A memory and a method of forming the same
By retaining ineffective memory structures in the memory stack and forming through-hole isolation holes, the problems of morphological depression and residual conductive materials caused by layer-by-layer isolation are solved, thereby improving the insulation reliability and data read/write accuracy of the memory.
Patent Information
- Application Number
- CN202611380425.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-07
- Publication Date
- 2026-11-24
AI Technical Summary
In the prior art, due to the accumulation of morphological depressions and residual conductive materials caused by layer-by-layer isolation and dielectric backfilling, the connection structure of the memory is prone to internal electrical short circuits with the surrounding network, resulting in low data read/write accuracy and poor insulation reliability.
In the stacked structure of the memory, the ineffective memory structure is retained to maintain the material uniformity of the polished interface. After the stacked structure is formed, the ineffective memory structure is removed in one go to form a through isolation hole, which is filled with insulating dielectric material and a connection structure is formed to ensure that the connection structure is completely isolated by the insulating isolation structure.
It effectively avoids local over-polishing and recess inheritance during the chemical mechanical polishing process, eliminates the risk of short circuits caused by residual conductive materials, improves the insulation reliability of the memory, and ensures the accuracy of data reading and writing.
Smart Images

Figure CN123164780A_ABST
Abstract
Description
Technical Field
[0001] This application relates to semiconductor technology, and to, but is not limited to, a memory and a method of forming the same. Background Technology
[0002] To achieve high-density integration, memory typically employs a stacked structure containing multiple memory layers between the lower and upper conductive layers, with vertical interconnects facilitating signal interaction between the layers. To prevent contact between the interconnects and the densely packed bit lines or word lines within the stacked structure, related technologies often utilize a layer-by-layer isolation approach. This involves locally removing conductive material and backfilling with insulating dielectric material in a predetermined area of the interconnects during the fabrication of each bit line or word line layer. Subsequently, chemical mechanical polishing (CMP) is used to planarize the surface before proceeding to the fabrication stage of the next layer.
[0003] However, this layer-by-layer isolation and dielectric backfilling method is prone to defects. Due to the significant difference in physical properties between the backfilled insulating dielectric and the surrounding conductive and storage materials, inconsistent polishing rates in the CMP process can lead to over-polishing of the insulating filling area and the formation of local depressions. As multiple layers are stacked alternately, these local depressions are continuously inherited and amplified downwards during layer-by-layer film formation and polishing, resulting in severe unevenness in the height of the upper surface. This makes it impossible for subsequent processes to completely remove the conductive material film buried deep at the bottom of the depressions, thus forming microscopic conductive material residues inside the stacked structure. Finally, when fabricating the interconnect structure that runs through the stacked structure, the vertically grown metal channels are very likely to physically overlap with the conductive material residues in the depressions, causing an internal electrical short circuit between the interconnect structure and the surrounding wire mesh. This morphological accumulation defect induced by the layer-by-layer isolation process makes the insulating isolation structure highly susceptible to leakage or breakdown failure. Once a local short circuit occurs, it will cause severe crosstalk or data errors in the read and write signals, resulting in low data read and write accuracy of the memory and poor overall insulation reliability of the device. Summary of the Invention
[0004] This application provides a memory and a method for forming the same, which can improve the overall insulation reliability of the memory and effectively ensure the accuracy of data read and write operations.
[0005] The technical solution of this application embodiment is implemented as follows: This application provides a method for forming a memory, the method comprising: forming a stacked structure including multiple memory structure layers, wherein the stacked structure includes an effective memory structure for implementing memory functions and an ineffective memory structure located in a connection region; removing the ineffective memory structure to form an isolation hole penetrating the connection region; filling the isolation hole with an insulating dielectric material to form an insulating isolation structure; and forming a connection structure within the insulating isolation structure, the connection structure being used to realize an electrical connection between an upper conductive structure and a lower conductive structure.
[0006] In the above scheme, removing the ineffective storage structure to form an isolation hole through the connection area includes: forming an etch mask layer with a first opening on the stacked structure, the first opening exposing the connection area; using the etch mask layer as a barrier, performing through etching on the stacked structure along a first direction perpendicular to the surface of the stacked structure to remove the ineffective storage structure and form the isolation hole.
[0007] In the above scheme, forming a connection structure within the insulating isolation structure includes: forming a via mask layer with a second opening on the stacked structure and the insulating isolation structure, wherein the second opening exposes the central region of the insulating isolation structure, and the cross-sectional dimension of the second opening is smaller than the cross-sectional dimension of the insulating isolation structure; etching the insulating isolation structure using the via mask layer as a barrier to form a via groove inside the insulating isolation structure; wherein an unetched side edge of the insulating isolation structure forms a dielectric isolation layer, which is used to isolate the subsequently formed connection structure from the sidewall of the isolation hole; and filling the via groove with conductive material to form the connection structure.
[0008] In the above scheme, the stacked structure includes: multiple layers of bit lines and multiple layers of word lines alternately stacked in a first direction, and phase change memory cells disposed between the bit lines and the word lines; the effective memory structure includes: the bit lines, the word lines, and the phase change memory cells located outside the connection region; the ineffective memory structure includes: the bit lines, the word lines, and the phase change memory cells within the connection region; the bit lines and the word lines in the stacked structure are formed by the following operations: depositing a conductive material thin film; and patterning the conductive material thin film to form the bit lines or word lines that remain continuous within the connection region.
[0009] In the above scheme, the stacked structure includes at least a lower storage layer and an upper storage layer stacked sequentially in the first direction; the patterning process is implemented using photolithography, wherein the lower bit line mask and the lower word line mask used to define the lower storage layer, and the upper bit line mask and the upper word line mask used to define the upper storage layer, are all configured as periodic continuous pattern arrays without avoidance windows at the positions corresponding to the connection areas.
[0010] In the above scheme, the step of filling the isolation hole with insulating dielectric material to form an insulating isolation structure includes: using a deposition process to deposit the insulating dielectric material inside the isolation hole, so that the insulating dielectric material completely covers the storage structure layer exposed on the sidewall of the isolation hole and fills the isolation hole; and performing planarization treatment on the insulating dielectric material located outside the isolation hole until the top surface of the stacked structure is exposed, so that the top surface of the formed insulating isolation structure is flush with the top surface of the stacked structure.
[0011] In the above scheme, the stacked structure is formed on a substrate with peripheral logic circuits; the effective memory structure has an electrical interconnection structure connected to the peripheral logic circuits, so that the effective memory structure can be accessed by the peripheral logic circuits; the ineffective memory structure does not have an electrical interconnection structure connected to the peripheral logic circuits, so that the ineffective memory structure is in an electrically floating state.
