Process for forming a synthesis gas and process for forming hydrocarbons using a synthesis gas
By mixing hydrogen and carbon dioxide during the preheating process of the feed gas in the reverse water gas shift reactor, and by adding steam and corrosion inhibitors to the heater and using corrosion-resistant alloy materials, the metal corrosion problem of the preheater equipment and pipelines has been solved, thereby improving the durability and production efficiency of the equipment.
Patent Information
- Application Number
- CN202580028771.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-05-09
- Filing Date
- 2025-02-14
- Publication Date
- 2026-11-24
AI Technical Summary
In the prior art, the preheating process of the feed gas in the reverse water gas shift reactor may cause metal corrosion and damage to the preheater equipment and pipelines. Especially under high temperature conditions, the reactivity of the mixed gas increases, resulting in a shortened equipment life and an increase in downtime.
By mixing and heating the feed gases of hydrogen and carbon dioxide to at least 400°C in a heater, and adding steam and corrosion inhibitors before they enter the heater, using corrosion-resistant nickel-chromium alloy materials, and controlling the feed gas pressure to below 20 bar, metal corrosion is reduced.
It effectively reduces metal corrosion in heaters and connecting pipes, improves equipment durability and production efficiency, and reduces equipment maintenance costs.
Smart Images

Figure CN123165352A_ABST
Abstract
Description
Technical Field
[0001] This specification relates to methods and systems for forming a synthesis gas (syngas) comprising carbon monoxide and hydrogen, and methods and systems for producing hydrocarbons from the synthesis gas. Background Technology
[0002] The Fischer-Tropsch process converts a mixture of carbon monoxide and hydrogen into liquid hydrocarbons. These reactions occur in the presence of a metal catalyst, typically at temperatures ranging from 150°C to 300°C and pressures from one atmosphere to tens of atmospheres. The Fischer-Tropsch process involves a series of chemical reactions that produce a variety of hydrocarbons, ideally possessing the formula (C...). n H 2n+2 A more useful reaction produces the following alkanes:
[0003] (2n+1)H2 + nCO → C n H 2n+2 +nH2O
[0004] Where n can be 1 to 100 or higher. The formation of methane (n=1) is undesirable. In addition to alkane formation, the competing reaction also produces small amounts of alkenes, as well as alcohols and other oxidized hydrocarbons. The Fischer-Tropsch reaction is highly exothermic because the combined reaction has a standard enthalpy of reaction (ΔH) of -165 kJ / mol CO.
[0005] Syngas fed into the Fischer-Tropsch process can be produced from a variety of feedstocks. For example, natural gas can be obtained through steam reforming and / or autothermal reforming, municipal solid waste and biomass can be obtained through high-temperature gasification, or carbon dioxide and hydrogen can be obtained through a reverse water-gas shift reaction. The reverse water-gas shift reaction can be described as follows:
[0006]
[0007] Using reverse water gas shift reaction to generate syngas may be beneficial because it utilizes carbon dioxide that would otherwise be emitted into the atmosphere.
[0008] WO2022079408 describes a method for generating a gas stream containing carbon monoxide by: feeding a gas mixture containing carbon dioxide and hydrogen into a burner disposed in a reverse-flow gas shift reactor; and burning the gas mixture with a substoichiometric stream of oxygen to form a combustion gas mixture containing carbon monoxide, carbon dioxide, hydrogen, and steam. The mixture is then passed through a reverse-flow gas shift catalyst to form a crude product gas containing carbon monoxide, carbon dioxide, hydrogen, and steam. The gas is then cooled so that water content condenses and can be separated and removed. The gas is then passed to a carbon dioxide removal unit to remove carbon dioxide (which can be recycled back to the feed gas mixture of the reverse-flow gas shift reactor), producing a gas containing carbon monoxide and hydrogen.
[0009] WO2022079408 also discloses a method for preheating the gas flow fed into a reverse-flow gas shifter. The preheating temperature of the feed gas to the reverse-flow gas shifter can be in the range of 400°C to 1000°C or 450°C to 800°C to maintain combustion. The hydrogen and carbon dioxide streams can be premixed before or after preheating. Preheating the feed gas to its preheating temperature can be accomplished by heat exchange with the crude product gas mixture and / or by steam heating, or by using a flame heater, or by electric heating, or by a combination of two or more of these. Preferably, the feed gas mixture containing carbon dioxide and hydrogen is heated by heat exchange with the crude product gas mixture.
