A gallium oxide-based vdmos and a method of manufacturing the same
By designing a multilayer structure and composite insulating layer in gallium oxide VDMOS devices, optimizing current distribution and electric field control, the problems of high on-resistance and low breakdown voltage of existing VDMOS devices in high-frequency, high-voltage and high-power applications are solved, achieving high withstand voltage, low loss and high reliability.
Patent Information
- Application Number
- CN202611398146.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-09
- Publication Date
- 2026-11-24
AI Technical Summary
Existing VDMOS devices suffer from high on-resistance, low breakdown voltage, large internal parasitic capacitance, necking resistance caused by the JFET effect, and long-term reliability issues of the gate oxide layer in high-frequency, high-voltage, and high-power applications, which limits their application in high-power-density and harsh environments.
Using a gallium oxide semiconductor substrate, an N-type heavily doped region, drain electrode, N-type buffer zone, N-type well region, P-type heterodoped region, trench gate region, N-type source region, and P-type source region are designed. The trench gate region is combined with a multilayer structure, including auxiliary gate region and gate region. A composite insulating layer structure of silicon dioxide and silicon oxynitride is used to optimize current distribution and electric field control.
It achieves high withstand voltage, low on-resistance, uniform current distribution and high gate reliability, improves the device's lifespan and application capability at high voltage levels, and reduces the risk of local temperature rise and switching losses.
Smart Images

Figure CN123164818A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of VDMOS technology, and more specifically to a gallium oxide-based VDMOS and its fabrication method. Background Technology
[0002] In recent years, with the rapid development of the electronics industry, power semiconductor devices have played a crucial role in modern power electronic systems. Existing VDMOS devices are mainly based on silicon, silicon carbide, or gallium nitride materials. However, they face several challenges when pursuing high-frequency, high-voltage, and high-power applications. Their channel mobility is significantly affected by interface states, resulting in high on-resistance (Ron) and low breakdown voltage. Large internal parasitic capacitance limits switching speed and increases switching losses. The necking resistance caused by the JFET effect and long-term gate oxide reliability issues also restrict their further application in higher power densities and more demanding operating environments. To address these issues, a gallium oxide-based VDMOS device is explored. Gallium oxide, as an ultra-wide bandgap semiconductor material, has a bandgap of 4.8–4.9 eV and a theoretical breakdown field strength of approximately 8 MV / cm. Its Baricard's figure of merit far exceeds that of silicon, silicon carbide, and gallium nitride, demonstrating enormous application potential in the field of high-voltage power devices. However, the source and body structures of traditional gallium oxide VDMOS often employ asymmetrical designs or simple symmetrical arrangements. When the device is turned on, the current distribution is uneven, which can easily lead to current congestion in local areas, generating hot spot effects and causing excessive local temperature rise, which seriously affects the reliability and lifespan of the device. In existing trench gate gallium oxide VDMOS, the gate structure has limited ability to control the electric field in the channel region. When the device is turned off, electric field concentration is likely to occur in the gate edge region, which reduces the breakdown voltage of the device and limits its application at higher voltage levels.
[0003] Therefore, there is an urgent need for a gallium oxide VDMOS device structure that can take into account high voltage withstand capability, low on-resistance, high gate reliability, and uniform current distribution, so as to give full play to the advantages of the ultra-wide bandgap of gallium oxide material and meet the urgent needs of high-voltage power electronic systems for high-performance power devices. Summary of the Invention
[0004] The purpose of this invention is to provide a gallium oxide-based VDMOS and its fabrication method. By using a gallium oxide semiconductor substrate, an N-type heavily doped region, drain electrode, N-type buffer region, N-type well region, P-type heterodoped region, trench gate region, N-type source region, P-type source region, source electrode, and gate electrode are fabricated on it. Combined with a multilayer trench gate region, including an auxiliary gate region and a gate region, a VDMOS chip is formed. This allows for a trench gate MOS device with an auxiliary gate, and also achieves better voltage withstand capability and other effects.
[0005] The specific technical solution of the present invention is as follows: A gallium oxide-based VDMOS comprises: a substrate made of gallium oxide semiconductor material; an N-type heavily doped region on the bottom layer of the substrate; a drain electrode on the lower surface of the N-type heavily doped region; an N-type buffer region on the upper surface of the N-type heavily doped region; an N-type well region on the upper surface of the N-type buffer region; a P-type hetero-doped region and a trench gate region on the N-type well region; the P-type hetero-doped region being disposed on both sides of the trench gate region and in contact with the trench gate region; an N-type source region and a P-type source region on the P-type hetero-doped region, the N-type source region in contact with the trench gate region; the P-type source region in contact with the N-type source region but away from the trench gate region; source electrodes on the N-type and P-type source regions; a gate electrode on the trench gate region; and an electrode insulating layer between the source electrodes and the trench gate region.
[0006] Furthermore, the slotted gate region includes an auxiliary gate region and a gate region. The auxiliary gate region is disposed on the upper surface of the gate region, and a gate electrode is provided on the upper surface of the auxiliary gate region. The auxiliary gate region is used to drive whether the gate region is charged, and the gate region is used to drive whether the P-type heterodoped region is connected to the N-type source region and the N-type well region.
[0007] Furthermore, the gate region includes a gate insulating layer and a gate polysilicon layer. The gate insulating layer is disposed on the N-type well region, the gate polysilicon layer is disposed on the upper surface of the gate insulating layer, and the auxiliary gate region is disposed on the gate polysilicon layer.
[0008] Furthermore, the gate insulating layer is selected from compound insulating materials. This can reduce gate leakage current, improve the withstand voltage and reliability of the insulating layer, etc. Examples include silicon dioxide.
[0009] Furthermore, the gate polysilicon layer can be selected as a heavily doped N+ or P+ type, which can help to improve the uniformity of electric field control and the reliability of long-term use.
[0010] Furthermore, the auxiliary gate region includes an auxiliary on / off region, an auxiliary insulating layer, and an auxiliary polysilicon layer. The auxiliary on / off region is disposed on the upper surface of the gate region, the auxiliary insulating layer is disposed on the upper surface of the auxiliary on / off region, the auxiliary polysilicon layer is disposed on the auxiliary insulating layer, and the gate electrode is disposed on the auxiliary polysilicon layer.
[0011] Furthermore, the auxiliary insulating layer includes a silicon dioxide layer and a SION layer. The silicon dioxide layer is disposed on the upper surface of the auxiliary switching region, the SION layer is disposed on the silicon dioxide layer, and the auxiliary polycrystalline silicon layer is disposed on the SION layer. The SION region here is formed using silicon oxynitride material. The use of silicon dioxide and silicon oxynitride enables the device to achieve high voltage resistance, high reliability, and high-frequency application performance. By using silicon dioxide as the silicon interface of the trench gate and combining SION with silicon dioxide, the electrical isolation of the device is enhanced. In the fabrication and use of this device, the use of silicon dioxide can act as a stress buffer layer, reducing the mechanical stress damage of the SION to the underlying substrate and avoiding crystal defects. The selection of a wider SION layer reduces the leakage current risk and tunneling current phenomenon of the thin dielectric layer between electrodes, improving the reliability of the device.
[0012] Furthermore, the auxiliary switching region includes an auxiliary N-type region, an auxiliary P-type region, and an auxiliary N-type electrode region. The auxiliary N-type region is disposed on the upper surface of the gate region. The upper surface of the auxiliary N-type region is provided with the auxiliary insulating layer and the auxiliary P-type region. The upper surface of the auxiliary P-type region is provided with the auxiliary N-type electrode region. The auxiliary insulating layer is in contact with the auxiliary N-type region, the auxiliary P-type region, and the auxiliary N-type electrode region respectively. An auxiliary gate region is disposed on the upper surface of the auxiliary N-type region. Alternatively, the auxiliary switching region includes an auxiliary P-type region, an auxiliary N-type region, and an auxiliary P-type electrode region. The auxiliary P-type region is disposed on the upper surface of the gate region. The upper surface of the auxiliary P-type region is provided with the auxiliary insulating layer and the auxiliary N-type region. The upper surface of the auxiliary N-type region is provided with the auxiliary P-type electrode region. The auxiliary insulating layer is in contact with the auxiliary P-type region, the auxiliary N-type region, and the auxiliary P-type electrode region, respectively. An auxiliary gate region is disposed on the upper surface of the auxiliary P-type region.
