A semiconductor device and a method of fabricating the same

By forming a patterned mask layer on the substrate of a MOS device and performing multi-window lightly doped drain ion implantation, the problem of threshold voltage regulation of MOS devices in small sizes is solved, and the differentiated control of threshold voltage and performance improvement of long and short channel devices are realized.

CN123164833APending Publication Date: 2026-11-24RONGXIN SEMICON (HUAIAN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611395693.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-09
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

As the gate size of metal-oxide-semiconductor (MOS) devices decreases, the short-channel effect becomes severe, and existing technologies struggle to effectively regulate the threshold voltage, leading to device performance degradation and reliability issues.

Method used

A patterned mask layer is formed on the substrate, and lightly doped drain ions are implanted through multiple implantation windows arranged at intervals to form a lightly doped drain region of a long and short channel MOS device. LDD implantation is completed before the gate structure is formed, and the threshold voltage is adjusted by utilizing the compensation effect of the mask layer.

Benefits of technology

It effectively reduces the threshold voltage difference between long and short channel MOS devices, suppresses the short channel effect, and improves device performance and reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123164833A_ABST
    Figure CN123164833A_ABST
Patent Text Reader

Abstract

This invention provides a semiconductor device and a method for fabricating the same, comprising: providing a substrate, the substrate including a first MOS device region and a second MOS device region, respectively used to form a long-channel MOS device and a short-channel MOS device; performing a first doping type of well ion implantation on the substrate to form a first well region and a second well region; forming a patterned mask layer on the substrate, the patterned mask layer having a first implantation window exposing the edge region of the first well region, a plurality of spaced second implantation windows exposing the middle region of the first well region, and a third implantation window exposing the edge region of the second well region; and performing a second doping type of lightly doped drain ion implantation on the substrate through the implantation windows to form a first lightly doped drain region in the first well region and a second lightly doped drain region in the second well region. This invention can reduce the difference between the threshold voltages of long-channel and short-channel devices; and simultaneously makes the implantation parameters of the LDD not limited by the gate thickness / length.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor technology, and more specifically to a semiconductor device and its fabrication method. Background Technology

[0002] As the gate size of metal-oxide-semiconductor (MOS) devices continues to shrink, the length of the conductive channel beneath the gate also decreases. When the length of the conductive channel shrinks to a certain range, it leads to short-channel effects, including drain-induced barrier lowering (DIBL) and source-drain punch-through.

[0003] In existing technologies, lightly doped drain (LDD) and pocket implant drain techniques are commonly used to reduce the junction depth of the PN junction and suppress the DIBL effect, thereby improving the performance of MOS devices. However, with the further reduction in device size, relying solely on LDD and pocket implant drain techniques is no longer sufficient to meet the performance requirements of MOS devices.

[0004] To address this issue, related technologies have proposed a threshold voltage regulation (VT) injection technique on the conductive channel surface, which adjusts the threshold voltage (VT) of the MOS device by controlling the injection dose and injection depth. However, for small-sized devices, the thickness of the gate polysilicon is continuously decreasing, the effective channel length of the device is shrinking, and the short-channel effect is becoming increasingly severe. This leads to a decrease in the LDD ion implantation energy of high-voltage devices, resulting in device performance degradation and problems such as increased junction leakage current, enhanced hot carrier injection (HCI), and decreased breakdown voltage (BV).

[0005] While increasing the LDD injection dose can improve the above situation to some extent, due to the limitation of gate length, increasing the LDD injection dose will gradually increase the threshold voltage gap between long-channel MOS devices and short-channel MOS devices, ultimately affecting device reliability and causing device performance degradation. Summary of the Invention

[0006] The summary section introduces a series of simplified concepts, which will be further explained in detail in the detailed description section. The summary section of this invention is not intended to limit the key features and essential technical features of the claimed technical solution, nor is it intended to determine the scope of protection of the claimed technical solution.

