Micro LED array structure and fabrication method with built-in common cathode metal bridge and limiting barrier
By introducing conductive metal bridges and limiting barriers into the Micro LED array, the problems of high-density Micro LED arrays scattering after peeling, high resistance, and solder contamination are solved, achieving array integrity and brightness uniformity, and improving mass production yield and optical performance.
Patent Information
- Application Number
- CN202611120284.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-07-27
- Publication Date
- 2026-11-24
AI Technical Summary
In the mass production of high-density Micro LED arrays, problems such as epitaxial block scattering after stripping, excessive common cathode resistance, solder overflow contamination, and limited N-GaN thickness lead to low yield, uneven brightness, and severe solder contamination.
A Micro LED array structure with conductive metal bridges and limiting walls deposited at the bottom of the isolation tank is formed. The N-regions of all pixels are connected by conductive metal bridges to form a low-resistance common cathode. Limiting walls are set around each pixel to prevent solder overflow. Combined with ICP dry etching and flip-chip bonding processes, the integrity of the array and brightness uniformity are ensured.
After stripping, the array remains intact, the common cathode resistance is reduced by an order of magnitude, the brightness uniformity is significantly improved, the risk of solder contamination is greatly reduced, the process compatibility is good, and the yield is significantly improved.
Smart Images

Figure CN123164901A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor optoelectronic devices and micro-display technology, specifically relating to a Micro LED array structure and fabrication method with built-in common cathode metal bridge and limiting barrier. Before substrate peeling, the common cathode connection is achieved through the conductive metal bridge at the bottom of the isolation trench, and limiting barrier is set around each pixel. It is particularly suitable for the mass production of high-density independently controllable pixel arrays. Background Technology
[0002] Currently, high-density Micro LED arrays typically employ the following technical approaches: GaN epitaxial layers (N-GaN, multiple quantum wells, P-GaN) are grown on sapphire or SiC substrates. Isolation trenches are formed by etching to divide the epitaxial layer into independent pixels; Fabricate P-electrode (independent) and N-electrode (can be shared); Flip-bonded to the CMOS driver backplane; Substrate removal via laser or chemical ablation; Obtain an independently controllable Micro LED array.
[0003] Although the above solutions have been widely adopted, the following technical bottlenecks still exist in the mass production of large-area, high-density arrays: Defect 1: After stripping, the epitaxial blocks scatter, making mass transfer difficult. After laser or chemical lift-off removes the substrate, the epitaxial blocks of individual pixels, which were originally supported by the substrate, lose their mechanical connection and are only fixed by their bonding points with the CMOS. In high-density arrays, thermal stress or mechanical impact can easily cause some pixels to detach, shift, or break, resulting in a significant decrease in yield.
[0004] Defect 2: The common cathode resistance is too high, resulting in uneven brightness in the large array. When using a continuous N-GaN layer as a common cathode, although N-GaN has a certain degree of conductivity, its sheet resistance is still relatively high for high-density arrays. Pixels farther from the common N electrode will have lower brightness due to IR voltage drop, resulting in uneven brightness across the screen, especially noticeable at high current densities.
[0005] Defect 3: Solder overflow contaminates the optical surface. During flip-chip bonding, anisotropic conductive adhesive or microbump solder is prone to lateral overflow under heat and pressure. The overflowing conductive material may seep into the light-emitting surface of the pixel along the isolation trench or chip edge, causing light path obstruction, increased scattering, and even short circuits between adjacent pixels. Existing technologies lack solutions for setting independent physical barrier structures around each pixel, making it difficult to effectively suppress lateral solder overflow in high-density arrays.
[0006] Defect 4: There is a contradiction between the N-GaN thickness and the stripping process: To reduce common cathode resistance, the N-GaN thickness is typically increased. However, a thicker N-GaN layer increases the difficulty of laser lift-off (requiring higher energy density) and is also more prone to introducing dislocation defects. This contradiction between "conductivity requirements" and "lift-off process window" limits the freedom of epitaxial design.