[0012] In the above scheme, the lower conductive structure is the second-to-top metal structure located below the stacked structure, and the upper conductive structure is the top metal structure formed on the stacked structure; the connection structure is a top through hole that vertically penetrates the stacked structure, the bottom end of the top through hole is connected to the second-to-top metal structure, and the top end of the top through hole is connected to the top metal structure.
[0013] In the above scheme, the insulating dielectric material includes oxide materials.
[0014] This application provides a memory that is prepared using the memory formation method described above.
[0015] The above scheme has the following beneficial effects: In this embodiment, during the fabrication of a stacked structure comprising multiple memory layers, ineffective memory structures are retained in the connection area. After the stacked structure is fully formed, the ineffective memory structures are removed in one step to form through-hole isolation holes and insulating isolation structures, thereby forming vertical connection structures within these insulating isolation structures. This process mechanism maintains the material uniformity of the polished interface by retaining homogeneous ineffective memory structures, effectively avoiding the accumulation of morphological depressions caused by traditional layer-by-layer isolation backfilling, and thus eliminating the risk of conductive material residue. Simultaneously, the through-hole connection structures are completely wrapped and isolated by the insulating isolation structures, directly cutting off the path for physical overlap between the connection structures and surrounding wires, thereby effectively solving the problem that the connection structures are prone to internal electrical short circuits with surrounding wires. This not only significantly improves the overall insulation reliability of the device but also effectively ensures the data read / write accuracy of the memory. Attached Figure Description
[0016] Figure 1 This is a schematic diagram illustrating the process evolution and defect mechanism of memory during the fabrication of interconnect structures in related technologies. Figure 2 This is a schematic flowchart of a method for forming a memory according to an embodiment of this application; Figure 3 This is a comparative schematic diagram of the mask pattern and layout design provided in the embodiments of this application; Figure 4A This is a schematic diagram comparing the process evolution provided in the embodiments of this application; Figure 4B This is a cross-sectional schematic diagram of the memory during the formation of isolation holes according to an embodiment of this application; Figure 4C This is a cross-sectional schematic diagram of the memory provided in the embodiments of this application during the stage of completing insulation isolation and forming the final connection structure. Detailed Implementation
[0017] To make the objectives, technical solutions, and advantages of this application clearer, the application will be further described in detail below with reference to the accompanying drawings. The described embodiments should not be regarded as limitations on this application. All other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0018] In the accompanying drawings, for clarity, the dimensions of layers, areas, and elements, as well as their relative dimensions, may be exaggerated. The same reference numerals denote the same elements throughout.
[0019] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of the embodiments of this application, the first element, component, area, layer, or portion discussed below may be referred to as a second element, component, area, layer, or portion. And when a second element, component, area, layer, or portion is discussed, it does not indicate that the embodiments of this application necessarily contain a first element, component, area, layer, or portion.
[0020] Spatial relation terms such as “below,” “under,” “below,” “below,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below” or “below” other elements or features will be oriented “above” other elements or features. Therefore, the exemplary terms “below” and “under” can include both upper and lower orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.
[0021] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the embodiments of this application. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “compose” and / or “comprising,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.
[0022] To fully understand the embodiments of this application, detailed steps and structures will be presented in the following description to illustrate the technical solutions of the embodiments of this application. Preferred embodiments of this application are described in detail below; however, in addition to these detailed descriptions, the embodiments of this application may have other implementation methods.
[0023] To meet the demands of high-capacity data storage, memory typically employs a stacked structure comprising multiple storage layers to achieve high-density integration. In this type of memory architecture, the stacked structure is usually positioned between the lower and upper conductive layers. To enable signal interaction between the upper and lower conductive layers, a vertical connection structure needs to be formed through the stacked structure.
[0024] Because the stacked structure contains densely packed conductive bit lines and word lines, to prevent the vertically penetrating connection structure from physically contacting these bit lines or word lines, the manufacturing process of related technologies mainly employs a layer-by-layer isolation method. For example, Figure 1 This is a schematic diagram illustrating the process evolution and defect mechanism of memory interconnection structures in related technologies. For example... Figure 1 As shown in the attached diagram, from top to bottom, the cross-sectional views of the memory at the lower bit line (BF) fabrication stage, the lower word line (BC) fabrication stage, the upper word line (TF) fabrication stage, and the upper bit line (TC) fabrication stage. In the fabrication process of related technologies, each bit line or word line, i.e. Figure 1 During fabrication, the conductive cross-sections that extend horizontally or are arranged periodically at the microscopic level are all placed within a pre-defined region to accommodate the connection structure (such as a top-layer via). Figure 1 Within the central area indicated by the dashed circle, an additional cutting layer window pattern is created to locally remove the conductive material from that area. Subsequently, insulating dielectric materials such as oxides are backfilled into the window locations, and the surface is planarized using a chemical mechanical polishing process to prepare for the next preparation stage.
[0025] However, in actual device fabrication, this layer-by-layer isolation and dielectric backfilling method can introduce some defects. (See also...) Figure 1 Because the insulating dielectric material filling the windowed area has significantly different physical properties from the surrounding bit lines, word lines, and memory devices, the grinding rates at the interfaces of these different materials during chemical mechanical polishing are inconsistent. This difference in grinding rate can cause over-polishing of the areas filled with insulating dielectric material, resulting in localized depressions on the surface of the insulating dielectric.
[0026] like Figure 1As shown by the solid arrow, the cross-stage evolution process involves the alternating fabrication and stacking of lower word lines (BC), upper word lines (TF), and upper bit lines (TC). Local depressions are inherited and amplified downwards during layer-by-layer film deposition and polishing, resulting in severe unevenness in the height of the upper surface. When conductive material films for forming subsequent bit lines or word lines are deposited on surfaces with deep pits, subsequent planarization or etching steps cannot completely remove the conductive material buried deep within the pits, thus creating microscopic conductive material residues within the stacked structure.
[0027] Ultimately, as Figure 1 As shown in the bottom structural state, during the fabrication of the connection structure (such as the top-layer via TV and metal TM) that runs through the entire stacked structure, the vertically grown metal channels are prone to physical contact with the conductive material remaining in the pits, causing an internal electrical short circuit between the connection structure and the surrounding network. This morphological accumulation defect induced by the layer-by-layer isolation process makes the resulting insulation structure highly susceptible to leakage or breakdown failure. Once a local short circuit occurs, it will cause severe crosstalk or data errors in the read / write signals of the corresponding memory area, resulting in low data read / write accuracy of the memory and poor overall insulation reliability of the device.
