Micro-led low crosstalk collimation structure for optical interconnection and preparation method thereof

By combining a BM isolation structure and a high-refractive-index optical material on a Micro-LED chip, the problems of crosstalk and low coupling efficiency in Micro-LED optical interconnects are solved, achieving optical interconnects with high collimation and high coupling efficiency.

CN123164907APending Publication Date: 2026-11-24SHANGHAI UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611463060.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-20
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing Micro-LED optical interconnects suffer from problems such as large crosstalk between adjacent optical channels, large light divergence angle, insufficient collimation, and low optical coupling efficiency. In particular, in high-density optical interconnect emission arrays, stray light is difficult to suppress effectively, affecting the coupling efficiency and transmission directionality of optical signals.

Method used

A pixel cavity is formed by enclosing a BM isolation structure and filling the cavity with high refractive index optical material. Combined with a microlens, an integrated high refractive index optical structure is formed. A low crosstalk collimation structure is prepared on the light-emitting side of the Micro-LED chip by inkjet printing technology, which physically blocks and optically controls the output light path to achieve isolation and collimation of the optical channel.

Benefits of technology

It effectively suppresses crosstalk between optical channels, improves optical collimation and optical coupling efficiency, and is suitable for high-density optical interconnect scenarios such as on-chip optical interconnect, board-level optical interconnect, and inter-chip optical interconnect. It reduces the overall thickness of the optical interconnect system and improves structural stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123164907A_ABST
    Figure CN123164907A_ABST
Patent Text Reader

Abstract

This invention relates to the field of Micro-LED optical structure technology for optical interconnects, specifically to a low-crosstalk collimation structure for Micro-LEDs used in optical interconnects and its fabrication method. The low-crosstalk collimation structure is disposed on the light-emitting side of the Micro-LED chip and includes a black matrix (BM) isolation structure between adjacent Micro-LED pixels and an integrated high-refractive-index optical structure. The BM isolation structure encloses and forms a pixel cavity; the integrated high-refractive-index optical structure includes a high-refractive-index filling portion within the pixel cavity and a microlens portion located at the light-emitting port thereon, both continuously formed from the same high-refractive-index optical material with a refractive index ≥1.6. This structure can suppress lateral stray light and leakage light between adjacent optical channels, and can converge and collimate the emitted light from the Micro-LED, improving the directionality of light emission and optical coupling efficiency. It is suitable for on-chip, board-level, chip-to-chip, and short-distance parallel optical interconnects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of Micro-LED optical structure technology for optical interconnects, and particularly to a low crosstalk collimation structure for Micro-LEDs used in optical interconnects and its fabrication method. Background Technology

[0002] With the rapid development of on-chip optical interconnects, board-level optical interconnects, chip-to-chip optical interconnects, short-distance optical interconnects in data centers, and high-density parallel optical interconnects, the requirements for optical interconnect emitters are constantly increasing, demanding high-speed response, miniaturization, high integration, low channel crosstalk, high output collimation, and high coupling efficiency. Micro-LEDs, due to their advantages such as high brightness, high response speed, high stability, low power consumption, and long lifespan, have become an important development direction for next-generation optical interconnect emitters, especially suitable for scenarios with high requirements for emission directionality and optical coupling efficiency, such as on-chip optical interconnects, board-level optical interconnects, chip-to-chip optical interconnects, and short-distance parallel optical interconnects.

[0003] Micro-LEDs typically exhibit an approximate Lambertian distribution in their light emission characteristics, meaning the emitted light diverges over a wide angular range. In high-density optical interconnect (OI) arrays, each Micro-LED pixel corresponds to an independent optical channel. The large divergence angle easily causes the emitted light to deviate from the target transmission direction and enter adjacent optical channel regions. This characteristic affects the coupling efficiency and transmission directionality of optical signals in high-speed OI systems. As pixel size and pixel pitch continue to decrease, laterally divergent light is more likely to enter adjacent pixels or adjacent channel regions, causing problems such as increased channel crosstalk and reduced system signal-to-noise ratio at the OI end.

[0004] Existing technologies typically employ the integration of microlens arrays on the surface of Micro-LEDs. The refraction of these microlenses shapes and collimates the emitted light, improving directionality and coupling efficiency. However, relying solely on microlenses for collimation has limitations: traditional microlenses only control the light direction through refraction, lacking effective blocking and absorption mechanisms for stray light propagating from pixel edges, pixel gaps, and non-target paths, making it difficult to suppress large-angle stray light and crosstalk at their source. Inkjet printing, as a digital maskless direct-write process, offers the advantages of in-situ precise microlens fabrication, high material utilization, flexible processes, and compatibility with wafer-level mass production, making it a preferred solution for microlens fabrication. However, current technologies fail to effectively combine inkjet-printed microlenses with pixel-level optical isolation structures, thus failing to simultaneously achieve low crosstalk, high collimation, and high optical coupling efficiency. Therefore, there is an urgent need for a low-crosstalk collimation structure that can be integrated into the light-emitting side of a Micro-LED chip and synergistically achieve stray light suppression, light output collimation, and improved optical coupling efficiency. This structure would meet the requirements of optical interconnects for high collimation, high coupling efficiency, and low channel interference, and solve the technical bottlenecks in existing technologies, such as insufficient stray light suppression, significant lateral light leakage between optical channels, large channel crosstalk, low optical coupling efficiency, and limited overall optical performance of optical interconnects. Summary of the Invention

[0005] In view of this, the purpose of the present invention is to provide a low crosstalk collimation structure for Micro-LEDs for optical interconnection and a method for fabricating the same. The low crosstalk collimation structure is used to solve the problems of large crosstalk between adjacent optical channels, large light divergence angle of Micro-LEDs, insufficient collimation and low optical coupling efficiency in the prior art.

