A photovoltaic module and photovoltaic system
By adopting a combination structure of high and low modulus adhesive film layers in photovoltaic modules, the problems of interface delamination and poor soldering during thermal cycling are solved, thereby improving the reliability and process stability of the modules and reducing costs.
Patent Information
- Application Number
- CN202611398278.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-09
- Publication Date
- 2026-11-24
AI Technical Summary
Existing photovoltaic modules suffer from interface delamination, poor soldering, and power attenuation during thermal cycling. Traditional solder ribbons are not fully welded to the cells, and the skin film cannot effectively buffer stress, resulting in insufficient reliability.
The photovoltaic module design adopts a combination structure of high-modulus and low-modulus adhesive film layers. The first adhesive film layer is formed by co-extrusion or coating. Combined with the stacked structure of high and low modulus adhesive film layers, it ensures strong binding force of conductive interconnect strips, excellent adsorption effect, and improves process stability and low-temperature bonding performance of solar cells.
It improves the thermal cycling reliability of photovoltaic modules, enhances process performance, reduces costs, and improves the overall stability and lifespan of modules.
Smart Images

Figure CN123164847A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of photovoltaic module technology, and more specifically, to a photovoltaic module and a photovoltaic system. Background Technology
[0002] As the photovoltaic industry enters a stage of high-quality development driven by technology, the long-term reliability of modules has become a core competitive factor for product differentiation. Among them, thermal cycling (TC) is a core indicator for measuring the quality of photovoltaic modules, and it has a crucial impact on the product's power generation stability, service life, and environmental adaptability.
[0003] In outdoor environments, the diurnal temperature range and seasonal climate changes can cause continuous thermomechanical stress in components, easily leading to problems such as interface delamination, poor soldering, and power degradation. However, the thermal conductivity (TC) performance of most products in the industry still has significant shortcomings. Some products experience excessive degradation and frequent failures after long-term thermal cycling tests. This is a key pain point that the entire industry urgently needs to overcome and continuously optimize.
[0004] In existing technologies, a skin film is typically placed between the solar cell and the encapsulation film as a buffer and protective material. Conventional skin films may not be able to effectively buffer stress during TC cycles due to low fluidity, or may delaminate from the solder ribbon and solar cell due to insufficient high viscosity, ultimately resulting in high and low temperature desoldering and shadows in EL testing.
[0005] Furthermore, the welding reliability of traditional photovoltaic solder ribbons to cell grid lines can directly affect TC performance. Traditional photovoltaic solder ribbons, such as conductive interconnect strips, have high melting points, and insufficient heating during lamination can lead to incomplete welding, increasing the risk of solder joint degradation during thermal cycling. While using low-temperature interconnect strips can lower the welding temperature window, the rheological behavior of the skin film and encapsulating film at the lamination temperature may be affected, making it difficult to ensure interfacial adhesion strength and long-term weather resistance.
[0006] Therefore, there is an urgent need for a photovoltaic module that can ensure technological feasibility while providing excellent reliability. Summary of the Invention
[0007] This application provides a photovoltaic module and a photovoltaic system that can solve the reliability problem of TC thermal cycling performance.
[0008] In a first aspect, a photovoltaic module is provided, comprising: Battery cells; Interconnecting strips are disposed on the surface of the battery cell; A first adhesive film layer is disposed on the surface of the interconnect strip away from the battery cell, and includes at least a first sub-adhesive film layer and a second sub-adhesive film layer stacked sequentially in a direction away from the battery cell, wherein the elastic modulus of the first sub-adhesive film layer is less than the elastic modulus of the second sub-adhesive film layer. A second adhesive film layer is disposed on the surface of the first adhesive film layer away from the battery cell. A protective layer is disposed on the surface of the second adhesive film layer away from the battery cell.
[0009] The photovoltaic module provided in this application embodiment can optimize the design of the first adhesive film layer material in the photovoltaic module by adopting a combination structure of high-modulus film layer and low-modulus film layer. The high-modulus film layer can ensure stronger resistance to high and low temperature impact deformation, stronger binding force on conductive interconnect strips, and better TC reliability. At the same time, the low-modulus film layer can ensure tighter adhesion to the suction cup, better adsorption effect, improve process stability and low temperature bonding performance of the cells. Thus, while improving product reliability, enhancing its process performance, and reducing costs.
[0010] In some embodiments, the elastic modulus of the first sub-film layer ranges from 5 MPa to 15 MPa, and the elastic modulus of the second sub-film layer ranges from 40 MPa to 60 MPa.
[0011] In some embodiments, the first adhesive film layer includes a first sub-adhesive film layer and a second sub-adhesive film layer stacked sequentially in a direction away from the battery cell, wherein the first sub-adhesive film layer is in contact with the surface of the interconnect strip away from the battery cell, and the second sub-adhesive film layer is in contact with the surface of the second adhesive film layer close to the battery cell.
[0012] In some embodiments, the first adhesive film layer includes two opposing first sub-adhesive film layers and a second sub-adhesive film layer located between the two first sub-adhesive film layers, one of the first sub-adhesive film layers being in contact with the surface of the interconnect strip away from the battery cell, and the other of the first sub-adhesive film layer being in contact with the surface of the second adhesive film layer close to the battery cell.
[0013] In some embodiments, the first adhesive film layer includes a first sub-adhesive film layer, a second sub-adhesive film layer, and a third sub-adhesive film layer sequentially disposed on the surface of the interconnect strip away from the battery cell. The first sub-adhesive film layer is in contact with the surface of the interconnect strip away from the battery cell, and the third sub-adhesive film layer is in contact with the surface of the second adhesive film layer near the battery cell. The elastic modulus of the second sub-adhesive film layer is less than that of the third sub-adhesive film layer.
[0014] In some embodiments, the total thickness of the first adhesive film layer ranges from 40 μm to 150 μm.
