Semiconductor device and method of manufacturing the same
By forming isolation trenches in semiconductor devices and epitaxially growing extended portions on both sides of the long axis of the active region, the problem of ensuring the contact area after the size of semiconductor devices is reduced is solved, thereby increasing the active region area and improving the overlap margin, thus improving device reliability.
Patent Information
- Application Number
- CN202610058721.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-22
- Filing Date
- 2026-01-16
- Publication Date
- 2026-11-24
AI Technical Summary
As semiconductor device dimensions shrink, it becomes increasingly difficult to ensure the contact area connecting the upper and lower structures, and existing photolithography processes struggle to achieve linewidths of fine patterns that are at or below a specific critical dimension.
The active region is defined by forming an isolation trench in the substrate, and an extension portion with a crystal plane (100) is formed on both sides of the long axis of the active region by an epitaxial growth process to increase the top surface area of the active region. The active region is separated by a buried gate structure to form a junction region to increase the overlap margin.
This increases the contact area of the active region and the overlap margin between the upper and lower structures, thereby improving the reliability of semiconductor devices.
Smart Images

Figure CN123164822A_ABST
Abstract
Description
Cross-references to related applications
[0001] This patent application claims priority to Korean Patent Application No. 10-2025-0066961, filed on May 22, 2025, the entire contents of which are incorporated herein by reference. Technical Field
[0002] Various embodiments of this disclosure generally relate to semiconductor devices, and more specifically, to semiconductor devices having increased active region contact area and methods of manufacturing the same. Background Technology
[0003] As semiconductor device dimensions shrink and integration increases, methods for achieving fine patterns are constantly being improved. While new exposure equipment is being developed to achieve fine patterns in existing photolithography processes, realizing patterns with linewidths at or below a certain critical dimension remains a challenge.
[0004] Furthermore, as the size of semiconductor devices decreases, it becomes difficult to ensure the contact area connecting the upper and lower structures. Summary of the Invention
[0005] Various embodiments of this disclosure are intended to provide a semiconductor device and a method thereof capable of increasing the area of the active region contact area.
[0006] In one embodiment of this disclosure, the semiconductor device may include a substrate and a plurality of active regions defined in the substrate by isolation trenches, each active region having a long axis and a short axis and including an extension portion having a crystal plane (100) on both sides of the long axis.
[0007] In one embodiment disclosed herein, the semiconductor device may include: a plurality of active regions defined in a substrate by a device isolation layer, each active region including an extension portion on both sides of the long axis of the active region, the extension portion including a crystal plane (100), a trench configured to intersect the plurality of active regions and the device isolation layer, a buried gate structure gap-filled in the trench, and a junction region separated from the buried gate structure and formed on both sides of the long axis of each of the plurality of active regions and on the extension portion.
[0008] In one embodiment of this disclosure, a method of manufacturing a semiconductor device may include: forming a plurality of active regions by forming isolation trenches in a substrate, each active region having a long axis having a crystal plane (110), and forming extended portions having crystal planes (100) on both sides of the long axis of each active region by performing an epitaxial growth process to form a device isolation layer that fills the gaps in the isolation trenches.
[0009] In one embodiment of this disclosure, a method of manufacturing a semiconductor device may include: forming an isolation trench in a semiconductor substrate to define and electrically isolate active regions, each active region being oriented to have a long axis aligned with the crystal direction of a crystal plane (110) of the substrate; and forming an extension portion including a crystal plane (100) on both sides of each active region.
[0010] The embodiments of this disclosure can increase the top surface area of the active region and increase the overlap margin between the upper and lower structures.
[0011] The embodiments disclosed herein can further ensure the reliability of semiconductor devices. Attached Figure Description
[0012] Figure 1A and Figure 1B These are plan views and cross-sectional views of a semiconductor device according to an embodiment of the present disclosure.