[0006] To achieve the above-mentioned objectives, the present invention provides the following technical solution: The present invention provides a low crosstalk collimation structure for Micro-LEDs used in optical interconnects. The Micro-LED chip includes a substrate and a plurality of Micro-LED pixels integrated on the surface of the substrate, and each Micro-LED pixel is provided with a low crosstalk collimation structure. The light-emitting area of ​​the Micro-LED pixel is rectangular, square, or nearly square, with its length and width independently ranging from 5 to 30 μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10 to 60 μm. The low crosstalk collimation structure includes a BM isolation structure and an integrated high refractive index optical structure. The BM isolation structure encloses and forms multiple pixel cavities corresponding to the multiple Micro-LED pixels. The BM isolation structure portions arranged around the different pixel cavities are spaced apart from each other, or at least partially connected to each other to form a continuous BM isolation structure. Each of the Micro-LED pixels is located at the bottom of its corresponding pixel cavity and at the center of the pixel cavity; The integrated high-refractive-index optical structure includes a first integrated high-refractive-index optical structure and a second integrated high-refractive-index optical structure. The first integrated high refractive index optical structure is filled into the pixel cavity, and the second integrated high refractive index optical structure is located at the microlens portion of the upper light outlet of the pixel cavity; The refractive index of the high-refractive-index optical material in the integrated high-refractive-index optical structure is ≥1.6.

[0007] Preferably, the shape of the microlens portion is hemispherical, near-hemispherical, spherical, quasi-spherical, or aspherical; The microlens portion has an equivalent bottom radius of 7~30μm, a sagitta of 7~30μm, and a radius of curvature of 7~80μm; the equivalent opening size of the pixel cavity is equal to the bottom size of the microlens portion. The horizontal shape of the pixel cavity is rectangular, circular, rounded rectangle, polygonal, or irregular shape that transitions from rectangular to ring. When the shape of the pixel cavity is rectangular, the inner length and inner width of the pixel cavity are independently 14~60μm; When the pixel cavity is circular, its inner diameter is 14~60μm.

[0008] Preferably, the thickness of the BM isolation structure is 5~15μm.

[0009] Preferably, the high refractive index optical material is one or more of NOA 170F UV adhesive, UV-curable resin containing high refractive index nanoparticles, epoxy optical adhesive, or acrylate optical adhesive.

[0010] The present invention also provides a method for preparing the low crosstalk collimation structure described in the above technical solution, comprising the following steps: A Micro-LED chip is provided, the Micro-LED chip including a substrate and Micro-LED pixels integrated on the surface of the substrate; the light-emitting area of ​​the Micro-LED pixel is rectangular, square or near square, and its length and width are independently 5~30μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10~60μm; After coating the surface of the Micro-LED chip with BM photoresist, pre-baking, mask lithography and development are performed in sequence to prepare a BM isolation structure around the light-emitting area of ​​each Micro-LED pixel. A high-refractive-index optical ink is deposited within the pixel cavity enclosed by each BM isolation structure using an inkjet printing system, and then cured to obtain an integrated high-refractive-index optical structure.

[0011] Preferably, the coating method is spin coating; The spin coating process involves a rotation speed of 700-1500 rpm, an acceleration of 700-1500 rpm / s, a time of 30-60 s, and a target thickness of 5-15 μm.

[0012] Preferably, the pre-baking temperature is 120~125℃ and the time is 5min.

[0013] Preferably, the photolithography conditions are as follows: full-spectrum exposure with a mercury lamp; exposure dose of 20~80 mJ / cm. 2 The exposure time is 1-5 seconds.

[0014] Preferably, the curing is UV curing or visible light curing; The UV curing wavelength is 315~395nm, and the curing time is 60~180s; The wavelength of the visible light curing is 400~450nm, and the curing time is 60~180s.

[0015] The present invention also provides the application of the low crosstalk collimation structure described in the above technical solution or the low crosstalk collimation structure prepared by the preparation method described in the above technical solution in the transmitter of a multi-core imaging fiber-coupled optical interconnect.

[0016] This invention provides a low-crosstalk collimation structure for Micro-LEDs used in optical interconnects. The Micro-LED chip includes a substrate and a plurality of Micro-LED pixels integrated on the surface of the substrate. Each Micro-LED pixel is provided with a low-crosstalk collimation structure. The light-emitting region of each Micro-LED pixel is rectangular, square, or nearly square, with its length and width independently ranging from 5 to 30 μm. The distance between the centers of the light-emitting regions of two adjacent Micro-LED pixels is 10 to 60 μm. The low-crosstalk collimation structure includes a BM isolation structure and an integrated high-refractive-index optical structure. The BM isolation structure encloses and forms a structure that is respectively connected to the plurality of Micro-LEDs. The ED pixel has multiple pixel cavities; the BM isolation structures surrounding different pixel cavities are spaced apart from each other, or at least partially connected to form a continuous BM isolation structure; each Micro-LED pixel is located at the bottom of its corresponding pixel cavity and at the center of the pixel cavity; the integrated high-refractive-index optical structure includes a first integrated high-refractive-index optical structure and a second integrated high-refractive-index optical structure; the first integrated high-refractive-index optical structure fills the pixel cavity, and the second integrated high-refractive-index optical structure is located at the microlens portion of the upper light-emitting port of the pixel cavity; the refractive index of the high-refractive-index optical material in the integrated high-refractive-index optical structure is ≥1.6.

