Composite mask layer and method of manufacturing the same and patterning process

By forming a photoresist layer and a mask layer on a photoresist pattern to form a composite mask layer, and by using anisotropic etching process to make its top and bottom widths equal, the problem of non-uniform critical size caused by negative photoresist patterns is solved, and the accuracy and consistency of the patterning process are improved.

CN123165080APending Publication Date: 2026-11-24NAN YA TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510702391.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-20
Filing Date
2025-05-28
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

The photoresist pattern formed by negative photoresist has an inverted trapezoidal profile, which leads to uneven critical dimensions in the patterning layer and affects the patterning effect.

Method used

A composite mask layer, comprising a photoresist pattern, a photoresist layer, and a mask layer, is used. The composite mask layer is formed by anisotropic etching process, ensuring that the top and bottom widths are equal, thus guaranteeing the uniformity of the patterned layer.

Benefits of technology

This achieves uniform critical dimensions for patterns in the patterned layer, improving the accuracy and consistency of the patterning process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123165080A_ABST
    Figure CN123165080A_ABST
Patent Text Reader

Abstract

This invention provides a composite mask layer, its manufacturing method, and a patterning process. The patterning process includes the following steps: forming a layer to be patterned on a substrate; forming a photoresist pattern on the layer to be patterned, wherein the width of the top of the photoresist pattern is greater than the width of the bottom of the photoresist pattern; conformally forming a mask layer on the layer to be patterned and the photoresist pattern; forming a photoresist layer on the mask layer; performing a first anisotropic etching process to remove a portion of the photoresist layer and a portion of the mask layer until the layer to be patterned is exposed, thereby forming a composite mask layer on the layer to be patterned; and using the composite mask layer as an etching mask, performing a second anisotropic etching process on the layer to be patterned. The width of the top of the composite mask layer is equal to the width of the bottom of the composite mask layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a mask layer, its manufacturing method, and semiconductor processes, and more particularly to a composite mask layer, its manufacturing method, and patterning process. Background Technology

[0002] In patterning processes using negative photoresist, due to the characteristics of negative photoresist, the photoresist patterns formed by negative photoresist have an inverted trapezoidal cross-sectional profile. That is, the width of the top of the photoresist pattern is greater than the width of the bottom of the photoresist pattern. Furthermore, when multiple photoresist patterns are formed, the widths of the bottom of these patterns are not uniform. During the patterning of the layer to be patterned, the critical dimension (CD) of the pattern formed in the layer to be patterned is mainly defined by the bottom of the photoresist pattern. Therefore, after using these photoresist patterns to define the pattern in the layer to be patterned, the resulting pattern will have a non-uniform critical dimension. Summary of the Invention

[0003] The present invention relates to a composite mask layer and its manufacturing method, wherein the composite mask layer includes a photoresist pattern, wherein the width of the top of the photoresist pattern is greater than the width of the bottom of the photoresist pattern, and the width of the top of the composite mask layer is equal to the width of the bottom of the composite mask layer.

[0004] The present invention relates to a patterning process in which the above-mentioned composite mask layer is used as an etching mask during an anisotropic etching process of the layer to be patterned.

[0005] The composite mask layer of the present invention includes a photoresist pattern, a photoresist layer, and a mask layer. The photoresist pattern is disposed on a layer to be patterned. The photoresist layer is located above the layer to be patterned and is disposed on the sidewall of the photoresist pattern. The mask layer is disposed between the photoresist layer and the photoresist pattern, and between the photoresist layer and the layer to be patterned. The top width of the photoresist pattern is greater than the bottom width of the photoresist pattern, and the top width of the composite mask layer is equal to the bottom width of the composite mask layer.

[0006] In one embodiment of the composite mask layer of the present invention, the top surface of the photoresist pattern, the top surface of the photoresist layer, and the top surface of the mask layer are coplanar.

[0007] In one embodiment of the composite mask layer of the present invention, the material of the photoresist pattern includes negative photoresist.

[0008] In one embodiment of the composite mask layer of the present invention, the material of the photoresist layer includes negative photoresist.

[0009] In one embodiment of the composite mask layer of the present invention, the material of the photoresist layer includes positive photoresist.

[0010] In one embodiment of the composite mask layer of the present invention, the material of the mask layer includes oxides.

[0011] The method for manufacturing a composite mask layer according to the present invention includes the following steps: forming a photoresist pattern on a layer to be patterned, wherein the width of the top of the photoresist pattern is greater than the width of the bottom of the photoresist pattern. A mask layer is conformally formed on the layer to be patterned and the photoresist pattern. A photoresist layer is formed on the mask layer. An anisotropic etching process is performed to remove portions of the photoresist layer and portions of the mask layer until the layer to be patterned is exposed. The width of the top of the composite mask layer is equal to the width of the bottom of the composite mask layer.