[0007] To address the existing problems, one embodiment of the present invention provides a method for fabricating a semiconductor device, comprising: A substrate is provided, the substrate including a first MOS device region and a second MOS device region, the first MOS device region being used to form a long-channel MOS device, and the second MOS device region being used to form a short-channel MOS device; A first type of doping trap ion implantation is performed on the substrate to form a first well region in the first MOS device region and a second well region in the second MOS device region; A patterned mask layer is formed on the substrate, wherein a first injection window is formed in the patterned mask layer to expose the edge region of the first well region, a plurality of second injection windows arranged at intervals to expose the middle region of the first well region, and a third injection window to expose the edge region of the second well region. Using the patterned mask layer as a mask, a second type of light doping drain ion implantation is performed on the substrate to form a first lightly doped drain region in the first well region through the first implantation window and the second implantation window, and a second lightly doped drain region in the second well region through the third implantation window; Remove the patterned mask layer.

[0008] In one embodiment, after removing the patterned mask layer, the method further includes: A first gate structure is formed above the first well region, and a second gate structure is formed above the second well region. The length of the first gate structure is greater than or equal to the length of the patterned mask layer formed above the first well region, and the length of the second gate structure is greater than or equal to the length of the patterned mask layer formed above the second well region. Using the first gate structure as a mask, the substrate is subjected to ion implantation of the second doping type to form a first source / drain region in the first well region and a second source / drain region in the second well region.

[0009] In one embodiment, when the long-channel MOS device and the short-channel MOS device are NMOS devices, the first doping type is P-type and the second doping type is N-type; when the long-channel MOS device and the short-channel MOS device are PMOS devices, the first doping type is N-type and the second doping type is P-type.

[0010] In one embodiment, the second injection windows are arranged at equal intervals in the channel width direction.

[0011] In one embodiment, the spacing of the second injection windows in the channel width direction is 0.01 μm to 5 μm.

[0012] In one embodiment, the height of the mask layer is from 0.1 μm to 5 μm.

[0013] In one embodiment, when the long-channel MOS device and the short-channel MOS device are PMOS devices, the implanted ions for the lightly doped drain ion implantation are boron, boron fluoride, or indium, the implantation angle is 0° to 45°, the implantation energy is 3 keV to 80 keV, and the implantation dose is 1.0e12 cm⁻¹. -2 up to 5.0e14 cm -2 ; When the long-channel MOS device and the short-channel MOS device are NMOS devices, the implanted ions are phosphorus or arsenic, the implantation angle is 0° to 45°, the implantation energy is 3 keV to 80 keV, and the implantation dose is 1.0e12 cm⁻¹. -2 up to 5.0e14 cm -2 .

[0014] In one embodiment, performing trap ion implantation of the first doping type on the substrate includes: First-trap ion implantation is performed at implantation energies ranging from 100 keV to 1000 keV; Second trap ion implantation is performed at implantation energies ranging from 50 keV to 500 keV; Third-trap ion implantation was performed at implantation energies ranging from 10 keV to 200 keV.

[0015] In one embodiment, the ion implantation concentration of the third well ion implantation is 1.0e12cm. -2 -9.0e13cm -2 .

[0016] In one embodiment, the mask layer includes a photoresist layer.

[0017] Another aspect of the present invention provides a semiconductor device prepared using the above-described method.

[0018] The semiconductor device and its fabrication method provided by this invention perform LDD ion implantation on a long-channel MOS device through multiple implantation windows arranged at intervals. This can neutralize and reduce the doping concentration on the channel surface of the long-channel MOS device. Under the condition that the threshold voltage of each long and short channel device meets the performance requirements, the VT gap between the long and short channel devices is effectively reduced. At the same time, by advancing the LDD implantation to before the gate formation, the implantation parameters are not limited by the gate thickness / length, suppressing the short-channel effect and improving the device performance. Attached Figure Description

[0019] The above and other objects, features, and advantages of the present invention will become more apparent from the more detailed description of the embodiments of the invention in conjunction with the accompanying drawings. The drawings are provided to further illustrate the embodiments of the invention and form part of the specification. They are used together with the embodiments of the invention to explain the invention and do not constitute a limitation thereof. In the drawings, the same reference numerals generally represent the same parts or steps.