[0013] Furthermore, the auxiliary polycrystalline silicon layer can be selected as a heavily doped N+ or P+ type, which can help to improve the uniformity of electric field control and the reliability of long-term use.
[0014] Furthermore, a metal composite layer is provided between the drain electrode, source electrode, and gate electrode and the substrate.
[0015] Furthermore, the metal composite layer includes a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, and a gold layer on the nickel layer.
[0016] Furthermore, the drain electrode, source electrode, and gate electrode all have the same thickness; as an electrode material for power devices, they can be deposited well on the substrate surface, form conductive interconnects with the doped regions on the substrate, and balance conductivity and thermal conductivity, thereby reducing costs and improving reliability.
[0017] Furthermore, the P-type heterodoped region is symmetrically arranged around the centerline of the trench gate region. This symmetrical arrangement facilitates balanced conduction and avoids the effects of asymmetry; it also ensures that the channels formed by the trench gate region are uniform and balanced, contributing to lower voltage withstand and lower losses.
[0018] Furthermore, the N-type source region is symmetrically arranged with respect to the centerline of the slotted gate region.
[0019] Furthermore, the P-type source region is symmetrically arranged with respect to the centerline of the slotted gate region. This arrangement ensures that the parasitic resistance and capacitance of the two source regions (N-type and P-type source regions) are symmetrical, guaranteeing identical electrical characteristics on both sides and preventing issues such as premature conduction or breakdown on one side. This arrangement also results in a uniform current density distribution, avoiding current congestion on one side and the risk of excessive local temperature rise, thus improving the reliability of carrier migration. If the arrangement is asymmetrical, a shorter current path or lower resistance on one side can lead to current concentration and potentially hot spots.
[0020] Furthermore, the auxiliary N-type region is symmetrically arranged with respect to the centerline of the slotted gate region; the auxiliary P-type region is symmetrically arranged with respect to the centerline of the slotted gate region; and the auxiliary N-type pole region is symmetrically arranged with respect to the centerline of the slotted gate region. Alternatively, the auxiliary P-type region is symmetrically arranged with respect to the centerline of the slotted gate region; the auxiliary N-type region is symmetrically arranged with respect to the centerline of the slotted gate region; and the auxiliary P-type pole region is symmetrically arranged with respect to the centerline of the slotted gate region.
[0021] Furthermore, the height of the P-type heterodoped region is smaller than the height of the N-type well region. This helps to avoid junction depth. Excessive electric field concentration can lead to a smoother surface electric field distribution, increasing breakdown voltage and preventing early avalanche breakdown.
[0022] Furthermore, the height of the heavily doped N-type region is greater than the height of the N-type buffer zone. The heavily doped N-type region provides an ohmic contact for the drain electrode and facilitates carrier inflow; the N-type buffer zone reduces on-resistance, mitigates impact from carriers (such as positive and negative charges), and protects the device.
[0023] Furthermore, the substrate is selected from 6-inch, 8-inch, 12-inch, and other specifications.
[0024] Furthermore, the width of the drain electrode is greater than the width of the source electrode, which is greater than the width of the gate electrode.
[0025] Furthermore, the width of the N-type source region is not less than the width of the P-type source region.
[0026] Furthermore, the height of the P-type heterodoped region is less than the height of the N-type source region.
[0027] Furthermore, a method for fabricating a gallium oxide-based VDMOS includes the following steps: Step 1: Structural Design of VDMOS Devices The gallium oxide-based VDMOS includes: a substrate made of gallium oxide semiconductor material; an N-type heavily doped region on the bottom layer of the substrate; a drain electrode on the lower surface of the N-type heavily doped region; an N-type buffer region on the upper surface of the N-type heavily doped region; an N-type well region on the upper surface of the N-type buffer region; a P-type hetero-doped region and a trench gate region on the N-type well region; the P-type hetero-doped region being disposed on both sides of the trench gate region and in contact with the trench gate region; an N-type source region and a P-type source region on the P-type hetero-doped region, the N-type source region in contact with the trench gate region; the P-type source region in contact with the N-type source region and away from the trench gate region; source electrodes on the N-type and P-type source regions; a gate electrode on the trench gate region; and an electrode insulating layer between the source electrodes and the trench gate region. Step 2: Formation of the substrate with an N-type buffer Based on the structural design in step 1, a semiconductor wafer is selected as the substrate. The upper and lower surfaces of the substrate are cleaned to remove surface oxides and oil stains. RCA cleaning agent is used for cleaning, followed by rinsing with deionized water and drying in a nitrogen atmosphere. After drying, a layer of positive photoresist is coated on the lower surface of the substrate. The substrate is exposed using a photolithography machine according to a pre-designed mask pattern with an N-type buffer. The exposed photoresist area is then developed and removed to expose the N-type buffer. The substrate is then transferred to an N-type ion implanter. N-type ions are lightly doped into the N-type buffer from the lower surface of the substrate until the lower surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using a photoresist stripping solution, cleaned with deionized water, and dried in a nitrogen atmosphere to obtain a substrate with an N-type buffer. Step 3: Formation of a substrate with heavily doped N-type regions Based on step 2, on the substrate with an N-type buffer, and located at the lower part of the N-type buffer, N-type ions are heavily doped using an N-type ion implanter. The N-type ions are heavily doped into the lower part of the substrate with the N-type buffer and extend to the lower surface of the substrate. Then, the remaining unexposed photoresist is removed using a photoresist stripping solution, and then cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with a heavily doped N-type region. Step 4: Formation of the substrate with N-type well regions Based on step 3, a substrate with a heavily doped N-type region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the N-type well region. The exposed photoresist is then developed and cleaned to remove it, exposing the N-type well region. The substrate is then transferred to an N-type ion implanter, and N-type ions are lightly doped into the N-type well region from the upper surface of the substrate through the N-type ion implanter until the upper surface of the N-type buffer zone is reached. The remaining unexposed photoresist is then removed by photoresist stripping solution, and the substrate is cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with an N-type well region. Step 5: Formation of a substrate with p-type heterodoped regions Based on step 4, a substrate with an N-type well region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the P-type hetero-doped region. The exposed photoresist is then developed and cleaned to remove it, exposing the P-type hetero-doped region. The trench region of the P-type hetero-doped region is then etched out by dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed by photoresist stripping solution, and the substrate is cleaned with deionized water and dried in a nitrogen atmosphere. Then, the P-type hetero-doped region is deposited at room temperature using radio frequency magnetron sputtering technology with a NiO ceramic target in an Ar / O2 mixed atmosphere. At this time, the trench regions of the N-type source region and the P-type source region are still retained, forming a substrate with a P-type hetero-doped region. Step 6: Formation of the substrate with N-type source region Based on step 5, a substrate with a P-type hetero-doped region is selected. Then, using radio frequency magnetron sputtering technology with a Ga2O3 ceramic target, gallium oxide regions are deposited at room temperature in an Ar / O2 mixed atmosphere, filling the trenches of the N-type and P-type source regions. Then, the excess gallium oxide is ground off using CMP technology until the upper surface of the substrate is reached. A layer of positive photoresist is then coated on the upper surface of the substrate. Photolithography is performed according to the pre-designed mask pattern of the N-type source region. The exposed photoresist is then developed and cleaned to remove it, exposing the N-type source region. The substrate is then placed in an N-type ion implanter, and N-type ions are re-doped into the N-type source region from the upper surface of the substrate until the upper surface of the P-type hetero-doped region is reached. Then, the remaining unexposed photoresist is removed using a photoresist stripping solution, and the substrate is cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with an N-type source region. Step 7: Formation of the substrate with the P-type source region Based on step 6, a substrate with an N-type source region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the P-type source region. The exposed