[0010] This specification relates to an improved method and system for producing syngas, with particular emphasis on preheating the feed gas of a countercurrent gas shift reactor. Summary of the Invention
[0011] As described in the background section, WO2022079408 teaches that preheating the carbon dioxide and hydrogen feed gases of a reverse-flow gas shift reactor (RFS) may be advantageous, and that the carbon dioxide and hydrogen streams can be premixed before or after preheating. From a production system perspective, the simplest and seemingly preferred method is to mix the hydrogen and carbon dioxide feed gases, preheat the gas mixture, and then pass the feed gas mixture into the RFS. However, it has been surprisingly found that under certain preheating conditions, the mixture of carbon dioxide and hydrogen feed gases may be more reactive than previously thought, and that preheating the mixed feed gas before it enters the RFS can at least partially trigger a RFS reaction. This can be problematic because such a reaction may generate a CO / H2 / CO2 / H2O mixture in the preheater equipment and pre-reactor piping, which can degrade standard preheater equipment and piping through material damage mechanisms such as carburization and metal dusting. This could shorten the lifespan of these components and require their replacement, thus increasing equipment costs and factory downtime.
[0012] The aforementioned problems may be exacerbated by the use of metallic structural materials in the preheater and / or piping preceding the reverse water-gas shift reactor to catalyze the reverse water-gas shift reaction. For example, heating the mixed gas feed on a large metallic heat exchange surface in the preheater can catalyze the reverse water-gas shift reaction.
[0013] Furthermore, preheating the mixed gas feed can trigger an exothermic methanation reaction, releasing heat and causing a temperature rise. Methanation can also be catalyzed by metallic structural materials, and when the rate of heat release exceeds the rate of heat dissipation, it can lead to a runaway reaction. This can cause the temperature to rise and exceed the design temperature of the preheater or piping, resulting in equipment damage and shutdown.
[0014] In view of the above, this specification provides a method for forming a synthesis gas, the method comprising:
[0015] A mixture of hydrogen and carbon dioxide feed gases is fed into the heater;
[0016] The mixture of hydrogen and carbon dioxide feed gases is heated to a temperature of at least 400°C in a heater; and
[0017] A mixture of heated hydrogen and carbon dioxide feed gases is fed into a refractory-lined reverse water gas shift reactor through a connecting pipe. The reverse water gas shift reaction in the reactor forms a synthesis gas containing hydrogen and carbon monoxide.
[0018] To suppress metal corrosion of the heater and the connecting pipe between the heater and the reverse water-gas shift reactor during operation, the method includes one or more of the following characterizing features:
[0019] The feed gas is supplied to the heater at an absolute pressure not exceeding 20 bar;
[0020] The steam is mixed with the feed gas before entering the heater;
[0021] The corrosion inhibitor is mixed with the feed gas before it enters the heater; and
[0022] Provide one or more components for the heater made of a nickel-chromium alloy that is corrosion resistant during operation.
[0023] According to some examples, all of the above-described characterizing features are combined to minimize metal corrosion in the heater and connecting pipes. However, it should be understood that for some applications, a combination of all four characterizing features may not be necessary. For example, operation at pressures above 20 bar may be acceptable if a suitable level of steam is provided in the feed gas. Similarly, corrosion can be adequately suppressed without the need for nickel-chromium alloy components if the parameters of the feed gas in terms of steam content and pressure are appropriately selected. Furthermore, the mixing of corrosion inhibitors (such as sulfur-based corrosion inhibitors) into the feed gas may not be necessary if the parameters of the feed gas and / or the construction materials of the heater are appropriately selected. That is, providing at least one of these characterizing features can at least partially solve the problem of metal corrosion in the heater and connecting pipes leading to the countercurrent gas shift reactor, while combining at least some and optionally all of these characterizing features enables the method to solve or at least substantially solve the problem of metal corrosion in the heater and connecting pipes leading to the countercurrent gas shift reactor.
[0024] In addition to the above, this specification also provides a method for synthesizing hydrocarbons, the method comprising: forming a synthesis gas as described above; and passing the synthesis gas through a Fischer-Tropsch system to form a hydrocarbon product stream. According to some examples, the hydrocarbon-containing recycle stream is also formed by the Fischer-Tropsch system itself and / or by a upgrading unit coupled to the Fischer-Tropsch system, and the method further comprises:
[0025] Steam is fed into a hydrocarbon-containing recirculation stream to form a recirculation stream containing a mixture of steam and hydrocarbons;
[0026] A recycle stream containing a mixture of steam and hydrocarbons is fed into a depleted reactor containing a depleted catalyst to generate a recycle stream containing steam and methane; and
[0027] Before the feed gas enters the heater, a recirculation stream containing steam and methane is mixed with the feed gas containing hydrogen and carbon dioxide, thereby providing steam mixed with the feed gas from the recirculation stream containing steam and methane.