[0015] In some embodiments, the thickness of the second sub-film layer is not less than 50% of the total thickness of the first film layer.
[0016] In some embodiments, the thickness of the first sub-adhesive film layer is not less than 10 μm.
[0017] In some embodiments, the first adhesive film layer comprises either EVA or TPO.
[0018] In some embodiments, the second adhesive film layer comprises any one of EVA, EPE, POE, PVB, PET, or liquid silicone.
[0019] Secondly, a method for preparing a photovoltaic module is provided, comprising: Provide battery cells; Interconnecting strips and a first adhesive film layer are sequentially placed on the surface of the battery cell and then strung together. The first adhesive film layer is disposed on the surface of the interconnecting strip away from the battery cell and includes at least a first sub-adhesive film layer and a second sub-adhesive film layer stacked sequentially in a direction away from the battery cell. The elastic modulus of the first sub-adhesive film layer is less than that of the second sub-adhesive film layer. Based on the battery cells after string processing, a second adhesive film layer and a protective layer are sequentially placed on the surface of the first adhesive film layer; the second adhesive film layer is disposed on the surface of the first adhesive film layer away from the battery cell. A lamination process is performed to make the interconnecting strips electrically connected to the contact area of the battery cell, and to encapsulate the layers of material into a single unit; After lamination, subsequent components are installed to complete the fabrication of the photovoltaic module.
[0020] The photovoltaic modules provided in this application can improve product reliability and enhance their process performance by using simple process methods and optimizing the design of the skin film material, and by making precise control over the product's elastic modulus.
[0021] In some embodiments, the preparation method further includes: The first film layer is formed by co-extrusion or coating.
[0022] Thirdly, a photovoltaic system is provided, comprising the photovoltaic module described in any of the above embodiments. Attached Figure Description
[0023] Figure 1 This is a schematic diagram of the first adhesive film layer provided in this application; Figure 2 This is a schematic diagram of the photovoltaic module provided in this application; Figure 3 This is a flowchart of the method for manufacturing photovoltaic modules provided in this application; Figure 4 This is a schematic diagram of the photovoltaic system provided in this application.
[0024] The accompanying drawings are not drawn to scale.
[0025] Figure label: 1: Second sub-encapsulant layer; 2: First sub-encapsulant layer; 4: Solar cell; 5: Interconnect strip; 6: First encapsulant layer; 7: Second encapsulant layer; 8: First protective layer; 9: Second protective layer; 10: Photovoltaic module; 1000: Photovoltaic system. Detailed Implementation
[0026] The descriptions of specific structures or functions implemented according to the concept of this application disclosed in this specification are merely illustrative examples for explaining embodiments based on the concept of this application. Those skilled in the art will understand that embodiments based on the concept of this application can have various variations and forms, and are not limited to the embodiments described in this specification, but also include various modifications, equivalents, or substitutions made within the scope of the purpose, concept, and technology of this application.
[0027] In the description of this application, it should be understood that the use of terms such as "center", "longitudinal", "lateral", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "clockwise", "counterclockwise", "axial", "radial", and "circumferential" indicates the relative orientation or positional relationship between different components, and is only for the convenience of describing this application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application.
[0028] Although the terms "first" or "second" may be used to describe various components or components, the components or components should not be limited by the terms. The terms above are used only for the purpose of distinguishing one component or component from another. For example, without departing from the scope of the claims according to the concept of this application, a first battery cell may be referred to as a second battery cell, and similarly, a second battery cell may be referred to as a first battery cell.
[0029] In this application, unless otherwise expressly specified and limited, the terms "connected," "fixed," "set," etc., should be interpreted broadly. For example, when one component is said to "connect" another component, it should be understood that it can be directly or indirectly connected to the other component, meaning that other components may also be present in between. Similarly, the terms "fixed" and "set" should be interpreted broadly in a similar way. Furthermore, the term "connected" can refer to a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can refer to the internal communication of two components or the interaction between two components, unless otherwise expressly limited. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances. In this application, unless otherwise expressly specified and limited, the description of "above" or "below" the second feature can mean that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediate medium. Moreover, "above," "on top of," and "over" the second feature can mean that the first feature is directly above or diagonally above the second feature, or simply that the first feature is at a higher horizontal level than the second feature. The first feature being "below", "under", or "below" the second feature can mean that the first feature is directly below or diagonally below the second feature, or simply that the first feature is at a lower horizontal level than the second feature.
[0030] To make the above-mentioned objectives, features and advantages of this application more apparent and understandable, the specific embodiments of this application will be described in detail below with reference to the accompanying drawings.
[0031] Research by the technical personnel involved in this application has revealed that in conventional technologies, a skin film is typically placed between the solar cell and the encapsulating film as a buffer and protective material. However, conventional skin films may fail to effectively buffer stress during thermal cycling due to low fluidity, or may delaminate from the solder ribbon and solar cell due to insufficient viscosity, ultimately resulting in high- and low-temperature desoldering and shadowing during EL testing. Traditional photovoltaic solder ribbons, such as conductive interconnects, have high melting points, and during lamination, insufficient heating can lead to incomplete welding, increasing the risk of solder joint degradation during thermal cycling.
[0032] Based on this, this application provides a photovoltaic module 10, with reference to Figure 1 and Figure 2 The photovoltaic module 10 includes: Battery cell 4; Interconnecting strip 5 is disposed on the surface of battery cell 4; The first adhesive layer 6 is disposed on the surface of the interconnecting strip 5 away from the battery cell 4, and includes at least a first sub-adhesive layer 1 and a second sub-adhesive layer 2 stacked sequentially in the direction away from the battery cell 4. The elastic modulus of the first sub-adhesive layer 1 is less than the elastic modulus of the second sub-adhesive layer 2. The second adhesive layer 7 is disposed on the surface of the first adhesive layer 6 away from the battery cell 4. A protective layer is disposed on the surface of the second adhesive film layer 7 away from the battery cell 4.
