LED glue proportioning rapid debugging method

By using tweezers to control the amount of adhesive and combining independent test cups with real-time observation, the problems of material waste, low efficiency, and unintuitive feedback in adhesive ratio adjustment in LED packaging technology are solved. This achieves low-cost and high-efficiency adhesive ratio adjustment, which is suitable for the rapid iteration of various LED products.

CN123165076APending Publication Date: 2026-11-24ANHUI COREACH TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611221123.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-12
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing LED packaging technologies suffer from problems such as significant material waste, low debugging efficiency, unintuitive feedback, and high operational barriers in adhesive mixing and adjustment, making it difficult to meet the needs of rapid iteration in R&D.

Method used

Using tweezers as a tool for controlling and transferring adhesive volume, the amount of adhesive can be precisely controlled by adjusting the opening and closing force, the clamping angle, and the residence time on the liquid surface. Combined with independent testing glue cups and real-time observation, adhesive can be directly applied and encapsulated, and the adhesive ratio can be judged in real time, eliminating the need for equipment cleaning and curing.

Benefits of technology

It achieves low-cost and efficient glue mixing and debugging, reduces material waste, improves debugging efficiency, lowers the operating threshold, and ensures the reliability of debugging results and real-time feedback.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_3
    Figure SMS_3
  • Figure SMS_4
    Figure SMS_4
Patent Text Reader

Abstract

This invention discloses a rapid adjustment method for LED adhesive mixing ratios, belonging to the field of LED packaging technology. Addressing the shortcomings of existing LED adhesive mixing adjustments that rely on dispensing machines, resulting in significant material waste, low efficiency, and unintuitive feedback, this method employs tweezers as the core tool for adhesive volume control and transfer. By adjusting the opening and closing force, gripping angle, and dwell time of the tweezers, the amount of adhesive transferred is precisely controlled. The adhesive to be tested is directly dispensed into a test cup, and an LED bead is placed to complete the initial encapsulation. The landing status of the LED bead and the adhesive spreading pattern are observed in real time, allowing for rapid assessment of the mixing ratio's rationality and iterative adjustments. This invention completely eliminates the cumbersome processes of machine dispensing, parameter calibration, and equipment cleaning. It requires no specialized equipment or complex operations and is suitable for rapid screening and optimization of adhesive mixing ratios during the LED packaging R&D stage. It boasts multiple advantages, including ease of operation, low cost, high efficiency, and reliable results.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of LED packaging technology, and specifically relates to a method for rapid adjustment of LED adhesive mixing ratio. Background Technology

[0002] In the field of LED packaging technology, encapsulating adhesives play a crucial role in protecting the chip, adjusting light color, improving light extraction efficiency, and ensuring structural reliability. The adhesive ratio directly determines the color temperature consistency, luminous efficacy, anti-aging performance, and lifespan of LED products. During product development and process optimization, multiple adhesive ratios need to be designed and verified one by one to select the optimal formula. The efficiency of ratio adjustment directly affects the new product development cycle and market response speed.

[0003] Currently, the mainstream debugging solution in the industry is the machine-programmed dispensing method, which relies on high-precision dispensing equipment to achieve quantitative dispensing. The specific process is as follows: after the operator prepares the adhesive to be tested, it is poured into the adhesive storage device of the dispensing machine, and parameters such as dispensing volume and dispensing position are set and calibrated. The machine is then started to complete the dispensing and LED bead mounting. After curing, the rationality of the mixing ratio is deduced through finished product testing. If the mixing ratio is not up to standard, the machine is stopped, the residual adhesive is drained, the equipment pipeline and needle are flushed, and then the next set of mixing ratios is used to repeat the process.

[0004] While this solution offers high precision in glue dosage control, it suffers from several significant drawbacks: First, it results in substantial material waste, requiring the entire equipment pipeline to be filled with glue in a single application, leading to an effective utilization rate of less than 5%. Furthermore, glue replacement and cleaning consume large amounts of glue and cleaning fluid, and the cost of debugging expensive fluorescent powders and special silicone materials is extremely high. Second, it suffers from low debugging efficiency, requiring over 30 minutes for a single batch of mixing, with the total time increasing linearly when screening multiple batches, resulting in slow R&D iterations. Third, it exhibits delayed feedback, requiring curing before test results can be obtained, making it impossible to observe glue spreading and LED bead adhesion in real time, hindering the rapid differentiation between glue dosage deviations and formulation defects, and leading to numerous ineffective iterations. Fourth, it has a high operational threshold, with expensive professional dispensing equipment and operators requiring extensive training, making it difficult for small and medium-sized R&D teams to afford.

[0005] Simple manual dispensing methods such as droppers and micropipettes suffer from poor dispensing accuracy, susceptibility to clogging by high-viscosity adhesives, and difficulty in cleaning, failing to meet the reliability requirements for debugging. Existing technologies are still limited by the technical bias that "proportioning and debugging must rely on high-precision equipment," making it difficult to balance accuracy, efficiency, and cost, and unable to adapt to the rapid iteration and R&D needs of current LED products. Summary of the Invention

[0006] One of the objectives of this invention is to provide a rapid adjustment method for LED adhesive mixing ratios, in order to solve the problems of serious material waste, low adjustment efficiency, and unintuitive feedback in existing technologies.