[0012] In one embodiment of the method for manufacturing the composite mask layer of the present invention, after the anisotropic etching process, the top surface of the photoresist pattern, the top surface of the photoresist layer, and the top surface of the mask layer are coplanar.

[0013] In one embodiment of the method for manufacturing the composite mask layer of the present invention, the material of the photoresist pattern includes negative photoresist.

[0014] In one embodiment of the method for manufacturing the composite mask layer of the present invention, the material of the photoresist layer includes negative photoresist.

[0015] In one embodiment of the method for manufacturing the composite mask layer of the present invention, the material of the photoresist layer includes positive photoresist.

[0016] In one embodiment of the method for manufacturing the composite mask layer of the present invention, the material of the mask layer includes oxides.

[0017] The patterning process of the present invention includes the following steps: A layer to be patterned is formed on a substrate. A photoresist pattern is formed on the layer to be patterned, wherein the width of the top of the photoresist pattern is greater than the width of the bottom of the photoresist pattern. A mask layer is conformally formed on the layer to be patterned and the photoresist pattern. A photoresist layer is formed on the mask layer. A first anisotropic etching process is performed to remove a portion of the photoresist layer and a portion of the mask layer until the layer to be patterned is exposed, thereby forming a composite mask layer on the layer to be patterned. A second anisotropic etching process is performed on the layer to be patterned using the composite mask layer as an etching mask. The width of the top of the composite mask layer is equal to the width of the bottom of the composite mask layer.

[0018] In one embodiment of the patterning process of the present invention, after the first anisotropic etching process, the top surface of the photoresist pattern, the top surface of the photoresist layer, and the top surface of the mask layer are coplanar.

[0019] In one embodiment of the patterning process of the present invention, the material of the photoresist pattern includes negative photoresist.

[0020] In one embodiment of the patterning process of the present invention, the material of the photoresist layer includes negative photoresist.

[0021] In one embodiment of the patterning process of the present invention, the material of the photoresist layer includes positive photoresist.

[0022] In one embodiment of the patterning process of the present invention, the material of the mask layer includes oxides.

[0023] Based on the above, the composite mask layer of the present invention includes a photoresist pattern, a photoresist layer disposed on the sidewalls of the photoresist pattern, and a mask layer disposed between the photoresist layer and the photoresist pattern, and between the photoresist layer and the layer to be patterned, wherein the width of the top of the composite mask layer is equal to the width of the bottom of the composite mask layer. Therefore, when the composite mask layer is used as an etching mask to define the pattern in the layer to be patterned during anisotropic etching processes, the resulting pattern can have a uniform critical size. Attached Figure Description

[0024] Figures 1A to 1F This is a schematic cross-sectional view of the patterning process according to an embodiment of the present invention. Detailed Implementation

[0025] The following description provides detailed examples and accompanying drawings, but these examples are not intended to limit the scope of the invention. Furthermore, the drawings are for illustrative purposes only and are not drawn to scale. For ease of understanding, the same components are indicated by the same symbols in the following description.

[0026] The terms "includes," "includes," and "has" used in the text are all open-ended, meaning "includes but not limited to."

[0027] When using terms such as "first" and "second" to describe components, it is only for distinguishing these components from one another and does not limit the order or importance of these components. Therefore, in some cases, the first component may also be called the second component, and the second component may also be called the first component, without departing from the scope of the present invention.

[0028] Furthermore, directional terms mentioned in this document, such as "up" and "down," are only used to refer to the directions in the accompanying drawings and are not intended to limit the invention.

[0029] Furthermore, in this document, the range expressed as "from one value to another" is a concise way of representing a range to avoid listing all the values ​​in the range one by one in the specification. Therefore, the description of a particular value range covers any value within the value range, as well as the smaller value range defined by any value within the value range.

[0030] Figures 1A to 1F This is a schematic cross-sectional view of the patterning process according to an embodiment of the present invention.

[0031] Reference Figure 1A A substrate 100 is provided. In this embodiment, there are no limitations on the substrate 100. For example, the substrate 100 may be a silicon substrate or a dielectric substrate, but the invention is not limited thereto. Then, a patterned layer 102 is formed on the substrate 100. In this embodiment, there are no limitations on the patterned layer 102. For example, in one embodiment, the patterned layer 102 may be an antireflection coating (ARC) material layer.

