Spin orbit torque magnetic memory and method of making
By using heavy metals and strong electron scattering dopants to form a composite film in the spin orbital moment magnetic memory, the spin orbital moment efficiency is enhanced, solving the problem of high power consumption in SOT-MRAM devices and achieving reduced device power consumption and compatibility of fabrication processes.
Patent Information
- Application Number
- CN202510628045.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-15
- Publication Date
- 2026-11-24
AI Technical Summary
Existing spin-orbit magnetic memory (SOT-MRAM) devices have high power consumption, and it is necessary to improve the SOT efficiency of spin source materials to reduce power consumption.
A spin source layer is formed by using heavy metal materials and strong electron scattering dopants to form a composite film. The spin orbital moment efficiency is enhanced through side-hopping and oblique scattering mechanisms, thereby reducing device power consumption.
It significantly improves spin-orbit moment efficiency, reduces device power consumption, and its fabrication process is compatible with CMOS and subsequent high-temperature processes, making it suitable for mass production.
Smart Images

Figure CN123164779A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of magnetic memory technology, and in particular to a spin orbital moment magnetic memory and its fabrication method. Background Technology
[0002] Spin-based magnetic memories possess advantages such as high speed, low power consumption, and non-volatility, and are expected to become one of the solutions to overcome the bottlenecks of the "post-Moore's Law" era in integrated circuits. Spin-orbit moment magnetic memories (SOT-MRAM) theoretically offer even lower power consumption, faster speeds, and longer lifespans, making them a potential next-generation magnetic memory solution. SOT-MRAM writes information by applying a horizontal current to the spin source material at the bottom of the magnetic tunnel junction (MTJ) memory cell, where the spin-orbit interaction is strong. This allows the spin source material to convert the charge flow into a spin current, changing the magnetization direction of the MTJ's free layer. One key to reducing the power consumption of SOT-MRAM is improving the SOT efficiency of the spin source material. Although materials such as W and Ta have relatively high SOT efficiencies compared to other metals, their use as spin source materials still results in relatively high power consumption in SOT-MRAM devices. Therefore, further improvements in the SOT efficiency of spin source materials are needed. Summary of the Invention
[0003] The spin-orbit-moment magnetic memory and its fabrication method provided by this invention can improve the efficiency of the spin-orbit-moment magnetic memory while reducing its power consumption.
[0004] In a first aspect, the present invention provides a spin-orbit magnetic memory, comprising:
[0005] Spin source layer, wherein the spin source layer comprises a composite film layer formed by combining heavy metal materials and strong electron scattering doping materials;
[0006] A storage bit is disposed on the spin source layer. The storage bit includes at least a free layer, a barrier layer and a reference layer formed sequentially, wherein the free layer is in contact with the spin source layer.
[0007] Optionally, the composite film layer includes a plurality of first film layers made of heavy metal materials and a plurality of second film layers made of strong electron scattering doped materials, wherein the first film layers and the second film layers are alternately stacked.
[0008] Optionally, the thickness of the spin source layer is 2–9 nm; wherein the thickness of the first film layer is 0.5–2 nm, and the thickness of the second film layer is 0.01–0.4 nm.
[0009] Optionally, the composite film is a composite film prepared by doping with heavy metal materials and the strong electron scattering doping material.
[0010] Optionally, the spin source layer further includes:
[0011] A strong electron scattering doped material film layer is formed by preparing a strong electron scattering doped material, and the strong electron scattering doped material film layer is disposed on the surface of the composite film layer near the memory bit.
[0012] Optionally, the spin source layer further includes:
[0013] A heavy metal film layer, which is prepared using heavy metal materials, is disposed on the surface of the composite film layer near the storage bit.
[0014] Optionally, the thickness of the spin source layer is 2–9 nm, and the mass ratio of the strong electron scattering dopant material in the composite film is 1%–30%.
[0015] Optionally, the spin source layer further includes a metal intercalation layer disposed on the surface of the composite film layer, and the metal intercalation layer is in contact with the free layer.
[0016] Optionally, the thickness of the metal intercalation layer is 0.2 to 2 nm.