[0007] Therefore, there is an urgent need for an integrated solution that can improve common cathode conductivity, provide mechanical support after stripping, and prevent solder contamination. Summary of the Invention
[0008] This invention provides a Micro LED array structure with an integrated common cathode metal bridge and limiting barrier, and its fabrication method, aiming to solve problems in existing technologies such as epitaxial block scattering after peeling, excessive common cathode resistance, solder overflow contamination, and limited N-GaN thickness. After peeling, the array remains intact and does not scatter, the common cathode resistance is reduced by more than an order of magnitude, brightness uniformity is significantly improved, the risk of solder contamination is greatly reduced, and it is fully compatible with existing CMOS flip-chip bonding processes.
[0009] The purpose of this invention is to address the aforementioned technical problems by providing a method for fabricating a Micro LED array structure with a built-in common cathode metal bridge and limiting barrier, comprising the following steps: Step 1: Grow a GaN epitaxial layer on a substrate; in Step 1, the substrate is selected as sapphire or SiC; the epitaxial layer structure is: N-GaN with a thickness of 1-3 μm, multiple quantum wells with 5-8 periods, and P-GaN with a thickness of 100-300 nm; Step 2: Etching isolation trenches; In step 2, photolithography is used to define the pixel array pattern, and ICP etching is performed using a mixed gas of Cl2, BCl3 and Ar to etch through P-GaN and multiple quantum wells, completely etch through the N-GaN layer, and expose the substrate surface. Step 3: Deposit conductive metal bridges; use electron beam evaporation for directional deposition, or first protect the sidewalls with photolithography before depositing the metal, so that the metal is deposited only at the bottom of the isolation trench; the metal bridge is in direct contact with the exposed N-GaN, bridging adjacent pixels, and the metal bridge connects the N regions of all pixels to form a common cathode; the metal material is Al or TiAl alloy, and the deposition thickness is 1-5μm.
[0010] Step 4: Deposit the insulating layer; using PECVD or ALD, deposit SiO2 or SiN on the entire inner wall and bottom of the isolation tank. x The insulating layer conformally covers the upper surface and sidewalls of the metal bridge to prevent subsequent short circuits with the P-region; the insulating layer also covers the sidewalls of the isolation trench to prevent direct contact between the P electrode and N-GaN. Step 5: Fabricate P-type electrodes; Define electrode windows by photolithography on the P-GaN mesa of each pixel, evaporate a 20nm nickel layer and a 200nm gold layer by electron beam evaporation, and after stripping, rapidly anneal at 550℃ under N2 conditions for 45 seconds to form independent ohmic contacts. Step 6: Create a limiting barrier; create a ring-shaped barrier around each pixel using photolithography or electroplating; the barrier completely surrounds each pixel, forming an independent closed ring; Step 7: Flip-chip bonding to the CMOS driver backplane; Align the epitaxial wafer with the CMOS wafer so that the P electrode of each pixel corresponds one-to-one with the corresponding driver pad on the CMOS; The bonding material is anisotropic conductive adhesive ACF or microbumps, the bonding temperature is ≤200℃, the pressure is 0.5-2MPa, and during the bonding process, the limiting barrier prevents the solder or conductive adhesive from overflowing laterally to the pixel area or the light-emitting surface; Step 8: Substrate stripping; 248nm KrF laser stripping is used for SiC substrates; chemical stripping is used for sapphire or substrates with dielectric sacrificial layers; after stripping, the epitaxial blocks are connected into a whole by the metal bridge at the bottom and will not fall apart, exposing the N-GaN light-emitting surface; wet etching or dry etching is performed on the exposed N-GaN light-emitting surface to roughen it and improve the light extraction efficiency. Step 9: Complete the packaging.
[0011] The Micro LED array structure with built-in common cathode metal bridge and limiting barrier wall includes, from bottom to top, a substrate and a GaN epitaxial layer. The GaN epitaxial layer includes, from bottom to top, N-GaN, multiple quantum wells, and P-GaN. The P-GaN and multiple quantum wells are etched through by multiple isolation trenches to form a pixel array. The isolation trenches completely etch through the N-GaN layer, exposing the substrate surface. The bottom of the isolation trench is a conductive metal bridge that is in direct contact with the N-GaN. The conductive metal bridge spans adjacent pixels, connecting all N-regions to form a common cathode. The sidewalls of the isolation trenches and the upper surface and sidewalls of the metal bridges are covered with an insulating layer. A P-GaN mesa is formed between adjacent isolation trenches. An independent P-type electrode is set on the P-GaN mesa, and the P-type electrode forms an ohmic contact with the P-GaN. The limiting barrier wall is a ring or rectangular closed structure surrounding each pixel.
