Method for manufacturing a curved photovoltaic module, manufacturing device, curved photovoltaic module
By controlling the vacuuming rate of the vacuum bag and gradually bending the flexible plate and encapsulating film, the problem of hidden cracks in curved photovoltaic modules during the bending process was solved, and efficient fabrication of curved photovoltaic modules was achieved.
Patent Information
- Application Number
- CN202510662040.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-21
- Publication Date
- 2026-11-24
AI Technical Summary
Existing curved photovoltaic modules are prone to developing microcracks during the bending process.
By controlling the vacuuming rate of the vacuum bag, and using a method where the first vacuuming rate is less than the second vacuuming rate, the flexible plate, encapsulation film, and battery are gradually bent to prevent microcracks from forming.
It effectively prevents microcracks in the battery during bending, reduces the difficulty of lamination processing, and improves product yield and production efficiency.
Smart Images

Figure CN123164864A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of photovoltaic module technology, and more specifically, to a method, apparatus, and method for preparing a curved photovoltaic module. Background Technology
[0002] Building-integrated photovoltaics (BIPV) involves installing photovoltaic modules on the surface of a building's exterior envelope to provide electricity. These modules also function as a part of the building structure, replacing some traditional structural elements such as roofing panels, tiles, windows, facades, and awnings. BIPV modules can also be made into multifunctional building components to achieve more functions, such as photovoltaic thermal systems, integration with lighting, and building shading. With the increasing popularity of BIPV, photovoltaic tiles, which can replace traditional roofing tiles, have emerged to better integrate with building surfaces. Compared to flat tiles, curved photovoltaic tiles, due to their unique shape, are more suitable for high-end buildings and can replace traditional clay tiles, combining aesthetics and power generation. Because crystalline silicon solar cells are prone to microcracks when bent, most curved tiles on the market currently use thin-film solar cells. Compared to thin-film solar cells, crystalline silicon cells have significant advantages in power generation efficiency and cost, making curved tiles with crystalline silicon cells the future development direction.
[0003] Therefore, a method, apparatus, and method for preparing curved photovoltaic modules that can avoid microcracks have become urgent technical problems to be solved. Summary of the Invention
[0004] The purpose of this invention is to provide a method, apparatus and a curved photovoltaic module that can avoid the occurrence of microcracks, thus solving the problem that existing curved photovoltaic modules are prone to microcracks after bending.
[0005] In view of this, the first aspect of the present invention proposes a method for preparing a curved photovoltaic module.
[0006] A second aspect of the present invention provides an apparatus for fabricating curved photovoltaic modules.
[0007] A third aspect of this invention provides a curved photovoltaic module.
[0008] The present invention provides a method for preparing a curved photovoltaic module, comprising: preparing a module to be encapsulated, the module comprising: a flexible plate, a first encapsulating film, a battery, a second encapsulating film, and curved glass; placing the module to be encapsulated in a vacuum bag; performing a first vacuuming process on the vacuum bag using a first vacuuming rate; performing a lamination process on the vacuum bag after the first vacuuming process, while simultaneously performing a second vacuuming process on the vacuum bag using a second vacuuming rate; and removing the module to be encapsulated from the vacuum bag after the lamination process to obtain a curved photovoltaic module; wherein the first vacuuming rate is less than the second vacuuming rate.
[0009] In this technical solution, a flexible plate, a first encapsulating film, a battery, a second encapsulating film, and curved glass are sequentially stacked to form the component to be encapsulated. The component is placed in a vacuum bag, and a first vacuuming process is performed on the vacuum bag using a first vacuuming rate. This bends the flexible plate, the first encapsulating film, the battery, and the second encapsulating film, causing them to also form a curved structure. The vacuum bag after the first vacuuming process is then laminated, and a second vacuuming process is performed on the vacuum bag using a second vacuuming rate. Because the first vacuuming rate is lower than the second vacuuming rate, the deformation rate of the flexible plate, the first encapsulating film, the battery, and the second encapsulating film is slowed down, thus preventing microcracks caused by the high rigidity of the battery. Therefore, the microcrack problem can be ignored during subsequent lamination, reducing the difficulty of the lamination process.
