Method for manufacturing a packaging cover plate, packaging cover plate and thermal sensor

By forming a high-precision photoresist layer and getter layer on the encapsulation cover plate through spraying and evaporation/sputtering processes, the problem of poor shielding effect of the shielding layer is solved, and the sensitivity and stability of the thermal sensor are improved.

CN123165136APending Publication Date: 2026-11-24TRIPLE WIN TECH (SHENZHEN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510645601.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-20
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Traditional photoresist layer formation processes often result in poor shielding effects and difficulty in precisely controlling the position of the shielding layer when a shielding layer is placed within the groove. This affects the positional and patterning accuracy of the getter layer, which in turn affects the sensitivity and performance of the thermal sensor.

Method used

A photoresist layer is formed in the first area and the first groove of the encapsulation cover using a spraying process. A getter material is then applied using a vapor deposition or sputtering process. The notch and coverage of the photoresist layer are precisely controlled through the spraying process to form a high-precision getter layer.

Benefits of technology

It improves the coverage and positional accuracy of the photoresist layer, ensures the patterning accuracy of the getter layer, optimizes the specific thermal environment of the thermal sensor, reduces gas interference, and improves the sensitivity and stability of the thermal sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123165136A_ABST
    Figure CN123165136A_ABST
Patent Text Reader

Abstract

This application relates to the field of packaging technology, and more particularly to a method for preparing a packaging cover, a packaging cover, and a thermal sensor, comprising the following steps: providing a wafer, one surface of which includes a first region and a second region, the first region being disposed around the outside of the second region, and the second region being recessed to form a first groove; forming a photoresist layer in the first region and the first groove using a spray coating process, the photoresist layer having a notch that exposes at least a portion of the first region; disposing a getter material on the surface of the photoresist layer and within the notch to obtain a first getter layer and a second getter layer, the first getter layer being located within the notch and connected to the surface of the wafer, and the second getter layer being located on the surface of the photoresist layer; removing the photoresist layer and the second getter layer to obtain a packaging cover with a first getter layer. The packaging cover preparation method of this application provides a first getter layer that can optimize the specific thermal environment within the thermal sensor, thereby improving the sensitivity of the thermal sensor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of packaging technology, and in particular to a method for preparing a packaging cover, and a packaging cover and a thermal sensor. Background Technology

[0002] Fab manufacturing refers to the process in semiconductor factories that specializes in producing packaging covers for wafer-level packaging structures. Its core objective is to manufacture packaging covers with grooves and getter layers from wafers through high-precision machining.

[0003] In the field of thermal sensing, a package cover can be assembled with sensor elements and device wafers to form a sealed and miniaturized thermal sensor. The getter layer inside the thermal sensor maintains a specific thermal environment. When fabricating this getter layer, it is formed in a specific area of ​​the package cover. A masking layer with a specific pattern must first be placed on a portion of the wafer surface of the package cover to facilitate the subsequent formation of the getter layer and reduce damage to other areas caused by the getter layer formation process. However, traditional photoresist layer formation processes suffer from drawbacks when placing the masking layer within the groove, such as ineffective masking and difficulty in precisely controlling the masking position. These drawbacks affect the positional and patterning accuracy of the subsequent getter layer formation, thus impacting the thermal sensor's performance, such as sensitivity. Summary of the Invention

[0004] In view of this, this application provides a method for preparing a packaging cover, a packaging cover and a thermal sensor, which can improve at least one of the above-mentioned technical problems.

[0005] In a first aspect, this application provides a method for preparing a package cover, comprising the following steps: providing a wafer, one surface of which includes a first region and a second region connected together, the first region surrounding the outer side of the second region, and the second region recessed to form a first groove; forming a photoresist layer on the inner wall surface of the first region and the first groove using a spraying process, the photoresist layer having a notch, the notch being configured to expose at least a portion of the first region; distributing a getter material on the surface of the photoresist layer and within the notch to obtain a first getter layer and a second getter layer, wherein the first getter layer is located within the notch and connected to the surface of the wafer, and the second getter layer is located on the surface of the photoresist layer; removing the photoresist layer and the second getter layer to obtain a package cover having the first getter layer.