[0012] The substrate is made of sapphire or silicon carbide and is used for epitaxial growth of the GaN-based light-emitting layer, which is eventually stripped away; the N-GaN layer has a thickness of 1-3 μm and a doping concentration of 1×10⁻⁶. 18 -5×10 18 cm -3 The multiple quantum wells are multiple quantum well layers of alternating InGaN and GaN, with 5-8 periods. The P-GaN has a thickness of 100-300 nm and a doping concentration of 1×10⁻⁶. 19 -5×10 19cm -3 The isolation trench has a width of 3-5 μm and a depth determined by the total thickness of the epitaxial layer, ensuring that the isolation trench completely penetrates the N-GaN layer and exposes the substrate surface. The conductive metal bridge material is aluminum or titanium-aluminum alloy, with a thickness of 1-5 μm and a resistivity much lower than that of N-GaN, significantly reducing the common cathode resistance. The insulating layer material is SiO2 or SiN. x The thickness is 100-300 nm to prevent short circuits caused by contact between the metal bridge and the P-GaN or MQW sidewalls; the P-type electrode is a nickel-gold electrode with an ohmic contact resistivity of <1×10⁻⁶ with P-GaN. -5 Ω·cm 2 The limiting barrier is a ring-shaped or rectangular closed structure, not lower than the height of the bonding frame space gap, and is made of photoresist, resin, metal or ceramic. It blocks the lateral overflow of solder or conductive adhesive during the bonding process and prevents foreign objects from entering the pixel area.
[0013] The array structure also includes a CMOS driving backplane, which serves as a carrier after bonding. It has driving pads that correspond one-to-one with the P electrodes and integrates an active matrix driving circuit.
[0014] The core innovations of this invention lie in the following aspects: 1. Conductive metal bridge as common cathode: A conductive metal bridge is deposited at the bottom of the isolation trench, directly contacting the N-GaN layer to connect the N-regions of all pixels, forming a low-resistance common cathode. The resistivity of the metal bridge is much lower than that of the N-GaN semiconductor, which can significantly reduce the IR voltage drop of the high-density array and improve brightness uniformity.
[0015] 2. Metal bridges also provide mechanical support: Metal bridges bridge adjacent pixels and physically connect each epitaxial block into a whole after the substrate is peeled off. This is equivalent to implanting "steel bars" inside the thin film, which significantly enhances mechanical strength and prevents pixels from falling off or breaking.
[0016] 3. Insulating layer protects metal bridges: An insulating layer is deposited on the sidewall of the isolation trench and the upper surface of the metal bridge to ensure that the metal bridge only contacts the N-GaN at the bottom and does not short-circuit with the P-GaN or the sidewall of the quantum well, thereby improving the process margin.
[0017] 4. Limiting barrier: A ring barrier is made around each pixel to block the lateral overflow of solder or conductive adhesive during bonding, prevent foreign objects from entering the optical surface, and prevent short circuits between adjacent pixels caused by solder overflow.
[0018] 5. GaN can be thinned: Since the metal bridge undertakes the main task of conduction, the thickness of the N-GaN layer is no longer limited by the conductivity requirements. The N-GaN layer can be designed to be thinner (e.g., 1-2 μm), which is beneficial for laser lift-off and reduces epitaxial defects.
[0019] 6. Pixel-level Independent Limiting Barriers: Unlike the traditional approach of setting a large annular barrier around the chip, this invention independently sets an annular barrier around each pixel, completely surrounding the individual pixel. These pixel-level barriers directly constrain the solder flow at each interconnect point during flip bonding. The solder between adjacent pixels is isolated by their respective independent barriers, preventing short circuits due to solder bridging across pixels even if solder volume fluctuates or alignment is misaligned.