[0020] In the attached image: Figure 1A-Figure 1B A schematic cross-sectional view of a semiconductor device obtained by sequentially performing each step of a semiconductor device fabrication method in the related art is shown. Figure 2 A flowchart illustrating a method for fabricating a semiconductor device according to an exemplary embodiment of the present invention is shown; Figures 3A-3D A cross-sectional schematic diagram of a semiconductor device obtained by sequentially performing each step of the semiconductor device fabrication method according to an embodiment of the present invention is shown. Figure 4 Simulation comparison diagrams of long-channel MOS devices based on related technologies and the present invention are shown; Figure 5 Simulation comparison diagrams of short-channel MOS devices based on related technologies and the present invention are shown; Figure 6 A comparison graph of the active doping concentration curves of short-channel MOS devices of related technologies and the present invention is shown. Detailed Implementation

[0021] In the following description, numerous specific details are set forth in order to provide a more thorough understanding of the invention. However, it will be apparent to those skilled in the art that the invention can be practiced without one or more of these details. In other instances, certain technical features well-known in the art have not been described in order to avoid obscuring the invention.

[0022] It should be understood that the invention can be embodied in various forms and should not be construed as being limited to the embodiments set forth herein. Rather, providing these embodiments will make the disclosure thorough and complete, and will fully convey the scope of the invention to those skilled in the art. In the drawings, for clarity, the dimensions and relative dimensions of layers and regions may be exaggerated. The same reference numerals denote the same elements throughout.

[0023] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this invention, the first element, component, area, layer, or portion discussed below may be referred to as the second element, component, area, layer, or portion.

[0024] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below” or “under” the other element or feature will be oriented “above” the other element or feature. Therefore, the exemplary terms “below” and “under” can include both upper and lower orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.

[0025] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the invention. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising” and / or “including,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.

[0026] Unless otherwise defined, all terms used herein (including technical and scientific terms) shall have the same meaning as commonly understood by one of ordinary skill in the art. It will also be understood that terms as defined in commonly used dictionaries shall be construed as having the meaning consistent with their meaning in the relevant field and / or the context of this specification, and shall not be interpreted in an ideal or overly formal sense, unless expressly defined herein.

[0027] To fully understand this invention, detailed steps and structures will be set forth in the following description to illustrate the technical solution proposed by this invention. Preferred embodiments of the invention are described in detail below; however, in addition to these detailed descriptions, the invention may have other embodiments.

[0028] Figure 1A and Figure 1B The process for forming the LDD region in the related art is illustrated. First, as... Figure 1A As shown, a substrate 100 is provided, in which shallow trench isolation structures 101 are formed, and active regions of MOS devices are defined between adjacent shallow trench isolation structures 101; then, well regions 102 are formed in the active regions by ion implantation; then, a gate dielectric layer 103 and a gate electrode layer 104 are formed above the well regions 102. Next, as... Figure 1B As shown, LDD ion implantation is performed using the gate electrode layer 104 and the gate dielectric layer 103 as masks, forming LDD regions 105 on both sides.

[0029] In the above process, LDD ion implantation is performed after the formation of the gate electrode layer 104 and the gate dielectric layer 103, using the gate electrode layer 104 as a self-aligned mask. However, as device dimensions continue to decrease, the thickness of the gate electrode layer 104 also decreases, and the LDD implantation energy is limited by the gate thickness and cannot be flexibly adjusted. Furthermore, the threshold voltage gap (VT gap) between long-channel MOS devices and short-channel MOS devices increases with the decrease in channel size, affecting device performance.

[0030] Therefore, in view of the aforementioned technical problems, the present invention proposes a method for fabricating a semiconductor device, such as... Figure 2 As shown, it mainly includes the following steps: In step S201, a substrate is provided, the substrate including a first MOS device region and a second MOS device region, the first MOS device region being used to form a long-channel MOS device, and the second MOS device region being used to form a short-channel MOS device; In step S202, a first type of doping trap ion implantation is performed on the substrate to form a first well region in a first MOS device region and a second well region in a second MOS device region; In step S203, a patterned mask layer is formed on the substrate. The patterned mask layer has a first injection window that exposes the edge region of the first well region, a plurality of second injection windows that expose the middle region of the first well region, and a third injection window that exposes the edge region of the second well region. In step S204, a lightly doped drain ion implantation of the second doping type is performed on the substrate using a patterned mask layer as a mask, so as to form a first lightly doped drain region in the first well region through a first implantation window and a second implantation window, and to form a second lightly doped drain region in the second well region through a third implantation window. In step S205, the patterned mask layer is removed.

