A core particle stack interconnection system and wafer level manufacturing method thereof
By employing a bonding-then-thinning process sequence and integrating decoupling capacitors and PMIC power management chips within the substrate, the manufacturing complexity and limited power distribution network performance issues in silicon interposer chip stacking interconnect schemes are resolved. This achieves efficient electromagnetic shielding and signal transmission, improving system power management and signal integrity.
Patent Information
- Application Number
- CN202611365259.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-03
- Publication Date
- 2026-11-24
AI Technical Summary
Existing silicon interposer stacked interconnect solutions suffer from problems such as complex manufacturing processes, limited power distribution network performance, poor high-frequency filtering effect of decoupling capacitors, long distance between power management functions and loads, complex thinning processes due to inconsistencies between TSV and groove depth, and lack of effective electromagnetic shielding between memory chips and logic chips.
The process adopts a bonding-then-thinning sequence. The interposer is aligned, bonded and fixed to the wafer at the wafer level. Then, the back side is ground and thinned to create a groove and expose the TSV in one go. Decoupling capacitors and/or PMIC power management chips are integrated. The redistribution layer inside the substrate is electrically connected to the TSV via nearby. The second functional chip is placed in the through channel to form an electromagnetic shielding structure.
It simplifies the manufacturing process, improves process yield, shortens the power distribution path, reduces parasitic parameters, and enhances signal integrity and electromagnetic shielding, meeting the storage bandwidth requirements of high-performance computing and AI training.
Smart Images

Figure CN123165145A_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present application relates to the field of semiconductor packaging, in particular to a core particle stacking interconnection system and a wafer-level manufacturing method thereof. BACKGROUND
[0002] Core particle heterogeneous integration technology realizes high-performance and high-bandwidth system-level integration by three-dimensional stacking and interconnection of multiple core particles with different functions and different process nodes, and has become an important technical path for continuing Moore's Law in the post-Moore era. Among them, the 2.5D / 3D packaging scheme based on silicon interposer is widely used in high-performance computing, artificial intelligence accelerator, high-end server chips and network processors, etc. due to its advantages such as good matching of thermal expansion coefficient between silicon-based material and core particle substrate, high interconnection density, and small signal transmission delay.
[0003] In a typical silicon interposer core particle interconnection scheme, multiple functional core particles (such as logic core particles and memory core particles) are arranged in a tiled or stacked manner above the interposer, signal interconnection between the core particles is realized through the redistribution layer (RDL) on the top of the interposer, and then the signal and power are introduced to the solder balls on the back of the interposer through the through-silicon via (TSV) penetrating the interposer, and finally mounted on a packaging substrate or printed circuit board. In recent years, in order to further improve the integration level and shorten the interconnection distance between core particles, the industry has begun to explore the vertical stacking of memory core particles and logic core particles, and to realize high-density signal transmission through vertical interconnection structures within the interposer.
[0004] However, the existing core particle stacking interconnection scheme based on silicon interposer still has obvious deficiencies in the following aspects: Firstly, it is difficult to operate in the groove in the manufacturing process, and the process window is narrow. In the traditional scheme, a groove is first etched on the surface of the interposer substrate, then the memory core particles are placed one by one into the groove, and then the bottom filling and interconnection alignment operations are completed in the limited space of the groove. The internal space of the groove is small, the alignment is difficult, the operation precision is high, which leads to narrow process window, low production efficiency and difficult to guarantee the yield. Especially when the groove aspect ratio is large or the number of grooves is large, the above problems are more prominent.
[0005] Secondly, the performance of the Power Distribution Network (PDN) is limited due to its long power supply path. As the operating frequency of the chips continues to increase and power consumption continues to rise, the power supply needs to be transmitted over long distances from the package substrate through the TSV and the RDL inside the interposer to each functional chip. The long power transmission path introduces large parasitic inductance and resistance, leading to increasingly prominent IR voltage drop and power supply noise problems, which seriously restricts the high-speed and stable operation of the chips. Especially when the data interface between logic chips and memory chips frequently switches, power supply noise can be coupled to the memory chips through the PDN, affecting their read / write reliability and signal integrity.
[0006] Third, the long distance between the decoupling capacitor and the load significantly reduces the high-frequency filtering effect. To suppress transient current spikes generated by the high-speed switching of the chip and high-frequency resonance in the PDN, decoupling capacitors are usually placed on the surface of the interposer or on the package substrate. However, due to space constraints, these decoupling capacitors often cannot be placed close to the load chip. The long connection path introduces additional parasitic inductance, which significantly weakens its filtering performance in the high-frequency range (>100MHz), resulting in high-frequency power supply noise not being effectively bypassed and affecting the power integrity of the system.
[0007] Fourth, the physical distance between the power management function and the main chip is relatively large, limiting power supply efficiency and dynamic response. In high-performance applications, the system needs to closely integrate the power management integrated circuit (PMIC) with the main chip to achieve local voltage regulation, dynamic power consumption management, and fast load response. In traditional solutions, the PMIC is usually placed on the package substrate or motherboard, and the power supply loop length between it and the load chip can be several millimeters or even centimeters. This not only occupies substrate area but also introduces additional power loss and PDN impedance, making it difficult to meet the requirements for power supply efficiency and dynamic response speed in high-current, low-voltage scenarios.
[0008] Fifth, the inconsistency between the TSV and the groove depth complicates the thinning process. During the interposer fabrication process, TSV formation and groove etching are typically performed separately at different depths, with the groove etching depth usually much smaller than the TSV depth. In subsequent back-side thinning processes, if the TSV and groove depths are inconsistent, it is difficult to simultaneously expose the bottom of the TSV and penetrate the bottom of the groove using a single chemical mechanical polishing (CMP) process. This often necessitates step-by-step thinning, multiple grinding operations, or additional over-polishing, increasing process complexity and defect risk. It also reduces the flatness of the back side of the interposer, which is detrimental to the subsequent fabrication of the redistribution layer.
[0009] Sixth, there is a lack of effective electromagnetic shielding between memory chips and logic chips. In a vertically stacked structure, the physical distance between memory chips and logic chips is relatively short. Electromagnetic interference generated by high-frequency digital signals can easily couple to the sensitive circuits of the memory chips, affecting their data retention characteristics and signal integrity, leading to an increase in the system bit error rate.
