Display panel, preparation method thereof and display device

By employing an isolation structure design in the display panel, the second electrode is connected to a local area of ​​the main body, reducing leakage current and solving the problems of high power consumption and short lifespan under high pixel density, thus achieving higher display quality.

CN123164973APending Publication Date: 2026-11-24HEFEI VISIONOX TECH CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202510662065.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-21
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing electronic display products struggle to improve display quality while maintaining high pixel density, particularly due to issues such as high power consumption caused by leakage current and short lifespan of light-emitting devices.

Method used

An isolation structure design is adopted, including an isolation structure for the bottom and the main body. The light-emitting device corresponds to the isolation opening. The second sub-bottom is only set in a local area around the isolation opening. The second electrode is connected to the main body through the second sub-bottom, which reduces the connection channel area between the light-emitting functional layer and the isolation structure and reduces leakage current.

Benefits of technology

It reduces the power consumption of the display panel, increases the lifespan of the light-emitting devices, improves the low grayscale image quality, and enhances the visual effect of the displayed image.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123164973A_ABST
    Figure CN123164973A_ABST
Patent Text Reader

Abstract

This disclosure provides a display panel and its fabrication method, as well as a display device. The display panel includes a substrate, an isolation structure, and a plurality of light-emitting devices located on the substrate. The isolation structure includes a bottom portion and a main body portion stacked sequentially on the substrate. The light-emitting devices correspond to the isolation openings of the isolation structure. Each light-emitting device includes a first electrode, a light-emitting functional layer, and a second electrode stacked on the substrate, with the light-emitting functional layer and the second electrode located in their respective isolation openings. The bottom portion includes a first sub-bottom portion and a second sub-bottom portion connected to each other. The first sub-bottom portion has a mesh structure, and the second sub-bottom portions are distributed in the mesh openings of the mesh structure. The orthographic projection of the first sub-bottom portion on the substrate at least partially coincides with the orthographic projection of the substrate-facing end of the main body portion on the substrate. The orthographic projection of the second sub-bottom portion on the substrate is outside the orthographic projection of the substrate-facing end of the main body portion on the substrate. The bottom portion has a conductive structure, and at least a portion of the second sub-bottom portion overlaps with the second electrode.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of display technology, specifically to a display panel and its manufacturing method, and a display device. Background Technology

[0002] Organic light-emitting diodes (OLEDs) are organic thin-film electroluminescent devices. They have attracted great attention and are widely used in electronic display products due to their advantages such as simple fabrication process, low cost, low power consumption, high brightness, wide viewing angle, high contrast and flexible display capability. The structure of this electronic display product can be found in the relevant descriptions in patents CN118251982A, 202410864269.8, PCT / CN2024 / 098407, PCT / CN2024 / 102783, PCT / CN2024 / 098217, PCT / CN2024 / 099419, PCT / CN2024 / 099072, CN117979755A, CN117998900A, CN117062489A, CN117580403A, CN116583155A, CN116669477A, ​​CN117396039A, CN116669480A, CN116600606A, and CN117500332A, and will not be repeated here.

[0003] However, current electronic display products are limited by their structural design, making it difficult to further improve display quality while ensuring a high pixel density (PPI). Summary of the Invention

[0004] This disclosure provides a display panel including a substrate, an isolation structure, and a plurality of light-emitting devices located on the substrate. The isolation structure includes a plurality of isolation openings and comprises a bottom portion and a main portion stacked sequentially on the substrate. The light-emitting devices correspond to the isolation openings, and each light-emitting device includes a first electrode, a light-emitting functional layer, and a second electrode stacked on the substrate, with the light-emitting functional layer and the second electrode located within their respective isolation openings. The orthographic projection of the support portion onto the substrate lies within the orthographic projection of the crown portion onto the substrate. The bottom portion includes a first sub-bottom portion connected to each other and a plurality of second sub-bottom portions extending from the first sub-bottom portions. The first sub-bottom portions have a mesh structure, and the second sub-bottom portions are distributed within the mesh openings of the mesh structure. The orthographic projection of the first sub-bottom portion onto the substrate at least partially coincides with the orthographic projection of the substrate-facing end of the main portion onto the substrate. The orthographic projection of the second sub-bottom portions onto the substrate lies outside the orthographic projection of the substrate-facing end of the main portion onto the substrate. The bottom portion has a conductive structure, and at least a portion of the second sub-bottom portions overlaps with a second electrode.

[0005] In the above scheme, the second sub-bottom is not distributed around the isolation opening, but is only set in a local area around the isolation opening. In this way, the second electrode can still connect with the main body (such as the support part described below) while still being connected to the second sub-bottom. Therefore, the impedance between the second electrode and the isolation structure is less affected. The light-emitting functional layer can only be indirectly connected to the main body through the second sub-bottom, thereby greatly reducing the channel area between the light-emitting functional layer and the isolation structure, so as to reduce the leakage current between the light-emitting functional layer and the isolation structure. This can reduce the power consumption of the display panel, improve the life of the light-emitting device, and improve the visual effect of the displayed image (such as improving the low grayscale image quality).

[0006] In one specific embodiment of the first aspect of this disclosure, the orthographic projection of the end of the main body facing the substrate onto the substrate is located within the orthographic projection of the end of the main body away from the substrate onto the substrate. In this way, the blocking capability of the main body to the light-emitting functional layer can be increased.

[0007] In one specific embodiment of the first aspect of this disclosure, the main body includes a support portion and a crown portion, the support portion being located between the bottom and the crown portion, and the orthographic projection of the support portion on the substrate being located within the orthographic projection of the crown portion on the substrate.

[0008] In one specific embodiment of the first aspect of this disclosure, the orthographic projection of the first sub-bottom onto the substrate coincides with the orthographic projection of the substrate-facing end of the support portion onto the substrate, or is located within the orthographic projection of the substrate-facing end of the support portion onto the substrate. In the above solution, the first sub-bottom is the main body portion of the bottom, which is located below the support portion so as not to overlap with the light-emitting functional layer, thereby reducing the overlap area between the light-emitting functional layer and the bottom (or the entire isolation structure) and reducing the leakage current generated at the light-emitting functional layer.

[0009] Optionally, the bottom is located between the second electrode and the substrate.

[0010] Optionally, the bottom is located between the light-emitting functional layer and the substrate.

[0011] In one specific embodiment of the first aspect of this disclosure, the orthographic projection of the crown-facing end of the support portion onto the substrate lies within the orthographic projection of the substrate-facing end of the support portion onto the substrate. Thus, the support portion can have relatively inclined side surfaces to facilitate the deposition of the second electrode, thereby reducing the impedance between the second electrode and the isolation structure.

[0012] In one specific embodiment of the first aspect of this disclosure, at least a portion of the orthographic projection of the second sub-bottom onto the substrate lies within the orthographic projection of the crown onto the substrate.

[0013] In one specific embodiment of the first aspect of this disclosure, the orthographic projection of the second sub-bottom onto the substrate lies within the orthographic projection of the crown onto the substrate. This further reduces the overlap area between the light-emitting functional layer and the bottom, thereby further reducing the overlap area between the light-emitting functional layer and the isolation structure, and thus reducing leakage current.

[0014] In another specific embodiment of the first aspect of this disclosure, the orthographic projection of the region of the second sub-bottom away from the first sub-bottom on the substrate lies outside the orthographic projection of the crown on the substrate, and the orthographic projection of the region of the second sub-bottom close to the first sub-bottom on the substrate lies within the orthographic projection of the crown on the substrate. This ensures sufficient overlap area between the second electrode and the bottom, avoiding the risk of poor overlap between the second electrode and the isolation structure due to manufacturing processes.

[0015] In one specific embodiment of the first aspect of this disclosure, the region of the second sub-bottom that is away from the first sub-bottom overlaps with the edge of the light-emitting functional layer, and the region of the second sub-bottom that is close to the first sub-bottom overlaps with the second electrode.

[0016] Optionally, multiple second sub-bottoms are arranged in the isolation opening.

[0017] Optionally, the support portion is a conductive structure, and the second electrode overlaps with the side wall of the support portion.

[0018] Optionally, the crown is a conductive structure.

[0019] Optionally, the crown, support, and bottom are made of titanium, aluminum, and molybdenum, respectively.

[0020] In one specific embodiment of the first aspect of this disclosure, the isolation opening includes a first side and a second side opposite to each other along a first direction, and a third side and a fourth side opposite to each other along a second direction. The second sub-bottom is disposed only at at least one of the first and second sides. When fabricating a light-emitting device using a vapor deposition process based on the isolation structure, the vapor deposition source (e.g., a line vapor deposition source) and the display panel can be moved relative to each other along the second direction. Thus, when forming the second electrode, the vapor deposition range of the second electrode in the first direction is larger, allowing the second electrode to have a larger extension below the crown at the first and second sides, thereby minimizing the impedance between the second electrode and the isolation structure at the first and second sides. Correspondingly, under the above process, the light-emitting functional layer is also more likely to extend at the first and second sides, resulting in more leakage current at the first and second sides. However, by adopting the above solution of this disclosure, the leakage current problem at the first and second sides can be solved.

[0021] In one specific embodiment of the first aspect of this disclosure, the size of the region of the second sub-bottom that is away from the first sub-bottom is smaller than the size of the region of the second sub-bottom that is in contact with the first sub-bottom. The region of the second sub-bottom that is in contact with the first sub-bottom mainly overlaps with the second electrode, while the region of the second sub-bottom that is away from the first sub-bottom may overlap with the light-emitting functional layer. This design can increase the overlap area between the second sub-bottom and the second electrode while reducing the overlap area between the second sub-bottom and the light-emitting functional layer, thereby further reducing leakage current. Optionally, the size of the second sub-bottom gradually decreases from the edge of the isolation opening to the centroid of the isolation opening.