[0007] The objective of this invention can be achieved through the following technical solutions: A method for rapid adjustment of LED adhesive mixing ratio includes the following steps: S1 Adhesive Preparation: Determine at least one set of adhesive ratios to be tested according to the LED packaging performance requirements. Weigh the LED packaging adhesive raw materials according to the ratio, mix them evenly to obtain the adhesive to be tested, and then package and label them for later use. S2 Adhesive Transfer: Tweezers are used as the adhesive volume control and transfer tool to pick up the adhesive to be tested. The amount of adhesive transferred in a single transaction is controlled by adjusting the opening and closing force of the tweezers, the gripping angle, and the residence time on the liquid surface. S3 dispensing encapsulation: The adhesive to be tested is dispensed into the preset position of the test cup using tweezers. Then, the LED bead is placed into the test cup and pressure is applied to ensure that the bottom of the bead is in full contact with the adhesive, thus completing the initial encapsulation. S4 Real-time Judgment and Iteration: After initial encapsulation, observe the LED bead landing status and adhesive spreading status in real time to determine whether the current adhesive ratio meets the preset requirements; if it does not meet the requirements, directly replace the test glue cup and the adhesive to be tested, and repeat steps S2~S3 to adjust the next set of ratios until the optimal adhesive ratio that meets the performance requirements is obtained.

[0008] To address the issue of forced overfilling of adhesive by the machine, a dedicated adhesive preparation procedure is implemented. Adhesive is precisely prepared and labeled according to actual testing requirements, eliminating the need for pre-filled equipment and preventing unnecessary material loss at the preparation stage. To address the issues of pipe residue and cumbersome cleaning, tweezers are used as the core tool for adhesive transfer. The surface tension of the adhesive allows it to adhere to the tweezers' heads, and the amount transferred can be flexibly controlled by adjusting the opening and closing force, gripping angle, and liquid surface dwell time. Adhesive deviation can be stably maintained within ±15%. The tweezers' small contact area results in minimal residue, and cleaning is unnecessary when changing the mixing ratio, completely eliminating the need for pipe cleaning. To address the issue of insufficient reference value in debugging results, an independent test adhesive cup is used to simulate the actual packaging cavity boundary. Centered adhesive application is limited, and LED beads are pressed and bonded together, ensuring that the adhesive spreading and bonding state is consistent with mass production packaging, guaranteeing that the debugging results have mass production guidance value. To address the issue of delayed feedback, a real-time observation and judgment process is implemented. After dispensing and application, the application point, spread, and bonding status can be intuitively assessed. If the application is unsatisfactory, the glue cup and glue can be replaced and the process repeated without waiting for curing or equipment reset. This enables seamless iteration of the mixing ratio and establishes a low-consumption, high-efficiency, and intuitive rapid debugging technical solution.

[0009] Furthermore, in step S1, the raw materials of the LED encapsulation adhesive include a silicone substrate, phosphor, and curing agent; the mixing ratio of the adhesive to be tested includes the mass ratio of phosphor to silicone substrate and the mass addition ratio of curing agent relative to silicone substrate.

[0010] Furthermore, in step S1, the specific method for achieving uniform mixing is as follows: first, the phosphor and silicone substrate are stirred at room temperature at a speed of 200~500 rpm for 3~10 minutes, then the curing agent is added and stirring is continued for 2~5 minutes. Subsequently, degassing is performed under a vacuum of -0.08~-0.1 MPa for 1~3 minutes to obtain a test adhesive without bubbles, particle sedimentation, or stratification. By controlling the powder dispersion effect through stepwise stirring parameters, and combining this with vacuum degassing to eliminate internal bubbles, the interference of preparation process deviations on the performance judgment of the formulation is eliminated, ensuring the consistency of preparation of each group of test samples, and allowing the debugging results to truly reflect the performance differences of the formulation itself.

[0011] Furthermore, in step S2, the tweezers are stainless steel medical tweezers or laboratory precision tweezers with smooth, polished tips, and the width of the tweezer tips is 0.8~2.5mm; the amount of adhesive transferred in a single transaction is 0.01~0.05g, and the relative deviation of the adhesive amount is controlled within ±15%. By limiting the material of the tweezers, the tip width, and the range of adhesive amounts, and by reducing adhesive residue on the walls through smooth polishing, the head size is matched with the amount of adhesive per cup test, stabilizing the adhesive amount deviation within an acceptable range for R&D screening, thus balancing adhesive control stability and ease of operation.

[0012] Furthermore, in step S2, when picking up the adhesive to be tested, the opening angle of the tweezers is 15°~45°, and the depth of insertion of the tweezers into the adhesive surface is 0.5~2mm. After picking up the adhesive, the tweezers are raised above the adhesive surface and held for 0.5~2 seconds to allow excess adhesive to drip off naturally before transferring it. Based on the positive correlation between liquid adhesion amount and contact area and dwell time, by limiting the opening angle and insertion depth to control the adhesive contact area, and by allowing excess adhesive to drip off naturally at the liquid surface, reproducible standardized operating parameters are formed, reducing operational differences among different operators and improving test consistency.

