Display panel, manufacturing method thereof and display device
By setting grooves on the first isolation layer of the isolation structure, the resistance of the conductive layer is increased or interrupted, thus solving the problem of 'bright spots' caused by local low-resistance conductive channels in OLED display panels and improving the display effect.
Patent Information
- Application Number
- CN202611459306.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-18
- Publication Date
- 2026-11-24
AI Technical Summary
In OLED display panels, abnormal current concentration caused by localized low-resistance conductive channels can create constantly lit "bright spots," reducing the display effect.
A groove is provided on the first isolation layer of the isolation structure so that the orthogonal projection of the conductive layer on the substrate covers the orthogonal projection of the groove, thereby increasing or blocking the resistance of the conductive layer and avoiding the formation of low-resistance metal-semiconductor ohmic contact points.
This improves the phenomenon where the driving current bypasses the light-emitting layer and is directly conducted to the semiconductor layer after passing through the conductive layer, reducing the 'bright spot' phenomenon and improving the display effect of the display panel.
Smart Images

Figure CN123164989A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of display technology, and more particularly to a display panel, a method for manufacturing the same, and a display device. Background Technology
[0002] Silicon-based micro-organic light-emitting diode (OLED) display panels have an undercut isolation structure. During the formation of the light-emitting functional layer of the OLED device, localized low-resistance conductive channels can easily appear within the OLED device. This causes the OLED device to overload and emit light due to abnormally concentrated current, forming constantly lit "bright spots" and reducing the display panel's performance. Summary of the Invention
[0003] This invention provides a display panel, a method for manufacturing the same, and a display device to improve the "bright spot" phenomenon of the display panel and enhance its display effect.
[0004] In a first aspect, embodiments of the present invention provide a display panel, comprising: Substrate; An isolation structure is disposed on one side of the substrate, the isolation structure having an opening area; the isolation structure includes a first isolation layer having a groove. A light-emitting functional layer is disposed within the opening area; A conductive layer is disposed on the side of the light-emitting functional layer away from the substrate; the orthogonal projection of the conductive layer on the substrate covers the orthogonal projection of the groove on the substrate.
[0005] Optionally, the depth of the groove is greater than or equal to the thickness of the conductive layer.
[0006] Optionally, the groove extends through the first insulating layer.
[0007] Optionally, the first isolation layer includes a first isolation structure and a second isolation structure; along the direction from the isolation structure to the opening area, the first isolation structure is disposed on one side of the groove, and at least a portion of the first isolation structure is located outside the opening area; the second isolation structure is disposed on the other side of the groove and located within the opening area; the width of the second isolation structure is greater than or equal to a first preset value.
[0008] Optionally, the orthographic projection of the first isolation structure on the substrate overlaps with the orthographic projection of the light-emitting functional layer on the substrate.
[0009] Optionally, the display panel further includes a cathode layer and a light extraction layer, wherein the cathode layer is disposed on the side of the conductive layer away from the substrate, and the light extraction layer is disposed between the conductive layer and the cathode layer, and the light extraction layer is used to planarize the surface of the conductive layer.
[0010] Optionally, the isolation structure further includes: The second isolation layer is disposed on the side of the first isolation layer away from the substrate, and the orthographic projection of the second isolation layer on the substrate is located within the orthographic projection of the first isolation structure on the substrate; A third isolation layer is disposed on the side of the second isolation layer away from the substrate, wherein the orthographic projection of the second isolation layer on the substrate lies within the orthographic projection of the third isolation layer on the substrate, and the orthographic projection of the third isolation layer on the substrate lies within the orthographic projection of the first isolation layer on the substrate.
[0011] Optionally, the light-emitting functional layer includes a first sub-light-emitting functional layer, a charge-generating layer, and a second sub-light-emitting functional layer stacked sequentially; within the opening region, the orthogonal projection of the second sub-light-emitting functional layer on the substrate lies within the orthogonal projection of the charge-generating layer on the substrate.