[0022] In one specific embodiment of the first aspect of this disclosure, the planar shape of the second sub-bottom is trapezoidal, the side of the second sub-bottom that connects with the first sub-bottom is the base side of the trapezoid, the side of the second sub-bottom that is away from the first sub-bottom is the top side of the trapezoid, and the length of the base side is greater than the length of the top side.

[0023] In another specific embodiment of the first aspect of this disclosure, the planar shape of the second sub-bottom is a triangle, and the side of the second sub-bottom that connects to the first sub-bottom is a side of the triangle. For example, the triangle can be an isosceles triangle, and the side of the second sub-bottom that connects to the first sub-bottom is the base of the triangle.

[0024] In one specific embodiment of the first aspect of this disclosure, the second sub-bottom is only disposed on the side where the first side of the isolation opening is located. Thus, in the vapor deposition process, the radiation direction of the vapor deposition angle can be controlled so that the vapor deposition material (e.g., forming the second electrode) can have a greater extension at the first side, thereby ensuring the deposition thickness and extension depth of the second electrode near the first side, thus ensuring the overlap between the second electrode and the isolation structure on the first side, and making the overlap have lower impedance.

[0025] Optionally, the height of the contact portion between the edge of the second electrode on the first side and the sidewall of the support is greater than the height of the contact portion between the edge of the second side and the sidewall of the support.

[0026] In one specific embodiment of the first aspect of this disclosure, second sub-bottoms are distributed on both the side containing the first side and the side containing the second side. This increases the number of second sub-bottoms, thereby increasing the overlap area between the bottom and the second electrode, and thus reducing the impedance between the isolation structure and the second electrode.

[0027] Optionally, the height of the contact portion between the edge of the second electrode on the first side and the sidewall of the support is greater than the height of the contact portion between the edge of the second side and the sidewall of the support.

[0028] In one specific embodiment of the first aspect of this disclosure, the second sub-bottom includes a first portion connected to the first sub-bottom and a second portion away from the first sub-bottom, the thickness of the second portion being less than the thickness of the first portion. Thus, a step is formed on the surface of the second sub-bottom, thereby blocking the climbing of the light-emitting functional layer, reducing the overlap area between the second sub-bottom and the light-emitting functional layer, and thus reducing leakage current.

[0029] Optionally, in the area of ​​the second part that overlaps with the light-emitting functional layer, the orthographic projection of the edge of the light-emitting functional layer on the substrate lies within the orthographic projection of the second sub-bottom on the substrate.

[0030] Optionally, the bottom of the first sub-part of the second part overlaps with the second electrode.

[0031] In another specific embodiment of the first aspect of this disclosure, the distance from the surface of the second sub-bottom away from the substrate to the substrate is greater than the distance from the surface of the first sub-bottom away from the substrate to the substrate. This effectively increases the height (or thickness) of the second sub-bottom, allowing it to block the extension of the light-emitting functional layer, thereby reducing the overlap area between the second sub-bottom and the light-emitting functional layer and thus reducing leakage current.

[0032] Optionally, the thickness of the second sub-bottom is greater than the thickness of the first sub-bottom;

[0033] In one specific embodiment of the first aspect of this disclosure, the shape of the second sub-bottom in a cross section perpendicular to the plane where the substrate is located is trapezoidal, extending from the side of the second sub-bottom that is connected to the first sub-bottom to the side of the second sub-bottom that is away from the first sub-bottom.

[0034] In another specific embodiment of the first aspect of this disclosure, the surface of the second sub-bottom that is away from the substrate is convex, and the shape of the surface of the second sub-bottom that is away from the substrate in a cross section perpendicular to the surface where the substrate is located is arc-shaped from the side of the second sub-bottom that is in contact with the first sub-bottom to the side of the second sub-bottom that is away from the first sub-bottom.

[0035] In one specific embodiment of the first aspect of this disclosure, the height of the contact portion between the edge of the second electrode on the first side and / or the second side and the sidewall of the support is greater than the height of the contact portion between the edge of the second electrode on the third side and the fourth side and the sidewall of the support.

[0036] In one specific embodiment of the first aspect of this disclosure, the distance between the first and second sides of the isolation opening is smaller than the distance between the third and fourth sides of the isolation opening. Thus, the first and second sides form the long side direction of the isolation opening. At the first and second sides, there is a larger connection area between the second electrode of the light-emitting device and the isolation structure, resulting in relatively low impedance. Therefore, during vapor deposition, the scanning direction of the vapor deposition is controlled to make it easier for the vapor-deposited material to be deposited at the first and second sides. However, this also makes it easier for the vapor-deposited film layer (light-emitting functional layer) to overlap with the support portion of the isolation structure at the first and second sides. That is, at the first and second sides, the leakage current is also greater when the light-emitting functional layer is connected to the support portion. By adopting the above-described solution of this disclosure, the leakage current occurring at the first and second sides can be avoided or reduced.

[0037] Optionally, the first direction and the second direction are perpendicular.

[0038] In one specific embodiment of the first aspect of this disclosure, the display panel may further include a pixel defining layer. The pixel defining layer is located on the substrate and includes pixel openings corresponding to the isolation openings. The pixel openings are in communication with the corresponding isolation openings. The light-emitting functional layer of the light-emitting device and the second electrode fill the pixel openings and extend to the surface of the pixel defining layer away from the substrate.

[0039] Optionally, the projection of the bottom onto the substrate lies within the orthographic projection of the pixel defining layer onto the substrate.

[0040] Optionally, the pixel defining layer is an inorganic film layer. Inorganic films are denser and have high insulation properties. In the process of fabricating light-emitting devices based on isolation structures, the pixel defining layer does not need to be thick enough to accommodate the light-emitting devices, which is beneficial for the thinner and lighter design of the display panel. In addition, as an inorganic film layer, the pixel defining layer can have a high bonding strength with the isolation structure and the cathode, reducing the risk of the isolation structure and the cathode falling off. Furthermore, the high density of the inorganic film layer can more effectively block the intrusion of water, oxygen, etc., thereby improving the encapsulation effect of the display panel.

[0041] Optionally, the orthographic projection of the pixel opening on the substrate is located within the orthographic projection of the isolation opening on the substrate;

[0042] Optionally, the orthographic projection of the pixel opening on the substrate is located within the orthographic projection of the first electrode on the substrate, and the edge portion of the first electrode is located between the pixel defining layer and the substrate.

[0043] Optionally, the pixel defining layer is located between the isolation structure and the substrate.

[0044] In one specific embodiment of the first aspect of this disclosure, the display panel may further include a first encapsulation layer, wherein the first encapsulation layer is located on the side of the light-emitting device facing away from the substrate and includes a plurality of encapsulation units, each encapsulation unit covering an isolation opening corresponding to the light-emitting device. During the batch fabrication of the light-emitting devices based on the isolation structure, the encapsulation units are fabricated synchronously with the light-emitting devices in batches, thereby protecting the already fabricated light-emitting devices during the process of fabricating the next batch of light-emitting devices (which involves etching).

[0045] Optionally, the packaging unit extends to the side of the isolation structure away from the substrate, and the portion of the packaging unit located on the side of the isolation structure away from the substrate is a suspended portion, which is spaced apart from the isolation structure.

[0046] Optionally, the first encapsulation layer is an inorganic film layer.

[0047] Optionally, the display panel further includes a second encapsulation layer and a third encapsulation layer, which cover the first encapsulation layer and the isolation structure, with the second encapsulation layer located between the first encapsulation layer and the third encapsulation layer.

[0048] Optionally, the second encapsulation layer is an organic film layer, and the third encapsulation layer is an inorganic film layer.

[0049] A second aspect of this disclosure provides a method for fabricating a display panel, the method comprising: providing a substrate and forming a plurality of spaced-apart first electrodes on the substrate; forming a pixel defining material layer covering the first electrodes; forming an isolation structure on the pixel defining material layer, wherein the isolation structure encloses a plurality of isolation openings, the isolation openings corresponding to the first electrodes respectively, the isolation structure including a bottom and a main body portion stacked sequentially on the substrate, the bottom including a first sub-bottom portion connected to each other and a plurality of second sub-bottom portions extending from the first sub-bottom portions, the first sub-bottom portions being a mesh structure, the second sub-bottom portions being distributed in the mesh openings of the mesh structure, the orthographic projection of the first sub-bottom portions on the substrate at least partially overlapping the orthographic projection of the substrate-facing end of the main body portion on the substrate, the orthographic projection of the second sub-bottom portions on the substrate being outside the orthographic projection of the substrate-facing end of the main body portion on the substrate, the bottom being a conductive structure; and performing a patterning process on the pixel defining material layer to form a pixel defining layer, the pixel defining layer forming a structure that exposes the first electrodes. A pixel opening is formed, at least a portion of which is connected to an isolation opening; a light-emitting material film and a conductive material film are deposited, the light-emitting material film and the conductive material film covering the isolation structure and the isolation opening, wherein the portions of the light-emitting material film and the conductive material film located in the isolation opening respectively form a light-emitting functional layer and a second electrode, and at least a portion of the bottom of the second electrode overlaps with the second electrode, the first electrode, the light-emitting functional layer and the second electrode stacked on each other constitute a light-emitting device; an encapsulation material film is deposited to cover the light-emitting device; a photoresist layer is formed on the encapsulation material film, and the photoresist layer is patterned to form a photoresist pattern, the photoresist pattern covering a portion of the isolation opening; the encapsulation material film and the light-emitting device are etched based on the photoresist pattern, wherein the remaining portion of the encapsulation material film forms an encapsulation unit, and the light-emitting functional layer and the second electrode not covered by the encapsulation unit are etched; the above process is repeated to form a light-emitting device and an encapsulation unit at the isolation opening where no light-emitting device is formed, all the encapsulation units constituting a first encapsulation layer. In the display panel obtained based on the above preparation method, the second sub-bottom is not distributed around the isolation opening, but is only set in a local area around the isolation opening. In this way, the second electrode can still be connected to the main body while still being connected to the second sub-bottom. Therefore, the impedance between the second electrode and the isolation structure is less affected. The light-emitting functional layer can only be indirectly connected to the main body through the second sub-bottom, thereby greatly reducing the channel area between the light-emitting functional layer and the isolation structure, so as to reduce the leakage current between the light-emitting functional layer and the isolation structure. This can reduce the power consumption of the display panel, improve the life of the light-emitting device, and improve the visual effect of the displayed image (e.g., improve the low grayscale image quality).

