Metal fluoride and plasma assisted atomic layer deposition coating
By using the ALD process to alternately deposit metal fluoride layers on optical components, the problem of poor coating uniformity in PVD processes on optical components with steep surface curvatures is solved, achieving uniform coating and simplifying the process, thereby improving the resolution and imaging capability of the optical system.
Patent Information
- Application Number
- CN202580030811.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-03-26
- Filing Date
- 2025-02-27
- Publication Date
- 2026-11-24
AI Technical Summary
Existing physical vapor deposition (PVD) processes struggle to uniformly coat anti-reflective coatings on optical components with steep surface curvatures, resulting in poor coating uniformity and increased process complexity, which in turn affects the resolution and imaging capabilities of the optical system.
Atomic layer deposition (ALD) is employed to form a coating on optical components using metal fluorides and plasma-assisted technology. Uniform coating is achieved by alternating deposition of different metal fluoride layers, such as LaF₃ and MgF₂.
Uniform coatings were achieved on optical components with steep surface curvature, improving the resolution and imaging capabilities of the optical system, reducing the risk of coating peeling, and simplifying the process.
Smart Images

Figure CN123165474A_ABST
Abstract
Description
[0001] This application claims priority to U.S. Provisional Patent Application Serial No. 63 / 569823, filed March 26, 2024, the contents of which are based and incorporated herein by reference in their entirety. Technical Field
[0002] This disclosure generally relates to coated optical components, and more specifically, to optical components comprising metal fluoride and plasma-assisted atomic layer deposition coatings for deep ultraviolet (DUV) applications, and to processes for producing such coatings. In embodiments, the metal fluoride and plasma-assisted atomic layer deposition coating is an anti-reflective coating. Background Technology
[0003] Anti-reflective (AR) coatings are used to prevent unwanted reflections of light from the surface of an object. Generally, light is more likely to be reflected from the surface of an object when it strikes the surface at a high angle of incidence. Therefore, objects with surfaces having steep curvature are more likely to reflect light incident on them because at least some of the light will strike the surface at a relatively high angle of incidence.
[0004] Current physical vapor deposition (PVD) processes for AR coatings suffer from the problem of uneven coating of steep surface curvatures because these processes rely on a substantially linear deposition of particles from the deposition source to the deposition target. To address this uniformity issue, complex motion and occlusion steps need to be incorporated into the process. This increases the complexity, cost, and time required to complete the process.
[0005] Therefore, there is a need for new methods for depositing anti-reflective coatings. Summary of the Invention
[0006] For optical applications, such as optical lenses, the reflection and / or absorption of light can be problematic. Reflection and / or absorption reduce the amount of light transmitted through an optical lens toward its desired target. This reduction in transmitted light can impair the resolution of optical systems that rely on optical lenses to collect and focus light. This decrease in resolution can impair the optical system's ability to accurately image an object.
[0007] The reflection and / or absorption of light can depend on the wavelength of light utilized by the optical system and the surface curvature of the optical lens used to focus the light. For example, high numerical aperture lenses (i.e., objectives) used in optical inspection systems can have steep surface curvatures to focus light at specific wavelengths or wavelength ranges. If light is reflected from such a steep surface, it can impair the inspection system's ability to accurately image an object. Accurate imaging of objects is important in many applications, such as semiconductor wafer inspection systems. For quality control purposes, these systems need to be able to accurately detect any contaminants (e.g., debris particles) on the surface of semiconductor wafers.
[0008] Due to the importance of accurate surface imaging, some optical inspection systems, such as semiconductor inspection systems, utilize light based on deep ultraviolet (DUV) lasers (i.e., light with wavelengths in the range of 157 nm and 193 nm to 266 nm) or light in the broadband spectrum (i.e., light with wavelengths in the range of 150 nm to 300 nm). These wavelengths enable higher resolution than other light wavelengths (e.g., visible light in the range of 400 nm to 700 nm). However, the light intensity at these wavelengths is relatively low. Low intensity can be problematic because it may reduce the resolution capability of the inspection system. Therefore, one or more high numerical aperture lenses with steep surface curvature may be needed to focus the light. Properly focusing the DUV or broadband wavelength increases the light intensity in the detection area, thereby achieving suitable detection resolution.
[0009] Embodiments of this disclosure include coatings for DUV or broadband wavelength-based optical systems. However, unlike conventional coatings, the coatings disclosed herein are not formed using a PVD process. Instead, the coatings disclosed herein are formed using an atomic layer deposition (ALD) process. PVD coatings can be applied to optical components to provide enhanced anti-reflective properties. However, PVD coatings are difficult to apply to optical components with steeply curved surfaces. For example, steeply curved surfaces can cause viewing problems during the PVD coating process, which may result in poor coating uniformity and / or require complex process modifications, such as repositioning the PVD coating apparatus when the coating is applied to the optical component. Steeply curved surfaces can also cause the PVD coating to detach from the surface during the coating process.
[0010] In the embodiments disclosed herein, an ALD process is used to deposit a coating onto an optical component. Specifically, the ALD coatings disclosed herein comprise a metal fluoride-based coating that uses a plasma fluorine source to reduce metallic impurities in the coating. The plasma may be sulfur hexafluoride. In some exemplary embodiments, the metal fluoride is lanthanum fluoride. The ALD coatings disclosed herein, deposited using the methods disclosed herein, exhibit enhanced uniformity and low surface roughness.
[0011] In one embodiment, a coated optical component is described, the coated optical component comprising: a substrate having at least one surface; and an atomic layer deposition coating deposited on the surface of the substrate, the atomic layer deposition coating comprising a first layer of lanthanum fluoride. Furthermore, the atomic layer deposition coating has a carbon concentration of about 10,000 ppm or less, an oxygen concentration of about 10,000 ppm or less, and a sulfur concentration of about 500 ppm or less.
[0012] In an embodiment, a method for coating an optical component with an atomic layer deposition coating is described, the method comprising: converting a fluorine source into a sulfur hexafluoride-based plasma by generating a plasma of a fluorine source while applying a current having a power of about 100 watts to about 400 watts at a temperature of about 5°C to about 20°C; and exposing the surface of a substrate to a cycle of the atomic layer deposition coating process in an atomic layer deposition chamber by: (i) exposing the surface of the substrate to one or more pulses of a lanthanum-based metal precursor while heating the substrate to a temperature of about 100°C to about 400°C; and (ii) exposing the surface of the substrate to one or more pulses of the sulfur hexafluoride-based plasma while heating the substrate to a temperature of about 100°C to about 400°C.
[0013] Additional features and advantages of the metal fluoride and plasma-assisted atomic layer deposition coatings and the methods for producing such coatings will be set forth in the detailed description below, and will be apparent in part to those skilled in the art from the description, or will be recognized by practice of the embodiments described herein (including the detailed description below, the claims, and the accompanying drawings).
[0014] It should be understood that both the foregoing general description and the following detailed description describe various embodiments and are intended to provide an overview or framework for understanding the nature and characteristics of the claimed subject matter. The accompanying drawings are included to provide a further understanding of the various embodiments, and are incorporated in and form a part of this specification. The drawings illustrate the various embodiments described herein and, together with the description, serve to explain the principles and operation of the claimed subject matter. Attached Figure Description
[0015] Figure 1 A partial view of an optical component coated with an ALD coating according to an embodiment disclosed herein is schematically depicted;
[0016] Figure 2 A side view of an optical inspection system with a high numerical aperture objective lens according to an embodiment disclosed herein is schematically depicted.