[0010] In the above technical solution, optionally, the first vacuuming rate and the second vacuuming rate are adjusted by a valve in the vacuuming assembly; when the first vacuuming rate is used, the valve is in the first valve opening ratio, which is greater than or equal to 0.5% and less than or equal to 1%; when the second vacuuming rate is used, the valve is in the second valve opening ratio, which is 100%.
[0011] In this technical solution, the vacuum rate of the vacuum pumping component is controlled by a valve. By reducing the first vacuum pumping rate, the generation of microcracks can be greatly reduced.
[0012] In the above technical solution, optionally, the time for the first vacuuming process is greater than or equal to 15 minutes and less than or equal to 20 minutes. The temperature for the first vacuuming process is greater than or equal to 10°C and less than or equal to 30°C.
[0013] In this technical solution, the initial vacuuming process needs to take more than 15 minutes to ensure the vacuum level in the vacuum bag. Simultaneously, vacuuming at room temperature is sufficient, reducing the difficulty of the initial vacuuming process.
[0014] In the above technical solution, optionally, the lamination temperature is greater than or equal to 145°C and less than or equal to 160°C; and / or the lamination time is greater than or equal to 40 minutes and less than or equal to 60 minutes.
[0015] In this technical solution, the lamination temperature ensures the fusion of the first and second encapsulating films, and the lamination processing time does not need to consider the elimination of microcracks, so it only needs to be greater than or equal to 40 minutes and less than or equal to 60 minutes, thus improving the efficiency of the lamination process.
[0016] Optionally, in the above technical solution, the battery includes a crystalline silicon battery.
[0017] In the above technical solution, optionally, the battery includes either an XBC battery (Back contact solar cell) or a BC battery (Back Contact).
[0018] In the above technical solution, optionally, the flexible sheet includes a PET (Polyethylene Terephthalate) layer and a weather-resistant layer; and / or the first encapsulating film includes one of EVA (Ethylene-vinyl Acetate copolymer), POE (Polyolefin Elastomer), PVB (Polyvinyl Butyral), or silicone film; and / or the second encapsulating film includes one of EVA, POE, PVB, or silicone film.
[0019] In the above technical solution, optionally, the curved glass includes a first curved area, a flat area, and a second curved area; wherein the first curved area and the second curved area are respectively disposed on both sides of the flat area.
[0020] In the above technical solution, optionally, the curvature directions of the first curved surface region and the second curved surface region are opposite; and / or the ratio of the area of the planar region to the area of the curved glass is greater than or equal to 80%; and / or the thickness of the curved glass is greater than or equal to 3mm and less than or equal to 6mm; and / or the radius of curvature of the first curved surface region is greater than or equal to 110mm and less than or equal to 400mm; and / or the radius of curvature of the second curved surface region is greater than or equal to 110mm and less than or equal to 400mm; and / or the radius of curvature of the first curved surface region is the same as the radius of curvature of the second curved surface region.
[0021] According to a second aspect of the present invention, an apparatus for fabricating curved photovoltaic modules is also provided, for implementing the method for fabricating curved photovoltaic modules as described in the first aspect above. The apparatus for fabricating curved photovoltaic modules includes: a vacuum bag for holding a module to be encapsulated, the module to be encapsulated including: a flexible plate, a first encapsulating film, a battery, a second encapsulating film, and curved glass; a vacuum pump assembly including a vacuum pump for vacuuming the vacuum bag; the vacuum pump assembly further includes: a valve connected between the vacuum bag and the vacuum pump, for adjusting the vacuum pumping rate according to a first valve opening ratio or a second valve opening ratio; and a laminator for laminating the vacuum bag after the first vacuuming process.