[0050] In one specific embodiment of the first aspect of this disclosure, the step of forming an isolation structure on a pixel-defining material layer may include: depositing a bottom conductive material film layer on the pixel-defining material layer, and then performing a patterning process on the bottom conductive material film layer to form a bottom; forming a main conductive material layer covering the bottom, and performing a patterning process on the main conductive material layer to form a main body.

[0051] The third aspect of this disclosure is a display device, which includes the display panel described in the first aspect or the display panel obtained by the preparation method of the second aspect. Attached Figure Description

[0052] Figure 1 This is a schematic diagram of the planar structure of a display panel provided in one embodiment of the present disclosure.

[0053] Figure 2 for Figure 1 The image shows an enlarged view of area S1 of the display panel in one design.

[0054] Figure 3A for Figure 2 The diagram shows a planar structural schematic of a sub-pixel of the display panel.

[0055] Figure 3B for Figure 3A The diagram shows a partial planar structure of a sub-pixel.

[0056] Figure 4A for Figure 2 and Figure 3A The diagram shows a cross-sectional view of the display panel along M1-N1 in one design.

[0057] Figure 4B for Figure 4A An enlarged view of a portion of the structure of a certain area of ​​the display panel shown.

[0058] Figure 5A for Figure 2 and Figure 3A The diagram shows a cross-sectional view of the display panel along M2-N2 in one design.

[0059] Figure 5B for Figure 5A An enlarged view of a portion of the structure of a certain area of ​​the display panel shown.

[0060] Figure 6 This is a planar structural schematic diagram of a portion of the structure of a sub-pixel in another design of a display panel provided in an embodiment of the present disclosure.

[0061] Figure 7AThis is a planar structural schematic diagram of a portion of the structure of a sub-pixel in another design of a display panel provided in an embodiment of the present disclosure.

[0062] Figure 7B This is a planar structural schematic diagram of a portion of the structure of a sub-pixel in another design of a display panel provided in an embodiment of the present disclosure.

[0063] Figure 8 This is a planar structural schematic diagram of a portion of the structure of a sub-pixel in another design of a display panel provided in an embodiment of the present disclosure.

[0064] Figure 9A for Figure 8 The diagram shows a cross-sectional view of the display panel along M3-N3.

[0065] Figure 9B for Figure 8 The diagram shows a cross-sectional view of the display panel along M4-N4.

[0066] Figure 10 This is an enlarged view of a portion of the structure of a portion of a display panel included in another design, as provided in one embodiment of the present disclosure.

[0067] Figure 11 This is an enlarged view of a portion of the structure of a portion of a display panel included in another design, as provided in one embodiment of the present disclosure.

[0068] Figure 12 This is a cross-sectional view of a portion of the structure of a display panel provided in an embodiment of this disclosure.

[0069] Figure 13 This is a flowchart illustrating a method for manufacturing a display panel according to an embodiment of the present disclosure.

[0070] Figures 14A to 14I An embodiment of this disclosure provides a method for forming such Figure 4A The diagram shows a process diagram of one method for manufacturing a display panel.

[0071] Figure 15 This is a schematic diagram showing the positional relationship between a portion of a film layer in a display panel and the vapor deposition source during vapor deposition, according to an embodiment of this disclosure.

[0072] Explanation of reference numerals in the attached figures:

[0073] 10-Display panel; 11-Display area; 12-Border area;

[0074] 100 - Substrate; 200 - Light-emitting device; 210 - First electrode; 220 - Light-emitting functional layer; 221 - First functional layer; 222 - Light-emitting layer; 223 - Second functional layer; 230 - Second electrode; 300 - Isolation structure; 301 - Isolation opening; 301a - First side; 301b - Second side; 301c - Third side; 301d - Fourth side; 302 - Pixel opening; 310 - Support portion; 310a - First material layer; 320 - Crown portion; 320a - Second material layer; 330 - Bottom; 330a - Third material layer; 331 - First sub-bottom; 332 - Second sub-bottom; 332a - First portion; 332b - Second portion; 340 - Pixel defining layer; 340a - Pixel defining material layer;

[0075] 400 - Packaging structure; 410 - First packaging layer; 410a - Packaging material film layer; 411 - Packaging unit; 420 - Second packaging layer; 430 - Third packaging layer;

[0076] 500 - Photoresist pattern; 500a - Filler film. Detailed Implementation

[0077] The technical solutions in the embodiments of this specification will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this specification, and not all embodiments. Based on the embodiments in this specification, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this specification.

[0078] In some scenarios, functional films in light-emitting devices are formed by vapor deposition. Each light-emitting device has multiple functional films, and the material composition of some functional films (such as the light-emitting layer) in light-emitting devices that emit different light is different. Therefore, when vapor deposition of these functional films using a mask (such as a fine mask), multiple alignments are required. To solve the positional offset problem caused by alignment accuracy errors, sufficient space (a safety margin related to alignment errors) needs to be reserved between different light-emitting devices to ensure that the actual light-emitting area of ​​the light-emitting device can have a certain overlap with the designed position (design area). This is equivalent to compressing the designed area of ​​the light-emitting area of ​​the light-emitting device, which not only limits the light-emitting area of ​​the light-emitting device, but also prevents the arrangement density of the light-emitting devices from being further increased, thus making it difficult to further improve the PPI (pixel density) of the display panel.

[0079] In the embodiments of this disclosure, by providing an isolation structure at the gap between the light-emitting devices, the functional film layers of adjacent light-emitting devices are separated. Thus, in the evaporation process of the functional film layers, only the entire display panel needs to be evaporated, without the need to individually prepare the functional film layer for each light-emitting device using a mask. This process does not require consideration of alignment accuracy during evaporation, thereby allowing the gaps between the light-emitting devices to be designed to be smaller, increasing the PPI (the principle of which can be found in the following...). Figures 14A to 14I (Related descriptions in the relevant embodiments).

[0080] It should be noted that when fabricating light-emitting devices based on the above-mentioned isolation structure, the evaporated film layer will extend towards the bottom of the isolation structure (the principle can be found in [reference needed]). Figure 15 (As described in the relevant embodiments), this causes some of the vapor-deposited layers of the light-emitting device (excluding its included electrodes) to connect to the isolation structure. Thus, during the driving of the light-emitting device, current is directly conducted along these vapor-deposited layers to the isolation structure (without being indirectly conducted to the isolation structure via the electrodes included in the light-emitting device, such as the second electrode in the following embodiment), resulting in leakage current. This leakage current can lead to poor display at low grayscale levels and reduced lifespan of the light-emitting device.

[0081] At least one embodiment of this disclosure provides a display panel and a method for manufacturing the same, as well as a display device, to at least solve the aforementioned technical problems. The display panel includes a substrate, an isolation structure, and a plurality of light-emitting devices located on the substrate. The isolation structure includes a plurality of isolation openings and includes a bottom portion and a support portion stacked sequentially on the substrate. The light-emitting devices correspond to the isolation openings respectively. Each light-emitting device includes a first electrode, a light-emitting functional layer, and a second electrode stacked on the substrate, with the light-emitting functional layer and the second electrode located in the corresponding isolation openings. The orthographic projection of the support portion on the substrate is located within the orthographic projection of the crown portion on the substrate. The bottom portion includes a first sub-bottom portion connected to each other and a plurality of second sub-bottom portions extending from the first sub-bottom portion. The first sub-bottom portion has a mesh structure, and the second sub-bottom portions are distributed in the mesh openings of the mesh structure. The orthographic projection of the first sub-bottom portion on the substrate at least partially coincides with the orthographic projection of the substrate-facing end of the main body portion on the substrate. The orthographic projection of the second sub-bottom portion on the substrate is located outside the orthographic projection of the substrate-facing end of the main body portion on the substrate. The bottom portion has a conductive structure, and at least a portion of the second sub-bottom portion overlaps with the second electrode. By using an isolation structure, light-emitting devices can be fabricated in batches, allowing for full-area vapor deposition during the fabrication of the light-emitting device's film layers. This eliminates the need to consider the alignment accuracy of the films formed by each vapor deposition process, significantly reducing the gaps between individual light-emitting devices and increasing their pixel density (PPI). In the aforementioned process, the edge of the light-emitting functional layer of the light-emitting device may come into contact with the sidewall of the isolation structure, potentially causing leakage. In the above solution, the second sub-bottom is not distributed around the isolation opening but is only located in a localized area around it. Thus, the second electrode can still connect to the main body (e.g., the support portion described below) while still being connected to the second sub-bottom, minimizing the impact on the impedance between the second electrode and the isolation structure. The light-emitting functional layer can only be indirectly connected to the main body through the second sub-bottom, greatly reducing the channel area between the light-emitting functional layer and the isolation structure. This reduces leakage current between the light-emitting functional layer and the isolation structure, thereby reducing the power consumption of the display panel, increasing the lifespan of the light-emitting devices, and improving the visual effect of the displayed image (e.g., improving low-grayscale image quality).