[0013] Figure 2A-2D to Figures 7A-7C This is a process flow diagram used to describe a method for manufacturing a semiconductor device according to an embodiment of the present disclosure. Detailed Implementation
[0014] Various embodiments of this disclosure will be described with reference to cross-sectional views, plan views, and block diagrams (i.e., simplified schematic diagrams of embodiments). Therefore, the form of the figures may vary due to manufacturing processes and / or tolerances. Consequently, embodiments of this disclosure are not limited to the specific forms shown and may include variations in form resulting from manufacturing processes. Therefore, the areas shown in the figures have approximate properties, and the forms of the areas shown in the figures are only for illustrating the specific forms of device areas and are not intended to limit the scope of this disclosure. For clarity, the dimensions and relative dimensions of the components shown in the figures may be exaggerated. Throughout the specification, the same reference numerals denote the same components. "And / or" includes each item mentioned or all combinations of one or more items.
[0015] In this disclosure, when each layer (or film), region, electrode, pattern, or structure is described as being formed “on,” “above,” or “below” an object or substrate, it means that each layer (or film), region, electrode, pattern, or structure is formed directly above or below the substrate, layer (or film), region, or pattern, or that another layer (or film), region, electrode, pattern, or structure may be additionally formed on an object or substrate.
[0016] Figure 1A and Figure 1B These are plan views and cross-sectional views of a semiconductor device according to an embodiment of the present disclosure. Figure 1B It is along Figure 1A The cross-sectional view taken from the I-I' line.
[0017] like Figure 1A and Figure 1B As shown, according to one embodiment, the active region 103 may include extension portions 103e on both sides of the long axis of the active region, the extension portions 103e including crystal planes (100).
[0018] The active region 103 may be formed in the substrate 101. The active region 103 may be defined by the isolation trench 102T.
[0019] The active region 103 is composed of strips and can be arranged in an array. The array of active regions 103 may include a row array and / or a column array. The row array of active regions 103 may include active regions 103 arranged in a first direction D1. The column array of active regions 103 may include active regions 103 arranged in a second direction D2 orthogonal to the first direction D1. The active regions 103 may be arranged along a third direction D3.
[0020] Each active region 103 may have a major axis and a minor axis. The direction of the major axis of each active region 103 may be represented as the "length direction of each active region 103". The direction of the minor axis of each active region 103 may be represented as the "width direction of each active region 103". The length direction of the active region 103, i.e., the third direction D3, may form an angle θ with the first direction D1 and the second direction D2, rather than being orthogonal to the first direction D1 and the second direction D2. In one embodiment, the angle θ between the first direction D1 and the third direction D3 of each active region 103 may be 45°. Therefore, the crystal plane of the major axis of the active region 103 may be (110).
[0021] In another embodiment, the angle θ between the first direction D1 and the third direction D3 of each active region 103 may be approximately 10° to 80°, but these embodiments are not limited thereto. The range of the angle θ may be affected by parameters such as the area of each active region 103, the linewidth of the bit line, and the linewidth of the buried gate structure. The angle θ may be adjusted such that the crystal plane of the active region 103 along the long axis of the active region has a smaller growth rate than the crystal plane (100). Alternatively, the angle θ may be adjusted such that the crystal plane of the active region along the long axis of the active region has a faster etch rate than the growth rate.
[0022] Each active region 103 may include extension portions 103e on both sides of the active region, and the extension portions 103e include crystal planes (100). In this case, the crystal plane (100) may represent a plane without a tilt angle. The crystal plane (100) may be parallel to the first direction D1. In this case, the crystal plane (110) may represent a plane with a tilt angle of approximately 45°. The crystal plane (110) may be parallel to the third direction D3. The crystal plane (110) may be the crystal plane of the active region 103 along the long axis of the active region.
[0023] The active region 103 has junction regions on both sides of its long axis that connect to bit line contacts or memory node contacts. The area of the junction regions can be increased by adding the extended portion 103e formed by the crystal plane (100) on both sides of the long axis of the active region. Therefore, the overlap margin with the bit line contacts or memory node contacts can be increased, and the contact resistance can be reduced.
