Fast recovery diode and method of manufacturing
By using a silicon oxide protective layer to cover the annealing process in the fabrication of fast recovery diodes, the problem of uneven forward voltage drop caused by phosphorus impurity ion diffusion was solved, achieving stability and consistency of forward conduction voltage and meeting the performance requirements of automotive applications.
Patent Information
- Application Number
- CN202611427035.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-14
- Publication Date
- 2026-11-24
AI Technical Summary
During the annealing process of existing fast recovery diodes, phosphorus impurity ions from the borosilicate glass diffuse into the contact hole area, resulting in uneven forward voltage drop, affecting device stability and consistency, and making it difficult to meet the stringent requirements of automotive applications.
After ion implantation, a silicon oxide layer is deposited as a protective layer, and annealing is performed under its cover to prevent contamination by mobile ions. The protective layer is then removed to form a heavily doped layer, ensuring the stability of the ohmic contact.
This significantly improves the batch-to-batch consistency of the forward conduction voltage VF of fast recovery diodes, enhances the stability of device parameters, and meets the requirements of automotive applications.
Smart Images

Figure CN123164789A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor device fabrication, and more specifically, to a fast recovery diode and its fabrication method. Background Technology
[0002] As the application areas of fast recovery diodes (FRDs) have gradually upgraded from industrial applications to automotive applications, customers' requirements for the performance of FRD products have significantly increased. In direct-bonded copper (DBC) modules, multiple FRDs are typically used in parallel. If the forward voltage (VF) distribution of each FRD is uneven, it can easily lead to voltage oscillations during the turn-on process of the entire DBC module and increase switching losses. Therefore, improving the stability of the forward voltage drop distribution of FRD products has become a key issue in device manufacturing.
[0003] In existing fast recovery diode manufacturing processes, annealing is typically performed after contact hole (CO) implantation. The main purpose of annealing is to repair lattice damage caused by implantation, activate dopant ions, and thus reduce the ohmic contact resistance between the metal and dielectric layers. The element implanted into the contact hole is usually boron (B). However, since the interlayer dielectric (ILD) is deposited using borosilicate glass (BPSG), its surface contains impurity ions such as phosphorus (P). During annealing, the presence of P in the borosilicate glass restricts the use of N-type furnace tubes. More importantly, phosphorus impurity ions from the borosilicate glass can diffuse from the wafer surface into the contact hole area, causing contamination of the open contact hole area with mobile phosphorus ions. This mobile ion contamination can cause fluctuations in the device's forward voltage drop, and in severe cases, even lead to device failure, making it difficult to meet the stringent requirements for forward voltage drop distribution stability in conventional applications.
[0004] Therefore, how to effectively prevent mobile P ions from entering the contact hole during the annealing process in order to improve the stability of the forward voltage drop distribution of fast recovery diode products is a technical problem that urgently needs to be solved in this field.
[0005] It should be noted that the information disclosed in the background section above is only used to enhance the understanding of the background of the present invention, and therefore may include information that does not constitute prior art known to those skilled in the art. Summary of the Invention
[0006] To address the problems in the prior art, the present invention aims to provide a fast recovery diode and its fabrication method, which effectively improves the stability and consistency of the forward conduction voltage VF of the fast recovery diode.
[0007] A first aspect of the present invention provides a method for fabricating a fast recovery diode, the method comprising the following steps: A substrate is provided, the substrate comprising a semiconductor substrate, an active region within the semiconductor substrate and a plurality of voltage divider rings surrounding the active region, and a field oxide layer and a dielectric layer stacked sequentially, wherein a plurality of contact holes are formed on the field oxide layer and the dielectric layer, and the plurality of contact holes respectively expose a portion of the surface of the active region and a portion of the surface of the voltage divider rings; An ion implantation region is formed in the active region and the voltage divider ring through the contact hole; A protective layer is deposited on the surface of the semiconductor substrate; The semiconductor substrate is annealed under the protective layer. Remove the protective layer and form a heavily doped layer in the active region and the voltage divider ring.
[0008] According to a first aspect of the invention, the protective layer is a silicon oxide layer.
[0009] According to a first aspect of the invention, the silicon oxide layer is deposited using the TEOS process.
[0010] According to a first aspect of the invention, the thickness of the protective layer is 500 to 1000 angstroms.
[0011] According to a first aspect of the invention, the protective layer is removed using a wet process.
[0012] According to a first aspect of the invention, the ion implantation process implants element B.
