Chip package structure manufacturing method and chip package structure

By depositing an anti-reflective layer in the chip packaging process, the problems of accidental exposure and photoresist residue caused by reflection at the copper pillar plating opening are solved, improving the fabrication efficiency and structural stability of the second conductive layer, and ensuring the plating quality and mechanical strength of the copper pillar.

CN123165104APending Publication Date: 2026-11-24SUZHOU GUOXIAN INNOVATION TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611160764.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-31
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In existing chip packaging processes, the electroplating openings of copper pillars are accidentally exposed and have photoresist residue due to the high reflectivity of the top of the first copper pillar, which affects the electroplating quality and structural stability of the second copper pillar.

Method used

An anti-reflective layer is deposited on the side of the first conductive layer away from the packaging substrate to absorb reflected light and avoid accidental exposure of non-exposed areas and photoresist residue. The second conductive layer is prepared by coating photoresist on the second substrate and patterning it.

Benefits of technology

This effectively avoids accidental exposure and photoresist residue, improves the fabrication efficiency and structural stability of the second conductive layer, ensures sufficient inflow of electroplating solution and copper ion concentration, and enhances mechanical strength and conductivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123165104A_ABST
    Figure CN123165104A_ABST
Patent Text Reader

Abstract

This application provides a chip packaging structure manufacturing method, including the following steps: S101. Providing a first substrate, wherein the first substrate includes a packaging substrate and a first conductive layer stacked together; S102. Depositing an anti-reflective layer on the surface of the first conductive layer away from the packaging substrate to obtain a second substrate; S103. Coating a first photoresist on the surface of the second substrate away from the packaging substrate and patterning it to obtain a third substrate; S104. Fabricating a second conductive layer on the surface of the third substrate away from the packaging substrate. This application, by depositing an anti-reflective layer on the surface of the first conductive layer away from the packaging substrate, can avoid accidental exposure of non-exposed areas and photoresist residue problems caused by surface reflection of the first conductive layer during exposure, ensuring the bottom size of the opening after exposure and development, and improving the fabrication efficiency and structural stability of the second conductive layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of chip packaging technology, specifically to a chip packaging structure manufacturing method and a chip packaging structure. Background Technology

[0002] In the field of modern electronic packaging, with the continuous improvement of chip integration and the increasing complexity of functional requirements, the application of multi-chip integrated packaging is becoming more and more widespread. Traditional multi-chip packaging is no longer able to meet current technological demands in many aspects, and chip packaging structure manufacturing methods need to be improved. Summary of the Invention

[0003] In view of this, the embodiments of this application aim to provide a chip packaging structure manufacturing method and chip packaging structure, which can effectively solve the problems of accidental exposure and photoresist residue.

[0004] The first aspect of this application provides a method for manufacturing a chip packaging structure, including the following steps:

[0005] S101. A first substrate is provided, wherein the first substrate includes a stacked encapsulation substrate and a first conductive layer, and the first conductive layer includes a plurality of spaced first conductive pillars; S102. An anti-reflective layer is deposited on the surface of the first conductive layer away from the packaging substrate to obtain a second substrate, wherein the anti-reflective layer includes a plurality of anti-reflective portions spaced apart, and the orthographic projection of the anti-reflective portions on the packaging substrate overlaps with the orthographic projection of the first conductive post on the packaging substrate. S103. A first photoresist is coated and patterned on the surface of the second substrate away from the packaging substrate to obtain a third substrate. S104. A second conductive layer is prepared on the surface of the third substrate away from the packaging substrate, wherein the second conductive layer includes a plurality of spaced second conductive pillars, and the second conductive pillars are in direct contact with the first conductive pillars.

[0006] Optionally, in some embodiments of this application, the thickness of the anti-reflective layer is 100–300 nm.

[0007] Furthermore, in some embodiments of this application, the antireflective layer has a transmittance of less than 1% at a wavelength of 365nm and a reflectance of less than 5% at a wavelength of 365nm.

[0008] Optionally, in some embodiments of this application, step S102 further includes: preparing a first electroplating solution, immersing the first substrate in the first electroplating solution, applying a voltage to the first substrate for electroplating for a period of time, and depositing an anti-reflective layer on the surface of the first conductive layer away from the packaging substrate.

[0009] Furthermore, in some embodiments of this application, the applied voltage is -0.5V to -2.0V.

[0010] Furthermore, in some embodiments of this application, the electroplating time is 30 to 120 seconds.

[0011] Optionally, in some embodiments of this application, the first electroplating solution includes: deionized water with a pH of 7 to 9, conductive salt, and light-absorbing dye.

[0012] Furthermore, in some embodiments of this application, the conductive salt is Na2SO4 or K2SO4, and the molar concentration of the conductive salt in the first electroplating solution is 0.1 to 0.5 mol / L.

[0013] Furthermore, in some embodiments of this application, the light-absorbing dye is Sudan Black or methyl orange, and the mass concentration of the light-absorbing dye in the first electroplating solution is 0.1 to 1 g / L.

[0014] Furthermore, in some embodiments of this application, the first electroplating solution further includes copper salt, wherein the mass concentration of the copper salt in the first electroplating solution is 0.01 to 0.1 g / L.

[0015] Furthermore, in some embodiments of this application, the copper salt is CuSO4·5H2O.