[0020] 7. Dry etching through the N-GaN layer: This invention directly uses ICP dry etching to penetrate the P-GaN, multiple quantum wells, and the entire N-GaN layer, etching to the substrate surface in one step. This "one-step" etching strategy significantly reduces the precision requirements for endpoint control. At the same time, because there is no need to retain an N-GaN residual layer, leakage paths are eliminated, improving the electrical reliability of the device.
[0021] The present invention has the following beneficial effects: 1. Complete array after peeling: The metal bridge acts as a "steel bar" to physically connect the epitaxial blocks of each pixel, completely solving the problem of pixel scattering after substrate peeling, and greatly improving the yield of mass transfer.
[0022] 2. Extremely low common cathode resistance: The metal bridge resistance is only one-thousandth to one-ten-thousandth of that of N-GaN, which significantly improves the brightness uniformity of the large array.
[0023] 3. Zero solder overflow pollution: Independent limiting barriers around each pixel effectively prevent the lateral diffusion of bonding glue / solder, resulting in a clean and pollution-free light-emitting surface.
[0024] 4. Large process allowance: The insulation layer covers the upper surface and sidewalls of the metal bridge, so even if the metal bridge size is slightly off, it will not cause a short circuit.
[0025] 5. Compatible with existing production lines: The processes used (photolithography, etching, evaporation, PECVD, flip bonding, laser lift-off) are all mature semiconductor packaging technologies that can be directly introduced into mass production.
[0026] 6. Completely eliminates inter-pixel crosstalk: The independent annular barrier around each pixel completely isolates the solder interconnection area of adjacent pixels, fundamentally eliminating electrical crosstalk caused by inter-pixel solder bridging, and significantly improving contrast.
[0027] 7. Significantly improved process robustness: Direct etching through the N-GaN layer makes the endpoint criterion clear (exposing the substrate surface), and the etching time window is greatly widened; pixel-level independent barriers increase the tolerance for solder amount deviation to ±20%, and the overall process yield is significantly improved compared with traditional solutions.
[0028] 8. Reduced requirements for CMOS pad flatness: Pixel-level limiting barriers confine the solder to the center area of the pixel. Even if there is a height difference of ±1μm in the CMOS pads, the solder is still confined inside the barrier and will not flow out laterally due to flatness issues. Attached Figure Description
[0029] Figure 1 This is a schematic cross-sectional view of the array structure of the present invention before substrate peeling; Figure 2 This is a top view of the perimeter limiting barrier wall of the pixel in this invention. Detailed Implementation
[0030] Example 1 like Figures 1-2 As shown, the Micro LED array structure with built-in common cathode metal bridge and limiting barrier wall includes, from bottom to top, a substrate and a GaN epitaxial layer. The GaN epitaxial layer includes, from bottom to top, N-GaN, multiple quantum wells, and P-GaN. The P-GaN and multiple quantum wells are etched through by multiple isolation trenches to form a pixel array. The isolation trenches completely etch through the N-GaN layer, exposing the substrate surface. The bottom of the isolation trench is a conductive metal bridge that is in direct contact with the N-GaN. The conductive metal bridge spans adjacent pixels, connecting all N-regions to form a common cathode. The sidewalls of the isolation trenches and the upper surface and sidewalls of the metal bridges are covered with an insulating layer. A P-GaN mesa is formed between adjacent isolation trenches. An independent P-type electrode is set on the P-GaN mesa. The P-type electrode forms an ohmic contact with the P-GaN. The limiting barrier wall is a ring or rectangular closed structure surrounding each pixel.
[0031] The substrate is made of sapphire or silicon carbide and is used for epitaxial growth of the GaN-based light-emitting layer, which is eventually stripped away; the N-GaN layer has a thickness of 1-3 μm and a doping concentration of 1×10⁻⁶. 18 -5×10 18 cm -3 The multiple quantum wells are multiple quantum well layers of alternating InGaN and GaN, with 5-8 periods. The P-GaN has a thickness of 100-300 nm and a doping concentration of 1×10⁻⁶. 19 -5×10 19 cm -3 The isolation trench has a width of 3-5 μm and a depth determined by the total thickness of the epitaxial layer, ensuring that the isolation trench completely penetrates the N-GaN layer and exposes the substrate surface. The conductive metal bridge material is aluminum (Al) or titanium-aluminum alloy (TiAl), with a thickness of 1-5 μm and a resistivity much lower than that of N-GaN, significantly reducing the common cathode resistance. The insulating layer material is SiO2 or SiN. xThe thickness is 100-300 nm to prevent short circuits caused by contact between the metal bridge and the P-GaN or MQW sidewalls; the P-type electrode is a nickel-gold electrode with an ohmic contact resistivity of <1×10⁻⁶ with P-GaN. -5 Ω·cm 2 The limiting barrier is a ring-shaped or rectangular closed structure, surrounding each pixel. It is made of photoresist or metal, which blocks the lateral overflow of solder or conductive adhesive during bonding, prevents foreign objects from entering the pixel area, and prevents short circuits between adjacent pixels caused by solder overflow.