[0017] The low crosstalk collimation structure described in this invention reduces channel crosstalk in the optical interconnect emission array by absorbing or blocking lateral scattered light and leakage light between adjacent optical channels at the physical optical path level through a BM isolation structure between adjacent Micro-LED pixels. The BM isolation structure encloses a pixel cavity corresponding to each Micro-LED pixel, defining the filling area of ​​the high-refractive-index optical material and the forming boundary of the microlens portion, thus spatially isolating the optical channels corresponding to each emitting pixel and reducing stray light propagating along non-target paths from entering adjacent channels. Meanwhile, a high-refractive-index optical material is filled within the pixel cavity enclosed by the BM isolation structure, and a microlens is formed at the upper light-emitting port of the pixel cavity. This helps improve the refractive index transition on the light-emitting side of the Micro-LED, and, in conjunction with the curved refraction effect of the microlens, modulates the emitted light path, thereby reducing some interface reflection loss and increasing the forward light emission ratio. Simultaneously, the microlens can focus and collimate the Lambertian emitted light from the Micro-LED, guiding large-angle divergent light to the optical interconnect transmission direction, improving the forward light emission ratio, light emission collimation, and optical coupling efficiency at the receiving end. Therefore, the Micro-LED low-crosstalk collimation structure of this invention can simultaneously achieve crosstalk suppression between adjacent optical channels, collimation of the emitted beam, and improvement of optical coupling efficiency. It is suitable for applications requiring low crosstalk, high collimation, and high coupling efficiency, such as on-chip optical interconnects, board-level optical interconnects, inter-chip optical interconnects, optical transceiver array coupling, waveguide coupling, fiber coupling, and short-distance parallel optical interconnects. Furthermore, the low-crosstalk collimation structure is directly integrated into the light-emitting side of the Micro-LED chip, eliminating the need for externally mounted lens films or complex composite optical components. This reduces the overall thickness of the integrated light-emitting unit and improves structural stability and integration. The high-refractive-index optical material, after UV or visible-light curing, forms a stable bond with the BM isolation structure, resulting in a tight interface that is not easily detached, thus improving the long-term reliability of the device in optical interconnect applications.

[0018] The present invention also provides a method for fabricating the Micro-LED low crosstalk collimation structure described in the above technical solution, comprising the following steps: providing a Micro-LED chip, the Micro-LED chip comprising a substrate and Micro-LED pixels integrated on the surface of the substrate; the light-emitting area of ​​the Micro-LED pixel is rectangular, square or near square, and its length and width are independently 5~30μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10~60μm; after coating the surface of the Micro-LED chip with BM photoresist, pre-baking, mask photolithography and development are performed sequentially to prepare a BM isolation structure around the light-emitting area of ​​each Micro-LED pixel; using an inkjet printing system, high refractive index optical ink is deposited in the pixel cavity formed by the enclosure of each BM isolation structure, and cured to obtain an integrated high refractive index optical structure. The fabrication method described in this invention employs mask photolithography to achieve microlenses (BM), combined with digital inkjet printing for in-situ fabrication of microlenses. This eliminates the need for thermal reflow and nanoimprint dies, resulting in a short process flow that can be implemented in batches at the wafer level. The inkjet printing system is a maskless direct-write process, flexibly adaptable to different pixel sizes and array arrangements, suitable for the needs of multi-variety, small-batch, and large-scale mass production. Compared to imprinting and photolithography lens processes, the method described in this invention helps reduce process investment, improve material utilization, and increase fabrication yield. Attached Figure Description

[0019] Figure 1 This is a cross-sectional schematic diagram of a low crosstalk collimation structure integrated on the light-emitting side of a Micro-LED chip, where 101 is the substrate, 102 is the Micro-LED pixel, 103 is the BM isolation structure, and 104 is the integrated high-refractive-index optical structure. Figure 2This is a top view of a low crosstalk collimation structure integrated on the light-emitting side of a Micro-LED chip, where 201 is the substrate, 202 is the Micro-LED pixel, 203 is the BM isolation structure, and 204 is the integrated high-refractive-index optical structure. Figure 3 This is a cross-sectional schematic diagram of the fabrication process of the Micro-LED low crosstalk collimation structure described in this invention, wherein (a) is a schematic diagram of BM photoresist exposure, (b) is a schematic diagram of BM isolation structure formed after development, (c) is a schematic diagram of microlens formed by inkjet printing high refractive index optical ink, and (d) is a schematic diagram of integrated high refractive index optical structure formed after curing. Figure 4 This is a schematic diagram of the process for fabricating the Micro-LED low crosstalk collimation structure according to the present invention, wherein 401 is cleaning, spin-coating BM photoresist and pre-baking, 402 is photolithography to form BM isolation structure, 403 is inkjet printing high refractive index optical ink, and 404 is curing to form an integrated high refractive index optical structure. Figure 5 An optical microscope image of the BM isolation structure described in Example 1; Figure 6 The simulation results of the Micro-LED light pattern and intensity distribution are shown in Comparative Example 1. Figure 7 The simulation results of the Micro-LED light pattern and intensity distribution are shown in Comparative Example 2. Figure 8 The simulation results of the Micro-LED light pattern and intensity distribution in Example 1 are shown. Figure 9 This is a comparison diagram of the normalized far-field light intensity angular distribution in two mutually orthogonal cross sections for Example 1, Comparative Example 1, and Comparative Example 2. Figure 10 This is a schematic diagram of an application of the Micro-LED low crosstalk collimation structure described in this invention in a multi-core imaging fiber coupled optical interconnect transmitter. In this diagram, 1001 is a CMOS chip, 1002 is a Micro-LED pixel, 1003 is a BM isolation structure, 1004 is an integrated high refractive index optical structure, 1005 is an optical coupling component, and 1006 is a multi-core imaging fiber. Detailed Implementation