[0082] The structure of a display panel according to at least one embodiment of the present disclosure will now be described in detail with reference to the accompanying drawings. Furthermore, in these drawings, a spatial rectangular coordinate system is established with the substrate as a reference to more intuitively present the positional relationships of the relevant structures in the display panel. In this spatial rectangular coordinate system, the X-axis and Y-axis are parallel to the plane of the substrate, and the Z-axis is perpendicular to the plane of the substrate.

[0083] like Figures 1 to 5BAs shown, the planar area of ​​the display panel 10 can be divided into a display area 11 and a border area 12 surrounding the display area 11. Sub-pixels (also called sub-pixels, etc.) can be arranged in the display area 11, such as P1, P2, P3 sub-pixels. The physical structure of the sub-pixel can be the light-emitting device in the following embodiment. Adjacent sub-pixels with different emitted light colors constitute a pixel (also called a pixel unit, large pixel, etc.). The arrangement density of the pixel in the display area 11 represents the pixel density PPI.

[0084] The physical structure of the display panel 10 may include a substrate 100, an isolation structure 300 located on the substrate 100, and a plurality of light-emitting devices 200. The isolation structure 300 includes a plurality of isolation openings 301, and includes a bottom portion 330 and a main body portion 30 sequentially stacked on the substrate 100 (see [link to documentation]). Figure 4A The light-emitting device 200 and the isolation opening 301 correspond to each other.

[0085] The light-emitting device 200 includes a first electrode 210, a light-emitting functional layer 220, and a second electrode 230 sequentially stacked on a substrate 100. The light-emitting functional layer 220 and the second electrode 230 are located in corresponding isolation openings 301. That is, the light-emitting functional layer 220 and the second electrode 230 can be formed by vapor deposition. Specifically, after forming the isolation structure 300 with the isolation openings 301, vapor deposition is performed on the entire surface to form the light-emitting functional layer 220 and the second electrode 230 in each isolation opening 301.

[0086] For example, such as Figure 4A As shown, the orthographic projection of the end of the main body 30 facing the substrate 100 onto the substrate 100 is located within the orthographic projection of the end of the main body 30 away from the substrate 100 onto the substrate 100. In this way, the blocking capability of the main body 30 to the light-emitting functional layer 220 can be increased.

[0087] For example, in some examples of this disclosure, the main body 30 can be an integral structure with a longitudinal cross-sectional shape that is an inverted trapezoid, the top of which faces the substrate 100.

[0088] For example, in other examples of this disclosure, such as Figure 4A As shown, the main body 30 includes a support portion 310 and a crown portion 320. The support portion 310 is located between the bottom 330 and the crown portion 320. The orthographic projection of the support portion 310 on the substrate 100 is located within the orthographic projection of the crown portion 320 on the substrate 100.

[0089] The structure of the display panel will now be described using the main body 30 of the isolation structure 300, including the support 310 and the crown 320, as an example.

[0090] In the isolation structure 300, the orthographic projection of the support portion 310 on the substrate 100 lies within the orthographic projection of the crown portion 320 on the substrate 100. Thus, the dimensional difference between the support portion 310 and the crown portion 320 acts as a barrier to the light-emitting functional layer 220. The bottom 330 includes a first sub-bottom 331 and a plurality of second sub-bottoms 332 connected to each other. The first sub-bottom 331 has a mesh structure, and the second sub-bottoms 332 are distributed within the mesh openings of the mesh structure. The orthographic projection of the first sub-bottom 331 on the substrate 100 at least partially overlaps with the orthographic projection of the support portion 310 on the substrate 100. The orthographic projection of the second sub-bottoms 332 on the substrate 100 lies outside the orthographic projection of the support portion 310 on the substrate 100. The crown portion 320 is a conductive structure, and at least a portion of the second sub-bottoms 332 overlaps with the second electrode 230. It should be noted that, without adopting the above-described solution of this disclosure, the second sub-bottom 332 can be regarded as a closed ring surrounding the isolation opening 301, thus having a large contact area with the light-emitting functional layer 220, and can therefore be regarded as a surface connection. However, after adopting the above-described solution of this disclosure, the second sub-bottom 332 is locally distributed around the isolation opening, thereby reducing the contact area between the second sub-bottom 332 and the light-emitting functional layer 220, and can therefore be regarded as a point connection. This reduces the amount of current in the light-emitting device 200 that is directly introduced from the light-emitting functional layer 220 into the isolation structure 300 without passing through the second electrode 230, thereby reducing leakage current.

[0091] It should be noted that in the embodiments of this disclosure, the number of second sub-bottoms 332 in each isolation opening 301 is not limited and can be selected according to actual process requirements. For example, one second sub-bottom 332 can be provided in each isolation opening 301, or multiple second sub-bottoms 332 can be provided. For example, on the side of the isolation opening 301 where the second sub-bottom 332 is provided, one can also be selected (e.g., Figure 7A (as shown) or multiple second child bottoms 332 (e.g.) Figure 7B (as shown in the example).

[0092] In at least one embodiment of this disclosure, such as Figure 4AAs shown, the light-emitting functional layer 220 includes at least one first functional layer 221, at least one light-emitting layer 222, and at least one second functional layer 223 sequentially stacked on the first electrode 210. The first functional layer 221 includes at least one hole-type film layer, such as at least one of a hole injection layer and a hole transport layer. The second functional layer 223 includes at least one electron-type film layer, such as at least one of an electron injection layer and an electron transport layer. For example, the first functional layer 221 may also include an electron blocking layer, and the second functional layer 223 may also include a hole blocking layer. It should be noted that the first functional layer 221 can be directly overlapped with the bottom 330. Since the hole-type film layer has high conductivity, it is the main film layer causing leakage current. Therefore, the above-described solution of this disclosure actually reduces the overlap area between the first functional layer 221 and the bottom 330 to reduce leakage current.

[0093] In at least one embodiment of this disclosure, such as Figure 4A and Figure 4B As shown, the orthographic projection of the first sub-bottom 331 on the substrate 100 coincides with the orthographic projection of the end of the support portion 310 facing the substrate 100 on the substrate 100; or, the orthographic projection of the first sub-bottom 331 on the substrate 100 may be located within the orthographic projection of the end of the support portion 310 facing the substrate 100 on the substrate 100. In this way, the first sub-bottom 331 is the main body of the bottom 330, which is located below the support portion 310 and thus does not overlap with the light-emitting functional layer 220, thereby reducing the overlap area between the light-emitting functional layer 220 and the bottom 330 (or the entire isolation structure 300) and reducing the leakage current generated at the light-emitting functional layer 220.

[0094] It should be noted that the light-emitting functional layer 220 and the second electrode 230 of the light-emitting device 200 are fabricated based on the isolation structure 300. Therefore, in the fabrication process, the isolation structure 300 is formed first, and then the light-emitting functional layer 220 and the second electrode 230 are formed. Thus, when the light-emitting functional layer 220 and the second electrode 230 overlap with the bottom 330, the bottom 330 will be located between the second electrode 230 and the substrate 100.

[0095] In at least one embodiment of this disclosure, such as Figure 4A and Figure 4B As shown, the orthographic projection of the end of the support portion 310 facing the crown portion 320 onto the substrate 100 lies within the orthographic projection of the end of the support portion 310 facing the substrate 100 onto the substrate 100. In this way, the support portion 310 can have a relatively inclined side surface to facilitate the deposition of the second electrode 230, thereby reducing the impedance between the second electrode 230 and the isolation structure 300.

[0096] In the embodiments disclosed herein, there is no limitation on the dimensional range between the second sub-bottom 332 and the crown 320. The second sub-bottom 332 may be configured to extend beyond the coverage of the crown 320 or may be configured to be completely covered by the crown 320. The following will describe different embodiments.

[0097] In at least one embodiment of this disclosure, such as Figure 4A , Figure 4B and Figure 6 As shown, at least a portion of the orthographic projection of the second sub-bottom 332 onto the substrate 100 lies within the orthographic projection of the crown 320 onto the substrate 100, as detailed below.

[0098] In some embodiments of this disclosure, such as Figure 4A and Figure 4B As shown, the orthographic projection of the region of the second sub-bottom 332 away from the first sub-bottom 331 onto the substrate 100 is outside the orthographic projection of the crown 320 onto the substrate 100, and the orthographic projection of the region of the second sub-bottom 332 close to the first sub-bottom 331 onto the substrate 100 is within the orthographic projection of the crown 320 onto the substrate 100. This ensures sufficient overlap area between the second electrode 230 and the bottom 330, avoiding the risk of poor overlap between the second electrode 230 and the isolation structure 300 due to process limitations. It should be noted that in this case, when performing the vapor deposition process based on the isolation structure 300, the crown 320 cannot completely block the second sub-bottom 332, causing the light-emitting functional layer 220 to be deposited on the second sub-bottom 332. Therefore, the technical solution in the above embodiments of this disclosure is particularly needed to solve the leakage current problem between the light-emitting functional layer 220 and the second sub-bottom 332.

[0099] In other embodiments of this disclosure, such as Figure 6 As shown, the orthographic projection of the second sub-bottom 332 on the substrate 100 lies within the orthographic projection of the crown 320 on the substrate 100. This further reduces the overlap area between the light-emitting functional layer 220 and the bottom 330, or even prevents the light-emitting functional layer 220 from overlapping with the bottom 330, thereby further reducing the overlap area between the light-emitting functional layer 220 and the isolation structure 300, and reducing leakage current.

[0100] See again for at least one embodiment of this disclosure. Figure 4A and Figure 4B The area of ​​the second sub-bottom 332 that is far from the first sub-bottom 331 overlaps with the edge of the light-emitting functional layer 220, and the area of ​​the second sub-bottom 332 that is close to the first sub-bottom 331 overlaps with the second electrode 230. That is, during vapor deposition, the coverage area of ​​the second electrode 230 is larger than the coverage area of ​​the light-emitting functional layer 220 to ensure that the overlap between the second electrode 230 and the bottom 330 is not completely blocked by the light-emitting functional layer 220.