[0017] In a second aspect, the present invention provides a method for fabricating a spin-orbit magnetic memory, used to fabricate a spin-orbit magnetic memory as described in any of the preceding claims, the method comprising:
[0018] A spin source layer is formed using heavy metal materials and strong electron scattering dopants, and storage bits are formed on the composite film layer.
[0019] Optionally, the formation of the spin source layer using heavy metal materials and strong electron scattering doped materials includes:
[0020] A composite film is formed by alternating deposition of heavy metal targets and strong electron scattering doped targets, resulting in alternating layers of a first film and a second film. The first film is formed of a heavy metal material, and the second film is formed of a strong electron scattering doped material. Alternatively...
[0021] A composite film layer was formed by dual-target co-sputtering deposition using heavy metal material targets and strong electron scattering doped material targets.
[0022] Optionally, the formation of the spin source layer using heavy metal materials and strong electron scattering doped materials includes:
[0023] After forming a composite film layer doped with heavy metal and strong electron scattering doped materials through dual-target co-sputtering deposition using both a heavy metal target and a strong electron scattering doped target, a heavy metal film layer is deposited on the composite film layer using a heavy metal target; or...
[0024] After forming a composite film layer by using a dual-target co-sputtering deposition of a heavy metal target and a strong electron scattering doped target, a strong electron scattering doped film layer is deposited on the composite film layer using a strong electron scattering doped target.
[0025] Optionally, the formation of the spin source layer using heavy metal materials and strong electron scattering doped materials includes:
[0026] After forming the composite film layer, a metal intercalation layer is formed on the composite film layer using a metal material.
[0027] In the technical solution provided by this invention, a spin source layer is formed using heavy metal materials and strong electron scattering dopants. In the spin source layer, the heavy metal material provides the spin effect, while the strong electron scattering dopants, which typically have a high dielectric constant, increase electron scattering in the heavy metal material. Through side-hopping and oblique scattering mechanisms, the efficiency of the heavy metal is enhanced, thereby significantly improving the spin-orbit moment efficiency and reducing device power consumption to some extent. The composition and thickness of the entire spin source layer are controllable and adjustable, meeting the requirements for 12-inch and smaller wafer sizes. Furthermore, the fabrication process has good compatibility with CMOS and subsequent high-temperature processes, making it suitable for large-scale mass production. Moreover, it eliminates the need for additional target materials in the material system construction, avoiding additional costs. Attached Figure Description
[0028] Figure 1 This is an exemplary structural diagram of a spin-orbit magnetic memory according to an embodiment of the present invention;
[0029] Figure 2 This is an exemplary structural diagram of a spin-orbit magnetic memory according to another embodiment of the present invention;
[0030] Figure 3 This is an exemplary structural diagram of a spin-orbit magnetic memory according to another embodiment of the present invention;
[0031] Figure 4 This is an exemplary structural diagram of a spin-orbit magnetic memory according to another embodiment of the present invention;
[0032] Figure 5 This is an exemplary structural diagram of a spin-orbit magnetic memory according to another embodiment of the present invention;
[0033] Figure 6This is an exemplary structural diagram of a spin-orbit magnetic memory according to another embodiment of the present invention;
[0034] Figure 7 This is a graph showing the effect of the content of strong electron scattering dopant material in the composite film layer of a spin-orbit magnetic memory on the SOT efficiency, according to another embodiment of the present invention.
[0035] Figure 8 This is a graph showing the relationship between the content of strong electron scattering dopant material in the composite film layer of a spin-orbit magnetic memory according to another embodiment of the present invention and the switching current density. Detailed Implementation
[0036] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0037] This invention provides a spin-orbit magnetic memory, such as... Figure 1 As shown, it includes:
[0038] Spin source layer, wherein the spin source layer comprises a composite film layer formed by combining heavy metal materials and strong electron scattering doping materials;
[0039] In some embodiments, the heavy metal material may be a metal-based material such as W, Pt, or Ta, and the strong electron scattering doping material may be an oxide, nitride, elemental metal, silicide, or carbide, such as MgO, SiO2, Si3N4, Cu, or WC.