[0031] Below, refer to Figures 3A-3D The method for fabricating the semiconductor device according to embodiments of the present invention will be described in detail.

[0032] Specifically, firstly, as Figure 3A As shown, a substrate is provided. The material of the substrate 300 includes, but is not limited to, at least one of the following materials: silicon (Si), germanium (Ge), silicon germanium (SiGe), silicon carbide (SiC), silicon germanium carbon (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP), sapphire, or other III / V compound semiconductors; or silicon on insulator (SOI), silicon on insulator (SSOI), silicon on insulator (S-SiGeOI), silicon on insulator (SiGeOI), and germanium on insulator (GeOI); or it may be a double-sided polished silicon wafer (DSP), a ceramic substrate such as alumina, a quartz or glass substrate, etc. The specific material of the substrate 300 is not limited in the embodiments of the present invention.

[0033] The substrate 300 includes a first MOS device region 300A and a second MOS device region 300B. The first MOS device region 300A is used to form a long-channel MOS device, and the second MOS device region 300B is used to form a short-channel MOS device. The channel length of the long-channel MOS device is greater than the channel length of the short-channel MOS device. A long-channel MOS device can refer to a device whose channel length is much greater than the width of the depletion layer; a short-channel MOS device can refer to a device whose channel length is comparable to or even smaller than the width of the depletion layer.

[0034] A shallow trench isolation structure 301 is formed in the substrate 300 to isolate adjacent MOS devices and define an active region. In one example, the steps of forming the shallow trench isolation structure 301 include: sequentially forming a pad oxide layer and a patterned photoresist layer on the substrate 300; using the patterned photoresist layer as a mask, etching the pad oxide layer and the substrate 300 to form at least one trench that penetrates the pad oxide layer and extends into the interior of the substrate 300; and filling the trench with an isolation material to form the shallow trench isolation structure 301. Specifically, a pad oxide layer is first formed on the substrate 300. The method for forming the pad oxide layer includes, but is not limited to, thermal oxidation or chemical vapor deposition (CVD). The material of the pad oxide layer can be silicon dioxide, etc., without specific limitation. Next, a patterned photoresist layer is formed on the pad oxide layer. The patterned photoresist layer defines the shape and position of the shallow trench isolation structure. The pad oxide layer and the substrate 300 are etched using the patterned photoresist layer as a mask to form at least one trench that penetrates the pad oxide layer and extends into the interior of the substrate 300. Finally, an isolation material is deposited in the trench. The method for depositing the isolation material includes, but is not limited to, physical vapor deposition (PVD) or plasma-enhanced chemical vapor deposition (PECVD). The isolation material includes, but is not limited to, silicon dioxide. After filling the isolation material, chemical mechanical polishing (CMP) can be used to remove excess isolation material and the pad oxide layer on the substrate 300 to form the shallow trench isolation structure 301.

[0035] Exemplarily, a protective layer is also formed on the surface of substrate 300 to protect the substrate surface during subsequent trap ion implantation and LDD ion implantation processes. The material of the protective layer may be silicon nitride, silicon oxide, or a combination of both.

[0036] Next, a first type of doping trap ion implantation is performed on substrate 300 to form a first well region 302A in the first MOS device region 300A and a second well region 302B in the second MOS device region 300B. The first well region 302A and the second well region 302B are the basic doped regions of the MOS device, providing an electrically isolated working space for the device and forming a PN junction isolation in the substrate to prevent leakage and crosstalk between different devices.

[0037] When the long-channel MOS device and the short-channel MOS device are NMOS devices, the first doping type is P-type, that is, the implanted ions in the aforementioned trap ion implantation are P-type ions such as boron (B) or indium (In). When the long-channel MOS device and the short-channel MOS device are PMOS devices, the first doping type is N-type, that is, the implanted ions in the aforementioned trap ion implantation are N-type ions such as phosphorus (P) or arsenic (As).

[0038] For example, the first type of doping trap ion implantation includes sequentially performing a first trap ion implantation, a second trap ion implantation, and a third trap ion implantation.

