessively increasing lamination temperature and pressure. On the other hand, because the drilling and chemical descaling processes are arranged after the prepreg lamination and curing and before the non-prepreg lamination, and the final lamination uses a non-prepreg with extremely low flowability to prevent overflow into the metal holes, this ensures no residual adhesive on the inner walls of the vias from the process source, eliminating quality risks such as abnormal hole resistance, poor conductivity, and hole burning. Simultaneously, the non-prepreg effectively fills the thin prepreg area exposed after controlled-depth milling, further ensuring board surface flatness and interlayer bonding. Each step of this invention is compatible with existing PCB mass production equipment and processes, requires no special material input, and can effectively control manufacturing costs while significantly improving product reliability. It is suitable for large-scale promotion and application in fields such as new energy BMS battery management systems, new energy vehicle electronic control systems, and energy storage systems. Attached Figure Description
[0015] Figure 1 This is a flowchart of the method for preparing a thick copper printed circuit board used in a new energy battery management system according to the present invention.
[0016] Figure 2 This is a schematic diagram of the structure of the thick copper double-sided panel of the present invention.
[0017] Figure 3 This is a schematic diagram of the thick copper double-sided panel structure after the first film application, exposure, development, etching, and film removal in this invention.
[0018] Figure 4 This is a schematic diagram of the thick copper double-sided panel structure formed by bonding a prepreg and a copper foil layer together under high temperature in this invention.
[0019] Figure 5 This is a schematic diagram of the thick copper double-sided panel structure after mechanical drilling in this invention.
[0020] Figure 6 This is a schematic diagram of the thick copper double-sided panel structure after copper deposition and electroplating in this invention.
[0021] Figure 7 This is a schematic diagram of the thick copper double-sided panel structure after the second film application, exposure, development, etching, and film removal in this invention.
[0022] Figure 8 This is a schematic diagram of the thick copper double-sided panel structure after controlled deep milling in this invention.
[0023] Figure 9 This is a schematic diagram of the thick copper double-sided panel structure formed by bonding a non-adhesive prepreg and a FR4 bare board under high temperature in this invention. Detailed Implementation
[0024] The present invention will now be described in detail with reference to specific embodiments. These embodiments will help those skilled in the art to further understand the present invention, but do not limit the invention in any way.
[0025] Example 1 like Figure 1 As shown, this invention provides a method for preparing a thick copper printed circuit board for use in a new energy battery management system, comprising the following steps: S1. Select a thick copper double-sided board.
[0026] The thick copper double-sided board includes an FR4 substrate and a first base copper layer and a second base copper layer symmetrically disposed on both sides of the FR4 substrate. The thickness of the copper layer of the thick copper double-sided board can be determined according to the current carrying requirements of the BMS circuit board, preferably 2oz to 6oz, more preferably 3oz to 4oz. The thickness of the FR4 substrate can be determined according to the design requirements, preferably 0.5mm to 2.0mm.
[0027] S2. After applying photosensitive dry film to both sides of the thick copper double-sided board, exposure, development, acid etching, and film removal are performed.
[0028] A photosensitive dry film is laminated onto the surfaces of the first and second copper base layers. The designed circuit pattern is then exposed using an exposure machine. The photosensitive dry film in the exposed areas undergoes photocuring, while the unexposed areas do not. The preferred exposure energy is 30–80 mJ / cm². 2 In actual operation, adjustments can be made based on the type and thickness of the photosensitive dry film.
[0029] The uncured photosensitive dry film is removed by developing, exposing the copper surface, while the photocured photosensitive dry film is retained. The developing solution is preferably a sodium carbonate solution with a concentration of 0.8% to 1.2% and a temperature of 28 to 32°C.
[0030] The copper is removed by acid etching, where an acidic solution reacts with the exposed copper. The etching solution is preferably an acidic copper chloride etching solution or an acidic ferric chloride etching solution, and the etching temperature is preferably 45–55°C.