[0028] This specification also provides a system configured to perform the methods described above. Attached Figure Description
[0029] Figure 1 A flowchart of a method for forming crude syngas according to this specification is shown.
[0030] Figure 2 This specification illustrates the process of passing through... Figure 1 The flowchart shows the method for forming syngas and the method for forming hydrocarbon product streams by combining Fischer-Tropsch units.
[0031] Figure 3 A flowchart of a method for forming a hydrocarbon product stream, which is not based on this specification, is shown.
[0032] Figure 4 (a) shows a graph illustrating the relationship between CO content and temperature for a heated feed mixture of carbon dioxide and hydrogen.
[0033] Figure 4 (b) shows Figure 4 (a) The graph extends beyond the 500°C test data to show the CO formation trend up to 650°C.
[0034] Figure 5 A flowchart of a method for forming crude syngas according to this specification is shown, and examples of how to modify it are illustrated. Figure 3 The flowchart shown illustrates how the present invention is implemented.
[0035] The table below provides an overview of the reference numerals used in the accompanying drawings.
[0036] Detailed Implementation
[0037] This specification provides a method for reducing metal corrosion in a reverse-flow gas shift system caused by methanation and CO formation in the preheater and pipelines preceding the reverse-flow gas shift reactor.
[0038] Hydrogen can react with carbon dioxide in a reverse water-gas shift (RWGS) reaction to produce syngas containing carbon monoxide and hydrogen. The RWGS reaction can be described as follows:
[0039]
[0040] Hydrogen can react with carbon dioxide and / or carbon monoxide to produce methane. The methanation reaction can be described as follows:
[0041]
[0042] Carbon monoxide can also react with hydrogen to produce carbon, as shown in the following reaction:
[0043]
[0044] In the reverse water-gas shift (RWS) flow diagram, the CO2 and H2 feed gases are advantageously heated (e.g., in an electric heater) to a typical temperature of approximately 550°C before entering the rWGS reactor, which is, for example, an autothermal reactor with a refractory lining. Test data highlight that the H2 and CO2 feed gases undergo a RWS reaction at 350°C, resulting in CO formation. The degree of CO formation increases with increasing temperature. Prior to testing, it was not anticipated that the feed gases would undergo a RWS reaction at 550°C in the absence of a catalyst. CO formation at 550°C could potentially lead to metal dust formation in the piping and electric heater over time. Furthermore, methanation may also occur, resulting in a temperature rise in the electric heater and outlet piping. If left uncontrolled, this temperature rise could damage the piping and equipment. Additionally, the literature emphasizes that the piping materials may also undergo catalytic reactions.
[0045] To reduce the degree of methanation and CO formation that cause metal dust in the preheater and pipelines of the reverse water gas conversion system, the following operations can be performed.
[0046] Reduce operating pressure
[0047] Based on Le Chatelier's principle, reducing pressure shifts the equilibrium to the left (hydrogen side), resulting in less methane formation in the heater. Furthermore, while pressure does not affect the equilibrium of the reverse water-gas shift reaction, operating at lower pressures reduces the partial pressure of CO, thus decreasing the CO reaction rate. Additionally, lower pressures reduce the methanation rate, leading to less methane exiting the reverse water-gas shift reactor. Since methane is inert in the downstream Fischer-Tropsch process, reducing the methane content in the syngas exiting the reverse water-gas shift reactor is advantageous.
[0048] Steam is introduced into the feed gas.
[0049] Based on Le Chatelier's principle of reverse water-gas shift reaction, increasing the steam content shifts the equilibrium towards the reactants side, thus reducing CO formation. Increasing the steam presence creates an oxidizing environment and reduces the amount of carbon formed by CO reduction. Furthermore, for methanation reactions, increasing the steam flow rate improves the conversion rate of methane to CO and H2, thereby lowering the gas temperature.
[0050] Before heating, steam can be added directly to the H2 and CO2 mixed feed stream. Alternatively, steam can be introduced into a hydrocarbon-containing recycle stream from a downstream hydrocarbon synthesis process, which is depleted to form a methane / steam stream, and then mixed with the H2 and CO2 feed stream before heating. In this regard, the depleted tail gas typically exits from the depleted reactor at approximately 530°C to 550°C, so it is clearly not feasible to connect it upstream of the electric heater for preheating to 550°C by flow diagram design. However, in this method, providing steam to the depleted tail gas and feeding it upstream of the electric heater suppresses metal corrosion within the heater by increasing the steam content of the H2 and CO2 mixed feed stream.
