Full-depletion broadband high-temperature working mercury cadmium telluride infrared material structure, detector and regulation method

By designing a stepped band structure and gradient depletion region in mercury cadmium telluride infrared materials, the problems of large dark current and narrow spectral response of fully depleted p-ν(π)-n structures were solved, realizing a wide-band spectral response and broadening of the process window at high temperatures, adapting to complex temperature field detection.

CN123164852APending Publication Date: 2026-11-2411TH RES INST OF CHINA ELECTRONICS TECH GROUP CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611112195.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-24
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing fully depleted p-ν(π)-n structure mercury cadmium telluride infrared detectors have large dark currents and narrow spectral response ranges at high temperatures, making them unsuitable for complex temperature environments. They also have narrow process windows and are difficult to control doping concentration, leading to device performance degradation.

Method used

A fully depleted, broadband, high-temperature operating mercury cadmium telluride infrared material with a stepped band structure was designed. By forming a gradient depletion region within the absorption region, utilizing the cadmium composition and band structure of different layers, and combining reverse bias to control the depletion region boundary, the spectral response was broadened and the dark current was reduced.

Benefits of technology

It broadens the process window, reduces dark current, expands the spectral response range, and enables high-precision detection of different temperature fields, adapting to complex temperature field environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123164852A_ABST
    Figure CN123164852A_ABST
Patent Text Reader

Abstract

The application discloses a full-depletion broadband high-temperature working tellurium-cadmium-mercury infrared material structure, a detector and a regulation and control method, relates to semiconductor and photoelectric material technology, and specifically comprises, from bottom to top, a substrate, an N+ type contact layer, a first transition layer, an absorption zone, a second transition layer and a P+ type contact layer. The absorption zone is provided with three sublayers v1, v2 and v3 with gradually increased cadmium components from bottom to top, so as to form a stepped energy band structure with gradually increased band gaps; the cadmium components of the N+ type and P+ type contact layers are higher than the highest component of the absorption zone, so as to shield the electric field from invading the heavily doped zone. The wide band gap characteristic of the third absorption sublayer v3 with a high component is used to guide the depletion zone to extend from the high band gap end to the low band gap end, so that the SRH recombination current is effectively inhibited; the intrinsic carrier concentration gradient of the absorption zone reduces the sensitivity to the doping concentration, and significantly widens the epitaxial process window.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the fields of semiconductor and optoelectronic materials technology, and in particular to a fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure, detector and control method. Background Technology

[0002] Infrared focal plane array detectors are widely used in industrial, environmental, and medical detection fields. Among numerous infrared detection materials, mercury cadmium telluride (HgCdTe) semiconductor materials have become the preferred detection material in the infrared band due to their advantages such as tunable bandwidth, high infrared absorption coefficient, and excellent carrier mobility. Currently, the mainstream detector structures include p-on-n and n-on-p structures. Although they have achieved large-scale application, they face challenges such as limited depletion region width, insufficient photogenerated carrier collection efficiency, and relatively large dark current, making it difficult to further improve quantum efficiency and detectivity. In addition, at high temperatures, thermally excited carriers significantly degrade device performance, requiring heavy reliance on cooling systems to ensure operational stability, which cannot meet the application requirements of lightweight and portable detection devices.

[0003] The fully depleted p-ν(π)-n structure is widely recognized in the international infrared detection field as one of the technologies with the greatest development potential. Its core principle is to reduce the carrier concentration in the absorption region to below the intrinsic carrier concentration through the effects of repulsion junction and extraction junction, thereby suppressing dark current and increasing operating temperature. Although there are relatively mature technical solutions for the fully depleted p-ν(π)-n structure, its narrow spectral response range is inevitably insufficient for infrared detection in complex application scenarios, such as infrared detection with a wide temperature range and complex temperature fields, making it difficult to achieve high-precision detection of different temperature fields.

[0004] Currently, there are still some technical problems in the processing and performance of fully depleted p-ν(π)-n structure mercury cadmium telluride materials: First, the higher the doping concentration, the higher the depletion voltage. If the doping concentration is unexpectedly high during the process, resulting in an excessively high depletion voltage, it will lead to an increase in dark current.