[0024] Figure 2A-2D to Figures 7A-7C This is a process flow diagram used to describe a method for manufacturing a semiconductor device according to an embodiment of the present disclosure. Figure 2A , Figure 3A , Figure 4A , Figure 5A , Figure 6A and Figure 7A It is a plan view used to describe a method of manufacturing a semiconductor device according to one embodiment. Figure 2B and Figure 2C , Figure 3B and Figure 3C , Figure 4B and Figure 4C , Figure 5B and Figure 5C , Figure 6B and Figure 6C as well as Figure 7B and Figure 7C This is a cross-sectional view used to describe a method of manufacturing a semiconductor device according to one embodiment. Figures 2A to 2C , Figures 3A to 3C , Figures 4A to 4C , Figures 5A to 5C , Figures 6A to 6C and Figures 7A to 7C They can represent the same technological operation. Figure 2B , Figure 3B , Figure 4B , Figure 5B , Figure 6B and Figure 7B They are along Figure 2A , Figure 3A , Figure 4A , Figure 5A , Figure 6A and Figure 7A The process cross-section diagram taken from line A-A' in the diagram. Figure 2C , Figure 3C , Figure 4C , Figure 5C , Figure 6C and Figure 7C It is along Figure 2A , Figure 3A , Figure 4A , Figure 5A , Figure 6A and Figure 7A The process cross-section diagram taken from the B-B' line. Figure 2D , Figure 3D and Figure 4D It is along Figure 2A , Figure 3A and Figure 4A The process cross-section diagram is taken from the C-C' line. For ease of understanding, please refer to... Figure 2A-2D to Figures 7A-7C Describe it.
[0025] like Figures 2A to 2D As shown, an isolation trench 12T defining an active region 13 can be formed in substrate 11. Substrate 11 can be a material suitable for semiconductor processing. Substrate 11 may include a semiconductor substrate. Substrate 11 may be made of a silicon-containing material. Substrate 11 may include silicon, monocrystalline silicon, polycrystalline silicon, amorphous silicon, silicon-germanium, monocrystalline silicon-germanium, polycrystalline silicon-germanium, carbon-doped silicon, combinations thereof, or multiples thereof. Substrate 11 may include another semiconductor material, such as germanium. Substrate 11 may include, for example, a group III / V semiconductor substrate, or a compound semiconductor substrate such as gallium arsenide (GaAs). Substrate 11 may include a silicon-on-insulator (SOI) substrate. In one embodiment, a flat region may be used. <100> The wafer serves as the wafer for forming substrate 11.
[0026] The active region 13 defined by the isolation trench 12T can be formed having a major axis and a minor axis. The active regions 13 can be arranged along a first direction D1 and a second direction D2 orthogonal to the first direction D1. Each active region 13 includes two long surfaces and two short surfaces opposite each other. Each active region 13 may include corners having a rounded parallelogram shape and can be arranged in an island configuration. That is, each active region 13 may include four rounded corners.
[0027] The major axis direction of each active region 13 can be represented as the "length direction of each active region 13". The minor axis direction of each active region 13 can be represented as the "width direction of each active region 13". The length direction of the active region 13, i.e., the third direction D3, can be inclined relative to the first direction D1 and the second direction D2. The third direction D3 can form an angle θ with the first direction D1 and the second direction D2 instead of being orthogonal to the first direction D1 and the second direction D2.
[0028] In one embodiment, the angle θ between the first direction D1 and the third direction D3 of each active region 13 is approximately 45°. Therefore, the crystal plane of the long axis of the active region 13 can be (110).
[0029] like Figures 3A to 3D As shown, an extended portion 13e, including a crystal plane (100), can be formed on both sides of the long axis of the active region 13.