[0033] A photovoltaic module 10 is a device that directly converts light energy into electrical energy through the photoelectric effect or photochemical effect. A photovoltaic module 10 typically has a multi-layered encapsulation structure. The structure of each layer of the photovoltaic module is described in detail below.
[0034] The solar cell 4 may include a semiconductor substrate, a first emitter of a first conductivity type, and a second emitter of a second conductivity type. It is understood that one of the first and second conductivity types is P-type, and the other is N-type. The semiconductor substrate may include an N-type silicon substrate or a P-type silicon substrate. N-type silicon substrates are typically formed by doping with Group V elements such as phosphorus, arsenic, or antimony, and have the characteristic that the majority carriers are electrons; P-type silicon substrates are typically formed by doping with Group III elements such as boron, gallium, or aluminum, and have the characteristic that the majority carriers are holes. The solar cell 4 may include opposing front and back sides.
[0035] In this invention, the battery cell 4 can employ a grid line design with no main busbar (OBB), multiple main busbars (MBB), or super multi-busbars (SMBB). In some embodiments, the grid line material can be selected as at least one of silver-based conductive paste or silver-coated copper composite paste. The paste uses highly conductive metal powder as the conductive substrate, and the substrate can be at least one of silver powder, copper powder, or silver-coated copper composite powder. To improve the ohmic contact performance, conductivity, and long-term weather resistance of the electrodes, a composite functional layer can be formed on the surface of the substrate or in the grid line structure. The functional layer material includes at least one of glass powder, organic carrier, nickel-based barrier layer, tin-based alloy layer, or anti-oxidation and corrosion-resistant coating.
[0036] It is understood that the solar cell 4 can be at least one of the following commonly used in the field: TOPCon (Tunnel Oxide Passivated Contact) cell, HJT (Heterojunction with Intrinsic Thin-film) cell, BC (Back Contact) cell, perovskite / tandem cell, etc.
[0037] Interconnect Strip 5 is a core conductive material used in photovoltaic modules for connecting cells in series. Essentially, it's a copper-based conductive lead strip coated with a solder alloy. Interconnect Strip 5 mainly consists of two parts: Copper substrate: As the conductive backbone, high-purity oxygen-free copper with a purity of over 99.95% is usually used to ensure excellent conductivity and appropriate mechanical strength.
[0038] Surface coating: A layer of solder alloy is applied to the surface of the copper substrate through processes such as electroplating or hot-dip coating. This alloy layer is key to achieving solderability, as it firmly welds the interconnects to the electrodes of the solar cell.
[0039] In this invention, the interconnect strip 5 can be a low-temperature interconnect strip, such as a conventional tin-lead-bismuth system (bismuth content of 10% to 40%), whose melting temperature is in the range of 120°C to 150°C. In the finished product design, it undertakes the function of current transmission and is tightly integrated with the photovoltaic cell. The interconnect strip 5 can be set on both surfaces of the cell 4, that is, on the front and back of the cell 4.
[0040] The first adhesive film layer 6 is disposed on the surface of the interconnecting strip 5 away from the battery cell 4. Its core function is to fix the conductive interconnecting strip 5 and to contact the battery cell 4. The material of the first adhesive film layer 6 should have high light transmittance and excellent UV aging resistance, and should maintain a low yellowing level under long-term outdoor exposure to ensure that light can efficiently penetrate and reach the battery surface.
[0041] Research has shown that in scenarios with frequent high and low temperature changes (e.g., during TC cycle testing), the binding ability of the skin film to the conductive interconnect strip is closely related to the elastic modulus of its material. The study found that within the elastic modulus range of 5 MPa to 60 MPa, the higher the elastic modulus of the first adhesive film layer 6, the stronger its resistance to high and low temperature impact deformation, the stronger its binding force on the conductive interconnect strip, and the better the TC reliability. Conversely, the lower the elastic modulus of the first adhesive film layer 6, the weaker its resistance to deformation, but its flexibility is better. During the manufacturing process, when in contact with the suction cup, the low-modulus film has better shape adaptability, a tighter fit with the suction cup, and a better adsorption effect. Simultaneously, it melts more easily at the same temperature, allowing it to adhere to the battery cell even in low-temperature environments, thus fixing the solder ribbon. Therefore, this invention uses a stack of a high-elastic-modulus adhesive film layer and a low-elastic-modulus adhesive film layer as the first adhesive film layer 6. Specifically, in the stacked structure of the first adhesive layer 6, a high-elastic-modulus adhesive layer is used as the main material, namely the second sub-adhesive layer 1, to fully leverage its advantage in improving TC reliability; simultaneously, a low-elastic-modulus adhesive layer, namely the first sub-adhesive layer 2, is provided on at least one surface of the second sub-adhesive layer 1. The stacked structure of the first adhesive layer 6 must satisfy the requirement that the layer closest to the battery cell 4 is a low-modulus adhesive layer. For example, when the first adhesive layer 6 has a two-layer structure, the modulus gradually decreases from the side away from the battery cell 4 to the side closer to the battery cell 4. In the case of a structure with three or more layers, the modulus of the sub-adhesive layers gradually decreases from the middle sub-adhesive layer to the two side sub-adhesive layers, or gradually decreases from the side away from the battery cell to the side closer to the battery cell. In some embodiments, the elastic modulus of the low-elastic-modulus adhesive layer ranges from 5 MPa to 15 MPa, and the elastic modulus of the high-elastic-modulus adhesive layer ranges from 40 MPa to 60 MPa. For example, in the case of the first film layer 6 with a two-layer structure, the elastic modulus of the first sub-film layer 2 ranges from 5 MPa to 15 MPa, and the elastic modulus of the second sub-film layer 1 ranges from 40 MPa to 60 MPa.