[0005] Secondly, the extremely low doping level in the absorption region places extremely high demands on the epitaxial process, making the process difficult to implement and the process window narrow. Even slight changes in epitaxial conditions can lead to changes in doping concentration, which in turn can lead to significant changes in the concentration of doped carriers in the material structure, resulting in the deterioration of material performance.

[0006] In addition, the spectral response of traditional fully depleted p-ν(π)-n structure mercury cadmium telluride materials is relatively simple and cannot be controlled by external bias voltage, resulting in insufficient adaptability to complex temperature fields. Summary of the Invention

[0007] This application provides a fully depleted wideband high-temperature working mercury cadmium telluride infrared material structure, detector, and control method, which broadens the spectral response while relaxing the doping concentration and expanding the process window.

[0008] This application provides a fully depleted broadband high-temperature working mercury cadmium telluride infrared material structure, including a substrate, an N+ type contact layer, a first transition layer, an absorption region, a second transition layer, and a P+ type contact layer stacked sequentially from bottom to top; The absorption region includes a first absorber layer, a second absorber layer, and a third absorber layer stacked sequentially along the growth direction. The cadmium content of the third absorber layer is greater than that of the first absorber layer, so as to form a stepped band structure with a gradually increasing band gap along the light incident direction in the absorption region. The cadmium composition values ​​of the N+ type contact layer and the P+ type contact layer are both higher than the cadmium composition value of the third absorber layer, so as to confine the depletion region to the inside of the absorption region.

[0009] This application also provides an infrared detector, including the aforementioned fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure.

[0010] This application also provides a method for modulating the spectral response of a fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure, comprising the following steps: A reverse bias voltage is applied between the P+ type contact layer and the N+ type contact layer; By adjusting the magnitude of the reverse bias voltage, the depletion region boundary within the absorption region is controlled to extend along the direction from the first absorber sublayer to the third absorber sublayer. When the reverse bias voltage is in the first preset range, the depletion region mainly covers the third absorber layer, and the detector response is in the short mid-wave infrared band. When the reverse bias voltage increases to the second preset range, the depletion region covers the third absorber layer and the second absorber layer, and the detector responds to the sub-short-medium wave infrared band. When the reverse bias voltage increases to the third preset range, the depletion region covers the third absorber layer, the second absorber layer and the first absorber layer, and the detector responds to a longer mid-wave infrared band.

[0011] This application embodiment designs a stepped composition in the absorption region and, through band engineering, achieves gradient depletion of carrier concentration under different applied bias voltages by varying the band structure and carrier concentration of the fully depleted structure in different layers. This reduces dark current and can broaden the spectral response while relaxing the doping concentration and expanding the process window.

[0012] The above description is only an overview of the technical solution of this application. In order to better understand the technical means of this application and to implement it in accordance with the contents of the specification, and to make the above and other objects, features and advantages of this application more obvious and understandable, the following are specific embodiments of this application. Attached Figure Description

[0013] Various other advantages and benefits will become apparent to those skilled in the art upon reading the following detailed description of preferred embodiments. The accompanying drawings are for illustrative purposes only and are not intended to limit the scope of this application. Furthermore, the same reference numerals denote the same parts throughout the drawings. In the drawings: Figure 1 This is a schematic diagram of the infrared material structure of mercury cadmium telluride according to an embodiment of this application; Figure 2 This is a schematic diagram illustrating the compositional variation with depth of the fully depleted broadband p-ν-n heterojunction mercury cadmium telluride material in a specific example of this application. Figure 3 This is a schematic diagram illustrating the compositional variation with depth of a fully depleted broadband p-ν-n heterojunction mercury cadmium telluride material in a specific example of this application. Detailed Implementation

[0014] Exemplary embodiments of the present disclosure will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of the present disclosure are shown in the drawings, it should be understood that the present disclosure may be implemented in various forms and should not be limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the disclosure to those skilled in the art.

[0015] This application provides a fully depleted, wide-band, high-temperature operating mercury cadmium telluride infrared material structure, such as... Figure 1 As shown, the structure includes a substrate, an N+ type contact layer, a first transition layer, an absorption region ν, a second transition layer, and a P+ type contact layer, stacked sequentially from bottom to top. In some embodiments, the substrate is a substrate for growing mercury cadmium telluride, such as cadmium zinc telluride, silicon, germanium, or gallium arsenide.