[0030] The extended portion 13e can be formed through an epitaxial growth process. In the epitaxial growth process that forms the extended portion 13e, due to the difference in growth rate between the crystal planes (according to...), <111> < <110> < <311> < <100> The growth rate of crystal facet (100) is faster than that of another crystal facet. The growth of crystal facet (100) on both sides of the long axis of the active region 13 can be faster than that of another crystal facet. Crystal facet (100) can represent a plane parallel to the first direction D1. In this embodiment, (100) represents a crystal facet, which represents the plane of the crystal being grown; <100> It indicates the crystallization direction, representing the direction perpendicular to the crystal plane, i.e., the direction of crystal growth.
[0031] Epitaxial growth processes can be performed in an atmosphere containing chlorine. For example, epitaxial growth processes can be performed using silicon (Si) source gas and hydrogen chloride (HCl). When using an epitaxial growth process including silicon source gas and hydrogen chloride, due to the difference in etch rate with chlorine (Cl) (according to...), <111> > <110> > <311> > <100> (In the order of crystal plane (100), the etching rate of the crystal plane (100) is slower than that of the other crystal plane), and the growth rate of the crystal plane (100) can be faster than that of the crystal plane (110).
[0032] In another embodiment, the epitaxial growth process may be performed using a chlorine-containing (Cl) silicon source gas. For example, chlorine-containing silicon source gases may include monochlorosilane (SiH3Cl), dichlorosilane (SiH2Cl2), and trichlorosilane (SiHCl3), but embodiments of this disclosure are not limited to these. Chlorine-containing silicon source gases can have the same effects as epitaxial growth processes using silicon source gases and hydrogen chloride.
[0033] In another embodiment, a precursor containing Si, H and Cl can be used in the epitaxial growth process.
[0034] In addition, to further increase the difference in growth rate based on the crystal facet, chlorine precursors, such as HCl and Cl2, can be used after etching begins.
[0035] Both sides of the long axis of the active region 13 are junction regions connected to the bit line contacts and the memory node contacts. The area of the junction regions can be increased by the extension portion 13e.
[0036] As a comparative example, if a polysilicon growth process is performed instead of an epitaxial growth process, the spacing between adjacent active regions 13 only narrows because the crystal plane grows along the contour of the active region 13 without any change. Therefore, the area increase effect of the junction region may not be expected.
[0037] Figure 3C The cross-sectional view taken along line B-B' is the cross-sectional view intersecting the active region 13 along the major axis. The extended portion 13e may have a second width W2.
[0038] Figure 3D The cross-sectional view taken along line C-C' is the cross-sectional view intersecting the end of the active region 13 along the second direction D2. The extended portion 13e may have a first width W1. The first width W1 may be greater than the second width W2.
[0039] like Figures 4A to 4D As shown, the component isolation layer 12 can be formed by filling the isolation trench 12T with gaps filled with insulating material. To achieve effective isolation, the trench 12T is filled with insulating material, which may include, for example, silicon dioxide (SiO2), silicon nitride (Si3N4), or a composite stack including both materials. These materials are chosen because they have excellent dielectric properties, thermal stability, and compatibility with manufacturing processes.
[0040] In one embodiment, after depositing insulating material in trench 12T, the insulating material can be thermally annealed to reduce stress and improve film quality. Excess material above the trench can be removed by chemical mechanical polishing (CMP) to obtain a smooth surface, facilitating subsequent photolithography operations.
[0041] like Figures 5A to 5C As shown, the first hard mask layer 14 can be formed on the active region 13 and the component isolation layer 12.
[0042] The first hard mask layer 14 may have a line shape extending along a first direction D1 and isolated in a second direction D2. The first hard mask layer 14 may include an insulating material having etch selectivity for the active region 13 and the component isolation layer 12. The first hard mask layer 14 may have a single-layer structure or a stacked structure. The stacked structure of the first hard mask layer 14 may include insulating materials with different etch selectivity.
[0043] like Figures 6A to 6C As shown, by using the first hard mask layer 14 as an etch barrier layer to etch the active region 13 and the component isolation layer 12, a trench 15 extending along the first direction D1 can be formed.