[0017] Figure 3A Another partial view of an optical component coated with an ALD coating according to an embodiment disclosed herein is schematically depicted;
[0018] Figure 3B Another partial view of an optical component coated with an ALD coating according to an embodiment disclosed herein is schematically depicted;
[0019] Figure 4 An ALD system for performing an ALD coating process according to embodiments disclosed herein is schematically depicted;
[0020] Figure 5 A pulse applied to a substrate during one cycle of an ALD coating process according to an embodiment disclosed herein is illustrated schematically;
[0021] Figure 6 A plot of the refractive index versus wavelength for ALD and PVD coatings produced according to the embodiments disclosed herein is shown;
[0022] Figure 7A The thickness values of each layer of an exemplary ALD coating on a substrate according to embodiments disclosed herein are shown, and Figure 7B A scanning electron microscope image of an exemplary ALD coating is shown; and
[0023] Figure 8 Examples according to the disclosure herein are shown. Figure 7A and 7B The reflectance of an exemplary coating before and after a humidity test. Detailed Implementation
[0024] As used herein, the term "substantially free" means that the composition contains less than 0.01% by weight of the said ingredient. For example, a substantially carbon-free ALD coating contains less than 0.01% by weight of carbon.
[0025] The terms “micrometer” and “µm” are used interchangeably in this document. The terms “nanometer” and “nm” are used interchangeably in this document.
[0026] As used herein, the term "plasma" refers to an ionized gas that comprises positive ions and electrons and is generated from a gas-phase starting material by applying ionization energy, such as energy in the form of heat, potential, or electric current.
[0027] As used herein, the term “ppm” means parts per million (in moles) and indicates atomic concentration. For example, a LaF3 layer with 1 ppm of carbon comprises 1 mole of carbon per million moles of LaF3.
[0028] As used herein, the term "conformal coating" refers to a coating that conforms to the surface profile of an article and has a substantially uniform thickness on all surfaces in contact with the coating.
[0029] As used herein, the term "anti-reflective (AR) coating" refers to a coating with a reflectivity of less than 1% over a specific wavelength range, where "reflectivity" refers to the fraction of the incident beam power reflected and returned from a given surface. The reflectivity (R) of a surface... X This can be represented as Rx = P r / P0, where P0 is the incident beam power, and P r It is the power of the beam returning from the surface.
[0030] Reference will now be made in detail to various embodiments of the disclosed ALD coating and optical components coated thereon. (See also...) Figure 1 An exemplary coated optical component 10 is disclosed, comprising a substrate 20 and an ALD coating 30 applied to one or more surfaces 22 of the substrate 20, the substrate being an optical component. In embodiments, the substrate 20 may include, for example, a lens, window, objective lens, prism, beam splitter, filter, and / or mirror. The ALD coating 30 may be a protective coating that provides a barrier on the surface 22 of the substrate 20. In embodiments, the ALD coating 30 may prevent or reduce the degradation and / or erosion of the material of the substrate 20. As further discussed below, in embodiments, the ALD coating 30 is an AR coating.
[0031] It is known in the art to extend the lifespan of optical components by coating them with physical vapor deposition (PVD). For example, PVD coatings can be applied to such optical components (e.g., lenses, windows, objectives, prisms, beam splitters, filters, and / or mirrors) to reduce surface degradation and thus extend their lifespan. PVD coatings can also be applied to provide anti-reflective properties to optical components. Examples of PVD coatings include, but are not limited to, silica PVD coatings or combinations of magnesium fluoride (MgF2) PVD coatings and silica PVD coatings. These PVD coatings have a relatively thick total thickness to ensure that the surface of the optical component is sealed by the PVD coating and that there are no gaps or pinholes in the PVD coating. However, PVD coatings can be difficult to apply to optical components with steeply curved surfaces. For example, steeply curved surfaces can cause visibility problems during the PVD coating process, which can lead to poor coating uniformity and lack of conformality and / or require complex process modifications, such as repositioning the PVD coating equipment when the coating is applied to the optical component. Steeply curved surfaces can also cause the PVD coating to peel off during the coating process.
[0032] Figure 2An exemplary optical inspection system 100 for optical inspection using DUV or broadband spectral wavelengths is shown. The optical inspection system 100 may include a number of different optical components, including, for example, high numerical aperture (NA) objectives 110 having one or more surfaces 115 with very steep curvature. As mentioned above, the steep curvature of surface 115 can introduce several problems during the PVD coating process, resulting in uneven coating and / or complex process modifications.
[0033] Compared to conventional PVD coatings, the ALD coatings disclosed herein can be applied to steeply curved surfaces (such as surface 115) without the problems associated with PVD coating processes. As discussed further below, the ALD coating process disclosed herein can provide an easily applied, uniform ALD coating, even for such steeply curved surfaces.
[0034] Refer again Figure 1 The ALD coating 30 disclosed herein provides a protective barrier on the surface 22 of the substrate 20, and / or provides the substrate 20 with anti-reflective properties. For example, the ALD coating can prevent or reduce the degradation and / or erosion of the material of the substrate 20. The ALD coating 30 may comprise a metal fluoride, a metal oxide, a quasi-metal oxide, or a combination thereof. Alternatively or additionally, the ALD coating 30 may comprise silicon dioxide, aluminum oxide, or a combination of these components. In embodiments, the ALD coating 30 comprises at least a high-refractive-index fluoride, such as lanthanum fluoride (LaF3) and / or gadolinium fluoride (GdF3). In further embodiments, the ALD coating 30 comprises both a high-refractive-index metal fluoride and a low-refractive-index metal fluoride. In embodiments, the high-refractive-index metal fluoride comprises LaF3 and / or GdF3, and the low-refractive-index metal fluoride comprises magnesium fluoride (MgF2) and / or aluminum fluoride (AlF3). Including LaF3 in the ALD coating 30 is advantageous because it has a relatively large band gap, high refractive index, high transmittance, and chemical and mechanical stability at wavelengths, for example, in the DUV range. Specifically, LaF3 has a band gap of 6.04 electron volts (eV) at DUV wavelengths from 193 nm to 266 nm. Including MgF2 in the ALD coating 30 is advantageous because it has a low refractive index, high transmittance, and chemical and mechanical stability at wavelengths, for example, in the DUV range. In some exemplary embodiments, as will be discussed further below, the ALD coating 30 comprises alternating layers of LaF3 and MgF2.
[0035] like Figure 3AAs shown, the ALD coating 30 may comprise multiple layers, including a first layer 32 and a second layer 34. Each of the first layer 32 and the second layer 34 may be applied to the substrate 20 by an ALD process, as discussed further below. The second layer 34 may comprise a material different from that of the first layer 32, such as a different metal fluoride. Furthermore, the second layer 34 may be directly attached to the first layer 32 without any intermediate coating or other material placed between the layers. It is also noted that the first layer 32 may be directly attached to the substrate 20 without any intermediate coating or material placed between the first layer 32 and the substrate 20. In other embodiments, the second layer 34 is directly attached to the substrate 20 without any intermediate coating or material placed between the second layer 34 and the substrate 20. Although Figure 3A The ALD coating 30 is depicted only as comprising a first layer 32 and a second layer 34, but it is contemplated herein that the ALD coating 30 may comprise more layers. For example, the ALD coating 30 may comprise two or more, three or more, four or more, five or more, six or more, seven or more, eight or more, nine or more, or ten or more layers of each of the first layer 32 and the second layer 34. One or more of the plurality of layers of the first layer 32 and the second layer 34 may have a different material (such as a different metal fluoride) than one or more of the other layers. In some embodiments, the ALD coating 30 comprises alternating layers of the first layer 32 and the second layer 34. It is also contemplated herein that the ALD coating 30 may comprise one or more additional layers in addition to the first layer 32 and the second layer 34.
[0036] In some embodiments, the first layer 32 comprises a metal fluoride having a relatively low refractive index, and the second layer 34 comprises a metal fluoride having a relatively high refractive index, such that the refractive index of the second layer 34 is higher than that of the first layer 32. For example, at a wavelength of 193 nm, the refractive index of the first layer 32 may be about 1.30 to about 1.60, or about 1.32 to about 1.58, or about 1.34 to about 1.56, or about 1.36 to about 1.54, or about 1.38 to about 1.52, or about 1.40 to about 1.50, or about 1.42 to about 1.48, or about 1.44 to about 1.46 (or any range covering these endpoints). Furthermore, at a wavelength of 193 nm, the refractive index of the second layer 34 may be from about 1.65 to about 1.75, or from about 1.66 to about 1.74, or from about 1.67 to about 1.73, or from about 1.68 to about 1.72, or from about 1.69 to about 1.71, or from about 1.70 to about 1.75 (or any range covering these endpoints). In some embodiments, the first layer 32 comprises MgF2 with a refractive index of 1.43 at 193 nm, and the second layer 34 comprises LaF3 with a refractive index of 1.72 at 193 nm.