[0042] In the first adhesive layer 6, the sub-adhesive layer with high elastic modulus has strong resistance to high and low temperature impact deformation, stronger binding force on conductive interconnect strips, and better TC reliability; the sub-adhesive layer with low elastic modulus is easier to melt at the same temperature, and can adhere to the battery cell in a low temperature environment, forming a fixing effect on the interconnect strips. The temperature is lower, the equipment energy consumption is lower, the cost is lower, and the process microcrack rate is lower.
[0043] The different sub-layers of the first adhesive film layer 6 can be strengthened through co-extrusion to prevent separation between layers during use.
[0044] The second adhesive layer 7 can be disposed on the surface of the first adhesive layer 6, that is, the second adhesive layer 7 can be disposed on both the front and back sides of the solar cell 4. The second adhesive layer 7 serves as a high-performance adhesive film between the glass and the internal first adhesive layer 6 / solar cell 4. Its surface can form a high-strength, aging-resistant chemical bond and physical adsorption with the glass surface, constructing a strong glass-adhesive layer interface, thereby ensuring the stability of the overall module structure. At the same time, after the second adhesive layer 7 is bonded to the first adhesive layer 6, it can block moisture intrusion, prevent the conductive interconnect strip 5 and the solar cell 4 from oxidizing and failing, and also buffer mechanical stress, protecting the brittle solar cell. In addition, the second adhesive layer 7 has a high light transmittance of >91% and excellent UV aging resistance, maintaining a low degree of yellowing under long-term outdoor exposure conditions, ensuring efficient light transmission and reaching the surface of the solar cell.
[0045] The protective layer may include a first protective layer 8 located on the front side of the solar cell. The first protective layer 8 may be a glass layer, i.e., a front cover plate, which protects the interior of the photovoltaic module and also provides water-blocking protection. The front cover plate may be made of a material with excellent light transmittance, impact resistance, corrosion resistance, and weather resistance, and may optionally include at least one of the following materials: tempered glass, plexiglass, transparent ceramics, organic fibers, or polymers. In some embodiments, the front cover plate may include at least one of an insulating barrier layer, a fluorinated weather-resistant layer, and a transition adhesive layer.
[0046] The protective layer may also include a second protective layer 9 located on the back of the solar cell. The second protective layer 9 can be a photovoltaic glass layer or a cover plate. The back cover plate typically needs to possess insulation, water resistance, aging resistance, weather resistance, and corrosion resistance. It may optionally include at least one of the following: tempered glass, plexiglass, metal backsheet, or composite backsheet with PET film as the substrate. Among them, the PET-based composite backsheet may optionally include various types such as composite type (e.g., TPT / KPK, TPE / KPE), coated type (e.g., TPC, KPC, CPC), and co-extruded type (e.g., PO) depending on the needs of different scenarios.
[0047] It is understandable that the material selection of the first protective layer 8 and the second protective layer 9 does not affect each other, and the same or different materials can be selected according to different application scenarios of the components (such as residential photovoltaics and building-integrated photovoltaics).
[0048] The photovoltaic module 10 may also include a frame. The frame surrounds the periphery of the laminated structure and is typically made of aluminum alloy or steel alloy. In some embodiments, the frame may also be a fiberglass frame or a plastic frame. The inner side of the frame usually has grooves for filling with sealant to achieve a sealed bond with the laminated components formed by the front cover, the first encapsulating film, the cell string layers, the second encapsulating film, and the back cover, thereby blocking moisture and buffering external impacts. In some embodiments, the frame can be assembled by connecting corner brackets.
[0049] The photovoltaic module 10 may also include a junction box. The junction box is located on one side of the rear cover and is electrically connected to the terminals of the bus electrodes in the cell string layer via a lead-out busbar for energy extraction. The junction box typically includes a housing and cover made of weather-resistant insulating material, conductive connecting tabs disposed within the housing, and one or more bypass diodes. The bypass diodes are connected in parallel with sub-units of the cell string. The electrical leads of the junction box include photovoltaic-specific connectors and cables. The cables preferably use cross-linked polyethylene insulation sheaths and tinned copper core wires. In some embodiments, the interior of the junction box may also be filled and encapsulated with potting compound to achieve insulation, thermal conductivity, moisture protection, and fixation.
[0050] The photovoltaic module provided in this application embodiment can optimize the design of the first encapsulant layer material in the photovoltaic module by adopting a combination structure of high-modulus encapsulant layer and low-modulus encapsulant layer. The high-modulus encapsulant layer can ensure stronger resistance to high and low temperature impact deformation, stronger binding force on conductive interconnect strips, and better TC reliability. At the same time, the low-modulus encapsulant layer can ensure tighter adhesion to the suction cup, better adsorption effect, improve process stability and low temperature bonding performance of the cells. Thus, while improving product reliability, enhancing its process performance, and reducing costs.
[0051] In some embodiments, the first encapsulant layer 6 includes a first sub-encapsulant layer 2 and a second sub-encapsulant layer 1 sequentially stacked in a direction away from the solar cell 4. The first sub-encapsulant layer 2 is in contact with the surface of the interconnect strip 5 away from the solar cell 4, and the second sub-encapsulant layer 1 is in contact with the surface of the second encapsulant layer 7 near the solar cell 4. In this case, the first sub-encapsulant layer 2 is defined as the front side of the first encapsulant layer 6, and the second sub-encapsulant layer 1 is defined as the back side of the first encapsulant layer 6. That is, in the structure of the photovoltaic module, the first sub-encapsulant layer 2 side of the first encapsulant layer 5 is in contact with the interconnect strip 5, i.e., the low-modulus encapsulant layer side is in contact with the interconnect strip 5.