[0040] A storage bit is disposed on the spin source layer. The storage bit includes at least a free layer, a barrier layer and a reference layer formed sequentially, wherein the free layer is in contact with the spin source layer.
[0041] In some embodiments, a memory bit typically includes a free layer, a barrier layer, and a reference layer. As a preferred embodiment, it may include a free layer, a barrier layer, a reference layer, a pinning layer, and a protective layer. The free layer and reference layer can be made of any one or more alloys of Co, Fe, Ni, B, and Pt, or multilayer films formed by combining the above elements or alloys with one or more of Co, Fe, Ni, Pt, Pd, Mo, W, Ir, Ta, Ru, Nb, and Hf. The barrier layer can be made of any one or more combinations of MgO, MgAl2O4, Al2O3, Gd2O3, and HfO2. The top view morphology of the memory bit includes, but is not limited to, circular, elliptical, and rectangular shapes.
[0042] In the technical solution provided by this invention, a spin source layer is formed using heavy metal materials and strong electron scattering dopants. In the spin source layer, the heavy metal material provides the spin effect, while the strong electron scattering dopants, which typically have a high dielectric constant, increase electron scattering in the heavy metal material. Through side-hopping and oblique scattering mechanisms, the efficiency of the heavy metal is enhanced, thereby significantly improving the spin-orbit moment efficiency and reducing device power consumption to some extent. The composition and thickness of the entire spin source layer are controllable and adjustable, meeting the requirements for 12-inch and smaller wafer sizes. Furthermore, the fabrication process has good compatibility with CMOS and subsequent high-temperature processes, making it suitable for large-scale mass production. Moreover, it eliminates the need for additional target materials to construct the material system, avoiding additional costs.
[0043] As an optional implementation method, such as Figure 1 and Figure 2 As shown, the composite film layer includes multiple first film layers made of heavy metal materials and multiple second film layers made of strong electron scattering doped materials, with the first film layers and the second film layers being stacked alternately.
[0044] In some embodiments, W is used as an exemplary heavy metal material, and MgO is used as an exemplary strong electron scattering dopant material. The two materials are alternately deposited using single-target magnetron sputtering to form a composite film layer with alternating layers of the first and second films. For example, as... Figure 1 As shown, the bottom and top layers of the W-MgO film system are both W layers. The thickness of each W layer can be the same or different. The thickness of each MgO layer can also be the same or different. For example, as... Figure 2As shown, the bottom layer of the W-MgO film system is W, and the top layer is MgO. The thickness of each W layer can be the same or different. The thickness of each MgO layer can also be the same or different. The foregoing provided two exemplary embodiments to illustrate the technical solution in this embodiment should be understood as follows: when the bottom layer is a heavy metal layer, the top layer can be a heavy metal layer or a strong electron scattering doped material layer; similarly, when the bottom layer is a strong electron scattering doped material layer, the top layer can be a heavy metal layer or a strong electron scattering doped material layer.
[0045] As an optional implementation, the thickness of the spin source layer is 2 to 9 nm; wherein the thickness of the first film layer is 0.5 to 2 nm, and the thickness of the second film layer is 0.01 to 0.4 nm.
[0046] In some embodiments, the total thickness of the spin source layer is 2–9 nm, preferably 3–6 nm. When the spin source layer is deposited alternately by single-target deposition of heavy metal material and strong electron scattering dopant material, the thickness of a single heavy metal layer is 0.5–2 nm, preferably 0.8–1 nm; the thickness of a single strong electron scattering dopant material layer is 0.01–0.4 nm, preferably 0.02–0.2 nm.
[0047] As an optional implementation, the composite film is a composite film prepared by doping with heavy metal materials and the strong electron scattering doping material.
[0048] In some embodiments, in addition to single-target alternating sputtering deposition, dual-target co-sputtering deposition can also be used to form a composite film prepared by a mixture. During the co-sputtering process, the proportion of strong electron scattering dopant is 1%-30%, preferably 2%-10%.
[0049] As an optional implementation method, such as Figure 3 As shown, the spin source layer further includes:
[0050] A strong electron scattering doped material film layer is formed by preparing a strong electron scattering doped material, and the strong electron scattering doped material film layer is disposed on the surface of the composite film layer near the memory bit.
