Display panel, manufacturing method of display panel and electronic device
By creating grooves in the organic insulating layer to expose the first conductive layer, the first inorganic layer can directly contact the first conductive layer, thus solving the problem of insufficient interface strength in OLED display panels and improving the reliability and production efficiency of the display panels.
Patent Information
- Application Number
- CN202510661984.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-21
- Publication Date
- 2026-11-24
AI Technical Summary
In existing OLED display panels, the yield and performance reliability of the display panels need to be improved, especially due to insufficient interface strength between the organic insulating layer and the inorganic layer, which makes the film layers easy to separate, affecting the reliability and lifespan of the display panel.
A groove is provided in the organic insulating layer to expose the first conductive layer, so that the first inorganic layer is in direct contact with the first conductive layer, thereby reducing the interfacial stress between the film layers and increasing the interfacial strength.
It improves the reliability and production efficiency of display panels, avoids the risk of separation between film layers, simplifies the manufacturing process, and is easy to implement.
Smart Images

Figure CN123164983A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of display panel technology, and more specifically, to a display panel, a method for manufacturing the display panel, and an electronic device. Background Technology
[0002] Organic light-emitting diodes (OLEDs) and flat panel displays based on light-emitting diodes (LEDs) are widely used in various consumer electronics products such as mobile phones, televisions, laptops, and desktop computers due to their advantages such as high image quality, energy saving, thin body and wide range of applications, becoming the mainstream of display devices.
[0003] However, the yield rate and performance reliability of current OLED display panels need to be improved. Summary of the Invention
[0004] In order to overcome the above-mentioned shortcomings in the prior art, the purpose of this application is to provide a display panel, the display panel comprising: A substrate, the substrate including a first surface and a second surface disposed opposite to the first surface; A first conductive layer is located on one side of the first surface of the substrate. The first conductive layer includes a first edge, and the orthographic projection of the first edge of the first conductive layer on the substrate is located within the substrate. An organic insulating layer is located on the side of the first conductive layer away from the substrate, the organic insulating layer including a groove that exposes at least a portion of the first conductive layer, wherein at least a portion of the first edge of the first conductive layer is projected onto the substrate in the orthogonal projection of the groove onto the substrate; A first inorganic layer is located on the side of the organic insulating layer away from the substrate, and at least a portion of the first inorganic layer extends into the groove and covers the first conductive layer exposed by the groove.
[0005] In one possible implementation, the opening width of the groove on the side near the first conductive layer is greater than the thickness of the organic insulating layer.
[0006] In one possible implementation, the angle between the sidewall of the organic insulating layer facing the groove and the plane of the substrate is less than 45°.
[0007] In one possible implementation, a recessed structure is provided on the side of the first conductive layer away from the substrate, and at least a portion of the first inorganic layer extends into the recessed structure.
[0008] In one possible implementation, the first conductive layer includes at least two first planar regions and a first sloping region connecting two adjacent first planar regions; The sidewall of the organic insulating layer facing the groove includes a first end close to the first conductive layer and a second end away from the first conductive layer, the first end being in contact with a first planar region of the first conductive layer.
[0009] In one possible implementation, the display panel further includes at least one array functional film layer located on a first surface of the substrate and a second inorganic layer located on the array functional film layer away from the substrate; The first conductive layer is located on the side of the second inorganic layer away from the substrate, and the orthographic projection of the first edge of the first conductive layer on the substrate is located within the orthographic projection of the second inorganic layer on the substrate; Preferably, the groove exposes the first conductive layer and the second inorganic layer, with the first inorganic layer in contact with the second inorganic layer exposed by the groove.
[0010] In one possible implementation, the second inorganic layer includes at least two second planar regions and a second sloping region connecting two adjacent second planar regions; The sidewall of the organic insulating layer facing the groove includes a third end close to the second inorganic layer and a fourth end away from the second inorganic layer, the third end being in contact with the second planar region of the second inorganic layer; Preferably, the display panel further includes a second conductive layer, which is located between the array functional film layer and the second inorganic layer. The second conductive layer includes at least two spaced traces, and at least a portion of the second planar region of the second inorganic layer has its orthographic projection on the substrate at least partially coincides with the orthographic projection of the traces on the substrate.
[0011] In one possible implementation, the orthographic projection of the first edge of the first conductive layer onto the second inorganic layer lies within a second planar region of the second inorganic layer.