[0051] Use corrosion inhibitors
[0052] Corrosion reduction within the heater can also be achieved by adding corrosion inhibitors, such as sulfur-based corrosion inhibitors (e.g., H2S or disulfides), to the feed gas upstream of the heater.
[0053] Improve the resistance of electric heater and pipe materials to metal dust formation
[0054] Using alloys with higher resistance or cladding (e.g., nickel-chromium alloys) in the heaters and piping leading to the reverse water-gas shift reactor can mitigate the problem of metal dusting.
[0055] The following describes an example of implementing the above methods to reduce metal corrosion in the heater and the piping leading to the reverse water gas shift reactor.
[0056] Figure 1 A flowchart of a method for forming crude syngas is shown. The method includes heating a mixed carbon dioxide and hydrogen feed gas 2 to a temperature of at least 400°C using a heater 8, thereby forming a heated mixed feed gas stream 10. To prevent metal corrosion in the heater 8 and subsequent piping, a steam feed 4 and a corrosion inhibitor 6 are mixed with the carbon dioxide and hydrogen feed gas 2 before entering the heater 8. The pressure of the feed gas 2 is also controlled to suppress corrosion within the heater, for example, controlling the pressure of the feed gas so that the absolute pressure does not exceed 20 bar (e.g., operation at a gauge pressure not exceeding 20 bar, optionally about 15 bar gauge pressure). Alternatively or additionally, the heater may be provided with one or more components formed of a nickel-chromium alloy, which is corrosion-resistant during operation.
[0057] Subsequently, the heated mixed feed gas stream 10 is fed from the heater 8 into the water-gas shift reactor 12 containing the water-gas shift catalyst, and the heated mixed feed gas stream is passed through the water-gas shift catalyst in the water-gas shift reactor 12 to form the crude syngas product stream 14 by converting at least a portion of the carbon dioxide into carbon monoxide.
[0058] Therefore, the flowchart provides a method for forming a synthesis gas, the method comprising:
[0059] A mixture 2 of hydrogen and carbon dioxide feed gases is fed into heater 8;
[0060] The mixture 2 of hydrogen and carbon dioxide feed gases is heated to a temperature of at least 400°C in a heater; and
[0061] A mixture 10 of heated hydrogen and carbon dioxide feed gas is fed into a refractory-lined reverse water gas shift reactor 12 through a connecting pipe, and a synthesis gas 14 containing hydrogen and carbon monoxide is formed through a reverse water gas shift reaction in the reverse water gas shift reactor 12.
[0062] To suppress metal corrosion of the heater 8 and the connecting pipe between the heater 8 and the reverse water-gas shift reactor 12 during operation, the method includes one or more of the following characterizing features:
[0063] Feed gas 2 is supplied to heater 8 at an absolute pressure not exceeding 20 bar;
[0064] Steam 4 is mixed with feed gas 2 before entering heater 8;
[0065] The corrosion inhibitor 6 is mixed with the feed gas 2 before entering the heater 8; and
[0066] The heater 8 is provided with one or more components made of a nickel-chromium alloy that is corrosion resistant during operation.
[0067] Optionally, the mixture of hydrogen and carbon dioxide feed gases is heated in a heater to the following temperatures: at least 450°C, 500°C, 550°C, 600°C, or 700°C; not exceeding 1500°C, 1300°C, 1200°C, 1100°C, 1000°C, 900°C, or 850°C; or within a range defined by any combination of the lower and upper limits above (e.g., in the range of 450°C to 1100°C, optionally operating near the upper end of that range). Such temperatures can be achieved by many different types of heaters, including heaters selected from: heat exchange heaters; turbomachinery heaters; electric heaters; resistance heaters; and radiant heaters. High preheating temperatures can be beneficial for improving the efficiency of the reverse water-gas shift reactor, but can exacerbate metal corrosion problems in the heater. Therefore, this method is particularly useful when using relatively high preheater temperatures.