[0037] As will be discussed further below, each of the multiple layers (e.g., first layer 32, second layer 34) may contain different materials, such as different metal fluorides. In some embodiments, first layer 32 contains MgF2 and second layer 34 contains LaF3, such that ALD coating 30 comprises alternating layers of MgF2 and LaF3. Figure 3A An exemplary embodiment is shown, wherein the ALD coating 30 comprises a first layer 32 and a second layer 34. Figure 3B Another exemplary embodiment is shown, wherein the ALD coating 30 comprises two first layers 32 and one second layer 34, such that the first layer 32 and the second layer 34 alternate. Figure 3B In some exemplary embodiments, the first layer 32 comprises MgF2 (with a refractive index of 1.43 at 193 nm) and the second layer 34 comprises LaF3 (with a refractive index of 1.72 at 193 nm).
[0038] Each individual layer (first layer 32, second layer 34) is formed by ALD deposition of the material of said individual layer. More specifically, as will be discussed below, one ALD coating cycle deposits one material deposition layer. The ALD coating cycle is then repeated multiple times to form each of the first layer 32 and the second layer 34. In one exemplary embodiment, one ALD coating cycle applies a MgF2 deposition layer on the substrate 20, and then the ALD coating cycle is repeated 300 times to form the first layer 32 on the substrate 20. Next, in this exemplary embodiment, one ALD coating cycle applies a LaF3 deposition layer on the first layer 32, and then the ALD coating cycle is repeated 500 times to form the second layer 34 on the first layer 32.
[0039] In embodiments, the deposited layer formed by each ALD coating cycle forms a monolayer of material with a thickness comparable to the size of a single molecule of the ALD-coated material. In the embodiments disclosed herein, each ALD coating cycle may be repeated 50 or more times, or 100 or more times, or 150 or more times, or 200 or more times, or 250 or more times, or 300 or more times, or 350 or more times, or 400 or more times, or 450 or more times, or 500 or more times, or 550 or more times, or 600 or more times, or 650 or more times, or 700 or more times, or 750 or more times, or 800 or more times, or 850 or more times, or 900 or more times, or 950 or more times, or 1000 or more times, or any range covering these endpoints, to produce each of a plurality of layers (e.g., first layer 32, second layer 34).
[0040] Each deposited layer formed by an ALD coating cycle may have a thickness of about 0.001 nm or greater, or about 0.005 nm or greater, or about 0.008 nm or greater, or about 0.010 nm or greater, or about 0.020 nm or greater, or about 0.030 nm or greater, or about 0.040 nm or greater, or about 0.050 nm or greater, or about 0.060 nm or greater, or about 0.070 nm or greater, or about 0.080 nm or greater, or about 0.090 nm or greater, or about 0.100 nm or greater. Alternatively, each deposited layer formed by an ALD coating cycle may have a thickness of about 0.100 nm or less, or about 0.090 nm or less, or about 0.080 nm or less, or about 0.070 nm or less, or about 0.060 nm or less, or about 0.050 nm or less, or about 0.040 nm or less, or about 0.030 nm or less, or about 0.020 nm or less, or about 0.010 nm or less, or about 0.008 nm or less, or about 0.005 nm or less, or about 0.001 nm or less. In some embodiments, the thickness is in the range of about 0.001 nm to about 0.100 nm, or about 0.005 nm to about 0.090 nm, or about 0.005 nm to about 0.080 nm, or about 0.008 nm to about 0.070 nm, or about 0.008 nm to about 0.060 nm, or about 0.010 nm to about 0.050 nm, or about 0.020 nm to about 0.040 nm, or about 0.020 nm to about 0.030 nm, or any range covering these endpoints.
[0041] Each of the multiple layers of the ALD coating 30 formed by layer-by-layer deposition through an ALD coating cycle (e.g., first layer 32, second layer 34) may have a thickness of about 2 nm or greater, or about 5 nm or greater, or about 10 nm or greater, or about 15 nm or greater, or about 20 nm or greater, or about 25 nm or greater, or about 30 nm or greater, or about 35 nm or greater, or about 40 nm or greater. Alternatively or alternatively, each of the multiple layers of the ALD coating 30 (e.g., first layer 32, second layer 34) may have a thickness of about 40 nm or less, or about 35 nm or less, or about 30 nm or less, or about 25 nm or less, or about 20 nm or less, or about 15 nm or less, or about 10 nm or less, or about 5 nm or less, or about 2 nm or less. In some embodiments, the thickness is in the range of about 2 nm to about 40 nm, or about 5 nm to about 35 nm, or about 10 nm to about 30 nm, or about 15 nm to about 25 nm, or about 20 nm to about 25 nm, or any range covering these endpoints.
[0042] The coated optical component 10 may also include a capping layer 40 disposed on and outside the ALD coating 30. The capping layer 40 may comprise, for example, silicon dioxide (SiO2). In embodiments, the material of the capping layer 40 is doped with one or more dopants, such as fluorine. The capping layer 40 can provide numerous benefits to the ALD coating 30, including improved environmental stability and laser exposure durability.
[0043] The substrate 20 may comprise any material capable of supporting the ALD coating 30. In some embodiments, the substrate 20 is a substrate comprising, for example, glass, glass-ceramic, or ceramic, such as silicate glass, soda-lime glass, alkali aluminosilicate glass, alkali borosilicate glass, alkali aluminosilicate glass, and / or fused silica. Exemplary glass substrates include, but are not limited to, HPFS sold by Corning Incorporated of Corning, New York, under glass codes 7980, 7979, and 8655. ® Molten silica, and EAGLE XG, also sold by Corning Incorporated in Corning, New York. ® Borosilicate glass. Other glass substrates include, but are not limited to, Lotus glass sold by Corning Incorporated, Corning, New York. TM NXT Glass, Iris TM Glass, Willow ® Glass, GORILLA ® Glass, Valor ®Glass or PYREX ® Glass. In some embodiments, the glass or glass-ceramic has a silica content of 50 wt.% or more, 60 wt.% or more, 70 wt.% or more, 80 wt.% or more, 90 wt.% or more, or 95 wt.% or more on an oxide basis. Exemplary glass-ceramics include, for example, lithium disilicate, nepheline, β-spodumene, and β-quartz. Exemplary commercially available materials include, for example, Macor sold by Corning Incorporated, Corning, NY. ® and Pyroceram ® In some embodiments, the substrate 20 is a glass, glass-ceramic, or ceramic comprising a metal, a metal fluoride (e.g., calcium fluoride (CaF2), magnesium fluoride (MgF2)), a metal alloy, and / or a metalloid. In some exemplary embodiments, the substrate 20 comprises aluminum, an aluminum alloy, silicon, or a combination of these materials. In some exemplary embodiments, the substrate 20 comprises silicon.
[0044] As described above, the substrate 20 may have one or more surfaces 22 with steep curvature. The steepness of each surface 22 may have a steepness value in the range of 0.5 to 1.0, where the steepness value is equal to the radius of curvature of the surface 22 divided by the aperture of the coated optical component 10, as shown in the following equation:
[0045] S = R / #
[0046] Where S is the steepness value, R is the radius of curvature of surface 22, and # is the aperture of the coated optical component 10. A steepness value in the range of 0.5 to 1.0 helps to focus DUV and / or broadband spectral light to an intensity suitable for accurate detection resolution in an optical inspection system (such as optical inspection system 100). "Aperture" is the diameter through which light passes through the optical component during its intended use. In some cases, "aperture" can be the diameter of the entire optical component measured between relative points on its peripheral edge. In some cases, for example, if the optical component is surrounded by a frame that ends above its peripheral edge, the "aperture" can be smaller than the diameter of the entire optical component. For non-circular optical components, "aperture" is the maximum external cross-sectional dimension through which light passes through the optical component during its intended use.