[0022] The apparatus for fabricating curved photovoltaic modules provided in the second aspect of the present invention, being used to implement the method for fabricating curved photovoltaic modules as described in the first aspect, thus possesses all the beneficial effects of the method for fabricating curved photovoltaic modules as described in the first aspect.
[0023] According to a third aspect of the present invention, a curved photovoltaic module is also provided, which is prepared by the method for preparing a curved photovoltaic module as described in the first aspect above.
[0024] The curved photovoltaic module provided in the third aspect of the present invention is manufactured using the method for manufacturing curved photovoltaic modules as described in the first aspect, and therefore has all the beneficial effects of the method for manufacturing curved photovoltaic modules as described in the first aspect.
[0025] Additional aspects and advantages of the invention will become apparent in the following description or may be learned by practice of the invention. Attached Figure Description
[0026] The above and / or additional aspects and advantages of the present invention will become apparent and readily understood from the description of the embodiments taken in conjunction with the following drawings, in which:
[0027] Figure 1 This is a schematic flowchart of a method for fabricating a curved photovoltaic module according to an embodiment of the present invention;
[0028] Figure 2 This is one of the schematic diagrams of a component to be packaged according to an embodiment of the present invention;
[0029] Figure 3 This is a schematic diagram of a curved photovoltaic module according to an embodiment of the present invention;
[0030] Figure 4 This is a second schematic diagram of a component to be packaged according to an embodiment of the present invention;
[0031] Figure 5 This is a schematic diagram of the first vacuuming process of a component to be packaged according to an embodiment of the present invention;
[0032] Figure 6 This is a schematic diagram of a fabrication apparatus for a curved photovoltaic module according to an embodiment of the present invention;
[0033] Figure 7 This is a schematic diagram of a vacuum pumping assembly according to an embodiment of the present invention.
[0034] in, Figures 2 to 7 The correspondence between the reference numerals and the component names is as follows:
[0035] 1. Component to be encapsulated, 11. Flexible board, 12. First encapsulation film, 13. Battery, 131. Crystalline silicon battery, 133. XBC battery, 135. BC battery, 14. Second encapsulation film, 15. Curved glass, 151. First curved area, 153. Planar area, 155. Second curved area, 2. Vacuum bag, 3. Vacuum pumping component, 31. Vacuum pump, 33. Valve, 4. Laminator, 5. Curved photovoltaic module, R1. Radius of curvature of the first curved area, R2. Radius of curvature of the second curved area. Detailed Implementation
[0036] To better understand the above-mentioned objectives, features, and advantages of the present invention, the present invention will be described in optional detail below with reference to the accompanying drawings and specific embodiments. It should be noted that, unless otherwise specified, the embodiments and features described in these embodiments can be combined with each other.
[0037] Many specific details are set forth in the following description in order to provide a full understanding of the invention. However, the invention may also be practiced in other ways different from those described herein, and therefore the scope of protection of the invention is not limited to the specific embodiments disclosed below.
[0038] The following reference Figures 1 to 7 This invention describes a method for preparing a curved photovoltaic module, a preparation apparatus, and a curved photovoltaic module according to some embodiments of the present invention.
[0039] According to one technical solution of the present invention, such as Figure 1 As shown, this invention proposes a method for fabricating curved photovoltaic modules, comprising:
[0040] S101: Prepare the component to be packaged, which includes: a flexible plate, a first encapsulating film, a battery, a second encapsulating film, and curved glass;
[0041] S103: Place the component to be packaged in a vacuum bag;
[0042] S105: Perform the first vacuuming process on the vacuum bag using the first vacuuming rate;
[0043] S107: The vacuum bag after the first vacuuming process is laminated, and the vacuum bag is then vacuumed a second time using the second vacuuming rate.
[0044] S109: Remove the component to be packaged from the vacuum bag after lamination to obtain the curved photovoltaic module.