[0028] To address the problem in related technologies where the accumulation of morphological depressions and residual conductive materials caused by layer-by-layer isolation and dielectric backfilling leads to internal electrical short circuits between vertical connection structures and surrounding wire meshes, resulting in low data read / write accuracy and poor overall insulation reliability of the memory, this application provides a method for forming a memory. This method, during the fabrication of a stacked structure containing multiple memory structure layers, completely preserves non-functional memory structures in the connection area to maintain material uniformity at the polishing interface. After the stacked structure is formed, non-functional memory structures are removed in one step to form through-hole isolation holes. Insulating dielectric material is then backfilled into these isolation holes to form the connection structure. This ensures that the through-hole connection structure is completely isolated by the insulating isolation structure, effectively avoiding localized over-polishing and depression inheritance during the chemical mechanical polishing process. This eliminates the risk of short circuits caused by residual conductive materials in the pits, thereby eliminating leakage and breakdown hazards in the internal wire meshes, improving the overall insulation reliability of the memory, and effectively ensuring the data read / write accuracy of the memory.
[0029] Figure 2 This is a schematic flowchart illustrating a method for forming a memory according to an embodiment of this application. Figure 2 As shown, the method for forming the memory includes steps 101 to 104: Step 101: Form a stacked structure comprising multiple storage structure layers, wherein the stacked structure includes effective storage structures for implementing storage functions and ineffective storage structures located in the connection area.
[0030] Here, a stacked structure refers to a three-dimensional array physical entity formed on a semiconductor substrate through multiple alternating film deposition processes to increase storage density in vertical space. This stacked structure is formed entirely on top of a lower conductive structure. Each memory structure layer constituting the stacked structure refers to the basic hierarchical unit of the three-dimensional memory array, which typically contains conductive networks for transmitting electrical signals, such as crisscrossing bit lines and word lines, as well as memory cells located at the network intersections, such as phase-change memory cells and resistive switching memory cells.
[0031] The connection area refers to a specific physical region in the overall spatial layout of the chip layout that is pre-planned for subsequent accommodation of vertical conductive channels (i.e., vias) that run through the stacked structure.
[0032] To achieve high-density integration of the memory array and ensure the structural stability of the manufacturing process, this embodiment of the application simultaneously forms effective and ineffective memory structures at the same horizontal level during the formation of the stacked structure. The effective memory structure is distributed in the main array area outside the connection region, possessing corresponding electrical interconnect structures, and serves as the core functional area responsible for implementing actual data read / write and storage functions. The ineffective memory structure (dummy structure) is distributed inside the connection region. In actual semiconductor manufacturing, this ineffective memory structure is electrically suspended or inaccessible, does not participate in the actual circuit operation, and only serves as a supporting entity in the process to maintain the consistency of the microstructure density.
[0033] In some embodiments, the stacked structure is formed on a substrate with peripheral logic circuitry; the effective memory structure has an electrical interconnection structure connected to the peripheral logic circuitry, so that the effective memory structure can be accessed by the peripheral logic circuitry; the ineffective memory structure does not have an electrical interconnection structure connected to the peripheral logic circuitry, so that the ineffective memory structure is electrically suspended.
[0034] It should be noted that the substrate, typically a silicon (Si) substrate, serves as the physical platform for the three-dimensional stacked structure formed above. The peripheral logic circuitry is usually a complementary metal-oxide-semiconductor (CMOS) control circuit integrated on or within this substrate. For the active memory structures within the main array region, a complete electrical interconnect structure is provided during manufacturing (this should be distinguished from the subsequent connection structures that run through the stack; these electrical interconnect structures are typically peripheral plugs or metal pins around the array perimeter). These electrical interconnect structures electrically connect the conductive nets within the active memory structures to the peripheral logic circuitry at the bottom. Conversely, for inactive memory structures located within the connection regions, the layout routing intentionally cuts off any signal paths to the peripheral logic circuitry and external power supply. This electrically floating state ensures that the inactive memory structures remain electrically inert during chip operation. During the semiconductor device's operating cycle, this suspended state ensures that the non-active memory structure is in a zero potential gradient, which not only prevents capacitive coupling or electromagnetic crosstalk to adjacent active signal networks, but also avoids leakage power consumption of parasitic paths, thus stably undertaking the process support role.
[0035] In some embodiments, the stacked structure includes: multiple layers of bit lines and multiple layers of word lines alternately stacked in a first direction, and phase-change memory cells disposed between the bit lines and word lines; the effective memory structure includes: the bit lines, word lines and phase-change memory cells located outside the connection region; the ineffective memory structure includes: the bit lines, word lines and phase-change memory cells within the connection region. In this case, the bit lines and word lines in the stacked structure mentioned above can be formed by the following operations: first, depositing a conductive material film; then, patterning the conductive material film to form bit lines or word lines that remain continuous in the connection area.
[0036] Here, the first direction usually refers to the main depth direction perpendicular to the surface of the semiconductor substrate, i.e., the Z-axis direction. In a three-dimensional cross-point memory architecture, multiple layers of bit lines and word lines are orthogonally arranged on a horizontal plane to construct a high-density addressing matrix, while phase-change memory cells (such as stacked core nodes containing phase-change materials such as chalcogenide glass) are precisely sandwiched and embedded at the orthogonal intersections of adjacent bit lines and word lines on the upper and lower layers, forming the basic memory device.
[0037] More specifically, in this embodiment, a thin film of conductive materials such as tungsten or copper is first deposited on the entire wafer surface using techniques such as physical vapor deposition (PVD) or chemical vapor deposition (CVD). Subsequently, the conductive material film is patterned using lithography and dry etching processes to create elongated, strip-shaped conductive lines. It should be noted that in related technologies, to avoid subsequent vertical vias, etching is typically performed intentionally within the connection area during patterning, cutting off the conductive film in that area and backfilling it with insulating material. However, in this embodiment, the conductive material and phase change material within the connection area are deliberately not etched off during patterning; instead, their original patterns are preserved, allowing the etched bit lines or word lines to completely and continuously traverse and pass through the entire connection area. By preserving continuous conductive lines and phase change material within the connection area, this application maintains a uniform pattern density across the entire wafer surface. This continuous interface, composed of homogeneous materials, exhibits highly consistent physical hardness and reactivity with chemical polishing slurries. Therefore, during subsequent chemical mechanical polishing (CMP), the polishing pad experiences uniform stress across the entire wafer surface, maintaining a highly uniform polishing rate.
[0038] By forming and retaining continuous conductive lines and phase change materials within the interconnect regions, this application constructs a uniform homogeneous interface at the physical level of semiconductor fabrication. Specifically, the wafer surface maintains a uniform pattern density globally (including the main array region and the interconnect regions). This continuous interface, composed of a network of single-property materials, exhibits highly consistent hardness, elastic modulus, and reactivity with chemical polishing slurries across all regions. Therefore, during subsequent multi-layer alternating chemical mechanical polishing (CMP), the polishing pad experiences uniform force across the entire wafer surface, maintaining a highly uniform polishing rate. This inherent physical uniformity enables planarization of each layer, completely blocking the physical path of downward inheritance and amplification of microstructure depressions between layers.