[0006] Compared to existing technologies, this application uses a spraying process to form a photoresist layer in the first region and the first groove. The spraying process can be carried out at multiple angles, which can effectively mask different positions on the inner wall of the first groove and the surface of the first region, resulting in better coverage of the photoresist layer. At the same time, it can precisely control the opening position and size of the notch on the photoresist layer, ensuring the positional and patterning accuracy when the first getter layer is set, and obtaining a first getter layer that meets the required performance parameters. The first getter layer can optimize the specific thermal environment inside the thermal sensor, reduce the interference of gas on the thermal sensor measurement, and thus improve the sensitivity of the thermal sensor.

[0007] In some embodiments, the wafer includes at least one of a silicon wafer, a glass wafer, or a ceramic wafer.

[0008] Wafers made of the aforementioned materials can meet the requirements of thermal sensors for thermal performance, environmental tolerance, and cost.

[0009] In some embodiments, the depth of the first groove is greater than 300 μm.

[0010] The depth of the first groove is within the aforementioned range, which allows for better accommodation of components such as sensor elements.

[0011] In some embodiments, forming a photoresist layer on the wall of the first region and the first groove using a spraying process includes: using at least one of the EVG150 series photoresist processing system, the EVG120 series photoresist processing system, and the EVG101 series photoresist processing system to spray and form a photoresist layer on the wall of the first region and the first groove.

[0012] Using the aforementioned high-precision spraying equipment, a photoresist layer with good coverage can be formed.

[0013] In some embodiments, the air-absorbing material is disposed on the surface of the photoresist layer and in the notch by means of depositing the air-absorbing material on the surface of the photoresist layer and in the notch using a vapor deposition process or a sputtering process.

[0014] Applying the gas-absorbing material using vapor deposition or sputtering processes results in better coverage, adhesion, and durability.

[0015] In some embodiments, the getter material includes at least one of Fe, Ni, and V.

[0016] Using the above-mentioned getter material, a first getter layer that meets production requirements can be obtained.

[0017] In some embodiments, removing the photoresist layer and the second getter layer includes: placing the wafer in a cleaning solution for ultrasonic cleaning to remove the photoresist layer and the second getter layer, wherein the cleaning solution includes at least one of isopropanol solution and acetone solution.

[0018] The photoresist layer can be removed by ultrasonic oscillation cleaning with the cleaning solution. Then, the second getter layer on the surface of the photoresist layer falls off along with the photoresist layer, leaving the required first getter layer on the wafer surface.

[0019] Secondly, this application provides a packaging cover, which is prepared using the packaging cover preparation method described in any one of the first aspects; One surface of the encapsulation cover includes a first region and a second region, the first region being disposed around the outside of the second region, and the second region being recessed to form a first groove; the encapsulation cover includes a first getter layer, the first getter layer being formed in the first region.

[0020] In some embodiments, the edge of the first region is provided with a protruding support layer and a bonding layer disposed on the support layer.

[0021] Thirdly, this application provides a thermal sensor, the thermal sensor including a device wafer, a sensor element and a packaging cover as described in the second aspect covering the device wafer, the sensor element being configured to be housed in a cavity formed by the packaging cover and the device wafer. Attached Figure Description

[0022] Figure 1 This is a schematic diagram of the structure of the encapsulation cover provided in this application.

[0023] Figure 2 A process diagram of the encapsulation cover provided in this application.

[0024] Figure 3 Another process diagram of the encapsulation cover provided in this application.

[0025] Explanation of key component symbols: 10. Encapsulation cover plate; 1. Wafer; 11. First region; 111. Second groove; 12. Second region; 121. First groove; 2. Photoresist layer; 21. Notch; 3. First getter layer; 4. Second getter layer; 5. Support layer; 6. Bonding layer. Detailed Implementation

[0026] The technical solutions of the embodiments of this application will be described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments.

[0027] To address the shortcomings of traditional photoresist layer 2 formation processes, such as ineffective shielding and difficulty in precisely controlling the shielding position when setting a shielding layer in the groove, this application provides a method for preparing an encapsulation cover plate 10, which obtains a photoresist layer 2 with better coverage through a spraying process.

[0028] In some embodiments, the thermal sensor includes a package cover 10, a device wafer, and a sensor element, wherein the package cover 10 and the device wafer are bonded together to form a cavity structure, and the sensor element is housed within the cavity to obtain the thermal sensor.