[0045] The first vacuum pumping rate is less than the second vacuum pumping rate.
[0046] In this technical solution, such as Figure 2As shown, a flexible plate 11, a first encapsulating film 12, a battery 13, a second encapsulating film 14, and curved glass 15 are sequentially stacked to form the component to be encapsulated 1. Only the curved glass 15 is curved, while the flexible plate 11, the first encapsulating film 12, the battery 13, and the second encapsulating film 14 are all planar structures. Figure 5 As shown, by placing the component to be packaged 1 in a vacuum bag 2 and performing a first vacuuming process on the vacuum bag 2 at a first vacuuming rate, the flexible plate 11, the first encapsulation film 12, the battery 13, and the second encapsulation film 14 can be bent, as shown. Figure 4 As shown, the flexible plate 11, the first encapsulating film 12, the battery 13, and the second encapsulating film 14 also form curved structures, with the same shape as the curved glass 15. Then, as... Figure 6 As shown, the vacuum bag 2, after the first vacuuming process, undergoes lamination. Simultaneously, a second vacuuming process is performed on the vacuum bag 2 using a second vacuuming rate. This second vacuuming ensures the vacuum level within the vacuum bag 2 during lamination, preventing slippage of the flexible plate 11, first encapsulation film 12, battery 13, second encapsulation film 14, and curved glass 15 in the component to be encapsulated 1. Since the first vacuuming rate is lower than the second vacuuming rate, the deformation rate of the flexible plate 11, first encapsulation film 12, battery 13, and second encapsulation film 14 is slowed down, thus preventing microcracks caused by the high rigidity of the battery 13. Subsequently, the issue of microcracks can be disregarded during lamination, reducing the difficulty of the lamination process. Figure 6 The arrows in the diagram indicate the direction of gas flow.
[0047] In the above technical solution, optionally, the first vacuuming rate and the second vacuuming rate are adjusted by the valve 33 in the vacuuming assembly 3; when the first vacuuming rate is used, the valve 33 is in the first valve opening ratio, which is greater than or equal to 0.5% and less than or equal to 10%; when the second vacuuming rate is used, the valve 33 is in the second valve opening ratio, which is 100%.
[0048] In this technical solution, the vacuum rate of the vacuum pumping assembly 3 is controlled by valve 33. By reducing the first vacuum pumping rate, the generation of microcracks can be greatly reduced. Preferably, the opening ratio of the first valve is greater than or equal to 0.5% and less than or equal to 5%, and further, the opening ratio of the first valve is greater than or equal to 0.5% and less than or equal to 1%. At the same time, the opening ratio of the second valve is 100%. When using the second valve opening ratio, its purpose is to maintain the vacuum degree of the vacuum bag 2. The vacuum degree in the vacuum bag 2 is guaranteed by the second vacuum pumping process, which can prevent the flexible plate 11, the first encapsulation film 12, the battery 13, the second encapsulation film 14 and the curved glass 15 in the component to be encapsulated 1 from sliding. At this time, the flexible plate 11, the first encapsulation film 12, the battery 13 and the second encapsulation film 14 have already completed bending, and there is no need to consider the possibility of microcracks in the battery 13 due to bending.
[0049] In the above technical solution, optionally, the time for the first vacuuming process is greater than or equal to 15 minutes and less than or equal to 20 minutes. The temperature for the first vacuuming process is greater than or equal to 10°C and less than or equal to 30°C.
[0050] In this technical solution, the initial vacuuming process needs to take more than 15 minutes to ensure the vacuum level in vacuum bag 2. Simultaneously, vacuuming at room temperature is sufficient, reducing the difficulty of the initial vacuuming process.
[0051] In the above technical solution, optionally, the lamination temperature is greater than or equal to 145°C and less than or equal to 160°C; and / or the lamination time is greater than or equal to 40 minutes and less than or equal to 60 minutes.