[0101] See again for at least one embodiment of this disclosure. Figure 4A and Figure 4B The support portion 310 is a conductive structure, and the second electrode 230 overlaps with the sidewall of the support portion 310. In this way, the conductive support portion 310 can connect the second electrodes 230 of each light-emitting device 200 in series to form a common electrode. Moreover, the support portion 310 is located in the gap between the light-emitting devices 200, so it does not need to transmit light and is not limited by thickness, thereby reducing the impedance of the common electrode and alleviating the voltage drop problem on each second electrode 230 when driving the light-emitting device 200.

[0102] See again for at least one embodiment of this disclosure. Figure 4A and Figure 4B The crown 320 is a conductive structure, thereby participating in the formation of the aforementioned common electrode to further alleviate the voltage drop problem on each of the second electrodes 230 when driving the light-emitting device 200.

[0103] In at least one embodiment of this disclosure, the crown 320, the support 310, and the bottom 330 are made of titanium, aluminum, and molybdenum, respectively. The corrosion resistance of aluminum, molybdenum, and titanium increases sequentially, and during etching, the film formed by these materials can form a film such as… Figures 4A to 5B The isolation structure 300 is shown.

[0104] In the vapor deposition process, the vapor deposition source moves relative to the display panel (i.e., the scanning direction of the vapor deposition), resulting in different degrees of vapor deposition on the display panel in different directions. For example, along the scanning direction of the vapor deposition source, the vapor deposition source is more limited by the vapor deposition angle, thus limiting the vapor deposition range and limiting the extension of the vapor deposition film below the crown. Conversely, in the direction perpendicular to the scanning direction, the vapor deposition source is less limited by the vapor deposition angle, thus limiting the vapor deposition range and allowing for a greater extension of the vapor deposition film below the crown. Accordingly, the specific arrangement and shape of the second sub-bottom 332 at the isolation opening 301 can be arranged to ensure overlap between the second electrode 230 and the isolation structure 300 with lower impedance while reducing leakage current. The different arrangements and shapes of the second sub-bottom 332 will be described below with reference to different embodiments.

[0105] See again for at least one embodiment of this disclosure. Figures 3A to 5BThe isolation opening 301 includes a first side 301a and a second side 301b opposite each other along a first direction (e.g., the X-axis direction), and a third side 301c and a fourth side 301d opposite each other along a second direction (e.g., the Y-axis direction). The second sub-bottom 332 is disposed only at at least one of the first side 301a and the second side 301b. When performing a vapor deposition process based on the isolation structure 300 to fabricate the light-emitting device 200, the vapor deposition source (e.g., a line vapor deposition source) and the display panel can be moved relative to each other along the second direction. Thus, when forming the second electrode 230, the vapor deposition range of the second electrode 230 in the first direction is larger, thereby allowing the second electrode 230 to have a larger extension below the crown 320 at the first side 301a and the second side 301b, so that the impedance between the second electrode 230 and the isolation structure 300 at the first side 301a and the second side 301b is minimized. Correspondingly, under the above process, the light-emitting functional layer 220 is also more likely to extend at the first side 301a and the second side 301b, which makes it easier for leakage current to occur at the first side 301a and the second side 301b. However, by adopting the above solution of this disclosure, the leakage current problem at the first side 301a and the second side 301b can be solved.

[0106] In at least one embodiment of this disclosure, such as Figure 3B and Figure 6 As shown, the second sub-bottom 332 extends from the edge of the isolation opening 301 toward the centroid of the isolation opening 301.

[0107] In at least one embodiment of this disclosure, such as Figure 7A and Figure 7B As shown, the size W1 of the region of the second sub-bottom 332 that is far from the first sub-bottom 331 (see...) Figure 7A The size of the second sub-bottom 332 is smaller than the size W2 of the area where it connects with the first sub-bottom 331. The area of ​​the second sub-bottom 332 that connects with the first sub-bottom 331 mainly overlaps with the second electrode 230, while the area of ​​the second sub-bottom 332 that is away from the first sub-bottom 331 may overlap with the light-emitting functional layer 220. This design can increase the overlap area between the second sub-bottom 332 and the second electrode 230 while reducing the overlap area between the second sub-bottom 332 and the light-emitting functional layer 220, thereby further reducing leakage current. For example, the size of the second sub-bottom 332 gradually decreases from the edge of the isolation opening 301 to the centroid of the isolation opening 301.

[0108] In some embodiments of this disclosure, such as Figure 7AAs shown, the planar shape of the second sub-bottom 332 is trapezoidal. The side of the second sub-bottom 332 that connects with the first sub-bottom 331 is the base of the trapezoid, and the side of the second sub-bottom 332 that is away from the first sub-bottom 331 is the top side of the trapezoid. The length of the base is greater than the length of the top side. For example, this trapezoid can be a regular trapezoid, etc.

[0109] In other embodiments of this disclosure, such as Figure 7B As shown, the planar shape of the second sub-bottom 332 is triangular, and one side of the triangle connects to the first sub-bottom 331. For example, further, as... Figure 7B As shown, the planar shape of the second sub-bottom 332 is an isosceles triangle, and the side of the second sub-bottom 332 that connects with the first sub-bottom 331 is the base of the isosceles triangle.

[0110] In some embodiments of this disclosure, a second sub-bottom 332 is provided on one side of the isolation opening 301. For example, as Figures 8 to 9B As shown, the second sub-bottom 332 is only located on the side where the first side 301a of the isolation opening 301 is located. In this way, in the vapor deposition process, the radiation direction of the vapor deposition angle can be controlled so that the vapor deposition material (e.g., forming the second electrode 230) can have a greater extension at the first side 301a, thereby ensuring the deposition thickness and extension depth of the second electrode 230 near the first side 301a, thereby ensuring the overlap between the second electrode 230 and the isolation structure 300 on the first side 301a side, and making the overlap have a smaller impedance.

[0111] In other embodiments of this disclosure, a second sub-bottom 332 is provided on both sides of the isolation opening 301. For example, as Figures 3A to 7B As shown, second sub-bottoms 332 are distributed on both the side where the first side 301a is located and the side where the second side 301b is located. In this way, the number of second sub-bottoms 332 can be increased to increase the overlap area between the bottom 330 and the second electrode 230, thereby reducing the impedance between the isolation structure 300 and the second electrode 230.

[0112] In at least one embodiment of this disclosure, the climbing height H of the edge of the second electrode 230 on the sidewall of the support 310 on the side where the first side 301a is located is (e.g., Figure 9AAs shown, the height of the portion in contact with the sidewall of the support 310 is greater than the climbing height of the edge on the sidewall of the support 310 on the side where the second side 301b is located. For example, when the second electrode 230 is formed by vapor deposition based on the isolation structure 300, the display panel and the vapor deposition source can be tilted relative to each other to make it easier for the vapor deposition film layer to be deposited below the crown 320 on the side where the first side 301a is located, so as to ensure that the second electrode 230 and the isolation structure 300 have better overlap at the first side 301a, thereby greatly reducing the impedance between the second electrode 230 and the isolation structure 300.

[0113] In some embodiments of this disclosure, such as Figure 10 As shown, the second sub-bottom 332 includes a first portion 332a connected to the first sub-bottom 331 and a second portion 332b away from the first sub-bottom 331, the thickness of the second portion 332b being less than the thickness of the first portion 332a. Thus, a step is formed on the surface of the second sub-bottom 332, thereby blocking the climbing of the light-emitting functional layer 220, reducing the overlap area between the second sub-bottom 332 and the light-emitting functional layer 220, and thus reducing leakage current.

[0114] For example, based on such Figure 10 In the embodiment shown, in the region of the second portion 332b that overlaps with the light-emitting functional layer 220, the orthographic projection of the edge of the light-emitting functional layer 220 on the substrate 100 lies within the orthographic projection of the second sub-bottom 332 on the substrate 100.

[0115] For example, based on such Figure 10 In the embodiment shown, the first sub-bottom 331 of the second portion 332b overlaps with the second electrode 230.

[0116] In some embodiments of this disclosure, such as Figure 11 As shown, the distance from the surface of the second sub-bottom 332 away from the substrate 100 to the substrate 100 is greater than the distance from the surface of the first sub-bottom 331 away from the substrate 100 to the substrate 100. This effectively increases the height (or thickness) of the second sub-bottom 332, allowing it to block the extension of the light-emitting functional layer 220, thereby reducing the overlap area between the second sub-bottom 332 and the light-emitting functional layer 220 and thus reducing leakage current.

[0117] For example, based on such Figure 11 In the embodiment shown, the thickness of the second sub-bottom 332 is greater than the thickness of the first sub-bottom 331;

[0118] For example, based on such Figure 11In some embodiments shown, the shape of the second sub-bottom 332 in a cross section perpendicular to the plane of the substrate 100 is trapezoidal (e.g., a regular trapezoid) from the side of the second sub-bottom 332 that is connected to the first sub-bottom 331 to the side of the second sub-bottom 332 that is away from the first sub-bottom 331.

[0119] For example, based on such Figure 11 In some other embodiments shown, the surface of the second sub-bottom 332 away from the substrate 100 is convex, and the shape of the surface of the second sub-bottom 332 away from the substrate 100 in a cross section perpendicular to the plane where the substrate 100 is located is arc-shaped from the side of the second sub-bottom 332 that is in contact with the first sub-bottom 331 to the side of the second sub-bottom 332 that is away from the first sub-bottom 331.

[0120] In at least one embodiment of this disclosure, such as Figure 9A and Figure 9B As shown, the second electrode 230 is located on the first side 301a and / or the second side 301b. Figure 9A The climbing height H (the height of the portion in contact with the side wall of the support 310) of the edge of the second sub-bottom 332 (showing the case where the second sub-bottom 332 is provided on one side of the first side 301a) on the side wall of the support 310 is greater than the climbing height of the edge of the second electrode 230 on the side wall of the support 310 where the third side 301c and the fourth side 301d are located.