[0039] In some embodiments, the stacked structure includes at least a lower storage layer and an upper storage layer stacked sequentially in a first direction; the patterning process described above is implemented using photolithography, wherein the lower bit line mask and the lower word line mask used to define the lower storage layer, and the upper bit line mask and the upper word line mask used to define the upper storage layer, are all configured as periodic continuous pattern arrays without avoidance windows at positions corresponding to the connection regions.
[0040] Here, the bottom cell and top cell constitute a typical two-layer (2-Stack) or multi-layer three-dimensional memory architecture. In this architecture, the bottom cell consists of a bottom bit line layer and a word line layer sandwiching phase-change units; the top cell is formed by stacking on top of the bottom cell, and is also composed of a top word line layer and a bit line layer sandwiching corresponding phase-change units.
[0041] In semiconductor manufacturing, the patterning of each of the above layers is highly dependent on photolithography. Typically, each conductive network layer requires an independent photomask for pattern transfer. More specifically, fabricating the above structure requires sequentially using a lower bit line mask to define the lower memory layer bit lines (e.g., BF layer), a lower word line mask to define the lower memory layer word lines (e.g., BC layer), an upper word line mask to define the upper memory layer word lines (e.g., TF layer), and an upper bit line mask to define the upper memory layer bit lines (e.g., TC layer).
[0042] It should be noted that, in the mask layout design of this application, a strategy is adopted in which periodic continuous pattern arrays without cut-out windows are configured at the positions corresponding to the connection areas. In the layout design of the previous related technologies, due to the need to reserve the position of vertical vias, the above-mentioned multilayer masks rigidly embedded local cut-out window patterns in the areas corresponding to the via projections. This approach of interrupting the array continuity will result in a large number of non-periodic and irregular geometric patterns on the layout, which will easily cause severe optical proximity effect (OPE) during the photolithography process and cause local micro-loading effect during the etching stage, ultimately resulting in an extremely high process defect rate in this area. In this embodiment, the design logic regarding via avoidance and isolation in the above-mentioned mask layers is completely removed. That is, the graphic arrangement of the lower bit line mask, lower word line mask, upper word line mask and upper bit line mask in the connection area is consistent with the graphic arrangement of the external main array area, that is, it presents a globally uninterrupted periodic continuous graphic array.
[0043] To more clearly illustrate the process advantages brought about by the above-mentioned mask configuration, a comparative schematic diagram of the mask pattern and layout design of the embodiments of this application is introduced here, namely... Figure 3 Please provide an explanation. For example... Figure 3In the original design logic shown on the left, each layer of the stacked structure relies heavily on independent photomasks for pattern transfer. During the initial layout design, to reserve via locations, multiple array masks 301 for both the lower and upper memory layers need to embed local cut-layer patterns. This disruption of array continuity results in numerous non-periodic, irregular geometric edges on the array masks 301, easily leading to severe optical proximity effects (OPE) and semiconductor process defects. Furthermore, as... Figure 3 As shown in the dynamic changes on the left, if the physical position of the via needs to be changed due to product specification upgrades (i.e., a redesign occurs), the deep coupling design, where the via avoidance area is bound to the underlying array, will render the original array mask 301 unusable. A completely new array mask 302 with a shifted notch position must be designed and manufactured. This means that up to four array masks must be simultaneously re-opened, resulting in high redesign costs.
[0044] And refer to Figure 3 The improved design logic shown on the right eliminates the via avoidance and isolation design logic in each layer of the mask. The pattern arrangement of the lower bit line mask, lower word line mask, upper word line mask, and upper bit line mask (collectively referred to as array mask 303) in the connection area is consistent with the pattern arrangement of the external main array area, that is, it presents an uninterrupted periodic continuous pattern array. This completely regular design of the mask pattern maintains the spatial periodicity of the lithographic pattern and the global consistency of the pattern density, eliminating optical distortion caused by irregular pattern edges from the root.
[0045] This fully regularized design of the photomask pattern offers several significant advantages in terms of process principle: First, it maintains the spatial periodicity and global density consistency of the photomask pattern, eliminating optical distortion caused by irregular edges of the pattern from a physical perspective, and significantly reducing the defect rate in photolithography and etching processes. Second, it decouples the layout data of the underlying basic memory structure and the via isolation structure, simplifying the logic algorithm for generating the photomask pattern and the computational complexity of Design Rule Check (DRC). Third, when the chip is subsequently modified (such as changing the position of the top-level via), it is not necessary to modify the underlying array photomask simultaneously; only the single photomask dedicated to subsequent via etching needs to be modified, greatly improving the flexibility of process iteration and saving manufacturing costs.
[0046] For example, Figure 4A This is a schematic diagram comparing the process evolution provided in the embodiments of this application. Figure 4AThe four dashed outlines, from top to bottom, define the microscopic cross-sectional states of the stacked structure at the lower bit line layer fabrication stage, the lower word line layer fabrication stage, the upper word line layer fabrication stage, and the upper bit line layer fabrication stage, respectively. Within the dashed outline of each process stage, the left half shows the process evolution state in related technologies, and the right half shows the process evolution state of the embodiment of this application. First, for the embodiment of this application (i.e. Figure 4A The mask configuration (right half) will be described. Within the dashed box of each stage, the elongated grid-like structure floating directly above the wafer solid structure schematically represents the array mask 403 used for patterning processing in that stage. It can be clearly seen that the array mask 403 used in this embodiment is configured with periodic, continuous patterns without avoidance windows at positions corresponding to the central connection region. Thanks to the continuous exposure transfer of the array mask 403, as described above... Figure 4A As shown in the cross-section of the wafer on the right, a stacked structure 402 is formed by progressively alternating film deposition on top of the lower conductive structure 401. This stacked structure 402 contains multiple memory structure layers 4021. Within the predetermined central connection region, due to the lack of avoidance windowing during photolithography, the ineffective memory structure 4022, composed of multiple homogeneous materials, is fully preserved; simultaneously, an effective memory structure 4023 is naturally formed around the central connection region. Figure 4A A direct comparison of the left and right sides reveals the advantages of this embodiment: In the process of the related technology on the left, the central notch in the mask causes the central area to be etched away after each film deposition, resulting in severe CMP polishing depressions. These depressions (as shown by the dark black lines on the left) are inherited and amplified downwards with the increase in the number of stacked layers. In contrast, the process of this embodiment on the right retains the non-disconnected ineffective storage structure 4022 throughout the entire central connection area. This ensures that the stacked structure 402 maintains a continuous surface composed of homogeneous materials (such as metal layers or phase change material layers) at each planarization stage of vertical fabrication. This design based on physical material uniformity fundamentally eliminates the polishing rate difference caused by heterogeneous materials during chemical mechanical polishing (CMP), avoids local over-polishing, achieves extremely high interlayer flatness of the stacked structure 402, and completely cuts off the physical path of downward inheritance and amplification of depression defects.