[0020] like Figures 1-2 As shown, the present invention provides a low crosstalk collimation structure for Micro-LEDs used in optical interconnects. The Micro-LED chip includes a substrate and a plurality of Micro-LED pixels integrated on the surface of the substrate, and each Micro-LED pixel is provided with a low crosstalk collimation structure. The light-emitting area of ​​the Micro-LED pixel is rectangular, square, or nearly square, with its length and width independently ranging from 5 to 30 μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10 to 60 μm. The low crosstalk collimation structure includes a BM isolation structure and an integrated high refractive index optical structure. The BM isolation structure encloses and forms multiple pixel cavities corresponding to the multiple Micro-LED pixels. The BM isolation structure portions arranged around the different pixel cavities are spaced apart from each other, or at least partially connected to each other to form a continuous BM isolation structure. Each of the Micro-LED pixels is located at the bottom of its corresponding pixel cavity and at the center of the pixel cavity; The integrated high-refractive-index optical structure includes a first integrated high-refractive-index optical structure and a second integrated high-refractive-index optical structure. The first integrated high refractive index optical structure is filled into the pixel cavity, and the second integrated high refractive index optical structure is located at the microlens portion of the upper light outlet of the pixel cavity; The refractive index of the high-refractive-index optical material in the integrated high-refractive-index optical structure is ≥1.6.

[0021] This invention does not particularly limit the material system, emission wavelength, array arrangement, array size, or specific packaging form of the Micro-LED chip; any method well-known to those skilled in the art can be used. In this invention, the array arrangement is more preferably a honeycomb hexagonal arrangement; the light-emitting region size of the Micro-LED pixel can be set according to the target light channel size, and the opening size of the pixel cavity is larger than the light-emitting region size of the Micro-LED pixel. In an embodiment of this invention, the light-emitting region size of a single Micro-LED pixel is 5μm × 5μm, and the distance between the centers of the light-emitting regions of adjacent Micro-LED pixels is 25μm.

[0022] In this invention, the refractive index of the high-refractive-index optical material is ≥1.6, preferably 1.6~1.8, and more preferably 1.7~1.8. The first integrated high-refractive-index optical structure and the second integrated high-refractive-index optical structure have the same refractive index.

[0023] In this invention, the shape of the microlens portion is preferably hemispherical, near-hemispherical, spherical, quasi-spherical, or aspherical, and more preferably hemispherical or near-hemispherical.

[0024] In this invention, the equivalent radius of the bottom surface of the microlens portion is preferably 7~30μm, more preferably 7~20μm; the sagitta is preferably 7~30μm, more preferably 7~20μm; and the radius of curvature is preferably 7~80μm, more preferably 7~40μm.

[0025] In this invention, when the shape of the microlens portion is a spherical cap or a spherical surface, its radius of curvature can preferably be determined according to Equation 1 based on the base radius and the sagitta. Formula 1; In Equation 1, R is the radius of curvature, r is the radius of the base, and h is the lens sagitta.

[0026] In this invention, when the microlens portion is hemispherical, its base radius, elevation, and radius of curvature are preferably equal. In an embodiment of this invention, the microlens portion is hemispherical, and its base radius, elevation, and radius of curvature are all 7 μm.

[0027] In this invention, the object-side focal length of the microlens portion is... sum of numerical aperture NA It can be determined based on its radius of curvature, sagitta, refractive index, and the target coupled optical path, as shown in Equations 2 and 3: Formula 2; In Equation 2, The object-side focal length, The refractive index of the high-refractive-index optical material after curing. The refractive index of the external medium of the microlens is in the surrounding environment. R The radius of curvature of the light-emitting surface of the microlens section; Formula 3; In Equation 3, NA Numerical aperture, n 0 The refractive index of the medium surrounding the microlens (typically in air). n 0 ≈1); θ It is the maximum half angle between the peripheral ray and the optical axis (i.e., the maximum angle at which the peripheral ray enters the lens).

[0028] The microlens portion and the high-refractive-index filling portion within the pixel cavity are continuously formed from the same high-refractive-index optical material. The axial distance from the effective light-emitting surface of the Micro-LED pixel to the vertex of the curved surface of the microlens portion is defined as the axial height of the integrated high-refractive-index optical structure. H When the height of the BM isolation structure is measured with the effective light-emitting surface of the Micro-LED pixel as the reference, the high refractive index filling part fills to the top of the BM isolation structure, and the sagitta of the microlens part is measured from the top of the BM isolation structure, the axial height is... H Determined according to Equation 4: Formula 4 In Equation 4, The height of the BM isolation structure, h Sagittal of the microlens section In this invention, for hemispherical, near-hemispherical, or spherical cap-shaped microlens portions, their light-emitting surfaces can be approximated as a single spherical refractive interface of a high-refractive-index optical material exiting into an external medium. Under paraxial conditions, to ensure that the light emitted by the Micro-LED pixel tends to be parallel after exiting through the single spherical refractive interface, the paraxial object-side focal length of the microlens portion is... Preliminary calculations can be performed according to Equation 2; In this invention, the axial height H Preferably, the focal length is the same as that of the paraxial object. Equal to or close to.