[0013] According to a first aspect of the invention, the dielectric layer comprises a borosilicate glass layer, or
[0014] The dielectric layer comprises a silicon oxide layer and a borosilicate glass layer stacked sequentially.
[0015] According to a first aspect of the invention, the semiconductor substrate subjected to annealing under the protective layer satisfies any of the following conditions: Annealing temperature is 800~1000℃; Annealing time is 10-120 minutes.
[0016] A second aspect of the present invention provides a fast recovery diode, the fast recovery diode comprising: A semiconductor substrate, wherein the semiconductor substrate is of a first conductivity type; An active region located within the semiconductor substrate and a plurality of voltage dividing rings sequentially surrounding the active region, wherein the active region and the voltage dividing rings contain ions of a second conductivity type; A field oxide layer and a dielectric layer are located on the semiconductor substrate. A plurality of contact holes are formed on the field oxide layer and the dielectric layer, and the plurality of contact holes respectively expose a portion of the surface of the active region and a portion of the surface of the voltage divider ring. A heavily doped layer located within the active region and the voltage divider ring, wherein the heavily doped layer contains ions of the second conductivity type; An anode metal layer is located on a first side of the semiconductor substrate and fills the contact hole.
[0017] In the fast recovery diode fabrication method of the present invention, in order to form an ohmic contact in the anode metal layer, a protective layer is deposited after ion implantation in the active region and several voltage divider ring regions and before annealing to activate the implanted ions. Under the protection layer, a heavily doped layer is formed by annealing. This effectively prevents movable ions from the N-type furnace tube from entering the active region and voltage divider ring, ensuring the quality of the heavily doped layer and significantly improving the stability of device parameters, especially the consistency of the forward conduction voltage VF within and between batches. The protective layer does not degrade the forward characteristics and does not affect the device structure after removal. Attached Figure Description
[0018] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this application and, together with the description, serve to explain the principles of this application. Other features, objects, and advantages of the invention will become more apparent from the following detailed description of non-limiting embodiments with reference to the accompanying drawings. It is obvious that the drawings described below are merely some embodiments of the invention, and those skilled in the art can obtain other drawings based on these drawings without inventive effort. Furthermore, the drawings are merely illustrative diagrams of this disclosure and are not necessarily drawn to scale. The same reference numerals in the drawings denote the same or similar parts, and therefore repeated descriptions of them will be omitted. Some block diagrams shown in the drawings are functional entities and do not necessarily correspond to physically or logically independent entities.
[0019] Figure 1 This is a flowchart illustrating a method for fabricating a fast recovery diode according to an embodiment of the present invention; Figures 2-7 This is a schematic diagram of the fabrication process of a fast recovery diode according to an embodiment of the present invention; Figure 8 This is a carrier concentration-depth distribution curve of a semiconductor substrate with 400 Å and 800 Å protective layers deposited by TEOS process placed in an N-type furnace tube for 7 days. Figure 9 and Figure 10Box plots and corresponding standard deviation comparisons of the forward conduction voltage over 6 months for fast recovery diodes prepared by the pre-annealing protective layer method of the present invention and the conventional method. Detailed Implementation
[0020] The following specific examples illustrate the implementation of the present invention. Those skilled in the art can easily understand other advantages and effects of the present invention from the content disclosed herein. The present invention can also be implemented or applied through other different specific embodiments, and various details in the present invention can be modified or changed according to different viewpoints and application systems without departing from the spirit of the present invention. It should be noted that, unless otherwise specified, the embodiments and features in the embodiments of the present invention can be combined with each other.
[0021] The present invention will now be described in detail with reference to the accompanying drawings, so that those skilled in the art can readily implement it. The present invention can be embodied in many different forms and is not limited to the embodiments described herein.
[0022] In this specification, the terms "one embodiment," "some embodiments," "example," "specific example," or "some examples," etc., refer to specific features, structures, materials, or characteristics represented in connection with that embodiment or example, which are included in at least one embodiment or example of this specification. Furthermore, the specific features, structures, materials, or characteristics represented may be combined in any suitable manner in one or more embodiments or examples. Moreover, without contradiction, those skilled in the art can combine and integrate the different embodiments or examples represented in this specification, as well as the features of different embodiments or examples.