[0031] Finally, the photopolymerized dry film is removed to expose the copper layer, yielding the desired patterned circuit. The stripping solution is preferably a sodium hydroxide solution with a concentration of 3%–5%, and the temperature is preferably 45–55°C.
[0032] In this process, the first base copper layer is fully exposed to preserve the copper surface, while the second base copper layer is etched with circuit patterns. The circuit patterns of the second base copper layer are determined according to the electrical design of the BMS circuit board, including power lines, signal lines, etc.
[0033] S3. Adhesive prepreg and copper foil layer are sequentially bonded to the surface of the second base copper layer and then pressed together at high temperature.
[0034] One side of the prepreg is bonded to a second base copper layer, and the other side is bonded to a copper foil layer (preferably 1 / 2 oz copper foil), and then pressed together using a high-temperature press. The prepreg exhibits fluidity under high temperature conditions, achieving full filling of the spacing between the lines in the second base copper layer under high pressure. The pressing temperature of the prepreg is 170–200°C, preferably 180–190°C; the pressing pressure is 280–450 psi, preferably 320–380 psi; and the pressing time is 60–120 minutes, preferably 75–90 minutes. The prepreg first melts and flows to fill the spacing between the lines under high temperature, and then the curing agent in the prepreg cures under high temperature and high pressure.
[0035] The preferred prepreg is a high-flow-rate FR4 prepreg with a flowability of 2.0 mm or more and a resin content of 65% to 75%.
[0036] S4. Mechanical drilling and chemical degumming are performed on the products after high-temperature pressing.
[0037] Based on actual design requirements, mechanical drilling is performed on the products after high-temperature pressing. Drilling is conducted using a PCB-specific CNC drilling machine. The drill bit diameter is determined according to the designed through-hole size, preferably 0.2mm to 1.0mm. The preferred drilling speed is 80,000 to 150,000 rpm, and the preferred feed rate is 1.0 to 2.5 m / min.
[0038] After drilling, chemical degumming is performed to ensure the borehole is clean and free of residual adhesive. Preferred chemical degumming methods include potassium permanganate degumming or plasma degumming. Taking potassium permanganate degumming as an example, the process includes swelling, potassium permanganate oxidation, and neutralization / reduction steps; taking plasma degumming as an example, plasma treatment is performed using a CF4 / O2 mixed gas. The cleanliness of the borehole wall after degumming must meet IPC standard requirements.
[0039] S5. Electroplated copper is deposited on the hole walls, the first base copper layer, and the copper foil layer of the product obtained in step S4.
[0040] Through an electrochemical reaction, a layer of electroplated copper is deposited on the hole wall, the first base copper layer, and the copper foil layer, thereby achieving interlayer conductivity between the first base copper layer, the second base copper layer, and the copper foil layer. The main component of the electroplating solution is copper sulfate, with a preferred concentration of 60–80 g / L, a preferred concentration of sulfuric acid of 180–220 g / L, and a preferred concentration of chloride ions of 40–80 ppm. The electroplating current density is 1.5–3.0 A / dm², preferably 2.0–2.5 A / dm²; the electroplating time is determined according to the required copper plating thickness, with a copper plating layer thickness of 20–35 μm, preferably 25–30 μm.
[0041] S6. Repeat step S2 for film application, exposure, development, etching, and film removal.
[0042] After applying a photosensitive dry film to the surfaces of the first base copper layer and the copper foil layer, exposure is performed. The first base copper layer is exposed according to the designed circuit pattern, while the copper foil layer only exposes and protects the areas where the copper is plated for vias; the dry film in the non-metallic via areas is not exposed. After development and etching, the copper layer in the non-metallic via areas of the copper foil layer is etched away, leaving only the copper layer in the areas where the copper is plated for vias, thus preserving the interlayer conductivity between the first base copper layer, the second base copper layer, and the copper foil layer. Finally, the dry film is removed.
[0043] S7. Set the milling machine's drilling depth to the thickness from the copper foil layer to the second base copper layer, and mill away the copper foil layer and its corresponding exposed metal hole area.