photoresist is then developed and cleaned to remove it, exposing the P-type source region. The trench area of the P-type source region is then etched out using dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using photoresist stripping solution, and the substrate is cleaned with deionized water. It is then dried in a nitrogen atmosphere. The P-type source region is then deposited using radio frequency magnetron sputtering technology with a Li-doped NiO ceramic target in an Ar / O2 mixed atmosphere. The excess Li-doped NiO and NiO are then ground off using CMP technology until the upper surface of the substrate is reached, thus forming the substrate with the P-type source region. Step 8: Formation of the substrate with the gate region in the trench gate region Based on step 7, a substrate with a P-type source region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. Photolithography is performed according to the pre-designed mask pattern of the grooved gate region. The exposed photoresist is then developed and cleaned to remove it, exposing the grooved gate region. The grooved gate region is then etched using dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using a photoresist stripping solution, followed by cleaning with deionized water and drying under nitrogen atmosphere. A silicon dioxide layer is then deposited on the inner wall of the grooved gate region using PECVD technology, and a polysilicon layer is deposited on the upper surface of the silicon dioxide layer to fill the grooved gate region. Then, the excess polysilicon and silicon dioxide layers are ground away using CMP technology until the upper surface of the substrate, i.e., the upper surface of the N-type source region, is reached. Next, a layer of positive photoresist is coated on the upper surface of the substrate. Photolithography is performed according to the mask pattern of the auxiliary gate region in the pre-designed grooved gate region. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary gate region in the grooved gate region. The groove region of the auxiliary gate region in the grooved gate region is then etched out using dry etching technology until the upper surface of the polysilicon layer is reached. The remaining unexposed photoresist is then removed using photoresist stripping solution, and the substrate is cleaned with deionized water and then dried in a nitrogen atmosphere. This process creates a substrate with the gate region in the grooved gate region. Step 9: Formation of the substrate for the auxiliary gate region in the slotted gate region Based on step 8, a substrate with a gate region in a grooved gate region is selected. Then, using RF magnetron sputtering technology with a Ga2O3 ceramic target, gallium oxide regions are deposited at room temperature in an Ar / O2 mixed atmosphere until the lower surface of the auxiliary P-type region is reached. Excess gallium oxide is then removed using CMP technology until the upper surface of the substrate is reached. A layer of positive photoresist is then coated on the upper surface of the substrate. Photolithography is performed according to a pre-designed mask pattern for the auxiliary N-type electrode region. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary N-type electrode region. This region is then placed in an N-type ion implanter, and N-type ions are re-implanted from the upper surface of the substrate into the auxiliary N-type electrode region until the upper surface of the polysilicon layer is reached. Then, [further details are needed for accurate translation]. The photoresist stripping solution removes the remaining unexposed photoresist, followed by cleaning with deionized water and drying in a nitrogen atmosphere. Then, using RF magnetron sputtering with a NiO ceramic target in an Ar / O2 mixed atmosphere, an auxiliary P-type region is deposited at room temperature. Excess NiO is then removed using CMP (Chemical Motion Processing) until the substrate surface is reached. Next, using RF magnetron sputtering with a Ga2O3 ceramic target in an Ar / O2 mixed atmosphere, a gallium oxide region is deposited at room temperature until the substrate surface is reached. Excess gallium oxide is then removed using CMP until the substrate surface is reached. Finally, a layer of positive photoresist is coated onto the substrate surface, and the pre-designed auxiliary N-type region is then applied. The mask pattern of the auxiliary N-type region is exposed using a photolithography machine. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary N-type region. This region is then placed in an N-type ion implanter, where N-type ions are re-implanted from the top surface of the substrate into the auxiliary N-type region, continuing until the top surface of the auxiliary P-type region. The remaining unexposed photoresist is then removed using a photoresist stripping solution, followed by cleaning with deionized water and drying under a nitrogen atmosphere. Next, a layer of positive photoresist is coated onto the top surface of the substrate. Based on the pre-designed mask pattern of the auxiliary insulating layer and auxiliary polysilicon layer in the trench gate region, the region is exposed using a photolithography machine. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary insulating layer and auxiliary polysilicon layer. Then, the trench areas of the auxiliary insulating layer and the auxiliary polysilicon layer are etched out using dry etching technology until the upper surface of the auxiliary N-type electrode region is reached. Then, the remaining unexposed photoresist is removed using photoresist stripping solution, and then cleaned with deionized water. After drying in a nitrogen environment, a silicon dioxide layer is deposited on the inner wall of the trench area of the auxiliary insulating layer and the auxiliary polysilicon layer using PECVD technology. A SION layer is deposited on the upper surface of the silicon dioxide layer, and then a polysilicon layer is deposited on the upper surface of the SION layer to fill the trench area of the trench gate region. Then, the excess polysilicon layer, SION layer and silicon dioxide layer are ground away using CMP technology until the upper surface of the substrate is reached, forming a substrate with a trench gate region. Step 10: Formation of the substrate with source and gate electrodes Based on step 9, a substrate with a grooved gate region is selected and transferred to a wafer electroplating device. A multilayer composite metal conductive layer is electroplated on the upper surface of the substrate, including a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, a gold layer on the nickel layer, and a copper or aluminum layer in contact with the gold layer. Then, a negative photoresist is coated on the metal conductive layer. Photolithography is performed according to the pre-designed mask pattern of the source electrode and the gate electrode. Then, the unexposed photoresist is developed and cleaned to remove it, exposing the non-source electrode and gate electrode areas. The metal conductive layer in the non-source electrode and gate electrode areas is cleaned by wet chemical etching with chemical reagents, leaving the source electrode and the gate electrode. Then, the remaining exposed photoresist is removed by another photoresist stripping solution, and then cleaned with deionized water. Finally, it is dried in a nitrogen environment to form a substrate with source electrodes and gate electrodes. Step 11: Formation of the substrate with drain electrode Based on step 10, a substrate with source and gate electrodes is selected and transferred to a wafer electroplating device. A multilayer composite metal conductive layer is electroplated on the lower surface of the substrate, including a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, a gold layer on the nickel layer, and a copper or aluminum layer in contact with the gold layer. Then, a negative photoresist is coated on the metal conductive layer, and exposure is performed using a photolithography machine with a mask pattern for the drain electrode. Here, the mask pattern for the drain electrode is the same as the mask pattern for the N-type buffer. Figure 1 The process involves developing and cleaning away the unexposed photoresist to expose the non-drain electrode area. The metal conductive layer in the non-drain electrode area is then cleaned away using a wet chemical etching technique with chemical reagents. The remaining exposed photoresist is then removed using another photoresist stripping solution. The area is then cleaned with deionized water and dried under a nitrogen atmosphere to form a substrate with a drain electrode, thus fabricating the VDMOS device. Beneficial effects