[0023] Throughout this specification, when it is said that a device is "connected" to another device, this includes not only "direct connection" but also "indirect connection" by placing other components in between. Terms indicating relative space, such as "front," "back," "up," and "down," are used to more easily explain the relationship of one device relative to another illustrated in the figures. These terms refer not only to their meaning in the figures but also to other meanings or operations of the device in use. For example, if the device in the figures is flipped, a device previously described as "below" another device may now be described as "above" another device. Therefore, the exemplary term "down" includes both "up" and "below." The device may be rotated 90° or other angles, and the terms representing relative space are interpreted accordingly.
[0024] Although the terms first, second, etc., are used in some instances herein to refer to various elements, these elements should not be limited by these terms. These terms are used only to distinguish one element from another. For example, first interface and second interface, etc., are used. Furthermore, as used herein, the singular forms “a,” “an,” and “the” are intended to also include the plural forms unless the context indicates otherwise. It should be further understood that the terms “comprising,” “including,” indicate the presence of the stated feature, step, operation, element, component, item, kind, and / or group, but do not exclude the presence, occurrence, or addition of one or more other features, steps, operations, elements, components, items, kinds, and / or groups. The terms “or” and “and / or” as used herein are interpreted as inclusive, or mean any one or any combination thereof. Thus, “A, B, or C” or “A, B, and / or C” means “any one of the following: A; B; C; A and B; A and C; B and C; A, B, and C.” Exceptions to this definition will only occur if the combination of elements, functions, steps, or operations is inherently mutually exclusive in some way.
[0025] Although not fully defined, all terms, including technical and scientific terms used herein, shall have the same meaning as commonly understood by one of ordinary skill in the art to which this specification pertains. Terms defined in commonly used dictionaries shall be further interpreted as having a meaning consistent with the relevant technical literature and the content of this present instruction, and shall not be over-interpreted as having an ideal or overly formulaic meaning unless otherwise defined.
[0026] The fast recovery diode and its preparation method of the present invention are further described below with reference to the accompanying drawings and specific embodiments. It should be understood that the specific embodiments are not intended to limit the scope of protection of the present invention.
[0027] This invention provides a method for fabricating a fast recovery diode. Figure 1 This is a flowchart of a method for fabricating a fast recovery diode according to an embodiment of the present invention. Specifically, the fabrication method includes the following steps: Step S100: Provide a substrate. The substrate may include a semiconductor substrate, an active region 41 formed within the semiconductor substrate, and a plurality of voltage dividing rings 42 surrounding the active region 41. The semiconductor substrate may be a silicon (Si) substrate. In other embodiments, the material of the semiconductor substrate may also include silicon carbide (SiC), silicon germanium (SiGe), or multi-element semiconductor materials composed of group III-V elements (such as InP, GaAs, GaP, InAs, InSb, InGaAs, or InGaAsP, etc.).
[0028] For example, the semiconductor substrate is a silicon substrate, which may include a substrate 10, a buffer layer 11 formed on the substrate 10, and an epitaxial layer 12 formed on the buffer layer 11. Optionally, the substrate 10 has a first conductivity type. If the first conductivity type is N-type, then the second conductivity type is P-type, and vice versa. The conductivity types of the buffer layer 11 and the epitaxial layer 12 are the same as those of the substrate 10. When the substrate 10 is N-type... + When using an N-type substrate, buffer layer 11 is an N-type buffer layer, and epitaxial layer 12 is an N-type epitaxial layer. - N-type epitaxial layer. Through N-type buffer layer and N... - The combination of the epitaxial layer is beneficial to improving the reverse breakdown voltage of the device, while also taking into account the forward current capability and forward conduction voltage.
[0029] In the above embodiment, the active region 41 and a plurality of voltage divider rings 42 are disposed on the side of the epitaxial layer 12 facing away from the buffer layer 11. The active region 41 may be located in the middle region of the semiconductor substrate, and the voltage divider rings 42 are disposed around the active region 41. The number of voltage divider rings 42 can be set according to the withstand voltage requirements, for example, two, three, four or more. Optionally, each voltage divider ring 42 has the same width, and the width between adjacent voltage divider rings 42 gradually increases from the inside to the outside.