[0016] like Figure 1 As shown, the absorption region ν includes a first absorber sublayer ν1, a second absorber sublayer ν2, and a third absorber sublayer stacked sequentially along the growth direction. v 3. The cadmium content of the third absorber layer is greater than that of the first absorber layer, so as to form a stepped band structure with a gradually increasing band gap along the light incident direction in the absorption region.

[0017] The cadmium composition values ​​of the N+ type contact layer and the P+ type contact layer are both higher than the cadmium composition value of the third absorber layer, so as to confine the depletion region to the inside of the absorption region.

[0018] In some embodiments, the N+ type contact layer is a highly doped n-type layer with a high cadmium composition. The cadmium composition value of the N+ type contact layer is at least 0.05 higher than that of the first absorber layer ν1. An exemplary thickness range is 1 μm to 8 μm, and the doping concentration is greater than 1× / Since the absorption region is heavily doped, when the absorption region is in a fully depleted state, the electric field extends to the N+ type contact layer. At this time, defects in the highly doped region will increase the recombination current. In this application, the composition value of the N+ type contact layer is designed to be higher than that of the absorption region ν, so as to shield the high defect region from the electric field and suppress dark current. At the same time, as a window layer that directly contacts the electrode, the high composition can reduce the loss of absorption wavelength in the heavily doped region.

[0019] In some embodiments, the first absorber sublayer v 1. Second absorber sublayer v 2 and the third absorber sublayer v The cadmium content of layer 3 ranges from 0.2 to 0.45, with the cadmium content increasing progressively from bottom to top, and the difference in cadmium content among the three layers ranging from 0.01 to 0.05. This application's first absorber sublayer... v 1. Second absorber sublayer v 2 and the third absorber sublayer v 3. Covering the short-wave to long-wave region, each layer has a thickness of 1.0 μm to 3.0 μm, and the overall doping concentration of the absorption region is less than 1× / .

[0020] In some embodiments, the first transition layer G1 is connected to the N+ type contact layer and the first absorber layer. v Between 1 and 1, and the cadmium composition changes linearly from the cadmium composition value of the N+ type contact layer to the first absorber layer. v The cadmium composition value of 1 has a gradient of 0.05~0.1 / μm and a thickness range of 0.5~1.5μm.

[0021] In some embodiments, the second transition layer G2 is connected to the third absorber layer. v 3. Between the P+ type contact layer and the cadmium component, the cadmium component is separated from the third absorber layer. v The cadmium composition value of 3 is linearly and gradually changed to the cadmium composition value of the P+ type contact layer, with a gradient of 0.05~0.1 / μm.

[0022] In some other embodiments, the P+ type contact layer is a highly doped p-type layer with a high cadmium content, and the cadmium content of the P+ type contact layer is higher than that of the third absorber layer. v The cadmium composition value of 3 is at least 0.05, the exemplary doping thickness is 1.0 μm to 3.0 μm, and the doping concentration is greater than 1× / The reason why the component values ​​of the P+ type contact layer are higher than those of the absorber layer is the same as that of the N+ layer, and will not be elaborated here.

[0023] In some embodiments, the N+ type contact layer and the absorption region v The total thickness of the P+ type contact layer is greater than or equal to 5 μm to ensure that long-wave infrared light is fully absorbed.

[0024] In some embodiments, the N+ type contact layer and the P+ type contact layer are heavily doped with indium or iodine to achieve n-type heavy doping, and heavily doped with arsenic or copper to achieve p-type heavy doping.

[0025] Compared with existing technologies, the gradient depletion mechanism of this application has a higher component content. v 3. With a larger band gap and lower intrinsic carrier concentration, it preferentially depletes under an applied bias voltage, and the depletion region gradually moves towards... v 1. Directional extension. The gradient depletion mechanism can effectively suppress SRH-recombination current, thereby reducing device dark current.

[0026] The structural process window of this application is widened. Due to the compositional steps in the absorption region, there is a gradient in the intrinsic carrier concentration. To achieve the same carrier concentration in the material, the doping concentration can be appropriately relaxed, thus widening the process window.

[0027] The structure of this application broadens the spectral response. Since different components in the absorption region correspond to different cutoff wavelengths, the combination of the three sublayers can broaden the spectral response range of the detector by 15% to 20%. Furthermore, by adjusting the magnitude of the reverse bias voltage, different sublayers can be selectively depleted, thereby achieving tunability of the spectral response.