[0028] This invention utilizes a gallium oxide semiconductor substrate to fabricate an N-type heavily doped region, drain electrode, N-type buffer region, N-type well region, P-type heterodoped region, trench gate region, N-type source region, P-type source region, source electrode, and gate electrode. Combined with a multilayer trench gate region, including an auxiliary gate region and a gate region, a VDMOS chip is formed. This allows for a trench gate MOS device with an auxiliary gate, achieving better voltage withstand and other performance characteristics. In this device, a composite gate consisting of an auxiliary gate region and a gate region is used in the slotted gate region. The auxiliary gate region has a composite insulating layer structure of silicon dioxide and silicon oxynitride, which achieves good interface quality and low interface state density. The silicon oxynitride layer is placed on top of the silicon dioxide layer. Utilizing its high dielectric constant and dense microstructure, it effectively increases the equivalent barrier thickness of the gate dielectric layer and significantly reduces the gate leakage current under high voltage bias. At the same time, the silicon dioxide layer acts as a stress buffer layer, which alleviates the mechanical stress caused by lattice mismatch and thermal expansion coefficient difference between the silicon oxynitride layer and the substrate, avoids the generation of interface microcracks and crystal defects, and further improves the long-term operational reliability of the device. In this design, an auxiliary gate region is added to the upper surface of the gate region. This auxiliary gate region includes an auxiliary on / off region (an alternating NPN or PNP doped structure) and an auxiliary polysilicon layer. The gate electrode transfers electricity to the auxiliary polysilicon layer, then turns on the auxiliary on / off region. When the auxiliary N-type or auxiliary P-type region of the auxiliary on / off region is energized, it transfers power to the gate polysilicon layer in the gate region, thereby turning on the channel of the P-type hetero-doped region, and the VDMOS device will operate. Conversely, if the channel is not turned on, the VDMOS device will not function. The device will not function properly. Specifically, the P-type heterodoped region, N-type source region, P-type source region, and each doped region within the auxiliary gate region are symmetrically arranged around the centerline of the trench gate region. This ensures matching of the conduction channel length, parasitic resistance, and junction capacitance on both sides of the device. When the device is turned on, electron current flows symmetrically from the N-type source regions on both sides into the N-type well region, resulting in a uniform current density distribution. This improves the unilateral current congestion phenomenon, avoids hot spot effects, significantly reduces the risk of excessive local temperature rise, and extends the device's lifespan. Furthermore, the height of the P-type heterodoped region is less than the height of the N-type well region, resulting in a moderate junction depth between the P-type heterodoped region and the N-type well region, avoiding phenomena such as surface electric field concentration caused by excessive junction depth. An N-type buffer is set between the heavily doped N-type region and the N-type well region. The N-type buffer has a moderate doping concentration and thickness. On the one hand, it provides a low-resistance path for electron transport from the drain to the channel region, reducing the overall on-resistance of the device. On the other hand, the N-type buffer can alleviate the expansion rate of the depletion layer under high voltage turn-off conditions, absorb some electric field shocks, and protect the device, thus balancing low conduction loss and high voltage withstand performance.Its drain electrode, source electrode, and gate electrode are all made of mature metal materials such as aluminum or copper, and each electrode has the same thickness. This ensures good ohmic contact and conductive interconnection with the corresponding doped regions, while also taking into account thermal uniformity and compatibility with the deposition process. This reduces the complexity of the fabrication process and is conducive to large-scale production. Attached Figure Description
[0029] Figure 1 This is a schematic diagram of a gallium oxide-based VDMOS according to the present invention.
[0030] Figure 2 This is a schematic diagram of the fabrication process of a gallium oxide-based VDMOS according to the present invention.
[0031] Figure descriptions: 01. Drain electrode; 02. N-type heavily doped region; 03. N-type buffer zone; 04. N-type well region; 05. P-type hetero-doped region; 06. Gate insulating layer; 07. Gate polysilicon layer; 08. Auxiliary N-type electrode region; 09. Auxiliary P-type region; 10. Auxiliary N-type region; 11. P-type source region; 12. N-type source region; 13. Silicon dioxide layer; 14. SION layer; 15. Gate electrode; 16. Auxiliary polysilicon layer; 17. Right source electrode; 18. Left source electrode; 19. Auxiliary gate electrode. Detailed Implementation
[0032] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0033] See Figure 1 and Figure 2As shown, the present invention provides a gallium oxide-based VDMOS and its fabrication method. The gallium oxide-based VDMOS includes: a substrate, the substrate being made of gallium oxide semiconductor material; an N-type heavily doped region 02 on the bottom layer of the substrate; a drain electrode 01 on the lower surface of the N-type heavily doped region; an N-type buffer region 03 on the upper surface of the N-type heavily doped region; an N-type well region 04 on the upper surface of the N-type buffer region; a P-type hetero-doped region 05 and a trench gate region on the N-type well region; the P-type hetero-doped region being disposed on both sides of the trench gate region and in contact with the trench gate region; an N-type source region 12 and a P-type source region 11 on the P-type hetero-doped region; the N-type source region being in contact with the trench gate region; the P-type source region being in contact with the N-type source region and away from the trench gate region; source electrodes on the N-type source region and the P-type source region; a gate electrode on the trench gate region; and an electrode insulating layer between the source electrode and the trench gate region. The source electrodes include a right source electrode 17 and a left source electrode 18. The substrates are selected from 6-inch, 8-inch, and 12-inch sizes.
[0034] The slotted gate region includes an auxiliary gate region and a gate region. The auxiliary gate region is located on the upper surface of the gate region, and a gate electrode is provided on the upper surface of the auxiliary gate region. The auxiliary gate region is used to drive whether the gate region is charged, and the gate region is used to drive whether the P-type hetero-doped region is connected to the N-type source region and the N-type well region. The gate region includes a gate insulating layer 06 and a gate polysilicon layer 07. The gate insulating layer is located on the N-type well region, and a gate polysilicon layer is provided on the upper surface of the gate insulating layer. The auxiliary gate region is provided on the gate polysilicon layer. The gate insulating layer is selected from compound insulating materials. It can reduce gate leakage current, improve the withstand voltage and reliability of the insulating layer, etc. For example, silicon dioxide, etc. The gate polysilicon layer can be selected as heavily doped N+ type or P+ type. The auxiliary gate region includes an auxiliary on / off region, an auxiliary insulating layer, and an auxiliary polysilicon layer 16. The auxiliary on / off region is located on the upper surface of the gate region, and an auxiliary insulating layer is provided on the upper surface of the auxiliary on / off region. An auxiliary polysilicon layer is provided on the auxiliary insulating layer, and a gate electrode is provided on the auxiliary polysilicon layer. The auxiliary switching region includes an auxiliary gate electrode 19, which can be connected to an external power supply. The auxiliary insulating layer includes a silicon dioxide layer 13 and a SION layer 14. A silicon dioxide layer is located on the upper surface of the auxiliary switching region, and a SION layer is located on the silicon dioxide layer. An auxiliary polysilicon layer is located on the SION layer. The SION region is formed using silicon oxynitride. The auxiliary switching region includes an auxiliary N-type region 10, an auxiliary P-type region 09, and an auxiliary N-type electrode region 08. The auxiliary N-type region is located on the upper surface of the gate region. An auxiliary insulating layer and an auxiliary P-type region are located on the upper surface of the auxiliary N-type region. An auxiliary N-type electrode region is located on the upper surface of the auxiliary P-type region. The auxiliary insulating layer is in contact with the auxiliary N-type region, the auxiliary P-type region, and the auxiliary N-type electrode region. An auxiliary gate region is located on the upper surface of the auxiliary N-type region. The auxiliary gate region is selected as the auxiliary gate electrode 19. The auxiliary polysilicon layer can be a heavily doped N+ or P+ type.
[0035] The drain electrode, source electrode, and gate electrode are all provided with a metal composite layer between themselves and the substrate. The metal composite layer includes a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, and a gold layer on the nickel layer. The drain electrode, source electrode, and gate electrode are all of the same thickness.
[0036] Among them, the P-type hetero-doped region is symmetrically arranged with respect to the center line of the trench gate region; the N-type source region is symmetrically arranged with respect to the center line of the trench gate region; the P-type source region is symmetrically arranged with respect to the center line of the trench gate region; the auxiliary N-type region is symmetrically arranged with respect to the center line of the trench gate region; the auxiliary P-type region is symmetrically arranged with respect to the center line of the trench gate region; and the auxiliary N-type electrode region is symmetrically arranged with respect to the center line of the trench gate region. In this configuration, the height of the P-type heterodoped region is less than the height of the N-type well region. The height of the heavily doped N-type region is greater than the height of the N-type buffer region. The width of the drain electrode is greater than the width of the source electrode, which is greater than the width of the gate electrode. The width of the N-type source region is not less than the width of the P-type source region. The height of the P-type heterodoped region is less than the height of the N-type source region.