[0047] Step 102: Remove non-valid storage structures to form isolation holes that penetrate the connection area.
[0048] Here, removing ineffective memory structures refers to the physical removal process used to peel off and remove ineffective memory structures located in the connection areas after the overall alternating molding of all memory structure layers within the stacked structure has been completed. For example, anisotropic dry etching processes (such as reactive ion etching, RIE) can be used, utilizing the highly directional bombardment characteristics of the etching gas to penetrate the multi-layered structure from top to bottom. Isolation vias refer to deep channels that physically cut through the stacked structure longitudinally, exposing the internal material of the sidewalls.
[0049] In some embodiments, removing invalid memory structures to form isolation holes through the connection area can be achieved by first forming an etch mask layer with a first opening on the stacked structure, the first opening exposing the connection area; then, using the etch mask layer as a barrier, through etching is performed on the stacked structure along a first direction perpendicular to the surface of the stacked structure to remove invalid memory structures and form isolation holes.
[0050] It should be noted that an etching mask layer can be a material layer used to protect non-target areas in a semiconductor etching process, such as a specific photoresist layer or hard mask layer, which possesses good etching resistance properties. See also... Figure 3 Since the underlying multi-layer array mask 303 no longer serves the function of avoiding vias, this embodiment introduces a separate mask (TV Cut Mask, e.g.) specifically for defining the via isolation area. Figure 3 The first via mask 304 (to the left of the middle arrow) serves as the etching mask layer. The size and shape of this first opening strictly correspond to the pre-planned connection area. The first direction is perpendicular to the main depth direction of the semiconductor substrate. Through etching along the first direction, a one-time through-hole etching of the multilayer stacked structure can be achieved. It is worth noting that, since this is a one-time large-area macroscopic through-hole removal process, the size of the first opening is significantly larger than the microscopic linewidth inside the array, thus the limit requirement for the resolution of the lithography machine is relatively low. The patterning of the first via mask 304 can be achieved using conventional lithography precision equipment such as dry argon fluoride (Dry ArF), which effectively optimizes the manufacturing cost structure while ensuring process reliability.
[0051] The first opening is a patterned transparent area formed on the aforementioned etched mask layer through an exposure and development process. The size and shape of the first opening strictly correspond to the horizontal cross-section of the pre-planned connection area. Its function is to precisely expose the connection area that needs to be hollowed out during the process, while using the surrounding unopened mask material to tightly shield and protect the effective storage structure in the array body area.
[0052] In the embodiments of this application, the first direction refers to the main depth direction perpendicular to the semiconductor substrate, such as the Z-axis direction.
[0053] Through-etching refers to a continuous etching process with high depth and anisotropy, performed on multilayered heterogeneous material systems in semiconductor manufacturing. Specifically, since the stacked structure of this application consists of multiple layers of materials with different physical properties (such as conductive metals, phase-change memory materials, etc.) stacked alternately, through-etching can employ dry plasma etching (such as reactive ion etching, which involves strong physical bombardment). During the etching process, using the first opening as a gas channel, the plasma continuously cuts through all metal and dielectric layers from top to bottom along a first direction without stopping or reapplying a new mask, until the entire multilayer structure in the exposed area is penetrated in one go.
[0054] For example, the process of forming isolation holes described above will be further illustrated by comparison with the cross-sectional view. Figure 4B This is a cross-sectional schematic diagram of the memory provided in the embodiment of this application during the stage of forming isolation holes. Figure 4B Within the dashed box, the left half illustrates the severe depressions and residual state caused by layer-by-layer hollowing in related technologies at this stage; the right half illustrates the physical state of a single through-etching operation performed in the embodiment of this application. For example... Figure 4B As shown on the right, after the complete stacked structure 402 is formed, the aforementioned etching mask layer (not shown in the figure) is deposited and patterned on its upper surface. The connection region is precisely exposed through a first opening in this etching mask layer; subsequently, using the etching mask layer as a strong barrier, a through-hole dry etching process is performed along the first direction. This etching process utilizes a high-selectivity plasma to physically cut and remove all non-functional memory structures 4022 (including multilayer metal lines and phase change units) within the connection region in a single top-to-bottom motion, thereby forming an isolation via 405 inside the stacked structure 402 that penetrates all memory structure layers, has a high aspect ratio, and flat sidewalls. (Comparison...) Figure 4B As can be clearly seen from the left and right sides, this embodiment of the application, by first maintaining flatness and then focusing on cutting through, completely eliminates the residual defects inside the channel.
[0055] By using a single etch mask layer with a first opening after the stacked structure has been formed as a whole, such as Figure 3 The scheme of performing a one-time vertical through-etch on the first via mask 304 in the process combines the local windowing actions scattered in various single-layer film deposition stages in related technologies. This process strategy of first planarizing the whole and then centrally opening the vias simplifies the originally deeply coupled N-layer layout into an orthogonal decoupled architecture of a bottom regular array plus a one-through mask. Continuing as... Figure 3As indicated by the revised arrow on the right, if the position or number of the top-layer vias needs to be changed due to product specification upgrades, since the bottom array mask 303 is arranged continuously and regularly globally, its pattern does not need to be altered and can be directly reused; only a second via mask 305 with a shifted window position needs to be designed and manufactured separately to replace the original first via mask 304. Furthermore, as... Figure 3 As shown in the independent mask 306 on the right, even in a conventional process that does not require relocation, the only process increment in this embodiment compared to related technologies is the addition of a low-precision independent mask 306 (i.e., the aforementioned via etching mask) at the end. This layout decoupling design not only shortens the iteration cycle of design verification but also avoids the risk of regenerating the underlying array mask, thereby reducing the cost of mask relocation.
[0056] Step 103: Fill the isolation hole with insulating dielectric material to form an insulating isolation structure.
[0057] Here, insulating dielectric material refers to a filling medium with excellent electrical insulation properties, used to construct a physical barrier in three-dimensional space to block current conduction.
[0058] In some embodiments, the insulating medium includes an oxide material.