[0030] When substrate 10 is N + When the substrate is P-type, the active region 41 and the voltage divider rings 42 are P-type. A field oxide layer 20 and a dielectric layer 30 are sequentially formed on the semiconductor substrate. The field oxide layer 20 can be formed on the surface of the epitaxial layer 12. The dielectric layer 30 may include a borosilicate glass layer, or a silicon oxide layer and a borosilicate glass layer stacked sequentially. The dielectric layer 30 covers the field oxide layer 20 and serves as the dielectric for subsequent contact hole etching and metal isolation. A plurality of contact holes are formed in the field oxide layer 20 and the dielectric layer 30 through photolithography and etching processes. The contact holes include contact holes C1 and C2, with contact hole C1 exposing a portion of the surface of the active region 41 and contact hole C2 exposing a portion of the surface of the voltage divider rings 42, such as... Figure 2 As shown. The width of the contact hole C1 is smaller than the width of the active region 41, so as to form a good ohmic contact in the active region 41, while avoiding the electric field concentration caused by the contact hole being too wide.
[0031] Step S200: Ion implantation is performed on the semiconductor substrate. It should be noted that the semiconductor substrate referred to below refers to the overall structure formed after the previous step, which includes the substrate 10 and the layers thereon.
[0032] Ion implantation is performed into the active region 41 and the voltage divider ring 42 through contact holes C1 and C2. The implanted ions are of the second conductivity type, such as element B. An ion implantation region 51 is formed in the active region 41 through contact hole C1, and an ion implantation region 52 is formed in the voltage divider ring 42 through contact hole C2. Figure 3As shown. Ion implantation can be performed in one or multiple stages, and the implantation dose and energy can be selected according to the concentration and depth of the target heavily doped layer. For example, the implantation dose can be 1E15~1E16 atoms / cm. 2 The implantation energy can be 30~80 keV. Ion implantation regions 51 and 52 are used to form a heavily doped layer (P) after subsequent annealing. + (Type) to reduce the contact resistance between the metal and the semiconductor and form a good ohmic contact.
[0033] Step S300: Deposit a protective layer 9 on the surface of the semiconductor substrate.
[0034] After ion implantation, a protective layer 9 is deposited on the surface of the semiconductor substrate. The protective layer 9 covers the entire semiconductor substrate, including the surface of the dielectric layer 30, the active region 41 exposed within contact hole C1, and the surface of the voltage divider ring 42 exposed within contact hole C2, as shown below. Figure 4 As shown. Protective layer 9 is a silicon oxide layer, which can be deposited using the TEOS process. Other processes capable of forming silicon oxide layers can also be used, such as LPCVD, PECVD, HDPCVD, SACVD, etc., as long as a silicon oxide protective layer with good coverage can be formed on the contact holes and exposed semiconductor surfaces, and it is compatible with existing fast recovery diode fabrication processes.
[0035] Step S400: Anneal the semiconductor substrate under the protective layer 9.
[0036] Under the protection layer 9, the semiconductor substrate is annealed, see... Figure 5 As shown. Annealing can be performed in a furnace tube, such as an N-type furnace tube. The annealing conditions can meet the following requirements: annealing temperature of 800~1000℃ and annealing time of 10~120 minutes. Through annealing, the implanted ions in ion implantation regions 51 and 52 are activated and propelled into the semiconductor material, thereby forming a heavily doped layer 51a (P) in the active region 41. + A heavily doped layer 52a (P) is formed within the voltage divider ring 42. + The heavily doped layers 51a and 52a have a second conductivity type, for example, N. + Heavy doping layer. Since the protective layer 9 covers the entire surface of the semiconductor substrate, it can effectively reduce mobile ion contamination during annealing and improve device parameter stability.
[0037] To examine the differences in resistance to P-ion contamination caused by different protective layer thicknesses, semiconductor substrates with 400 Å and 800 Å protective layers deposited using the TEOS process were placed in an N-type furnace tube for 7 days. Ion concentration-depth analysis was then performed using the spread resistance profile (SRP) method. The experimental results show that the carrier concentration at approximately 1 μm of the surface of the semiconductor substrate with the 400 Å protective layer is reduced; while the carrier concentration of the semiconductor substrate with the 800 Å protective layer remains relatively consistent at both the surface and within the substrate. (See [link to relevant documentation]). Figure 8 This demonstrates that the silicon oxide layer deposited by the 800 angstrom TEOS process can function as a protective layer, effectively preventing mobile ion contamination in the N-type furnace tube. Therefore, the thickness of the protective layer 9 is preferably 500-1000 angstroms, more preferably about 800 angstroms. The function of the protective layer 9 includes at least preventing mobile ion contamination introduced from the furnace tube from entering the semiconductor substrate surface during subsequent annealing processes, especially during annealing in the N-type furnace tube.
[0038] Step S500: Remove protective layer 9.