[0052] In this embodiment, the first adhesive layer 6 adopts a stacked structure of two sub-adhesive layers. The first sub-adhesive layer 2 with low elastic modulus has a better fit to the shape of the suction cup, a tighter fit with the suction cup, and a better adsorption effect. The second sub-adhesive layer 1 with high elastic modulus has strong resistance to high and low temperature impact deformation, stronger binding force on the conductive interconnect strip, and better TC reliability. At the same time, the stacked structure of the two sub-adhesive layers makes the thickness of the first adhesive layer thinner, which can effectively reduce the junction temperature and improve the power tolerance and long-term life of the device.
[0053] In some embodiments, the first adhesive layer 6 includes two opposing first sub-adhesive layers 2 and a second sub-adhesive layer 1 located between the two first sub-adhesive layers 2. One of the first sub-adhesive layers 2 is in contact with the surface of the interconnecting strip 5 away from the battery cell 4, and the other of the first sub-adhesive layers 2 is in contact with the surface of the second adhesive layer 7 near the battery cell 4. In this case, in the structure of the first adhesive layer 6, a high-elastic modulus film is located between low-elastic modulus films, and the elastic modulus gradually decreases from the center to both sides. The two first sub-adhesive layers 2 are generally identical sub-adhesive layers.
[0054] In this embodiment, the first adhesive layer 6 adopts a stacked structure of first sub-adhesive layer 2 / second sub-adhesive layer 1 / first sub-adhesive layer 2, which effectively improves the reliability of TC, further increases the stability of the process, reduces equipment energy consumption, thereby reducing costs and the rate of microcracks in the process.
[0055] In some embodiments, the first adhesive layer 6 includes a first sub-adhesive layer 2, a second sub-adhesive layer 1, and a third sub-adhesive layer sequentially disposed on the surface of the interconnecting strip 5 away from the battery cell 4. The first sub-adhesive layer 2 is in contact with the surface of the interconnecting strip 5 away from the battery cell 4, and the third sub-adhesive layer is in contact with the surface of the second adhesive layer 7 near the battery cell 4. The elastic modulus of the first sub-adhesive layer 1 is less than that of the second sub-adhesive layer 1, and the elastic modulus of the second sub-adhesive layer 1 is less than that of the third sub-adhesive layer. That is, the modulus of the sub-adhesive layers gradually decreases from the side away from the battery cell 4 to the side near the battery cell 4.
[0056] In this embodiment, the first adhesive layer 6 adopts a stacked structure of a first sub-adhesive layer 2 / a second sub-adhesive layer 1 / a third sub-adhesive layer with gradually increasing elastic modulus. This achieves a tighter fit with the suction cup, better adsorption effect, and thus increases the stability of the process. At the same time, the stacking of sub-adhesive layers with high elastic modulus can more effectively improve the binding force on the conductive interconnect strip and the reliability of TC.
[0057] In some embodiments, the total thickness of the first adhesive film layer 6 ranges from 40 μm to 150 μm. The thickness of the second sub-adhesive film layer 1 is not less than 50% of the total thickness of the first adhesive film layer 6. For example, the thickness of the second sub-adhesive film layer 1 can be 50% to 90% of the total thickness of the first adhesive film layer 6. Furthermore, the thickness of the first sub-adhesive film layer 2 is not less than 10 μm.
[0058] For example, when the first film layer 6 includes a first sub-film layer 2 and a second sub-film layer 1 stacked sequentially in a direction away from the battery cell, when the total thickness of the first film layer 6 is 40 μm, the thickness of the first sub-film layer 2 can be 12 μm and the thickness of the second sub-film layer 1 can be 28 μm; when the total thickness of the first film layer 6 is 80 μm, the thickness of the first sub-film layer 2 can be 24 μm and the thickness of the second sub-film layer 1 can be 56 μm; when the total thickness of the first film layer 6 is 150 μm, the thickness of the first sub-film layer 2 can be 15 μm and the thickness of the second sub-film layer 1 can be 135 μm.
[0059] When the first adhesive layer 6 includes two opposing first sub-adhesive layers 2 and a second sub-adhesive layer 1 located between the two first sub-adhesive layers 2, when the total thickness of the first adhesive layer 6 is 40 μm, the thickness of each first sub-adhesive layer 2 can be 10 μm and the thickness of each second sub-adhesive layer 1 can be 20 μm; when the total thickness of the first adhesive layer 6 is 100 μm, the thickness of each first sub-adhesive layer 2 can be 16 μm and the thickness of each second sub-adhesive layer 1 can be 48 μm; when the total thickness of the first adhesive layer 6 is 150 μm, the thickness of each first sub-adhesive layer 2 can be 30 μm and the thickness of each second sub-adhesive layer 1 can be 90 μm.
[0060] When the thickness of the first adhesive film layer 6 and the thickness of each sublayer are within the above range or meet the above requirements, the long-term reliability of the device can be effectively improved.
[0061] In some embodiments, the first film layer 6 comprises either EVA or TPO. For example, when the first film layer 6 comprises EVA, the elastic modulus can be adjusted by using different grades of VA particles. Generally, the higher the grade, the lower the modulus and the softer the material, and vice versa. Alternatively, the elastic modulus can be adjusted by changing the crosslinking agent system, adding fillers, etc., thereby achieving a laminated structure of film layers with different elastic moduli. For example, when the first film layer 6 comprises EVA, the VA particles in the first sub-film layer 2 with a low modulus are different from those in the second sub-film layer 1 with a high modulus; comparatively, the grade of the first sub-film layer 2 can be higher than that of the second sub-film layer 1.
[0062] In some embodiments, the material of the second film layer 7 may be selected from at least one of ethylene-vinyl acetate copolymer (EVA) film, polyvinyl octene coelastomer (POE) film, EVA-POE-EVA (EPE) co-extruded film, polyvinyl butyral (PVB) film, polyethylene terephthalate (PET) film, or liquid silicone.
[0063] In some embodiments, the second adhesive film layer 7 may further include one or more functional additives selected from the group consisting of crosslinking agents, coupling agents, antioxidants, ultraviolet absorbers, etc., to improve the crosslinking degree, weather resistance, bonding strength, and anti-aging properties of the second adhesive film layer. It is understood that the second adhesive film layers located on both surfaces of the solar cell may be made of the same or different materials.