[0121] See again for at least one embodiment of this disclosure. Figure 3A The distance D1 between the first side 301a and the second side 301b of the isolation opening 301 is less than the distance D2 between the third side 301c and the fourth side 301d of the isolation opening 301. Thus, the first side 301a and the second side 301b are along the long side of the isolation opening 301. At the first side 301a and the second side 301b, there is a large connection area between the second electrode 230 of the light-emitting device 200 and the isolation structure 300, resulting in a relatively small impedance. Therefore, during the evaporation process, the scanning direction of the evaporation is controlled to make it easier for the evaporation material to be deposited at the first side 301a and the second side 301b. However, this also makes it easier for the evaporation film layer (light-emitting functional layer 220) to overlap with the support portion 310 of the isolation structure 300 at the first side 301a and the second side 301b. That is, at the first side 301a and the second side 301b, when the light-emitting functional layer 220 is connected to the support portion 310, the leakage current will be larger. By adopting the above-described solution of this disclosure, the leakage current at the first side 301a and the second side 301b can be avoided or reduced.

[0122] In at least one embodiment of this disclosure, the first direction and the second direction are perpendicular; for example, the first direction can be as follows: Figure 3A The X-axis direction is shown, and the second direction can be as follows: Figure 3A The Y-axis direction is shown.

[0123] See again for at least one embodiment of this disclosure. Figure 4A The display panel may also include a pixel defining layer 340, which is located on the substrate 100 and includes pixel openings 302 corresponding to the isolation openings 301 respectively. The pixel openings 302 are connected to the corresponding isolation openings 301. The light-emitting functional layer 220 of the light-emitting device 200 fills the pixel openings 302 and extends to the surface of the pixel defining layer 340 away from the substrate 100.

[0124] In at least one embodiment of this disclosure, the pixel defining layer 340 is an inorganic film layer. Inorganic film layers are denser and have higher insulation properties. In the process of fabricating the light-emitting device 200 based on the isolation structure 300, the pixel defining layer 340 does not need a high thickness to accommodate the light-emitting device 200, thus facilitating a thinner and lighter display panel design. Furthermore, as an inorganic film layer, the pixel defining layer 340 can have a higher bonding strength with the isolation structure 300 and the first electrode 210, reducing the risk of the isolation structure 300 and the first electrode 210 detaching. Additionally, the high density of the inorganic film layer can more effectively block the intrusion of water, oxygen, etc., thereby improving the encapsulation effect of the display panel. Moreover, when the pixel defining layer 340 is an inorganic layer, it can have a smaller thickness, thereby reducing the discontinuity at the edge of the pixel opening 302, improving the film continuity of the second electrode 230 at that location, reducing the impedance of the second electrode 230, and thus ensuring the display effect of the display panel.

[0125] In at least one embodiment of this disclosure, such as Figure 4A As shown, the orthographic projection of the pixel opening 302 on the substrate 100 is located within the orthographic projection of the isolation opening 301 on the substrate 100. In this way, the thickness of the portion of the vapor-deposited film layer falling in the pixel opening 302 can be relatively uniform, so as to ensure the luminous efficiency and quality of the luminous area (the area defined by the pixel opening 302) of the light-emitting device 200.

[0126] In at least one embodiment of this disclosure, such as Figure 4AAs shown, the orthographic projection of the pixel opening 302 onto the substrate 100 lies within the orthographic projection of the first electrode 210 onto the substrate 100, and the edge portion of the first electrode 210 lies between the pixel defining layer 340 and the substrate 100. The pixel opening 302 exposes at least a portion of the first electrode 210. The pixel defining layer 340 can space the conductive isolation structure 300 and the first electrode 210 of the light-emitting device 200, thereby allowing the gap between the light-emitting devices 200 to have a smaller design size, thereby increasing the pixel density (PPI) of the display panel.

[0127] In at least one embodiment of this disclosure, such as Figure 4A As shown, the pixel defining layer 340 is located between the isolation structure 300 and the substrate 100. When the pixel defining layer 340 is provided in the display panel, the first electrode 210 of the light-emitting device 200 can be designed to have a larger area to avoid positional misalignment (error caused by process precision) between the first electrode 210 and the isolation structure 300 during actual manufacturing, which would make it difficult to guarantee the actual light-emitting area of ​​the light-emitting device, thereby improving the aperture ratio (related to the light-emitting area of ​​the light-emitting device) and brightness of the displayed image of the display panel. For example, without the pixel defining layer 340, to avoid connection between the first electrode 210 and the isolation structure 300, the design area of ​​the first electrode 210 is limited. If the position of the first electrode 210 is misaligned, the light-emitting area of ​​the light-emitting device may be smaller than the designed area (the light-emitting area expected during design), resulting in a decrease in the brightness of the light-emitting device.

[0128] In at least one embodiment of this disclosure, such as Figure 4A As shown, the display panel may further include a first encapsulation layer 410, wherein the first encapsulation layer 410 is located on the side of the light-emitting device 200 facing away from the substrate 100 and includes a plurality of encapsulation units 411, each of which covers the corresponding isolation opening 301 of the light-emitting device 200. During the batch fabrication of the light-emitting device 200 based on the isolation structure 300, the encapsulation units 411 are fabricated synchronously with the light-emitting device 200, thereby protecting the already fabricated light-emitting device 200 during the process of fabricating the next batch of light-emitting devices 200 (which involves etching).

[0129] In cases where the light-emitting device 200 is divided into multiple types that emit different colors of light, each light-emitting device 200 emitting different colors of light is manufactured independently. However, the film layer (evaporated film layer, such as the light-emitting functional layer, etc.) in each light-emitting device 200 is deposited on the entire display panel during the evaporation process. For example, see [link to previous section]. Figures 2 to 5BThe light-emitting devices 200 are classified into three types: a first type (P1), a second type (P2), and a third type (P3) that emit different colors of light. During the manufacturing process, light-emitting devices P1, P2, and P3 are prepared sequentially. When preparing light-emitting device P1, a light-emitting device P1 is formed in each isolation opening 301. A first encapsulation layer 410 is prepared on the display panel to cover the light-emitting device P2. Then, the first encapsulation layer 410, as well as the anode and light-emitting functional layer of the light-emitting device P1, are removed from some of the isolation openings 301 (used to form light-emitting devices P2 and P3 in the final product) to obtain an encapsulation unit 411. In this process, the encapsulation unit 411 protects the light-emitting devices P1 in other isolation openings 301. Based on this method, light-emitting devices P2 and P3 are then prepared sequentially, ultimately forming a display panel as shown in the image. Figure 4A The first encapsulation layer 410 shown, that is, the first encapsulation layer 410 on the entire display panel, is obtained by multiple processes. This process can be found below. Figures 14A to 14I The relevant descriptions in the embodiments are not repeated here.

[0130] For example, the first type of light-emitting device (P1), the second type of light-emitting device (P2), and the third type of light-emitting device (P3) can emit red light, green light, and blue light respectively (in no particular order).

[0131] For example, such as Figure 4A As shown, the encapsulation unit 411 extends to the side of the isolation structure 300 facing away from the substrate 100. The portion of the encapsulation unit 411 located on the side of the isolation structure 300 facing away from the substrate 100 is a suspended portion, which is spaced apart from the isolation structure 300. In the above process, since the film layers used to form the structure of the light-emitting device 200 are separated by the isolation structure 300, these film layers are deposited on the display panel in their entirety. That is, these film layers cover the isolation structure 300. In the etching process of forming the encapsulation unit 411, the etching material etches the portion of the film layer covering the isolation structure 300, thereby making the edge portion of the encapsulation unit 411 suspended, thus forming a suspended portion.

[0132] In at least one embodiment of this disclosure, such as Figure 12As shown, the display panel further includes a second encapsulation layer 420 and a third encapsulation layer 430 covering the first encapsulation layer 410. The second encapsulation layer 420 is located between the first encapsulation layer 410 and the third encapsulation layer 430, and the third encapsulation layer 430 is located on the side of the second encapsulation layer 420 facing away from the substrate 100. The first encapsulation layer 410, the second encapsulation layer 420, and the third encapsulation layer 430 constitute an encapsulation structure 400. Optionally, the second encapsulation layer 420 is a planarization layer. Optionally, the second encapsulation layer 420 is an organic film layer, and the third encapsulation layer 430 is an inorganic film layer. Optionally, the second encapsulation layer 420 and the third encapsulation layer 430 are continuous film layers. The second encapsulation layer 420 can improve the flatness of the display panel surface, so as to facilitate the placement of other components on the encapsulation layer. In addition, the second encapsulation layer 420 can have a certain degree of flexibility to relieve the stress of the first encapsulation layer 410 and the third encapsulation layer 430, thereby improving the reliability of the display panel and making it more suitable for application in the field of flexible displays. Furthermore, the third encapsulation layer 430 has high density and a high barrier effect against water, oxygen, etc., and the third encapsulation layer 430 has higher strength, so as to facilitate the fabrication of other components (such as touch-related structures, optical films, etc.) on it.

[0133] In at least one embodiment of this disclosure, such as Figure 12 As shown, the substrate 100 may include a substrate and a driving circuit layer located on the substrate. The driving circuit layer includes multiple pixel driving circuits located in the display area, and the display function layer is located on the side of the driving circuit layer away from the substrate. For example, the pixel driving circuit may include multiple transistors (TFTs), capacitors, etc., and may be formed in various forms such as 7T1C (i.e., 7 transistors (TFTs) and 1 capacitor (C)), 8T1C, or 8T2C. The pixel driving circuit is connected to the light-emitting device 200 to control the switching state and brightness of the light-emitting device 200.