[0039] After annealing, the protective layer 9 is removed. This removal can be done using a wet etching process, such as using DHF or BOE wet etching solutions to remove the silicon oxide protective layer. Removing the protective layer 9 exposes the heavily doped layer 51a in the active region 41 and the heavily doped layer 52a in the voltage divider ring 42, facilitating the subsequent formation of the anode metal layer and the achievement of ohmic contact. Since the protective layer 9 has been removed after annealing, it is not retained in the final fast recovery diode device structure. Figure 6 As shown.
[0040] Step S600: Form an anode metal layer 60.
[0041] An anode metal layer 60 is formed on a semiconductor substrate, such as... Figure 7 As shown. The anode metal layer 60 fills contact holes C1 and C2, and makes ohmic contact with the heavily doped layer 51a in the active region 41 and the heavily doped layer 52a in the voltage divider ring 42. The anode metal layer can be made of aluminum, or other suitable metals or metal stacks.
[0042] Alternatively, the fabrication method of the fast recovery diode also includes forming a back-side structure (not shown in the figure) such as a cathode metal layer on the other surface of the semiconductor substrate. The cathode metal layer may be a Ti / Ni / Ag alloy structure.
[0043] This invention also provides a fast recovery diode, which can be fabricated using the above-described method. The fast recovery diode includes: The semiconductor substrate may include: a substrate 10, a buffer layer 11 formed on the substrate 10, and an epitaxial layer 12 formed on the buffer layer 11. In one embodiment, the substrate 10 is an N-type semiconductor substrate. + The substrate is an N-type buffer layer, the buffer layer 11 is an N-type buffer layer, and the epitaxial layer 12 is an N-type substrate. - Type epitaxial layer.
[0044] An active region 41 is located within a semiconductor substrate, and a plurality of voltage-dividing rings 42 sequentially surround the active region 41. Ions of a second conductivity type are present within the active region 41 and the voltage-dividing rings 42. In one embodiment, the second conductivity type is P-type, meaning the active region 41 and the voltage-dividing rings 42 are P-type. The active region 41 may be located in the middle region of the semiconductor substrate, and the voltage-dividing rings 42 are disposed around the active region 41. Optionally, the width of each voltage-dividing ring 42 gradually increases from the inside out (from the active region 41 outwards).
[0045] A field oxide layer 20 and a dielectric layer 30 are located on a semiconductor substrate. The field oxide layer 20 may be formed on the surface of the epitaxial layer 12. The dielectric layer 30 covers the field oxide layer 20 and serves as a dielectric for subsequent contact hole etching and metal isolation. The dielectric layer 30 may include a borosilicate glass layer, or may include a silicon oxide layer and a borosilicate glass layer stacked sequentially. A plurality of contact holes are formed on the field oxide layer 20 and the dielectric layer 30, and the contact holes expose a portion of the surface of the active region 41 and a portion of the surface of the voltage divider ring 42, respectively. The contact holes include contact hole C1 and contact hole C2, with contact hole C1 exposing a portion of the surface of the active region 41 and contact hole C2 exposing a portion of the surface of the voltage divider ring 42. Optionally, the width of contact hole C1 is smaller than the width of the active region 41.
[0046] The heavily doped layer 51a is located within the active region 41, and the heavily doped layer 52a is located within the voltage divider ring 42. The heavily doped layers 51a and 52a contain ions of a second conductivity type. In one embodiment, the heavily doped layers 51a and 52a are P... + Heavy doped layer.
[0047] The anode metal layer 60 is located on the first side of the semiconductor substrate, and fills contact holes C1 and C2, and makes ohmic contact with the heavily doped layer 51a in the active region 41 and the heavily doped layer 52a in the voltage divider ring 42. The anode metal layer can be made of Al metal, or other suitable metals or metal stacks.
[0048] Optionally, the fast recovery diode also includes a cathode metal layer located on the semiconductor substrate opposite to the surface of the anode metal layer 60. The cathode metal layer may employ a Ti / Ni / Ag alloy structure.
[0049] The fast recovery diode provided by this invention, due to the presence of a protective layer 9 after ion implantation and before annealing, and the annealing process performed under the protection layer 9, effectively blocks mobile ion contamination introduced from the N-type furnace tube, improving device parameter stability, especially the batch-to-batch stability of the forward conduction voltage VF. Simultaneously, combined with the N-type buffer layer and N... - The structure of the P-type epitaxial layer, P-type active region, and P-type voltage divider ring is beneficial to improving the reverse breakdown voltage, forward current capability, and reverse recovery characteristics, which can meet the requirements of fast recovery diodes for high reverse withstand voltage, large current capability, and short recovery time in applications such as air conditioner inverters.