[0059] It should be noted that the oxide material can be, for example, silicon dioxide (SiO2) or doped silicon oxides (such as fluorosilicone glass FSG, phosphosilicate glass PSG, etc.). Oxide materials are used as the filling material inside the isolation vias for two reasons. First, oxide materials possess extremely high dielectric strength and excellent intrinsic insulation properties, effectively blocking leakage paths between cut metal wire meshes in high-density stacked structures and preventing internal electrical breakdown. Second, oxide materials exhibit uniform flowability and step coverage in the aforementioned chemical vapor deposition (CVD) process, and demonstrate stable and controllable etching selectivity in subsequent chemical mechanical polishing (CMP) and through-hole dry etching processes. These material properties allow for good process compatibility with surrounding conductive metals and phase change materials, thereby ensuring that the insulating isolation structure maintains extremely high physical morphological stability throughout the demanding semiconductor manufacturing process.
[0060] In some embodiments, an insulating dielectric material is filled into the isolation hole to form an insulating isolation structure. Specifically, an insulating dielectric material can be deposited inside the isolation hole using a deposition process, so that the insulating dielectric material completely covers the storage structure layer exposed on the sidewall of the isolation hole and fills the isolation hole. Then, the insulating dielectric material located outside the isolation hole is planarized until the top surface of the stacked structure is exposed, so that the top surface of the formed insulating isolation structure is flush with the top surface of the stacked structure.
[0061] The deposition process employed here can include high-density plasma-chemical vapor deposition (HDP-CVD) or atomic layer deposition (ALD), which have good step coverage capabilities, to ensure that the isolation vias with high aspect ratios are densely filled without internal void defects. During deposition, the insulating dielectric material fills the isolation via from bottom to top and conformally covers the memory structure layers (including the conductive end faces of multilayer bit lines and word lines) exposed by the previous through-etching on the sidewalls of the isolation via, thereby directly constructing a physical and electrical isolation barrier around the exposed conductive end faces.
[0062] When performing the above deposition process to ensure that the isolation holes are completely filled, the insulating dielectric material is often in an over-deposited state, causing some insulating dielectric material to overflow and cover the top surface of the stacked structure outside the isolation holes. The above planarization process can be performed using chemical mechanical polishing (CMP) or dry etch-back process to remove the excess insulating dielectric material located outside the isolation holes. The planarization process is precisely controlled at the top surface of the stacked structure, that is, the surface of the topmost dielectric layer or conductive layer of the stacked structure is used as the grinding stop layer.
[0063] Step 104: Form a connection structure within the insulating isolation structure. The connection structure is used to realize the electrical connection between the upper conductive structure and the lower conductive structure.
[0064] Here, the upper conductive structure and the lower conductive structure refer to the global or local conductive paths located above and below the stacked structure, used for transmitting electrical signals within the chip. Specifically, the lower conductive structure can be the bottom-level interconnect wiring pre-formed in the front-end processes of chip manufacturing, while the upper conductive structure can be the top signal traces formed on the entire stacked structure. The two work together to achieve signal interaction between the memory array and external control circuitry. The connection structure refers to a vertical conductive channel made of low-resistivity conductive material, such as conductive plugs. As a physical bridge spanning three dimensions, it is used to penetrate the stacked structure, directly connecting the upper and lower conductive structures vertically, thereby constructing a complete signal transmission closed loop.
[0065] In some embodiments, the lower conductive structure is a subtop metal structure located below the stacked structure, and the upper conductive structure is a top metal structure formed on the stacked structure; the connection structure is a top through-hole that vertically penetrates the stacked structure, with the bottom end of the top through-hole connected to the subtop metal structure and the top end of the top through-hole connected to the top metal structure.
[0066] The second-to-top metal structure, such as the common M(n-1) layer, is typically a metal wiring layer pre-formed during the front-end semiconductor manufacturing process, located below the memory array. It connects downwards to the peripheral logic control circuitry in the substrate. The top metal structure, formed at the top of the entire stack, is the global signal routing layer or power distribution network deployed after the memory array is manufactured. Top vias, acting as conductive bridges spanning the entire physical thickness of the memory device, physically penetrate the aforementioned insulating structure. Through direct physical contact between their bottom and the second-to-top metal structure, and between their top and top metal structures, they vertically connect the two, thus linking the signal transmission and data addressing paths between the peripheral logic circuitry and the top metal.
[0067] In some embodiments, a connection structure is formed within an insulating isolation structure. Specifically, a via mask layer with a second opening is formed on top of the stacked structure and the insulating isolation structure. The second opening exposes the central region of the insulating isolation structure, and the cross-sectional dimension of the second opening is smaller than the cross-sectional dimension of the insulating isolation structure. Then, the insulating isolation structure is etched using the via mask layer as a barrier to form a via groove inside the insulating isolation structure. A dielectric isolation layer is formed on the unetched side edges of the insulating isolation structure to isolate the subsequently formed connection structure from the sidewalls of the isolation hole. Finally, conductive material is filled into the via groove to form the connection structure.
[0068] It should be noted that a via mask layer is a patterned mask material used in semiconductor photolithography to define the location of the final actual conductive channels (e.g., vias). It can be a composite mask system composed of photoresist, an anti-reflective coating, and a hard mask layer (such as an amorphous carbon layer or a silicon oxynitride layer). The second opening is a transparent area opened on this via mask layer through an exposure and development process. In actual device fabrication, using a high-precision photolithography overlay process, this second opening is precisely aligned, thereby exposing the central region of the insulating isolation structure.
[0069] In this embodiment, the cross-sectional dimension of the second opening is smaller than that of the insulating isolation structure. This means that in the semiconductor manufacturing process, the perimeter or outer diameter of the via to be etched subsequently is intentionally designed to be strictly smaller than the outer diameter of the insulating isolation structure formed in the preceding step. This dimensional difference can be understood as a reserved lithographic safety margin, thereby ensuring, from a physical geometry perspective, that the effective range of the etching gas is forcibly limited to the internal core area of the insulating isolation structure, thus preventing it from touching the external boundary of the insulating isolation structure. Simultaneously, due to the objective existence of slight overlay shifts in modern high-precision lithography machines during layer-to-layer overlay alignment, this application provides ample process tolerance for lithographic alignment by reserving the aforementioned cross-sectional dimension difference. Even if the second opening slightly shifts relative to the physical center of the insulating isolation structure during actual exposure, as long as the shift does not exceed the preset safety margin, the etching drilling process will still be confined within the insulating isolation entity, thereby avoiding penetration of the outer insulating barrier and thus providing the device with extremely high manufacturing resilience at the micro-process level.
[0070] Through-holes are deep channels hollowed out inside insulating structures. When etching insulating structures, anisotropic dry plasma etching processes with high etching selectivity for the insulating dielectric material (such as silicon oxide or silicon nitride) are typically used to ensure that the hole walls have extremely high verticality.