[0013] Furthermore, in step S3, the test cup has a circular, flat-bottomed structure with an inner diameter of 2-5 mm and a depth of 1-2.5 mm, and its inner wall has a smooth, hydrophobic surface. The dispensing position is at the center of the bottom surface of the test cup, and the deviation of the dispensing position does not exceed 0.5 mm. Based on the principle of the influence of boundary constraints on the adhesive spreading pattern, the size, structure, and surface characteristics of the test cup are limited to ensure that they are highly matched with the boundary conditions of the actual packaging cavity. This ensures that the adhesive spreading and bonding effect under test conditions is consistent with mass production packaging, and ensures that the debugging results have mass production guidance value.

[0014] Furthermore, in step S3, the pressure applied to the LED bead is 0.1~0.5N. After pressing, the adhesive completely covers the chip and pad area at the bottom of the bead, and the distance between the edge of the adhesive spread and the edge of the bead is 0.1~0.3mm. Limiting the pressing pressure and spreading boundary requirements simulates the pressure conditions of mass production mounting, ensuring that the chip area at the bottom of the bead is completely covered by adhesive, while avoiding adhesive overflow or insufficient adhesive, thus improving the reliability of the debugging results.

[0015] Furthermore, in step S4, the real-time observation includes: whether the LED bead landing point is centered, whether the glue spreads evenly, whether there is glue overflow or insufficient glue, whether the LED bead tilt angle is ≤2°, and whether there are air bubbles inside the glue. By clearly defining the core dimensions of real-time observation, intuitive indicators such as landing point, spread, glue overflow / insufficiency, tilt, and air bubbles are used as rapid screening criteria. This allows for the quick elimination of obviously unqualified formulations without the need for professional testing equipment, thus improving the efficiency of initial screening.

[0016] Furthermore, step S4 also includes a preliminary light emission detection step: connecting the pre-packaged LED beads to the rated operating current, observing the uniformity of the light emission color temperature and the shape of the light spot in real time, to help determine the rationality of the glue ratio.

[0017] Furthermore, in step S4, if the current glue ratio is determined to be unacceptable, the current test glue cup and glue are discarded directly without cleaning the tweezers. The next set of glue to be tested can then be used to begin a new round of debugging. This completely eliminates the cleaning step, maximizes the compression of iteration intervals, and further enhances the advantages of rapid debugging.

[0018] The beneficial effects of this invention are: (1) The present invention determines the ratio of the adhesive to be tested according to the performance requirements, weighs the raw materials according to the ratio, mixes them evenly, and then packages and marks them. There is no need to prepare a large amount of adhesive for filling equipment pipelines. The amount of adhesive transferred at one time is precisely controlled by adjusting the opening and closing force of the tweezers, the clamping angle and the liquid surface dwell time. The adhesive only acts on the actual test sample. Then the adhesive is directly applied to the independent test cup to complete the encapsulation. When the ratio is not qualified, the current test cup and adhesive are directly discarded. The design of iterative without cleaning the equipment completely avoids the large amount of adhesive residue in the storage tank, pipeline and needle in the traditional machine solution, and also eliminates the loss of cleaning fluid and flushing adhesive during the adhesive change process.

[0019] (2) The present invention eliminates the redundant steps of traditional machine debugging: Step S2 uses tweezers to directly control and transfer the amount of glue, replacing the tedious preparation steps such as glue pouring, parameter calibration, and glue dispensing debugging; Step S3 only requires applying glue to the preset position of the test glue cup, placing the LED beads and applying pressure to press, which can complete the initial encapsulation without equipment positioning and program operation; When it is determined in Step S4 that the ratio does not meet the requirements, the test glue cup and the glue to be tested can be directly replaced, and Steps S2~S3 can be repeated to carry out a new round of debugging without performing equipment emptying, cleaning, resetting parameters and other reset processes.

[0020] (3) After the initial encapsulation is completed in step S3, the present invention can observe the landing status of the LED beads and the spreading status of the adhesive in real time, directly identify problems such as landing point deviation, excess adhesive, insufficient adhesive, and residual air bubbles, and can also quickly evaluate the light color performance by combining with the initial light emission test, and can judge the rationality of the current adhesive ratio without waiting for the curing to be completed. This technical feature can help the debugging personnel quickly distinguish between "adhesive quantity operation deviation" and "formula performance defects", eliminate obviously unqualified ratios in advance, and avoid ineffective curing and finished product testing processes.

[0021] (4) This invention only requires an independent test glue cup to complete the entire debugging process, eliminating the need to purchase expensive high-precision dispensing equipment, resulting in low total hardware investment. Furthermore, the entire method consists of only four steps: glue preparation, tweezers for volume control, glue cup dispensing and pressing, and real-time observation and iteration. Operators can complete the operation independently after a simple 10-minute training session, without needing to master complex equipment programming, parameter calibration, and pipeline maintenance skills. This method is suitable for rapid pre-screening of formulations in the R&D stage of large enterprises, as well as for basic research in small and medium-sized R&D teams and university laboratories. It is also compatible with various product specifications, requiring only the replacement of tweezers and test glue cups of the corresponding specifications for adaptation, making its application scenarios extremely wide. Detailed Implementation

[0022] The specific embodiments of the present invention will be described in detail below, but it should be understood that the scope of protection of the present invention is not limited to the specific embodiments.