[0012] Another object of this application is to provide a method for manufacturing a display panel, the method comprising: A substrate is provided, the substrate including a first surface and a second surface disposed opposite to the first surface; A first conductive layer is disposed on one side of the first surface of the substrate; the first conductive layer includes a first edge, and the orthographic projection of the first edge of the first conductive layer on the substrate is located within the substrate; An organic insulating layer is disposed on the side of the first conductive layer away from the substrate, the organic insulating layer including a groove that exposes at least a portion of the first conductive layer, wherein at least a portion of the first edge of the first conductive layer is orthographically projected onto the substrate within the orthographically projected groove onto the substrate; A first inorganic layer is disposed on the side of the organic insulating layer away from the substrate, at least a portion of the first inorganic layer extending into the groove and covering the first conductive layer exposed by the groove.
[0013] Another object of this application is to provide an electronic device, the electronic device including the display panel provided in this application or the display panel manufactured by the method of manufacturing the display panel provided in this application.
[0014] Compared with the prior art, this application has the following beneficial effects: This application provides a display panel, a method for manufacturing the display panel, and an electronic device. Since the interfacial bonding strength between inorganic and organic materials is relatively weak, significantly less than that between inorganic and metallic materials, by providing a groove in the organic insulating layer that exposes the first edge of the first conductive layer, the first inorganic layer can directly contact the first conductive layer, thereby reducing the interfacial stress between the film layers and increasing the interfacial strength between the film layers. This avoids the risk of separation between the film layers and improves the reliability and production efficiency of the display panel. Attached Figure Description
[0015] To more clearly illustrate the technical solutions of the embodiments of this application, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of this application and should not be regarded as a limitation of the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.
[0016] Figure 1a This is one of the structural schematic diagrams of a display panel in related technologies; Figure 1b This is the second schematic diagram of the structure of a display panel in related technologies; Figure 2 This is one of the structural schematic diagrams of the display panel provided in the embodiments of this application; Figure 3 for Figure 2 One of the enlarged schematic diagrams of position A in the middle; Figure 4 for Figure 3 A partial sectional view at the location of BB' in the middle section; Figure 5 for Figure 2 Second enlarged schematic diagram of position A in the middle; Figure 6 This is a second schematic diagram of the structure of the display panel provided in the embodiments of this application; Figure 7 This is the third schematic diagram of the structure of the display panel provided in the embodiments of this application; Figure 8 Fourth schematic diagram of the structure of the display panel provided in the embodiments of this application; Figure 9 Fifth schematic diagram of the structure of the display panel provided in the embodiments of this application; Figure 10 A schematic flowchart illustrating the manufacturing method of the display panel provided in this application embodiment; Figure 11 This is a schematic diagram illustrating the manufacturing process of the display panel provided in an embodiment of this application.
[0017] Icons: 100-Substrate; 110-First surface; 120-Second surface; 200-First conductive layer; 201-Recessed structure; 210-First edge; 220-Second edge; 300-Organic insulating layer; 310-Groove; 301-First end; 302-Second end; 303-Third end; 304-Fourth end; 400-First inorganic layer; 500-Array functional film layer; 600-Second conductive layer; 700-Second inorganic layer; 810-Display area; 820-Non-display area. Detailed Implementation
[0018] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. The components of the embodiments of this application described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.
[0019] Therefore, the following detailed description of the embodiments of this application provided in the accompanying drawings is not intended to limit the scope of the claimed application, but merely to illustrate selected embodiments of the application. All other embodiments obtained by those skilled in the art based on the embodiments of this application without inventive effort are within the scope of protection of this application.
[0020] It should be noted that similar labels and letters in the following figures indicate similar items. Therefore, once an item is defined in one figure, it does not need to be further defined and explained in subsequent figures.
[0021] In the description of this application, it should be noted that the terms "center," "upper," "lower," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship commonly used when the product of the invention is in use. They are used only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application. In addition, the terms "first," "second," and "third," etc., are used only to distinguish descriptions and should not be construed as indicating or implying relative importance.
[0022] It should be noted that, where there is no conflict, different features in the embodiments of this application can be combined with each other.
[0023] Please refer to Figure 1a and Figure 1b The OLED display panel may include a substrate 100', a second inorganic layer 700', a first conductive layer 200', an organic insulating layer 300' and a first inorganic layer 400' stacked in sequence, wherein the orthographic projection of the first edge 210' of the first conductive layer 200' onto the substrate 100' is located within the substrate 100'.
[0024] Currently, in existing technologies, to reduce the risk of peeling at the interface, process methods are typically used to improve the interface strength between the organic insulating layer 300' and the first inorganic layer 400'. For example, the composition of the interface plasma treatment gas can be adjusted, or no gas can be used for interface treatment. However, this method cannot significantly improve the interface strength between the organic insulating layer 300' and the first inorganic layer 400', and its impact range is also relatively large. Furthermore, as the structure of display panels becomes more complex, the effectiveness of this method gradually decreases.