[0032] Reference Figure 1B A photoresist pattern 104 is formed on the patterning layer 102. Figure 1B The diagram shows two photoresist patterns 104, but the invention is not limited thereto. The desired number of photoresist patterns 104 can be formed as needed. In this embodiment, the material of the photoresist patterns 104 is a negative photoresist. The method for forming the photoresist patterns 104 is, for example, performing a photolithography process on the photoresist material layer.

[0033] Due to the characteristics of negative photoresist, the photoresist pattern 104 formed after the photolithography process has an inverted trapezoidal cross-sectional profile. That is, the width W1 of the top of the photoresist pattern 104 is greater than the width W2 of the bottom of the photoresist pattern 104. Therefore, the photoresist pattern 104 has sloping sidewalls from top to bottom.

[0034] Furthermore, the width W1 of the photoresist pattern 104 will be uniform. For example, the width W1 of the photoresist pattern 104 can be the same. However, the width W2 of the photoresist pattern 104 may be non-uniform. During the patterning of the layer to be patterned, the critical size of the pattern formed in the layer to be patterned is mainly defined by the bottom of the photoresist pattern. Therefore, if the photoresist pattern 104 is used alone as an etching mask to define the pattern in the layer to be patterned 102 during the anisotropic etching process, the pattern formed in the layer to be patterned 102 will have a non-uniform critical size.

[0035] Reference Figure 1CA mask layer 106 is conformally formed on the patterned layer 102 and the photoresist pattern 104. The mask layer 106 covers the top surface of the patterned layer 102 and the top surface and sidewalls of the photoresist pattern 104. The thickness of the mask layer 106 depends on the critical dimension of the pattern formed in the patterned layer 102.

[0036] In this embodiment, the material of the mask layer 106 is an oxide, but the invention is not limited to this, as long as the photoresist pattern 104 is not damaged during the formation of the mask layer 106. The mask layer 106 can be formed, for example, by performing a chemical vapor deposition (CVD) process.

[0037] Reference Figure 1D A photoresist layer 108 is formed on the mask layer 106. The material of the photoresist layer 108 can be either negative or positive photoresist. Based on the characteristics of the photoresist, the photoresist layer 108 covers the photoresist pattern 104 and completely fills the spaces between the photoresist patterns 104. In this embodiment, during the anisotropic etching process, the etching rate of the photoresist layer 108 is greater than the etching rate of the mask layer 106. That is, the etchant used in the anisotropic etching process between the photoresist layer 108 and the mask layer 106 has a high etch selectivity.

[0038] Reference Figure 1E A first anisotropic etching process ET1 is performed to remove a portion of the photoresist layer 108 and a portion of the mask layer 106 until the patterned layer 102 is exposed, so as to form a composite mask layer 10 on the patterned layer 102.

[0039] In detail, during the first anisotropic etching process ET1, because the photoresist pattern 104 has an inverted trapezoidal cross-sectional profile and the etching rate of the photoresist layer 108 is greater than the etching rate of the mask layer 106, the region R of the photoresist layer 108 adjacent to the inclined sidewall of the photoresist pattern 104 (e.g., Figure 1D The portion shown can be protected from anisotropic etching by the mask layer 106 above, and the rest of the photoresist layer 108 can be completely removed by anisotropic etching.

[0040] In this way, after the first anisotropic etching process ET1, the mask layer 106 on the inclined sidewalls of the photoresist pattern 104 and the photoresist layer 108 in region R are retained, and the mask layer 106 extends between the remaining photoresist layer 108 and the patterned layer 102. Furthermore, the top surfaces of the photoresist pattern 104, the photoresist layer 108, and the mask layer 106 can be coplanar. The photoresist pattern 104, the mask layer 106, and the photoresist layer 108 constitute a composite mask layer 10.

[0041] In other words, in this embodiment, after the first anisotropic etching process ET1, the composite mask layer 10 formed on the patterned layer 102 includes a photoresist pattern 104, a photoresist layer 108 disposed on the sidewalls of the photoresist pattern 104, and a mask layer 106 disposed between the photoresist layer 108 and the photoresist pattern 104, and between the photoresist layer 108 and the patterned layer 102. Furthermore, due to the first anisotropic etching process ET1, the composite mask layer 10 may have vertical sidewalls. Therefore, the width W3 of the top of the composite mask layer 10 may be equal to the width W4 of the bottom of the composite mask layer 10.