[0037] 15. Gate electrode; 16. Auxiliary polysilicon layer; 17. Right source electrode; 18. Left source electrode; 19. Auxiliary gate electrode.
[0038] The thickness of the heavily doped N-type region is 2.5 μm, and its doping concentration is 1.2 × 10⁻⁶. 18 cm -3 The N-type buffer has a thickness of 2 μm and a doping concentration of 3 × 10⁻⁶. 15 cm -3 The thickness of the N-type well region is 5 μm, and its doping concentration is 3.5 × 10⁻⁶. 15 cm -3 The thickness of the P-type heterodoped region is 700 nm, and its doping concentration is 3 × 10⁻⁶. 17 cm -3 The thickness of the N-type source region is 2 μm, and its doping concentration is 1 × 10⁻⁶. 18 cm -3 The thickness of the P-type source region is 2 μm, and its doping concentration is 6 × 10⁻⁶. 17 cm -3 The titanium layer of the metal composite layer is 30 nm, the aluminum layer is 120 nm, the nickel layer is 50 nm, the gold layer is 50 nm, and the copper layer is 200 nm; the thickness of the gate insulating layer (silicon dioxide) is 60 nm; the thickness of the gate polysilicon layer is 1 μm; the thickness of the auxiliary N-type region is 500 nm, the thickness of the auxiliary P-type region is 500 nm, the thickness of the auxiliary N-type region is 800 nm, the thickness of the auxiliary insulating layer is 50 nm, the thickness of SiON is 30 nm, and the thickness of the auxiliary polysilicon layer is 1.5 μm.
[0039] One method for fabricating a gallium oxide-based VDMOS includes the following steps: Step 1: Structural Design of VDMOS Devices The gallium oxide-based VDMOS includes: a substrate made of gallium oxide semiconductor material; an N-type heavily doped region on the bottom layer of the substrate; a drain electrode on the lower surface of the N-type heavily doped region; an N-type buffer region on the upper surface of the N-type heavily doped region; an N-type well region on the upper surface of the N-type buffer region; a P-type hetero-doped region and a trench gate region on the N-type well region; the P-type hetero-doped region being disposed on both sides of the trench gate region and in contact with the trench gate region; an N-type source region and a P-type source region on the P-type hetero-doped region, the N-type source region in contact with the trench gate region; the P-type source region in contact with the N-type source region and away from the trench gate region; source electrodes on the N-type and P-type source regions; a gate electrode on the trench gate region; and an electrode insulating layer between the source electrodes and the trench gate region. Step 2: Formation of the substrate with an N-type buffer Based on the structural design in step 1, a semiconductor wafer is selected as the substrate. The upper and lower surfaces of the substrate are cleaned to remove surface oxides and oil stains. RCA cleaning agent is used for cleaning, followed by rinsing with deionized water and drying in a nitrogen atmosphere. After drying, a layer of positive photoresist is coated on the lower surface of the substrate. The substrate is exposed using a photolithography machine according to a pre-designed mask pattern with an N-type buffer. The exposed photoresist area is then developed and removed to expose the N-type buffer. The substrate is then transferred to an N-type ion implanter. N-type ions are lightly doped into the N-type buffer from the lower surface of the substrate until the lower surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using a photoresist stripping solution, cleaned with deionized water, and dried in a nitrogen atmosphere to obtain a substrate with an N-type buffer. Step 3: Formation of a substrate with heavily doped N-type regions Based on step 2, on the substrate with an N-type buffer, and located at the lower part of the N-type buffer, N-type ions are heavily doped using an N-type ion implanter. The N-type ions are heavily doped into the lower part of the substrate with the N-type buffer and extend to the lower surface of the substrate. Then, the remaining unexposed photoresist is removed using a photoresist stripping solution, and then cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with a heavily doped N-type region. Step 4: Formation of the substrate with N-type well regions Based on step 3, a substrate with a heavily doped N-type region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the N-type well region. The exposed photoresist is then developed and cleaned to remove it, exposing the N-type well region. The substrate is then transferred to an N-type ion implanter, and N-type ions are lightly doped into the N-type well region from the upper surface of the substrate through the N-type ion implanter until the upper surface of the N-type buffer zone is reached. The remaining unexposed photoresist is then removed by photoresist stripping solution, and the substrate is cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with an N-type well region. Step 5: Formation of a substrate with p-type heterodoped regions Based on step 4, a substrate with an N-type well region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the P-type hetero-doped region. The exposed photoresist is then developed and cleaned to remove it, exposing the P-type hetero-doped region. The trench region of the P-type hetero-doped region is then etched out by dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed by photoresist stripping solution, and the substrate is cleaned with deionized water and dried in a nitrogen atmosphere. Then, the P-type hetero-doped region is deposited at room temperature using radio frequency magnetron sputtering technology with a NiO ceramic target in an Ar / O2 mixed atmosphere. At this time, the trench regions of the N-type source region and the P-type source region are still retained, forming a substrate with a P-type hetero-doped region. Step 6: Formation of the substrate with N-type source region Based on step 5, a substrate with a P-type hetero-doped region is selected. Then, using radio frequency magnetron sputtering technology with a Ga2O3 ceramic target, gallium oxide regions are deposited at room temperature in an Ar / O2 mixed atmosphere, filling the trenches of the N-type and P-type source regions. Then, the excess gallium oxide is ground off using CMP technology until the upper surface of the substrate is reached. A layer of positive photoresist is then coated on the upper surface of the substrate. Photolithography is performed according to the pre-designed mask pattern of the N-type source region. The exposed photoresist is then developed and cleaned to remove it, exposing the N-type source region. The substrate is then placed in an N-type ion implanter, and N-type ions are re-doped into the N-type source region from the upper surface of the substrate until the upper surface of the P-type hetero-doped region is reached. Then, the remaining unexposed photoresist is removed using a photoresist stripping solution, and the substrate is cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with an N-type source region. Step 7: Formation of the substrate with the P-type source region Based on step 6, a substrate with an N-type source region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the P-type source region. The exposed photoresist is then developed and cleaned to remove it, exposing the P-type source region. The trench area of the P-type source region is then etched out using dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using photoresist stripping solution, and the substrate is cleaned with deionized water. It is then dried in a nitrogen atmosphere. The P-type source region is then deposited using radio frequency magnetron sputtering technology with a Li-doped NiO ceramic target in an Ar / O2 mixed atmosphere. The excess Li-doped NiO and NiO are then ground off using CMP technology until the upper surface of the substrate is reached, thus forming the substrate with the P-type source region. Step 8: Formation of the substrate with the gate region in the trench gate region Based on step 7, a substrate with a P-type source region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. Photolithography is performed according to the pre-designed mask pattern of the grooved gate region. The exposed photoresist is then developed and cleaned to remove it, exposing the grooved gate region. The grooved gate region is then etched using dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using a photoresist stripping solution, followed by cleaning with deionized water and drying under nitrogen atmosphere. A silicon dioxide layer is then deposited on the inner wall of the grooved gate region using PECVD technology, and a polysilicon layer is deposited on the upper surface of the silicon dioxide layer to fill the grooved gate region. Then, the excess polysilicon and silicon dioxide layers are ground away using CMP technology until the upper surface of the substrate, i.e., the upper surface of the N-type source region, is reached. Next, a layer of positive photoresist is coated on the upper surface of the substrate. Photolithography is performed according to the mask pattern of the auxiliary gate region in the pre-designed grooved gate region. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary gate region in the grooved gate region. The groove region of the auxiliary gate region in the grooved gate region is then etched out using dry etching technology until the upper surface of the polysilicon layer is reached. The remaining unexposed photoresist is then removed using photoresist stripping solution, and the substrate is cleaned with deionized water and then dried in a nitrogen atmosphere. This process creates a substrate with the gate region in the grooved gate region. Step 9: Formation of the substrate for the auxiliary gate region in the slotted gate region Based on step 8, a substrate with a gate region in a grooved gate region is selected. Then, using RF magnetron sputtering technology with a Ga2O3 ceramic target, gallium oxide regions are deposited at room temperature in an Ar / O2 mixed atmosphere until the lower surface of the auxiliary P-type region is reached. Excess gallium oxide is then removed using CMP technology until the upper surface of the substrate is reached. A layer of positive photoresist is then coated on the upper surface of the substrate. Photolithography is performed according to a pre-designed mask pattern for the auxiliary N-type electrode region. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary N-type electrode region. This region is then placed in an N-type ion implanter, and N-type ions are re-implanted from the upper surface of the substrate into the auxiliary N-type electrode region until the upper surface of the polysilicon layer is reached. Then, [further details are needed for accurate translation]. The photoresist stripping solution removes the remaining unexposed photoresist, followed by cleaning with deionized water and drying in a nitrogen atmosphere. Then, using RF magnetron sputtering with a NiO ceramic target in an Ar / O2 mixed atmosphere, an auxiliary P-type region is deposited at room temperature. Excess NiO is then removed using CMP (Chemical Motion Processing) until the substrate surface is reached. Next, using RF magnetron sputtering with a Ga2O3 ceramic target in an Ar / O2 mixed atmosphere, a gallium oxide region is deposited at room temperature until the substrate surface is reached. Excess gallium oxide is then removed using CMP until the substrate surface is reached. Finally, a layer of positive photoresist is coated onto the substrate surface, and the pre-designed auxiliary N-type region is then applied. The mask pattern of the auxiliary N-type region is exposed using a photolithography machine. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary N-type region. This region is then placed in an N-type ion implanter, where N-type ions are re-implanted from the top surface of the substrate into the auxiliary N-type region, continuing until the top surface of the auxiliary P-type region. The remaining unexposed photoresist is then removed using a photoresist stripping solution, followed by cleaning with deionized water and drying under a nitrogen atmosphere. Next, a layer of positive photoresist is coated onto the top surface of the substrate. Based on the pre-designed mask pattern of the auxiliary insulating layer and auxiliary polysilicon layer in the trench gate region, the region is exposed using a photolithography machine. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary insulating layer and auxiliary polysilicon layer. Then, the trench areas of the auxiliary insulating layer and the auxiliary polysilicon layer are etched out using dry etching technology until the upper surface of the auxiliary N-type electrode region is reached. Then, the remaining unexposed photoresist is removed using photoresist stripping solution, and then cleaned with deionized water. After drying in a nitrogen environment, a silicon dioxide layer is deposited on the inner wall of the trench area of the auxiliary insulating layer and the auxiliary polysilicon layer using PECVD technology. A SION layer is deposited on the upper surface of the silicon dioxide layer, and then a polysilicon layer is deposited on the upper surface of the SION layer to fill the trench area of the trench gate region. Then, the excess polysilicon layer, SION layer and silicon dioxide layer are ground away using CMP technology until the upper surface of the substrate is reached, forming a substrate with a trench gate region. Step 10: Formation of the substrate with source and gate electrodes Based on step 9, a substrate with a grooved gate region is selected and transferred to a wafer electroplating device. A multilayer composite metal conductive layer is electroplated on the upper surface of the substrate, including a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, a gold layer on the nickel layer, and a copper or aluminum layer in contact with the gold layer. Then, a negative photoresist is coated on the metal conductive layer. Photolithography is performed according to the pre-designed mask pattern of the source electrode and the gate electrode. Then, the unexposed photoresist is developed and cleaned to remove it, exposing the non-source electrode and gate electrode areas. The metal conductive layer in the non-source electrode and gate electrode areas is cleaned by wet chemical etching with chemical reagents, leaving the source electrode and the gate electrode. Then, the remaining exposed photoresist is removed by another photoresist stripping solution, and then cleaned with deionized water. Finally, it is dried in a nitrogen environment to form a substrate with source electrodes and gate electrodes. Step 11: Formation of the substrate with drain electrode Based on step 10, a substrate with source and gate electrodes is selected and transferred to a wafer electroplating device. A multilayer composite metal conductive layer is electroplated on the lower surface of the substrate, including a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, a gold layer on the nickel layer, and a copper or aluminum layer in contact with the gold layer. Then, a negative photoresist is coated on the metal conductive layer, and exposure is performed using a photolithography machine with a mask pattern for the drain electrode. Here, the mask pattern for the drain electrode is the same as the mask pattern for the N-type buffer. Figure 1 The process involves developing and cleaning away the unexposed photoresist to expose the non-drain electrode area. The metal conductive layer in the non-drain electrode area is then cleaned away using a wet chemical etching technique with chemical reagents. The remaining exposed photoresist is then removed using another photoresist stripping solution. The area is then cleaned with deionized water and dried under a nitrogen atmosphere to form a substrate with a drain electrode, thus fabricating the VDMOS device.
[0040] The specific implementation principle of this invention patent is as follows: When the device is off, a high voltage is applied to the drain electrode, and the N-type heavily doped region, the N-type buffer region and the N-type well region jointly bear the reverse bias voltage. The N-type buffer serves two purposes: firstly, it provides a low-resistance path for electron transport from the drain to the channel region, reducing on-resistance; secondly, during high-voltage turn-off, the N-type buffer can mitigate the expansion rate of the depletion layer, absorb some electric field impacts, and prevent excessive concentration of the electric field at the junction of the P-type heterodoped region and the N-type well region, thereby improving the breakdown voltage of the device. In the on-state of the device, a forward driving voltage is applied to the gate electrode. This voltage is coupled to the auxiliary on-off region through the auxiliary polysilicon layer and the auxiliary insulating layer (silicon dioxide / SION composite layer) in sequence. The auxiliary on-off region adopts an alternating doping structure. When the potential of the auxiliary polysilicon layer reaches the threshold condition of the auxiliary on-off region, the auxiliary on-off region undergoes carrier modulation and conducts, transferring the potential to the lower gate polysilicon layer, thus charging the gate region. At this time, the gate insulating layer (preferably silicon dioxide) induces an inversion layer on the surface of the N-type well region, forming an electron conductive channel connecting the N-type source region and the N-type well region. Because the P-type hetero-doped region adopts a NiO / Ga2O3 heterojunction structure, its valence band shift forms a hole barrier on the Ga2O3 surface, effectively suppressing gate leakage current. Simultaneously, the NiO layer, as a hetero-P-type region, modulates the surface electric field together with the N-type well region, avoiding the channel control difficulties caused by the lack of shallow P-type doping in traditional gallium oxide devices. The P-type hetero-doped region, N-type source region, P-type source region, and each doped region within the auxiliary gate region are symmetrically arranged around the centerline of the slotted gate region. This symmetrical structure ensures a strict match between the conduction channel length, parasitic resistance, and junction capacitance on both sides of the device. During conduction, electron current flows symmetrically from the N-type source regions on both sides into the N-type well region, and then enters the drift region through the channel. The current density distribution is uniform, thereby improving the unilateral current congestion phenomenon, avoiding hot spot effects, significantly reducing the risk of excessive local temperature rise, and extending the device's lifespan. Meanwhile, the height of the P-type heterodoped region is smaller than that of the N-type well region, resulting in a moderate junction depth between the P-type heterodoped region and the N-type well region. This avoids the surface electric field concentration caused by excessive junction depth, making the surface electric field distribution smoother and further improving the breakdown voltage, thus preventing early avalanche breakdown. In addition, the trench gate region adopts a composite gate structure of auxiliary gate region and gate region. The auxiliary insulating layer in the auxiliary gate region is composed of silicon dioxide layer and SION layer. The silicon dioxide layer acts as a stress buffer layer, alleviating the mechanical stress caused by lattice mismatch and thermal expansion coefficient difference between SION layer and gallium oxide substrate, and avoiding the generation of interface microcracks and crystal defects. The SION layer, with its high dielectric constant and dense microstructure, effectively increases the equivalent barrier thickness of the gate dielectric layer, significantly reducing the risk of gate leakage current and tunneling current under high voltage bias, and improving the long-term operating reliability of the device.Achieving high withstand voltage, low on-resistance, uniform current distribution, and high gate reliability to meet the urgent needs of high-voltage power electronic systems for high-performance power devices.