[0029] The encapsulation cover 10 of this application has a plate-like structure; please refer to... Figures 1-3 The surface of the encapsulation cover 10 facing the device wafer includes a first region 11 and a second region 12 connected to each other. The first region 11 is disposed around the outside of the second region 12. The second region 12 is recessed to form a first groove 121. At least a portion of the first region 11 is recessed to form a second groove 111. The first groove 121 and the second groove 111 are connected, and the second groove 111 is disposed around the first groove 121. It can be understood that the arrangement of the first groove 121 and the second groove 111 allows the encapsulation cover 10 and the device wafer to form a cavity structure to accommodate components such as sensor elements after assembly.

[0030] The encapsulation cover 10 also includes a first getter layer 3, a support layer 5, and a bonding layer 6. The first getter layer 3 is formed on the bottom surface of the second groove 111 along the thickness direction of the encapsulation cover 10. The first getter layer 3 chemically or physically adsorbs trace amounts of gases such as H2O, O2, H2, and CO2 remaining inside the cavity of the thermal sensor, optimizing the specific thermal environment inside the thermal sensor, reducing or even avoiding interference from gases on the sensor's heat conduction, oxidation, or electrical performance, thereby improving the sensitivity of the thermal sensor and ensuring the stability and reliability of the thermal sensor's operation. The support layer 5 is arranged around and protruding at the edge of the first region 11, providing a mounting base for the bonding layer 6 and improving the support stability of the bonding layer 6. The bonding layer 6 is disposed on the surface of the support layer 5 away from the first region 11. The bonding layer 6 achieves the sealing between the encapsulation cover 10 and the device wafer through bonding, isolating the sensor element from the influence of external environments such as humidity or dust.

[0031] Optionally, the thickness of the encapsulation cover 10 in this application can be 380 μm, the thickness of the support layer 5 can be 3 μm, and the first groove 121 and the second groove 111 of the wafer 1 are cylindrical. The depth of the first groove 121 is greater than 300 μm, and the depth of the second groove 111 is 5 μm. Specifically, the depth of the first groove 121 can be 301 μm, 305 μm, 310 μm, 315 μm, or 320 μm, or other values ​​within the range, which can be selected according to actual needs and are not limited here. It is understood that as the depth of the first groove 121 increases, the volume of the cavity of the thermal sensor also increases, which can better accommodate the sensor elements and other components. Furthermore, for the first groove 121 at this depth, this application uses a spray coating process to form the photoresist layer 2. Compared with the spin coating method, the spray coating process can better coat the wall area of ​​the first groove 121, and obtain a photoresist layer with good coverage in the first groove 121 at this depth.

[0032] The preparation method of the encapsulation cover 10 that meets the usage requirements of the first getter layer 3 includes the following steps: A wafer 1 is provided, and one surface of the wafer 1 includes a first region 11 and a second region 12 connected to each other. The first region 11 is disposed around the outside of the second region 12, and the second region 12 is recessed to form a first groove 121. A photoresist layer 2 is formed on the inner wall surface of the first region 11 and the first groove using a spraying process. The photoresist layer 2 has a notch 21, which is configured to expose at least a portion of the first region 11. A getter material is provided on the surface of the photoresist layer 2 and in the notch 21 to obtain a first getter layer 3 and a second getter layer 4. The first getter layer 3 is located in the notch 21 and connected to the surface of the wafer 1, and the second getter layer 4 is located on the surface of the photoresist layer 2. Remove the photoresist layer 2 and the second getter layer 4 to obtain the encapsulation cover plate 10 with the first getter layer 3.

[0033] The preparation method of the encapsulation cover 10 of this application is described below with reference to specific embodiments: Before step S10, there is also step S10', which cleans the surface of wafer 1. It can be understood that cleaning can ensure the surface of wafer 1 is clean and avoid particle or organic contamination from affecting the adhesion of the subsequent photoresist layer 2 and the first getter layer 3.

[0034] Step S10: A wafer 1 is provided. One surface of the wafer 1 includes a first region 11 and a second region 12 connected to each other. The first region 11 is disposed around the outside of the second region 12, and the second region 12 is recessed to form a first groove 121.