[0052] In this technical solution, the lamination temperature ensures the fusion of the first encapsulating film 12 and the second encapsulating film 14. Since the lamination processing time does not need to consider the elimination of microcracks, it only needs to be greater than or equal to 40 minutes and less than or equal to 60 minutes to improve the efficiency of the lamination process.
[0053] Optionally, in the above technical solution, the battery 13 includes a crystalline silicon battery 131.
[0054] In this technical solution, the battery 13 is defined as a crystalline silicon battery 131. Due to the high rigidity of the crystalline silicon battery 131, microcracks may occur during the first vacuuming process. By reducing the first vacuuming rate, the time of the first vacuuming process is greatly increased, which reduces the deformation rate of the crystalline silicon battery 131, thereby reducing the occurrence of microcracks in the crystalline silicon battery 131 during the first vacuuming process.
[0055] Optionally, in the above technical solution, the battery 13 includes either an XBC battery 133 or a BC battery 135.
[0056] In the above technical solution, optionally, the flexible board 11 includes a PET layer and a weather-resistant layer; and / or the first encapsulating film 12 includes one of EVA film, POE film, PVB film or silicone film; and / or the second encapsulating film 14 includes one of EVA film, POE film, PVB film or silicone film.
[0057] In the above technical solution, optionally, the curved glass 15 includes a first curved area 151, a flat area 153, and a second curved area 155; wherein the first curved area 151 and the second curved area 155 are respectively disposed on both sides of the flat area 153.
[0058] In the above technical solutions, optionally, such as Figure 4 As shown, the curvature directions of the first curved surface region 151 and the second curved surface region 155 are opposite; and / or the ratio of the area of the flat region 153 to the area of the curved glass 15 is greater than or equal to 80%; and / or the thickness of the curved glass 15 is greater than or equal to 3 mm and less than or equal to 6 mm; and / or the radius of curvature R1 of the first curved surface region is greater than or equal to 110 mm and less than or equal to 400 mm; and / or the radius of curvature R2 of the second curved surface region is greater than or equal to 110 mm and less than or equal to 400 mm; and / or the radius of curvature R1 of the first curved surface region is the same as the radius of curvature R2 of the second curved surface region.
[0059] In the above technical solution, by limiting the curvature of the glass and using a unique flexible encapsulation process, a curved photovoltaic product with a crystalline silicon cell 131 can be provided. A portion of the crystalline silicon cell 131 is located in the curved area of the glass. Through a flexible encapsulation process, it is laminated in one step, ensuring that the cell 13 at the curved part of the glass does not break during the lamination process, which can significantly improve the product yield. Because the crystalline silicon cell 131 is thin and has a certain degree of rigidity, it is prone to microcracks when applied to curved photovoltaic products. If the portion of the crystalline silicon cell 131 located on the curved surface is rapidly bent and deformed during the lamination process, it is very easy to break. If the cell 13 slowly conforms to the curved part, the cell 13 is less likely to develop microcracks. This solution provides a flexible encapsulation method in which the curved photovoltaic product is placed in a vacuum bag 2. A vacuum pump 31 with adjustable vacuum rate is used to first evacuate the vacuum bag 2 without heating, so that the cell 13 slowly conforms to the curved part of the glass. After the cell 13 and the glass are completely conformed, heating and lamination are performed, and the cell 13 will not develop microcracks.
[0060] Furthermore, since the vacuum pumps 31 currently available on the market do not have an adjustable evacuation rate, this invention provides a method for controlling the evacuation rate, such as... Figure 7As shown, in this invention, the vacuum pumping rate is adjusted by controlling the valve opening ratio of the vacuum pump. For example, an adjustable flow valve 33, preferably a ball valve, is installed on the vacuum pumping pipeline. The evacuation rate can be adjusted by controlling the opening and closing size of valve 33, i.e., the valve opening ratio. Different evacuation rates have a certain impact on the microcracks of battery 13. The higher the evacuation intensity, the greater the probability of microcracks in battery 13, and vice versa. The proportion of microcracks in battery 13 corresponding to different valve opening ratios is shown in Table 1. Specifically, the vacuum pump model used in this invention is JBL1500W. Table 1 shows the influence of different valve opening ratios on microcracks in battery cells when using a JBL1500W vacuum pump.