[0041] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A gallium oxide-based VDMOS, characterized in that, The gallium oxide-based VDMOS includes: a substrate made of gallium oxide semiconductor material; an N-type heavily doped region on the bottom layer of the substrate; a drain electrode on the lower surface of the N-type heavily doped region; an N-type buffer region on the upper surface of the N-type heavily doped region; an N-type well region on the upper surface of the N-type buffer region; a P-type hetero-doped region and a trench gate region on the N-type well region; the P-type hetero-doped region being disposed on both sides of the trench gate region and in contact with the trench gate region; an N-type source region and a P-type source region on the P-type hetero-doped region; the N-type source region in contact with the trench gate region; the P-type source region in contact with the N-type source region but away from the trench gate region; source electrodes on the N-type and P-type source regions; a gate electrode on the trench gate region; and an electrode insulating layer between the source electrodes and the trench gate region.
2. The gallium oxide-based VDMOS according to claim 1, characterized in that, The slotted gate region includes an auxiliary gate region and a gate region. The auxiliary gate region is disposed on the upper surface of the gate region, and a gate electrode is provided on the upper surface of the auxiliary gate region. The auxiliary gate region is used to drive whether the gate region is charged. The gate region is used to drive whether the P-type heterodoped region is connected to the N-type source region and the N-type well region.
3. A gallium oxide-based VDMOS according to claim 2, characterized in that, The gate region includes a gate insulating layer and a gate polysilicon layer. The gate insulating layer is disposed on the N-type well region. The gate polysilicon layer is disposed on the upper surface of the gate insulating layer. The auxiliary gate region is disposed on the gate polysilicon layer.
4. A gallium oxide-based VDMOS according to claim 2, characterized in that, The auxiliary gate region includes an auxiliary on / off region, an auxiliary insulating layer, and an auxiliary polysilicon layer. The auxiliary on / off region is disposed on the upper surface of the gate region. The auxiliary insulating layer is disposed on the upper surface of the auxiliary on / off region. The auxiliary polysilicon layer is disposed on the auxiliary insulating layer. The gate electrode is disposed on the auxiliary polysilicon layer.
5. A gallium oxide-based VDMOS according to claim 4, characterized in that, The auxiliary insulating layer includes a silicon dioxide layer and a SION layer. The silicon dioxide layer is disposed on the upper surface of the auxiliary switching region. The SION layer is disposed on the silicon dioxide layer. The auxiliary polycrystalline silicon layer is disposed on the SION layer.
6. A gallium oxide-based VDMOS according to claim 4, characterized in that, The auxiliary switching region includes an auxiliary N-type region, an auxiliary P-type region, and an auxiliary N-type electrode region. The auxiliary N-type region is disposed on the upper surface of the gate region. The upper surface of the auxiliary N-type region is provided with the auxiliary insulating layer and the auxiliary P-type region. The upper surface of the auxiliary P-type region is provided with the auxiliary N-type electrode region. The auxiliary insulating layer is in contact with the auxiliary N-type region, the auxiliary P-type region, and the auxiliary N-type electrode region, respectively.
7. A gallium oxide-based VDMOS according to claim 1, characterized in that, The drain electrode, source electrode, and gate electrode are all provided with a metal composite layer between themselves and the substrate.
8. A gallium oxide-based VDMOS according to claim 1, characterized in that, The P-type heterodoped region is symmetrically arranged around the centerline of the grooved gate region.
9. A gallium oxide-based VDMOS according to claim 1, characterized in that, The N-type source region is symmetrically arranged with respect to the centerline of the slotted gate region.
10. A method for fabricating a gallium oxide-based VDMOS, characterized in that, The preparation method comprises the following steps: Step 1: Structural Design of VDMOS Devices The gallium oxide-based VDMOS includes: a substrate made of gallium oxide semiconductor material; an N-type heavily doped region on the bottom layer of the substrate; a drain electrode on the lower surface of the N-type heavily doped region; an N-type buffer region on the upper surface of the N-type heavily doped region; an N-type well region on the upper surface of the N-type buffer region; a P-type hetero-doped region and a trench gate region on the N-type well region; the P-type hetero-doped region being disposed on both sides of the trench gate region and in contact with the trench gate region; an N-type source region and a P-type source region on the P-type hetero-doped region, the N-type source region in contact with the trench gate region; the P-type source region in contact with the N-type source region and away from the trench gate region; source electrodes on the N-type and P-type source regions; a gate electrode on the trench gate region; and an electrode insulating layer between the source electrodes and the trench gate region. Step 2: Formation of the substrate with an N-type buffer Based on the structural design in step 1, a semiconductor wafer is selected as the substrate. The upper and lower surfaces of the substrate are cleaned to remove surface oxides and oil stains. RCA cleaning agent is used for cleaning, followed by rinsing with deionized water and drying in a nitrogen atmosphere. After drying, a layer of positive photoresist is coated on the lower surface of the substrate. The substrate is exposed using a photolithography machine according to a pre-designed mask pattern with an N-type buffer. The exposed photoresist area is then developed and removed to expose the N-type buffer. The substrate is then transferred to an N-type ion implanter. N-type ions are lightly doped into the N-type buffer from the lower surface of the substrate until the lower surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using a photoresist stripping solution, cleaned with deionized water, and dried in a nitrogen atmosphere to obtain a substrate with an N-type buffer. Step 3: Formation of a substrate with heavily doped N-type regions Based on step 2, on the substrate with an N-type buffer, and located at the lower part of the N-type buffer, N-type ions are heavily doped using an N-type ion implanter. The N-type ions are heavily doped into the lower part of the substrate with the N-type buffer and extend to the lower surface of the substrate. Then, the remaining unexposed photoresist is removed using a photoresist stripping solution, and then cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with a heavily doped N-type region. Step 4: Formation of the substrate with N-type well regions Based on step 3, a substrate with a heavily doped N-type region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the N-type well region. The exposed photoresist is then developed and cleaned to remove it, exposing the N-type well region. The substrate is then transferred to an N-type ion implanter, and N-type ions are lightly doped into the N-type well region from the upper surface of the substrate through the N-type ion implanter until the upper surface of the N-type buffer zone is reached. The remaining unexposed photoresist is then removed by photoresist stripping solution, and the substrate is cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with an N-type well region. Step 5: Formation of a substrate with p-type heterodoped regions Based on step 4, a substrate with an N-type well region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the P-type hetero-doped region. The exposed photoresist is then developed and cleaned to remove it, exposing the P-type hetero-doped region. The trench region of the P-type hetero-doped region is then etched out by dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed by photoresist stripping solution, and the substrate is cleaned with deionized water and dried in a nitrogen atmosphere. Then, the P-type hetero-doped region is deposited at room temperature using radio frequency magnetron sputtering technology with a NiO ceramic target in an Ar / O2 mixed atmosphere. At this time, the trench regions of the N-type source region and the P-type source region are still retained, forming a substrate with a P-type hetero-doped region. Step 6: Formation of the substrate with N-type source region Based on step 5, a substrate with a P-type hetero-doped region is selected. Then, using radio frequency magnetron sputtering technology with a Ga2O3 ceramic target, gallium oxide regions are deposited at room temperature in an Ar / O2 mixed atmosphere, filling the trenches of the N-type and P-type source regions. Then, the excess gallium oxide is ground off using CMP technology until the upper surface of the substrate is reached. A layer of positive photoresist is then coated on the upper surface of the substrate. Photolithography is performed according to the pre-designed mask pattern of the N-type source region. The exposed photoresist is then developed and cleaned to remove it, exposing the N-type source region. The substrate is then placed in an N-type ion implanter, and N-type