[0068] When the heater is equipped with one or more components formed of a nickel-chromium alloy that is corrosion-resistant during operation, the nickel-chromium alloy can be a pure nickel-chromium alloy, a nickel-chromium-aluminum alloy, or a nickel-chromium-copper alloy. Examples include one or more of the following: Alloy 310, 310S, 310Si, 800 / H / HT, RA 330, Alloy 600 / H, 625, 890, RA330, RA230, Alloy X, CT15C, Paralloy CR39W, H39WMR, H39WM+, HK40, HPW, HPNb, HP microalloy, Alloy 601, 602 CA, 603XL, 617, 671, 690, 693, 803, NEXAGE ™ 696, VDM ® Alloy 699 XA, HAYNES ® HR-235 ® HR214, HR120, HR160, H46M, RA253MA, RA333, RA353MA, 45TM, Paralloy OPTIM-AL, H46M, or H48T. The alloy can also provide pressure resistance in the heater, or it can be coated with another metal to provide mechanical support for pressure resistance in the heater. To further improve the corrosion resistance of heater components, nickel-chromium alloys may include coatings such as aluminum diffusion coatings, chromium diffusion coatings, silicon coatings, or catalytic coatings.
[0069] To further reduce corrosion, corrosion inhibitors can be added to one or more feed streams before the mixing zone. For example, corrosion inhibitors can be sulfur-based corrosion inhibitors, such as H₂S or disulfides. These agents cause sulfur to adsorb onto the metal surface, thereby preventing carbon penetration into the base alloy. Therefore, to enhance corrosion protection, low levels of reactive sulfur substances, such as H₂S or disulfides, can be provided in the process environment. Sulfur levels less than 10 ppm (e.g., in the range of 1 ppb to 10 ppm, optionally 1 ppm to 10 ppm) are sufficient to mitigate metal dusting. Other non-sulfur inhibitors are also known.
[0070] To further reduce corrosion, the feed gas may be supplied to the heater at the following absolute pressures: not exceeding 20 bar, 19 bar, 18 bar, 17 bar or 16 bar; not less than 5 bar, 10 bar, 12 bar or 14 bar; or within the range defined by any combination of the above upper and lower limits.
[0071] To further reduce corrosion, the vapor can be mixed with the feed gas to achieve the following feed gas vapor content: at least 0.1 mol%, 0.2 mol%, 0.3 mol%, 0.5 mol%, 1 mol%, 2 mol%, 2.5 mol%, 3 mol%, 3.5 mol%, 4 mol%, or 4.5 mol%; not exceeding 10 mol%, 9 mol%, 8 mol%, 7 mol%, 6 mol%, or 5 mol%; or within the range defined by any combination of the lower and upper limits above (e.g., 2.5 mol% to 5 mol%).
[0072] In addition, the connecting pipe between the heater and the reverse water gas shift reactor may be lined with a refractory lining or formed of a nickel-chromium alloy that is corrosion resistant during operation (such as the one described above for the heater).
[0073] The synthesis gas formed using the method described above can be used to produce hydrocarbons using a Fischer-Tropsch system. Therefore, this specification also provides a method for synthesizing hydrocarbons, the method comprising: forming the synthesis gas as described above; and passing the synthesis gas through a Fischer-Tropsch system to form a hydrocarbon product stream. The hydrocarbon-containing recycle stream is also formed by the Fischer-Tropsch system itself and / or by a upgrading unit coupled to the Fischer-Tropsch system. In this case, the method may further comprise: feeding steam into the hydrocarbon-containing recycle stream to form a recycle stream containing a mixture of steam and hydrocarbons; feeding the recycle stream containing the mixture of steam and hydrocarbons into a lean reactor containing a lean catalyst to generate a recycle stream containing steam and methane; and mixing the recycle stream containing steam and methane with a feed gas containing hydrogen and carbon dioxide before the feed gas enters a heater, wherein the steam mixed with the feed gas is provided by the recycle stream containing steam and methane.
[0074] Figure 2 It shows how to... Figure 1 The flowchart illustrates the syngas formation method and the process of forming a hydrocarbon product stream by combining Fischer-Tropsch units. The production method of the crude syngas product stream 14 is similar to that described above. Figure 1 The methods described are the same or similar, and for the sake of brevity, these steps / parts will not be repeated.
[0075] The crude syngas from the reverse-flow gas shift reactor is advantageously treated to remove water and carbon dioxide before being fed into the Fischer-Tropsch unit. Thus, the crude syngas 14 can be passed to the water removal unit 22 to form a separated water stream 24 and dehydrated syngas 26. The separated water stream 24 can be fed into an electrolyzer 28 to generate a hydrogen stream 30, which is then recycled to the feed gas 2 containing hydrogen and carbon dioxide for use in the reverse-flow gas shift reactor 12. The electrolyzer 28 can also generate an oxygen stream 32, which is fed into the burner of the reverse-flow gas shift reactor 12.