[0012] Optionally, the display panel further includes an anode layer disposed between the first isolation layer and the substrate, with at least a portion of the anode layer located within the opening region.
[0013] Secondly, embodiments of the present invention provide a method for manufacturing a display panel, comprising: An isolation structure is formed on one side of a substrate; the isolation structure has an opening region; the isolation structure includes a first isolation layer; The first isolation layer is patterned to form grooves; A light-emitting functional layer is formed within the opening area; A conductive layer is formed on the light-emitting functional layer; the orthogonal projection of the conductive layer on the substrate covers the orthogonal projection of the groove on the substrate.
[0014] Optionally, the first isolation layer is patterned to form grooves, including: A photoresist is formed on the isolation structure; the photoresist exposes the groove location of the first isolation layer; The first isolation layer is etched to form the groove; Remove the photoresist.
[0015] Thirdly, embodiments of the present invention provide a display device, including the display panel described in the first aspect.
[0016] The technical solution of this invention, by setting a groove on the first isolation layer, allows the orthogonal projection of the conductive layer on the substrate to cover the orthogonal projection of the groove on the substrate. This increases the resistance of the conductive layer at the groove or isolates it, preventing the formation of a low-resistance metal-semiconductor ohmic contact between the conductive layer and the semiconductor layer in the light-emitting functional layer. During the operation of the display panel, this improves the phenomenon where the driving current, after passing through the conductive layer, bypasses part of the light-emitting functional layer and directly conducts to the semiconductor layer in the light-emitting functional layer. This also improves the problem of local low-resistance conductive channels overloading and emitting "bright spots" due to abnormal current concentration, thus enhancing the display effect of the display panel.
[0017] It should be understood that the description in this section is not intended to identify key or essential features of the embodiments of the present invention, nor is it intended to limit the scope of the invention. Other features of the invention will become readily apparent from the following description. Attached Figure Description
[0018] To more clearly illustrate the technical solutions in the embodiments of the present invention, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0019] Figure 1 This is a schematic diagram of the structure of a display panel provided in an embodiment of the present invention; Figure 2 for Figure 1 A partially enlarged schematic diagram of the dashed frame E of the provided display panel; Figure 3 This is a schematic diagram of another display panel structure provided in an embodiment of the present invention; Figure 4 A schematic flowchart illustrating a method for manufacturing a display panel according to an embodiment of the present invention; Figure 5 This is a schematic diagram of a display panel forming an isolation structure according to an embodiment of the present invention; Figure 6 This is a schematic diagram of a patterned structure of a first isolation layer provided in an embodiment of the present invention; Figure 7 This is a schematic diagram of a display panel forming a light-emitting functional layer, provided by an embodiment of the present invention. Figure 8 This is a schematic diagram of a structure for forming a conductive layer on a display panel according to an embodiment of the present invention; Figure 9 This is a schematic diagram of an isolation structure with photoresist provided in an embodiment of the present invention; Figure 10This is a schematic diagram of an etching first isolation layer provided in an embodiment of the present invention; Figure 11 This is a schematic diagram of the structure of a display device provided in an embodiment of the present invention. Detailed Implementation
[0020] To enable those skilled in the art to better understand the present invention, the technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of the present invention.
[0021] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this invention are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of the invention described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover a non-exclusive inclusion; for example, a process, method, system, product, or apparatus that comprises a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, methods, products, or apparatus.
[0022] In existing technologies, OLED devices in OLED display panels can be stacked or cascaded OLEDs. In this case, different light-emitting layers can be connected through a charge-generating layer to improve the performance of the OLED devices. When the light-emitting functional layers of different OLED devices are disconnected by an undercut-type isolation structure, the charge-generating layer is prone to physical short-circuiting with the conductive layer on the side of the light-emitting functional layer furthest from the substrate. This forms a metal-semiconductor ohmic contact point between the charge-generating layer and the conductive layer, establishing a locally low-resistance conductive channel. When the OLED device emits light, the current in the OLED device bypasses the normal light-emitting layer and is directly transmitted through the charge-generating layer. This causes the locally low-resistance conductive channel to overload and emit light due to abnormal current concentration, forming a constantly lit "bright spot" and reducing the display effect of the display panel.