[0051] In some embodiments, when forming a composite film using dual-target co-sputtering, a layer of strongly electron-scattering doped material can also be formed on the composite film.
[0052] As an optional implementation method, such as Figure 4 As shown, the spin source layer further includes:
[0053] A heavy metal film layer, which is prepared using heavy metal materials, is disposed on the surface of the composite film layer near the storage bit.
[0054] In some embodiments, when forming a composite film using dual-target co-sputtering, a heavy metal film layer can also be formed on the composite film layer.
[0055] As an optional implementation, the thickness of the spin source layer is 2-9 nm, and the mass ratio of the strong electron scattering dopant material in the composite film is 1%-30%.
[0056] In some embodiments, when a composite film is formed by dual-target co-sputtering, the total thickness of the composite film is 2-9 nm, preferably 3-6 nm, and the proportion of strong electron scattering dopant is 1%-30%, preferably 2%-10%.
[0057] As an optional implementation method, such as Figure 5 As shown, the spin source layer further includes a metal intercalation layer, which is disposed on the surface of the composite film layer and is in contact with the free layer.
[0058] In some embodiments, a metal intercalation layer, such as a tantalum layer, is inserted between the composite film and the free layer. The metal intercalation layer improves the interface and enhances the magnetic anisotropy of the free layer. It should be understood that, when a metal intercalation layer is present, the composite film can be formed by alternating single-target deposition or by dual-target co-sputtering deposition.
[0059] As an optional implementation, the thickness of the metal intercalation layer is 0.2 to 2 nm.
[0060] In the foregoing embodiments, the magnetic storage bits are all positioned above the spin source layer. It should be understood that alternative methods, such as..., can also be used. Figure 6 The bottom studded structure shown is an example. It should be understood that the use of a bottom studded structure is not limited to, for instance. Figure 6 The structures shown in the preceding embodiments can all be flipped up and down to form corresponding bottom studded structures.
[0061] like Figure 7 As shown, the curves illustrating the effect of the amount of strong electron scattering dopant in the spin source layer on the SOT efficiency are illustrated. Process 1 corresponds to the case where the first and second films are alternately stacked to form a composite film, while Process 2 corresponds to the case where a composite film is prepared using a mixture. According to... Figure 7It can be seen that, regardless of process one or process two, the SOT efficiency increases significantly with the increase of the strong electron scattering dopant content. Moreover, after exceeding 4%, it shows a slow downward trend. Therefore, it can be determined that when preparing composite films, the optimal doping concentration can be around 4% of the strong electron scattering dopant content.
[0062] like Figure 8 As shown, the effect of composite films formed with different doping concentrations on device power consumption is illustrated. Figure 8 In the diagram, the horizontal axis represents the external magnetic field strength, and the vertical axis represents the overturning current density, based on... Figure 8 It is known that when there is a strong electron scattering dopant in the spin source layer, the switching current density can be effectively reduced, and the switching current density will decrease significantly as the content of the strong electron scattering dopant increases.
[0063] This invention also provides a method for fabricating a spin-orbit magnetic memory, used to fabricate a spin-orbit magnetic memory as described in any of the preceding claims, the method comprising:
[0064] A spin source layer is formed using heavy metal materials and strong electron scattering dopants, and storage bits are formed on the composite film layer.
[0065] As an optional implementation, the method of forming a spin source layer using heavy metal materials and strong electron scattering doped materials includes:
[0066] A composite film is formed by alternating deposition of heavy metal targets and strong electron scattering doped targets, resulting in alternating layers of a first film and a second film. The first film is formed of a heavy metal material, and the second film is formed of a strong electron scattering doped material. Alternatively...
[0067] A composite film layer was formed by dual-target co-sputtering deposition using heavy metal material targets and strong electron scattering doped material targets.
[0068] As an optional implementation, the method of forming a spin source layer using heavy metal materials and strong electron scattering doped materials includes:
[0069] After forming a composite film layer doped with heavy metal and strong electron scattering doped materials through dual-target co-sputtering deposition using both a heavy metal target and a strong electron scattering doped target, a heavy metal film layer is deposited on the composite film layer using a heavy metal target; or...