[0025] However, a discontinuous change in structural stiffness occurs at the first edge 210' of the first conductive layer 200'. At locations of discontinuity or abrupt change in structural stiffness, stress concentration easily occurs, resulting in significant interfacial normal and tangential stresses. When the interfacial stress exceeds the interfacial strength, peeling occurs between the organic insulating layer 300' and the first inorganic layer 400'. Furthermore, since the first conductive layer 200' is a single layer, the peeling area will be relatively large, thus affecting the reliability and lifespan of the display panel.
[0026] In view of this, this embodiment provides a solution to the above problems, and the solution provided in this embodiment will be described in detail below.
[0027] Please refer to Figure 2, Figure 2 Example: A schematic diagram of the structure of the display panel provided in this embodiment. The display panel may include a display area 810 and a non-display area 820 arranged around the display area 810.
[0028] Please refer to Figure 3 and Figure 4 , Figure 3 for Figure 2 An enlarged view of position A in the middle. Figure 4 for Figure 3 A partial cross-sectional view at the BB' position shows that the display panel may include a substrate 100, a first conductive layer 200, an organic insulating layer 300, and a first inorganic layer 400 stacked sequentially.
[0029] The substrate 100 may include a first surface 110 and a second surface 120 disposed opposite to the first surface 110. The material of the substrate 100 may be polyimide (PI).
[0030] The first conductive layer 200 may be located on the first surface 110 of the substrate 100. The first conductive layer 200 may include a first edge 210 and a second edge 220 connected to the first edge 210. The orthographic projection of the first edge 210 of the first conductive layer 200 on the substrate 100 may be located within the substrate 100.
[0031] In this embodiment, the orthographic projection area of the first conductive layer 200 on the substrate 100 can be smaller than the area of the first surface 110 of the substrate 100. The first conductive layer 200 can be a single piece. The orthographic projection of the first edge 210 of the first conductive layer 200 on the substrate 100 can be located within the substrate 100. The orthographic projection of the second edge 220 of the first conductive layer 200 on the substrate 100 can coincide with a portion of the edge of the substrate 100.
[0032] The material of the first conductive layer 200 can be a metallic material, such as titanium-aluminum-titanium (Ti-Al-Ti).
[0033] It should be noted that the shape of the first edge 210 of the first conductive layer 200 can be stepped or other shapes, such as L-shaped. The shape of the first edge 210 of the first conductive layer 200 can be adjusted according to actual needs, and no specific limitation is made here.
[0034] The organic insulating layer 300 may be located on the side of the first conductive layer 200 away from the substrate 100. The organic insulating layer 300 may include a groove 310 that exposes at least a portion of the first conductive layer 200. The orthographic projection of at least a portion of the first edge 210 of the first conductive layer 200 onto the substrate 100 may lie within the orthographic projection of the groove 310 onto the substrate 100. The material of the organic insulating layer 300 may be an organic adhesive.
[0035] In this embodiment, the cross-sectional area of the organic insulating layer 300 can be equal to the area of the first surface 110 of the substrate 100, that is, the orthographic projection of the organic insulating layer 300 on the substrate 100 can completely cover the orthographic projection of the first conductive layer 200 on the substrate 100. The surface of the organic insulating layer 300 away from the substrate 100 can be planar, and the organic insulating layer 300 may include a groove 310 provided along the first edge 210 of the first conductive layer 200. Please refer to... Figure 5 The groove 310 can expose the first edge 210 of the first conductive layer 200. The length of the groove 310 can be equal to the length of the first edge 210, and the shape of the groove 310 also matches the shape of the first edge 210. For example, in the extension direction of the groove 310, when the shape of the first edge 210 is stepped, the shape of the groove 310 can also be stepped.
[0036] The first inorganic layer 400 may be located on the side of the organic insulating layer 300 away from the substrate 100. At least a portion of the first inorganic layer 400 extends into the groove 310 and covers the first conductive layer 200 exposed in the groove 310. The material of the first inorganic layer 400 may be an inorganic material, such as silicon oxide and silicon nitride.
[0037] In this embodiment, the orthographic projection of the first inorganic layer 400 on the substrate 100 can completely cover the substrate 100. The first inorganic layer 400 can extend into the groove 310 of the organic insulating layer 300 and completely cover the first conductive layer 200 exposed in the groove 310. In this way, it can be ensured that the first edge 210 of the first conductive layer 200 is covered by the first inorganic layer 400, forming an inorganic-metal interface.
[0038] In the direction away from the substrate 100, the thickness of the first inorganic layer 400 in the groove 310 can be equal to the thickness of the first inorganic layer 400 at other locations. The surface of the first inorganic layer 400 on the side away from the substrate 100 may not be planar. The first inorganic layer 400 can form a recessed structure at the location of the groove 310, and the shape of the recessed structure matches the shape of the groove 310.