[0010] To address the shortcomings of existing technologies, this invention proposes a wafer-level manufacturing method and packaging structure for a chip stacked interconnect system. By employing a bonding-then-thinning process sequence, the interposer and the mother wafer are first aligned, bonded, and fixed at the wafer level. Then, grinding and thinning are performed from the back side to create a through-hole and expose the TSV, effectively simplifying the manufacturing process and improving yield. By integrating decoupling capacitors and / or PMIC power management chips within the substrate (interposer), local power supply and filtering are achieved, significantly shortening the power distribution path and reducing parasitic parameters. By placing a second functional chip (such as a storage chip) within the through-channel and ensuring it is completely surrounded by the substrate, the conductivity of silicon forms a natural electromagnetic shielding structure, improving the system's signal integrity. Summary of the Invention
[0011] This invention aims to overcome the problems in existing silicon interposer stack interconnect schemes, such as complex manufacturing process, limited power distribution network performance, poor high-frequency filtering effect of decoupling capacitors, long distance between power management function and load, complex thinning process due to inconsistency between TSV and groove depth, and lack of effective electromagnetic shielding between memory chips and logic chips.
[0012] To address the above problems, this invention provides a wafer-level manufacturing method for a chip-particle stacked interconnect system, comprising the following steps: S1: A substrate and a wafer are provided. A groove array is etched on the surface of the substrate. A through-silicon via (TSV) array is fabricated in the substrate. A decoupling capacitor and / or power management chip are integrated in the substrate and electrically connected to the TSV vias through a redistribution layer. A bonding layer and a first pad are formed on the surface of the substrate with groove openings and around the grooves. A plurality of first functional chips are pre-set on the wafer, and a second pad and a third pad are formed on the side of the wafer facing the substrate. S2: Align and bond the substrate with the surface having the groove opening toward the wafer, so that the first solder pad and the second solder pad are perpendicular to each other, and fix them through the bonding layer; S3: Grind and thin the bottom side of the substrate until the bottom of the groove and the through-silicon via are fully exposed, so that the groove forms a channel that runs through the surface and back of the substrate; S4: Provide a second functional chip, form a fourth bonding pad on the surface of the second functional chip, place it into the channel, so that the second functional chip is entirely located in the channel and surrounded by the substrate; fix the second functional chip to the wafer surface, so that the fourth bonding pad of the second functional chip is perpendicularly opposite to the third bonding pad of the first functional chip. S5: Deposit an insulating dielectric layer into the channel to fill the gap between the sidewall of the second functional core and the substrate, so that the back side of the insulating dielectric layer is flush with the exposed end face of the through silicon via; S6: Prepare a redistribution layer on the back side of the substrate, and electrically connect the redistribution layer to the bottom end of the through-silicon via and the pad of the second functional chip, respectively; fabricate conductive solder balls on the surface of the redistribution layer; provide a carrier board to electrically connect it to the conductive solder balls; S7: The composite wafer with completed wiring and solder ball preparation is diced and diced to obtain independent chip stacked interconnect packaging units.
[0013] Optionally, in step S1, the etching depth of the groove is less than the initial thickness of the substrate, the through-silicon via penetrates the substrate, and the bottom end face of the through-silicon via and the bottom end face of the groove are coplanar on the front side of the substrate.
[0014] Optionally, in step S1, the sidewall of the groove is a vertical sidewall or a stepped sidewall that slopes inward from the base surface toward the bottom of the groove, and the angle between the sidewall and the base surface is 85° to 90°.
[0015] Optionally, in step S2, after the substrate is bonded and fixed to the wafer, a metal microbump is formed between the vertically opposite first and second solder pads to achieve electrical interconnection.
[0016] Optionally, in step S4, after the second functional chip is fixed to the wafer surface, a metal microbump is formed between the vertically opposite fourth and third pads, and electrical interconnection is achieved through the metal microbump.
[0017] Optionally, in step S3, a chemical mechanical polishing process is used to complete the thinning treatment of the back side of the intermediate layer.
[0018] A chip-and-particle stacked interconnect system, manufactured by the above-described wafer-level fabrication method for chip-and-particle stacked interconnect systems, includes: A wafer, wherein a first functional chip is disposed on the wafer, and a second and a third bonding pad are disposed on the side of the wafer facing the substrate; A substrate is disposed above the wafer, and a channel is formed in the substrate that runs through its front and back sides. An array of through-silicon vias (TSVs) is provided within the substrate. Decoupling capacitors and / or power management chips are integrated within the substrate, and the decoupling capacitors and / or power management chips are electrically connected to the TSVs through a redistribution layer on the surface of the substrate. A bonding layer and a first bonding pad are provided on the side of the substrate facing the parent wafer. The substrate is bonded and fixed to the parent wafer through the bonding layer. The first bonding pad and a second bonding pad are perpendicularly opposite to each other and electrically interconnected. The channel contains a second functional chip, which is fixed to the wafer surface. The second functional chip has a fourth bonding pad, which is perpendicular to and electrically interconnected with the third bonding pad of the first functional chip. The second functional chip is completely surrounded by the substrate in the horizontal direction. The back side of the substrate is filled with an insulating dielectric layer, which fills the gap between the second functional chip in the channel and the substrate. The back side of the insulating dielectric layer is flush with the end face of the through silicon via. The substrate has a redistribution layer on its back side, which is connected to the through silicon via and the pads of the second functional chip, and the redistribution layer has conductive solder balls on its surface.
[0019] Optionally, the annular wall of the groove is provided with at least one narrow slit opening, the narrow slit opening penetrating the inner sidewall and the outer sidewall of the groove.
[0020] Optionally, the second functional chip is disposed on the wafer in a flip-chip manner, with its active surface facing the wafer, and the pads of the second functional chip are exposed on the wafer surface.
[0021] Optionally, there may be multiple second functional cores, which are stacked in multiple layers on top of the first functional cores in the vertical direction.
[0022] The present invention has at least the following beneficial effects: 1. This solution adopts a bonding-then-thinning process sequence. First, the interposer is aligned, bonded, and fixed to the wafer at the wafer level. Then, the back side is ground and thinned to open the groove and expose the TSV in one go. This effectively simplifies the manufacturing process and improves the process yield. At the same time, it avoids difficult operations such as bottom filling and interconnect alignment in the confined space of the groove, which greatly widens the process window and solves the problems of small internal space of the groove, high alignment difficulty, low production efficiency, and difficulty in guaranteeing yield in traditional solutions.