[0047] In this embodiment, the substrate 20 is in direct contact with the ALD coating 30, without any intermediate coating or other material placed between the substrate 20 and the ALD coating 30.
[0048] The substrate 20 can be coated with ALD coating 30 using an ALD coating system 200, such as... Figure 4As schematically illustrated, the ALD coating system 200 includes an ALD chamber 202 that supports and accommodates a substrate 20 during the coating process. The ALD chamber 202 may be a sealed chamber, and in embodiments, the sealed chamber is heated by one or more heating devices 204 that are in thermal communication with the ALD chamber 202. Similarly, as... Figure 4 As shown, the ALD chamber 202 includes an inlet 206 and an outlet 208. The inlet 206 is configured to introduce various components used in the ALD coating process into the ALD chamber 202, as discussed further below. The outlet 208 is configured to remove various components from the ALD chamber 202. In an embodiment, the outlet 208 is in fluid communication with a throttle valve 210 located downstream of the ALD chamber 202. The throttle valve 210 is configured to control the flow rate of components exiting the ALD chamber 202. The ALD coating system 200 also includes a vacuum pump 212 coupled to the outlet 208 and located downstream of the throttle valve 210. The vacuum pump 212 is configured to create a vacuum within the ALD chamber 202 to draw in ALD reactive components and extract unreacted components, reaction products, inert gases, and other materials from the ALD chamber 202.
[0049] The ALD coating system 200 also includes one or more sources of reactants in fluid communication with inlet 208. Specifically, the ALD coating system 200 may include a metal precursor reservoir 220 that contains a metal precursor 225 and is in fluid communication with inlet 208. One or more inert gases (such as argon) may also be in fluid communication with inlet 208 to facilitate the delivery of the metal precursor 225 into the ALD chamber 202. A metal precursor control valve 222 may be located between the metal precursor reservoir 220 and the ALD chamber 202 and is operable to control the flow rate of the metal precursor 225 into the ALD chamber 202. The ALD coating system 200 may also include a fluorine reservoir 230 containing a fluorine source 235, an oxygen reservoir 240 containing an oxygen source 245, and an inert gas reservoir 250 containing one or more inert gases 255. Fluorine source 235, oxygen source 245, and / or inert gas 255 can flow into ALD chamber 202 through inductively coupled plasma (ICP) reactor 207. Fluorine source control valve 232 can be located between fluorine reservoir 230 and reactor 207 and is operable to control the flow rate of fluorine source 235 into reactor 207. Oxygen source control valve 242 can be located between oxygen reservoir 240 and reactor 207 and is operable to control the flow rate of oxygen source 245 into reactor 207. Inert gas source control valve 252 can be located between inert gas reservoir 250 and reactor 207 and is operable to control the flow rate of inert gas 255 into reactor 207.
[0050] The metal precursor 225 may be in vapor, solid, liquid, or atomized liquid form. Depending on the desired metal composition of the ALD coating 30, the metal precursor 225 may comprise one or more of the following: lanthanum precursor, gadolinium precursor, aluminum precursor, magnesium precursor, lithium precursor, and calcium precursor. In some exemplary embodiments, when the ALD coating 30 comprises LaF3, the metal precursor 225 comprises lanthanum metallocene (e.g., La(isopropylcyclopentadienyl)2(isopropylamidinyl)), tris(N,N'-diisopropylmethylamidinyl)lanthanum, (2,2,6,6-tetramethyl-3,5-heptadecyl)lanthanum, tris[N,N-bis(trimethylsilyl)amide]lanthanum(III), tris(tetramethylcyclopentadienyl)lanthanum(III), or LANA from Air Liquide. TM Branded lanthanum precursors and their combinations.
[0051] Alternatively, the metal precursor 225 may comprise tris(N,N'-isopropylacetamidine)gadolinium, tris(isopropylcyclopentadienyl)gadolinium(III) (Gd(iPrCp)3), tris(OCMe2CH2OMe)gadolinium(III) (Gd(mmp)3), tris(2,3-dimethyl-2-butoxy)gadolinium(III) (Gd(DMB)3), tris(2,2,6,6-tetramethyl-3,5-heptanedionyl)gadolinium(III) (Gd(thd)3), or GANBETTA, which is available from Air Liquide. TM GAUDI, a brand of gadolinium precursors, is available from Air Liquide. TM Branded gadolinium precursors and their combinations.
[0052] Alternatively, metal precursor 225 may comprise a metal ligand complex including aluminum, trimethylamine (TMA), aluminum dimethylisopropoxy (DMAI), aluminum dimethylhydride:dimethylethylamine, ethylpiperidine:dimethylaluminum hydride, aluminum dimethylchloride (DMAC), aluminum hexafluoroacetylacetonate (Al(hfac)3), triisobutylaluminum (Al(i-Bu)3), tris(2,2,6,6-tetramethyl-3,5-heptanedionyl)aluminum (Al(TMHD)3), a magnesium-containing metal ligand complex, bis(ethylcyclopentadienyl)magnesium, bis(cyclopentadienyl)magnesium(II), bis(2,2,6,6-tetramethyl-3,5-heptanedionyl)magnesium, bis(N,N'-disec-butylacetamidine)magnesium, bis(pentamethylcyclopentadienyl)magnesium, Ca(2,2,6,6-tetramethyl-3,5-heptanedionyl) 2、Bis(N,N'-diisopropylformamidinyl)calcium(II), bis(N,N'-diisopropylacetamidine)calcium(II), [Ca3(2,2,6,6-tetramethyl-3,5-heptanedionyl)6], Ca(1,2,4-triisopropylcyclopentadienyl)2], lithium tert-butoxide, 2,2,6,6-tetramethyl-3,5-heptanedionyllithium and combinations thereof.
[0053] Fluorine source 235 may be derived from a fluorinated precursor selected from the group consisting of sulfur hexafluoride (SF6), nitrogen trifluoride (NF3), ammonium fluoride (NH4F), methyl trifluoroiodide (CF3I), hydrogen fluoride (HF), and combinations thereof. In embodiments, the ALD process is a plasma-assisted ALD process, wherein the fluorine source is a plasma fluorine source derived from a fluorinated precursor or a fluorinated precursor and argon (Ar) plasma. The fluorine source may comprise, for example, plasma comprising SF6, SF6 and Ar (SF6 / Ar) or NF3 and Ar (NF3 / Ar). In embodiments, the fluorine source may be derived from one or more organic fluorine sources, such as, but not limited to, hexafluoroacetylacetone or other fluorinated organic compounds.
[0054] In some exemplary embodiments, the fluorine source 235 comprises SF6 or SF6-derived plasma (i.e., SF6-based plasma). In embodiments, the fluorine source 235 may comprise, consist of, or substantially consist of: an SF6-based fluorine source, such as SF6 or SF6-based plasma. In embodiments, the fluorine source 235 may comprise, consist of, or substantially consist of: a plasma derived from SF6 and argon (i.e., SF6 / Ar plasma) and / or another inert gas. When the fluorine source 235 contains SF6 / Ar plasma, the flow rate ratio of Ar to SF6 can be 0.1:1 to 10:1, 0.1:1 to 5:1, 0.1:1 to 2:1, 0.5:1 to 10:1, 0.5:1 to 5:1, 0.5:1 to 2:1, 1:1 to 10:1, 1:1 to 5:1, 1:1 to 2:1, 2:1 to 10:1, 2:1 to 5:1, or approximately 2:1, where the flow rate is a volumetric flow rate expressed in sccm (standard cubic centimeters per minute). SF6 is advantageous as a fluorine source because its use is safer than, for example, HF, which is hazardous and highly corrosive, especially in contact with water.