[0076] The crude syngas (advantageously after water removal) is fed into the carbon dioxide removal unit 34 to form a separated carbon dioxide stream 36 and a decarbonized syngas 38. The separated carbon dioxide stream 36 can be recycled back into the feed gas 2 containing hydrogen and carbon dioxide.
[0077] After removing water and carbon dioxide, and optionally further processing to remove other contaminants, the syngas is passed to the Fischer-Tropsch unit 40 to produce a hydrocarbon product stream 42 and a tail gas stream 44. Advantageously, the tail gas stream 44 is recycled to the reverse water-gas shift reactor 12. In this case, the tail gas stream is mixed with the steam stream 4 and passed through a lean reactor 46 to form a stream 48 containing methane and steam. This stream is mixed with the feed stream 2 before entering the heater 8 to increase the steam content of the feed stream and reduce corrosion in the heater and the piping leading to the reverse water-gas shift reactor 12. Both the reverse water-gas shift reaction and the steam methane reforming reaction can occur within the reverse water-gas shift reactor 12 to produce crude syngas.
[0078] To illustrate the benefits of this method, a counterexample is described below, followed by a summary of experiments that have been modified according to this specification.
[0079] Figure 3 An example flowchart of a method for forming crude syngas, not according to this specification, is shown. Carbon dioxide feed gas is mixed with hydrogen feed gas to produce mixed feed gas 2. Mixed feed gas 2 is passed through mixed feed gas heat exchanger 52, where it is heated using a hot syngas product stream from a countercurrent gas shift reactor. For example, the mixed feed gas at this stage may be at a temperature of approximately 400°C (398°C in the illustrated example). The mixed feed gas is then passed through mixed feed gas heater 8 to further increase its temperature. For example, in the illustrated example, the mixed feed gas is heated to 550°C. The heated mixed feed gas 10 is then passed to countercurrent gas shift reactor 12.
[0080] The tail gas stream 44 (e.g., recycled from a downstream hydrocarbon synthesis unit) is passed through a tail gas heat exchanger 58, where it is heated using a hot syngas product stream from a reverse-flow gas shift reactor. The tail gas is then passed through a lean reactor 46 to produce a methane-containing gas stream 59, which is mixed with a heated mixed feed gas stream 10. In the illustrated example, the methane-containing gas stream from the lean reactor is at a temperature of 530°C, the heated mixed H2 / CO2 gas stream is at 550°C, and the feed gas is at a temperature of 548°C when the two streams are mixed and fed into the reverse-flow gas shift reactor. It can be noted that the heating element of the feed gas heater will be at a higher temperature than the process gas temperature.
[0081] Oxygen feed 60 is also fed into the reverse-flow gas shift reactor 12 and combusted to further increase the temperature of the reactants, thereby driving the reverse-flow gas shift reaction and producing a crude syngas product stream. In the illustrated example, the crude syngas exiting the reactor is at a temperature of 900°C. The hot crude syngas can be used to generate steam in the syngas boiler 62, and then passed through the tail gas heat exchanger 58 and the H2 / CO2 feed gas heat exchanger 52.
[0082] The inventors have determined that the mixed feed gas heater 8 and the gas pipeline 10 from the heater 8 to the reverse water gas shift reactor 12 may be prone to damage under certain operating conditions and after prolonged operation. Figure 3 (The area highlighted in the image). This is because CO can potentially form in this area, leading to metal degradation.
[0083] To address the above situation, experiments have been conducted to determine the effectiveness of preheating the mixed H2 and CO2 feed before it enters the reverse water-gas shift reactor (e.g., Figure 3 (The flowchart illustrates how much CO can be formed.) A mixed H2 and CO2 feed was preheated from 300°C to 500°C through an empty reactor. The reactor was preheated with nitrogen before switching to the H2 and CO2 mixture. Each temperature test was conducted for 1 hour, then gradually switched to higher temperatures within the test temperature range. The amount of CO was measured at each test temperature. The test conditions are summarized below:
[0084] • H2 – 70.1 mol%, CO2 – 29.9 mol%
[0085] • Test pressure – 24.7 bar gauge pressure
[0086] • Reactor tube material - coated alloy
[0087] • Reactor ID (inner diameter) – 28mm
[0088] • Sample the gas at the reactor outlet and measure the CO content.
[0089] The result is Figure 4 As illustrated in (a), this graph shows the relationship between CO content (mol%) and temperature. Between 300°C and 400°C (which corresponds to...) Figure 3 During the temperature range of the mixed feed gas between the feed heat exchanger 52 and the heater 8, the amount of CO remains relatively low. However, as the temperature rises to 500°C or higher (which corresponds to...), the CO content increases. Figure 3 The temperature of the mixed feed gas in the heater 8 and the gas line 10 leading to the reactor increases significantly, as does the CO content. Figure 4 (b) shows Figure 4(a) The graph extends beyond the 500°C test data to show the CO formation trend up to 650°C.