ions are re-doped into the N-type source region from the upper surface of the substrate until the upper surface of the P-type hetero-doped region is reached. Then, the remaining unexposed photoresist is removed using a photoresist stripping solution, and the substrate is cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with an N-type source region. Step 7: Formation of the substrate with the P-type source region Based on step 6, a substrate with an N-type source region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. The substrate is exposed by a photolithography machine according to the pre-designed mask pattern of the P-type source region. The exposed photoresist is then developed and cleaned to remove it, exposing the P-type source region. The trench area of the P-type source region is then etched out using dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using photoresist stripping solution, and the substrate is cleaned with deionized water. It is then dried in a nitrogen atmosphere. The P-type source region is then deposited using radio frequency magnetron sputtering technology with a Li-doped NiO ceramic target in an Ar / O2 mixed atmosphere. The excess Li-doped NiO and NiO are then ground off using CMP technology until the upper surface of the substrate is reached, thus forming the substrate with the P-type source region. Step 8: Formation of the substrate with the gate region in the trench gate region Based on step 7, a substrate with a P-type source region is selected, and a layer of positive photoresist is coated on the upper surface of the substrate. Photolithography is performed according to the pre-designed mask pattern of the grooved gate region. The exposed photoresist is then developed and cleaned to remove it, exposing the grooved gate region. The grooved gate region is then etched using dry etching technology until the upper surface of the N-type well region is reached. The remaining unexposed photoresist is then removed using a photoresist stripping solution, followed by cleaning with deionized water and drying under nitrogen atmosphere. A silicon dioxide layer is then deposited on the inner wall of the grooved gate region using PECVD technology, and a polysilicon layer is deposited on the upper surface of the silicon dioxide layer to fill the grooved gate region. Then, the excess polysilicon and silicon dioxide layers are ground away using CMP technology until the upper surface of the substrate, i.e., the upper surface of the N-type source region, is reached. Next, a layer of positive photoresist is coated on the upper surface of the substrate. Photolithography is performed according to the mask pattern of the auxiliary gate region in the pre-designed grooved gate region. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary gate region in the grooved gate region. The groove region of the auxiliary gate region in the grooved gate region is then etched out using dry etching technology until the upper surface of the polysilicon layer is reached. The remaining unexposed photoresist is then removed using photoresist stripping solution, and the substrate is cleaned with deionized water and then dried in a nitrogen atmosphere. This process creates a substrate with the gate region in the grooved gate region. Step 9: Formation of the substrate for the auxiliary gate region in the slotted gate region Based on step 8, a substrate with a gate region in a grooved gate region is selected. Then, using RF magnetron sputtering technology with a Ga2O3 ceramic target, gallium oxide regions are deposited at room temperature in an Ar / O2 mixed atmosphere until the lower surface of the auxiliary P-type region is reached. Excess gallium oxide is then removed using CMP technology until the upper surface of the substrate is reached. A layer of positive photoresist is then coated on the upper surface of the substrate. Photolithography is performed according to a pre-designed mask pattern for the auxiliary N-type electrode region. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary N-type electrode region. This region is then placed in an N-type ion implanter, and N-type ions are re-implanted from the upper surface of the substrate into the auxiliary N-type electrode region until the upper surface of the polysilicon layer is reached. Then, [further details are needed for accurate translation]. The photoresist stripping solution removes the remaining unexposed photoresist, followed by cleaning with deionized water and drying in a nitrogen atmosphere. Then, using RF magnetron sputtering with a NiO ceramic target in an Ar / O2 mixed atmosphere, an auxiliary P-type region is deposited at room temperature. Excess NiO is then removed using CMP (Chemical Motion Processing) until the substrate surface is reached. Next, using RF magnetron sputtering with a Ga2O3 ceramic target in an Ar / O2 mixed atmosphere, a gallium oxide region is deposited at room temperature until the substrate surface is reached. Excess gallium oxide is then removed using CMP until the substrate surface is reached. Finally, a layer of positive photoresist is coated onto the substrate surface, and the pre-designed auxiliary N-type region is then applied. The mask pattern of the auxiliary N-type region is exposed using a photolithography machine. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary N-type region. This region is then placed in an N-type ion implanter, where N-type ions are re-implanted from the top surface of the substrate into the auxiliary N-type region, continuing until the top surface of the auxiliary P-type region. The remaining unexposed photoresist is then removed using a photoresist stripping solution, followed by cleaning with deionized water and drying under a nitrogen atmosphere. Next, a layer of positive photoresist is coated onto the top surface of the substrate. Based on the pre-designed mask pattern of the auxiliary insulating layer and auxiliary polysilicon layer in the trench gate region, the region is exposed using a photolithography machine. The exposed photoresist is then developed and cleaned to remove it, exposing the auxiliary insulating layer and auxiliary polysilicon layer. Then, the trench areas of the auxiliary insulating layer and the auxiliary polysilicon layer are etched out using dry etching technology until the upper surface of the auxiliary N-type electrode region is reached. Then, the remaining unexposed photoresist is removed using photoresist stripping solution, and then cleaned with deionized water. After drying in a nitrogen environment, a silicon dioxide layer is deposited on the inner wall of the trench area of the auxiliary insulating layer and the auxiliary polysilicon layer using PECVD technology. A SION layer is deposited on the upper surface of the silicon dioxide layer, and then a polysilicon layer is deposited on the upper surface of the SION layer to fill the trench area of the trench gate region. Then, the excess polysilicon layer, SION layer and silicon dioxide layer are ground away using CMP technology until the upper surface of the substrate is reached, forming a substrate with a trench gate region. Step 10: Formation of the substrate with source and gate electrodes Based on step 9, a substrate with a grooved gate region is selected and transferred to a wafer electroplating device. A multilayer composite metal conductive layer is electroplated on the upper surface of the substrate, including a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, a gold layer on the nickel layer, and a copper or aluminum layer in contact with the gold layer. Then, a negative photoresist is coated on the metal conductive layer. Photolithography is performed according to the pre-designed mask pattern of the source electrode and the gate electrode. Then, the unexposed photoresist is developed and cleaned to remove it, exposing the non-source electrode and gate electrode areas. The metal conductive layer in the non-source electrode and gate electrode areas is cleaned by wet chemical etching with chemical reagents, leaving the source electrode and the gate electrode. Then, the remaining exposed photoresist is removed by another photoresist stripping solution, and then cleaned with deionized water. Finally, it is dried in a nitrogen environment to form a substrate with source electrodes and gate electrodes. Step 11: Formation of the substrate with drain electrode Based on step 10, a substrate with source and gate electrodes is selected and transferred to a wafer plating apparatus. A multilayer composite metal conductive layer is electroplated on the lower surface of the substrate, including a titanium layer in contact with the substrate, an aluminum layer on the titanium layer, a nickel layer on the aluminum layer, a gold layer on the nickel layer, and a copper or aluminum layer in contact with the gold layer. Then, a negative photoresist is coated on the metal conductive layer, and exposure is performed using a photolithography machine with a mask pattern for the drain electrode. The mask pattern for the drain electrode is the same as that for the N-type buffer. Then, development and cleaning are performed to remove the non-exposed photoresist, exposing the non-drain electrode area. The metal conductive layer in the non-drain electrode area is cleaned by wet chemical etching with chemical reagents. Then, the remaining exposed photoresist is removed by another photoresist stripping solution, and then cleaned with deionized water. Finally, it is dried in a nitrogen atmosphere to form a substrate with a drain electrode; the VDMOS device is fabricated.