[0023] The basic raw materials and tools used in the following examples are described below: Methyl silica gel substrate: refractive index 1.54, viscosity 5000 mPa at 25°C. s, vinyl content 0.8%; Phenyl silica gel substrate: refractive index 1.58, viscosity 8000 mPa at 25℃ s; YAG yellow phosphor: aluminate system, central particle size 15μm, excitation wavelength 450nm; Nitride red phosphor: central particle size 12μm, emission wavelength 620nm; Platinum-based curing agent: platinum content 5000ppm, addition reaction type; Diffusion powder: Organosilicon microspheres, particle size 2μm; Test cup: PC material, round flat bottom structure, smooth inner wall, regular model inner diameter 3.0mm, depth 1.5mm, Mini model inner diameter 1.5mm, depth 0.8mm; Tweezers: 304 stainless steel medical straight-tipped tweezers with polished tips. The standard model has a head width of 1.2mm, while the precision model has a head width of 0.8mm. LED chips: 2835 type blue light chip (10mil×23mil, rated current 30mA), 3535 type blue light chip, 0402 type Mini LED chip.

[0024] Example 1 This embodiment focuses on the rapid adjustment of the encapsulation adhesive ratio for general lighting white LEDs with a color temperature of 4000K. The specific steps are as follows: S1 glue preparation Based on the target performance requirements, the designed test ratio is: YAG phosphor to methyl silicone substrate in a mass ratio of 1:4, and the amount of curing agent added is 0.6% of the mass of silicone substrate.

[0025] Accurately weigh 0.2g of YAG phosphor and 0.8g of methyl silica gel according to the mixing ratio, and add them to a 5mL polypropylene centrifuge tube. Fix the centrifuge tube on a micro magnetic stirrer and stir at 300rpm for 5 minutes at room temperature to ensure that the phosphor is fully dispersed in the silica gel. Then add 4.8mg of platinum-based curing agent, reduce the speed to 200rpm and continue stirring for 3 minutes to ensure that the curing agent is mixed evenly. After stirring, place the centrifuge tube in a vacuum degassing device and degas for 2 minutes under a pressure of -0.09MPa to remove air bubbles from the glue and obtain a uniform, particle-free glue for testing. Seal and label it as sample #1 for later use.

[0026] S2 Adhesive Transfer Take the #1 glue to be tested. Hold a standard straight-tipped tweezers with the tip facing down, controlling the opening angle to approximately 30°. Gently insert the tweezers tip about 1mm below the glue surface. Slowly close the tweezers, controlling the gripping force to approximately 4N, allowing the glue to naturally adhere to the tweezers tip. After gripping, vertically lift the tweezers above the glue surface, hold for 1 second, and allow excess glue to drip off naturally. Weighing verification shows that the amount of glue held by the tweezers at this point is approximately 0.025g, with a glue quantity deviation of approximately ±10%.

[0027] S3 dispensing and encapsulation Move the tweezers holding the glue directly above the standard test glue cup, aligning them with the center of the bottom surface of the cup. Slowly open the tweezers to allow the glue to drip naturally into the center of the cup, ensuring the glue application position deviation is less than 0.2mm. After dispensing, use a vacuum pen to pick up the 2835 LED bead and place it steadily into the test glue cup. Apply approximately 0.2N of pressure and gently press the top of the bead to spread the glue evenly outwards under pressure. Finally, the glue completely covers the chip area at the bottom of the bead, with the edge of the spread approximately 0.2mm from the edge of the bead, without any overflow. This completes the initial encapsulation.

[0028] S4 Real-time Judgment and Verification After initial encapsulation, observation under a 10x stereomicroscope revealed that the LED beads were centered with an offset of less than 0.2mm; the adhesive was evenly spread with no visible air bubbles; and the LED beads were not tilted with an angle of less than 1°. A preliminary light emission test was then conducted with a rated current of 30mA. The observed light spot was round and uniform with no obvious color shift, and the visual color temperature was approximately 4000K. Preliminary assessment indicates that the formulation meets the design requirements.

[0029] To verify the final performance, five parallel samples were prepared using the same procedure and placed in an electric heating oven for curing at 120°C for 2 hours. After curing, the optical performance was tested using an integrating sphere and the bonding strength was tested using a push-pull force tester. The results were as follows: color temperature 4050K, color rendering index Ra=82, luminous efficacy 128lm / W, and average push-pull force of the LED beads 8.2N. These results fully meet the performance requirements of general lighting LEDs, and the formulation was determined to be a qualified solution.

[0030] In this embodiment, the complete debugging cycle for a single batch of formulations is approximately 6 minutes, the total glue consumption is approximately 0.5g, and there is no cleaning fluid consumption.

[0031] Example 2 This embodiment focuses on the adjustment and optimization of adhesive ratio for white LEDs used in backlighting with a color temperature of 5000K. The specific steps are as follows: S1 glue preparation The initial test formulation was designed as follows: YAG phosphor to methyl silicone mass ratio 1:3.5, curing agent addition 0.5%, and diffusing powder addition 0.3% of silicone mass. 0.2g phosphor, 0.7g silicone, and 2.1mg diffusing powder were weighed according to the formulation and added to a centrifuge tube. The mixture was stirred at 350rpm for 6 minutes, followed by the addition of the curing agent and continued stirring for 2 minutes. Vacuum degassing was then performed for 2 minutes to obtain adhesive #2 for testing.