[0023] To address the aforementioned technical problems, embodiments of the present invention provide a display panel. Figure 1 This is a schematic diagram of the structure of a display panel provided in an embodiment of the present invention. Figure 2 for Figure 1 A partially enlarged schematic diagram of the dashed frame E of the provided display panel. (See attached image.) Figure 1 and Figure 2As shown, the display panel includes a substrate ( Figure 1 (Not shown in the image) An isolation structure 20, a light-emitting functional layer 30, and a conductive layer 40. The isolation structure 20 is disposed on one side of the substrate and has an opening region A; the isolation structure 20 includes a first isolation layer 210, on which a groove B is provided; the light-emitting functional layer 30 is disposed within the opening region A; the conductive layer 40 is disposed on the side of the light-emitting functional layer 30 away from the substrate; the orthographic projection of the conductive layer 40 on the substrate covers the orthographic projection of the groove B on the substrate.
[0024] Specifically, the isolation structure 20 has an opening region A, which defines the position of the OLED device. The isolation structure 20 can be an undercut type structure. The conductive layer 40 can be made of an alloy of Yb and Mg / Ag. The conductive layer 40 has a relatively thin film thickness, for example, the thickness of the conductive layer 40 can be in the range of 100~150 Å. The OLED device composed of the light-emitting functional layer 30 can be a stacked or tandem OLED. In this case, the light-emitting functional layer 30 includes at least two light-emitting layers, and adjacent light-emitting layers are connected in series through a charge generation layer. Anode and cathode layers can also be disposed on both sides of the light-emitting functional layer 30 to form a microcavity. The conductive layer 40 is disposed in the microcavity to enhance the microcavity effect of the OLED device. When the light-emitting functional layer 30 and the conductive layer 40 are formed in the opening region A, the isolation structure 20 can isolate the light-emitting functional layer 30 and the conductive layer 40 in different opening regions A, thereby improving the crosstalk phenomenon between different OLED devices. When the conductive layer 40 in different opening regions A is separated by the isolation structure 20, the conductive layer 40 is prone to physical short-circuiting with the semiconductor layer (which can be a charge-generating layer) in the light-emitting functional layer 30. Simultaneously, the orthogonal projection of the conductive layer 40 onto the substrate overlaps the orthogonal projection of the groove B onto the substrate, resulting in poor flatness of the conductive layer 40 at the groove B. When the conductive layer 40 is relatively thin, its resistance increases or it is directly blocked at the groove B. The groove B is located on the first isolation layer 210, near the edge of the opening region A. Therefore, the resistance of the conductive layer 40 increases or it is directly blocked near the edge of the opening region A. At this point, the conductive layer 40 and the semiconductor layer in the light-emitting functional layer 30 cannot form a low-resistance metal-semiconductor ohmic contact point, and a local low-resistance conductive channel cannot be established. During the light emission process of the OLED device, when the driving current flows through the conductive layer 40, it can improve the phenomenon where the driving current bypasses part of the light-emitting functional layer 30 and is directly conducted to the semiconductor layer in the light-emitting functional layer 30. This improves the display panel's display effect by preventing "bright spots" from forming due to overload caused by abnormal current concentration in local low-resistance conductive channels.
[0025] The technical solution of this embodiment, by setting a groove on the first isolation layer, allows the orthogonal projection of the conductive layer on the substrate to cover the orthogonal projection of the groove on the substrate. This increases the resistance of the conductive layer at the groove or isolates it, preventing the formation of a low-resistance metal-semiconductor ohmic contact between the conductive layer and the semiconductor layer in the light-emitting functional layer. During the operation of the display panel, this improves the phenomenon where the driving current, after passing through the conductive layer, bypasses part of the light-emitting functional layer and directly conducts to the semiconductor layer in the light-emitting functional layer. This improves the problem of local low-resistance conductive channels overloading and emitting "bright spots" due to abnormal current concentration, thereby enhancing the display effect of the display panel.