[0071] The dielectric isolation layer is an insulating entity created by the aforementioned difference in cross-sectional dimensions. Because the opening of the second etching is strictly confined to the central region of the insulating isolation structure, the periphery of the insulating isolation structure, i.e., the portion not exposed by the second opening, is shielded by the via mask layer and is not bombarded by plasma. Therefore, these unetched side edges are completely preserved, forming a tubular dielectric isolation layer. The sidewalls of the isolation holes are the hole walls containing multiple layers of metal bit lines or word lines exposed during step 102 when the stacked structure is cut through. Thus, the preserved dielectric isolation layer can be considered a dense and continuous insulating sleeve located between the centrally formed via groove and the outer metal line cross-section, severing the physical contact path between them.
[0072] Filling with conductive material refers to filling the vias with a low-resistivity material (such as tungsten W, copper Cu, or their alloys) using processes such as physical vapor deposition (PVD), chemical vapor deposition (CVD), or electroplating. Typically, before filling with the main conductive metal, a very thin adhesion / barrier layer (such as titanium nitride TiN or tantalum nitride TaN) can be compliantly deposited on the inner wall of the via to prevent metal ions from diffusing into the dielectric layer. After filling, excess metal material on the top surface of the stacked structure is removed by chemical mechanical polishing (CMP), resulting in a flush-surface connection structure.
[0073] For example, Figure 4C This is a cross-sectional schematic diagram of the memory provided in the embodiments of this application during the stage of completing insulation isolation and forming the final connection structure. Figure 4C The left half of the dashed box illustrates the failure state of related technologies where residual deep pits lead to a short circuit in the final vertical through-hole; the right half illustrates the successful state of this application's embodiment achieving good insulation. Figure 4C As shown on the right, after forming the aforementioned dense insulating isolation structure 406, a through-hole groove was successfully constructed in the center of the insulating isolation structure 406 through the etching guidance of the second opening, and filled with conductive metal to form a connection structure 407 (i.e., a top through-hole). The bottom end of this connection structure 407 achieves stable electrical connection with the lower conductive structure 401. Combined with... Figure 4C The microscopic cross-section on the right side is clearly visible. Because the cross-sectional dimension of the connection structure 407 (corresponding to the internal through-hole groove) is strictly smaller than the overall cross-sectional dimension of the insulating isolation structure 406, a solid insulating dielectric entity, undamaged by the second etching, is naturally retained around the central connection structure 407. This retained insulating entity constitutes the dielectric isolation layer. As a stable physical barrier, this dielectric isolation layer provides excellent electrical insulation between the central connection structure 407 and the exposed multilayer conductive cross-sections in the stacked structure 402. More importantly, because this application maintains a high degree of flatness by retaining the ineffective storage structure in the preceding steps, the dielectric isolation layer used for isolation here is extremely dense and regular, and its interior does not contain any metal residue left by grinding depressions. Therefore, this electrical connection fabrication method based on first forming a large-size isolation entity and then nesting holes inside fundamentally eliminates the short circuit phenomenon caused by physical overlap between the connection structure 407 and the surrounding internal network, significantly improving the overall insulation reliability and process yield of the three-dimensional high-density memory device.
[0074] The memory formation method provided in this application maintains homogeneity and global pattern density consistency on the wafer surface by completely preserving non-effective memory structures in the connection areas during the fabrication of a stacked structure containing multiple memory structure layers. This effectively avoids the problems of local over-polishing and microstructure recess inheritance during chemical mechanical polishing (CMP) from a physical mechanism perspective. Furthermore, by performing a one-time through-etching and insulating dielectric backfilling in the final stage, and nesting holes inside the formed insulating isolation structure, the through-connection structure is completely wrapped by a dense and regular dielectric isolation layer. This series of processes synergistically eliminates the risk of conductive material residue in local pits, cuts off the path of physical overlap and electrical short circuit between the connection structure and the surrounding internal network, thereby improving the overall insulation reliability of the three-dimensional memory device in a high-density integration environment and effectively ensuring the accuracy of the memory during read and write processes. At the same time, this application avoids the practice of setting avoidance windows layer by layer in related technologies, so that the pattern arrangement of multiple array masks at the bottom layer returns to an uninterrupted periodic continuous pattern array. Thus, during the photolithography exposure stage, this fully regularized design eliminates the optical proximity effect (OPE) caused by irregular edges at its source, ensuring high-fidelity transfer of the photoresist pattern and significantly reducing the defect rate in the photolithography and etching processes. Furthermore, this embodiment decouples the physical isolation requirements of vertical vias from the underlying array layout data. If subsequent product specification upgrades require changes to the position of the connection structure, there is no need to simultaneously modify the underlying multi-layer array mask; only a single independent mask used for centralized via drilling needs modification. This orthogonal decoupling architecture not only simplifies the formula complexity of Design Rule Check (DRC) but also significantly shortens the iteration cycle of layout verification, substantially reducing the financial costs associated with mask redesign. In addition, this embodiment not only maintains extremely high flatness physically through homogeneous structures but also cuts off signal paths of ineffective memory structures in the layout routing design, placing them in an electrically floating state. This ensures that the support structure residing in the array does not generate any parasitic capacitive coupling or additional leakage power consumption, balancing process requirements with the chip's high electrical reliability. Furthermore, this application reserves the difference in inner and outer cross-sectional dimensions when forming the connection structure, providing ample process window for the inherent overlay shift in modern high-precision lithography machines. Even if a slight center offset occurs during actual via exposure, the etching process will still be confined within the insulating isolation entity, ensuring that the outer insulating barrier is never breached. This high-tolerance nested manufacturing strategy gives the production line extremely high resilience, reducing the difficulty of three-dimensional high aspect ratio via overlay processes and significantly improving the yield of mass-produced products.
[0075] Based on the same inventive concept, this application also provides a memory, which is fabricated using the memory formation method of any of the above embodiments. The memory includes at least a substrate, a lower conductive structure, a stacked structure containing multiple memory structure layers, an upper conductive structure, and an insulating isolation structure and a connection structure located within a connection region. Within the connection region, the insulating isolation structure vertically penetrates the stacked structure, and the connection structure is embedded in the center of the insulating isolation structure. Because this memory employs the aforementioned process of completely preserving the non-effective memory structure in the connection region to maintain the uniformity of the polishing interface material, the insulating isolation structure remains flush with the top surface of the stacked structure, and the interfaces of each memory structure layer around the insulating isolation structure exhibit a flat physical morphology without microscopic dishing or conductive residue. Simultaneously, because the cross-sectional size of the insulating isolation structure is larger than the cross-sectional size of the embedded connection structure, a dense and continuous dielectric isolation layer is naturally preserved around the connection structure. Based on this dual spatial constraint of an outer insulating barrier and an internal nested via, the memory eliminates the physical overlap and short circuit problem between the vertical connection channel and the surrounding horizontal network in terms of physical structure, thus achieving extremely high three-dimensional insulation reliability and extremely low data leakage rate in the overall architecture.