[0016] Optionally, in some embodiments of this application, the first electroplating solution comprises: a polymer matrix and a light-absorbing dye. Preferably, the polymer matrix is ​​selected from one of polyvinyl alcohol, polyacrylic acid, or polymethyl methacrylate copolymer; Preferably, the light-absorbing dye is one of Sudan Black, methyl orange, coumarin derivatives, or azo dyes.

[0017] Optionally, in some embodiments of this application, step S101 further includes: providing a packaging substrate, depositing a first conductive layer on the packaging substrate to obtain a first substrate.

[0018] Furthermore, in some embodiments of this application, step S101 further includes depositing a first conductive layer on the packaging substrate and then grinding and planarizing the side of the first conductive layer away from the packaging substrate to obtain the first substrate.

[0019] Optionally, in some embodiments of this application, step S103 further includes: coating a second photoresist layer on the surface of the second substrate away from the packaging substrate, exposing it through a mask, developing to remove a portion of the second photoresist layer and the anti-reflection portion to obtain the third substrate; the orthographic projection of the removed portion of the second photoresist layer on the packaging substrate covers at least a portion of the orthographic projection of the first conductive pillar on the packaging substrate.

[0020] Optionally, in some embodiments of this application, step S104 further includes: immersing the third substrate in a second electroplating solution to electroplat the second conductive layer.

[0021] Furthermore, in some embodiments of this application, step S104 further includes: the third substrate includes a first region and a second region, the first region is partially disposed around the first region, and after shielding the surface of the first conductive pillar located in the second region on the side away from the packaging substrate, the third substrate is immersed in the second electroplating solution to electroplat the second conductive layer.

[0022] Optionally, in some embodiments of this application, the third substrate includes a first region and a second region, the first region is partially disposed around the second region, and the orthographic projection of the second conductive post on the third substrate is located within the first region. The method further includes: S105. Electrically connecting the first conductive post located within the second region to a semiconductor bridge.

[0023] Optionally, in some embodiments of this application, the manufacturing method further includes: S106. Electrically connecting the chip layer to the semiconductor bridge and / or the second conductive pillar.

[0024] The second aspect of this application provides a chip packaging structure, which is prepared by the chip packaging structure manufacturing method described in the above embodiments.

[0025] The beneficial effects of this application are as follows: The chip packaging structure manufacturing method provided by this application can avoid accidental exposure of non-exposed areas and photoresist residue caused by surface reflection of the first conductive layer during exposure by depositing an anti-reflection layer on the surface of the first conductive layer away from the packaging substrate, thus ensuring the bottom size of the opening after exposure and development, which is beneficial to improving the fabrication efficiency and structural stability of the second conductive layer. Attached Figure Description

[0026] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.

[0027] Figure 1 This is a schematic diagram of a chip packaging structure manufacturing method according to one embodiment of this application; Figure 2 This is a schematic diagram of step S101 of one embodiment of this application; Figures 3 to 8 This is a schematic diagram of a chip packaging structure manufacturing method according to one embodiment of this application; Figure 9 This is a schematic diagram of a chip packaging structure according to one embodiment of this application.

[0028] Explanation of reference numerals in the attached figures: 100 - Package substrate, 101 - First wiring layer, 1011 - First wiring circuit, 102 - Second wiring layer, 1021 - Second wiring circuit, 103 - Conductive channel layer, 1031 - Trajectory. 110 - Conductive seed layer, 110a - Third region, 110b - Fourth region 111 - First photoresist layer, 112 - Second photoresist layer 121 - First conductive layer, 1211 - First conductive pillar, 122 - Second conductive layer, 1221 - Second conductive pillar 130-Semiconductor Bridge 200-chip layer, 100a - First surface of the package substrate, O - Reference plane 141 - First substrate, 142 - Second substrate, 143 - Third substrate, 143a - First region, 143b - Second region 151-Anti-reflective part, 161 - First connecting electrode, 162 - Second connecting electrode, 163 - Third connecting electrode. Detailed Implementation

[0029] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. The components of the embodiments of this application described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.

[0030] Therefore, the following detailed description of the embodiments of this application provided in the accompanying drawings is not intended to limit the scope of the claimed application, but merely to illustrate selected embodiments of the application. All other embodiments obtained by those skilled in the art based on the embodiments of this application without inventive effort are within the scope of protection of this application. It should be noted that similar reference numerals and letters in the following drawings denote similar items; therefore, once an item is defined in one drawing, it does not need to be further defined and explained in subsequent drawings. It should be noted that, unless otherwise specified, different features in the embodiments of this application can be combined with each other.

[0031] For ease of understanding, the accompanying drawings show mutually orthogonal X-axis, Y-axis, and Z-axis. The direction along the X-axis is called the X-direction, the direction along the Y-axis is called the Y-direction, and the direction along the Z-axis is called the Z-direction. The Z-direction is the normal direction relative to the plane containing the X and Y directions. Furthermore, the view of various elements parallel to the plane containing the X and Y directions is called a top view. Alternatively, the planes in the X and Y directions can be planes parallel to the horizontal plane, and the Z-direction can be a direction parallel to the thickness direction of the chip package structure.

[0032] For certain elements, terms like "above" or "overhead" are sometimes used when describing the position of an element in the Z direction, and "below" or "under" are used when describing the position of an element in the opposite direction. Furthermore, when using terms like "above," "overhead," "below," "under," or "relative" to define the positional relationship between two elements, this includes not only the state where the two elements are directly adjacent, but also the state where the two elements are separated by gaps or other elements. Additionally, terms like "first," "second," and "third" are used only for distinguishing descriptions and should not be interpreted as indicating or implying relative importance.