[0044] In this step, the controlled depth milling depth is the thickness from the upper surface of the copper foil layer to the upper surface of the second base copper layer, with a control accuracy of ±0.05mm. The milling cutter diameter is preferably 0.8–2.0mm, the milling speed is preferably 30,000–60,000rpm, and the feed rate is preferably 0.5–1.5m / min.
[0045] After controlled-depth milling, the final metal hole only connects the first and second base copper layers, and the copper foil layer is completely removed in this area. After controlled-depth milling, the surface of the cured prepreg is exposed, providing a bonding surface for the non-cured prepreg lamination in step S8.
[0046] S8. After the product obtained in step S7 has cured, the non-cured semi-cured sheet and the bare plate FR4 are sequentially bonded to one side, and then pressed and fixed by a high-temperature press.
[0047] One side of the non-flowing prepreg is attached to one side of the cured, flowing prepreg that was exposed in step S7, and the other side is attached to the bare board FR4. The non-flowing prepreg has extremely low flowability at high temperatures, with a flowability of 0.2–0.5 mm and a resin content of 55%–65%. It cannot fill the line spacing on the surface of the second base copper layer, nor will there be any excess adhesive entering the metal holes. However, it can fill the areas where the very thin cured flowing prepreg has been milled away.
[0048] FR4 blank sheet does not melt or flow under high temperature and high pressure conditions, and mainly serves to thicken and improve the hardness and flatness of the final product. The thickness of the FR4 blank sheet is determined according to the thickness requirements of the final product, and is preferably 0.5mm to 1.5mm.
[0049] The lamination temperature of the non-flowing prepreg is 180–210°C, preferably 190–200°C; the lamination pressure is 300–450 psi, preferably 350–400 psi; and the lamination time is 90–150 minutes, preferably 100–120 minutes.
[0050] The final thick copper printed circuit board has no missing or delaminating adhesive layers in the second base copper layer and no residual adhesive in the holes, meeting the high reliability requirements of the BMS circuit board.
[0051] Example 2 The difference between this embodiment and Embodiment 1 is that: In step S1, the thickness of the first base copper layer and the second base copper layer is 2oz, and the thickness of the FR4 substrate is 0.5mm.
[0052] In step S3, the pressing temperature of the prepreg is 170°C, the pressing pressure is 280 psi, and the pressing time is 60 minutes. The flowability of the prepreg is 2.0 mm, and the resin content is 65%.
[0053] In step S5, the electroplating current density for depositing copper is 1.5 A / dm². 2 The thickness of the electroplated copper layer is 20μm.
[0054] In step S7, the depth control accuracy of controlled depth milling is ±0.05mm.
[0055] In step S8, the flowability of the non-flowing prepreg is 0.2 mm, and the resin content is 55%; the lamination temperature of the non-flowing prepreg is 180°C, the lamination pressure is 300 psi, and the lamination time is 90 minutes.
[0056] The remaining steps and parameters are the same as in Example 1.
[0057] Example 3 The difference between this embodiment and Embodiment 1 is that: In step S1, the thickness of the first base copper layer and the second base copper layer is 3oz, and the thickness of the FR4 substrate is 1.0mm.
[0058] In step S3, the pressing temperature of the prepreg is 185°C, the pressing pressure is 350 psi, and the pressing time is 90 minutes. The flowability of the prepreg is 2.5 mm, and the resin content is 70%.
[0059] In step S5, the electroplating current density for depositing copper is 2.5 A / dm². 2 The thickness of the electroplated copper layer is 25μm.
[0060] In step S7, the depth control accuracy of controlled depth milling is ±0.04mm.
[0061] In step S8, the flowability of the non-flowing prepreg is 0.3 mm, and the resin content is 60%; the lamination temperature of the non-flowing prepreg is 190°C, the lamination pressure is 380 psi, and the lamination time is 120 minutes.
[0062] The remaining steps and parameters are the same as in Example 1.