[0032] The array structure also includes a CMOS driving backplane, which serves as a carrier after bonding. It has driving pads that correspond one-to-one with the P electrodes and integrates an active matrix driving circuit.
[0033] Example 2 A method for fabricating a Micro LED array structure with a built-in common cathode metal bridge and limiting barrier includes the following steps: Step 1: Grow a GaN epitaxial layer on a substrate; in Step 1, the substrate is selected as sapphire or SiC; the epitaxial layer structure is: N-GaN with a thickness of 1-3 μm, multiple quantum wells with 5-8 periods, and P-GaN with a thickness of 100-300 nm; Step 2: Etching isolation trenches; In step 2, photolithography is used to define the pixel array pattern, and ICP etching is performed using a mixed gas of Cl2, BCl3 and Ar to etch through P-GaN and multiple quantum wells, completely etch through the N-GaN layer, expose the substrate surface, and the trench width is 3-5μm. Step 3: Deposit conductive metal bridges; use electron beam evaporation for directional deposition, or first protect the sidewalls with photolithography before depositing metal, so that the metal is deposited only at the bottom of the isolation trench; the metal bridge is in direct contact with the exposed N-GaN, bridging adjacent pixels, and the metal bridge connects the N regions of all pixels to form a common cathode; the metal material is aluminum (Al) or titanium aluminum alloy (TiAl), and the deposition thickness is 1-5μm.
[0034] Step 4: Deposit the insulating layer; using PECVD or ALD, deposit SiO2 or SiN on the entire inner wall and bottom of the isolation tank. x The insulating layer conformally covers the upper surface and sidewalls of the metal bridge to prevent subsequent short circuits with the P-region; the insulating layer also covers the sidewalls of the isolation trench to prevent direct contact between the P electrode and N-GaN. Step 5: Fabricate P-type electrodes; Define electrode windows by photolithography on the P-GaN mesa of each pixel, evaporate a 20nm nickel layer and a 200nm gold layer by electron beam evaporation, and after stripping, rapidly anneal at 550℃ under N2 conditions for 45 seconds to form independent ohmic contacts. Step 6: Create Ni limiting barriers around each pixel using photolithography and electroplating. The barriers are 3~5μm high and 50μm wide, surrounding each pixel.
[0035] Step 7: Flip-chip bonding to the CMOS driver backplane; Align the epitaxial wafer with the CMOS wafer so that the P electrode of each pixel corresponds one-to-one with the corresponding driver pad on the CMOS; The bonding material is anisotropic conductive adhesive ACF or microbumps, the bonding temperature is ≤200℃, the pressure is 0.5-2MPa, and during the bonding process, the limiting barrier prevents the solder or conductive adhesive from overflowing laterally to the pixel area or the light-emitting surface; Step 8: Substrate stripping; 248nm KrF laser stripping is used for SiC substrates; chemical stripping is used for sapphire or substrates with dielectric sacrificial layers; after stripping, the epitaxial blocks are connected into a whole by the metal bridge at the bottom, and will not fall apart, exposing the N-GaN light-emitting surface; before completing the packaging, the N-surface is roughened, and the exposed N-GaN light-emitting surface is roughened by wet etching or dry etching to improve the light extraction efficiency; Step 9: Complete the packaging.
[0036] Example 3
[0037] This embodiment illustrates the integration process of a 248×72 array metal bridge and a limiting retaining wall.