[0055] Oxygen source 245 may include water (H2O), H2O plasma, ozone (O3), O3 plasma, oxygen (O2), O2 plasma, hydrogen peroxide (H2O2), H2O2 plasma, other oxygen-containing gases, other oxygen-containing liquids, or combinations thereof. Oxygen source 245 may be in a liquid, gaseous, or plasma state.
[0056] The inert gas 255 may include non-reactive gases, such as, but not limited to, rare gases (e.g., Ar, He, Ne, etc.). The inert gas 255 may be used as a carrier gas for delivering the precursor into the ALD chamber 202.
[0057] The ALD coating process can begin by placing a substrate 20 in an ALD chamber 202. During the ALD coating process, in a single ALD coating cycle, the substrate 20 is exposed to alternating pulses of one or more precursor compounds (e.g., metal precursor 225, fluorine source 235, oxygen source 245), wherein the alternating pulses of exposure to the precursor compounds cause an ALD coating 30 to be deposited layer by layer onto the surface of the substrate 20, wherein the thickness of each layer is comparable to the size of a single molecule of the ALD coating material (e.g., a monolayer cover of the surface). The ALD coating process is capable of coating all surfaces of the substrate 20 with atomic-layer precision in a single deposition run.
[0058] In an embodiment, the ALD coating process can be a direct reduction ALD process, during which a metal precursor 225 is deposited onto the surface 22 of a substrate 20 and then directly reduced using a fluorine source 235 as a reducing agent. Specifically, the surface 22 of the substrate 20 can be exposed within an ALD chamber 202 to alternating pulses of the metal precursor 225 and the fluorine source 235. The pulses of the metal precursor 225 may include the metal precursor 225 and one or more inert gases 255, which serve as carrier gases for delivering the metal precursor 225 into the ALD chamber 202.
[0059] Figure 5 An exemplary cycle of the ALD coating process is shown, wherein substrate 20 is exposed to one or more pulses of metal precursor 225, followed by a first purging. After the first purging, substrate 20 is exposed to one or more pulses of fluorine source 235, followed by a second purging. Figure 5 The cycle shown can produce a deposited layer of ALD coating 30 (in this embodiment, the deposited layer has a single-layer thickness). The cycle can be repeated multiple times to produce a layer-by-layer deposition of ALD coating 30 (and thus, produce multiple layers 32, 34). Although Figure 5 Two pulses of the metal precursor 225 are shown in an exemplary cycle; however, it should be noted that the substrate 20 may be exposed to more or fewer pulses of the metal precursor 225 per cycle. In embodiments, the substrate 20 may be exposed to 1 to 5 pulses, or 1 to 4 pulses, or 1 to 3 pulses, or 2 to 4 pulses, or 2 to 3 pulses of the metal precursor 225 during one cycle of the ALD coating process. Similarly, although Figure 5Only one pulse of fluorine source 235 is shown in the ALD coating process cycle; however, it should be noted that substrate 20 may be exposed to more pulses of fluorine source 235 per cycle. In the embodiments, substrate 20 may be exposed to 1 to 5 pulses, or 1 to 4 pulses, or 1 to 3 pulses, or 2 to 4 pulses, or 2 to 3 pulses of fluorine source 235 during one cycle of the ALD coating process.
[0060] In an embodiment, before introducing the metal precursor 225 into the ALD chamber 202, the metal precursor 225 is heated to approximately 95°C to approximately 200°C, or approximately 100°C to approximately 190°C, or approximately 110°C to approximately 180°C, or approximately 120°C to approximately 170°C, or approximately 130°C to approximately 160°C, or approximately 140°C to approximately 150°C, or any range of temperatures covering these endpoints. During each ALD coating cycle, the substrate 20 may be exposed to one or more pulses of the metal precursor 225 within the ALD chamber 202. The pulses of the metal precursor 225 for each ALD coating cycle may be sustained for a sufficient duration to allow the metal precursor 225 to react with at least 90%, at least 95%, at least 98%, at least 99%, or at least 99.9% of the reaction sites on the surface 22 of the substrate 20 (or the outer surface of a previously applied coating). In embodiments, each pulse of the metal precursor 225 within a single cycle of the ALD coating process can last for a duration of about 0.01 seconds to about 10 seconds, or about 0.10 seconds to about 9 seconds, or about 0.50 seconds to about 8 seconds, or about 1 second to about 7 seconds, or about 2 seconds to about 6 seconds, or about 3 seconds to about 5 seconds, or about 4 seconds to about 10 seconds, or any combination of these ranges. As an example, in some embodiments, for each ALD coating process cycle, the substrate 20 may be exposed to two pulses of the metal precursor 225, with each pulse having a duration of about 0.50 seconds. Factors affecting the pulse duration of the metal precursor 225 include the vapor pressure of the precursor, the flow rate of the precursor, the reactivity of the precursor with the surface 22 of the substrate 20, the volume of the ALD chamber 202, and the size of the substrate 20. In an embodiment, the pulse duration of the metal precursor 225 is sustained for a sufficient duration to produce at least 90%, or at least 95%, or at least 98%, or at least 99%, or at least 99.9% conformal coverage over the area of the substrate 20 to be coated (thus producing a conformal coating).
[0061] like Figure 5 As shown, during the same ALD coating cycle and after a pulse that exposes the substrate 20 to the metal precursor 225, the ALD chamber 202 can then be purged with an inert gas 255 to remove any residual metal precursor 225 from the ALD chamber 202 before continuing the ALD process.
[0062] The ALD coating process may further include exposing the substrate 20, on which the metal precursor 225 layer is adsorbed, to one or more pulses of a fluorine source 235 after purging the ALD chamber 202 with an inert gas 255 and during the same ALD coating cycle. The pulses of the fluorine source 235 for each ALD coating cycle may be sustained for a sufficient duration to allow the fluorine source 235 to react with at least 95%, at least 98%, at least 99%, or at least 99.9% of the reaction sites on the metal precursor 225 disposed on the substrate 20. In embodiments, each pulse of the fluorine source 235 within a single cycle of the ALD coating process may last for a duration of about 0.01 seconds to about 30 seconds, or about 0.10 seconds to about 28 seconds, or about 0.50 seconds to about 25 seconds, or about 1 second to about 22 seconds, or about 2 seconds to about 20 seconds, or about 3 seconds to about 15 seconds, or about 4 seconds to about 10 seconds, or about 5 seconds to about 10 seconds, or any combination of these ranges. In an embodiment, during the same ALD coating cycle, the duration of each pulse of the fluorine source 235 can be longer than the duration of each pulse of the metal precursor 225.
[0063] Similarly, Figure 5 As shown, during the same ALD coating cycle and after a pulse that exposes the substrate 20 to the fluorine source 235, the ALD chamber 202 can be purged again with inert gas 255 to remove any residual fluorine source 235 from the ALD chamber 202 before continuing the ALD process.
[0064] Figure 5 The ALD coating cycle depicted can be repeated multiple times to increase the thickness of the ALD coating. Each iteration of the ALD coating cycle adds another molecular layer of ALD coating material to the ALD coating 30 to form each of the multiple layers (e.g., first layer 32, second layer 34). The thickness of each layer (first layer 32, second layer 34), and therefore the thickness of the ALD coating 30, can be controlled by controlling the number of iterations of the ALD coating cycle, thereby controlling the number of molecular layers of ALD coating material in the ALD coating 30.
[0065] In some exemplary embodiments, as disclosed above, the ALD coating process includes using at least one La-based metal precursor as a metal precursor 225 and an SF6-Ar plasma mixture as a fluorine source 235 to produce an ALD coating 30 containing at least LaF3. Furthermore, in some exemplary embodiments, also as disclosed above, the ALD coating process includes using a Mg-based metal precursor as a metal precursor 225 and an SF6-Ar plasma mixture as a fluorine source 235 to produce a first layer 32 of the ALD coating 30, and the ALD coating process includes using a La-based metal precursor as a metal precursor 225 and an SF6-Ar plasma mixture as a fluorine source 235 to produce a second layer 34 of the ALD coating 30.