[0076] In some embodiments, the memory stacking structure includes multiple layers of bit lines and multiple layers of word lines stacked alternately in the vertical direction, and phase-change memory cells disposed between the bit lines and word lines. The active memory structures located within the main array region are equipped with electrical interconnects connected to peripheral logic circuits for addressing and access by the bottom peripheral logic circuits; while the inactive memory structures remaining at the edge of the insulating isolation structure do not have electrical interconnects connected to peripheral logic circuits. This electrical topology design allows the inactive memory structures to provide process support while remaining electrically floating, avoiding the introduction of additional parasitic capacitance charging / discharging or signal crosstalk in the dense three-dimensional array.
[0077] In some embodiments, the substrate is a silicon substrate with peripheral logic circuits (such as CMOS circuits); the lower conductive structure is a subtop metal structure located below the stacked structure, and the upper conductive structure is a top metal structure formed on the stacked structure; the connection structure is a top via that vertically penetrates the stacked structure, with its bottom end connected to the subtop metal structure and its top end connected to the top metal structure.
[0078] In some embodiments, the memory can also be integrated into a high-capacity standalone phase-change memory (StandalonePCM) chip, an embedded non-volatile memory (eNVM) module in a microcontroller, or a heterogeneously integrated compute-in-memory (CIM) chip architecture; the insulating isolation structure can be a dense entity containing oxide materials such as silicon dioxide (SiO2); the connection structure can be made of low resistivity materials such as tungsten (W) or copper (Cu), and a titanium nitride (TiN) or tantalum nitride (TaN) adhesion barrier layer with a thickness of 1 nm to 5 nm can also be compliantly included between the conductive metal outer wall of the connection structure and the dielectric isolation layer that serves as a barrier.
[0079] It should be understood that the phrase "an embodiment" or "one embodiment" throughout the specification means that a specific feature, structure, or characteristic related to the embodiment is included in at least one embodiment of this disclosure. Therefore, "in one embodiment" or "one embodiment" appearing throughout the specification does not necessarily refer to the same embodiment. Furthermore, these specific features, structures, or characteristics can be combined in any suitable manner in one or more embodiments. It should be understood that in the various embodiments of this disclosure, the sequence numbers of the above-described processes do not imply a sequential order of execution; the execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of this disclosure. The sequence numbers of the above-described embodiments are for descriptive purposes only and do not represent the superiority or inferiority of the embodiments.
[0080] The above description is merely an embodiment of this disclosure and is not intended to limit the scope of protection of this disclosure. Any modifications, equivalent substitutions, and improvements made within the spirit and scope of this disclosure are included within the scope of protection of this disclosure.
Claims
1. A method for forming a memory, characterized in that, include: A stacked structure comprising multiple storage structure layers is formed, wherein the stacked structure includes effective storage structures for implementing storage functions and ineffective storage structures located in the connection area; Remove the ineffective storage structure to form an isolation hole through the connection area; An insulating dielectric material is filled into the isolation hole to form an insulating isolation structure. A connection structure is formed within the insulating isolation structure, the connection structure being used to realize the electrical connection between the upper conductive structure and the lower conductive structure.
2. The method according to claim 1, characterized in that, The removal of the ineffective storage structure to form an isolation hole penetrating the connection region includes: An etch mask layer with a first opening is formed on the stacked structure, the first opening exposing the connection region; Using the etching mask layer as a barrier, the stacked structure is etched through along a first direction perpendicular to the surface of the stacked structure to remove the ineffective storage structure and form the isolation hole.
3. The method according to claim 1, characterized in that, The formation of a connection structure within the insulating isolation structure includes: A via mask layer with a second opening is formed on the stacked structure and the insulating isolation structure, wherein the second opening exposes the central region of the insulating isolation structure, and the cross-sectional dimension of the second opening is smaller than the cross-sectional dimension of the insulating isolation structure; Using the via mask layer as a barrier, the insulating isolation structure is etched to form via grooves inside the insulating isolation structure; wherein, the unetched side edges of the insulating isolation structure form a dielectric isolation layer, which is used to isolate the subsequently formed connection structure from the sidewall of the isolation hole; The through-hole groove is filled with conductive material to form the connection structure.
4. The method according to claim 1, characterized in that, The stacked structure includes: multiple layers of bit lines and multiple layers of word lines stacked alternately in a first direction, and a phase-change memory cell disposed between the bit lines and the word lines; The effective storage structure includes: the bit line, the word line, and the phase-change memory cell located outside the connection region; the ineffective storage structure includes: the bit line, the word line, and the phase-change memory cell located within the connection region; The bit lines and word lines in the stacked structure are formed through the following operations: Depositing conductive material thin films; The conductive material film is patterned to form the bit line or word line that remains continuous within the connection area.
5. The method according to claim 4, characterized in that, The stacked structure includes at least a lower storage layer and an upper storage layer stacked sequentially in the first direction; The patterning process is achieved using photolithography. The lower bit line mask and lower word line mask used to define the lower storage layer, and the upper bit line mask and upper word line mask used to define the upper storage layer, are all configured as periodic continuous pattern arrays without avoidance windows at the positions corresponding to the connection areas.
6. The method according to claim 1, characterized in that, The process of filling the isolation hole with an insulating dielectric material to form an insulating isolation structure includes: An insulating dielectric material is deposited inside the isolation hole using a deposition process, such that the insulating dielectric material completely covers the storage structure layer exposed on the sidewall of the isolation hole and fills the isolation hole; The insulating dielectric material located outside the isolation hole is planarized until the top surface of the stacked structure is exposed, so that the top surface of the formed insulating isolation structure is flush with the top surface of the stacked structure.
7. The method according to any one of claims 1 to 6, characterized in that, The stacked structure is formed on a substrate with peripheral logic circuitry; The effective storage structure has an electrical interconnection structure connected to the peripheral logic circuit, so that the effective storage structure can be accessed by the peripheral logic circuit. The ineffective memory structure does not have an electrical interconnection structure connected to the peripheral logic circuit, so that the ineffective memory structure is in an electrically floating state.
8. The method according to any one of claims 1 to 6, characterized in that, The lower conductive structure is the second-to-top metal structure located below the stacked structure, and the upper conductive structure is the top metal structure formed on the stacked structure. The connection structure is a top through hole that vertically penetrates the stacked structure. The bottom end of the top through hole is connected to the second-to-top metal structure, and the top end of the top through hole is connected to the top metal structure.
9. The method according to any one of claims 1 to 6, characterized in that, The insulating dielectric material includes oxide materials.
10. A memory, characterized in that, The memory is formed using the method described in any one of claims 1 to 9.