[0090] Therefore, these experiments show that, at least under these operating conditions, CO generation in heater 8 and gas line 10 may be a potential problem if the mixed feed gas conditions and construction materials are not properly managed.
[0091] Furthermore, there is some evidence in the literature suggesting that certain metal alloys used in the manufacture of reactor equipment may affect the amount of CO2 converted to CO via the reverse water-gas shift reaction. For example, in "High-Temperature Kinetics of the Homogeneous Reverse Water–Gas Shift Reaction" by F. Bustamante and RM Enick, AICHE Journal, Vol. 50, No. 5, May 2004, p. 1039, a comparison of the reverse water-gas shift reaction in an Inconel 600 (nickel-chromium alloy) reactor and a quartz reactor was made. This paper found that Inconel 600 catalyzed the reverse water-gas shift reaction compared to an inert quartz reactor and showed some evidence of CO2 conversion in a temperature range starting from 820 K, which is similar to... Figure 3 The temperature of the heated mixed feed gas stream 2 in the flowchart is shown. Therefore, it is believed that alloy materials commonly used in the feed heater 8 and gas line 10 may help drive the countercurrent gas shift reaction in the heater and gas line, thereby producing CO before entering the countercurrent gas reactor.
[0092] The formation mechanisms of carbon and metal dust include the following…
[0093] [CO is formed via RWGS reaction]
[0094] [CO forms carbon through the Boudouard carbon evolution reaction]
[0095] CO is reduced to form carbon.
[0096] Methane cracking (e.g., in recycled, lean tail gas) can also form carbon. Carbon formation leads to metal dusting, a form of corrosion that occurs when susceptible materials are exposed to environments with high carbon activity. Metal components corrode over time, which can lead to equipment failure. While not bound by theory, initial data suggest that in... Figure 3Under the current conditions of the mixed feed gas heated in heater 8 and gas line 10, carbon formation via CO reduction is more likely to be problematic than carbon formation via the Budoar pathway. Thermodynamically, the feed gas composition falls into the region where carbon is formed via CO reduction. This means that, thermodynamically, the feed gas composition can form carbon. However, how much of a problem this might cause in practice will depend on the kinetics of the carbon formation process. Below 400°C to 450°C, the process kinetics are slow enough that metal dust formation is generally not a problem. However, the currently low feed heater temperature in the syngas production process reduces process efficiency. Therefore, from a process efficiency perspective, it is desirable to preheat the feed gas to a temperature exceeding 500°C.
[0097] Figure 5 An improved flow chart for solving this problem is shown. In this flow chart, steam 4 is added in sufficient quantity to the tail gas stream 44 so that the resulting methane stream 48, after the lean reactor 46, also contains a significant amount of steam. Furthermore, this mixed methane / steam stream 48 is directed to mix with the carbon dioxide and hydrogen feed stream 2 before the heater 8, thereby increasing the steam content of the feed stream entering the heater 8. This helps to reduce reactions that could lead to metal corrosion in the heater 8 and pipe 10, as previously described.
[0098] In addition to the above, a corrosion inhibitor 6 is introduced into the feed stream 2 before the heater 8 to further reduce corrosion in the heater. Furthermore, the pressure of the feed stream 2 can be reduced to, for example, less than 20 bar absolute pressure, and / or the heater components can be formed of a corrosion-resistant nickel-chromium alloy. In other aspects, Figure 5 The system and Figure 3 The system is the same. These improvements are sufficient to reduce or eliminate metal corrosion problems while maintaining the efficient operation of the syngas production system.
[0099] While the invention has been specifically shown and described with reference to certain examples, those skilled in the art will understand that various changes in form and detail may be made without departing from the scope of the invention as defined by the appended claims.