[0044] A trench 15 may be formed in each active region 13. The trench 15 may intersect the center of each active region 13. The trenches 15 may be spaced apart from each other in a second direction D2. The depth of the trench 15 may be shallower than the depth of the device isolation layer 12. That is, the bottom surface of the trench 15 may be at a level higher than the bottom surface of the device isolation layer 12. In another embodiment (not shown), the lower part of the trench 15 may have curvature. In one embodiment, the trench 15 is a space for forming a buried gate structure and may be referred to as "gate trench 15".
[0045] like Figures 7A to 7C As shown, a gate insulating layer 16 can be formed covering the inner surface of the trench 15.
[0046] The gate insulating layer 16 may be conformally formed on the bottom surface and inner wall of the trench 15.
[0047] The gate insulating layer 16 may include silicon oxide, silicon nitride, silicon oxynitride, a high-k material, or a combination thereof. The high-k material may include a material with a dielectric constant greater than that of silicon dioxide. For example, the high-k material may include a material with a dielectric constant greater than about 3.9. In another embodiment, the high-k material may include a material with a dielectric constant greater than about 10. In another embodiment, the high-k material may include a material with a dielectric constant of about 10 to about 30. The high-k material may include a metallic element. The high-k material may include a hafnium-containing material. Such a hafnium-containing material may include hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, or a combination thereof. In another embodiment, the high-k material may include lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, zirconium silicon oxide, zirconium oxynitride, aluminum oxide, or a combination thereof. Other known high-k materials may also be used selectively. The gate insulating layer 16 may include a metal oxide.
[0048] Next, a buried gate structure can be formed by sequentially stacking a buried conductive layer 17 and a gate capping layer 18 on the gate insulating layer 16.
[0049] The buried conductive layer 17 may be referred to as "gate electrode 17". The buried conductive layer 17 may be a low-resistance material to reduce the resistance of the gate thin layer. The buried conductive layer 17 may include semiconductor materials, metal-based materials, or combinations thereof. The buried conductive layer 17 may include polysilicon, metal, metal oxide, or combinations thereof. For example, the buried conductive layer 17 may include N-type doped polysilicon, tantalum nitride (TaN), titanium nitride (TiN), tungsten (W), tungsten nitride (WN), molybdenum (Mo), ruthenium (Ru), or combinations thereof. In another embodiment, the buried conductive layer 17 may be formed of only titanium nitride or only molybdenum. In another embodiment, the buried conductive layer 17 may be formed of a stack of titanium nitride and tungsten (i.e., TiN / W) or a stack of titanium nitride and polysilicon (i.e., TiN / polysilicon).
[0050] In another embodiment, a dual-gate structure including an upper gate and a lower gate can be applied to the buried conductive layer 17. In yet another embodiment, a triple-gate structure including an upper gate, a middle gate, and a lower gate can be applied to the buried conductive layer 17.
[0051] In another embodiment, the embedded conductive layer 17 may have a high work function. In this case, a high work function refers to a work function higher than the intermediate bandgap work function of silicon. A low work function refers to a work function lower than the intermediate bandgap work function of silicon. Incidentally, a high work function may have a work function higher than about 4.5 eV. A low work function may have a work function lower than about 4.5 eV. The embedded conductive layer 17 may include p-type polycrystalline silicon or nitrogen-rich titanium nitride (TiN).
[0052] In another embodiment, the buried conductive layer 17 may have an increased work function. The buried conductive layer 17 may include metal silicon nitride. Metal silicon nitride can be formed by doping a metal nitride with silicon. The buried conductive layer 17 may include metal silicon nitride with an adjusted silicon content. For example, the buried conductive layer 17 may include tantalum silicon nitride (TaSiN) or titanium silicon nitride (TiSiN). Titanium nitride (TiN) may have a high work function and may contain silicon to further improve the work function of titanium nitride (TiN). The silicon content of titanium silicon nitride (TiSiN) can be adjusted to have an increased high work function. In another embodiment, the buried conductive layer 17 may include titanium aluminum nitride (TiAlN).