[0039] Based on the above design, in the display panel provided in this embodiment, since the interfacial bonding strength between inorganic and organic materials is weaker and significantly less than that between inorganic and metallic materials, by providing a groove 310 in the organic insulating layer 300 that exposes the first edge 210 of the first conductive layer 200, the first inorganic layer 400 can directly contact the first conductive layer 200, which can reduce the interfacial stress between the film layers and increase the interfacial strength between the film layers, thereby avoiding the risk of separation between the film layers and improving the reliability and production efficiency of the display panel.
[0040] In addition, compared with the existing technology that uses process methods to improve the interface strength between the organic insulating layer 300 and the first inorganic layer 400, the influence range of this embodiment is smaller, and the manufacturing process is simple and easy to implement.
[0041] In one possible implementation, please refer to Figure 6 The opening width W of the groove 310 near the first conductive layer 200 can be greater than the thickness H of the organic insulating layer 300.
[0042] In this embodiment, the opening width of the groove 310 near the first conductive layer 200 can be smaller than the opening width of the groove 310 away from the first conductive layer 200. That is, the sidewall of the organic insulating layer 300 facing the groove 310 is inclined. In the extension direction of the groove 310, the opening width of the groove 310 near the first conductive layer 200 is equal at all positions, and the opening width W of the groove 310 near the first conductive layer 200 can be greater than the maximum thickness H of the organic insulating layer 300. In this way, the stress of the first inorganic layer 400 can be dispersed over a larger area, avoiding local stress exceeding the interfacial bonding strength. At the same time, it can also ensure that the contact area between the first inorganic layer 400 and the first conductive layer 200 is larger, thereby improving the interfacial bonding strength between the first inorganic layer 400 and the first conductive layer 200.
[0043] In one possible implementation, please refer again. Figure 6 The angle α between the sidewall of the organic insulating layer 300 facing the groove 310 and the plane of the substrate 100 can be less than 45°.
[0044] In this embodiment, the angles between the two sidewalls of the organic insulating layer 300 facing the groove 310 and the plane of the substrate 100 can be equal and both less than 45°.
[0045] For example, the angle α between the sidewall of the organic insulating layer 300 facing the groove 310 and the plane of the substrate 100 may include 15°, 19°, 20°, 22°, 25°, 30°, 31°, 35°, 40° and 42°, etc. Preferably, the angle α between the sidewall of the organic insulating layer 300 facing the groove 310 and the plane of the substrate 100 may be 30°.
[0046] It should be noted that the angle between the sidewall of the organic insulating layer 300 facing the groove 310 and the plane of the substrate 100 can be adjusted according to actual needs, and no specific limitation is made here.
[0047] In the above design, the smaller the angle α between the sidewall of the organic insulating layer 300 facing the groove 310 and the plane of the substrate 100, the more dispersed the interfacial stress. This not only effectively avoids the risk of separation between the film layers, but also ensures that the first inorganic layer 400 can uniformly cover the sidewall of the organic insulating layer 300 facing the groove 310, further improving the interfacial bonding strength between the first inorganic layer 400 and the first conductive layer 200.
[0048] In one possible implementation, please refer to Figure 7 A recessed structure 201 is provided on the side of the first conductive layer 200 away from the substrate 100, and at least a portion of the first inorganic layer 400 can extend into the recessed structure 201.
[0049] In this embodiment, a recessed structure is provided on the side of the first conductive layer 200 away from the substrate 100. The groove 310 can expose the recessed structure 201 of the first conductive layer 200, so that when the first inorganic layer 400 comes into contact with the first conductive layer 200, a portion of the first inorganic layer 400 can extend into the recessed structure 201 of the first conductive layer 200, thereby increasing the interfacial bonding strength between the first inorganic layer 400 and the first conductive layer 200.
[0050] It should be noted that the size and shape of the recessed structure 201 of the first conductive layer 200 can be adjusted according to actual needs, and no specific limitation is made here.
[0051] In one possible implementation, please refer to Figure 8 The first conductive layer 200 may include at least two first planar regions and a first sloping region connecting two adjacent first planar regions. The sidewall of the organic insulating layer 300 facing the groove 310 may include a first end 301 close to the first conductive layer 200 and a second end 302 away from the first conductive layer 200, and the first end 301 of the sidewall may contact the first planar region of the first conductive layer 200.
[0052] In this embodiment, the thickness of the first conductive layer 200 is equal at all locations in the direction away from the substrate 100. Since other film layers on the side of the first conductive layer 200 near the substrate 100 may include multiple protrusions, the first conductive layer 200 may include at least one first planar region located on the side of the protrusions away from the substrate 100. The first conductive layer 200 may also include at least one first planar region located between two adjacent protrusions. A first sloped region may be used to connect at least one adjacent first planar region located on the side of the protrusions away from the substrate 100 and at least one first planar region located between two adjacent protrusions. The first planar region may be a flat surface, and the first sloped region may be a slope connecting two adjacent first planar regions, with the slope angle ranging from 20° to 45°.