[0039] The first well ion implantation is a high-energy and high-concentration well ion implantation. For example, the implantation energy of the first well ion implantation is 100 keV to 1000 keV, the implantation angle is 0 degrees, and the implantation depth can reach the micrometer level. The depth of the first well region 302A and the second well region 302B in the substrate 300 is greater than the depth of the subsequently formed lightly doped drain region in the substrate 300.

[0040] The second-well ion implantation is a medium-energy and medium-concentration anti-source-drain punch-through ion implantation. For example, the second-well ion implantation has an implantation energy of 50 keV to 500 keV and an implantation angle of 0 degrees, and is implanted into the channel and near the lower surface of the channel to prevent punch-through between the subsequently formed source and drain regions.

[0041] Third-well ion implantation is used to adjust the threshold voltage. For example, the implantation energy of the third-well ion implantation is from 10 keV to 200 keV, and the implantation angle can be 0°, 7°, or 15°, implanted near the channel surface. Since the doping concentration on the surface of the first well region 302A in the first MOS device region 300A will be reduced subsequently by LDD ion implantation, the ion implantation concentration of the third-well ion implantation can be increased to improve the threshold voltage of the short-channel MOS device while keeping the threshold voltage of the long-channel MOS device essentially unchanged. For example, the ion implantation concentration of the third-well ion implantation is 1.0e12 cm⁻¹. -2 -9.0e13cm -2 .

[0042] The first-well ion implantation, second-well ion implantation, and third-well ion implantation mentioned above are all first-type doping, differing only in implantation energy, implantation angle, and implantation dose to achieve different doping depths and doping concentrations.

[0043] Continue, as Figure 3B As shown, a patterned mask layer 303 is formed on the substrate 300. Exemplarily, the mask layer 303 is a photoresist layer.

[0044] Specifically, a photoresist layer is spin-coated onto a substrate 300, and a patterned mask layer 303 is formed through exposure and development processes. The patterned mask layer 303 has multiple first implantation windows 304A and second implantation windows 304B exposing the first well region 302A, and two third implantation windows 304C exposing the second well region 302B. The first implantation windows 304A, second implantation windows 304B, and third implantation windows 304C are openings in the photoresist layer; during ion implantation, implanted ions enter the substrate 300 below through these openings. The length (i.e., the dimension along the channel width direction) of the patterned mask layer formed above the first well region 302A is X2, and the length of the patterned mask layer formed above the second well region 302B is X3.

[0045] For example, there are two first injection windows 304A, exposing the edge region of the first well region 302A (the dashed box regions on both sides of the first well region 302A). Multiple second injection windows 304B are located in the channel width direction (i.e., parallel to the surface of the substrate 300 and perpendicular to the gate extension direction, i.e.) Figure 3B The second implantation windows 304B are arranged at intervals along the horizontal direction of the channel. Furthermore, the multiple second implantation windows 304B are equally spaced along the channel width direction, and the dimensions (i.e., opening widths) X1 of the multiple second implantation windows 304B along the channel width direction are equal, making the lateral diffusion of subsequently implanted ions more uniform after annealing. In other examples, the multiple second implantation windows 304B can also be non-equally spaced along the channel width direction, and the opening widths of different second implantation windows 304B can be different, for example, the opening width at the edge is larger, and the opening width at the center is smaller, etc., without specific limitations.

[0046] For example, the dimension X1 of the second implantation window 304B along the channel width direction is 0.01 μm to 5 μm. This range ensures sufficient ion throughput for a single window while maintaining photolithographic accuracy, and also guarantees the formation of a continuous lightly doped drain region with uniform doping distribution after annealing. The thickness Y1 of the patterned mask layer 303 is 0.1 μm to 5 μm. This thickness range effectively blocks LDD implanted ions from penetrating while ensuring the pattern transfer accuracy of the implantation window.

[0047] The number of secondary implantation windows 304B is at least three. The larger the total area of ​​the secondary implantation windows 304B, the higher the effective doping concentration. Figure 3A In the example, there are four second injection windows 304B. There are two third injection windows 304C, located on the edge regions on both sides of the second well region 302B (the dashed box regions on both sides of the second well region 302B), corresponding to the positions of the source and drain extension regions of the short-channel MOS device.