[0053] The gate capping layer 18 serves to protect the buried conductive layer 17. The gate capping layer 18 can be formed by filling the upper portion of the trench 15 on the buried conductive layer 17. The top surface of the gate capping layer 18 may be at the same level as the top surfaces of the first and second junction regions 19 and 20. The gate capping layer 18 may include an insulating material. The gate capping layer 18 may include silicon nitride, silicon oxynitride, or a combination thereof. In another embodiment, the gate capping layer 18 may include a combination of silicon nitride and silicon oxide. The gate capping layer 18 may include a silicon nitride pad and a spin-on dielectric layer (SOD).
[0054] Next, first and second junction regions 19 and 20 may be formed in the substrate 11 on both sides of the trench 15.
[0055] This embodiment can increase the area of each of the first and second junction regions 19 and 20 because additional extension portions 13e are formed on both sides of the long axis of the active region 13. Therefore, the overlap margin with the substrate 11 and the upper structure (e.g., bit lines or memory elements) can be increased.
[0056] The first and second junction regions 19 and 20 may not be arranged in a straight line along the second direction D2. The first and second junction regions 19 and 20 may be arranged alternately on both sides, so that there is no overlapping area in the second direction D2.
[0057] The first and second junction regions 19 and 20 are each regions doped with their respective conductive dopants. For example, the conductive dopants may include phosphorus (P), arsenic (As), antimony (Sb), or boron (B). The first and second junction regions 19 and 20 may be doped with dopants having the same conductivity type. The first and second junction regions 19 and 20 may be configured to be isolated from each other by trench 15. The bottom surfaces of both the first and second junction regions 19 and 20 may be disposed at a predetermined depth from the top surface of the substrate 11. The bottom surfaces of both the first and second junction regions 19 and 20 may be higher than the bottom surface of the trench 15. The first junction region 19 may be referred to as "source region 19", "first impurity region 19", "first doped region 19", or "first junction region 19". The second junction region 20 may be referred to as "drain region 20", "second impurity region 20", "second doped region 20", or "second junction region 20".
[0058] The buried gate structure may consist of a gate insulating layer 16, a buried conductive layer 17, and a gate capping layer 18 sequentially interleaved within a trench 15. A channel may be defined between the first and second junction regions 19 and 20 by the buried gate structure. The channel may be defined along the contour of the trench 15.
[0059] As a subsequent process, a bit line BL electrically connected to the first junction region 19 and a memory storage element CAP electrically connected to the second junction region 20 can be formed.
[0060] Bit line BL can be electrically connected to the first junction region 19 via bit line contact 21. Memory storage element CAP can be electrically connected to the second junction region 20 via storage node contact 22.
[0061] The bit line BL and the memory storage element CAP can be located at a level higher than the buried gate structure. The bit line BL and the memory storage element CAP can be located at different levels. The memory storage element CAP can be located at a level higher than the bit line BL. The memory storage element CAP may include a capacitor. In another embodiment, the memory storage element CAP may be a thyristor, a phase change material, a magnetic tunnel junction (MTJ), or a variable resistance material.
[0062] refer to Figure 2A-2D to Figures 7A-7CThe semiconductor device may include multiple memory cells. Adjacent memory cells may be isolated by a component isolation layer 12. A memory cell may be formed on an active region 13, which may be represented as "a memory cell having a gate and an active region (1G1A) structure". In a memory cell with a 1G1A structure, a memory cell may be connected to a bit line BL, because the bit line BL is connected to an active region 13. A memory cell with a 1G1A structure may include a transistor and a capacitor (1T1C). As a comparative example, in a typical DRAM, two memory cells are formed in an active region, two gate electrodes are formed in an active region, and two adjacent memory cells share a bit line.
[0063] While various embodiments have been described for ease of illustration, those skilled in the art will understand that various changes and modifications can be made without departing from the technical concept and scope of this disclosure as defined in the following claims. Furthermore, these embodiments can be combined to form other embodiments.