[0035] The wafer 1 used to fabricate the encapsulation cover 10 includes at least one of silicon wafers, glass wafers, or ceramic wafers. The material of the wafer 1 can be selected according to actual needs and is not limited here. It is understood that silicon wafer 1 has high thermal conductivity, glass wafer 1 can achieve high hermeticity encapsulation through anodic bonding, and ceramic wafer 1 has both high mechanical strength, chemical stability, and high temperature resistance. Selecting wafer 1 of the above materials can meet the requirements of thermal sensors for thermal performance, environmental tolerance, and cost.

[0036] In some embodiments, the first groove 121 may be formed by processes including but not limited to cutting or etching, and may be selected in combination with the groove depth, groove accuracy, wafer material and production cost of the first groove 121, and is not limited here.

[0037] Step S20, please refer to Figure 2 A photoresist layer 2 is formed on the inner wall surface of the first region 11 and the first groove 121 using a spraying process. The photoresist layer 2 has a notch 21, which is configured to expose at least a portion of the first region 11.

[0038] The equipment used in the spraying process can be at least one of the EVG150 series photoresist processing system, the EVG120 series photoresist processing system, and the EVG101 series photoresist processing system. The choice is based on actual needs and is not limited here. Using the aforementioned high-precision spraying equipment can form a photoresist layer 2 with good coverage, further improving the sensitivity of the thermal sensor.

[0039] It should be noted that this application does not limit the spraying pressure, spraying flow rate, or nozzle diameter in the spraying process. It is understood that spraying pressure affects the atomization degree of the photoresist material, thus affecting the coverage of the photoresist layer 2. Excessive spraying pressure leads to overly fine atomization of the photoresist material, easily forming an excessively thin photoresist layer 2 on wafer 1, resulting in insufficient coverage. Insufficient spraying pressure leads to insufficient atomization of the photoresist material, forming larger droplets, easily forming an uneven photoresist layer 2 on wafer 1, affecting coverage. The spraying flow rate directly affects the thickness of the photoresist layer 2. If the spraying flow rate is too high, a large amount of photoresist material will be sprayed out in a short time, resulting in excessively thick photoresist layer 2 in some areas of the wafer, affecting the uniformity of the photoresist layer 2 coverage. If the spraying flow rate is too low, the photoresist layer 2 will be too thin, unable to effectively cover the area to be masked, resulting in missed areas or incomplete coverage. The nozzle diameter affects the atomization effect and spraying pattern of the photoresist material. A larger diameter nozzle produces larger atomized particles, reducing the uniformity of the photoresist layer 2 coverage; a smaller diameter nozzle produces finer atomized particles, which can easily form an excessively thin photoresist layer 2 on wafer 1, resulting in insufficient coverage of the photoresist layer 2, requiring repeated spraying, and leading to low spraying efficiency. The spraying pressure, spraying flow rate, and nozzle diameter can be selected according to the type of photoresist material and the specifications of the wafer.

[0040] Step S30, please refer to Figure 3 A getter material is provided on the surface of the photoresist layer 2 and in the notch 21 to obtain a first getter layer 3 and a second getter layer 4. The first getter layer 3 is located in the notch 21 and connected to the surface of the wafer 1, and the second getter layer 4 is located on the surface of the photoresist layer 2.

[0041] The getter material can be deposited using either vapor deposition or sputtering. In vapor deposition, the getter material is heated above its melting point in a vacuum chamber using resistance heating or an electron beam, causing it to evaporate into gaseous atoms. These gaseous atoms condense into a solid film on the surface of the photoresist layer 2 away from the wafer 1 and within the notch 21, forming the first getter layer 3 and the second getter layer 4. In sputtering, a high-voltage electric field ionizes the gas in an inert gas environment to form plasma. This plasma bombards the surface of the getter material target, sputtering target atoms. These sputtered target atoms deposit on the surface of the photoresist layer 2 away from the wafer 1 and within the notch 21, forming the first getter layer 3 and the second getter layer 4. The deposition method can be selected based on actual needs. It is understandable that both vapor deposition and sputtering methods can produce a first getter layer 3 with good coverage, adhesion, and durability.

[0042] The getter material used in step S30 includes at least one of Fe, Ni, and V, which can be selected according to actual needs and is not limited here. It is understood that Fe, Ni, and V all have strong adsorption capacity, and by using the getter material of the above materials, the first getter layer 3 that meets the production requirements can be obtained.