[0048] Next, as Figure 3CAs shown, a patterned mask layer 303 is used as a mask to perform lightly doped drain (LDD) ion implantation of the substrate 300, a second doping type. A first lightly doped drain region 305A is formed in the first well region 302A through a first implantation window 304A and a second implantation window 304B, and a second lightly doped drain region 305B is formed in the second well region 302B through a third implantation window 304C. Due to the shielding effect of the mask layer 303, implanted ions can only enter the substrate 300 through the implantation windows, while the area covered by the mask layer 303 remains unimplanted. The first lightly doped drain region 305A and the second lightly doped drain region 305B are located near the surface of the well region and are relatively shallow.

[0049] The second doping type is the opposite of the first doping type. For example, the implantation angle of the lightly doped drain ions in the second doping type is from 0° to 45°, and the implantation dose is 1.0e12 cm⁻¹. -2 up to 5.0e14 cm -2 When the long-channel MOS device and the short-channel MOS device are PMOS devices, the implanted ions are P-type ions such as boron (B), boron fluoride (BF2), or indium (In), and the implantation energy is 3keV to 80keV; when the long-channel MOS device and the short-channel MOS device are NMOS devices, the implanted ions are N-type ions such as phosphorus (P) or arsenic (As), and the implantation energy is 3keV to 80keV.

[0050] In this embodiment of the invention, the doping type of LDD implantation is opposite to that of the well region. During LDD implantation in the first MOS device region 300A through multiple spaced second implantation windows 304B, the implanted impurity ions compensate for the impurities on the surface of the first well region 302A, reducing the effective doping concentration on the channel surface of the long-channel MOS device. This adjusts the threshold voltage of the long-channel MOS device to the target value, narrowing the VT gap with the short-channel MOS device, thereby achieving differentiated control of the threshold voltage between long and short-channel MOS devices. Simultaneously, the equally spaced multiple implantation windows ensure more uniform lateral diffusion of the implanted ions after annealing, and the compensation effect is uniformly distributed on the channel surface, ensuring the consistency of the device's electrical characteristics.

[0051] After forming the first lightly doped drain region 305A and the second lightly doped drain region 305B, as Figure 3D As shown, the patterned mask layer 303 is removed. Specifically, the photoresist mask layer 303 can be removed using an ashing process or a wet stripping process to expose the surface of the substrate 300, providing a clean interface for subsequent process steps.

[0052] After removing the patterned mask layer 303, continue referencing Figure 3DA first gate structure 306A is formed above the first well region 302A, and a second gate structure 306B is formed above the second well region 302B. The length X4 of the first gate structure 306A is greater than or equal to the length X2 of the patterned mask layer 303 formed above the first well region 302A, and the length X5 of the second gate structure 306B is greater than or equal to the length X3 of the patterned mask layer 303 formed above the second well region 302B.

[0053] The gate structure includes at least a gate dielectric layer, a gate electrode layer, and a gate sidewall. Exemplarily, the gate dielectric layer may be made of silicon oxide, silicon oxynitride, or a high-k dielectric material, and the gate electrode layer may be made of polysilicon or a metal. A method for forming the gate structure includes: sequentially depositing a gate dielectric material layer and a gate electrode material layer on a substrate 300; then forming a patterned photoresist layer on the gate electrode material layer; and etching the gate electrode material layer and the gate dielectric material layer using the patterned photoresist layer as a mask to form the gate dielectric layer and the gate electrode layer.

[0054] Next, gate sidewalls (spacers) are formed on both sides of the gate electrode layer. The gate sidewalls can be made of silicon nitride or silicon oxide, and the formation method includes: depositing a sidewall material layer on the substrate; and using an anisotropic etching process to etch back the sidewall material layer to form the gate sidewalls on the sidewalls of the gate electrode layer. The gate sidewalls are used to protect the gate structure in subsequent processes and further define the location of the source and drain regions during source and drain implantation.