[0026] In some embodiments, the depth of the groove B is greater than or equal to the thickness of the conductive layer 40.
[0027] Specifically, the light-emitting functional layer 30 is formed using a vapor deposition process. After the light-emitting functional layer 30 is formed, the surface of the light-emitting functional layer 30 away from the substrate also has grooves. The conductive layer 40 extends along the sidewall of the groove to the bottom of the groove on one side of the groove B, and then extends upward along the sidewall of the groove. When the depth of the groove B is greater than or equal to the thickness of the conductive layer 40, the conductive layer 40 breaks as it extends upward along the sidewall of the groove, thus isolating the conductive layer 40 at the groove B. This completely breaks the local low-resistance conductive channel, further improving the "bright spot" phenomenon of the display panel and enhancing the display effect of the display panel.
[0028] Figure 3 This is a schematic diagram of another display panel structure provided in an embodiment of the present invention. Figure 3 As shown, groove B penetrates the first isolation layer 210.
[0029] Specifically, when the groove B penetrates the first isolation layer 210, the depth of the groove B is equal to the thickness of the first isolation layer 210, which maximizes the depth of the groove B and improves the reliability of the conductive layer 40 being isolated at the groove B.
[0030] Continue to refer to Figure 1 and Figure 3 The first isolation layer 210 includes a first isolation structure 211 and a second isolation structure 212. Along the direction X pointing from the isolation structure 20 to the opening area A, the first isolation structure 211 is disposed on one side of the groove B, and at least a portion of the first isolation structure 211 is located outside the opening area A. The second isolation structure 212 is disposed on the other side of the groove B and is located inside the opening area A. The width of the second isolation structure 212 is greater than or equal to a first preset value.
[0031] Specifically, the first preset value can be set according to the fluctuation error of the etching process. The first preset value can be greater than or equal to the fluctuation error of the etching process. The width of the second isolation structure 212 is greater than or equal to the first preset value. After etching the first isolation layer 210, the second isolation structure 212 is ensured to be present on the other side of the groove B. This ensures that the conductive layer 40 extends upward along the sidewall of the groove, ensuring that the conductive layer 40 is isolated at the groove B, thus improving the "bright spot" phenomenon of the display panel.
[0032] Continue to refer to Figure 1 and Figure 3 The orthographic projection of the first isolation structure 211 on the substrate overlaps with the orthographic projection of the light-emitting functional layer 30 on the substrate.
[0033] Specifically, the isolation structure 20 is an undercut structure. During the deposition of the light-emitting functional layer 30, the thickness uniformity of the light-emitting functional layer 30 located at the edge of the opening region A is relatively poor. At this time, the first isolation structure 211 isolates the light-emitting functional layer 30 with poor thickness uniformity from the electrode layer, preventing it from emitting light. Within the opening region A, the light-emitting functional layer 30 with uniform thickness emits light under the action of the driving current, which can improve the poor light emission of the light-emitting functional layer 30 and enhance the display effect of the display panel.
[0034] Continue to refer to Figure 1 and Figure 3 The display panel also includes a cathode layer 50 and a light extraction layer 60. The cathode layer 50 is disposed on the side of the conductive layer 40 away from the substrate, and the light extraction layer 60 is disposed between the conductive layer 40 and the cathode layer 50. The light extraction layer 60 is used to planarize the surface of the conductive layer 40.