[0023] 2. This solution significantly shortens the power distribution path, reduces parasitic inductance and resistance, and effectively suppresses IR voltage drop and power supply noise by integrating decoupling capacitors and / or PMIC power management chips inside the substrate ring and electrically connecting them to TSV vias on the substrate surface through a redistribution layer. This solves the problems of long power supply paths and limited power distribution network performance in traditional solutions. At the same time, the decoupling capacitors and PMICs are placed close to the load chips, which significantly improves high-frequency filtering efficiency and power supply dynamic response speed, meeting the requirements for power supply efficiency and dynamic response speed in high-current and low-voltage scenarios.
[0024] 3. This solution places the second functional chip within the through-channel and completely surrounds it with the substrate. Utilizing the conductivity of silicon, a natural electromagnetic shielding structure is formed, effectively suppressing electromagnetic interference from high-frequency digital signals from coupling to the sensitive circuitry of the storage chip. This improves signal integrity and reduces the system's bit error rate. Especially when multiple second functional chips are stacked vertically, all horizontal sides of each layer of second functional chips are completely surrounded by the closed-loop structure of the interposer, providing overall electromagnetic shielding protection for the multi-layer stack.
[0025] 4. This solution uses 2-layer, 4-layer, or 8-layer HBM memory chips stacked vertically on top of the first functional chip, which can significantly increase storage capacity and bandwidth without increasing the horizontal package size, meeting the massive storage bandwidth requirements of high-performance computing and AI training. The second functional chip is set on the wafer in a flip-chip manner, with the active surface directly facing the third pad on the wafer surface. The vertical interconnect path is extremely short, the signal transmission delay is small, the parasitic capacitance is low, and the entire active surface can be used to arrange pads. The interconnect density is much higher than that of wire bonding, meeting the thousands of I / O requirements of high-bandwidth storage interfaces.
[0026] 5. This solution provides alternatives to C-shaped or U-shaped annular grooves. The openings can be used as heat dissipation airflow channels to improve the heat dissipation performance of the package, and reserve space for additional wiring. At the same time, the opening structure releases the thermomechanical stress generated by the closed-loop silicon ring during thermal cycling, improving package reliability and meeting the application scenarios with high heat dissipation requirements or additional wiring resources. By providing variant solutions that integrate only decoupling capacitors or only PMICs, it meets the flexible selection needs of cost-sensitive or space-constrained applications. Attached Figure Description
[0027] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0028] Figure 1This is a schematic diagram of the structure of the substrate provided in step S1 of embodiment one of the present invention; Figure 2 This is a schematic diagram of the structure of the wafer provided in step S1 of embodiment one of the present invention; Figure 3 This is a schematic diagram of the alignment and bonding structure of the substrate and the wafer in step S2 of embodiment one of the present invention; Figure 4 This is a schematic diagram of the structure for forming channels by thinning the substrate in step S3 of embodiment one of the present invention; Figure 5 This is a schematic diagram of the structure in step S4 of embodiment one of the present invention, in which the second functional core is placed into the channel; Figure 6 This is a schematic diagram of the structure in step S40 of an embodiment of the present invention, in which the first and second pads, as well as the third and fourth pads are interconnected by metal microbumps. Figure 7 This is a schematic diagram of the structure in step S5 of embodiment one of the present invention, in which an insulating dielectric layer is deposited into the channel; Figure 8 This is a schematic diagram of the structure of an independent chip stacked interconnect packaging unit in Embodiment 1 of the present invention; Figure 9 This is a schematic diagram of the structure with an open groove in Embodiment 3 of the present invention.
[0029] Icon labels: 10-Substrate; 11-Through Silicon Via; 12-Decoupling Capacitor; 13-First Bonding Pad; 14-Groove; 15-Channel; 20-Wafer; 21-First Functional Chip; 22-Second Bonding Pad; 23-Third Bonding Pad; 30-Bonding Layer; 40-Second Functional Chip; 41-Fourth Bonding Pad; 50-Metallic Microbump; 60-Dielectric Layer; 70-Carrier; 80-Conductive Solder Ball. Detailed Implementation
[0030] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and specific embodiments. It is to be understood that the specific embodiments described herein are merely illustrative of the invention and not intended to limit it. All other embodiments obtained by those skilled in the art based on the embodiments of this invention without inventive effort are within the scope of protection of this invention.
[0031] In the description of this invention, it should be understood that the terms "center", "longitudinal", "lateral", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.
[0032] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0033] Example 1
[0034] This invention provides a wafer-level 20-stage manufacturing method for a chip stacked interconnect system, comprising the following steps: S1: A substrate 10 and a wafer 20 are provided. An array of grooves 14 is etched on the surface of the substrate 10. An array of through-silicon vias 11 is formed in the substrate 10. A decoupling capacitor 12 and / or a power management chip are integrated in the substrate 10 and electrically connected to the through-silicon vias 11 through a redistribution layer. A bonding layer 30 and a first pad 13 are formed on the surface of the substrate 10 with the groove openings 14 and around the grooves 14. A plurality of first functional chips 21 are pre-set on the wafer 20, and a second pad 22 and a third pad 23 are formed on the side of the wafer 20 facing the substrate 10. refer to Figure 1As shown, a substrate 10 is provided, which is a single-crystal silicon substrate 10 as an interposer layer with a thickness of 725μm-775μm. Photoresist is coated on the surface of the substrate 10, and a photoresist mask with a groove pattern 14 is formed by exposure and development. The substrate 10 is etched using Bosch deep silicon etching technology, with SF6 as the etching gas and C4F8 as the passivation gas. The etching rate is controlled at 4μm / min-10μm / min, and the etching depth is 50μm-150μm (less than the initial thickness of the single-crystal silicon substrate 10), forming an array of grooves 14 on the surface of the substrate 10. The planar shape of each empty groove 14 is square or rectangular. The internal cavity size of the groove 14 is determined according to the size of the second functional chip 40 to be placed. In this embodiment, the groove size is 10μm-50μm larger than the planar size of the second functional chip 40 to allow for clearance in subsequent assembly. The sidewalls of the groove 14 are formed by process control to form vertical sidewalls or slightly inwardly inclined stepped sidewalls, and the angle between the sidewalls and the front of the substrate 10 is 85°-90°.
[0035] The vertical or slightly inwardly inclined sidewalls facilitate the smooth insertion of the second functional chip 40 into the channel 15 from the back, avoiding chip damage caused by jamming or sidewall collisions. The sidewall angle is controlled at 85°-90° to ensure the verticality of the channel 15, which is conducive to the uniform filling of the subsequent insulating dielectric layer 60 in the annular gap, while ensuring the electromagnetic shielding effect of the second functional chip 40 being completely surrounded by the substrate 10.