[0053] In addition, the sidewall of the organic insulating layer 300 facing the groove 310 may include a first end 301 close to the first conductive layer 200 and a second end 302 away from the first conductive layer 200. The first end 301 of the sidewall contacts the first planar region of the first conductive layer 200 but does not contact the first slope region. In this way, the end of the first inorganic layer 400 that contacts the first conductive layer 200 can be located in the first planar region of the first conductive layer 200, thereby reducing the interface stress and improving the interface bonding strength between the first inorganic layer 400 and the first conductive layer 200.
[0054] In one possible implementation, please refer again. Figure 8 The display panel may further include at least one array functional film layer 500 located on the first surface 110 of the substrate 100 and a second inorganic layer 700 located on the array functional film layer 500 away from the substrate 100. The first conductive layer 200 may be located on the side of the second inorganic layer 700 away from the substrate 100, and the orthographic projection of the first edge 210 of the first conductive layer 200 on the substrate 100 may be located within the orthographic projection of the second inorganic layer 700 on the substrate 100.
[0055] In this embodiment, at least one array functional film layer 500 may be located on the first surface 110 of the substrate 100. The orthographic projection of the array functional film layer 500 on the substrate 100 may completely cover the substrate 100. The number of array functional film layers 500 located on the first surface 110 of the substrate 100 may be one, two, three, etc. When there are multiple array functional film layers 500, the multiple array functional film layers 500 may be stacked, and the orthographic projection area of the multiple array functional film layers 500 on the substrate 100 may be equal. For example, the multiple array functional film layers 500 may be capacitor insulating layer CI, gate insulating layer GI, buffer layer, etc.
[0056] The second inorganic layer 700 can be located on the side of the array functional film layer 500 away from the substrate 100, and the orthographic projection of the second inorganic layer 700 on the substrate 100 can completely coincide with the orthographic projection of the array functional film layer 500 on the substrate 100. The material of the second inorganic layer 700 can be an inorganic material, such as silicon oxide or silicon nitride. The first conductive layer 200 can be disposed on the side of the second inorganic layer 700 away from the substrate 100, and the orthographic projection of the first edge 210 of the first conductive layer 200 on the substrate 100 can lie within the orthographic projection of the second inorganic layer 700 on the substrate 100. That is, the first conductive layer 200 does not completely cover the second inorganic layer 700, and a portion of the second inorganic layer 700 can be exposed. The first edge 210 of the first conductive layer 200 can contact the second inorganic layer 700.
[0057] In one possible implementation, please refer to Figure 9 The groove 310 can expose the first conductive layer 200 and the second inorganic layer 700, and the first inorganic layer 400 can contact the second inorganic layer 700 exposed by the groove 310.
[0058] In this embodiment, the organic insulating layer 300 can be located on the side of the first conductive layer 200 and the second inorganic layer 700 away from the substrate 100. The groove 310 of the organic insulating layer 300 can simultaneously expose a portion of the first conductive layer 200 and a portion of the second inorganic layer 700 on the side of the organic insulating layer 300 close to the substrate 100. The bottom shape of the groove 310 matches the shape of the surface of the first conductive layer 200 away from the substrate 100 and the surface of the second inorganic layer 700 away from the substrate 100. The first inorganic layer 400 located on the side of the organic insulating layer 300 away from the substrate 100 can contact the first conductive layer 200 and the second inorganic layer 700 exposed in the groove 310, and the groove 310... The shape of the first inorganic layer 400 on the bottom surface matches the shape of the first conductive layer 200 and the second inorganic layer 700 exposed in the groove 310. For example, if the first conductive layer 200 and the second inorganic layer 700 exposed in the groove 310 are both planar, then the shape of the first inorganic layer 400 that contacts the first planar region of the first conductive layer 200 on the bottom surface of the groove 310 is also planar, and the shape of the first inorganic layer 400 that contacts the second inorganic layer 700 on the bottom surface of the groove 310 is also planar. If the shape of the first conductive layer 200 and the second inorganic layer 700 exposed in the groove 310 is an uneven stepped shape, then the shape of the first inorganic layer 400 on the bottom surface of the groove 310 is also stepped.