[0035] Specifically, the cathode layer 50 can be made of a metal oxide, such as IZO. The cathode layer 50 can be a single, continuous film layer, enabling common cathode connections for different OLED devices. A light extraction layer 60 is disposed between the conductive layer 40 and the cathode layer 50 to adjust the microcavity effect of the OLED device and improve its light extraction efficiency. Simultaneously, the light extraction layer 60 can planarize the surface of the conductive layer 40. When the cathode layer 50 is formed on the side of the light extraction layer 60 away from the conductive layer 40, a flat surface can be provided for the cathode layer 50, preventing breakage and ensuring common cathode connections for different OLED devices. During the operation of the display panel, the cathode layer 50 has a low voltage, providing electrons to the conductive layer 40. The light-emitting functional layer 30 has an anode layer 70 on the side closest to the substrate. An electric field exists between the cathode layer 50 and the anode layer 70. After the resistance of the conductive layer 40 increases or is directly blocked at the groove B, electrons on the conductive layer 40 can be transferred to the light-emitting functional layer 30 under the influence of the electric field, causing the light-emitting functional layer 30 to emit light according to the driving current. The design improves the low-resistance conductive channel formed by electrons on the conductive layer 40 bypassing the light-emitting functional layer through the short-circuited semiconductor layer, thus reducing the "bright spot" phenomenon in the display panel. Simultaneously, the groove B is positioned on the side of the opening area A, ensuring the continuity of the conductive layer 40 in the middle region of opening area A. When the conductive layer 40 provides electrons to the light-emitting functional layer 30, the effectiveness of the electron supply from the conductive layer 40 is guaranteed, thereby ensuring the light-emitting effect of the light-emitting functional layer 30.
[0036] Continue to refer to Figure 1 and Figure 3 The isolation structure 20 also includes: The second isolation layer 220 is disposed on the side of the first isolation layer 210 away from the substrate, and the orthographic projection of the second isolation layer 220 on the substrate is located within the orthographic projection of the first isolation structure 211 on the substrate. The third isolation layer 230 is disposed on the side of the second isolation layer 220 away from the substrate. The orthographic projection of the second isolation layer 220 on the substrate is located within the orthographic projection of the third isolation layer 230 on the substrate. The orthographic projection of the third isolation layer 230 on the substrate is located within the orthographic projection of the first isolation layer 210 on the substrate.
[0037] Specifically, the orthographic projection of the second isolation layer 220 onto the substrate lies within the orthographic projection of the third isolation layer 230 onto the substrate, such that the third isolation structure 230 forms an "eave" on the side of the second isolation structure 220 away from the substrate. That is, the second isolation layer 220 and the third isolation layer 230 form an undercut structure to isolate the light-emitting functional layer 30 of different opening regions A. For example, the materials of the first isolation layer 210 and the third isolation layer 230 can be silicon oxide, and the material of the second isolation layer 220 can be silicon nitride.
[0038] In some embodiments, such as Figure 1 and Figure 3 As shown, the light-emitting functional layer 30 includes a first sub-light-emitting functional layer 310, a charge-generating layer 320 and a second sub-light-emitting functional layer 330 stacked sequentially; in the opening region A, the orthogonal projection of the second sub-light-emitting functional layer 330 on the substrate is located within the orthogonal projection of the charge-generating layer 320 on the substrate.
[0039] Specifically, the light-emitting functional layer 30 may include multiple sub-light-emitting functional layers, with adjacent sub-light-emitting functional layers connected in series through a charge generation layer. Each light-emitting functional layer may include a hole transport functional layer, a light-emitting layer, and an electron transport functional layer. For example, such as... Figure 1 and Figure 2 As shown, the light-emitting functional layer 30 includes two sub-light-emitting functional layers, namely a first sub-light-emitting functional layer 310 and a second sub-light-emitting functional layer 330, with a charge-generating layer 320 between them for connecting the first sub-light-emitting functional layer 310 and the second sub-light-emitting functional layer 330 in series. Figure 1 and Figure 3 In the diagram, the first sub-light-emitting functional layer 310 is exemplarily shown to include a hole transport layer 311 and a first light-emitting layer 312. The second sub-light-emitting functional layer 330 is exemplarily shown to include a second light-emitting layer 331. During the manufacturing process of the display panel, the conductive layer 40 is prone to short-circuiting with the charge-generating layer 320. In this case, the resistance of the conductive layer 40 is increased at the groove B or it is directly blocked. When the conductive layer 40 and the charge-generating layer 320 overlap at the edge, electrons on the conductive layer 40 cannot be transferred to the charge-generating layer 320 through the low-resistance conductive channel. This avoids electrons bypassing the second light-emitting layer 331 and conducting directly inside the charge-generating layer 320, improving the "bright spot" phenomenon caused by abnormal current concentration at the low-resistance conductive channel.