[0036] Next, in the area forming the groove 14, a TSV silicon via 11 is fabricated through the monocrystalline silicon substrate 10 using Bosch deep silicon etching technology.
[0037] Specifically, photoresist is recoated in the groove 14 area, and the through-silicon via (TSV) 11 pattern is formed by exposure and development. Deep silicon etching is then performed using the same Bosch process as described above until the vias completely penetrate the substrate 10. The TSV 11 has a diameter of 1μm-20μm and an aspect ratio of 10:1-30:1. After etching, the photoresist mask is removed.
[0038] Subsequently, an insulating layer, a barrier layer, and a seed layer are sequentially formed on the inner wall of the through-silicon via 11. The insulating layer is a silicon dioxide layer with a thickness of 0.1 μm to 1 μm grown by thermal oxidation. The barrier layer is Ti, TiN, or Ta with a thickness of 50 nm to 200 nm. The seed layer is copper with a thickness of 100 nm to 500 nm. Then, copper is filled into the through-silicon via 11 by electroplating. After annealing to eliminate internal stress, excess copper on the surface of the substrate 10 is removed by chemical mechanical polishing, so that the top of the through-silicon via 11 is flush with the front side of the substrate 10.
[0039] The TSV and the groove 14 have a coplanar bottom end face on the front side of the substrate 10, which allows the bottom end of the TSV and the bottom of the groove 14 to be exposed simultaneously in the back-side thinning process of the subsequent step S3 by a single CMP, without the need for step-by-step thinning, multiple grinding or additional over-polishing, reducing process complexity and defect risk, while obtaining a flat back side of the interposer layer, which is beneficial for the subsequent fabrication of the redistribution layer.
[0040] Next, on the surface of the substrate 10 in the groove 14 region, an atomic layer deposition process is used to sequentially deposit a lower electrode metal layer, a dielectric layer, and an upper electrode metal layer, forming a thin-film decoupling capacitor 12 with a metal-insulator-metal (MIM) structure through photolithography and etching. The decoupling capacitor 12 is electrically connected to the through-silicon via 11 through the redistribution layer on the surface of the substrate 10 to suppress high-frequency switching noise in the power distribution network.
[0041] Integration method of PMIC power management chip: A groove with a depth of 50μm-200μm is opened on the front or back of the substrate 10 in the groove 14 area. A pre-made PMIC power management chip with a thickness of 50μm-150μm is embedded in the groove. It is electrically connected to the redistribution layer on the surface of the substrate 10 through microbumps or conductive adhesive, and then fixed with epoxy resin.
[0042] Next, a redistribution layer (RDL) is fabricated on the front side of the substrate 10. This redistribution layer consists of alternating layers of insulating dielectric layers 60 with a thickness of 2μm-10μm and metal wiring layers with a thickness of 1μm-5μm. The insulating dielectric layer 60 can be made of polyimide, benzocyclobutene, or silicon dioxide; the metal wiring layers are made of copper. The RDL is used to interconnect the through-silicon vias 11, decoupling capacitors 12, and PMIC electrodes to predetermined pad locations on the front side of the substrate 10. On the surface of the substrate 10 where a groove 14 is formed, and in the area surrounding the groove 14, a first bonding pad 13 and a bonding layer 30 are formed to obtain an interposer layer. The positions of the first bonding pad 13 correspond one-to-one with the second bonding pad 22 on the subsequent wafer 20 in the vertical direction.
[0043] refer to Figure 2 As shown, a wafer 20 is provided, and a plurality of first functional chips 21 are formed on the wafer 20 using CMOS front-end process. The first functional chips 21 are logic main chips, including GPU, CPU or AI computing chips.
[0044] Subsequently, a bonding layer 30 and a second solder pad 22 are formed on the surface of wafer 20 facing the interposer (i.e., the front side), with the second solder pad 22 perpendicularly opposite to the first solder pad 13 on the substrate 10. The input / output pads of each first functional chip 21 are led out through the redistribution layer on the surface of wafer 20 to the corresponding second solder pad 22 position on the front side of wafer 20.
[0045] S2: Align and bond the surface of the substrate 10 with the opening of the groove 14 toward the wafer 20, so that the first solder pad 13 and the second solder pad 22 are perpendicular to each other, and are fixed by the bonding layer 30; refer to Figure 3 As shown, the surface of the substrate 10 with the opening of the groove 14 is aligned and bonded to the front side of the wafer 20.
[0046] Specifically, a wafer 20-level alignment device is used. By using alignment marks pre-set on the two wafers 20, the first pad 13 of the interposer layer and the second pad 22 of the wafer 20 are perpendicularly aligned one by one, and the alignment accuracy is controlled within ±1μm.
[0047] Under room temperature or low temperature conditions of 150℃-300℃, a bonding pressure of 0.5MPa-5MPa is applied to bond the bonding layer 30 of the interposer to the bonding layer 30 of the wafer 20 through intermolecular forces between dielectric materials (SiO2 or SiCN). After bonding, the interposer and the wafer 20 are permanently fixed through the bonding layer 30 dielectric, while a gap is maintained between the vertically opposite first pad 13 and second pad 22. This gap is determined by the thickness of the bonding layer 30, typically 0.1μm-2μm. At this time, no electrical connection is formed between the pads.
[0048] S3: Grind and thin the bottom side of the substrate 10 until the bottom of the groove 14 and the through-silicon via 11 are fully exposed, so that the groove 14 forms a channel 15 that runs through the surface and back of the substrate 10; refer to Figure 4 As shown, the bonded composite wafer 20 is flipped so that the back side of the interposer is facing up.
[0049] First, a coarse grinding process is used with a diamond grinding wheel at a speed of 2000rpm-5000rpm to mechanically grind the back of the interlayer, reducing the interlayer thickness from the initial 725μm-775μm to 200μm-300μm. Then, a fine grinding process is used to further thin it to approximately 20μm-50μm from the bottom of the groove 14.
[0050] Next, a chemical mechanical polishing (CMP) process is employed, using a polishing slurry composed of silica abrasive and cerium oxide, with the polishing pressure controlled at 1psi-5psi to eliminate surface stress and microcracks introduced by the grinding process. This process finely thins the back side of the interposer until the bottom of the groove 14 is completely removed, forming a through-hole channel 15 that connects both sides of the interposer. Simultaneously, the bottom end of the silicon via 11 is exposed on the back side of the interposer. After thinning, the final thickness of the interposer is 50μm-150μm.