[0066] As discussed above, heating device 204 can heat ALD chamber 202 during the ALD coating process. Therefore, heating device 204 can heat ALD chamber 202 during pulse delivery of metal precursor 225 and / or fluorine source 235. In embodiments, during pulse delivery of metal precursor source 225 and / or pulse delivery of fluorine source 235, the temperature of ALD chamber 202 is heated to a processing temperature within the range of about 100°C to about 400°C, or about 125°C to about 375°C, or about 150°C to about 350°C, or about 175°C to about 325°C, or about 200°C to about 300°C, or about 225°C to about 275°C, or about 250°C to about 300°C, or any range covering these endpoints. When the temperature is too low, such as below 100°C, more impurities will form in the deposited ALD coating 30. However, when the temperature is too high, such as above 400°C or above 300°C, the deposited metal precursor begins to be etched, which slows down the growth rate of the ALD coating 30.
[0067] In embodiments where the fluorine source 235 is based on plasma, the fluorine source 235 can be converted into plasma by heating the material and subjecting it to an electric current, voltage, or a strong electromagnetic field. Specifically, as... Figure 4As shown, within reactor 207 of the ALD coating system 200, a fluorine source 235 can be exposed to an ICP to convert the fluorine source 235 into plasma. The ICP generates fluorine-containing radicals or ions in reactor 207, which subject the fluorine source 235 to an electric current, thereby converting the material into plasma. In embodiments, converting the material into plasma may involve heating the material to a temperature of about 5°C to about 20°C, or about 10°C to about 15°C, or about 12°C to about 18°C (or any range covering these endpoints), and applying an electric current having a power of about 100 watts (W) to about 400 W, or about 125 W to about 375 W, or about 150 W to about 350 W, or about 175 W to about 325 W, or about 200 W to about 300 W, or about 225 W to about 375 W, or about 250 W to about 300 W (or any range covering these endpoints).
[0068] Reactor 207 may include a remote plasma generator because the fluorine source 235 is converted into plasma located remotely from and outside the ALD chamber 202. In other embodiments, the fluorine source 235 may be converted into plasma within the ALD chamber 202.
[0069] The ALD process disclosed herein may also include cleaning the surface of the substrate 20 prior to depositing the ALD coating 30 thereon. Furthermore, the ALD process disclosed herein may include pulses exposing the substrate 20 to the metal precursor 225 and a first purging (such as...) Figure 5 (As shown in the diagram) After this, the substrate 20 is exposed to one or more pulses of oxygen source 245. Exposing the substrate 20 to such oxygen-containing pulses can oxidize the metal precursor 225 absorbed on the substrate 20 to form a metal oxide on the surface 22 of the substrate 20. The pulses of oxygen source 245 for each ALD coating process cycle can last for a sufficient duration to allow the oxygen source 245 to react with at least 95%, at least 98%, at least 99%, or at least 99.9% of the reaction sites disposed on the metal precursor 225 on the substrate 20. In embodiments, each pulse of oxygen source 245 within a single cycle of the ALD coating process can last for a duration of about 0.01 seconds to about 10 seconds, or about 0.10 seconds to about 9 seconds, or about 0.50 seconds to about 8 seconds, or about 1 second to about 7 seconds, or about 2 seconds to about 6 seconds, or about 3 seconds to about 5 seconds, or about 4 seconds to about 10 seconds, or any combination of these ranges. After the substrate 20 is exposed to the oxygen source 245 by a pulse, the ALD chamber 202 can then be purged with an inert gas 255 to remove any residual oxygen source 245 from the ALD chamber 202 before continuing the ALD process.
[0070] In the embodiments disclosed herein, the ALD coating 30 may have a total thickness sufficient to cover the surface 22 of the substrate 20 without substantially exposing the surface of the substrate 20 to the atmosphere in the coated area. In embodiments, the ALD coating 30 may have a total thickness of about 200 nm or less, or about 190 nm or less, or about 180 nm or less, or about 170 nm or less, or about 160 nm or less, or about 150 nm or less, or about 140 nm or less, or about 130 nm or less, or about 120 nm or less, or about 110 nm or less, or about 100 nm or less, or about 90 nm or less, or about 80 nm or less, or about 70 nm or less, or about 60 nm or less, or about 50 nm or less, or about 40 nm or less, or about 30 nm or less, or about 20 nm or less (which includes the combined thickness of each of the plurality of layers 32, 34). Alternatively, the ALD coating 30 may have a total thickness of about 20 nm or greater, or about 30 nm or greater, or about 40 nm or greater, or about 50 nm or greater, or about 60 nm or greater, or about 70 nm or greater, or about 80 nm or greater, or about 90 nm or greater, or about 100 nm or greater, or about 110 nm or greater, or about 120 nm or greater, or about 130 nm or greater, or about 140 nm or greater, or about 150 nm or greater, or about 160 nm or greater, or about 170 nm or greater, or about 180 nm or greater, or about 190 nm or greater, or about 200 nm or greater. In some exemplary embodiments, the total thickness is within the range of about 20 nm to about 200 nm, or about 30 nm to about 190 nm, or about 40 nm to about 180 nm, or about 50 nm to about 170 nm, or about 60 nm to about 160 nm, or about 70 nm to about 150 nm, or about 80 nm to about 140 nm, or about 90 nm to about 130 nm, or about 100 nm to about 120 nm, or about 100 nm to about 110 nm, or any range covering these endpoints.
[0071] As disclosed herein, the ALD coating 30 is an atomically dense, pinhole-free protective coating. The ALD coating process disclosed herein can advantageously produce such coatings without the expensive and time-consuming processes involved in PVD coating. Therefore, the process disclosed herein can reduce coating stress and extend the lifespan of coated optical components.
[0072] In the embodiments, the ALD coating 30 produced according to the process disclosed herein has reduced surface roughness. Specifically, the surface 22 of the substrate 20 coated with the ALD coating 30 may have a surface roughness (Ra) of about 1.5 nm or less, or about 1.25 nm or less, or about 1.00 nm or less, or about 0.75 nm or less, or about 0.60 nm or less, or about 0.50 nm or less, or about 0.40 nm or less, or about 0.30 nm or less, or about 0.20 nm or less, or about 0.10 nm or less, or about 0.05 nm or less, or about 0.01 nm or less, or any range covering these endpoints. The Ra surface roughness is determined by measuring a 2 μm × 2 μm square region using an atomic force microscope with a resolution of 512 × 512 pixels.
[0073] ALD coating 30 can be a conformal coating with a uniform thickness across all coated surfaces. In embodiments, the variation in thickness of ALD coating 30 across the entire coated area relative to the average thickness of ALD coating 30 can be less than or equal to 5%, less than or equal to 4%, less than or equal to 3%, less than or equal to 2%, less than or equal to 1%, or even less than or equal to 0.5%. The average thickness of ALD coating 30 is the thickness of ALD coating 30 averaged over the entire surface area of the surface 22 in contact with ALD coating 30. The “thickness variation” of the coating layer is calculated using the following equation:
[0074] T = SD / A × 100
[0075] Where T equals the thickness variation, SD equals the standard deviation of a representative set of thickness measurements, and A equals the average of that representative set of thickness measurements. The thickness variation is defined by the thickness variation over the entire surface area of the coating or over the entire surface area of the coating on a surface defined by a peripheral edge represented by a set of thickness measurements. In an embodiment, the ALD coating 30 may cover the entire surface 22 defined by the peripheral edge of the substrate 20. In such embodiments, the thickness variation of the ALD coating 30 is defined by the thickness variation of the ALD coating 30 disposed over the entire surface 22. The thickness values disclosed herein are measured by a spectroscopic ellipsometry. A representative set of thickness measurements includes at least three measurements. For the purpose of selecting the points for the thickness measurements, these points should be spaced apart to provide representativeness of the entire film being measured and should not all be located in a single region of the coating (i.e., not all at the edges of the coating).