[0055] After forming the first gate structure 306A and the second gate structure 306B, the method further includes: using the first gate structure 306A and the second gate structure 306B as masks, performing source / drain ion implantation of the second doping type on the substrate 300 to form a first source / drain region in the first well region 302A and a second source / drain region in the second well region 302B. The doping type of the source / drain ion implantation is the same as that of the lightly doped drain implantation, which is the second doping type, but the implantation dose is higher (e.g., 1.0e15 cm⁻¹). -2 Up to 1.0e16 cm -2 The injection energy is higher to form heavily doped source and drain regions. Since the gate structure acts as a self-aligned mask, source and drain implanted ions are only implanted into the substrate on both sides of the gate structure to form heavily doped source and drain regions, while the channel region below the gate structure is not implanted.

[0056] In this embodiment of the invention, since lightly doped drain implantation is completed before the gate structure is formed, there is no need to use the gate structure as a mask for LDD implantation. Therefore, the formation of the lightly doped drain region is not limited by the gate length. Even if the gate length is further reduced, the solution of the present invention can still flexibly adjust the doping concentration and distribution of the lightly doped drain region, thereby effectively suppressing the hot carrier effect.

[0057] Reference Figures 4-6 ,in Figure 4 Simulation comparison diagrams of long-channel MOS devices based on related technologies and embodiments of the present invention are shown. Figure 5 Simulation comparison diagrams of short-channel MOS devices based on related technologies and embodiments of the present invention are shown. Figure 6 A comparison graph of the active doping concentration curves of short-channel MOS devices in related technologies and embodiments of the present invention is shown.

[0058] The mask layer pattern of the long-channel MOS device before LDD implantation in an embodiment of the present invention is as follows: Figure 4 As shown, the uniformly spaced implantation windows make ion implantation diffusion more uniform. Figures 4 to 6 Simulation results show that, in this embodiment of the invention, setting the LDD of the long-channel MOS device to multi-window implantation and performing it before gate formation, the implantation parameters are no longer limited by the gate thickness and length, and the LDD implantation energy and dose can be flexibly increased. At the same time, by increasing the third well ion implantation concentration, the linear threshold voltage (VTlin) of the short-channel MOS device is increased from 0.542V to 0.659V, while the VTlin of the long-channel MOS device remains basically unchanged at 0.65V. This reduces the VT gap between the long and short channels from 0.108V to 0.009V, effectively suppressing the short-channel effect and improving device performance.

[0059] This completes the process steps of the semiconductor device fabrication method according to an embodiment of the present invention. It is understood that the semiconductor device fabrication method of this embodiment includes not only the above-described steps, but may also include other necessary steps before, during, or after the above-described steps, all of which are included within the scope of the fabrication method of this embodiment.

[0060] In summary, the semiconductor device fabrication method provided by this invention advances LDD implantation to before the formation of the gate structure. LDD implantation is performed by forming multiple implantation windows spaced apart in the long-channel device region. Since the impurity type implanted by LDD is opposite to the doping type in the well region, the implanted dopant ions have a compensating effect on the doping concentration on the well surface, uniformly neutralizing a portion of the well concentration on the channel surface of the long-channel device. Therefore, by increasing the LDD implantation energy and increasing the implantation concentration of the third well ion used to adjust the threshold voltage, the threshold voltage of the long-channel MOS device can be increased simultaneously without changing the threshold voltage of the short-channel MOS device, thereby reducing the VTgap between the long-channel and short-channel MOS devices and achieving differentiated control of the threshold voltage of long and short-channel devices. Furthermore, in this embodiment, an independent mask layer is used instead of the gate structure as the mask for LDD implantation. The thickness of the mask layer can be freely adjusted according to the implantation energy, no longer limited by the thickness of the gate structure. This solves the problem of device performance degradation caused by the forced reduction of LDD implantation energy as the gate size continues to thin. It allows for flexible increases in LDD implantation energy and dosage, further improving the short-channel effect.

[0061] The present invention also provides a semiconductor device, which can be prepared by the method of the aforementioned embodiment one, or can be prepared by other suitable preparation methods.

[0062] The semiconductor devices of this invention include long-channel MOS devices and short-channel MOS devices. The long-channel MOS device includes a first well region in a substrate and a first lightly doped drain region in the first well region. The short-channel MOS device includes a second well region in a substrate and a second lightly doped drain region in the second well region. The first and second well regions have a first doping type, and the first and second lightly doped drain regions have a second doping type, which is opposite to the first doping type. In the long-channel MOS device, the first lightly doped drain region is uniformly distributed on the surface of the first well region, providing a compensation effect on the doping concentration of the first well region surface, thereby reducing the effective doping concentration on the channel surface of the long-channel MOS device.