[0050] To verify the effect of protective layer 9 on the performance of fast recovery diodes, the following experiment was conducted.
[0051] A fast recovery diode was selected. First, it was verified whether adding a silicon oxide protective layer deposited by the TEOS process would affect the forward conduction voltage VF of the fast recovery diode. The process conditions are shown in Table 1. Table 1
[0052] Table 1 shows that adding a silicon oxide protective layer has little effect on the forward conduction voltage VF under a 150A current condition. The difference in forward conduction voltage VF between the fast recovery diode prepared using the pre-annealing protective layer method of this invention and the existing method is within ~20mV. These test results confirm that the preparation method of this invention does not affect the forward conduction voltage VF of the prepared fast recovery diode, meaning that the preparation method of this invention does not deteriorate the forward characteristics of the fast recovery diode.
[0053] Track the forward conduction voltage VF trend of the above fast recovery diode over 6 months, see Figure 9 and Figure 10 It can be seen that the fast recovery diode prepared by adding a protective layer before annealing according to the present invention exhibits significantly improved stability of its forward conduction voltage VF.
[0054] The above description, in conjunction with specific preferred embodiments, provides a further detailed explanation of the present invention and should not be construed as limiting the specific implementation of the invention to these descriptions. It will be apparent to those skilled in the art that this application is not limited to the details of the above exemplary embodiments, and that the application can be implemented in other specific forms without departing from its spirit or essential characteristics. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of this application is defined by the appended claims rather than the foregoing description. Thus, all variations falling within the meaning and scope of equivalents of the claims are intended to be embraced within this application. No reference numerals in the claims should be construed as limiting the scope of the claims.
Claims
1. A method for fabricating a fast recovery diode, characterized in that, The preparation method includes the following steps: A substrate is provided, the substrate comprising a semiconductor substrate, an active region within the semiconductor substrate and a plurality of voltage divider rings surrounding the active region, and a field oxide layer and a dielectric layer stacked sequentially, wherein a plurality of contact holes are formed on the field oxide layer and the dielectric layer, and the plurality of contact holes respectively expose a portion of the surface of the active region and a portion of the surface of the voltage divider rings; An ion implantation region is formed in the active region and the voltage divider ring through the contact hole; A protective layer is deposited on the surface of the semiconductor substrate; The semiconductor substrate is annealed under the protective layer. Remove the protective layer and form a heavily doped layer in the active region and the voltage divider ring.
2. The method for fabricating a fast recovery diode according to claim 1, characterized in that, The protective layer is a silicon oxide layer.
3. The method for fabricating a fast recovery diode according to claim 2, characterized in that, The silicon oxide layer was deposited using the TEOS process.
4. The method for fabricating a fast recovery diode according to claim 1, characterized in that, The thickness of the protective layer is 500 to 1000 angstroms.
5. The method for fabricating a fast recovery diode according to claim 1, characterized in that, The protective layer is removed using a wet process.
6. The method for fabricating a fast recovery diode according to claim 1, characterized in that, The ion implantation process implants element B.
7. The method for fabricating a fast recovery diode according to claim 1, characterized in that, The dielectric layer includes a borosilicate glass layer, or The dielectric layer comprises a silicon oxide layer and a borosilicate glass layer stacked sequentially.
8. The method for fabricating a fast recovery diode according to claim 1, characterized in that, The semiconductor substrate undergoing annealing under the protective layer meets any of the following conditions: Annealing temperature is 800~1000℃; Annealing time is 10-120 minutes.
9. A fast recovery diode, characterized in that, The fast recovery diode includes: A semiconductor substrate, wherein the semiconductor substrate is of a first conductivity type; An active region located within the semiconductor substrate and a plurality of voltage dividing rings sequentially surrounding the active region, wherein the active region and the voltage dividing rings contain ions of a second conductivity type; A field oxide layer and a dielectric layer are located on the semiconductor substrate. A plurality of contact holes are formed on the field oxide layer and the dielectric layer, and the plurality of contact holes respectively expose a portion of the surface of the active region and a portion of the surface of the voltage divider ring. A heavily doped layer located within the active region and the voltage divider ring, wherein the heavily doped layer contains ions of the second conductivity type; An anode metal layer is located on a first side of the semiconductor substrate and fills the contact hole.