[0076] In one exemplary example, using the process disclosed herein, an ALD coating 30 is applied to a 150 mm diameter substrate containing Si. In this exemplary example, the ALD coating 30 comprises a layer of LaF3 with an average thickness of 31.8 nm. The process used to produce this exemplary example includes first exposing the substrate to three separate pulses of a La-based metal precursor at a temperature of 160 °C. Each pulse lasts for 0.5 seconds. The substrate is then purged with an inert gas. Next, the substrate is exposed to one pulse of SF6 / Ar plasma, with the pulse lasting for 15 seconds. The SF6 / Ar plasma is formed by flowing SF6 and Ar materials through an ICP reactor 207 at a temperature of 200 °C while simultaneously applying an electrical power of 200 W to the materials. The flow rate ratio of Ar to SF6 is 15:30. After the pulsed delivery of the SF6 / Ar plasma, the substrate is purged with an inert gas again, thus completing one cycle of the ALD coating process. This cycle is repeated 600 times until the coating process produces a coating with an average thickness of 31.8 nm. The thickness of the resulting ALD coating was measured on the left, right, top, bottom, and center portions of the substrate to determine coating thickness uniformity. Additionally, the refractive index of the coated substrate at 550 nm was measured at these same locations. The results are shown in Table 1 below.
[0077] Table 1
[0078]
[0079] As shown in Table 1 above, the ALD coating 30 in this exemplary example has a very uniform thickness, thus advantageously providing a uniform refractive index across the entire coated substrate. The refractive index disclosed herein is obtained using CompleteEASE. TM The software uses a Cauchy model to fit data from a variable-angle spectral ellipsometer (Woollam VUV-Vase ellipsometer, scanning wavelengths from 150 nm to 1600 nm, incident angles from 45 degrees to approximately 80 degrees) for measurement.
[0080] Figure 6 A plot of the refractive index versus wavelength is shown for a first optical component 300 and a second optical component 310. The first optical component comprises a glass substrate coated with a 24 nm thick LaF3 ALD coating using the methods disclosed herein, and the second optical component comprises the same glass substrate but coated with a 35 nm thick LaF3 PVD coating. Figure 6As shown, both the first optical component 300 and the second optical component 310 have similar refractive index values within the indicated wavelength range, indicating that the ALD coating process disclosed herein provides coating uniformity similar to that of the PVD process. Specifically, both the first optical component 300 and the second optical component 310 have a refractive index of 1.72 at 193 nm. Furthermore, the first optical component 300 has a refractive index of 1.61 at 550 nm, and the second optical component 310 has a very similar refractive index of 1.60 at 550 nm.
[0081] In embodiments, the ALD coating 30 produced using the embodiments disclosed herein may be substantially carbon-free. In embodiments, the ALD coating 30 may have a carbon concentration of about 10,000 ppm or less, or about 5,000 ppm or less, or about 1,000 ppm or less, or less than about 500 ppm or less, or about 100 ppm or less, or any range covering these endpoints. The ALD coating 30 may have a carbon content of about 1.2 atomic percent or less, or about 1 atomic percent or less, at a depth of 0.02 micrometers measured using secondary ion mass spectrometry. In some embodiments, at a depth of 0.02 micrometers measured using secondary ion mass spectrometry, the carbon content is in the range of about 0.01 atomic percent to about 1.2 atomic percent, or in the range of about 0.01 atomic percent to about 1 atomic percent. Specifically, carbon content was measured using a Cs micro-beam ion gun with the following parameters: (i) energy (volts) 1000, (ii) scan size - X: 400.0 micrometers (µm), (iii) scan size - Y: 400.0 micrometers (µm), (iv) beam current: 20 nanoamps (nA), (v) main beam angle: 45 degrees, and (vi) sputtering rate: 2.9 × 10⁻⁶ -5 Micrometers per second. Data were normalized based on standard samples with controlled carbon concentrations.
[0082] In embodiments, the ALD coating 30 produced using the embodiments disclosed herein may also be substantially sulfur-free. In embodiments, the ALD coating 30 may have a sulfur concentration of about 1,000 ppm or less, or about 750 ppm or less, or about 500 ppm or less, or about 250 ppm or less, or about 200 ppm or less, or about 150 ppm or less, or about 100 ppm or less, or about 75 ppm or less, or about 50 ppm or less, or about 40 ppm or less, or about 30 ppm or less, or less than about 20 ppm or less, or about 10 ppm or less, or about 5 ppm or less, or about 1 ppm or less, or any range covering these endpoints. Alternatively, the ALD coating 30 may have a sulfur content greater than 0 ppm, such as greater than 0 ppm to about 1,000 ppm or less, or greater than 0 ppm to about 750 ppm or less, or greater than 0 ppm to about 500 ppm or less, or greater than 0 ppm to about 250 ppm or less, or greater than 0 ppm to about 200 ppm or less, or greater than 0 ppm to about 150 ppm or less, or greater than 0 ppm to about 100 ppm or less, or greater than 0 ppm to about 75 ppm or less, or greater than 0 ppm to about 50 ppm or less, or greater than 0 ppm to about 40 ppm or less, or greater than 0 ppm to about 30 ppm or less, or greater than 0 ppm to about 20 ppm or less, or greater than 0 ppm to about 10 ppm or less, or greater than 0 ppm to about 5 ppm or less, or greater than 0 ppm to about 1 ppm or less. Sulfur content was measured using a Cs micro-beam ion gun with the following parameters: (i) energy (volts) 1000, (ii) scan size - X: 400.0 micrometers (µm), (iii) scan size - Y: 400.0 micrometers (µm), (iv) beam current: 20 nanoamps (nA), (v) main beam angle: 45 degrees, and (vi) sputtering rate: 2.9 × 10⁻⁶. -5 Micrometers per second. Data were normalized based on standard samples with controlled sulfur concentrations.
[0083] In embodiments, the ALD coating 30 produced using the embodiments disclosed herein may be substantially oxygen-free. In embodiments, the ALD coating 30 may have an oxygen concentration of about 10,000 ppm or less, or about 5,000 ppm or less, or about 1,000 ppm or less, or less than about 500 ppm or less, or about 100 ppm or less, or any range covering these endpoints. The ALD coating 30 may have an oxygen content of about 1.2 atomic percent or less, or about 1 atomic percent or less, at a depth of 0.02 micrometers measured using secondary ion mass spectrometry. In some embodiments, at a depth of 0.02 micrometers measured using secondary ion mass spectrometry, the oxygen content is in the range of about 0.01 atomic percent to about 1.2 atomic percent, or in the range of about 0.01 atomic percent to about 1 atomic percent. Specifically, oxygen content was measured using a Cs micro-beam ion gun with the following parameters: (i) energy (volts) 1000, (ii) scan size - X: 400.0 micrometers (µm), (iii) scan size - Y: 400.0 micrometers (µm), (iv) beam current: 20 nanoamps (nA), (v) main beam angle: 45 degrees, and (vi) sputtering rate: 2.9 × 10⁻⁶ -5 Micrometers per second. Data were normalized based on standard samples with controlled oxygen concentrations.
[0084] Figure 7A and 7A Another exemplary embodiment of an ALD coating 500 produced using the methods disclosed herein is shown. Figure 7A and 7B As shown, the ALD coating 500 in this embodiment comprises two first layers 32 containing MgF2 and one second layer 34 containing LaF3. Furthermore, the ALD coating 500 is deposited on a CaF2 substrate. Figure 7A and 7B The thickness values of each layer of ALD coating 500 are shown. ALD coating 500 was subjected to a humidity test to determine its stability as an AR coating. The humidity test consisted of placing the coated substrate in an 80% humid atmosphere at 80°C for 6 hours. The reflectance of ALD coating 500 was measured before and after the humidity test, and the results are shown in [the table / image / image]. Figure 8 Specifically, reference numeral 510 shows the reflectance of the ALD coating 500 before the humidity test at an incident (θ) angle of 15 degrees, and reference numeral 520 shows the reflectance of the ALD coating 500 after the humidity test. Figure 8 As shown, the reflectivity of the ALD coating 500 is very similar before and after the humidity test, demonstrating the durability and stability of the coating.