[0038] Step 1: MOCVD growth of GaN epitaxy on a 6-inch SiC substrate: N-GaN thickness 2μm, doped with 3×10⁻⁶ ppm. 18 cm -3 ; 8-period MQW with alternating InGaN and GaN stacks; P-GaN thickness 200nm, doped with 3×10 19 cm -3 .
[0039] Step 2: Define a 248×72 pixel array (pixel pitch 10μm) using photolithography, and etch isolation trenches (a mixture of Cl2, BCl3 and Ar gas) to completely penetrate the N-GaN layer and expose the substrate surface. The trench width is 4μm.
[0040] Step 3: Electron beam evaporation of Al metal bridge: Evaporation at an inclined angle so that Al is deposited only at the bottom of the isolation trench, with a thickness of 2μm, directly contacting N-GaN and bridging adjacent pixels.
[0041] Step 4: PECVD deposits a SiO2 insulating layer with a thickness of 200nm, conformally covering the sidewalls of the isolation trench and the upper surface of the metal bridge.
[0042] Step 5: Fabricate nickel-gold electrodes (20nm nickel layer, 200nm gold layer) on the P-GaN mesa of each pixel, and anneal at 550℃ after stripping.
[0043] Step 6: Create Ni limiting barriers around each pixel using photolithography and electroplating. The barriers are 3~5μm high and 50μm wide, surrounding each pixel.
[0044] Step 7: Apply anisotropic conductive adhesive (ACF) to the CMOS wafer, flip-chip align the epitaxial wafer, and hot-press bond at 200℃ and 1MPa for 10 minutes. A limiting barrier prevents ACF from overflowing into the array.
[0045] Step 8: Laser lift-off of SiC substrate (248nm KrF, energy density 700mJ / cm²) 2 After peeling, the epitaxial block is intact without any fragments, and the metal bridge is clearly visible; N-face roughening: hot phosphoric acid 85% 200℃ corrosion for 3 minutes to form a pyramid-shaped roughened structure.
[0046] Step 9: After peeling, none of the 17,856 pixels fell off; the common cathode resistance was reduced by 98% compared to the pure N-GaN solution; the overall screen brightness uniformity (U%) was improved from 85% to 97%; there was no solder contamination on the light-emitting surface; the limiting walls around each pixel were intact, with no traces of solder overflow.
Claims
1. A method for fabricating a Micro LED array structure with a built-in common cathode metal bridge and limiting barrier, characterized in that, Includes the following steps: Step 1: Grow a GaN epitaxial layer on the substrate; Step 2: Etch isolation grooves; Step 3: Deposit conductive metal bridges; Electron beam evaporation directional deposition or photolithography is used to protect the sidewalls, so that the metal is deposited only at the bottom of the isolation trench; the metal bridge is in direct contact with the N-GaN at the bottom and bridges adjacent pixels. The metal bridge connects the N regions of all pixels to form a common cathode. Step 4: Deposit insulating layer; using PECVD or ALD, deposit an insulating layer on the entire inner wall and bottom of the isolation tank. The insulating layer material is SiO2 or SiN. x The insulating layer conformally covers the upper surface and sidewalls of the metal bridge; the insulating layer also covers the sidewalls of the isolation groove. Step 5: Fabricate the P-type electrode; Step 6: Create a limiting barrier; create a ring-shaped barrier around each pixel using photolithography or electroplating; the barrier completely surrounds each pixel, forming an independent closed ring; Step 7: Flip-bond to the CMOS driver backplane; Step 8: Remove the substrate; Step 9: Complete the packaging.
2. The method according to claim 1, characterized in that, In step 1, the substrate is selected as sapphire or SiC; the epitaxial layer structure is: N-GaN with a thickness of 1-3 μm, multiple quantum wells with 5-8 cycles, and P-GaN with a thickness of 100-300 nm; in step 2, the pixel array pattern is defined by photolithography, and ICP etching is performed using a mixed gas of Cl2, BCl3 and Ar to etch through the P-GaN and multiple quantum wells, completely etch through the N-GaN layer, and expose the substrate surface.
3. The method according to claim 1, characterized in that, In step 3, the metal material is Al or TiAl alloy, and the deposition thickness is 1-5 μm; in step 4, the thickness of the deposited insulating layer is 100-300 nm.