[0032] S2 Adhesive Transfer Using standard tweezers, control the opening and closing angle to approximately 25°, the gripping force to approximately 3.5N, hold for 0.8 seconds after gripping, and control the amount of adhesive transferred in a single transaction to approximately 0.02g.

[0033] S3 dispensing and encapsulation Apply glue to the center of the test cup, place a 2835 LED bead inside, apply 0.15N pressure, and press to complete the initial encapsulation.

[0034] S4 Real-time Judgment and Iteration Microscopic observation revealed that the glue spread quickly, with slight overflow at the edge of the glue cup, the overflow width being approximately 0.1 mm; preliminary lighting tests showed that the light spot was uniform, but the color temperature was too high, visually approximately 5200K.

[0035] Overall assessment: The low phosphor content in this formulation leads to a high color temperature, and the slightly high fluidity of the adhesive causes overflow. The formulation needs adjustment. Discard the current test cup; do not clean the tweezers. Immediately use freshly prepared #3 adhesive (phosphor:silicone = 1:3.2, curing agent 0.6%, diffusing powder 0.3%) and repeat steps S2-S3 for adjustment.

[0036] After adjustments and observation: the adhesive showed no overflow, spread evenly, and the LED beads were centered; the initial lighting color temperature was approximately 5000K, meeting the target requirements. After curing, comprehensive testing results showed: color temperature 5020K, Ra=84, luminous efficacy 125lm / W, and push-pull force 7.9N, meeting performance standards.

[0037] In this embodiment, the total time for completing the two sets of formulation adjustments and iterations was approximately 11 minutes, and the cumulative glue consumption was approximately 0.9g, achieving rapid optimization of the formulation.

[0038] Example 3 This embodiment targets high color rendering warm white LEDs and uses a high refractive index phenyl silicone system for formulation and adjustment. The specific steps are as follows: S1 glue preparation The designed formulation is as follows: YAG yellow powder and nitride red powder are mixed at a mass ratio of 4:1 to form a mixed phosphor. The mass ratio of the mixed phosphor to the phenyl silicone substrate is 1:4.5, and the amount of curing agent added is 0.7%. Weigh 0.16g of yellow powder, 0.04g of red powder, and 0.9g of phenyl silicone according to the formulation and add them to a centrifuge tube. Stir at 400rpm for 8min to ensure that the two phosphors are evenly dispersed. After adding the curing agent, continue stirring for 3min. Degas under vacuum at -0.095MPa for 3min to obtain the No. 4 adhesive to be tested.

[0039] S2 Adhesive Transfer Because phenyl silicone has a higher viscosity, use curved tweezers with a head width of 1.8mm, control the opening and closing angle to about 20°, the gripping force to about 5N, hold for 1.5s after gripping, and control the amount of adhesive transferred in a single transaction to about 0.03g.

[0040] S3 dispensing and encapsulation Apply glue to the center of a test glue cup with an inner diameter of 4mm, place a 3535 LED bead inside, and apply 0.3N of pressure to press it down so that the glue completely covers the bottom of the LED bead.

[0041] S4 Real-time Judgment and Verification Observations revealed that the adhesive was spread evenly, without bubbles or excess, and the LED beads were centered. Upon initial illumination, the light was soft, appearing as a warm white, with no obvious color patches. After curing, the test results were: color temperature 3020K, color rendering index Ra=90, R9=85, luminous efficacy 118lm / W, and push-pull force 9.1N, meeting the performance requirements for high color rendering lighting products.

[0042] Example 4 This embodiment focuses on the 0402 type Mini LED product, demonstrating rapid adjustment of the adhesive ratio for the micro LED beads. The specific steps are as follows: S1 glue preparation The designed formulation is as follows: the mass ratio of nano-sized YAG fluorescent powder to methyl silicone is 1:5, and the amount of curing agent added is 0.5%. Nano-fluorescent powder with a particle size of 2μm is used. The mixture is stirred at 250rpm for 10min to ensure that the fluorescent powder is fully dispersed. Vacuum degassing is performed for 1.5min to obtain the No. 5 adhesive to be tested.

[0043] S2 Adhesive Transfer Precision micro-tweezers with a head width of 0.8mm were used, with the opening and closing angle controlled at about 15°, the gripping force at about 2N, and the gripping time held for 0.5s. The amount of adhesive transferred in a single transaction was controlled at about 0.01g.

[0044] S3 dispensing and encapsulation Apply glue to the center of the Mini test glue cup with an inner diameter of 1.5mm, ensuring the glue application position deviation is less than 0.1mm; place the 0402 Mini LED bead inside, apply 0.1N of pressure and press gently to complete the initial encapsulation.

[0045] S4 Real-time Judgment and Verification Under a 50x metallographic microscope, the LED bead placement deviation was less than 0.1mm, the adhesive was spread evenly without excess adhesive or bubbles, and the LED bead tilt angle was less than 1.5°. After initial lighting, the light emission was uniform with no obvious color shift. After curing, the color temperature was measured at 4500K, and the color temperature deviation among samples in the same group was less than 3nm, meeting the consistency requirements for Mini LED packaging.