[0051] CMP process can precisely control the thinning endpoint, expose the bottom of TSV and open the bottom of groove 14 in one go, and ensure that the two are coplanar; at the same time, it can eliminate the surface stress and microcracks introduced by coarse grinding and fine grinding, and obtain a flat and smooth back side, which is conducive to the subsequent deposition of insulating dielectric layer 60 and redistribution layer, improving signal integrity and process yield.
[0052] After thinning and opening, the back side of the exposed interposer is cleaned to remove silicon chips and polishing fluid residue generated during grinding and polishing.
[0053] S4: Provide a second functional chip 40, form a fourth bonding pad 41 on the surface of the second functional chip 40, place it into the channel 15, so that the second functional chip 40 is entirely located in the channel 15 and surrounded by the substrate 10; fix the second functional chip 40 to the surface of the wafer 20, so that the fourth bonding pad 41 of the second functional chip 40 is perpendicularly opposite to the third bonding pad 23 of the first functional chip 21; refer to Figure 5 As shown, a second functional chip 40 is provided, and the second functional chip 40 is inserted into each groove 14 from the back of the interposer layer. The second functional chip 40 is a memory chip, including HBM, DRAM, etc.
[0054] The second functional chip 40 has been prefabricated before insertion. Its surface facing the wafer 20 is provided with a fourth solder pad 41 and a bonding layer 30. The position of the fourth solder pad 41 is opposite to the position of the third solder pad 23 corresponding to the first functional chip 21 on the wafer 20.
[0055] Using a pick-and-place device, the second functional chip 40 is placed one by one from the back side into the corresponding channel 15, with the surface of the second functional chip 40 facing the front side of the wafer 20. The second functional chip 40 is bonded and fixed to the surface of the wafer 20 by the bonding layer 30 on the bottom surface of the second functional chip 40. The bonding temperature is 150℃-300℃, and the bonding pressure is 0.5MPa-5MPa, thus fixing the second functional chip 40 to the wafer 20. After fixing, the fourth pad 41 of the second functional chip 40 is perpendicular to the third pad 23 corresponding to the first functional chip 21, and a gap is maintained between them. This gap is determined by the thickness of the bonding layer 30, which is usually 0.1μm-2μm. At this time, no electrical connection has been formed.
[0056] The planar dimensions of the second functional core 40 are smaller than the inner cavity dimensions of the groove 14. The second functional core 40 is entirely housed within the channel 15, and all its horizontal sides are completely surrounded by the closed-loop annular structure of the intermediate layer. A 5μm-25μm annular gap is maintained between the sidewall of the second functional core 40 and the inner wall of the intermediate layer ring, without any sidewall bonding.
[0057] The second functional chip 40 is flip-chip mounted on the wafer 20, with its active surface facing the wafer 20. The fourth bonding pad 41 is disposed on the active surface of the second functional chip 40, and after fixing, the fourth bonding pad 41 is perpendicularly opposite to the third bonding pad 23 on the surface of the wafer 20. The pads of the second functional chip 40 are interconnected with the third bonding pad 23 on the surface of the wafer 20 via the bottom of the channel 15, forming the electrical lead-out structure of the flip chip.
[0058] The second functional chip 40 is flip-chip mounted on the wafer 20, with its active surface directly facing the third pad 23 on the surface of the wafer 20. The vertical interconnect path is extremely short (only 2μm-20μm in height for the microbumps), resulting in low signal transmission delay and low parasitic capacitance, meeting the requirements for high-frequency and high-speed signal transmission. Pads can be arranged on the entire active surface, and the interconnect density is much higher than that of wire bonding, meeting the thousands of I / O requirements of high-bandwidth memory interfaces (such as HBM). The back side of the second functional chip 40 is exposed on the top of the channel 15, facilitating subsequent heat sink mounting and improving heat dissipation performance.
[0059] After step S4, the method further includes: after the second functional chip 40 is fixed to the surface of the wafer 20, a metal microbump 50 is formed between the vertically opposite fourth pad 41 and the third pad 23, and electrical interconnection is achieved through the metal microbump 50; after the substrate 10 is bonded and fixed to the wafer 20, a metal microbump 50 is formed between the vertically opposite first pad 13 and the second pad 22, and electrical interconnection is achieved through the metal microbump 50.
[0060] For details, please refer to Figure 6 As shown, the composite wafer 20, after bonding the second functional core 40, is immersed in an activation solution to selectively activate the exposed surfaces of the first bonding pad 13, the second bonding pad 22, the third bonding pad 23, and the fourth bonding pad 41. The activation solution can be a palladium salt solution (such as a PdCl2 / HCl system). Palladium ions undergo a displacement reaction on the copper surface, forming catalytic active centers, so that the chemical plating reaction occurs selectively only on the conductive bonding pad surface, while the insulating bonding layer 30 surface does not undergo a chemical plating reaction.
[0061] Next, the activated composite wafer 20 is immersed in a chemical plating solution. A self-aligned selective deposition of metal layers is performed simultaneously on the opposite sides of the first pad 13 and the second pad 22, and on the opposite sides of the fourth pad 41 and the third pad 23. The chemical plating solution can be a copper plating solution or a nickel plating solution. When using copper plating, the solution composition is copper sulfate, EDTA complexing agent, formaldehyde reducing agent, and stabilizer, with the pH controlled at 12-13 and the solution temperature controlled at 40℃-60℃. When using nickel plating, the solution composition is nickel sulfate, sodium hypophosphite reducing agent, and complexing agent, with the pH controlled at 4-6 and the solution temperature controlled at 80℃-90℃.
[0062] During the electroless plating process, metal layers are simultaneously deposited and grown on the surfaces of the vertically opposite first pad 13 and second pad 22, as well as on the surfaces of the fourth pad 41 and third pad 23. As the deposition time increases, the metal layers grown on both sides of each pad pair gradually approach each other in the gap and eventually fuse to form a complete metal microbump 50, electrically connecting the vertically opposite pad pairs. Because electroless plating has self-alignment characteristics, the plating layer grows only on the pad surface and not on the bonding layer 30 surface, thus achieving selective synchronous interconnection between all pad pairs without the need for a photolithography mask.