[0029] The aforementioned paraxial object-side focal length is used to determine the initial design parameters of the integrated high-refractive-index optical structure. Since Micro-LED pixels have a limited light-emitting area, the actual emitted light is also affected by microlens surface deviation, spherical aberration, material dispersion, pixel cavity boundaries, interface reflections, and non-paraxial rays. Therefore, the height of the BM isolation structure, the sag of the microlens, and the radius of curvature are preferably further verified and adjusted through optical simulation to reduce the far-field divergence angle of the Micro-LED emitted light and increase the light collection ratio within the target optical channel.

[0030] In Example 1, the height of the BM isolation structure is 10 μm, and the sagitta of the microlens portion is 7 μm. With the light-emitting surface of the Micro-LED pixel as the measurement reference for the BM thickness, the axial distance from the pixel's light-emitting surface to the apex of the microlens portion is approximately 17 μm. This distance is close to the corresponding object-side focal length in the simulation model, placing the light-emitting surface of the Micro-LED pixel in or near the object-side focal region of the microlens portion. This facilitates the focusing of the Micro-LED emitted light and reduces its far-field divergence angle.

[0031] In this invention, the equivalent opening size of the pixel cavity is matched with the bottom surface size of the microlens portion.

[0032] In this invention, the horizontal shape of the pixel cavity is preferably rectangular, circular, rounded rectangle, polygonal, or irregular shape transitioning from rectangular to annular; when the shape of the pixel cavity is rectangular, the inner length and inner width of the pixel cavity are preferably 14~60μm; when the shape of the pixel cavity is circular, the inner diameter of the pixel cavity is preferably 14~60μm.

[0033] In this invention, the equivalent opening diameter or width of the pixel cavity is preferably equal to or close to the bottom diameter of the microlens portion.

[0034] In this invention, the high refractive index optical material is preferably one or more of NOA 170F UV adhesive, UV-curable resin containing high refractive index nanoparticles, epoxy optical adhesive, or acrylate optical adhesive. This invention does not impose any special limitation on the type of UV-curable resin containing high refractive index nanoparticles, epoxy optical adhesive, or acrylate optical adhesive; any type well known to those skilled in the art can be used.

[0035] In this invention, the BM isolation structure is preferably a pixel-level BM isolation structure.

[0036] In this invention, there are no special limitations on the external dimensions, linewidth, or ring width of the BM isolation structure. Dimensions, linewidth, or ring width well-known to those skilled in the art are used, ensuring that the BM isolation structure forms a continuous light-shielding barrier between adjacent Micro-LED pixels, does not obstruct the effective light-emitting area of ​​the corresponding Micro-LED pixel, and maintains positional correspondence between each pixel cavity and the corresponding Micro-LED pixel. The height of the BM isolation structure is preferably 5~15μm, more preferably 8~12μm, and even more preferably 10μm; in the embodiments of this invention, the height of the BM isolation structure is specifically 10μm, and the linewidth is 3μm.

[0037] In this invention, the material of the BM isolation structure is preferably BM photoresist. This invention does not impose any special limitations on the black photoresist, and any material well known to those skilled in the art can be used.

[0038] In this invention, by changing the mask pattern of the BM isolation structure, the opening shape and opening size of the pixel cavity can be adjusted, thereby changing the spreading boundary of the high refractive index optical ink, the bottom surface morphology, curvature and effective focal length of the microlens.

[0039] In this invention, the rectangular pixel cavity is easy to correspond to the rectangular Micro-LED pixel and the rectangular array layout; the circular pixel cavity has better rotational symmetry, which is beneficial to forming a microlens part with a high degree of axisymmetry and to reducing the difference in light intensity angular distribution in two orthogonal sections.

[0040] like Figure 4 As shown in the flowchart, the present invention also provides a method for preparing the low crosstalk collimation structure described in the above technical solution, comprising the following steps: A Micro-LED chip is provided, the Micro-LED chip including a substrate and Micro-LED pixels integrated on the surface of the substrate; the light-emitting area of ​​the Micro-LED pixel is rectangular, square or near square, and its length and width are independently 5~30μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10~60μm; After coating the surface of the Micro-LED chip with BM photoresist, pre-baking, mask lithography and development are performed in sequence to prepare a BM isolation structure around the light-emitting area of ​​each Micro-LED pixel. A high-refractive-index optical ink is deposited within the pixel cavity enclosed by each BM isolation structure using an inkjet printing system, and then cured to obtain an integrated high-refractive-index optical structure.

[0041] In this invention, unless otherwise specified, all raw materials used in the preparation are commercially available products well known to those skilled in the art.

[0042] A Micro-LED chip is provided, the Micro-LED chip including a substrate and Micro-LED pixels integrated on the surface of the substrate; the light-emitting area of ​​the Micro-LED pixel is rectangular, square or near square, and its length and width are independently 5~30μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10~60μm; This invention does not impose any particular limitations on the material system, emission wavelength, array arrangement, array size, or specific packaging form of the Micro-LED chip; any method well-known to those skilled in the art can be used. In this invention, the array arrangement is more preferably a honeycomb hexagonal arrangement.

[0043] In this invention, after coating the surface of a Micro-LED chip with BM photoresist, pre-baking, mask lithography, and development are performed sequentially to prepare a BM isolation structure around the light-emitting area of ​​each Micro-LED pixel.

[0044] Before coating, the present invention preferably includes sequentially cleaning and drying the Micro-LED chip. The cleaning is preferably performed sequentially using isopropanol, anhydrous ethanol, and deionized water; the drying is preferably achieved by air drying. In this invention, the cleaning and drying processes can remove organic matter and impurities from the surface of the Micro-LED chip, improve the adhesion of the subsequent BM photoresist, and avoid pattern defects.