[0059] In addition, the width of the first inorganic layer 400 located on the bottom surface of the groove 310 and in contact with the first conductive layer 200 can be greater than the width of the first inorganic layer 400 located on the bottom surface of the groove 310 and in contact with the second inorganic layer 700. In this way, the contact area between the first inorganic layer 400 and the first conductive layer 200 can be increased, thereby improving the interfacial bonding strength between the first inorganic layer 400 and the first conductive layer 200 and avoiding the risk of separation between the film layers.
[0060] It should be noted that the width of the first inorganic layer 400 located on the bottom surface of the groove 310 and in contact with the first conductive layer 200 can also be equal to or less than the width of the first inorganic layer 400 located on the bottom surface of the groove 310 and in contact with the second inorganic layer 700. The specific width can be adjusted according to actual needs, and no specific limitation is made here.
[0061] In one possible implementation, please refer again. Figure 8 The second inorganic layer 700 may include at least two second planar regions and a second slope region connecting two adjacent second planar regions. The sidewall of the organic insulating layer 300 facing the groove 310 may include a third end 303 close to the second inorganic layer 700 and a fourth end 304 away from the second inorganic layer 700. The third end 303 is in contact with the second planar region of the second inorganic layer 700.
[0062] In this embodiment, the display panel may further include a second conductive layer 600. The second conductive layer 600 may be located on the side of the second inorganic layer 700 near the substrate 100. The second conductive layer 600 may be in contact with the second inorganic layer 700 and the array functional film layer 500. The orthographic projection of the second conductive layer 600 on the substrate 100 may be located within the orthographic projection of the array functional film layer 500 on the substrate 100. The second conductive layer 600 may include at least two spaced-apart traces. The material of the second conductive layer 600 is a metallic material.
[0063] The second inorganic layer 700 can cover at least two spaced traces of the second conductive layer 600. The thickness of the second inorganic layer 700 is equal at all locations in the direction away from the substrate 100. Therefore, the second inorganic layer 700 can form at least two second planar regions and a second slope region connecting adjacent second planar regions. At least one second planar region of the second inorganic layer 700 can be located on the surface of the second conductive layer 600 away from the substrate 100, and at least one second planar region of the second inorganic layer 700 can be located on the surface of the array functional film layer 500 away from the substrate 100. The second slope region of the second inorganic layer 700 can be used to connect adjacent second planar regions located on the side of the second conductive layer 600 away from the substrate 100 and second planar regions located on the side of the array functional film layer 500 away from the substrate 100. The second planar regions can be flat areas, and the second slope regions can be slopes connecting adjacent second planar regions, with an inclination angle ranging from 20° to 45°.
[0064] The first conductive layer 200 is located on the side of the second inorganic layer 700 away from the substrate 100, and the thickness of the first conductive layer 200 is equal at all locations in the direction away from the substrate 100. Therefore, the surface shape of the first conductive layer 200 on the side away from the substrate 100 can match the surface shape of the second inorganic layer 700 on the side away from the substrate 100. That is, the position of the first planar region of the first conductive layer 200 can correspond to the position of the second planar region of the second inorganic layer 700, and the position of the first slope region of the first conductive layer 200 can correspond to the position of the second slope region of the second inorganic layer 700.
[0065] In addition, the sidewall of the organic insulating layer 300 facing the groove 310 may also include a third end 303 near the second inorganic layer 700 and a fourth end 304 away from the second inorganic layer 700. The third end 303 of the sidewall may contact the second planar region of the second inorganic layer 700, but not the second slope region of the second inorganic layer 700. In this way, the end of the first inorganic layer 400 that contacts the second inorganic layer 700 can be located in the second planar region of the second inorganic layer 700, thereby reducing the interface stress.
[0066] In one possible implementation, the orthographic projection of the first edge 210 of the first conductive layer 200 onto the second inorganic layer 700 may lie within the second planar region of the second inorganic layer 700.
[0067] In this embodiment, the first edge 210 of the first conductive layer 200 can contact the second planar region of the second inorganic layer 700, but not the second slope region of the second inorganic layer 700. Specifically, the first edge 210 of the first conductive layer 200 can contact the second planar region located on the side of the second conductive layer 600 away from the substrate 100, and the first edge 210 of the first conductive layer 200 can also contact the second planar region located on the side of the array functional film layer 500 away from the substrate 100. In this way, the interfacial stress between the film layers can be further reduced, while the interfacial bonding strength between the film layers can be increased.
[0068] This application also provides a method for manufacturing a display panel, please refer to... Figure 10 The method for manufacturing a display panel may include the following steps.
[0069] Step S110: A substrate 100 is provided, the substrate 100 including a first surface 110 and a second surface 120 disposed opposite to the first surface 110.
[0070] In this embodiment, the substrate 100 may include a first surface 110 and a second surface 120 disposed opposite to each other, wherein the material of the substrate 100 may be polyimide (PI).