[0070] After forming a composite film layer by using a dual-target co-sputtering deposition of a heavy metal target and a strong electron scattering doped target, a strong electron scattering doped film layer is deposited on the composite film layer using a strong electron scattering doped target.
[0071] As an optional implementation, the method of forming a spin source layer using heavy metal materials and strong electron scattering doped materials includes:
[0072] After forming the composite film layer, a metal intercalation layer is formed on the composite film layer using a metal material.
[0073] The above description is merely a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in the present invention should be included within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be determined by the scope of the claims.
Claims
1. A spin-orbit magnetic storage device, characterized in that, include: Spin source layer, wherein the spin source layer comprises a composite film layer formed by combining heavy metal materials and strong electron scattering doped materials; A storage bit is disposed on the spin source layer. The storage bit includes at least a free layer, a barrier layer and a reference layer formed sequentially, wherein the free layer is in contact with the spin source layer.
2. The spin-orbit magnetic storage device according to claim 1, characterized in that, The composite film layer includes multiple first film layers made of heavy metal materials and multiple second film layers made of strong electron scattering doped materials, with the first film layers and the second film layers being stacked alternately.
3. The spin-orbit magnetic storage device according to claim 2, characterized in that, The thickness of the spin source layer is 2–9 nm; wherein the thickness of the first film layer is 0.5–2 nm, and the thickness of the second film layer is 0.01–0.4 nm.
4. The spin-orbit magnetic storage device according to claim 1, characterized in that, The composite film is prepared by doping with heavy metal materials and the strong electron scattering doping material.
5. The spin-orbit magnetic storage device according to claim 4, characterized in that, The spin source layer further includes a strong electron scattering doped material film or a heavy metal film: wherein... The strong electron scattering doped material film is prepared using a strong electron scattering doped material, and the strong electron scattering doped material film is disposed on the surface of the composite film near the memory bit. The heavy metal film layer is prepared using heavy metal materials and is disposed on the surface of the composite film layer near the storage bit.
6. The spin-orbit magnetic storage device according to any one of claims 4-5, characterized in that, The thickness of the spin source layer is 2–9 nm, and the mass ratio of the strong electron scattering dopant material in the composite film is 1%–30%.
7. The spin-orbit magnetic storage device according to claim 2 or 4, characterized in that, The spin source layer further includes a metal intercalation layer, which is disposed on the surface of the composite film layer and is in contact with the free layer; the thickness of the metal intercalation layer is 0.2 to 2 nm.
8. A method for fabricating a spin-orbit magnetic memory, characterized in that, The method for preparing a spin-orbit magnetic memory as described in any one of claims 1-7 comprises: A spin source layer is formed using heavy metal materials and strong electron scattering dopants, and storage bits are formed on the composite film layer; wherein... The method of forming a spin source layer using heavy metal materials and strong electron scattering doped materials includes: A composite film is formed by alternating deposition of heavy metal targets and strong electron scattering doped targets, resulting in alternating layers of a first film and a second film. The first film is formed of a heavy metal material, and the second film is formed of a strong electron scattering doped material. Alternatively... A composite film layer was formed by dual-target co-sputtering deposition using heavy metal material targets and strong electron scattering doped material targets.
9. The method according to claim 8, characterized in that, The method of forming a spin source layer using heavy metal materials and strong electron scattering doped materials includes: After forming a composite film layer doped with heavy metal and strong electron scattering doped materials through dual-target co-sputtering deposition using both a heavy metal target and a strong electron scattering doped target, a heavy metal film layer is deposited on the composite film layer using a heavy metal target; or... After forming a composite film layer by using a dual-target co-sputtering deposition of a heavy metal target and a strong electron scattering doped target, a strong electron scattering doped film layer is deposited on the composite film layer using a strong electron scattering doped target.
10. The method according to claim 8, characterized in that, The method of forming a spin source layer using heavy metal materials and strong electron scattering doped materials includes: After forming the composite film layer, a metal intercalation layer is formed on the composite film layer using a metal material.