[0033] In existing chip packaging processes, to achieve high-density interconnects between the substrate and the semiconductor bridge dies and chips, it is typically necessary to fabricate a high-density copper pillar array with a height exceeding 200 μm on the substrate. These copper pillars play a crucial role in absorbing the total thickness deviation (TTV) of the packaged substrate, providing interconnect channels, and supporting subsequent semiconductor bridge and chip mounting.

[0034] The inventors discovered that in existing methods, to fabricate copper pillars and achieve selective copper deposition in specific areas, a conductive seed layer needs to be deposited across the entire surface first. Then, a thick photoresist layer exceeding the target electroplating height (over 200 μm) is applied as a physical barrier to isolate non-electroplating areas and define the electroplating pattern. A first electroplating process is then performed to form the first copper pillar. Before forming the second copper pillar on the first layer, photoresist needs to be applied again, followed by exposure and development to form the electroplating opening for the second copper pillar. The inventors found that the electroplating opening becomes abnormal and affects the quality of subsequent electroplating. Further analysis revealed that the abnormality is due to the fact that the top of the first copper pillar is a flat metal surface with a reflectivity of over 80% for ultraviolet light. When photoresist is applied above the first copper pillar and exposure is performed, the photoresist in the area above the first copper pillar, which should not normally be exposed due to the mask, is blocked by the photomask. However, due to the high reflectivity of the top of the first copper pillar, reflected light returns upwards, causing accidental exposure of the photoresist bottom in that area. This results in partial cross-linking of the photoresist bottom, which is retained after development. The photoresist in the unexposed area (the area blocked by the mask) is removed after development, forming an electroplating opening. At this point, because the bottom portion of the photoresist in the area above the first copper pillar is retained, the bottom size of the electroplating opening is smaller than the design value. This makes it difficult for the electroplating solution for the second copper pillar to flow sufficiently into the bottom of the electroplating opening, restricting solution exchange, reducing the copper ion concentration at the bottom, and requiring a longer electroplating time. In severe cases, internal voids may form due to copper ion depletion, reducing the mechanical strength and conductivity of the second copper pillar. In some cases, the photoresist residue at the bottom may completely cover the top surface of the first copper pillar, preventing the formation of the second copper pillar.

[0035] To address the aforementioned problems, the inventors, after extensive research, have innovatively proposed a method for manufacturing a chip packaging structure. The technical solution of this invention will be explained in detail below with reference to the accompanying drawings.

[0036] The first aspect of this application provides a method for manufacturing a chip packaging structure. Figure 1 This is a schematic diagram of a chip packaging structure manufacturing method according to one embodiment of the present invention. See also: Figure 1 The chip packaging structure manufacturing method includes the following steps: S101. A first substrate is provided, wherein the first substrate includes a stacked encapsulation substrate and a first conductive layer, and the first conductive layer includes a plurality of spaced first conductive pillars.

[0037] S102. An anti-reflective layer is deposited on the surface of the first conductive layer away from the packaging substrate to obtain a second substrate, wherein the anti-reflective layer includes a plurality of anti-reflective portions spaced apart, and the orthographic projection of the anti-reflective portions on the packaging substrate overlaps with the orthographic projection of the first conductive pillar on the packaging substrate.

[0038] S103. A first photoresist is coated and patterned on the surface of the second substrate away from the packaging substrate to obtain a third substrate.

[0039] S104. A second conductive layer is prepared on the surface of the third substrate away from the packaging substrate, wherein the second conductive layer includes a plurality of spaced second conductive pillars, and the second conductive pillars are in direct contact with the first conductive pillars.

[0040] This application provides a chip packaging structure manufacturing method that, by depositing an anti-reflection layer on the surface of the first conductive layer away from the packaging substrate, can avoid accidental exposure of non-exposed areas and photoresist residue caused by surface reflection of the first conductive layer during exposure, ensuring the bottom size of the opening after exposure and development, which is beneficial to improving the fabrication efficiency and structural stability of the second conductive layer.

[0041] Figures 2 to 8 This is a schematic diagram of a manufacturing process for a chip packaging structure according to one embodiment of this application. The following will be combined with... Figures 2 to 8 This section introduces the steps involved in manufacturing a chip packaging structure.

[0042] Figure 2 This is a schematic diagram of step S101 of one embodiment of this application. Figure 2 As shown, in some embodiments of this application, S101. A first substrate is provided, wherein the first substrate includes a stacked encapsulation substrate and a first conductive layer, and the first conductive layer includes a plurality of spaced-apart first conductive pillars. The process includes the following steps: S1011. Provide a packaging substrate.

[0043] S1012. Deposit a first conductive layer on the packaging substrate.

[0044] S1013. The side of the first conductive layer away from the packaging substrate is ground and planarized to obtain the first substrate.

[0045] Specifically, step S1011: Provide a packaging substrate. Figure 3 This is a schematic diagram of a cross-section of a packaging substrate along its thickness direction. See also... Figure 3 ,along Figure 3 In the Z-direction, the packaging substrate 100 includes a first wiring layer 101, a second wiring layer 102, and a conductive channel layer 103. The conductive channel layer 103 is located between the first wiring layer 101 and the second wiring layer 102. A first wiring circuit 1011 is disposed in the first wiring layer 1012. A second wiring circuit 1021 is disposed in the second wiring layer 102. A trace 1031 is disposed in the conductive channel layer 103. The first wiring circuit 1011 is electrically connected to the second wiring circuit 1021 through the trace 1031.