[0063] The semiconductor device provided by this invention improves the electrical performance of the device by using the compensation effect of inverted LDD dopant ions on the surface of the well region to make the threshold voltage of the long-channel MOS device more consistent with that of the short-channel MOS device.

[0064] The present invention has been described through the above embodiments. However, it should be understood that the above embodiments are for illustrative purposes only and are not intended to limit the invention to the scope of the described embodiments. Furthermore, those skilled in the art will understand that the present invention is not limited to the above embodiments, and many more variations and modifications can be made based on the teachings of the present invention, all of which fall within the scope of protection claimed by the present invention. The scope of protection of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for fabricating a semiconductor device, characterized in that, The preparation method includes: A substrate is provided, the substrate including a first MOS device region and a second MOS device region, the first MOS device region being used to form a long-channel MOS device, and the second MOS device region being used to form a short-channel MOS device; A first type of doping trap ion implantation is performed on the substrate to form a first well region in the first MOS device region and a second well region in the second MOS device region; A patterned mask layer is formed on the substrate, wherein a first injection window is formed in the patterned mask layer to expose the edge region of the first well region, a plurality of second injection windows arranged at intervals to expose the middle region of the first well region, and a third injection window to expose the edge region of the second well region. Using the patterned mask layer as a mask, a second type of light doping drain ion implantation is performed on the substrate to form a first lightly doped drain region in the first well region through the first implantation window and the second implantation window, and a second lightly doped drain region in the second well region through the third implantation window; Remove the patterned mask layer.

2. The preparation method according to claim 1, characterized in that, After removing the patterned mask layer, the process further includes: A first gate structure is formed above the first well region, and a second gate structure is formed above the second well region. The length of the first gate structure is greater than or equal to the length of the patterned mask layer formed above the first well region, and the length of the second gate structure is greater than or equal to the length of the patterned mask layer formed above the second well region. Using the first gate structure as a mask, the substrate is subjected to ion implantation of the second doping type to form a first source / drain region in the first well region and a second source / drain region in the second well region.

3. The preparation method according to claim 1 or 2, characterized in that, When the long-channel MOS device and the short-channel MOS device are NMOS devices, the first doping type is P-type and the second doping type is N-type; when the long-channel MOS device and the short-channel MOS device are PMOS devices, the first doping type is N-type and the second doping type is P-type.

4. The preparation method according to claim 1, characterized in that, The second injection windows are arranged at equal intervals in the channel width direction.

5. The preparation method according to claim 4, characterized in that, The spacing of the second injection windows in the channel width direction is 0.01 μm to 5 μm.

6. The preparation method according to claim 1, characterized in that, The height of the mask layer is from 0.1 μm to 5 μm.

7. The preparation method according to claim 1, characterized in that, When the long-channel MOS device and the short-channel MOS device are PMOS devices, the implanted ions for the lightly doped drain ion implantation are boron, boron fluoride, or indium, the implantation angle is 0° to 45°, the implantation energy is 3 keV to 80 keV, and the implantation dose is 1.0e12 cm⁻¹. -2 up to 5.0e14 cm -2 ; When the long-channel MOS device and the short-channel MOS device are NMOS devices, the implanted ions for the lightly doped drain ion implantation are phosphorus or arsenic, the implantation angle is 0° to 45°, the implantation energy is 3 keV to 80 keV, and the implantation dose is 1.0e12cm. -2 up to 5.0e14 cm -2 .

8. The preparation method according to claim 1, characterized in that, The first type of trap ion implantation on the substrate includes: First-trap ion implantation is performed at implantation energies ranging from 100 keV to 1000 keV; Second trap ion implantation is performed at implantation energies ranging from 50 keV to 500 keV; Third-trap ion implantation was performed at implantation energies ranging from 10 keV to 200 keV.

9. The preparation method according to claim 8, characterized in that, The ion implantation concentration for the third well is 1.0e12cm. -2 -9.0e13cm -2 .

10. A semiconductor device, characterized in that, The semiconductor device is obtained by the fabrication method according to any one of claims 1 to 9.