[0045] In this invention, the BM photoresist is preferably Startech SUN-2210 negative photoresist.

[0046] In this invention, the coating method is preferably spin coating, the spin coating speed is preferably 700~1500 rpm, more preferably 1000 rpm; the acceleration is preferably 700~1500 rpm / s, more preferably 1000 rpm / s; the spin coating time is preferably 30~60s, more preferably 40s; and the target thickness is preferably 5~15μm, more preferably 10μm.

[0047] In this invention, spin coating can make the BM photoresist thickness uniform, ensuring the accuracy of subsequent photolithography patterns and the consistency of light shielding.

[0048] In this invention, the pre-baking temperature is preferably 120~125℃, more preferably 120℃, 121℃, 122℃, 123℃, 124℃ or 125℃; the time is preferably 5min.

[0049] In this invention, the pre-baking process removes residual solvent from the BM photoresist, enhances the adhesion of the photoresist layer, and prevents the photoresist from floating or peeling off during development.

[0050] In this invention, the mask lithography process is preferably performed using a contact exposure machine equipped with a pixel-level matrix pattern mask (e.g., Figure 3 (as shown in a). The preferred conditions for the mask lithography are: full-spectrum exposure with a mercury lamp; and an exposure dose preferably of 20-80 mJ / cm². 2 More preferably 40 mJ / cm 2 The exposure time is preferably 1 to 5 seconds, and more preferably 3 seconds.

[0051] In this invention, the mask lithography process involves the cross-linking reaction and solidification of the areas irradiated by ultraviolet light, while the unirradiated areas are removed during the subsequent development process. In this process, the light-transmitting areas of the mask lithography correspond to the positions of the subsequent BM isolation structures, and the light-shielding areas correspond to the pixel light-emitting areas, thereby forming an exposure pattern in the BM photoresist layer that matches the pixel array.

[0052] In this invention, the developing solution used for developing is preferably an alkaline aqueous developing solution, which includes one of Startech 025D, KOH aqueous solution, TMAH aqueous solution, Na2CO3 aqueous solution or NaOH aqueous solution, and more preferably Startech 025D.

[0053] In this invention, the development time is preferably 5 to 20 minutes, more preferably 6 minutes.

[0054] After the development is completed, the present invention preferably includes rinsing with deionized water and then drying.

[0055] In this invention, the developed structure is as follows: Figure 3 As shown in b, the development process can remove the photoresist in the pixel area that has not been exposed to ultraviolet light, leaving only the exposed and cured part to form a pixel-level BM isolation structure. The BM isolation structure consists of vertically distributed black light-shielding structures that enclose independent pixel cavities, achieving optical isolation of adjacent pixels, while providing physical boundaries for subsequent inkjet high-refractive-index optical ink filling and microlens forming.

[0056] After obtaining the BM isolation structure, the present invention uses an inkjet printing system to deposit high-refractive-index optical ink within the pixel cavity enclosed by each BM isolation structure (e.g., Figure 3 As shown in Figure c, the dashed line in the figure represents the droplet deposition process, and the solid line represents the final lens shape of the droplet, which is then solidified (e.g., Figure 3 As shown in d), an integrated high-refractive-index optical structure is obtained.

[0057] In this invention, the high refractive index optical ink is preferably one of NOA 170F UV adhesive, UV-curable resin containing high refractive index nanoparticles, epoxy optical adhesive, or acrylate optical adhesive, and more preferably NOA 170F UV adhesive.

[0058] In this invention, an inkjet printing system is used to fill the pixel cavity with high refractive index optical ink, and a hemispherical, near-hemispherical, spherical, quasi-spherical, or aspherical microlens portion is formed at the upper light outlet of the pixel cavity by relying on surface tension.

[0059] In this invention, the curing is preferably UV curing or visible light curing, and heat treatment may be used if necessary. The wavelength of UV curing is preferably 315~395nm, more preferably 365nm, and the curing time is preferably 60~180s. The wavelength of visible light curing is preferably 400~450nm, and the curing time is preferably 60~180s.

[0060] In this invention, the curing process enables the high-refractive-index optical ink to rapidly cross-link and solidify, locking the convex morphology of the lens, preventing leveling collapse, and forming a structurally stable integrated high-refractive-index optical structure array. Simultaneously, the cured high-refractive-index optical structure is tightly bonded to the BM isolation structure and the pixel light-emitting surface, achieving collimation and enhanced light extraction of the emitted light, and is beneficial to improving the hardness, transmittance, and adhesion of the microlens, ensuring the long-term reliability of the Micro-LED device.

[0061] In this invention, the curing process preferably includes an auxiliary heat treatment, wherein the temperature of the auxiliary heat treatment is preferably 50-90°C, more preferably 60-80°C, and the time is preferably 5-30 min, more preferably 10-20 min. In this invention, whether or not to perform the auxiliary heat treatment is preferably determined based on the morphology of the microlens obtained by inkjet printing; when the morphology of the inkjet-printed microlens is poor, auxiliary heat treatment is preferably performed.

[0062] After the curing is completed, the present invention preferably packages and tests the Micro-LED chip with the low crosstalk collimation structure formed thereon according to actual needs.

[0063] This invention also provides the application of the low crosstalk collimation structure described in the above technical solution or the low crosstalk collimation structure prepared by the preparation method described in the above technical solution in the transmitter of a multi-core imaging fiber-coupled optical interconnect (application diagram as shown in the figure). Figure 10 (As shown).