[0046] Example 5 This embodiment performs rapid batch screening of multiple formulations, quickly comparing six groups of adhesives with different proportions of phosphor to select the optimal formulation for a target color temperature of 4500K. The specific steps are as follows: S1 Batch Adhesive Preparation Six sets of test formulations were designed sequentially, with the mass ratios of fluorescent powder to methyl silicone being 1:6, 1:5, 1:4.5, 1:4, 1:3.5, and 1:3, respectively, and the amount of curing agent added being 0.6% for each set. 1g of adhesive was prepared for each set and labeled as 6-1# to 6-6#, and all were mixed and degassed before use.

[0047] S2~S3 Batch dispensing and encapsulation The dispensing operation was performed sequentially according to the numbering, with two parallel test samples prepared for each group. The operating parameters were uniform: tweezers opening angle 30°, gripping force 4N, dwell time 1s, and dispensing amount of approximately 0.025g per dot. The dispensing and encapsulation operation for a single group took approximately 3 minutes.

[0048] S4 Batch Filtering and Verification After the initial encapsulation of the six samples was completed, real-time status observation and preliminary luminescence testing were performed sequentially: 6-1# (1:6) and 6-2# (1:5): The color temperature is significantly too high, exceeding 5500K, and the phosphor content is insufficient, so they are directly eliminated. 6-5# (1:3.5) and 6-6# (1:3): Both exhibit varying degrees of glue overflow and have low color temperatures, below 4000K, and are therefore rejected. 6-3# (1:4.5) and 6-4# (1:4): The spreading condition is good, and the color temperature is about 4800K and 4300K ​​respectively, which is close to the target range. They will proceed to the next round of verification.

[0049] For the two candidate ratios, the phosphor ratio was further fine-tuned to 1:4.2. Validation samples were prepared and cured for testing. The final measured color temperature was 4520K, Ra=83, and luminous efficacy was 127lm / W, which was determined to be the optimal ratio.

[0050] In this embodiment, the preliminary screening of the 6 formulations takes about 32 minutes in total, with a total glue consumption of about 6.2g and no cleaning fluid consumption. Compared with the traditional machine solution, the efficiency is increased by more than 80% and the material consumption is reduced by more than 95%.

[0051] Comparative Example 1 This comparative example demonstrates the programmed dispensing debugging of existing technology equipment. A mainstream pneumatic high-precision dispensing machine was used for mixing and debugging. Tests were conducted according to standard procedures for six sets of adhesive ratios identical to those in Example 5. Prepare 25g of 6-1# adhesive and pour it into the dispensing machine's storage tank. Connect the tubing to the dispensing needle. Set the target dispensing amount to 0.025g / point, adjust the air pressure and dispensing time parameters, and calibrate the accuracy by weighing 10 consecutive points until the dispensing amount deviation is ≤±5%. The calibration process takes 12 minutes. Two test samples were prepared by formal dispensing, and after placing the LED beads, they were placed in an oven at 120℃ for 2 hours to cure. After curing, optical performance testing is performed to determine if the mixing ratio is unqualified, which takes about 15 minutes. After stopping the machine and emptying the residual glue in the glue tank, pour in anhydrous ethanol to rinse the glue tank, tubing and needle three times. After drying, it is ready for use. The cleaning process takes 10 minutes. Replace with 6-2# adhesive and repeat the above process of filling, calibrating, dispensing, curing, testing, and cleaning until all 6 sets of mixing tests are completed.

[0052] According to statistics, the average debugging time for a single group of this comparative sample was about 33 minutes, and the total debugging time for 6 groups was about 198 minutes; the cumulative consumption of glue was about 152g and anhydrous ethanol was about 82g; the debugging process required certified professional operators to complete, and the purchase cost of the dispensing equipment was about 85,000 yuan.

[0053] Comparative Example 2 This comparative example demonstrates manual dispensing calibration using a micropipette. A 100μL micropipette was used for manual dispensing calibration, and tests were conducted using the same mixing ratio as in Example 1. Prepare the same adhesive as in Example 1; The pipette was set to a volume of 25 μL, and the adhesive was drawn up and dispensed into the test cup. Due to the high viscosity of the adhesive, the pipette piston did not push smoothly, resulting in severe adhesive residue on the pipette wall. The actual dispensing volume deviated by more than ±30%, with some samples showing excessive adhesive overflow and others showing insufficient adhesive. After inserting the LED beads, the sample consistency was poor, making it impossible to accurately determine the formula performance. When changing the mixing ratio, the pipette tip must be rinsed repeatedly with anhydrous ethanol more than 5 times to avoid cross-contamination. Each set of cleaning takes about 5 minutes.

[0054] According to statistics, the debugging time for a single set of this comparative example was about 15 minutes. The glue volume control accuracy was poor and the debugging results were unreliable. In addition, the gun head was difficult to clean, and a total of about 18.5g of glue and about 15g of cleaning fluid were consumed, and the problem of material waste was still prominent.