[0134] At least one embodiment of this disclosure provides a method for manufacturing the above-described display panel, the method including, for example, Figure 11 Steps S100 to S900 are as follows.

[0135] S100 provides a substrate and forms a plurality of first electrodes spaced apart from each other on the substrate.

[0136] S200, forming a pixel defining material layer, the pixel defining material layer covering the first electrode.

[0137] S300, an isolation structure is formed on a pixel defining material layer, wherein the isolation structure encloses and forms a plurality of isolation openings, the isolation openings corresponding to the first electrode respectively, the isolation structure includes a bottom and a main body portion stacked sequentially on a substrate, the orthographic projection of the support portion on the substrate is located within the orthographic projection of the crown portion on the substrate, the bottom includes a first sub-bottom portion connected to each other and a plurality of second sub-bottom portions extending from the first sub-bottom portion, the first sub-bottom portion is a mesh structure, the second sub-bottom portions are distributed in the mesh holes of the mesh structure, the orthographic projection of the first sub-bottom portion on the substrate at least partially coincides with the orthographic projection of the substrate-facing end of the main body portion on the substrate, the orthographic projection of the second sub-bottom portion on the substrate is located outside the orthographic projection of the substrate-facing end of the main body portion on the substrate, and the bottom is a conductive structure.

[0138] S400, a patterning process is performed on the pixel defining material layer to form a pixel defining layer, the pixel defining layer having a pixel opening that is at least a portion of the first electrode exposed and communicates with the isolation opening.

[0139] S500, depositing a light-emitting material thin film and a conductive material thin film, the light-emitting material thin film and the conductive material thin film covering an isolation structure and an isolation opening, wherein the portions of the light-emitting material thin film and the conductive material thin film located in the isolation opening respectively form a light-emitting functional layer and a second electrode, at least a portion of the bottom of the second electrode overlaps with the second electrode, and the first electrode, the light-emitting functional layer and the second electrode stacked on top of each other constitute a light-emitting device.

[0140] S600, deposits a film of encapsulating material to cover the light-emitting device.

[0141] S700 forms a photoresist layer on the packaging material film layer and performs a patterning process on the photoresist layer to form a photoresist pattern, which covers part of the isolation opening.

[0142] S800 is based on photoresist pattern etching of encapsulation material film and light-emitting device, wherein the remaining part of the encapsulation material film is formed into encapsulation unit, and the light-emitting functional layer and the second electrode not covered by the encapsulation unit are etched.

[0143] S900, repeat the above process to form a light-emitting device and a packaging unit at the isolation opening where no light-emitting device is formed, and all the packaging units constitute the first packaging layer.

[0144] In the display panel obtained in steps S100 to S900 above, the second sub-bottom at the bottom is not distributed around the isolation opening, but is only set in a local area around the isolation opening. In this way, the second electrode can still connect with the main body while still being connected to the second sub-bottom, so the impedance between the second electrode and the isolation structure is less affected. The light-emitting functional layer can only be indirectly connected to the main body through the second sub-bottom, thereby greatly reducing the channel area between the light-emitting functional layer and the isolation structure, so as to reduce the leakage current between the light-emitting functional layer and the isolation structure. This can reduce the power consumption of the display panel, improve the life of the light-emitting device, and improve the visual effect of the displayed image (e.g., improve the low grayscale image quality). The specific structure of the display panel obtained in steps S100 to S900, the technical problems faced, the technical means and principles for solving the technical problems, and further improvements can be found in the relevant descriptions in the foregoing embodiments, and will not be repeated here.

[0145] In at least one embodiment of this disclosure, step S300 described above may include: depositing a bottom conductive material film layer on a pixel defining material layer, and then performing a patterning process on the bottom conductive material film layer to form a bottom; forming a main conductive material layer covering the bottom, and performing a patterning process on the main conductive material layer to form a main body. This process can be found in the following description... Figures 14A to 14I The specific details will not be elaborated here.

[0146] Below, as follows Figure 4A Taking the display panel shown as an example, the method for manufacturing the display panel will be explained by way of example.

[0147] like Figure 14A As shown, a substrate 100 is provided and first electrodes 210 arranged in an array are formed on the substrate 100.

[0148] like Figure 14B As shown, a pixel defining material layer 340a is formed on a substrate 100 on which the first electrode 210 is formed.

[0149] like Figure 14C As shown, a bottom conductive material film layer 330a is formed on the pixel defining material layer 340a (considering that there are multiple conductive material film layers, they are numbered here and defined as the third material layer 330a).

[0150] like Figure 14D As shown, in the case of Figure 14C The third material layer 330a shown is patterned to form the bottom 330; then a main conductive material layer is deposited. For example, the main conductive material layer includes a first material layer 310a and a second material layer 320a.

[0151] For example, the material of the third material layer 330a can be molybdenum, the material of the first material layer 310a can be aluminum, and the material of the second material layer 320a can be titanium.

[0152] like Figure 14E As shown, the first material layer 310a and the second material layer 320a are patterned so that the first material layer 310a is formed as a support portion 310 and the second material layer 320a is formed as a crown portion 320, the edge of the crown portion 320 defining the edge of the isolation opening 301. The specific structure of this isolation structure 300 and its included bottom 330 can be found in the relevant descriptions in the foregoing embodiments, and will not be repeated here.

[0153] In embodiments of this disclosure, the patterning process can be a photolithographic patterning process, which may include, for example, coating a structural layer to be patterned with photoresist, exposing the photoresist using a photomask, developing the exposed photoresist to obtain a photoresist pattern, etching the structural layer using the photoresist pattern (optionally wet or dry etching), and then optionally removing the photoresist pattern. It should be noted that when the material of the structural layer (e.g., the photoresist pattern described below) includes photoresist, the structural layer can be directly exposed using a photomask to form the desired pattern.

[0154] like Figure 14F As shown, a patterning process is performed on the pixel defining material layer 340a based on the isolation structure 300 to form a pixel defining layer 340. The pixel defining layer 340 covers the gap between adjacent first electrodes 210, so that the planar shape of the pixel defining layer 340 is a grid.

[0155] like Figure 14G As shown, a light-emitting material thin film and a conductive material thin film are vapor-deposited on the substrate 100 to form a light-emitting functional layer 220 and a second electrode 230 in each isolation opening 301 of the isolation structure 300. The first electrode 210, the light-emitting functional layer 220 and the second electrode 230 stacked on each other at the isolation opening 301 form a light-emitting device 200. No mask is used in the vapor deposition process, so the vapor-deposited material will also be deposited on the crown 320. It should be noted that in the actual process, the vapor-deposited material will be deposited on the upper surface of the crown 320 away from the substrate 100 and on the sidewalls (not shown in the figure) to form a filling film 500a. Then, an encapsulation material film layer 410a is deposited to cover the light-emitting device 200 and the isolation structure 300.

[0156] For example, the light-emitting layer in the vapor-deposited light-emitting functional layer 220 can be light of the color corresponding to the second type of light-emitting device P2. That is, in this stage, the second type of light-emitting device P2 is formed in each isolation opening 301 of the isolation structure 300.

[0157] like Figure 14HAs shown, a photoresist is formed (e.g., coated) on a substrate 100 on which an encapsulation material film layer 410a is formed, and then a patterning process is performed on it to form a photoresist pattern 500, which only covers a portion of the isolation opening 301 of the isolation structure 300.

[0158] like Figure 14I As shown, the surface of the display panel is etched using the photoresist pattern 500 as a mask to remove the encapsulation material film layer 410a, the filling film 500a, the second electrode 230 and the light-emitting functional layer 220 that are not covered by the photoresist pattern 500. The remaining part of the encapsulation material film layer 410a forms the encapsulation unit of the first encapsulation layer 410. Then, the residual photoresist pattern 500 is removed.

[0159] It should be noted that, in cases such as Figure 14I In the process shown, the filler film 500a can be completely removed, or... The etching degree can be controlled so that at least a portion of the filler film 500a remains to support the suspended portion of the package unit, thereby reducing the risk of package unit breakage.

[0160] Repeat the above Figures 14G to 14I The steps are as follows: to form a first type of light-emitting device P1 and a third type of light-emitting device P3 in other isolation openings 301 respectively, and to form as shown in the figure. Figure 4A The display panel shown. The process of forming the first type of light-emitting device P1 and the third type of light-emitting device P3 differs from that of forming the second type of light-emitting device P2 in that the isolation opening 301 covered by the photoresist pattern 500 is different.

[0161] like Figure 15 As shown, when depositing the light-emitting functional layer (e.g., the first functional layer), if the deposition source P moves to face the isolation structure 300, the boundary of its deposition angle corresponds to lines A1 and A2 on the display panel. That is, the area between lines A1 and A2 will not be deposited in this case. However, the area on the side of lines A1 and A2 away from the isolation structure 300 will be deposited regardless of the position of the deposition source P. In other words, starting from the area of ​​line A1 or line A2, the closer to the isolation structure 300, the smaller the thickness of the light-emitting functional layer.

[0162] At least one embodiment of this disclosure provides a display device, which may include the display panel in the above embodiments or a display panel obtained by the manufacturing method in the above embodiments. For example, the display device may include a touch structure, an optical film (e.g., a microlens, a polarizer), a cover plate, or other structures disposed on the light-emitting side of the display panel.

[0163] For example, the display device can be any product or component with a display function, such as a television, digital camera, mobile phone, watch, tablet computer, laptop computer, or navigator.

[0164] It should be understood that the various forms of processes shown above can be used, with steps reordered, added, or deleted. For example, the steps described in this invention can be executed in parallel, sequentially, or in different orders, as long as the desired result of the technical solution of this invention can be achieved, and this is not limited herein.