[0028] according to Figure 1 The present application also provides specific application examples of the above-mentioned mercury cadmium telluride infrared material structure, as shown in the example. Figure 2 The compositional variation with depth is shown. Excluding the substrate, the structural parameters from bottom to top are as follows: 1. High-component, highly doped n-type layer (N + (layer), N + A 2.5 μm thick layer of mercury cadmium telluride was grown with a cadmium composition of 0.40. In was used as the n-type dopant with a doping concentration of 2 × 10⁻⁶. 17 cm -3 .

[0029] 2. Gradient transition layer (G1 layer): The G1 layer has a growth thickness of 1 μm. The composition value in the gradient region linearly transitions from 0.40 to 0.28. As is used as the p-type dopant, with a doping concentration starting from 5 × 10⁻⁶. 13 cm -3Gaussian gradient to 2×10 17 cm -3 3. The lightly doped n-type absorption region (ν layer) is divided into three stepped composition regions (ν1, ν2, ν3), each with a growth thickness of 2 μm and a 0.2 μm composition gradient region in the middle. The composition values ​​are 0.28, 0.30, and 0.32, respectively. In is used as the n-type dopant with a doping concentration of 5 × 10⁻⁶. 13 cm -3 .

[0030] 4. Gradient transition layer (G2 layer): The G2 layer has a growth thickness of 0.8 μm, with the composition value linearly varying from 0.32 to 0.43. As is used as the p-type dopant, with a doping concentration starting from 5 × 10⁻⁶. 13 cm -3 Gaussian gradient to 4×10 17 cm -3 .

[0031] 5. High-component, highly doped p-type layer (P + (layer), P + The layer was 1.2 μm thick with a composition of 0.43, using As as the dopant at a concentration of 4 × 10⁻⁶. 17 cm -3 .

[0032] according to Figure 3 As shown, at a high temperature of 230K, without reverse bias, the carrier concentration in the material is mainly intrinsic carriers. Under an applied bias, the hole concentration decreases rapidly: at a reverse bias of 0.08V, the ν3 region is depleted first, with a concentration lower than the doping concentration; at a reverse bias of 0.1V, the ν2 region continues to be depleted, with a concentration lower than the doping concentration. By applying an applied bias, a stepwise depletion of the absorption region can be achieved; at a reverse bias of 0.6V, the hole concentration decreases to ~10-10 6 cm -3 Extremely low level.

[0033] This application also proposes an infrared detector, including the aforementioned fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure.

[0034] This application also proposes a method for modulating the spectral response of a fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure, comprising the following steps: A reverse bias voltage is applied between the P+ type contact layer and the N+ type contact layer; By adjusting the magnitude of the reverse bias voltage, the depletion region boundary within the absorption region is controlled to extend along the direction from the first absorber sublayer to the third absorber sublayer. When the reverse bias voltage is in the first preset range, the depletion region mainly covers the third absorber layer, and the detector responds to the first mid-wave infrared band. When the reverse bias voltage increases to the second preset range, the depletion region covers the third absorber layer and the second absorber layer, and the detector responds to the second mid-wave infrared band. When the reverse bias voltage increases to the third preset range, the depletion region covers the third absorber layer, the second absorber layer, and the first absorber layer. The detector responds to the third mid-wave infrared band, wherein the wavelength of the first mid-wave infrared band is shorter than the wavelength of the second mid-wave infrared band, and the wavelength of the second mid-wave infrared band is shorter than the wavelength of the third mid-wave infrared band. For example, the first mid-wave infrared band can be a shorter mid-wave infrared band, the second mid-wave infrared band can be a second shorter mid-wave infrared band, and the third mid-wave infrared band can be a longer mid-wave infrared band.

[0035] It should be noted that, in the embodiments of this application, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes that element.

[0036] The sequence numbers of the embodiments in this application are for descriptive purposes only and do not represent the superiority or inferiority of the embodiments.

[0037] Through the above description of the embodiments, those skilled in the art can clearly understand that the methods of the above embodiments can be implemented by means of software plus necessary general-purpose hardware platforms. Of course, they can also be implemented by hardware, but in many cases the former is a better implementation method. Based on this understanding, the technical solution of this application, in essence, or the part that contributes to the prior art, can be embodied in the form of a software product. This computer software product is stored in a storage medium (such as ROM / RAM, magnetic disk, optical disk) and includes several instructions to cause a terminal (which may be a mobile phone, computer, server, air conditioner, or network device, etc.) to execute the methods described in the various embodiments of this application.