[0040] It should be noted that, in other embodiments, the light-emitting functional layer 30 may also include multiple stacked sub-light-emitting functional layers, with adjacent sub-light-emitting functional layers connected in series through the charge generation layer 320.
[0041] Continue to refer to Figure 1 and Figure 3 The display panel also includes an anode layer 70, which is disposed between the first isolation layer 210 and the substrate, with at least a portion of the anode layer 70 located within the opening region A.
[0042] Specifically, the anode layer 70 has a high voltage, and there is a voltage difference between the cathode layer 50 and the anode layer 70. When at least a portion of the anode layer 70 is located within the opening region A, the anode layer 70 and the cathode layer 50 provide a driving current to the light-emitting functional layer 30, driving the light-emitting functional layer 30 to emit light. The anode layer 70 is disposed between the first isolation layer 210 and the substrate. When the first isolation layer 210 has a groove B, the planarization of the anode layer 70 can be ensured. When the anode layer 70 provides holes for the light-emitting functional layer 30, the uniformity of the holes can be ensured, thereby ensuring the light-emitting performance of the light-emitting functional layer 30 and improving the display effect of the display panel.
[0043] This invention also provides a method for manufacturing a display panel, which is used to manufacture the display panel provided in any embodiment of this invention. Figure 4 This is a flowchart illustrating a method for manufacturing a display panel according to an embodiment of the present invention. Figure 4 As shown, the manufacturing method of this display panel includes: S110. An isolation structure is formed on one side of the substrate; the isolation structure has an opening region; the isolation structure includes a first isolation layer.
[0044] Specifically, Figure 5 This is a schematic diagram illustrating a display panel forming an isolation structure according to an embodiment of the present invention. Figure 5 As shown, on the substrate ( Figure 5 An isolation structure 20 is formed on one side of the OLED device (not shown). The isolation structure 20 has an opening region A for defining the position of the OLED device. The isolation structure 20 is an undercut structure. The isolation structure 20 includes a first isolation layer 210.
[0045] It should be noted that in the process of forming the isolation structure, the isolation structure film layer needs to undergo front-end process technologies such as HM (hard mask), AND (active ion etching), EB (edge processing of photoresist), PDO (polysilicon virtual pattern), and PDL (polysilicon virtual layer) to form the isolation structure 20.
[0046] S120. Pattern the first isolation layer to form grooves.
[0047] Specifically, Figure 6 This is a schematic diagram of a patterned first isolation layer provided in an embodiment of the present invention. Figure 6 As shown, after the first isolation layer 210 is patterned, a groove B is formed on the first isolation layer 210.
[0048] S130, A light-emitting functional layer is formed in the opening area.
[0049] Specifically, Figure 7 This is a schematic diagram illustrating the structure of a display panel forming a light-emitting functional layer, provided as an embodiment of the present invention. Figure 7 As shown, a light-emitting functional layer 30 is formed within the opening region A. The light-emitting functional layer 30 can be formed by a vapor deposition process. During the vapor deposition of the entire light-emitting functional layer 30, the light-emitting functional layer 30 also has a groove at the groove B, causing the groove to move upward, so that the surface of the light-emitting functional layer 30 also has a groove.
[0050] S140. A conductive layer is formed on the light-emitting functional layer; the orthogonal projection of the conductive layer on the substrate covers the orthogonal projection of the groove on the substrate.