[0071] Step S120: A first conductive layer 200 is disposed on one side of the first surface 110 of the substrate 100; the first conductive layer 200 includes a first edge 210 and a second edge 220 connected to the first edge 210, and the orthographic projection of the first edge 210 of the first conductive layer 200 on the substrate 100 is located within the substrate 100.
[0072] In this embodiment, at least one array functional film layer 500 can be formed on the first surface 110 of the substrate 100 provided in step S110. The orthographic projection of the array functional film layer 500 on the substrate 100 can completely cover the substrate 100. When there are multiple array functional film layers 500, the multiple array functional film layers 500 can be stacked, and the orthographic projection area of the multiple array functional film layers 500 on the substrate 100 can be equal. For example, the multiple array functional film layers 500 can be buffer layer, inorganic semiconductor active layer P-Si, gate insulating layer GI, gate M1, capacitor insulating layer CI, and interlayer dielectric layer ILD, etc.
[0073] Additionally, a second conductive layer 600 and a second inorganic layer 700 can be sequentially disposed on the side of the array functional film layer 500 away from the substrate 100. The second conductive layer 600 can be located on the side of the second inorganic layer 700 closer to the substrate 100. The second conductive layer 600 can be in contact with the second inorganic layer 700 and the array functional film layer 500. The orthographic projection of the second conductive layer 600 on the substrate 100 can be located within the orthographic projection of the array functional film layer 500 on the substrate 100. Multiple protrusion structures can be formed on the surface of the second conductive layer 600 on the side of the array functional film layer 500 away from the substrate 100. The second inorganic layer 700 can cover the multiple protrusion structures formed by the second conductive layer 600, thereby forming at least two second planar regions and a second slope region connecting two adjacent second planar regions.
[0074] After forming the second inorganic layer 700, a first conductive layer 200 can be disposed on the side of the second inorganic layer 700 away from the substrate 100. The orthographic projection area of the first conductive layer 200 on the substrate 100 can be smaller than the area of the first surface 110 of the substrate 100. The orthographic projection of the first edge 210 of the first conductive layer 200 on the substrate 100 can be located within the substrate 100, and the orthographic projection of the second edge 220 of the first conductive layer 200 on the substrate 100 can coincide with a portion of the edge of the substrate 100. In addition, the thickness of the first conductive layer 200 is equal at all locations in the direction away from the substrate 100. Therefore, the surface shape of the side of the first conductive layer 200 away from the substrate 100 can match the surface shape of the side of the second inorganic layer 700 away from the substrate 100. That is, the first conductive layer 200 can include a first planar region corresponding to the second planar region and a first slope region corresponding to the second slope region.
[0075] In step S130, an organic insulating layer 300 is provided on the side of the first conductive layer 200 away from the substrate 100. The organic insulating layer 300 includes a groove 310 that exposes at least a portion of the first conductive layer 200. The orthographic projection of at least a portion of the first edge 210 of the first conductive layer 200 on the substrate 100 lies within the orthographic projection of the groove 310 on the substrate 100.
[0076] In this embodiment, please refer to Figure 11An organic insulating layer 300 can be formed on the side of the first conductive layer 200 and the second inorganic layer 700 away from the substrate 100, which is formed in step S120. The surface of the organic insulating layer 300 on the side away from the substrate 100 can be planar. After the organic insulating layer 300 is formed, it can be etched to form a groove 310 that exposes at least a portion of the first conductive layer 200 and at least a portion of the second inorganic layer 700. The bottom shape of the groove 310 matches the shape of the surface of the first conductive layer 200 away from the substrate 100 and the surface of the second inorganic layer 700 away from the substrate 100. The groove 310 can expose the first edge 210 of the first conductive layer 200, and the length of the groove 310 can be equal to the length of the first edge 210.
[0077] In some cases, the groove 310 can be formed by dry etching or wet etching.
[0078] In step S140, a first inorganic layer 400 is disposed on the side of the organic insulating layer 300 away from the substrate 100. At least a portion of the first inorganic layer 400 extends into the groove 310 and covers the first conductive layer 200 exposed in the groove 310.
[0079] In this embodiment, a first inorganic layer 400 can be provided on the side of the organic insulating layer 300 provided in step S130 away from the substrate 100. The first inorganic layer 400 can contact the first conductive layer 200 and the second inorganic layer 700 exposed in the groove 310, and the shape of the first inorganic layer 400 located on the bottom surface of the groove 310 matches the shape of the first conductive layer 200 and the second inorganic layer 700 exposed in the groove 310.
[0080] In the above design, by etching the organic insulating layer 300 above the first edge 210 of the first conductive layer 200 to form a groove 310 exposing the first edge 210, the first inorganic layer 400 above the organic insulating layer 300 can directly contact the first conductive layer 200, thereby reducing the interfacial stress between the film layers and increasing the interfacial strength between the film layers, thus avoiding the risk of separation between the film layers and improving the reliability and production efficiency of the display panel.