[0063] The height of the metal microbumps 50 is determined by the gap size between the pad pairs and the thickness of the bonding layer 30, with a typical height of 2μm-20μm. The gap size between each pad pair is 0.1μm-2μm, and this gap is completely filled by the metal layer after electroless plating growth.
[0064] A selective electroless plating self-alignment process is adopted to simultaneously form metal microbumps 50 between all vertically opposite pad pairs in the same electroless plating step. The plating layer grows only on the surface of the conductive pads, without the need for photolithography masks, additional photolithography and etching processes, and avoids the thermal stress effect of high-temperature reflow soldering on the bonded interface. Moreover, all pad pairs can form electrical interconnections in batches and in parallel in the plating solution, which significantly reduces manufacturing costs and improves production efficiency. At the same time, the electroless plating solution can freely penetrate into the pad area through the 5μm-25μm annular gap between the sidewall of the second functional core 40 and the inner wall of the intermediate layer ring, without generating parasitic deposition on the surface of the insulating sidewall, and has excellent adaptability to narrow spaces with high aspect ratio.
[0065] After the chemical plating is completed, the composite wafer 20 is cleaned and dried.
[0066] S5: Deposit an insulating dielectric layer 60 into the channel 15 to fill the gap between the sidewall of the second functional core 40 and the substrate 10, so that the back side of the insulating dielectric layer 60 is flush with the exposed end face of the through silicon via 11. refer to Figure 7 As shown, an insulating dielectric layer 60 is deposited inside the channel 15 to fill the annular gap between the sidewall of the second functional core 40 and the inner wall of the intermediate layer ring, as well as the gap between the second functional core 40 and the wafer 20.
[0067] The material of the insulating dielectric layer 60 is selected from epoxy resin, polyimide (PI) or silicon dioxide insulating dielectric.
[0068] Specifically, when epoxy resin is selected, liquid epoxy resin is evenly coated on the back of the intermediate layer using spin coating, spraying or molding processes, so that the epoxy resin can fully flow into all the gaps in the through window, and then cured at 150℃-200℃ for 1h-4h.
[0069] When polyimide is selected, the polyimide precursor solution is coated by spin coating and then imidized by step temperature increase curing (80℃ / 1h, 150℃ / 1h, 250℃ / 1h, 350℃ / 1h).
[0070] When silicon dioxide is selected, a silicon dioxide dielectric layer 60 is deposited using the PECVD process.
[0071] The insulating dielectric layer 60 is continuously deposited until its back side is slightly higher than the exposed bottom end face of the through-silicon via 11 (approximately 5μm-20μm thick). Subsequently, a chemical mechanical polishing (CMP) process is used to planarize the back side of the insulating dielectric layer 60, making it flush with the exposed bottom end face of the through-silicon via 11, forming a flat and coplanar composite back side. The CMP polishing pressure is controlled between 1psi and 5psi to ensure no damage to the end face of the through-silicon via 11.
[0072] S6: A redistribution layer is prepared on the back side of the substrate 10, and the redistribution layer is electrically connected to the bottom end of the through-silicon via 11 and the pad of the second functional chip 40, respectively; conductive solder balls are prepared on the surface of the redistribution layer; a carrier board 70 is provided so as to be electrically connected to the conductive solder balls. refer to Figure 8 As shown, a metal redistribution layer is prepared on the back side of the planarized interposer.
[0073] First, an insulating dielectric layer 60 is deposited on the back side of the composite substrate. Contact holes are then created at the locations of the bottom ends of the TSV vias 11 and the lead-out pads of the second functional chip 40 using photolithography and etching processes. Next, a Ti / Cu seed layer is sputtered or copper is electroplated to deposit a metal layer with a total thickness of 2μm-10μm. Metal interconnects are then formed through photolithography and etching. The above steps can be repeated as needed to form a multi-layer redistribution structure (e.g., 2-4 layers) to meet complex wiring requirements.
[0074] The metal redistribution layer forms an electrical connection with the bottom end of the through silicon via 11 and the lead-out pad of the second functional chip 40.
[0075] Conductive solder balls, such as solder balls or copper core balls, with a diameter of 100μm-300μm are made on the outermost layer of the metal redistribution layer. The solder ball material can be selected from lead-free solder alloys such as SnAg and SnAgCu.
[0076] Through ball-mounting processes, such as solder paste printing, reflow soldering, or ball placement and reflow soldering, conductive solder balls are fixed on the pads on the surface of the metal redistribution layer. The peak temperature of the reflow soldering is controlled at 230℃-260℃, enabling the electrical leads of the package to be exposed to the outside.
[0077] S7: The composite wafer 20, after wiring and solder ball preparation, is diced to obtain independent chip stacked interconnect packaging units.
[0078] refer to Figure 8 As shown, the composite wafer 20, after wiring and solder ball fabrication, is diced. A diamond blade or laser cutting process is used to perform a full cut along the dicing path between adjacent packaging units, separating the composite wafer 20 array into several independent chip stacked interconnect packaging units.
[0079] After cutting, the packaging units are cleaned and inspected to obtain independent chip stacked interconnect packaging units.
[0080] By adopting a process sequence of bonding first and then thinning, the interposer layer and wafer 20 are first aligned, bonded and fixed at wafer 20 level, and then the back side is ground and thinned to open up the groove 14 and expose the TSV in one go. This effectively simplifies the manufacturing process and improves the process yield. At the same time, it avoids difficult operations such as bottom filling and interconnect alignment in the limited space of groove 14, and greatly widens the process window.
[0081] The present invention also provides a chip stacking interconnect system, manufactured by the above-described wafer 20-level manufacturing method for chip stacking interconnect systems, comprising: Wafer 20, on which a first functional chip 21 is disposed, and a second bonding pad 22 and a third bonding pad 23 are disposed on the side of the wafer 20 facing the substrate 10; A substrate 10 is disposed above the wafer 20. A channel 15 is formed in the substrate 10, penetrating its front and back sides. An array of through-silicon vias 11 is provided within the substrate 10. Decoupling capacitors 12 and / or power management chips are integrated within the substrate 10. The decoupling capacitors 12 and / or power management chips are electrically connected to the through-silicon vias 11 through a redistribution layer on the surface of the substrate 10. A bonding layer 30 and a first bonding pad 13 are provided on the side of the substrate 10 facing the parent wafer 20. The substrate 10 is bonded and fixed to the parent wafer 20 through the bonding layer 30. The first bonding pad 13 and the second bonding pad 22 are perpendicularly opposite to each other and electrically interconnected. The channel 15 contains a second functional chip 40, which is fixed to the surface of the wafer 20. The second functional chip 40 has a fourth bonding pad 41, which is perpendicular to and electrically interconnected with the third bonding pad 23 of the first functional chip 21. The second functional chip 40 is completely surrounded by the substrate 10 in the horizontal direction. The back side of the substrate 10 is filled with an insulating dielectric layer 60, which fills the gap between the second functional core 40 and the substrate 10 in the channel 15. The back side of the insulating dielectric layer 60 is flush with the end face of the through silicon via 11. A redistribution layer is provided on the back side of the substrate 10. The redistribution layer is electrically connected to the through-silicon via 11 and the pads of the second functional chip 40. Conductive solder balls are provided on the surface of the redistribution layer. 80 Example 2 The difference between this embodiment and Embodiment 1 is that there are multiple second functional chips 40, such as 2-layer, 4-layer or 8-layer HBM memory chips, and multiple second functional chips 40 are stacked in multiple layers on top of the first functional chip 21 in the vertical direction.