[0055] Comparative Example 3 This comparative example is a tweezers dispensing test without real-time observation. It uses the exact same tweezers dispensing operation as the present invention, but omits the real-time observation and preliminary judgment steps. All samples were cured uniformly after dispensing before testing. Tests were conducted on the six formulations of Example 5: Following the operating parameters of Example 5, dispensing and encapsulation of 12 samples in 6 groups were completed without any status observation or initial lighting. Place all samples in an oven and cure at 120℃ for 2 hours; After curing, performance tests were conducted on each sample. It was found that three groups of samples had problems with glue overflow or insufficient glue, which was caused by deviation in the amount of glue applied. This could not reflect the true performance of the formula and needed to be re-formulated and retested. The adhesive for the substandard groups was re-formulated and tested repeatedly until all screenings were completed.

[0056] According to statistics, the total debugging time for this comparison model was approximately 180 minutes, with a significant amount of time spent on curing and retesting, and invalid tests accounting for 50% of the time. The total glue consumption was approximately 10.8g, resulting in a substantial decrease in debugging efficiency and first-time success rate.

[0057] Performance testing To comprehensively verify the technical effectiveness of this invention in different application scenarios, systematic comparative tests were conducted on all five sets of examples and three sets of comparative examples for two typical scenarios in LED packaging R&D: single-group ratio verification and optimization, and multi-group ratio batch screening. All tests were carried out in a clean environment at room temperature of 25°C and relative humidity of 50%, by the same operator, and the adhesive raw material system, LED chip specifications, and performance evaluation standards were kept consistent to ensure the objectivity and comparability of the comparison results.

[0058] 1. Performance comparison in single-group ratio adjustment scenarios This scenario corresponds to the routine needs of single-formula verification and small-scale parameter optimization in the R&D stage, covering various sub-conditions such as conventional LED beads, high-viscosity adhesives, and micro LED beads. The test results are shown in Table 1.

[0059] Table 1. Comparison of overall performance in single-group ratio adjustment scenarios

[0060] 2. Performance comparison in batch screening scenarios with multiple proportions This scenario addresses the core needs of parallel screening of multiple formulations and optimization of a wide range of parameters during the R&D phase. Six groups of adhesives with different proportions of phosphors were used as test objects to verify the overall efficiency and cost performance under batch debugging. The test results are shown in Table 2.

[0061] Table 2. Comparison of overall performance in batch screening scenarios with 6 different proportions.

[0062] In single-group debugging scenarios, the debugging time for each group in Examples 1 to 4 is only 5.3 to 7 minutes, which is about 1 / 5 to 1 / 4 of the machine solution in Comparative Example 1 and about 1 / 3 to 1 / 2 of the pipette solution in Comparative Example 2. Even in more challenging scenarios such as high-viscosity phenyl silica gel and small-volume Mini LED adhesive, the debugging time of the present invention does not show a significant increase, demonstrating strong scenario adaptability.

[0063] In batch screening scenarios, the total debugging time for the 6 formulations in Example 5 was only 32 minutes, which is only 16.2% of the time required for the machine solution in Comparative Example 1, and 82.2% shorter than that of Comparative Example 3. The efficiency improvement comes from two aspects: First, non-core steps such as machine gluing, parameter calibration, and equipment cleaning are completely eliminated, and the pure operation time accounts for nearly 100%; second, the real-time observation mechanism can eliminate obviously unqualified formulations in advance, avoiding ineffective curing waiting and finished product testing, and greatly reducing redundant workload.

[0064] In terms of material costs, this invention demonstrates advantages in all scenarios: In single-group debugging scenarios, the single-group glue consumption of Examples 1-4 is only 0.3-0.7g, which is only 1.2%-2.8% of the machine solution in Comparative Example 1, and there is no consumption of cleaning fluid throughout the process; In batch screening scenarios, the total glue consumption of Example 5 is only 4.1% of that in Comparative Example 1, while saving 82g of cleaning fluid. Material waste in existing technologies mainly comes from two parts: first, glue residue inside the machine's glue storage tank, pipelines, and needles cannot be recycled, resulting in an effective utilization rate of less than 5% for a single glue filling; second, repeated rinsing during mixing ratio changes consumes a large amount of cleaning fluid and flushing glue. In the testing mode of this invention, the glue is only used for the actual test sample, leaving no equipment residue, and no cleaning is required when changing samples, eliminating ineffective material loss at the source. The cost-saving value is particularly significant for high-priced raw materials such as rare earth phosphors and high-refractive-index special silicone.

[0065] Regarding the accuracy of adhesive volume control, the relative deviation of adhesive volume in this invention is stable at ±10%~±15%. Although the absolute value is slightly lower than ±3%~±5% of high-precision dispensing machines, it is far superior to ±30% of the pipette solution, and it can fully meet the qualitative screening of formulations in the R&D stage. Small deviations in adhesive volume will not affect the qualitative judgment of the formulation's quality. Thanks to the real-time observation and preliminary luminescence verification mechanism, the first-time success rate of this invention is significantly higher than that of existing technologies: in single-group scenarios, Examples 1 to 4 all achieved the target in one go or in one iteration; in batch scenarios, the first-time success rate reached 83.3%, higher than the 66.7% of the machine solution in Comparative Example 1, and far higher than the 50% of Comparative Example 3. Traditional solutions can only detect operational problems such as adhesive overflow, insufficient adhesive, and misaligned placement after curing, which can easily lead to invalid tests; while this invention can identify operational deviations immediately after dispensing, greatly reducing invalid iterations, and the actual debugging reliability is better.