Claims
1. A semiconductor device, comprising: Substrate; and Multiple active regions are defined in the substrate by isolation trenches, each active region having a long axis and a short axis, and including extended portions having crystal planes (100) on both sides of the long axis.
2. The semiconductor device according to claim 1, wherein, The crystal plane of the long axis of each of the plurality of active regions is (110).
3. The semiconductor device according to claim 2, wherein, The plurality of active regions are spaced apart from each other along a first direction and a second direction orthogonal to the first direction.
4. The semiconductor device according to claim 3, wherein, The major axis of each of the plurality of active regions has an inclination angle of approximately 45° relative to the first direction or the second direction.
5. A semiconductor device, comprising: Multiple active regions are defined in a substrate by a device isolation layer, each active region including an extension portion on both sides of the long axis of the active region, the extension portion including a crystal plane (100); The trench intersects with the plurality of active regions and the element isolation layer; An embedded gate structure, the gaps of which fill the trench; and The junction region is separated by the buried gate structure and formed on both sides of the long axis of each of the plurality of active regions and on the extended portion.
6. The semiconductor device according to claim 5, wherein: Each of the plurality of active regions has the major axis and the minor axis, and The crystal plane of the long axis of each of the plurality of active regions is (110).
7. The semiconductor device according to claim 5, wherein, The plurality of active regions are spaced apart from each other in a first direction and in a second direction orthogonal to the first direction.
8. The semiconductor device according to claim 7, wherein, The major axis of each of the plurality of active regions has a tilt angle of 45° relative to the first direction or the second direction.
9. The semiconductor device according to claim 5, wherein, The trench extends along the first direction.
10. The semiconductor device according to claim 5, wherein, The junction region includes a first junction region and a second junction region disposed on both sides of the long axis of the active region.
11. The semiconductor device of claim 10, further comprising: Bit lines are formed on the substrate and connected to the first junction region; and A storage element is formed on the substrate and connected to the second junction region.
12. A method for manufacturing a semiconductor device, the method comprising: Multiple active regions are formed by forming isolation trenches in the substrate, each active region having a long axis having a crystal plane (110). An extended portion having a crystal plane (100) is formed on both sides of the long axis of each active region by performing an epitaxial growth process; as well as A component isolation layer is formed, and the gaps in the component isolation layer fill the isolation trench.
13. The method of claim 12, further comprising: After the extended portion is formed, a trench is formed that intersects with the active region and the component isolation layer; An embedded gate structure is formed, wherein the gaps in the embedded gate structure are filled in the trench; as well as A first junction region and a second junction region, separated by the buried gate structure, are formed on both sides of the long axis of each of the plurality of active regions and in the extended portion.
14. The method of claim 13, further comprising: A bit line connected to the first junction region is formed on the substrate; as well as A memory element connected to the second junction region is formed on the substrate.
15. The method according to claim 12, wherein, The active regions are spaced apart from each other along a first direction and a second direction orthogonal to the first direction.
16. The method according to claim 15, wherein, The major axis of each of the plurality of active regions has a tilt angle of 45° relative to the first direction or the second direction.
17. The method according to claim 12, wherein, The epitaxial growth process is performed using a gas containing silicon (Si), hydrogen (H), and chloride (Cl).
18. The method according to claim 12, wherein, The epitaxial growth process is performed using a mixture of SiH4 and HCl gas.
19. The method according to claim 12, wherein, The epitaxial growth process is performed using a silicon source gas containing chlorine (Cl), which is selected from monochlorosilane (SiH3Cl), dichlorosilane (SiH2Cl2), and trichlorosilane (SiHCl3).
20. A method for manufacturing a semiconductor device, the method comprising: Isolation trenches are formed in a semiconductor substrate to define and electrically isolate active regions, each active region being oriented to have a long axis aligned with the crystal direction of the crystal plane (110) of the substrate; as well as An extended portion including a crystal plane (100) is formed on both sides of each active region.
Citation Information
Patent Citations
Double Protection of Bottle Lid and Main Body
KR1020250066961A