[0064] This application also provides a method for preparing a photovoltaic module, referring to... Figure 3 The preparation method includes: S1: Provides battery cells.
[0065] In this step, cell 4 can be any of the aforementioned cell types. Before proceeding to subsequent processes, cell 4 typically undergoes electrical performance sorting (classified by parameters such as power and current) to ensure performance matching among cells 4 within the module and reduce mismatch losses. Simultaneously, visual inspection is required to remove cells 4 with defects such as microcracks, fragments, or color differences.
[0066] In addition, preparation work for interconnect strip 5 is also included. Interconnect strip 5 (i.e., solder strip) usually needs to be prepared in advance or cut to a suitable length. For interconnect strip 5 using a low-temperature tin-lead-bismuth system, it needs to be immersed in flux in advance to ensure wettability and reliability during soldering.
[0067] S2: Interconnecting strips and the first adhesive film layer are placed sequentially on the surface of the battery cells for stringing.
[0068] In this step, the interconnecting strip 5 is placed on the surface of the battery cell 4, and then the first adhesive film layer 6 is covered. Multiple battery cells 4 are connected in series to form a battery string through stringing.
[0069] The interconnecting strip 5 is precisely placed at the corresponding positions of the front and / or back electrodes of the battery cell 4. For OBB batteries, the interconnecting strip 5 is directly aligned with the fine grid lines or pads on the surface of the battery cell 4. In this invention, the interconnecting strip 5 is fixed by an adhesive film fixing method, that is, after the interconnecting strip 5 is arranged on the surface of the battery cell 4, it is temporarily fixed by the first adhesive film layer 6.
[0070] Then, the first adhesive film layer 6 is placed on the surface of the interconnecting strip 5 away from the battery cell 4. Its function is to fix the interconnecting strip 5 and provide encapsulation protection.
[0071] Specifically, the first adhesive film layer 6 is disposed on the surface of the interconnect strip 5 away from the battery cell 4, and the first adhesive film layer 6 is disposed in such a way that the first sub-adhesive film layer 2 with a low elastic modulus contacts the interconnect strip 5. The first sub-adhesive film layer 2 with a lower elastic modulus (closer to the battery cell / interconnect strip) is more likely to flow and deform during lamination, which can fully wrap the interconnect strip and fill the tiny gaps between it and the battery cell, ensuring close contact; while the second sub-adhesive film layer 4 with a higher elastic modulus (away from the battery cell) provides sufficient structural support and impact protection to prevent the battery cell 4 from microcracking due to stress in subsequent processes.
[0072] Finally, multiple battery cells 4 are connected in series to form a battery string by interconnecting strips. The stringing can be completed by a string welding machine: the battery cells 4 are arranged on the welding table, and the interconnecting strips 5 connect adjacent battery cells (the front of one battery cell to the back of the adjacent battery cell), and then welded to form a battery string.
[0073] In this step, the first film layer 6 can also be formed first by co-extrusion or coating.
[0074] S3: Based on the battery cells after string processing, a second adhesive layer and a protective layer are placed sequentially on the surface of the first adhesive layer.
[0075] In this step, a second adhesive film layer 7 and a protective layer are sequentially applied to the battery string that has already been processed into a string, thus completing the preparation for lamination.
[0076] Specifically, a second encapsulating layer 7 is disposed on the surface of the first encapsulating layer 6 away from the solar cell 4. Preferably, the second encapsulating layer 7 is disposed on both the front and back surfaces of the first encapsulating layer 6. The second encapsulating layer 7 and the first encapsulating layer 6 together constitute a complete encapsulation system, encapsulating the solar cell string. The second encapsulating layer 7 typically also needs to have good light transmittance (when located on the front of the module) or anti-aging properties (when located on the back of the module).
[0077] Then, a first protective layer 8 is provided on the front side of the battery cell 4, and a second protective layer 9 is provided on the back side of the battery cell. Thus, for example, a structure can be formed in which the second protective layer 9, the second adhesive film layer 7, the first adhesive film layer 6, the interconnecting strip 5, the battery cell 4, the interconnecting strip 5, the first adhesive film layer 6, the second adhesive film layer 7, and the first protective layer 8 are stacked sequentially from bottom to top in the thickness direction.
[0078] S4: Perform lamination to create an electrical connection between the interconnect strips and the contact area of the battery cells, and encapsulate each layer of material into a single unit.
[0079] In this step, the stacked materials are fed into a laminator and laminated under vacuum and heating conditions to form an electrical connection between the interconnecting strip 5 and the battery cell 4, and to encapsulate each layer of material into a whole.
[0080] During the lamination process, the solder layer (such as Sn-Pb-Bi low-temperature solder) on the surface of the interconnect strip 5 is heated and melted, and undergoes an alloying reaction with the grid lines or pads of the battery cell 4 to form a reliable ohmic contact (i.e., electrical connection).
[0081] At the same time, the first adhesive film layer 6 and the second adhesive film layer 7 undergo cross-linking and curing at the lamination temperature, firmly encapsulating all materials such as the battery cell 4, interconnect strip 5, and protective layer (such as the glass box backplate) into a whole.
[0082] In the first adhesive film layer 6, the first sub-adhesive film layer 2, with its lower elastic modulus, can fully encapsulate the interconnect strips and fill the tiny gaps between them and the solar cells after being heated and flowing, ensuring tight contact and reliable current transmission. The second sub-adhesive film layer 1, with its higher elastic modulus, maintains better structural integrity and provides mechanical support.
[0083] S5: After lamination, subsequent components are installed to complete the fabrication of the photovoltaic module.
[0084] In this step, after lamination is completed, subsequent processes such as frame installation and junction box installation are carried out to complete the final fabrication of photovoltaic module 10.