[0063] Example 4 The difference between this embodiment and Embodiment 1 is that: In step S1, the thickness of the first base copper layer and the second base copper layer is 4 oz, and the thickness of the FR4 substrate is 1.2 mm.
[0064] In step S3, the pressing temperature of the prepreg is 190°C, the pressing pressure is 400 psi, and the pressing time is 100 minutes. The flowability of the prepreg is 2.8 mm, and the resin content is 72%.
[0065] In step S4, chemical degumming is performed using plasma degumming technology.
[0066] In step S5, the electroplating current density for depositing copper is 2.0 A / dm². 2 The thickness of the electroplated copper layer is 28μm.
[0067] In step S7, the depth control accuracy of controlled depth milling is ±0.03mm.
[0068] In step S8, the flowability of the non-flowing prepreg is 0.4 mm, and the resin content is 62%; the lamination temperature of the non-flowing prepreg is 200°C, the lamination pressure is 420 psi, and the lamination time is 130 minutes.
[0069] The remaining steps and parameters are the same as in Example 1.
[0070] Example 5 The difference between this embodiment and Embodiment 1 is that: In step S1, the thickness of the first base copper layer and the second base copper layer is 5 oz, and the thickness of the FR4 substrate is 1.5 mm.
[0071] In step S3, the pressing temperature of the prepreg is 200°C, the pressing pressure is 450 psi, and the pressing time is 120 minutes. The flowability of the prepreg is 3.0 mm, and the resin content is 75%.
[0072] In step S4, the chemical degumming process uses potassium permanganate.
[0073] In step S5, the electroplating current density for depositing copper is 3.0 A / dm². 2 The thickness of the electroplated copper layer is 35μm.
[0074] In step S7, the depth control accuracy of controlled depth milling is ±0.02mm.
[0075] In step S8, the flowability of the non-flowing prepreg is 0.5 mm, and the resin content is 65%; the lamination temperature of the non-flowing prepreg is 210°C, the lamination pressure is 450 psi, and the lamination time is 150 minutes.
[0076] The remaining steps and parameters are the same as in Example 1.
[0077] Example 6 The difference between this embodiment and Embodiment 1 is that: In step S1, the thickness of the first base copper layer and the second base copper layer is 6 oz, and the thickness of the FR4 substrate is 2.0 mm.
[0078] In step S3, the pressing temperature of the prepreg is 175°C, the pressing pressure is 320 psi, and the pressing time is 75 minutes. The flowability of the prepreg is 2.2 mm, and the resin content is 68%.
[0079] In step S5, the electroplating current density for depositing copper is 2.2 A / dm². 2 The thickness of the electroplated copper layer is 22μm.
[0080] In step S7, the depth control accuracy of controlled depth milling is ±0.05mm.
[0081] In step S8, the flowability of the non-flowing prepreg is 0.25 mm, and the resin content is 58%; the lamination temperature of the non-flowing prepreg is 185°C, the lamination pressure is 340 psi, and the lamination time is 100 minutes.
[0082] The remaining steps and parameters are the same as in Example 1.
[0083] Example 7 The difference between this embodiment and Embodiment 1 is that: In step S1, the thickness of the first base copper layer and the second base copper layer is 3.5 oz, and the thickness of the FR4 substrate is 0.8 mm.
[0084] In step S3, the pressing temperature of the prepreg is 180°C, the pressing pressure is 380 psi, and the pressing time is 80 minutes. The flowability of the prepreg is 2.6 mm, and the resin content is 70%.
[0085] In step S5, the electroplating current density for depositing copper is 2.8 A / dm². 2 The thickness of the electroplated copper layer is 32μm.
[0086] In step S7, the depth control accuracy of controlled depth milling is ±0.035mm.
[0087] In step S8, the flowability of the non-flowing prepreg is 0.35 mm, and the resin content is 60%; the lamination temperature of the non-flowing prepreg is 195°C, the lamination pressure is 360 psi, and the lamination time is 110 minutes.
[0088] The remaining steps and parameters are the same as in Example 1.