[0043] Step S40: Remove the photoresist layer 2 and the second getter layer 4 to obtain... Figure 1 The encapsulation cover 10 shown has a first getter layer 3.

[0044] The photoresist layer 2 and the second getter layer 4 can place the wafer 1 in cleaning solutions such as isopropanol solution and acetone solution for ultrasonic cleaning. Through ultrasonic cleaning of the cleaning solution, the photoresist layer 2 can be removed without affecting the first getter layer 3. Then the second getter layer 4 on the surface of the photoresist layer 2 will fall off along with the photoresist layer 2, so that the surface of the wafer 1 retains the required first getter layer 3, achieving a highly efficient cleaning effect.

[0045] In steps S10 to S40 above, a photoresist layer 2 is formed on the wall surface of the first region 11 and the first groove 121 using a spraying process. The spraying process can be carried out at multiple angles, which can effectively mask different positions of the inner wall surface of the first groove 121 and the first region 11, resulting in better coverage of the photoresist layer 2. At the same time, the size and shape of the notch 21 are the size and pattern shape of the first getter layer 3 to be prepared later. By using the spraying process to precisely control the spraying process, the opening position and size of the notch 21 on the photoresist layer 2 can be precisely controlled, ensuring the positional accuracy and pattern accuracy when the first getter layer 3 is set later, and obtaining the first getter layer 3 that meets the required performance parameters. The first getter layer 3 can optimize the specific thermal environment inside the thermal sensor, reduce the interference of gas on the thermal sensor measurement, and thus improve the sensitivity of the thermal sensor.

[0046] Furthermore, those skilled in the art should recognize that the above embodiments are merely illustrative of this application and are not intended to limit this application. Any appropriate changes and variations made to the above embodiments within the essential spirit and scope of this application fall within the scope of this application's disclosure.

Claims

1. A method of making a package lid, comprising: Includes the following steps: ​ A wafer is provided, one surface of which includes a first region and a second region connected to each other, the first region being disposed around the outside of the second region, and the second region being recessed to form a first groove; A photoresist layer is formed on the inner wall of the first region and the first groove using a spraying process. The photoresist layer has a notch, which is configured to expose at least a portion of the first region. A getter material is disposed on the surface of the photoresist layer and in the notch to obtain a first getter layer and a second getter layer, wherein the first getter layer is located in the notch and connected to the surface of the wafer, and the second getter layer is located on the surface of the photoresist layer; Remove the photoresist layer and the second getter layer to obtain a packaging cover plate with the first getter layer.

2. The method of claim 1, wherein The wafer includes at least one of silicon wafers, glass wafers, or ceramic wafers.

3. The method of claim 1, wherein the method further comprises: The depth of the first groove is greater than 300 μm.

4. The method of claim 1, wherein Forming a photoresist layer on the wall surface of the first region and the first groove using a spraying process includes: At least one of the EVG150 series photoresist processing systems, the EVG120 series photoresist processing system, and the EVG101 series photoresist processing system is used to spray a photoresist layer onto the wall of the first region and the first groove.

5. The method of claim 1, wherein The air-absorbing material disposed on the surface of the photoresist layer and within the notch includes: The gas-absorbing material is deposited on the surface of the photoresist layer and inside the notch using a vapor deposition or sputtering process.

6. The method of claim 5, wherein the cover plate is prepared by the steps of: The getter material includes at least one of Fe, Ni, and V.

7. The method of claim 1, wherein Removing the photoresist layer and the second getter layer includes: The wafer is placed in a cleaning solution for ultrasonic cleaning to remove the photoresist layer and the second getter layer. The cleaning solution includes at least one of isopropanol solution and acetone solution.

8. A package lid, characterized by The encapsulation cover is prepared using the encapsulation cover preparation method according to any one of claims 1 to 7; One surface of the encapsulation cover includes a first region and a second region, the first region being disposed around the outside of the second region, and the second region being recessed to form a first groove; The encapsulation cover includes a first getter layer formed in the first region.

9. The package lid of claim 8, wherein, The edge of the first region is provided with a protruding support layer and a bonding layer disposed on the support layer.

10. A thermal sensor, characterized by The thermal sensor includes a device wafer, a sensor element, and a package cover as described in claim 9 covering the device wafer, wherein the sensor element is configured to be housed within a cavity formed by the package cover and the device wafer.