[0046] The packaging substrate 100 is a packaging substrate with total thickness variation (TTV). For example... Figure 3 As shown, one side surface of the packaging substrate 100 has an uneven area. Specifically, the packaging substrate 100 has a flat reference surface O. A portion of the first surface 100a of the packaging substrate is at a distance A from the reference surface O. Another portion of the first surface 100a of the packaging substrate is at a distance B from the reference surface O. A and B are not equal. For example, the minimum distance from the first surface 100a of the packaging substrate to the reference surface O is denoted as Amin, and the maximum distance is denoted as Amax. The difference between Amax and Amin is usually denoted as the total thickness deviation. Generally, the total thickness deviation of the packaging substrate 100 is around 40 μm. It can be understood that when the packaging substrate 100 has a total thickness deviation, due to the obvious warping deformation on its surface and the poor uniformity of the overall total thickness deviation, the unevenness of the substrate surface has a large error, which will lead to insufficient alignment and bonding accuracy of the subsequent chip layers.

[0047] Step S1012. Deposit a first conductive layer on the packaging substrate. Specifically, in some embodiments of this application, step S1012 includes: Step S10121. Deposit and prepare a conductive seed layer on the packaging substrate. Figure 4 This is a schematic diagram of the structure after conductive seeds have been deposited on the packaging substrate. See also... Figure 4 A conductive seed layer material is deposited over the entire surface of the first surface 100a of the packaging substrate to form a conductive seed layer 110. The conductive seed layer material can be copper or gold. The thickness of the conductive seed layer 110 is 180 nm to 220 nm. In some embodiments, a barrier layer material is first deposited over the entire surface of the packaging substrate before depositing the conductive seed layer material to form a barrier layer (not shown in the figure). The barrier layer material is selected from titanium, titanium-tungsten alloy, tantalum, tantalum nitride, or ruthenium. The thickness of the barrier layer is 40 nm to 60 nm. The barrier layer enhances the bonding force between the conductive seed layer and the packaging substrate, providing support for the subsequent conductive pillar structure. The conductive seed layer can effectively guide the uniform and dense growth of the conductive pillars. For example, a 50 nm layer of titanium is deposited on the first surface 100a of the packaging substrate as a barrier layer, and a 200 nm layer of copper is deposited as the conductive seed layer 110, forming a stacked structure.

[0048] Step S1012 further includes step S10122: forming a patterned first photoresist layer on the side of the conductive seed layer away from the packaging substrate to obtain a first intermediate structure. Figure 5 This is a schematic diagram of the first substrate. See also... Figure 5Specifically, a photoresist layer is coated on the side of the conductive seed layer 110 away from the packaging substrate. Using a photomask, after exposure and development, a patterned first photoresist layer 111 is obtained, thus forming the first intermediate structure. The first photoresist layer 111 includes a cutout area that exposes the surface of the conductive seed layer away from the packaging substrate. By setting the patterned first photoresist layer, a channel for fabricating the first conductive layer can be constructed, ensuring insulation between adjacent first conductive pillars after their formation. Furthermore, it effectively supports the first conductive pillars, preventing them from becoming eccentric or even collapsing due to lack of support in subsequent processes.

[0049] Step S1012 further includes step S10123: depositing a first conductive layer on the first intermediate structure. See also: Figure 5 After immersing the first intermediate structure in an acidic electroplating solution, a voltage is applied to the first intermediate structure for electroplating, forming a first conductive layer 121 on the surface of the conductive seed layer 110 exposed from the first photoresist layer 111, away from the packaging substrate 100. The first conductive layer 121 includes a plurality of spaced-apart first conductive pillars 1211. The surface of the conductive seed layer 110 in the first intermediate structure away from the packaging substrate 100 includes a fourth region 110b, which is shielded by the first photoresist layer 111, and a third region 110a, which is exposed by the cutout area. The conductivity of the third region 110a and the fourth region 110b is significantly different. During electroplating, almost all the current flows through the third region 110a, and conductive ions in the electroplating solution are reduced and deposited only in the third region 110a. Optionally, in this embodiment, the electroplating solution is a copper-containing electroplating solution. Understandably, the first conductive pillars 1211 are copper pillars. The height of the first conductive pillars 1211 can be adjusted by controlling the electroplating time and current density. Understandably, the packaging substrate 100 has a protective film on the side away from the conductive seed layer 110. This protects the packaging substrate during the electroplating of the conductive layer material, preventing the conductive layer material from depositing in unwanted areas.

[0050] Step S1013. The side of the first conductive layer away from the packaging substrate is planarized by grinding to obtain the first substrate. (Continue to the previous step) Figure 5 The surface of the first conductive layer 121 away from the packaging substrate 100 is planarized by grinding, so that the surface of the first conductive pillar 1211 away from the packaging substrate 100 is coplanar with the surface of the first photoresist layer 111 away from the packaging substrate 100, thus obtaining the first substrate 141. Planarization by grinding can improve the problems of warpage and poor uniformity of overall thickness caused by the packaging substrate, thereby improving the alignment and bonding accuracy of subsequent chip layers. Understandably, planarization, in addition to ensuring the flatness of the surface away from the packaging substrate, also needs to expose the surface of the first conductive pillar away from the packaging substrate.