[0042] Since the width W1 of the photoresist pattern 104 can be uniform, the width W3 of the top of the composite mask layer 10 can also be uniform. Therefore, the width W4 of the bottom of the composite mask layer 10 can also be uniform. In this way, when the composite mask layer 10 is used as an etching mask to define the pattern in the patterned layer 102 during anisotropic etching processes, the pattern formed in the patterned layer 102 can have a uniform critical size.

[0043] In addition, in this embodiment, during the first anisotropic etching process ET1, a portion of the photoresist pattern 104 is also removed, resulting in a smaller thickness for the photoresist pattern 104; however, the invention is not limited to this. In other embodiments, during the first anisotropic etching process ET1, only the photoresist layer 108 and the mask layer 106 are removed.

[0044] Reference Figure 1F Using a composite mask layer 10 as an etching mask, a second anisotropic etching process ET2 is performed on the patterned layer 102 to remove the exposed portions of the patterned layer 102. In this way, a patterned layer 110 is formed on the substrate 100. In this embodiment, since the bottom widths of these composite mask layers 10 are uniform, the formed patterned layers 110 can also have uniform critical dimensions.

[0045] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A composite mask layer, characterized in that, include: The photoresist pattern is set on the layer to be patterned; A photoresist layer is located above the layer to be patterned and is disposed on the sidewall of the photoresist pattern; as well as A mask layer is disposed between the photoresist layer and the photoresist pattern, and between the photoresist layer and the layer to be patterned. The top width of the photoresist pattern is greater than the bottom width of the photoresist pattern, and the top width of the composite mask layer is equal to the bottom width of the composite mask layer.

2. The composite mask layer of claim 1, wherein, The top surface of the photoresist pattern, the top surface of the photoresist layer, and the top surface of the mask layer are coplanar.

3. The composite mask layer of claim 1, wherein, The material of the photoresist pattern includes negative photoresist.

4. The composite mask layer of claim 1, wherein, The photoresist layer is made of negative photoresist.

5. The composite mask layer of claim 1, wherein, The photoresist layer is made of positive photoresist.

6. The composite mask layer of claim 1, wherein, The material of the mask layer includes oxides.

7. A method of manufacturing a composite mask layer, characterized by, include: A photoresist pattern is formed on the layer to be patterned, wherein the width of the top of the photoresist pattern is greater than the width of the bottom of the photoresist pattern; A mask layer is formed conformally on the layer to be patterned and the photoresist pattern; A photoresist layer is formed on the mask layer; as well as An anisotropic etching process is performed to remove portions of the photoresist layer and the mask layer until the patterned layer is exposed. The width of the top of the composite mask layer is equal to the width of the bottom of the composite mask layer.

8. The method of manufacturing a composite mask layer according to claim 7, wherein After the anisotropic etching process, the top surface of the photoresist pattern, the top surface of the photoresist layer, and the top surface of the mask layer are coplanar.

9. The method for manufacturing the composite mask layer according to claim 7, characterized in that, The material of the photoresist pattern includes negative photoresist.

10. The method for manufacturing the composite mask layer according to claim 7, characterized in that, The photoresist layer is made of negative photoresist.

11. The method for manufacturing the composite mask layer according to claim 7, characterized in that, The photoresist layer is made of positive photoresist.

12. The method for manufacturing the composite mask layer according to claim 7, characterized in that, The material of the mask layer includes oxides.

13. A patterning process, characterized in that, include: A patterned layer is formed on a substrate; A photoresist pattern is formed on the layer to be patterned, wherein the width of the top of the photoresist pattern is greater than the width of the bottom of the photoresist pattern; A mask layer is formed conformally on the layer to be patterned and the photoresist pattern; A photoresist layer is formed on the mask layer; A first anisotropic etching process is performed to remove a portion of the photoresist layer and a portion of the mask layer until the patterned layer is exposed, so as to form a composite mask layer on the patterned layer. as well as Using the composite mask layer as an etching mask, a second anisotropic etching process is performed on the layer to be patterned. The width of the top of the composite mask layer is equal to the width of the bottom of the composite mask layer.

14. The patterning process according to claim 13, characterized in that, After the first anisotropic etching process, the top surface of the photoresist pattern, the top surface of the photoresist layer, and the top surface of the mask layer are coplanar.

15. The patterning process according to claim 13, characterized in that, The material of the photoresist pattern includes negative photoresist.

16. The patterning process according to claim 13, characterized in that, The photoresist layer is made of negative photoresist.

17. The patterning process according to claim 13, characterized in that, The photoresist layer is made of positive photoresist.

18. The patterning process according to claim 13, characterized in that, The material of the mask layer includes oxides.