[0061] Table 1. Effect of different valve opening ratios on microcracks in solar cells.
[0062] Valve opening percentage (%) Temperature (°C) Vacuuming time (min) Percentage of microcracks in solar cells (%) 100 10-30 10-15 50-55 50-60 10-30 10-15 40-45 10-20 10-30 10-15 20-25 5-10 10-30 15-20 5-7 0.5-1 10-30 15-20 1-2
[0063] Furthermore, the product is slowly evacuated in a vacuum bag for 15-20 minutes. Once the vacuum gauge on the vacuum pump reaches -100 kPa, the product to be laminated is pushed into the heating chamber. Then, the valve on the vacuum pump's air pipe is opened to its maximum position, at which point the vacuum pump's evacuation intensity reaches -100 kPa. The equipment is then turned on for heating, and the product completes the entire lamination process within the heating chamber. Curved photovoltaic tiles are laminated using a laminating furnace. Since the product is already in a complete vacuum state before entering the heating chamber, no pre-vacuuming is required after entering the lamination chamber; lamination can proceed directly. The entire lamination process does not require a buffer temperature; the temperature can be directly raised to the required lamination parameters without affecting product quality and shortening the lamination time. Detailed data is shown in Table 2.
[0064] Table 2 Lamination parameters for lamination ovens
[0065]
[0066] Furthermore, by controlling the initial vacuuming rate through a distributed evacuation process, the microcracks in the crystalline silicon cell 131 during the conformal process with the curved glass 15 can be reduced, significantly improving product yield. Simultaneously, the curved photovoltaic products, through flexible encapsulation technology, achieve one-time lamination molding, improving production efficiency and saving energy.
[0067] According to a second aspect of the present invention, a fabrication apparatus for curved photovoltaic modules is also provided, for realizing the fabrication method of curved photovoltaic modules as described in the first aspect above. The fabrication apparatus for curved photovoltaic modules includes: a vacuum bag 2 for placing a component 1 to be packaged, the component 1 including: a flexible plate 11, a first encapsulating film 12, a battery 13, a second encapsulating film 14, and curved glass 15; a vacuum pump assembly 3 including a vacuum pump 31 for vacuuming the vacuum bag 2; the vacuum pump assembly 3 further includes: a valve 33 connected between the vacuum bag 2 and the vacuum pump 31, for adjusting the vacuum pumping rate of the vacuum pump 2 according to a first valve opening ratio or a second valve opening ratio; and a laminator 4 for laminating the vacuum bag 2 after the first vacuuming process.
[0068] The apparatus for fabricating curved photovoltaic modules provided in the second aspect of the present invention, being used to implement the method for fabricating curved photovoltaic modules as described in the first aspect, thus possesses all the beneficial effects of the method for fabricating curved photovoltaic modules as described in the first aspect.
[0069] According to a third aspect of the present invention, a curved photovoltaic module 5 is also provided, such as... Figure 3 As shown, the curved photovoltaic module is prepared using the preparation method proposed in the first aspect above.
[0070] The curved photovoltaic module 5 provided in the third aspect of the present invention is manufactured by the method for manufacturing curved photovoltaic modules as described in the first aspect, and therefore has all the beneficial effects of the method for manufacturing curved photovoltaic modules as described in the first aspect.
[0071] In this specification, the term "multiple" refers to two or more unless otherwise expressly defined. The terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; "linking" can be a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0072] In the description of this specification, the terms "one embodiment," "some embodiments," etc., refer to specific features, structures, materials, or characteristics described in connection with that embodiment or example, which are included in at least one embodiment or example of the invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.