[0051] Step S102. An anti-reflective layer is deposited on the surface of the first conductive layer away from the packaging substrate to obtain a second substrate. The anti-reflective layer includes a plurality of spaced-apart anti-reflective portions, the orthographic projection of which overlaps with the orthographic projection of the first conductive pillar on the packaging substrate. Optionally, in some embodiments of this application, the thickness of the anti-reflective layer is 100–300 nm. The thickness of the anti-reflective layer can be adjusted by controlling the electroplating time and current density. Optionally, in some embodiments of this application, the transmittance of the anti-reflective layer at a wavelength of 365 nm is less than 1%, and the reflectance at a wavelength of 365 nm is less than 5%. This ensures the absorption effect of the anti-reflective layer on reflected light and avoids accidental exposure of non-exposed areas and photoresist residue problems caused by reflection from the surface of the first conductive layer during exposure.

[0052] In some embodiments of this application, step S102 includes: S1021. Prepare the first electroplating solution.

[0053] S1022. Immerse the first substrate in the first electroplating solution, apply voltage to the first substrate for electroplating for a period of time, and then deposit an anti-reflective layer on the surface of the first conductive layer away from the packaging substrate.

[0054] Specifically, in some embodiments, step S1021, preparing the first electroplating solution, includes: taking deionized water with a pH of 7-9, mixing a conductive salt and a light-absorbing dye to obtain the first electroplating solution. Optionally, in some embodiments of this application, the conductive salt is Na2SO4 or K2SO4, and the molar concentration of the conductive salt in the first electroplating solution is 0.1-0.5 mol / L. Optionally, in some embodiments of this application, the light-absorbing dye is Sudan Black or methyl orange, and the mass concentration of the light-absorbing dye in the first electroplating solution is 0.1-1 g / L. Optionally, in some embodiments of this application, the first electroplating solution further includes a copper salt, and the mass concentration of the copper salt in the first electroplating solution is 0.01-0.1 g / L. Optionally, the copper salt is CuSO4·5H2O. Using this first electroplating solution can ensure the deposition effect of the light-absorbing dye, which is beneficial to the subsequent absorption of reflected light.

[0055] In some embodiments, step S1021, preparing the first electroplating solution, includes: mixing a polymer matrix and a light-absorbing dye to obtain the first electroplating solution. Optionally, in some embodiments, the polymer matrix can be a water-soluble polymer or an alkali-soluble polymer. Optionally, the polymer matrix is ​​selected from polyvinyl alcohol, polyacrylic acid, or polymethyl methacrylate copolymer. Optionally, in some embodiments, the light-absorbing dye is selected from Sudan Black, methyl orange, coumarin derivatives, or azo dyes. Using this first electroplating solution can ensure the deposition effect of the light-absorbing dye, which is beneficial for subsequent absorption of reflected light.

[0056] Step S1022. Immerse the first substrate in the first electroplating solution, apply voltage to the first substrate for electroplating for a period of time, and then deposit an anti-reflective layer on the surface of the first conductive layer away from the packaging substrate. Figure 6 This is a schematic diagram of the second substrate. Specifically, in some embodiments, the first substrate is immersed in the first electroplating solution, and a voltage of -0.5V to -2.0V is applied to the first substrate as the cathode. An inert counter electrode (such as Pt or graphite) is used as the anode. Optionally, in some embodiments of this application, the electroplating time is 30 to 120 seconds. In some embodiments, a constant current mode is used, and the current density can be 0.1 to 1 mA / cm². Using the above parameters can ensure the electroplating effect of the anti-reflective layer.

[0057] The surface of the first substrate 141 furthest from the packaging substrate 100, corresponding to the third region 110a, forms the surface of the first conductive pillar 1211 furthest from the packaging substrate 100. The surface of the first photoresist layer 111 furthest from the packaging substrate 100, corresponding to the fourth region 110b, forms the surface of the first photoresist layer 111 furthest from the packaging substrate 100. The conductivity of the two regions differs significantly. During electroplating, almost all the current flows through the surface corresponding to the third region 110a. The light-absorbing dye in the plating solution is deposited only on the surface corresponding to the third region 110a, forming the anti-reflective portion 151 of the anti-reflective layer, thus obtaining the second substrate 142. Understandably, the anti-reflective portion may include light-absorbing dye molecules, or a mixed composite layer formed by the co-deposition of copper and light-absorbing dye molecules. By depositing an anti-reflective layer on the surface of the first conductive layer furthest from the packaging substrate, accidental exposure of non-exposed areas due to reflection from the surface of the first conductive layer and photoresist residue problems can be avoided during exposure. Ensuring the bottom size of the opening after exposure and development allows the plating solution for the second conductive layer to flow fully into the bottom of the opening, ensuring sufficient exchange of the plating solution, maintaining the copper ion concentration at the bottom of the opening, and saving plating time. This also avoids internal voids during the fabrication of the second conductive layer, thereby improving the mechanical strength and conductivity of the second conductive layer.