[0165] The specific embodiments described above do not constitute a limitation on the scope of protection of this invention. Those skilled in the art should understand that various modifications, combinations, sub-combinations, and substitutions can be made according to design requirements and other factors. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this invention should be included within the scope of protection of this invention.

Claims

1. A display panel, characterized in that, include: substrate; An isolation structure is located on the substrate and includes a plurality of isolation openings, wherein the isolation structure includes a bottom portion and a main body portion stacked sequentially on the substrate; Multiple light-emitting devices are disposed on the substrate and correspond to the isolation openings respectively. Each light-emitting device includes a first electrode, a light-emitting functional layer, and a second electrode stacked on the substrate. The light-emitting functional layer and the second electrode are located in the corresponding isolation openings. The bottom includes a first sub-bottom connected to each other and a plurality of second sub-bottoms extending from the first sub-bottoms. The first sub-bottoms are a mesh structure, and the second sub-bottoms are distributed in the mesh openings of the mesh structure. The orthographic projection of the first sub-bottom on the substrate at least partially coincides with the orthographic projection of the end of the main body facing the substrate on the substrate. The orthographic projection of the second sub-bottom on the substrate is outside the orthographic projection of the end of the main body facing the substrate on the substrate. The bottom is a conductive structure, and at least a portion of the second sub-bottom overlaps with the second electrode.

2. The display panel according to claim 1, characterized in that, The orthographic projection of the end of the main body facing the substrate onto the substrate is located within the orthographic projection of the end of the main body away from the substrate onto the substrate. Preferably, the main body includes a support portion and a crown portion, the support portion is located between the bottom and the crown portion, and the orthographic projection of the support portion on the substrate is located within the orthographic projection of the crown portion on the substrate; Preferably, the orthographic projection of the first sub-bottom on the substrate coincides with the orthographic projection of the end of the support facing the substrate on the substrate, or is located within the orthographic projection of the end of the support facing the substrate on the substrate.

3. The display panel according to claim 2, characterized in that, The orthographic projection of the end of the support portion facing the crown portion on the substrate is located within the orthographic projection of the end of the support portion facing the substrate on the substrate.

4. The display panel according to claim 3, characterized in that, At least a portion of the orthographic projection of the second sub-bottom onto the substrate lies within the orthographic projection of the crown onto the substrate; Preferably, the orthographic projection of the second sub-bottom on the substrate is entirely within the orthographic projection of the crown on the substrate.

5. The display panel according to claim 1, characterized in that, The region of the second sub-bottom that is away from the first sub-bottom overlaps with the edge of the light-emitting functional layer, and the region of the second sub-bottom that is close to the first sub-bottom overlaps with the second electrode; Preferably, a plurality of second sub-bottoms are arranged in the isolation opening.

6. The display panel according to any one of claims 1 to 5, characterized in that, The isolation opening includes a first side and a second side opposite to each other along a first direction, and a third side and a fourth side opposite to each other along a second direction. The second sub-bottom can be set only for the first side and the second side, or the second sub-bottom can be set only for one of the first side and the second side.

7. The display panel according to claim 6, characterized in that, The size of the region of the second sub-bottom that is far from the first sub-bottom is smaller than the size of the region of the second sub-bottom that is connected to the first sub-bottom; Preferably, the size of the second sub-bottom gradually decreases from the edge of the isolation opening to the centroid of the isolation opening.

8. The display panel according to claim 6, characterized in that, The second sub-bottom has a trapezoidal planar shape, the side of the second sub-bottom that connects to the first sub-bottom is the base of the trapezoid, and the side of the second sub-bottom that is furthest from the first sub-bottom is the top of the trapezoid. The length of the base is greater than the length of the top; or The planar shape of the second sub-bottom is a triangle, and the side of the second sub-bottom that connects with the first sub-bottom is the side of the triangle.

9. The display panel according to claim 6, characterized in that, The second sub-bottom is only located on the side where the first side of the isolation opening is located; Preferably, the height of the portion of the second electrode that contacts the sidewall of the support on the side where the first side is located is greater than the height of the portion of the second electrode that contacts the sidewall of the support on the side where the second side is located.

10. The display panel according to claim 6, characterized in that, The second sub-bottom is distributed on both the side where the first side is located and the side where the second side is located; Preferably, the height of the portion of the second electrode that contacts the sidewall of the support on the side where the first side is located is greater than the height of the portion of the second electrode that contacts the sidewall of the support on the side where the second side is located.

11. The display panel according to claim 6, characterized in that, The second sub-bottom includes a first portion connected to the first sub-bottom and a second portion away from the first sub-bottom, wherein the thickness of the second portion is less than the thickness of the first portion; Preferably, in the region of the second portion that overlaps with the light-emitting functional layer, the orthographic projection of the edge of the light-emitting functional layer on the substrate lies within the orthographic projection of the second sub-bottom on the substrate; Preferably, the first sub-bottom of the second portion overlaps with the second electrode.

12. The display panel according to claim 6, characterized in that, The distance from the surface of the second sub-bottom away from the substrate to the substrate is greater than the distance from the surface of the first sub-bottom away from the substrate to the substrate; Preferably, the thickness of the second sub-bottom is greater than the thickness of the first sub-bottom.

13. The display panel according to claim 12, characterized in that, From the side of the second sub-bottom that connects to the first sub-bottom to the side of the second sub-bottom that is away from the first sub-bottom, the shape of the second sub-bottom in a cross-section perpendicular to the plane of the substrate is trapezoidal; or The surface of the second sub-bottom that is away from the substrate is convex, and the shape of the surface of the second sub-bottom that is away from the substrate in a cross section perpendicular to the plane where the substrate is located is arc-shaped, from the side of the second sub-bottom that is in contact with the first sub-bottom to the side of the second sub-bottom that is away from the first sub-bottom.

14. The display panel according to claim 6, characterized in that, The height of the second electrode at the edge of the first side and / or the side where the second side is located, which contacts the sidewall of the support, is greater than the height of the second electrode at the edge of the third side and the fourth side where it contacts the sidewall of the support.

15. The display panel according to claim 14, characterized in that, The distance between the first side and the second side of the isolation opening is less than the distance between the third side and the fourth side of the isolation opening; Preferably, the first direction and the second direction are perpendicular.

16. The display panel according to claim 1, characterized in that, It also includes a pixel defining layer, wherein the pixel defining layer is located on the substrate and includes pixel openings corresponding to the isolation openings. The pixel opening is connected to the corresponding isolation opening, and the light-emitting functional layer of the light-emitting device and the second electrode fill the pixel opening and extend to the surface of the pixel defining layer away from the substrate.

17. The display panel according to claim 1, characterized in that, It also includes a first encapsulation layer, wherein the first encapsulation layer is located on the side of the light-emitting device away from the substrate and includes a plurality of encapsulation units, the encapsulation units respectively covering the isolation opening corresponding to the light-emitting device.

18. A method for manufacturing a display panel, characterized in that, include: A substrate is provided, and a plurality of first electrodes spaced apart from each other are formed on the substrate; A pixel defining material layer is formed, the pixel defining material layer covering the first electrode; An isolation structure is formed on the pixel defining material layer, wherein the isolation structure encloses a plurality of isolation openings, each of which corresponds to the first electrode. The isolation structure includes a bottom and a main body portion stacked sequentially on the substrate. The bottom includes a first sub-bottom portion connected to each other and a plurality of second sub-bottom portions extending from the first sub-bottom portion. The first sub-bottom portion is a mesh structure, and the second sub-bottom portions are distributed in the mesh openings of the mesh structure. The orthographic projection of the first sub-bottom portion on the substrate at least partially overlaps with the orthographic projection of the substrate-facing end of the main body portion on the substrate. The orthographic projection of the second sub-bottom portion on the substrate is located outside the orthographic projection of the substrate-facing end of the main body portion on the substrate. The bottom is a conductive structure. The pixel defining material layer is patterned to form a pixel defining layer, the pixel defining layer having pixel openings that are at least partially exposed with respect to the first electrode and communicate with the isolation opening; A light-emitting material thin film and a conductive material thin film are deposited, wherein the light-emitting material thin film and the conductive material thin film cover the isolation structure and the isolation opening, wherein the portions of the light-emitting material thin film and the conductive material thin film located in the isolation opening respectively form a light-emitting functional layer and a second electrode, and at least a portion of the bottom of the second electrode overlaps with the second electrode, and the first electrode, the light-emitting functional layer and the second electrode stacked on top of each other constitute a light-emitting device; Deposit an encapsulation material film to cover the light-emitting device; A photoresist layer is formed on the encapsulation material film, and the photoresist layer is patterned to form a photoresist pattern, the photoresist pattern covering a portion of the isolation opening; The encapsulation material film and the light-emitting device are etched based on the photoresist pattern, wherein the remaining portion of the encapsulation material film forms an encapsulation unit, and the light-emitting functional layer and the second electrode not covered by the encapsulation unit are etched; and The above process is repeated to form the light-emitting device and the packaging unit at the isolation opening where the light-emitting device is not formed, and all the packaging units constitute the first packaging layer.

19. The preparation method according to claim 18, characterized in that, The formation of the isolation structure on the pixel-defining material layer includes: A bottom conductive material film is deposited on the pixel defining material layer, and then the bottom conductive material film is patterned to form the bottom. A main conductive material layer is formed to cover the bottom, and the main conductive material layer is patterned to form the main body.

20. A display device, characterized in that, The display panel includes any one of claims 1 to 17 or a display panel obtained by the preparation method described in claim 18 or 19.

Citation Information

Patent Citations

  • Display panel

    CN116583155A

  • Display panel and display device

    CN116600606A

  • Display panel, manufacturing method thereof and display device

    CN116669477A

  • Display panel and display device

    CN116669480A

  • Display panel and display device

    CN117062489A