Claims
1. A method for forming a synthesis gas, the method comprising: A mixture of hydrogen and carbon dioxide feed gases is fed into the heater; The mixture of hydrogen and carbon dioxide feed gases is heated to a temperature of at least 400°C in the heater; and A mixture of heated hydrogen and carbon dioxide feed gases is fed into a refractory-lined reverse-flow gas shift reactor through a connecting pipe, and a synthesis gas containing hydrogen and carbon monoxide is formed through a reverse-flow gas shift reaction in the reactor. In order to suppress metal corrosion of the heater and the connecting pipe between the heater and the countercurrent gas shift reactor during operation, the connecting pipe between the heater and the countercurrent gas shift reactor is lined with a refractory lining or formed of a corrosion-resistant nickel-chromium alloy during operation, and the method further includes at least one corrosion reduction feature selected from the group consisting of: The steam is mixed with the feed gas before entering the heater; The corrosion inhibitor is mixed with the feed gas before it enters the heater; The feed gas is supplied to the heater at an absolute pressure not exceeding 20 bar; and The heater is provided with one or more components formed of a nickel-chromium alloy, which is corrosion-resistant during operation.
2. The method according to claim 1, The mixture of hydrogen and carbon dioxide feed gases is heated in the heater to the following temperatures: at least 450°C, 500°C, 550°C, 600°C or 700°C; not exceeding 1500°C, 1300°C, 1200°C, 1100°C, 1000°C, 900°C or 850°C; or within the range defined by any combination of the lower and upper limits above.
3. The method according to claim 1 or 2, The heater is selected from: heat exchange heaters; turbomachinery heaters; electric heaters; resistance heaters; and radiation heaters.
4. The method according to any of the preceding claims, One or more nickel-chromium alloy components of the heater are formed of pure nickel-chromium alloy, nickel-chromium-aluminum alloy, or nickel-chromium-copper alloy.
5. The method according to claim 4, wherein the nickel-chromium alloy is selected from one or more of the following: Alloy 310, 310S, 310Si, 800 / H / HT, RA330, Alloy 600 / H, 625, 890, RA330, RA230, Alloy X, CT15C, Paralloy CR39W, H39WMR, H39WM+, HK40, HPW, HPNb, HP Microalloy, Alloy 601, 602CA, 603XL, 617, 671, 690, 693, 803, NEXAGE ™ 696、VDM ® Alloy 699 XA, HAYNES ® HR-235 ® , HR214, HR120, HR160, H46M, RA253MA, RA333, RA353MA, 45TM, Paralloy OPTIMAL, H46M, or H48T.
6. The method according to any of the preceding claims, The nickel-chromium alloy mentioned above includes a coating.
7. The method according to claim 6, The coating is an aluminum diffusion coating, a chromium diffusion coating, a silicon coating, or a catalytic coating.
8. The method according to any of the preceding claims, The corrosion inhibitor that is mixed with the feed gas before entering the heater is a sulfur-based corrosion inhibitor.
9. The method according to claim 8, The corrosion inhibitor is H2S or disulfide.
10. The method according to claim 8 or 9, The corrosion inhibitor is added to the feed gas to achieve a sulfur level in the range of 1 ppb to 10 ppm.
11. The method according to any of the preceding claims, The feed gas is supplied to the heater at an absolute pressure not exceeding 19 bar, 18 bar, 17 bar or 16 bar; not less than 5 bar, 10 bar, 12 bar or 14 bar; or within the range defined by any combination of the above upper and lower limits.
12. The method according to any of the preceding claims, The steam is mixed with the feed gas to achieve the following feed gas steam content: at least 0.1 mol%, 0.2 mol%, 0.3 mol%, 0.5 mol%, 1 mol%, 2 mol%, 2.5 mol%, 3 mol%, 3.5 mol%, 4 mol%, or 4.5 mol%; not exceeding 10 mol%, 9 mol%, 8 mol%, 7 mol%, 6 mol%, or 5 mol%; or within the range defined by any combination of the lower and upper limits above.
13. A method for synthesizing hydrocarbons, the method comprising: Forming a synthesis gas according to any of the preceding claims; as well as The synthesis gas is passed through a Fischer-Tropsch system to form a hydrocarbon product stream.
14. The method according to claim 13, The hydrocarbon-containing recycle stream is also formed by the Fischer-Tropsch system itself and / or by a upgrading unit coupled to the Fischer-Tropsch system, and the method further includes: Steam is fed into the hydrocarbon-containing recirculation stream to form a recirculation stream containing a mixture of steam and hydrocarbons; The recycle stream containing a mixture of steam and hydrocarbons is fed into a depleted reactor containing a depleted catalyst to generate a recycle stream containing steam and methane; and Before the feed gas enters the heater, the recirculation stream containing steam and methane is mixed with the feed gas containing hydrogen and carbon dioxide, thereby providing the steam mixed with the feed gas from the recirculation stream containing steam and methane.
15. A system configured to perform the method according to any of the preceding claims.
Citation Information
Patent Citations
Process for producing a gas stream comprising carbon monoxide
WO2022079408A1