[0058] Optionally, in some embodiments of this application, step S103 further includes: coating a second photoresist layer on the surface of the second substrate away from the packaging substrate, exposing it through a mask, developing to remove a portion of the second photoresist layer and the anti-reflection portion, and obtaining a third substrate; the orthographic projection of the removed portion of the second photoresist layer on the packaging substrate covers the orthographic projection of the first conductive pillar on the packaging substrate. Figure 7 This is a schematic diagram of one possible structure of the third substrate. See [link / reference] for details. Figure 7A second photoresist is coated on the surface of the second substrate 142 away from the packaging substrate 100 to form a second photoresist layer 112. Then, exposure is performed through a mask, and development removes a portion of the second photoresist layer 112, exposing the surface of the first conductive pillar 1211 away from the packaging substrate 100. During this process, the developer simultaneously removes the anti-reflective portion of the surface of the first conductive pillar 1211. Finally, a third substrate 143 is obtained. The orthographic projections of the removed portion of the second photoresist layer and the anti-reflective portion on the packaging substrate cover at least a portion of the orthographic projection of the first conductive pillar on the packaging substrate.

[0059] Optionally, in some embodiments of this application, step S104 further includes: immersing the third substrate in the second electroplating solution to electroplat and prepare the second conductive layer. Figure 9 This is a schematic diagram of a chip packaging structure prepared by a chip manufacturing method according to this application. See also... Figure 9 Specifically, after immersing the third substrate in the second electroplating solution, a voltage is applied to the third substrate to perform electroplating to form a second conductive layer 122. The second conductive layer 122 includes a plurality of spaced second conductive pillars 1221.

[0060] Furthermore, in some embodiments of this application, before electroplating to prepare the second conductive layer in step S104, the method further includes: a third substrate comprising a first region and a second region, the first region partially surrounding the second region; after shielding the surface of the first conductive pillar in the second region on the side furthest from the encapsulation substrate, the third substrate is immersed in a second electroplating solution to electroplat the second conductive layer. See also Figure 7 The third substrate 143 includes a first region 143a and a second region 143b, with the first region 143a partially surrounding the second region 143b. After step S103, a second photoresist layer 112 is present in the first region 143a, but not in the second region 143b, and the surface of the first conductive pillar 1211 in the first conductive layer 121 away from the packaging substrate 100 is exposed. The surface of the first conductive pillar 1211 in the second region 143b away from the packaging substrate 100 is shielded. Understandably, at this time, the surface of the third substrate 143 in the first region 143a away from the packaging substrate includes the surface of the second photoresist layer 112 and the surface of the first conductive pillar 1211. The surface of the second region 143b away from the packaging substrate includes the surface of the first photoresist layer 111 and the shielded surface of the first conductive pillar 1211. The conductivity of the surface of the first conductive pillar 1211 on the side away from the packaging substrate 100 in the first region 143a is significantly different from that of the surface of the second photoresist layer, the surface of the first photoresist layer, and the surface of the first conductive pillar 1211 that is blocked.

[0061] Optionally, the surface of the first conductive pillar 1211 located in the second region 143b on the side away from the packaging substrate 100 is shielded, and the shielding layer material can be a self-assembled monolayer. Optionally, the self-assembled monolayer can be removed by heating.

[0062] Subsequently, the third substrate is immersed in the second electroplating solution, and a voltage is applied to the third substrate to electroplating form a second conductive layer 122. The second conductive layer 122 includes a plurality of spaced second conductive pillars 1221. At this time, due to the large difference in surface conductivity, almost all the current flows through the surface of the first conductive pillars 1211 in the first region 143a away from the packaging substrate 100. Conductive ions in the second electroplating solution are reduced and deposited only on the surface of the first conductive pillars 1211 away from the packaging substrate 100. That is, the orthogonal projection of the second conductive pillars 1221 on the third substrate is located in the first region 143a. In the first region 143a, the first conductive pillars 1211 and the second conductive pillars 1221 are in direct contact. Optionally, in this embodiment, the second electroplating solution is a copper-containing electroplating solution. It is understood that the second conductive pillars 1221 are copper pillars. The height of the second conductive pillars 1221 can be adjusted by controlling the electroplating time and current density. It is understood that the second electroplating solution can be the same as the electroplating solution in step S1012.

[0063] Optionally, in some embodiments of this application, the manufacturing method of the chip package structure further includes: S105. Electrically connecting the first conductive post located in the second region to the semiconductor bridge. Specifically, see... Figure 9 Step S105 includes the following steps: S1051. Remove the shielding layer material from the surface of the first conductive pillar 1211 in the second region 143b of the structure after step S104. Optionally, when the shielding layer material is a self-assembled monolayer, it can be removed by heating. After removing the shielding layer material, the surface of the first conductive layer 121 in the second region 143b away from the packaging substrate 100 is exposed.

[0064] S1052. A second connection electrode 162 is formed on the surface of the first conductive layer 121 in the second region 143b on the side away from the packaging substrate 100. Optionally, the second connection electrode 162 may be made of Ni / Sn.

[0065] S1053. At least a portion of the first conductive pillar 1211 within the second region 143b is electrically connected to the semiconductor bridge 130 via the second connecting electrode 162. Optionally, the semiconductor bridge 130 may be a silicon bridge.

[0066] Optionally, some embodiments of this application further include: S106. Electrically connecting the chip to the semiconductor bridge and / or the second conductive pillar. Specifically, see... Figure 9 Step S106 includes the following steps: S1061. Electrically connect the chip layer to the second conductive pillar. Specifically, at least a portion of the second conductive pillar 1221 in the first region 143a is electrically connected to the chip layer 200 via the first connection electrode 161.

[0067] S1062. Electrically connect the chip layer to the semiconductor bridge. Specifically, electrically connect the semiconductor bridge 130 to the chip layer 200 via the third connection electrode 163.