[0082] Vertical interconnection is achieved between the second functional cores 40 of each layer through hybrid bonding.
[0083] Specifically, the top surface of the lower second functional core 40 is provided with conductive pads and a bonding layer 30, and the bottom surface of the upper second functional core 40 is provided with corresponding conductive pads and a bonding layer 30. The two are thermo-press bonded at 150℃-300℃ and 0.5MPa-5MPa to achieve vertical electrical interconnection. The pad pairs between the second functional cores 40 can also be interconnected by growing metal microbumps 50 using a chemical plating process, or by using direct copper-copper diffusion bonding.
[0084] The total height of the multilayer secondary functional core 40 is 50μm-400μm. The depth of the annular hollow groove 14 of the intermediary layer and the thickness of the final intermediary layer are adjusted accordingly based on the total height of the multilayer stack to ensure that all secondary functional cores 40 are contained within the channel 15, and that all horizontal sides of each layer of secondary functional cores 40 are completely surrounded by the closed-loop annular structure of the intermediary layer.
[0085] The power supply and signal transmission paths of each layer of second functional chip 40 are as follows: the first functional chip 21 is connected to the bottommost second functional chip 40, and the two are electrically interconnected through vertical hybrid bonding or metal microbumps 50; the second functional chips 40 of each layer are electrically interconnected through vertical hybrid bonding or microbumps; the lead-out pads of the second functional chip 40 are connected to the redistribution layer on the back of the interposer, and then connected to the through silicon via 11 through the redistribution layer, and finally connected to the wafer 20 through the through silicon via 11.
[0086] Power supply can be locally decoupled and regulated through the decoupling capacitor 12 and / or power management chip integrated inside the intermediate layer ring to suppress the increased power noise caused by multilayer stacking.
[0087] By stacking 2-layer, 4-layer, or 8-layer HBM memory chips vertically above the first functional chip 21, the storage capacity and bandwidth can be significantly increased without increasing the horizontal package size (such as achieving a 1024-bit wide data bus), meeting the massive storage bandwidth requirements of high-performance computing and AI training. All horizontal sides of the second functional chips 40 in each layer are completely surrounded by the closed-loop ring structure of the interposer layer, and the entire multi-layer stack is electromagnetically shielded. Multi-layer stacking brings greater transient current and power supply noise, but the increased power supply noise caused by multi-layer stacking can be effectively suppressed by local decoupling and adjustment through the decoupling capacitor 12 and / or PMIC integrated inside the interposer ring.
[0088] Example 3
[0089] refer to Figure 9 As shown, the difference between this embodiment and Embodiment 1 is that the groove formed by etching in step S1 is not a completely closed "U"-shaped square ring, but has one or more narrow slit openings on the ring wall of the groove. The narrow slit openings penetrate the inner and outer sidewalls of the groove, and the width of the openings is 50μm-500μm. These narrow slit openings only cut off a local section of the sidewall of the ring, and the silicon solid portions at both ends of the sidewall are still retained, rather than removing the entire sidewall. The narrow slit openings of each annular groove in the array are independent of each other, and adjacent annular grooves are completely isolated by the interposer silicon substrate. The windows are not interconnected through the openings. These narrow slit openings are used to reserve space for subsequent wiring, stress relief, or heat dissipation channels.
[0090] In the subsequent insulating medium deposition and filling process, the insulating medium will simultaneously fill the gap space of the narrow slit opening. In the packaged finished product state, the inside of the narrow slit opening is completely filled with the insulating medium, and there is no cavity inside the package.
[0091] In the final package structure, the horizontal side of the second functional chip is surrounded by a ring structure of the interposer, meaning most of the side is covered by the silicon ring, with only a small section corresponding to the narrow slot opening uncovered by silicon sidewalls. Electrical connections at the narrow slot opening of the interposer ring can be supplemented by additional metal bridging structures or substrate wiring. The metal bridging structure involves the redistribution layer on the back of the interposer crossing the narrow slot opening after the insulating medium is filled, extending into the window to achieve interconnection. The substrate wiring involves the redistribution layer on the mother wafer surface extending into the window along the vertical projection of the narrow slot opening to complete signal extraction. The main power supply and signal paths within the window still primarily rely on the TSV (Through Silicon Via) array inside the silicon ring.
[0092] This embodiment is suitable for applications with high heat dissipation requirements or those requiring additional wiring resources. Regarding heat dissipation, the narrow slit opening before dielectric filling forms a gas flow channel; after dielectric filling, the insulating dielectric within the opening forms a lateral heat conduction path, transferring heat from the chip sidewalls to the interposer silicon substrate. Since most of the horizontal sides of the second functional chip are still surrounded by a silicon ring, the through-silicon vias and the power devices integrated within the ring can still provide sufficient power supply and signal transmission channels, resulting in superior performance compared to a pure flat-layout solution.
[0093] The groove 14 adopts an annular structure with one or more narrow slit openings. The openings can form heat dissipation channels to improve the heat dissipation performance of the package. Space is reserved for additional wiring, and additional metal bridging structures or substrate wiring can be set at the openings to supplement electrical connections. At the same time, the openings interrupt the continuity of the closed-loop silicon ring, release the thermomechanical stress generated by the closed-loop silicon ring in thermal cycling, and improve the reliability of the package. Meanwhile, most of the horizontal sides of the second functional chip are still surrounded by the silicon ring, and its main electromagnetic shielding and local power supply performance are still better than the pure flat solution.