[0064] The technical solutions of this invention will be clearly and completely described below with reference to the embodiments thereof. Obviously, the described embodiments are only a part of the embodiments of this invention, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this invention without creative effort are within the scope of protection of this invention.

[0065] Example 1 A low-crosstalk collimation structure for Micro-LEDs is disposed on the light-emitting side of a Micro-LED chip, wherein the Micro-LED chip includes a substrate and a plurality of Micro-LED pixels integrated on the surface of the substrate. In this embodiment, the light-emitting region size of a single Micro-LED pixel is 5μm × 5μm, and the distance between the centers of the light-emitting regions of adjacent Micro-LED pixels is 25μm. The low crosstalk collimation structure includes a pixel-level BM isolation structure disposed between adjacent Micro-LED pixels and an integrated high refractive index optical structure; The BM isolation structure is a rectangular frame structure, which encloses a rectangular pixel cavity with an inner length and inner width of 14μm; the height of the BM isolation structure is 10μm, the line width is 3μm, and the raw material is BM photoresist; The pixel cavity is filled with a high-refractive-index optical material to form a high-refractive-index filling portion. At the upper light-emitting port of the pixel cavity, the high-refractive-index optical material forms a microlens portion due to surface tension. The high-refractive-index filling portion and the microlens portion are continuously formed from the same high-refractive-index optical material. In this embodiment, the high-refractive-index optical material used has a refractive index of 1.7, and the raw material is NOA 170F UV adhesive. The microlens portion has a hemispherical structure with a base radius of 7μm, a sagittal height of 7μm, and a radius of curvature of 7μm. The axial height of the integrated high-refractive-index optical structure from the light-emitting surface of the Micro-LED pixel to the apex of the microlens portion is approximately 17μm. The height of the BM isolation structure is 10 μm, and the sagitta of the microlens portion is 7 μm. Using the light-emitting surface of the Micro-LED pixel as the measurement reference for the BM thickness, the axial distance from the pixel light-emitting surface to the apex of the microlens portion is approximately 17 μm. The object-side focal length calculated or simulated based on the material refractive index, microlens radius of curvature, and external medium conditions used in this embodiment is close to this axial distance, ensuring that the light-emitting surface of the Micro-LED pixel is located in or near the object-side focal region of the microlens portion, thereby helping to reduce the far-field divergence angle. This relationship is only used to explain this embodiment and does not constitute a limitation on other structural dimensions. Method for fabricating a low crosstalk collimation structure for Micro-LEDs: A Micro-LED chip is provided, the Micro-LED chip comprising a substrate and Micro-LED pixels integrated on the surface of the substrate; The Micro-LED chip was sequentially cleaned with isopropanol, anhydrous ethanol, and deionized water, and then dried. BM photoresist was spin-coated onto the surface of the Micro-LED chip (rotation speed 1000 rpm, acceleration 1000 rpm / s, time 40 s, target thickness 10 μm), followed by pre-baking (120~125℃, 5 min). Then, mask lithography was performed using a contact exposure machine equipped with a pixel-level matrix pattern mask (using a mercury lamp full-spectrum exposure, exposure dose 40 mJ / cm²). 2 The exposure time is 3s), and then the chip is immersed in the developer (Startech 025D) for 6 minutes. After rinsing with deionized water and drying, a BM isolation structure is prepared around each Micro-LED pixel in the Micro-LED chip. Using an inkjet printing system, NOA 170F UV adhesive is deposited within the pixel cavity formed by each BM isolation structure, filling the pixel cavity and forming a microlens portion at the upper light emission port of the pixel cavity; subsequently, curing is performed to form the Micro-LED low crosstalk collimation structure on the light emission side of the Micro-LED chip.

[0066] To verify the optical performance of the low crosstalk collimation structure, an optical simulation model was built using Light Tools. In the model, the light-emitting area of ​​the Micro-LED pixel is 5μm×5μm, the rectangular pixel cavity is 14μm×14μm, the height of the BM isolation structure is 10μm and the linewidth is 3μm, the microlens is a hemispherical structure with a base radius and sagitta of 7μm, and the refractive index of the high-refractive-index optical material is 1.7. The BM structure is prepared on a wafer substrate according to the method described above. Figure 5 The microscopic image of the BM isolation structure is provided by Figure 5It can be seen that the prepared pixel-level BM isolation structure has a clear shape, neat arrangement and complete pattern, uniform pixel cavity opening size, no residual glue or structural defects, and can provide good physical isolation and boundary definition for subsequent inkjet printing of high refractive index optical ink and microlens forming. Figure 8 The simulation results of the Micro-LED light pattern and intensity distribution in Example 1 are provided by... Figure 8 It can be seen that after the emitted light from Micro-LED is converged and collimated by the integrated high-refractive-index optical structure, the beam is highly concentrated in a narrow angle range in the forward direction, and the lateral stray light and leakage light are greatly suppressed, exhibiting excellent beam collimation and forward light directionality.

[0067] Comparative Example 1 Referring to Example 1, the difference is that the light-emitting side of the Micro-LED chip does not have a BM isolation structure and an integrated high-refractive-index optical structure, i.e., a bare Micro-LED chip. Figure 6 The simulation results of the Micro-LED light pattern and intensity distribution are shown in Comparative Example 1. Figure 6 It is known that the emitted light of a bare Micro-LED exhibits a typical Lambertian distribution with a very large divergence angle. A large amount of light diffuses and propagates laterally at a large angle, which can easily enter the adjacent pixel area and cause serious channel crosstalk.