[0089] Although Examples 2-7 used different specific process parameter values, they all followed the core process flow of steps S1 to S8 of this invention. Specifically, the thick copper circuit gaps were first filled using a prepreg with flowable adhesive under conventional lamination parameters, followed by drilling, electroplating, and controlled-depth milling. Finally, a non-flowable prepreg was used to complete the final lamination. Testing showed that the thick copper printed circuit boards obtained in Examples 2-7 all achieved the technical effect of no missing adhesive layer delamination in the second copper base layer and no residual adhesive in the holes. This fully demonstrates that the technical solution of this invention has good feasibility and stability within various process parameter ranges and can meet the high-reliability mass production requirements of BMS circuit boards.
[0090] The foregoing has provided a detailed description of a method for preparing a thick copper printed circuit board for use in a new energy battery management system. Specific examples have been used to illustrate the principles and implementation methods of the invention. The descriptions of these embodiments are merely illustrative of the core ideas of the invention. It should be noted that those skilled in the art can make various improvements and modifications to the invention without departing from its principles, and these improvements and modifications also fall within the scope of protection of the claims.
Claims
1. A method for fabricating thick copper printed circuit boards used in new energy battery management systems, characterized in that, The method includes the following steps: S1. Select a thick copper double-sided board, which includes an FR4 substrate and a first base copper layer and a second base copper layer symmetrically disposed on both sides of the FR4 substrate. S2. After applying photosensitive dry film to both sides of the thick copper double-sided board, exposure, development, acid etching and film removal are performed. The first base copper layer is exposed to the entire surface to preserve the copper surface, and the second base copper layer is etched to form the circuit pattern. S3. Adhesive prepreg and copper foil layer are sequentially bonded to the surface of the second base copper layer and pressed at high temperature to make the adhesive prepreg fill the line spacing of the second base copper layer and cure. S4. Mechanical drilling and chemical degumming are performed on the products after high-temperature pressing. S5. Electroplating copper is deposited on the hole wall, the first base copper layer and the copper foil layer of the product obtained in step S4 to make the interlayer of the first base copper layer, the second base copper layer and the copper foil layer conductive. S6. Repeat the film application, exposure, development, etching and film removal operations of step S2 to process the circuit pattern on the first base copper layer, with only the copper-plated hole area remaining in the copper foil layer. S7. Set the milling machine's drilling depth to the thickness from the copper foil layer to the second base copper layer, and mill away the copper foil layer and its corresponding exposed metal hole area; S8. After the product obtained in step S7 has cured, the non-cured semi-cured sheet and the bare board FR4 are sequentially bonded to one side, and then pressed and fixed by a high-temperature press to obtain the final thick copper printed circuit board.
2. The preparation method according to claim 1, characterized in that, In step S1, the thickness of the first base copper layer and the second base copper layer is 2oz to 6oz.
3. The preparation method according to claim 1, characterized in that, In step S3, the pressing temperature of the prepreg is 170–200°C, the pressing pressure is 280–450 psi, and the pressing time is 60–120 minutes.
4. The preparation method according to claim 1, characterized in that, In step S3, the flowability of the prepreg is above 2.0 mm, and the resin content is 65% to 75%.
5. The preparation method according to claim 1, characterized in that, In step S4, chemical degumming is performed using either potassium permanganate degumming or plasma degumming.
6. The preparation method according to claim 1, characterized in that, In step S5, the electroplating current density for depositing electroplated copper is 1.5–3.0 A / dm², and the thickness of the electroplated copper layer is 20–35 μm.
7. The preparation method according to claim 1, characterized in that, In step S7, the control accuracy of the milling machine's drilling depth is ±0.05mm.
8. The preparation method according to claim 1, characterized in that, In step S8, the flowability of the non-flowing prepreg is 0.2-0.5 mm, and the resin content is 55%-65%.
9. The preparation method according to claim 1, characterized in that, In step S8, the lamination temperature of the non-flowing prepreg is 180–210°C, the lamination pressure is 300–450 psi, and the lamination time is 90–150 minutes.