[0066] This invention is stably applicable to all scenarios, including conventional 2835 LEDs, high-power 3535 LEDs, miniature 0402 Mini LEDs, and high-viscosity phenyl silicone. Only the tweezers and test cups of the corresponding specifications need to be replaced; no additional parameter adjustments are required. In contrast, traditional instrument solutions require recalibrating the dispensing path and parameters when changing LED specifications, and pipette solutions may experience clogging and adhesion issues in high-viscosity, low-volume scenarios, significantly limiting their applicability.

[0067] In terms of cost and barriers to entry, the core tools of this invention are only ordinary tweezers and disposable test cups, resulting in low total equipment investment. Operators can operate independently after a simple 10-minute training session without needing to master complex equipment programming and maintenance skills. This significantly reduces the equipment and human resource barriers for LED adhesive formulation development, making it suitable for rapid pre-screening in large enterprises as well as for basic research by small and medium-sized R&D teams and university laboratories.

[0068] The above-disclosed embodiments are merely a few specific examples of the present invention. However, the embodiments of the present invention are not limited thereto, and any variations that can be conceived by those skilled in the art should fall within the protection scope of the present invention.

Claims

1. A method for rapid adjustment of LED adhesive mixing ratio, characterized in that, Includes the following steps: S1 Adhesive Preparation: Determine at least one set of adhesive ratios to be tested according to the LED packaging performance requirements. Weigh the LED packaging adhesive raw materials according to the ratio, mix them evenly to obtain the adhesive to be tested, and then package and label them for later use. S2 Adhesive Transfer: Tweezers are used as the adhesive volume control and transfer tool to pick up the adhesive to be tested. The amount of adhesive transferred in a single transaction is controlled by adjusting the opening and closing force of the tweezers, the gripping angle, and the residence time on the liquid surface. S3 dispensing encapsulation: The adhesive to be tested is dispensed into the preset position of the test cup using tweezers. Then, the LED bead is placed into the test cup and pressure is applied to ensure that the bottom of the bead is in full contact with the adhesive, thus completing the initial encapsulation. S4 Real-time Judgment and Iteration: After initial encapsulation, observe the LED bead landing status and adhesive spreading status in real time to determine whether the current adhesive ratio meets the preset requirements; if it does not meet the requirements, directly replace the test glue cup and the adhesive to be tested, and repeat steps S2~S3 to adjust the next set of ratios until the optimal adhesive ratio that meets the performance requirements is obtained.

2. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, In step S1, the raw materials of the LED encapsulation adhesive include a silicone substrate, phosphor, and curing agent; the mixing ratio of the adhesive to be tested includes the mass ratio of phosphor to silicone substrate and the mass addition ratio of curing agent relative to silicone substrate.

3. The method for rapid adjustment of LED adhesive mixing ratio according to claim 2, characterized in that, In step S1, the specific method for uniform mixing is as follows: First, the fluorescent powder and the silicone substrate are stirred at room temperature at a speed of 200~500 rpm for 3~10 minutes, then the curing agent is added and stirring is continued for 2~5 minutes. Subsequently, the adhesive is degassed under vacuum conditions of -0.08~-0.1MPa for 1~3 minutes to obtain a test adhesive without bubbles, particle sedimentation, or stratification.

4. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, In step S2, the tweezers are stainless steel medical tweezers or laboratory precision tweezers with smooth polished tips, and the width of the tweezers tip is 0.8~2.5mm; the amount of adhesive transferred in a single transaction is 0.01~0.05g, and the relative deviation of the adhesive amount is controlled within ±15%.

5. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, In step S2, when picking up the glue to be tested, the opening angle of the tweezers is 15°~45°, and the depth of the tweezers inserted into the glue surface is 0.5~2mm. After picking up the glue, lift the tweezers above the glue surface and hold for 0.5~2s. After the excess glue has dripped off naturally, transfer the glue.

6. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, In step S3, the test cup has a circular flat bottom structure with an inner diameter of 2~5mm and a depth of 1~2.5mm, and the inner wall has a smooth hydrophobic surface; the dispensing position is the center of the bottom surface of the test cup, and the deviation of the dispensing position does not exceed 0.5mm.

7. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, In step S3, the pressure of pressing the LED bead is 0.1~0.5N. After pressing, the adhesive completely covers the chip and pad area at the bottom of the bead, and the distance between the edge of the adhesive and the edge of the bead is 0.1~0.3mm.

8. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, In step S4, the real-time observation includes: whether the LED bead landing point is centered, whether the glue is spread evenly, whether there is any glue overflow or lack of glue, whether the LED bead tilt angle is ≤2°, and whether there are any air bubbles inside the glue.

9. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, Step S4 also includes a preliminary light emission detection step: connect the pre-packaged LED beads to the rated operating current, observe the uniformity of the light emission color temperature and the shape of the light spot in real time, and help judge the rationality of the glue ratio.

10. The method for rapid adjustment of LED adhesive mixing ratio according to claim 1, characterized in that, In step S4, if the current glue ratio is determined to be unacceptable, the current test glue cup and glue are discarded directly. There is no need to clean the tweezers. The next set of glue to be tested can be used to start a new round of debugging.