[0073] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A method for fabricating a curved photovoltaic module, characterized in that, include: Prepare a component to be packaged, the component to be packaged includes: a flexible plate, a first encapsulating film, a battery, a second encapsulating film, and curved glass; Place the component to be packaged in a vacuum bag; The vacuum bag is subjected to a first vacuuming process using a first vacuuming rate. The vacuum bag after the first vacuuming process is laminated, and the vacuum bag is then vacuumed a second time using a second vacuuming rate. The component to be packaged is removed from the vacuum bag after lamination to obtain the curved photovoltaic module; Wherein, the first vacuum pumping rate is less than the second vacuum pumping rate.
2. The method of claim 1, wherein the method further comprises: The first vacuuming rate and the second vacuuming rate are adjusted by valves in the vacuuming assembly; When the first vacuum rate is used, the valve is in a first valve opening ratio, which is greater than or equal to 0.5% and less than or equal to 1%. When the second vacuum rate is used, the valve is in the second valve opening ratio, which is 100%.
3. The method of claim 1, wherein the method further comprises: The time for the first vacuuming process is greater than or equal to 15 minutes and less than or equal to 20 minutes; and / or The temperature of the first vacuuming process is greater than or equal to 10°C and less than or equal to 30°C.
4. The method of claim 1, wherein the method further comprises: The lamination process is performed at a temperature greater than or equal to 145°C and less than or equal to 160°C; and / or The lamination process takes a time that is greater than or equal to 40 minutes and less than or equal to 60 minutes.
5. The method for preparing a curved photovoltaic module according to claim 1, characterized in that, The battery includes a crystalline silicon battery.
6. The method for preparing a curved photovoltaic module according to claim 5, characterized in that, The battery includes either an XBC battery or a BC battery.
7. The method for preparing a curved photovoltaic module according to any one of claims 1 to 6, characterized in that, The flexible sheet includes a PET layer and a weather-resistant layer; and / or The first encapsulating film includes one of EVA film, POE film, PVB film, or silicone film; and / or The second encapsulating film includes one of EVA film, POE film, PVB film or silicone film.
8. The method of claim 1 to 6, wherein The curved glass includes a first curved area, a planar area, and a second curved area; The first curved surface region and the second curved surface region are respectively located on both sides of the planar region.
9. The method for preparing a curved photovoltaic module according to claim 8, characterized in that, The first curved surface region and the second curved surface region have opposite curvature directions; and / or The ratio of the area of the planar region to the area of the curved glass is greater than or equal to 80%; and / or The thickness of the curved glass is greater than or equal to 3 mm and less than or equal to 6 mm; and / or The radius of curvature of the first curved surface region is greater than or equal to 110 mm and less than or equal to 400 mm; and / or The radius of curvature of the second curved surface region is greater than or equal to 110 mm and less than or equal to 400 mm; and / or The radius of curvature of the first surface region is the same as the radius of curvature of the second surface region.
10. An apparatus for fabricating curved photovoltaic modules, characterized in that, A method for fabricating a curved photovoltaic module as described in any one of claims 1 to 9, wherein the fabrication apparatus for the curved photovoltaic module comprises: A vacuum bag is used to hold components to be packaged, the components to be packaged including: a flexible plate, a first encapsulation film, a battery, a second encapsulation film, and curved glass; A vacuum assembly, including a vacuum pump, is used to vacuum the vacuum bag. The vacuuming assembly further includes a valve connected between the vacuum bag and the vacuum pump, used to adjust the vacuuming rate of the vacuum pump according to the opening ratio of the first valve or the opening ratio of the second valve. A laminator is used to laminate the vacuum bag after the first vacuuming process.
11. A curved photovoltaic module, characterized in that, It is manufactured using the method for preparing curved photovoltaic modules as described in any one of claims 1 to 9.