[0051] Specifically, Figure 8 This is a schematic diagram illustrating the structure of a display panel forming a conductive layer, provided by an embodiment of the present invention. Figure 8 As shown, the conductive layer 40 is relatively thin. During the formation of the conductive layer 40 via vapor deposition, the resistance of the conductive layer 40 increases or it is directly blocked at the grooves. When the conductive layer 40 overlaps with the semiconductor layer in the light-emitting functional layer 30 at the edge, it avoids the formation of low-resistance metal-semiconductor ohmic contact points between the conductive layer 40 and the semiconductor layer in the light-emitting functional layer 30, thus preventing the establishment of localized low-resistance conductive channels. During the light emission process of the OLED device, when the driving current flows through the conductive layer 40, it can improve the phenomenon where the driving current bypasses part of the light-emitting functional layer and directly conducts into the semiconductor layer within the light-emitting functional layer after passing through the conductive layer 40. This improves the situation where localized low-resistance conductive channels overload and emit "bright spots" due to abnormal current concentration, thereby improving the display effect of the display panel.
[0052] The technical solution of this embodiment, by setting a groove on the first isolation layer, allows the orthogonal projection of the conductive layer on the substrate to cover the orthogonal projection of the groove on the substrate. This increases the resistance of the conductive layer at the groove or isolates it, preventing the formation of a low-resistance metal-semiconductor ohmic contact between the conductive layer and the semiconductor layer in the light-emitting functional layer. During the operation of the display panel, this improves the phenomenon where the driving current, after passing through the conductive layer, bypasses part of the light-emitting functional layer and directly conducts into the semiconductor layer within the light-emitting functional layer. It also improves the problem of local low-resistance conductive channels overloading and emitting "bright spots" due to abnormal current concentration, thus enhancing the display effect of the display panel.
[0053] In some embodiments, patterning the first insulating layer to form grooves includes: Photoresist is formed on the isolation structure; the photoresist exposes the groove location of the first isolation layer.
[0054] Specifically, Figure 9 This is a schematic diagram of an isolation structure with photoresist provided in an embodiment of the present invention. Figure 9As shown, photoresist 80 is formed on the isolation structure 20. The photoresist 80 exposes the position of the groove B to be formed on the first isolation layer 210. In the process of forming the photoresist 80, the entire layer of photoresist 80 can be coated first, and then the photoresist 80 can be exposed and developed to achieve patterning of the photoresist 80, so that the photoresist 80 exposes the position of the groove B on the first isolation layer 210.
[0055] The first isolation layer is etched to form a groove.
[0056] Specifically, Figure 10 This is a schematic diagram of an etching of the first isolation layer provided in an embodiment of the present invention. Figure 10 As shown, the first isolation layer 210 is etched to form a groove B.
[0057] Remove the photoresist.
[0058] For details, please refer to [link / reference]. Figure 6 After forming a groove B on the first isolation layer 210, the photoresist 80 is removed.
[0059] In some embodiments, the display panel further includes a light extraction layer 60 and a cathode layer 50. After the conductive layer 40 is formed, the light extraction layer 60 and the cathode layer 50 can be formed sequentially by a vapor deposition process. The light extraction layer 60 can planarize the surface of the conductive layer 40, preventing the cathode layer 50 from being interrupted at the groove B, thus realizing the common cathode connection of different OLED devices.
[0060] It should be noted that after forming the cathode layer 50, the display panel can be sequentially encapsulated, filled with OC (overlay) material (capsule filling), and processed with CF (color filter) material. When the display panel is a silicon-based microdisplay panel, a microlens array (MLA) process can also be performed.
[0061] This invention also provides a display device. Figure 11 This is a schematic diagram of a display device provided in an embodiment of the present invention. Figure 11 As shown, the display device 100 includes the display panel 101 provided in any embodiment of the present invention. Since the display device 100 includes the display panel 101 provided in any embodiment of the present invention, it has the same beneficial effects as the display panel 101 provided in any embodiment of the present invention, which will not be described again here.