[0068] Optionally, in some embodiments of this application, another third substrate can be obtained after step S103. Figure 8 This is a schematic diagram of another structure for the third substrate. See below for details. Figure 8 A second photoresist layer 112 is formed by coating the surface of the second substrate 142 away from the packaging substrate 100 with a second photoresist layer. Then, exposure is performed through a mask, and development removes a portion of the second photoresist layer 112, exposing the surface of the first conductive pillar 1211 away from the packaging substrate 100. During this process, the developer simultaneously removes the anti-reflective portion of the surface of the first conductive pillar 1211. Finally, a third substrate 143 is obtained. The third substrate 143 includes a first region 143a and a second region 143b, with the first region 143a partially surrounding the second region 143b. After step S103, the second photoresist layer 112 exists within both the first region 143a and the second region 143b. Within the first region 143a, the second photoresist layer 112 exposes the surface of the first conductive pillar 1211 away from the packaging substrate 100. Within the second region 143b, the surface of the first conductive pillar 1211 away from the packaging substrate 100 still retains the anti-reflective portion 151. That is, the second photoresist layer 112 in the second region 143b was not removed, covering the first conductive pillar 1211 and the anti-reflection part 151 in the second region 143b.

[0069] When the preparation yields as follows Figure 8After the third substrate structure is shown, it can be understood that the surface of the third substrate 143 in the first region 143a away from the packaging substrate includes the surface of the second photoresist layer 112 and the surface of the first conductive pillar 1211. The surface of the second region 143b away from the packaging substrate is the surface of the second photoresist layer 112. Subsequently, after step S104 is performed to immerse the third substrate in the second electroplating solution, a voltage is applied to the third substrate to electroplating to form the second conductive layer 122. The second conductive layer 122 includes a plurality of spaced second conductive pillars 1221. Since the conductivity difference between the surface of the first conductive pillar 1211 in the first region 143a away from the packaging substrate 100 and the surface of the second photoresist layer is large, during electroplating, almost all the current flows through the surface of the first conductive pillar 1211 in the first region 143a away from the packaging substrate 100. The conductive ions in the second electroplating solution are reduced and deposited only on the surface of the first conductive pillar 1211 in the first region 143a away from the packaging substrate 100. That is, within the first zone 143a, the first conductive post 1211 and the second conductive post 1221 are in direct contact.

[0070] Optionally, in some embodiments, step S105 further includes: S1054. Removing the second photoresist layer 112 and the anti-reflective portion 151 within the second region 143b. Specifically, the second photoresist layer 112 within the second region 143b is removed using a photoresist remover. The anti-reflective portion 151 is removed using a developer. Finally, the surface of the first conductive layer 121 within the second region 143b away from the packaging substrate 100 is exposed. Subsequently, steps S1052 and S1053 in the above embodiments can be performed to complete the electrical connection between at least a portion of the first conductive pillars 1211 within the second region 143b and the semiconductor bridge 130.

[0071] Optionally, in some embodiments, the manufacturing method of the chip package structure further includes: after fabricating the first conductive layer 121 and the second conductive layer 122, removing the first photoresist layer 111 and the second photoresist layer 112 using a resist remover, and then filling a dielectric layer between adjacent first conductive pillars 1211 and adjacent second conductive pillars 1221. Optionally, the dielectric layer can be made of an insulating material, such as photoresist, ABF (Ajinomoto Build-up Film), or NPI (Non-Photosensitive Polyimide).

[0072] Optionally, in some embodiments, the method further includes etching the conductive seed layer 110 after the first conductive layer 121 or the second conductive layer 122 is fabricated to remove a portion of the conductive seed layer corresponding to the region between adjacent first conductive pillars. This operation can prevent short circuits.

[0073] It should be clarified that this application is not limited to the specific configurations and processes described above and shown in the figures. For the sake of brevity, detailed descriptions of known methods are omitted here. In the above embodiments, several specific steps are described and shown as examples. However, the manufacturing process of this application is not limited to the specific steps described and shown. Those skilled in the art can make various changes, modifications, and additions, or change the order of steps, after understanding the spirit of this application.

[0074] The second aspect of this application provides a chip packaging structure, which is prepared using the chip packaging structure manufacturing method described in the above embodiments. Figure 9 This is a schematic diagram of a chip packaging structure prepared by a chip manufacturing method according to this application. See also... Figure 9 Along the thickness direction, i.e. Figure 9 In the Z-direction, the chip packaging structure includes a packaging substrate 100. The packaging substrate 100 includes a first wiring layer 101, a second wiring layer 102, and a conductive channel layer 103. The conductive channel layer 103 is located between the first wiring layer 101 and the second wiring layer 102. A first wiring circuit 1011 is disposed in the first wiring layer 1012. A second wiring circuit 1021 is disposed in the second wiring layer 102. A trace 1031 is disposed in the conductive channel layer 103. The first wiring circuit 1011 is electrically connected to the second wiring circuit 1021 through the trace 1031. A conductive seed layer 110 is disposed above the packaging substrate 100. A first conductive layer 121 is disposed above the conductive seed layer 110. The first conductive layer 121 includes a plurality of spaced-apart first conductive pillars 1211. A second conductive layer 122 is disposed above the first conductive layer 121. The second conductive layer 122 includes a plurality of spaced-apart second conductive pillars 1221. The first conductive layer and the second conductive layer include a first region 143a and a second region 143b. The first region 143a partially surrounds the second region 143b. A semiconductor bridge 130 is disposed within the second region 143b. A portion of the first conductive post 1211 located within the second region 143b is electrically connected to the semiconductor bridge 130 via a second connecting electrode 162. The semiconductor bridge 130 is electrically connected to the chip layer 200 via a third connecting electrode 163. At least a portion of the second conductive post 1221 within the first region 143a is electrically connected to the chip layer 200 via a first connecting electrode 161.