[0085] All processes in this step can employ conventional techniques known to those skilled in the art. For example, the laminated components can be fitted into an aluminum alloy frame, which serves to reinforce the structure, provide sealing protection, and facilitate installation.
[0086] Then, a junction box is installed on the back of the component. The junction box is the interface for connecting the component to external circuitry.
[0087] The solder pads inside the junction box need to be soldered to the busbars extending from the back of the module. The junction box typically contains bypass diodes to protect the module from hot spot damage when the cells are shaded.
[0088] Optionally, after the subsequent components are installed, the components need to undergo electrical performance testing (such as IV curve testing) to verify whether the components' output power, open-circuit voltage, short-circuit current and other parameters meet the standards.
[0089] The photovoltaic module provided in this application embodiment can achieve a "flexible inside and rigid outside" double-layer structure through simple process methods and optimized design of the first encapsulant layer material. This structure, achieved through precise control of the product's elastic modulus, balances the full wrapping of interconnect strips (ensuring reliable electrical connections) and structural support (ensuring mechanical reliability such as resistance to microcracks) during lamination. This enhances both product reliability and process performance.
[0090] This application provides a photovoltaic system 1000, such as... Figure 4As shown, the photovoltaic system 1000 can be applied in photovoltaic power plants, such as ground power plants, rooftop power plants, and water-based power plants. It can also be applied to equipment or devices that use solar energy to generate electricity, such as user solar power supplies, solar streetlights, solar cars, solar buildings, and so on.
[0091] It is understandable that the application scenarios of the photovoltaic system 1000 are not limited to this; that is to say, the photovoltaic system 1000 can be applied in all fields that require solar power generation. Taking a photovoltaic power generation system as an example, the photovoltaic system 1000 may include a photovoltaic array, a combiner box, and an inverter. The photovoltaic array may be an array combination of multiple photovoltaic modules 10 mentioned above. For example, multiple photovoltaic modules 10 can form multiple photovoltaic arrays. The photovoltaic array is connected to the combiner box, which can collect the current generated by the photovoltaic array. The collected current flows through the inverter and is converted into AC power required by the mains power grid before being connected to the mains power grid to realize solar power supply.
[0092] The photovoltaic module of the present invention will be further described below with reference to embodiments.
[0093] It should be noted that the photovoltaic modules in the following embodiments and comparative examples are identical in structure except for the first encapsulant layer, and the methods for preparing the photovoltaic modules are the same.
[0094] Example 1
[0095] A photovoltaic module, from bottom to top, consists of: a backsheet, a second encapsulant layer, a first encapsulant layer, interconnect strips, solar cells, interconnect strips, a first encapsulant layer, a second encapsulant layer, and a glass layer.
[0096] The first adhesive film layer comprises a two-layer structure, specifically a first sub-adhesive film layer and a second sub-adhesive film layer stacked sequentially along the direction away from the battery cell. The elastic modulus of the first sub-adhesive film layer is 5 MPa, and the elastic modulus of the second sub-adhesive film layer is 40 MPa.
[0097] Example 2
[0098] A photovoltaic module, from bottom to top, consists of: a backsheet, a second encapsulant layer, a first encapsulant layer, interconnect strips, solar cells, interconnect strips, a first encapsulant layer, a second encapsulant layer, and a glass layer.
[0099] The first encapsulant layer comprises a three-layer structure, specifically consisting of a first sub-encapsulant layer, a second sub-encapsulant layer, and a first sub-encapsulant layer stacked sequentially along the direction away from the battery cell. The elastic modulus of the first sub-encapsulant layer is 5 MPa, and the elastic modulus of the second sub-encapsulant layer is 40 MPa.
[0100] Example 3
[0101] A photovoltaic module, from bottom to top, consists of: a backsheet, a second encapsulant layer, a first encapsulant layer, interconnect strips, solar cells, interconnect strips, a first encapsulant layer, a second encapsulant layer, and a glass layer.
[0102] The first encapsulant layer comprises a three-layer structure, specifically consisting of a first sub-encapsulant layer, a second sub-encapsulant layer, and a first sub-encapsulant layer stacked sequentially along the direction away from the battery cell. The elastic modulus of the first sub-encapsulant layer is 15 MPa, and the elastic modulus of the second sub-encapsulant layer is 60 MPa.
[0103] Example 4
[0104] A photovoltaic module, from bottom to top, consists of: a backsheet, a second encapsulant layer, a first encapsulant layer, interconnect strips, solar cells, interconnect strips, a first encapsulant layer, a second encapsulant layer, and a glass layer.
[0105] The first encapsulant layer comprises a three-layer structure, specifically a first sub-encapsulant layer, a second sub-encapsulant layer, and a third sub-encapsulant layer stacked sequentially along the direction away from the battery cell. The elastic modulus of the first sub-encapsulant layer is 10 MPa, and the elastic modulus of the second sub-encapsulant layer is 50 MPa.
[0106] Example 5
[0107] A photovoltaic module, from bottom to top, consists of: a backsheet, a second encapsulant layer, a first encapsulant layer, interconnect strips, solar cells, interconnect strips, a first encapsulant layer, a second encapsulant layer, and a glass layer.
[0108] The first encapsulant layer comprises a three-layer structure, specifically a first sub-encapsulant layer, a second sub-encapsulant layer, and a third sub-encapsulant layer stacked sequentially along the direction away from the battery cell. The elastic modulus of the first sub-encapsulant layer is 10 MPa, the elastic modulus of the second sub-encapsulant layer is 50 MPa, and the elastic modulus of the third sub-encapsulant layer is 60 MPa.
[0109] Comparative Example 1
[0110] A photovoltaic module, from bottom to top, consists of: a backsheet, a second encapsulant layer, a first encapsulant layer, interconnect strips, solar cells, interconnect strips, a first encapsulant layer, a second encapsulant layer, and a glass layer.