[0038] The embodiments of this application have been described above with reference to the accompanying drawings. However, this application is not limited to the specific embodiments described above. The specific embodiments described above are merely illustrative and not restrictive. Those skilled in the art can make many other forms under the guidance of this application without departing from the spirit and scope of the claims. All of these forms are within the protection scope of this application.

Claims

1. A fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure, characterized in that, It includes a substrate, an N+ type contact layer, a first transition layer, an absorption region, a second transition layer, and a P+ type contact layer, which are stacked sequentially from bottom to top; The absorption region includes a first absorber layer, a second absorber layer, and a third absorber layer stacked sequentially along the growth direction. The cadmium content of the third absorber layer is greater than that of the first absorber layer, so as to form a stepped band structure with a gradually increasing band gap along the light incident direction in the absorption region. The cadmium composition values ​​of the N+ type contact layer and the P+ type contact layer are both higher than the cadmium composition value of the third absorber layer, so as to confine the depletion region to the inside of the absorption region.

2. The fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure as described in claim 1, characterized in that, In the absorption region, the cadmium composition of the first absorber layer, the second absorber layer, and the third absorber layer ranges from 0.2 to 0.45, and the difference in cadmium composition among the three layers ranges from 0.01 to 0.

05. The overall doping concentration of the absorption region is less than 1× / .

3. The fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure as described in claim 1, characterized in that, The first transition layer connects the N+ type contact layer and the first absorber layer, and the cadmium composition changes linearly from the cadmium composition value of the N+ type contact layer to the cadmium composition value of the first absorber layer, with a gradient of 0.05~0.1 / μm.

4. The fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure as described in claim 3, characterized in that, The second transition layer is connected between the third absorber layer and the P+ type contact layer, and the cadmium composition changes linearly from the cadmium composition value of the third absorber layer to the cadmium composition value of the P+ type contact layer, with a gradient of 0.05~0.1 / μm.

5. The fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure as described in claim 1, characterized in that, The cadmium composition value of the N+ type contact layer is at least 0.05 higher than that of the first absorber layer, and the doping concentration is greater than 1× / ; The cadmium composition value of the P+ type contact layer is at least 0.05 higher than that of the third absorber layer, and the doping concentration is greater than 1× / .

6. The fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure as described in claim 1, characterized in that, The total thickness of the N+ type contact layer, the absorption region, and the P+ type contact layer is greater than or equal to 5 μm to ensure that long-wave infrared light is fully absorbed.

7. The fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure as described in claim 1, characterized in that, The substrate is selected from one of zinc cadmium telluride, silicon, germanium, or gallium arsenide; The N+ type contact layer and P+ type contact layer are heavily doped with indium or iodine to achieve n-type doping, and heavily doped with arsenic or copper to achieve p-type doping.

8. An infrared detector, characterized in that, Includes the fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure as described in any one of claims 1 to 7.

9. A method for modulating the spectral response of a fully depleted broadband high-temperature operating mercury cadmium telluride infrared material structure according to any one of claims 1 to 7, characterized in that, Includes the following steps: A reverse bias voltage is applied between the P+ type contact layer and the N+ type contact layer; By adjusting the magnitude of the reverse bias voltage, the depletion region boundary within the absorption region is controlled to extend along the direction from the first absorber sublayer to the third absorber sublayer. When the reverse bias voltage is in the first preset range, the depletion region mainly covers the third absorber layer, and the detector responds to the first mid-wave infrared band. When the reverse bias voltage increases to the second preset range, the depletion region covers the third absorber layer and the second absorber layer, and the detector responds to the second mid-wave infrared band. When the reverse bias voltage increases to the third preset range, the depletion region covers the third absorber layer, the second absorber layer and the first absorber layer, and the detector responds to the third mid-wave infrared band, wherein the wavelength of the first mid-wave infrared band is smaller than the wavelength of the second mid-wave infrared band, and the wavelength of the second mid-wave infrared band is smaller than the wavelength of the third mid-wave infrared band.