[0081] This application also provides an electronic device, which may include the display panel provided in this application or a display panel manufactured using the method described in this application. The electronic device may include devices with display functions such as monitors, video walls, mobile phones, tablets, laptops, and televisions.
[0082] In summary, the embodiments of this application provide a display panel, a method for manufacturing the display panel, and an electronic device. Since the interfacial bonding strength between inorganic and organic materials is relatively weak, significantly less than that between inorganic and metallic materials, by providing a groove in the organic insulating layer that exposes the first edge of the first conductive layer, the first inorganic layer can directly contact the first conductive layer, thereby reducing the interfacial stress between the film layers and increasing the interfacial strength between the film layers. This avoids the risk of separation between the film layers and improves the reliability and production efficiency of the display panel.
[0083] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0084] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.
Claims
1. A display panel, characterized by, The display panel includes: A substrate, the substrate including a first surface and a second surface disposed opposite to the first surface; A first conductive layer is located on one side of the first surface of the substrate. The first conductive layer includes a first edge, and the orthographic projection of the first edge of the first conductive layer on the substrate is located within the substrate. An organic insulating layer is located on the side of the first conductive layer away from the substrate, the organic insulating layer including a groove that exposes at least a portion of the first conductive layer, wherein at least a portion of the first edge of the first conductive layer is projected onto the substrate in the orthogonal projection of the groove onto the substrate; A first inorganic layer is located on the side of the organic insulating layer away from the substrate, and at least a portion of the first inorganic layer extends into the groove and covers the first conductive layer exposed by the groove.
2. The display panel of claim 1, wherein, The opening width of the groove on the side closest to the first conductive layer is greater than the thickness of the organic insulating layer.
3. The display panel of claim 1, wherein, The angle between the sidewall of the organic insulating layer facing the groove and the plane of the substrate is less than 45°.
4. The display panel of claim 1, wherein, The first conductive layer has a recessed structure on the side away from the substrate, and at least a portion of the first inorganic layer extends into the recessed structure.
5. The display panel of claim 1, wherein, The first conductive layer includes at least two first planar regions and a first sloping region connecting two adjacent first planar regions; The sidewall of the organic insulating layer facing the groove includes a first end close to the first conductive layer and a second end away from the first conductive layer, the first end being in contact with a first planar region of the first conductive layer.
6. The display panel of claim 1, wherein, The display panel further includes at least one array functional film layer located on a first surface of the substrate and a second inorganic layer located away from the substrate from the array functional film layer; The first conductive layer is located on the side of the second inorganic layer away from the substrate, and the orthographic projection of the first edge of the first conductive layer on the substrate is located within the orthographic projection of the second inorganic layer on the substrate; Preferably, the groove exposes the first conductive layer and the second inorganic layer, with the first inorganic layer in contact with the second inorganic layer exposed by the groove.
7. The display panel of claim 6, wherein, The second inorganic layer includes at least two second planar regions and a second sloping region connecting two adjacent second planar regions; The sidewall of the organic insulating layer facing the groove includes a third end close to the second inorganic layer and a fourth end away from the second inorganic layer, the third end being in contact with the second planar region of the second inorganic layer; Preferably, the display panel further includes a second conductive layer, which is located between the array functional film layer and the second inorganic layer. The second conductive layer includes at least two spaced traces, and at least a portion of the second planar region of the second inorganic layer has its orthographic projection on the substrate at least partially coincides with the orthographic projection of the traces on the substrate.
8. The display panel of claim 7, wherein, The orthographic projection of the first edge of the first conductive layer onto the second inorganic layer lies within the second planar region of the second inorganic layer.
9. A manufacturing method of a display panel, comprising: The method includes: A substrate is provided, the substrate including a first surface and a second surface disposed opposite to the first surface; A first conductive layer is disposed on one side of the first surface of the substrate; the first conductive layer includes a first edge, and the orthographic projection of the first edge of the first conductive layer on the substrate is located within the substrate; An organic insulating layer is disposed on the side of the first conductive layer away from the substrate, the organic insulating layer including a groove that exposes at least a portion of the first conductive layer, wherein at least a portion of the first edge of the first conductive layer is orthographically projected onto the substrate within the orthographically projected groove onto the substrate; A first inorganic layer is disposed on the side of the organic insulating layer away from the substrate, at least a portion of the first inorganic layer extending into the groove and covering the first conductive layer exposed by the groove.
10. An electronic device, comprising: The electronic device includes a display panel as described in any one of claims 1-8 or a display panel manufactured by the method described in claim 9.