4. The method according to claim 1, characterized in that, In step 5, electrode windows are defined by photolithography on the P-GaN mesa of each pixel, and a nickel-gold alloy is evaporated by electron beam evaporation, wherein the Ni layer is 20nm and the Au layer is 200nm. After peeling, it is rapidly thermally annealed at 550°C under N2 conditions for 45 seconds to form independent ohmic contacts.
5. The method according to claim 1, characterized in that, In step 6, the retaining wall is made by one of the following methods: photoresist retaining wall made by photolithography, metal dam made of nickel or copper made by electroplating, or resin retaining wall made by dispensing.
6. The method according to claim 1, characterized in that, In step 7, the epitaxial wafer is aligned with the CMOS wafer so that the P electrode of each pixel corresponds one-to-one with the corresponding driving pad on the CMOS. The bonding material is anisotropic conductive adhesive ACF or microbumps, the bonding temperature is ≤200℃, and the pressure is 0.5-2MPa. During the bonding process, the limiting barrier prevents the solder or conductive adhesive from overflowing laterally to the pixel area or the light-emitting surface.
7. The method according to claim 1, characterized in that, In step 8, a 248nm KrF laser is used to lift the SiC substrate; chemical lift is used for sapphire or substrates with a dielectric sacrificial layer; after lift, the epitaxial blocks are connected into a whole by the metal bridge at the bottom, exposing the N-GaN light-emitting surface; before packaging, the N-surface is roughened, and the exposed N-GaN light-emitting surface is roughened by wet etching or dry etching.
8. The Micro LED array structure with built-in common cathode metal bridge and limiting barrier prepared by any one of claims 1-7, characterized in that, From bottom to top, the array comprises a substrate and a GaN epitaxial layer. The GaN epitaxial layer comprises N-GaN, multiple quantum wells, and P-GaN from bottom to top. The P-GaN and multiple quantum wells are etched through by multiple isolation trenches to form a pixel array. The isolation trenches completely etch through the N-GaN layer, exposing the substrate surface. Conductive metal bridges are deposited on the bottom and sidewalls of the isolation trenches, directly contacting the exposed N-GaN on the sidewalls of the isolation trenches and bridging adjacent pixels. The conductive metal bridges bridge adjacent pixels, connecting all N-regions to form a common cathode. The sidewalls of the isolation trenches and the upper and sidewalls of the metal bridges are covered with an insulating layer. P-GaN mesa are formed between adjacent isolation trenches. Independent P-type electrodes are disposed on the P-GaN mesa, and the P-type electrodes form ohmic contacts with the P-GaN. Limiting walls are provided around each pixel.
9. The Micro LED array structure with built-in common cathode metal bridge and limiting barrier as described in claim 8, characterized in that, The substrate is made of sapphire or silicon carbide and is used for epitaxial growth of the GaN-based light-emitting layer, which is eventually stripped away; the N-GaN layer has a thickness of 1-3 μm and a doping concentration of 1×10⁻⁶. 18 -5×10 18 cm -3 The multiple quantum wells are multiple quantum well layers of alternating InGaN and GaN, with 5-8 periods. The P-GaN has a thickness of 100-300 nm and a doping concentration of 1×10⁻⁶. 19 -5×10 19 cm -3 The isolation trench has a width of 3-5 μm and a depth determined by the total thickness of the epitaxial layer, ensuring that the isolation trench completely penetrates the N-GaN layer and exposes the substrate surface. The conductive metal bridge material is Al, TiAl alloy, or nickel-gold alloy, with a thickness of 1-5 μm and a resistivity much lower than that of N-GaN. The insulating layer material is SiO2 or SiN. x The thickness is 100-300 nm; the P-type electrode is a nickel-gold electrode with an ohmic contact resistivity of <1×10⁻⁶ with P-GaN. -5 Ω·cm 2 The limiting barrier is a ring-shaped or rectangular closed structure, surrounding each pixel, and is made of photoresist or metal.
10. The Micro LED array structure with built-in common cathode metal bridge and limiting barrier as described in claim 8, characterized in that, The array structure also includes a CMOS driving backplane, which serves as a carrier after bonding. It has driving pads that correspond one-to-one with the P electrodes and integrates an active matrix driving circuit.