[0111] The first adhesive film layer has a single-layer structure and an elastic modulus of 10 MPa.
[0112] Comparative Example 2
[0113] A photovoltaic module, from bottom to top, consists of: a backsheet, a second encapsulant layer, a first encapsulant layer, interconnect strips, solar cells, interconnect strips, a first encapsulant layer, a second encapsulant layer, and a glass layer.
[0114] The first adhesive film layer has a single-layer structure and an elastic modulus of 50 MPa.
[0115] The photovoltaic modules in Examples 1 to 5 and Comparative Examples 1 to 2 were subjected to TC reliability testing, and the results are shown in Table 1 below.
[0116] In Table 1, the TC reliability degradation percentage refers to the percentage decrease in power after the TC reliability test compared to before the TC reliability test. The specific test method for the TC reliability degradation percentage is as follows: After initially performing a power test (T0) on the photovoltaic modules in Examples 1 to 5 and Comparative Examples 1 to 2, they were placed in a standard temperature environment ranging from -40℃ to +85℃ for 200 high and low temperature cycles. Then, after removal, the power (T0) of the photovoltaic modules was tested again. 200 The percentage of TC reliability degradation is calculated using the following formula.
[0117] TC reliability degradation percentage = (T0 - T) 200 ) / T0
[0118] Air pressure value refers to the air pressure value of the suction cup during the film application process.
[0119] Table 1
[0120] As can be seen from Table 1 above, when the structure of the first adhesive film layer according to the present invention is adopted, after high and low temperature cycles of TC reliability testing, the TC reliability decay percentage is lower than that of the comparative example, which indicates that the TC reliability is improved; at the same time, since the low elastic modulus quantum adhesive film layer is in contact with the suction cup during the process, the air pressure value of the suction cup is effectively reduced, and the process stability is improved.
Claims
1. A photovoltaic module, characterized by, include: Battery cells; Interconnecting strips are disposed on the surface of the battery cell; A first adhesive film layer is disposed on the surface of the interconnect strip away from the battery cell, and includes at least a first sub-adhesive film layer and a second sub-adhesive film layer stacked sequentially in a direction away from the battery cell, wherein the elastic modulus of the first sub-adhesive film layer is less than the elastic modulus of the second sub-adhesive film layer. A second adhesive film layer is disposed on the surface of the first adhesive film layer away from the battery cell. A protective layer is disposed on the surface of the second adhesive film layer away from the battery cell.
2. The photovoltaic module according to claim 1, characterized in that, The elastic modulus of the first sub-film layer ranges from 5 MPa to 15 MPa, and the elastic modulus of the second sub-film layer ranges from 40 MPa to 60 MPa.
3. The photovoltaic module according to claim 2, characterized in that, The first adhesive film layer includes a first sub-adhesive film layer and a second sub-adhesive film layer stacked sequentially in a direction away from the battery cell. The first sub-adhesive film layer is in contact with the surface of the interconnect strip away from the battery cell, and the second sub-adhesive film layer is in contact with the surface of the second adhesive film layer close to the battery cell.
4. The photovoltaic module according to claim 1 or 2, characterized in that, The first adhesive film layer includes two first sub-adhesive film layers disposed opposite each other and a second sub-adhesive film layer located between the two first sub-adhesive film layers. One of the first sub-adhesive film layers is in contact with the surface of the interconnect strip away from the battery cell, and the other of the first sub-adhesive film layers is in contact with the surface of the second adhesive film layer close to the battery cell.
5. The photovoltaic module according to claim 1 or 2, characterized in that, The first adhesive film layer includes a first sub-adhesive film layer, a second sub-adhesive film layer, and a third sub-adhesive film layer sequentially disposed on the surface of the interconnect strip away from the battery cell. The first sub-adhesive film layer is in contact with the surface of the interconnect strip away from the battery cell, and the third sub-adhesive film layer is in contact with the surface of the second adhesive film layer close to the battery cell. The elastic modulus of the second sub-adhesive film layer is less than that of the third sub-adhesive film layer.
6. The photovoltaic module according to claim 1 or 2, characterized in that, The total thickness of the first adhesive film layer ranges from 40 μm to 150 μm.
7. The photovoltaic module according to claim 1, characterized in that, The thickness of the second sub-film layer is not less than 50% of the total thickness of the first film layer.
8. The photovoltaic module according to claim 7, characterized in that, The thickness of the first sub-film layer is not less than 10 μm.
9. The photovoltaic module according to claim 1, characterized in that, The first adhesive film layer includes either EVA or TPO.
10. The photovoltaic module according to claim 1, characterized in that, The second adhesive film layer includes any one of EVA, EPE, POE, PVB, PET or liquid silicone.
11. A method for preparing a photovoltaic module, characterized in that, include: Provide battery cells; Interconnecting strips and a first adhesive film layer are sequentially placed on the surface of the battery cell and then strung together. The first adhesive film layer is disposed on the surface of the interconnecting strip away from the battery cell and includes at least a first sub-adhesive film layer and a second sub-adhesive film layer stacked sequentially in a direction away from the battery cell. The elastic modulus of the first sub-adhesive film layer is less than that of the second sub-adhesive film layer. Based on the battery cells after string processing, a second adhesive film layer and a protective layer are sequentially placed on the surface of the first adhesive film layer; the second adhesive film layer is disposed on the surface of the first adhesive film layer away from the battery cell. A lamination process is performed to make the interconnecting strips electrically connected to the contact area of the battery cell, and to encapsulate the layers of material into a single unit; After lamination, subsequent components are installed to complete the fabrication of the photovoltaic module.
12. The method for preparing a photovoltaic module according to claim 11, characterized in that, The preparation method further includes: The first film layer is formed by co-extrusion or coating.
13. A photovoltaic system, characterized in that, Including the photovoltaic module as described in any one of claims 1 to 10.