[0075] Optionally, a dielectric layer may be provided between adjacent first conductive pillars 1211 and between adjacent second conductive pillars 1221. The dielectric layer may be made of an insulating material, for example, photoresist, ABF (Ajinomoto Build-up Film), or NPI (Non-Photosensitive Polyimide).

[0076] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0077] The above embodiments merely illustrate several implementation methods of the present invention, and their descriptions are relatively specific and detailed, but they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.

Claims

1. A method for manufacturing a chip packaging structure, characterized in that, Includes the following steps: S101. A first substrate is provided, wherein the first substrate includes a stacked encapsulation substrate and a first conductive layer, and the first conductive layer includes a plurality of spaced first conductive pillars; S102. An anti-reflective layer is deposited on the surface of the first conductive layer away from the packaging substrate to obtain a second substrate, wherein the anti-reflective layer includes a plurality of anti-reflective portions spaced apart, and the orthographic projection of the anti-reflective portions on the packaging substrate overlaps with the orthographic projection of the first conductive post on the packaging substrate. S103. A first photoresist is coated and patterned on the surface of the second substrate away from the packaging substrate to obtain a third substrate. S104. A second conductive layer is prepared on the surface of the third substrate away from the packaging substrate, wherein the second conductive layer includes a plurality of spaced second conductive pillars, and the second conductive pillars are in direct contact with the first conductive pillars.

2. The chip packaging structure manufacturing method according to claim 1, characterized in that, The thickness of the anti-reflective layer is 100–300 nm. Preferably, the antireflective layer has a transmittance of less than 1% at a wavelength of 365nm and a reflectance of less than 5% at a wavelength of 365nm.

3. The chip packaging structure manufacturing method according to claim 1, characterized in that, Step S102 further includes: preparing a first electroplating solution, immersing the first substrate in the first electroplating solution, applying a voltage to the first substrate for electroplating for a period of time, and depositing an anti-reflection layer on the surface of the first conductive layer away from the packaging substrate. Preferably, the applied voltage is -0.5V to -2.0V; Preferably, the electroplating time is 30 to 120 seconds.

4. The chip packaging structure manufacturing method according to claim 3, characterized in that, The first electroplating solution includes: deionized water with a pH of 7-9, conductive salt, and light-absorbing dye; Preferably, the conductive salt is Na2SO4 or K2SO4, and the molar concentration of the conductive salt in the first electroplating solution is 0.1 to 0.5 mol / L; Preferably, the light-absorbing dye is Sudan Black or methyl orange, and the mass concentration of the light-absorbing dye in the first electroplating solution is 0.1–1 g / L; Preferably, the first electroplating solution further includes copper salt, and the mass concentration of the copper salt in the first electroplating solution is 0.01 to 0.1 g / L; Preferably, the copper salt is CuSO4·5H2O.

5. The chip packaging structure manufacturing method according to claim 3, characterized in that, The first electroplating solution comprises: a polymer matrix and a light-absorbing dye. Preferably, the polymer matrix is ​​selected from one of polyvinyl alcohol, polyacrylic acid, or polymethyl methacrylate copolymer; Preferably, the light-absorbing dye is one of Sudan Black, methyl orange, coumarin derivatives, or azo dyes.

6. The chip packaging structure manufacturing method according to any one of claims 1-4, characterized in that, Step S101 further includes: providing a packaging substrate, depositing a first conductive layer on the packaging substrate to obtain a first substrate; Preferably, step S101 further includes depositing a first conductive layer on the packaging substrate and then grinding and planarizing the side of the first conductive layer away from the packaging substrate to obtain the first substrate.

7. The chip packaging structure manufacturing method according to any one of claims 1-4, characterized in that, Step S103 further includes: coating a second photoresist layer on the surface of the second substrate away from the packaging substrate, exposing it through a mask, developing and removing a portion of the second photoresist layer and the anti-reflection portion to obtain the third substrate; the orthographic projection of the removed portion of the second photoresist layer on the packaging substrate covers at least a portion of the orthographic projection of the first conductive pillar on the packaging substrate.

8. The method for manufacturing a chip packaging structure according to any one of claims 1-4, characterized in that, Step S104 further includes: immersing the third substrate in the second electroplating solution to electroplat the second conductive layer; Preferably, step S104 further includes: the third substrate includes a first region and a second region, the first region is partially disposed around the second region, and after shielding the surface of the first conductive post in the second region on the side away from the packaging substrate, the third substrate is immersed in the second electroplating solution to electroplat the second conductive layer.

9. The method for manufacturing a chip packaging structure according to any one of claims 1-4, characterized in that, The third substrate includes a first region and a second region, with the first region partially surrounding the second region, and the orthographic projection of the second conductive post on the third substrate located within the first region. The manufacturing method further includes: S105. Electrically connecting the first conductive post located in the second region to a semiconductor bridge; Preferably, the manufacturing method further includes: S106. Electrically connecting the chip to the semiconductor bridge and / or the second conductive post.

10. A chip packaging structure, characterized in that, It is prepared by the chip packaging structure manufacturing method as described in any one of claims 1-9.