[0068] Comparative Example 2 Referring to Example 1, the difference is that only a BM isolation structure is set on the light-emitting side of the Micro-LED chip, and no integrated high-refractive-index optical structure is set; Figure 7 The simulation results of the Micro-LED light pattern and intensity distribution in Comparative Example 2 are presented by... Figure 7 It can be seen that the BM isolation structure can effectively absorb and block large-angle side-scattered light and leakage light, and narrow the light divergence angle. However, due to the lack of collimation and refraction control by microlenses, large-angle light is directly absorbed, resulting in low light extraction efficiency, and the light intensity at the positive center is not improved. Figure 9 This is a comparison diagram of the normalized far-field light intensity angular distribution in two mutually orthogonal cross sections for Example 1, Comparative Example 1, and Comparative Example 2. Figure 9 It can be seen that, compared with the wide-angle Lambertian distribution of bare Micro-LED (Comparative Example 1), setting only the BM isolation structure (Comparative Example 2) can block large-angle lateral divergence light and narrow the divergence angle; while the low crosstalk collimation structure (Example 1) which sets both the BM isolation structure and the integrated high refractive index optical structure can effectively suppress lateral light crosstalk and significantly improve the collimation and forward light directionality of the beam.

[0069] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention in any way. It should be noted that those skilled in the art can make various improvements and modifications without departing from the principles of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.

Claims

1. A low crosstalk collimation structure for Micro-LEDs used in optical interconnection, wherein the Micro-LED chip includes a substrate and a plurality of Micro-LED pixels integrated on the surface of the substrate, characterized in that, Each Micro-LED pixel is equipped with a low crosstalk collimation structure; The light-emitting area of ​​the Micro-LED pixel is rectangular, square, or nearly square, with its length and width independently ranging from 5 to 30 μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10 to 60 μm. The low crosstalk collimation structure includes a BM isolation structure and an integrated high refractive index optical structure. The BM isolation structure encloses and forms multiple pixel cavities corresponding to the multiple Micro-LED pixels. The BM isolation structures arranged around different pixel cavities are spaced apart from each other, or at least partially connected to each other to form a continuous BM isolation structure; Each of the Micro-LED pixels is located at the bottom of its corresponding pixel cavity and at the center of the pixel cavity; The integrated high-refractive-index optical structure includes a first integrated high-refractive-index optical structure and a second integrated high-refractive-index optical structure. The first integrated high refractive index optical structure is filled into the pixel cavity, and the second integrated high refractive index optical structure is located at the microlens portion of the upper light outlet of the pixel cavity; The refractive index of the high-refractive-index optical material in the integrated high-refractive-index optical structure is ≥1.

6.

2. The low crosstalk collimation structure as described in claim 1, characterized in that, The shape of the microlens portion is hemispherical, near-hemispherical, spherical, quasi-spherical, or aspherical; The microlens portion has an equivalent bottom radius of 7~30μm, a sagitta of 7~30μm, and a radius of curvature of 7~80μm; the equivalent opening size of the pixel cavity is equal to the bottom size of the microlens portion. The horizontal shape of the pixel cavity is rectangular, circular, rounded rectangle, polygonal, or irregular shape that transitions from rectangular to ring. When the shape of the pixel cavity is rectangular, the inner length and inner width of the pixel cavity are independently 14~60μm; When the pixel cavity is circular, its inner diameter is 14~60μm.

3. The low crosstalk collimation structure as described in claim 1 or 2, characterized in that, The height of the BM isolation structure is 5~15μm.

4. The low crosstalk collimation structure as described in claim 1, characterized in that, The high refractive index optical material is one or more of NOA170F UV adhesive, UV-curable resin containing high refractive index nanoparticles, epoxy optical adhesive, and acrylate optical adhesive.

5. A method for preparing the low crosstalk collimation structure according to any one of claims 1 to 4, characterized in that, Includes the following steps: A Micro-LED chip is provided, the Micro-LED chip including a substrate and Micro-LED pixels integrated on the surface of the substrate; the light-emitting area of ​​the Micro-LED pixel is rectangular, square or near square, and its length and width are independently 5~30μm; the distance between the centers of the light-emitting areas of two adjacent Micro-LED pixels is 10~60μm; After coating the surface of the Micro-LED chip with BM photoresist, pre-baking, mask lithography and development are performed in sequence to prepare a BM isolation structure around the light-emitting area of ​​each Micro-LED pixel. A high-refractive-index optical ink is deposited within the pixel cavity enclosed by each BM isolation structure using an inkjet printing system, and then cured to obtain an integrated high-refractive-index optical structure.

6. The preparation method according to claim 5, characterized in that, The coating method is spin coating; The spin coating process involves a rotation speed of 700-1500 rpm, an acceleration of 700-1500 rpm / s, a time of 30-60 s, and a target thickness of 5-15 μm.

7. The preparation method according to claim 5, characterized in that, The pre-baking temperature is 120~125℃ and the time is 5min.

8. The preparation method according to claim 5, characterized in that, The conditions for the mask lithography are as follows: full-spectrum exposure with a mercury lamp; exposure dose of 20~80 mJ / cm. 2 The exposure time is 1-5 seconds.

9. The preparation method according to claim 5, characterized in that, The curing process is either UV curing or visible light curing. The UV curing wavelength is 315~395nm, and the curing time is 60~180s; The wavelength of the visible light curing is 400~450nm, and the curing time is 60~180s.

10. The application of the low crosstalk collimation structure according to any one of claims 1 to 4 or the low crosstalk collimation structure prepared by the preparation method according to any one of claims 5 to 9 in a multi-core imaging fiber-coupled optical interconnect transmitter.