[0094] In other embodiments, narrow slit openings can be made on the two opposing side walls of the same annular groove 14 to further enhance stress release and heat dissipation capabilities. However, this will expand the electromagnetic shielding failure area and reduce the area of silicon rings on which TSVs can be arranged. This is suitable for scenarios with high stress and high tolerance for electromagnetic shielding.
[0095] Example 4
[0096] The difference between this embodiment and Embodiment 1 is that this embodiment provides a variant solution that integrates only decoupling capacitors or only PMIC power management chips.
[0097] For cost-sensitive or space-constrained applications, decoupling capacitors can be integrated inside the intermediate layer ring without integrating the PMIC (or vice versa).
[0098] Integrated decoupling capacitors only: A thin-film decoupling capacitor array with a MIM structure is fabricated inside the ring, without setting up embedding grooves for the PMIC. This solution is suitable for scenarios where power management is already completed by external circuitry and only local high-frequency decoupling is required, which can reduce the manufacturing cost and process complexity of the interposer layer.
[0099] Integrated PMIC only: Only the PMIC power management chip is embedded inside the ring, without fabricating decoupling capacitors. This solution is suitable for scenarios that require local voltage regulation and power management but have relatively low requirements for high-frequency noise suppression.
[0100] In both schemes, the integrated single-type power devices are electrically connected to TSV vias through the redistribution layer on the surface of the interposer to achieve local power supply.
[0101] The above description is merely an embodiment of this application and does not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, such as the combination of technical features between embodiments, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.
Claims
1. A wafer-level manufacturing method for a chip-particle stacked interconnect system, characterized in that, Includes the following steps: S1: A substrate and a wafer are provided. A groove array is etched on the surface of the substrate. A through-silicon via (TSV) array is fabricated in the substrate. A decoupling capacitor and / or power management chip are integrated in the substrate and electrically connected to the TSV vias through a redistribution layer. A bonding layer and a first pad are formed on the surface of the substrate with groove openings and around the grooves. A plurality of first functional chips are pre-set on the wafer, and a second pad and a third pad are formed on the side of the wafer facing the substrate. S2: Align and bond the substrate with the surface having the groove opening toward the wafer, so that the first solder pad and the second solder pad are perpendicular to each other, and fix them through the bonding layer; S3: Grind and thin the bottom side of the substrate until the bottom of the groove and the through-silicon via are fully exposed, so that the groove forms a channel that runs through the surface and back of the substrate; S4: Provide a second functional chip, form a fourth bonding pad on the surface of the second functional chip, place it into the channel, so that the second functional chip is entirely located in the channel and surrounded by the substrate; fix the second functional chip to the wafer surface, so that the fourth bonding pad of the second functional chip is perpendicularly opposite to the third bonding pad of the first functional chip. S5: Deposit an insulating dielectric layer into the channel to fill the gap between the sidewall of the second functional core and the substrate, so that the back side of the insulating dielectric layer is flush with the exposed end face of the through silicon via; S6: Prepare a redistribution layer on the back side of the substrate, and electrically connect the redistribution layer to the bottom end of the through-silicon via and the pad of the second functional chip, respectively; fabricate conductive solder balls on the surface of the redistribution layer; Provide a carrier plate for electrical connection with the conductive solder balls; S7: The composite wafer with completed wiring and solder ball preparation is diced and diced to obtain independent chip stacked interconnect packaging units.
2. The method as described in claim 1, characterized in that, In step S1, the etching depth of the groove is less than the initial thickness of the substrate, the through-silicon via penetrates the substrate, and the bottom end face of the through-silicon via and the bottom end face of the groove are coplanar on the front side of the substrate.
3. The method as described in claim 1, characterized in that, In step S1, the sidewall of the groove is a vertical sidewall or a stepped sidewall that slopes inward from the base surface toward the bottom of the groove, and the angle between the sidewall and the base surface is 85° to 90°.
4. The method as described in claim 1, characterized in that, In step S2, after the substrate is bonded and fixed to the wafer, metal microbumps are formed between the vertically opposite first and second solder pads, and electrical interconnection is achieved through the metal microbumps.
5. The method as described in claim 1, characterized in that, In step S4, after the second functional chip is fixed to the wafer surface, a metal microbump is formed between the vertically opposite fourth and third pads, and electrical interconnection is achieved through the metal microbump.
6. The method as described in claim 1, characterized in that, In step S3, a chemical mechanical polishing process is used to thin the back side of the intermediate layer.
7. A chip stack interconnect system, characterized in that, The wafer-level fabrication method of the chip stacked interconnect system according to any one of claims 1 to 6 is used to manufacture the system, comprising: A wafer, wherein a first functional chip is disposed on the wafer, and a second and a third bonding pad are disposed on the side of the wafer facing the substrate; A substrate is disposed above the wafer, and a channel is formed in the substrate that runs through its front and back sides. An array of through-silicon vias (TSVs) is provided within the substrate. Decoupling capacitors and / or power management chips are integrated within the substrate, and the decoupling capacitors and / or power management chips are electrically connected to the TSVs through a redistribution layer on the surface of the substrate. A bonding layer and a first bonding pad are provided on the side of the substrate facing the parent wafer. The substrate is bonded and fixed to the parent wafer through the bonding layer. The first bonding pad and a second bonding pad are perpendicularly opposite to each other and electrically interconnected. The channel contains a second functional chip, which is fixed to the wafer surface. The second functional chip has a fourth bonding pad, which is perpendicular to and electrically interconnected with the third bonding pad of the first functional chip. The second functional chip is completely surrounded by the substrate in the horizontal direction. The back side of the substrate is filled with an insulating dielectric layer, which fills the gap between the second functional chip in the channel and the substrate. The back side of the insulating dielectric layer is flush with the end face of the through silicon via. The substrate has a redistribution layer on its back side, which is connected to the through silicon via and the pads of the second functional chip, and the redistribution layer has conductive solder balls on its surface.
8. The chip stack interconnect system as claimed in claim 1, characterized in that, The groove has at least one narrow slit opening on its annular wall, the narrow slit opening penetrating the inner and outer walls of the groove.
9. The chip stack interconnect system as claimed in claim 1, characterized in that, The second functional chip is flip-chip disposed on the wafer with its active surface facing the wafer and the pads of the second functional chip exposed on the wafer surface.
10. The chip stack interconnect system as claimed in claim 1, characterized in that, The second functional core is multiple and is stacked in multiple layers on top of the first functional core in a vertical direction.