[0062] It should be understood that the various forms of processes shown above can be used, with steps reordered, added, or deleted. For example, the steps described in this invention can be executed in parallel, sequentially, or in different orders, as long as the desired result of the technical solution of this invention can be achieved, and this is not limited herein.
[0063] The specific embodiments described above do not constitute a limitation on the scope of protection of this invention. Those skilled in the art should understand that various modifications, combinations, sub-combinations, and substitutions can be made according to design requirements and other factors. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this invention should be included within the scope of protection of this invention.
Claims
1. A display panel, characterized in that, include: Substrate; An isolation structure is disposed on one side of the substrate, the isolation structure having an opening area; the isolation structure includes a first isolation layer having a groove. A light-emitting functional layer is disposed within the opening area; A conductive layer is disposed on the side of the light-emitting functional layer away from the substrate; the orthogonal projection of the conductive layer on the substrate covers the orthogonal projection of the groove on the substrate.
2. The display panel according to claim 1, characterized in that, The depth of the groove is greater than or equal to the thickness of the conductive layer.
3. The display panel according to claim 2, characterized in that, The groove penetrates the first isolation layer.
4. The display panel according to claim 3, characterized in that, The first isolation layer includes a first isolation structure and a second isolation structure; along the direction from the isolation structure to the opening area, the first isolation structure is disposed on one side of the groove, and at least a portion of the first isolation structure is located outside the opening area; The second isolation structure is disposed on the other side of the groove and located within the opening area; The width of the second isolation structure is greater than or equal to the first preset value.
5. The display panel according to claim 4, characterized in that, The orthographic projection of the first isolation structure on the substrate overlaps with the orthographic projection of the light-emitting functional layer on the substrate.
6. The display panel according to claim 1, characterized in that, It also includes a cathode layer and a light extraction layer, wherein the cathode layer is disposed on the side of the conductive layer away from the substrate, and the light extraction layer is disposed between the conductive layer and the cathode layer, and the light extraction layer is used to planarize the surface of the conductive layer.
7. The display panel according to any one of claims 1-6, characterized in that, The isolation structure also includes: The second isolation layer is disposed on the side of the first isolation layer away from the substrate, and the orthographic projection of the second isolation layer on the substrate is located within the orthographic projection of the first isolation structure on the substrate; A third isolation layer is disposed on the side of the second isolation layer away from the substrate, wherein the orthographic projection of the second isolation layer on the substrate lies within the orthographic projection of the third isolation layer on the substrate, and the orthographic projection of the third isolation layer on the substrate lies within the orthographic projection of the first isolation layer on the substrate.
8. The display panel according to claim 1, characterized in that, The light-emitting functional layer includes a first sub-light-emitting functional layer, a charge-generating layer, and a second sub-light-emitting functional layer stacked sequentially; within the opening region, the orthogonal projection of the second sub-light-emitting functional layer on the substrate lies within the orthogonal projection of the charge-generating layer on the substrate.
9. The display panel according to claim 1, characterized in that, It also includes an anode layer disposed between the first isolation layer and the substrate, at least a portion of which is located within the opening region.
10. A method for manufacturing a display panel, characterized in that, include: An isolation structure is formed on one side of a substrate; the isolation structure has an opening region; the isolation structure includes a first isolation layer; The first isolation layer is patterned to form grooves; A light-emitting functional layer is formed within the opening area; A conductive layer is formed on the light-emitting functional layer; the orthogonal projection of the conductive layer on the substrate covers the orthogonal projection of the groove on the substrate.
11. The method for manufacturing a display panel according to claim 10, characterized in that, Patterning the first isolation layer to form grooves includes: A photoresist is formed on the isolation structure; the photoresist exposes the groove location of the first isolation layer; The first isolation layer is etched to form the groove; Remove the photoresist.
12. A display device, characterized in that, Includes the display panel as described in any one of claims 1-9.