[0085] In embodiments, the ALD coating produced using the embodiments disclosed herein is an AR coating. In some embodiments, the ALD coating 30 has an optical absorptivity value of about 1% or less, or about 0.75% or less, or about 0.5% or less for light in the DUV range of wavelengths from 157 nm to 266 nm and at all incident angles (θ) within a range of 15 degrees or less. Therefore, the optical absorptivity values disclosed herein are for each wavelength in the DUV range of 157 nm to 266 nm. An “optical absorptivity value” is the percentage of light absorbed by a material layer or film for a given wavelength and a given incident angle (θ). Light absorption means that photons of light are neither reflected from nor pass through the layer or film, but are instead absorbed by the layer or film and released as energy, typically as heat. A given wavelength can be a specific wavelength value or a range of wavelength values. For a range of wavelength values, the optical absorptivity is calculated by averaging the optical absorptivity over each integer wavelength in the wavelength range. An incident angle (θ) is the angle at which light is incident on the surface of a material layer or film, measured relative to a line perpendicular to the surface of the material layer or film at the incident position.
[0086] The optical absorptivity values described herein were measured according to the following procedure. The material film to be tested was deposited on an 8655 fused silica substrate. The material film was deposited on opposite sides of the fused silica substrate, and the total optical absorptivity of the film across both sides of the substrate was determined. Optical transmittance and optical reflectance were measured using an Agilent Cary 5000UV-Vis-NIR spectrophotometer with a wavelength range of 400 nm to 200 nm. The following instrument parameters were used: (i) incident angle: within 15 degrees or less, (ii) data interval: 1 nm, 150 nm / min, and (iii) average measurement time: 0.4 seconds. No polarizer was used. The transmittance and reflectance measurements were corrected to correspondences between the true surface reflectance and transmittance of 8655 fused silica and the measured surface reflectance and transmittance. This correlation used the standard Fresnel equation for s-polarized and p-polarized reflectance intensities. The optical absorptivity was calculated using the following formula:
[0087] %A=100 - %T - %R
[0088] Where: %A equals the optical absorptivity, %T equals the percentage of transmitted light, and %R equals the percentage of reflected light.
[0089] In the embodiments, the ALD coating 30 produced using the embodiments disclosed herein has an optical transmittance value of approximately 94% or greater, or approximately 95% or greater, or approximately 96% or greater, or approximately 97% or greater, or approximately 98% or greater, or approximately 99% or greater for light at all incident angles (θ) within a range of 15 degrees or less in the DUV range of wavelengths from 157 nm and 193 nm to 266 nm. Therefore, the optical transmittance disclosed herein, which is an “optical transmittance value” for each wavelength in the DUV range of 157 nm and 193 nm to 266 nm, is the percentage of light passing through the material layer or film for a given wavelength and a given incident angle (θ). The given wavelength can be a specific wavelength value or a range of wavelength values. For a range of wavelength values, the optical transmittance is calculated by averaging the optical transmittance over each integer wavelength in the wavelength range. The optical transmittance values disclosed in this paper were measured using an Agilent Cary 5000 UV-Vis-NIR spectrophotometer according to the measurement procedures discussed above.
[0090] In the embodiments, the ALD coating 30 produced using the embodiments disclosed herein has an optical reflectance value of about 5% or less, or about 4% or less, or about 3% or less, or about 2% or less, or about 1% or less for light at all incident angles (θ) within the DUV range of 157 nm and 193 nm to 266 nm, and within a range of 15 degrees or less. Therefore, the optical reflectance disclosed herein is for each wavelength within the DUV range of 157 nm and 193 nm to 266 nm. An “optical reflectance value” is the percentage of light reflected from the surface of a material layer or film for a given wavelength and a given incident angle (θ). The given wavelength can be a specific wavelength value or a range of wavelength values. For a range of wavelength values, the optical reflectance is calculated by averaging the optical reflectance over each integer wavelength within the wavelength range. The optical reflectance values disclosed herein were measured using an Agilent Cary 5000 UV-Vis-NIR spectrophotometer according to the measurement procedures discussed above.
[0091] In this embodiment, the coated optical component 10 is a high-NA objective lens coated with a LaF3 / MgF2 or LaF3 / AlF3 ALD coating. In this embodiment, the ALD coating is an AR coating.
[0092] According to a first aspect, a coated optical component comprises: a substrate having at least one surface; and an atomic layer deposition coating deposited on the surface of the substrate, the atomic layer deposition coating comprising a first layer of lanthanum fluoride. Furthermore, the atomic layer deposition coating has a carbon concentration of about 10,000 ppm or less, an oxygen concentration of about 10,000 ppm or less, and a sulfur concentration of about 500 ppm or less.
[0093] According to the second aspect, the coated optical component according to the first aspect, wherein the atomic layer deposition coating comprises at least a second layer of magnesium fluoride or aluminum fluoride.
[0094] According to a third aspect, the coated optical component according to the first or second aspect, wherein the atomic layer deposition coating comprises a first layer of two lanthanum fluoride layers and a second layer of magnesium fluoride layer.
[0095] According to a fourth aspect, a coated optical component according to any one of the first to third aspects, wherein the surface of the substrate has a steepness value in the range of 0.5 to 1.0, the steepness value being equal to the radius of curvature of the surface divided by the aperture of the coated optical component.
[0096] According to the fifth aspect, the coated optical component according to any one of the first to fourth aspects, wherein the thickness of the first layer of the atomic layer deposition coating is in the range of about 2 nm to about 50 nm.
[0097] According to a sixth aspect, the coated optical component according to the fifth aspect, wherein the thickness of the first layer of the atomic layer deposition coating is in the range of about 10 nm to about 30 nm.
[0098] According to the seventh aspect, the coated optical component according to the sixth aspect, wherein the total thickness of the atomic layer deposition coating is in the range of about 20 nm to about 200 nm.
[0099] According to the eighth aspect, the coated optical component according to the seventh aspect, wherein the total thickness of the atomic layer deposition coating is in the range of about 40 nm to about 180 nm.
[0100] According to the ninth aspect, the coated optical component according to any one of the first to eighth aspects, wherein the atomic layer deposition coating comprises at least a plurality of layers, the plurality of layers including the first layer and the second layer, the first layer comprising a metal fluoride different from the second layer.
[0101] According to the tenth aspect, the coated optical component according to the ninth aspect, wherein the refractive index of the second layer is higher than that of the first layer.
[0102] According to the eleventh aspect, the coated optical component according to the tenth aspect, wherein the refractive index of the second layer is in the range of about 1.65 to about 1.75.
[0103] According to the twelfth aspect, the coated optical component according to the tenth aspect, wherein the refractive index of the first layer is in the range of about 1.30 to about 1.60.
[0104] According to the thirteenth aspect, the coated optical component according to any one of the first to twelfth aspects, wherein the atomic layer deposition coating has a surface area (Ra) of about 1.5 nm or less.
[0105] According to the fourteenth aspect, the coated optical component according to the thirteenth aspect, wherein the surface roughness (Ra) is about 1.00 nm or less.
[0106] According to the fifteenth aspect, the coated optical component according to the fourteenth aspect, wherein the surface roughness (Ra) is about 0.75 nm or less.
[0107] According to the sixteenth aspect, the coated optical component according to any one of the first to fifteenth aspects, wherein the thickness of the atomic layer deposition coating varies across the entire surface with respect to the average thickness of the atomic layer deposition coating by about 5% or less.
[0108] According to the seventeenth aspect, the coated optical component according to any one of the first to sixteenth aspects, wherein the carbon concentration of the atomic layer deposition coating is about 5,000 ppm or lower.
[0109] According to the eighteenth aspect, the coated optical component according to any one of the first to seventeenth aspects, wherein the oxygen concentration of the atomic layer deposition coating is about 5,000 ppm or lower.
[0110] According to the nineteenth aspect, the coated optical component according to any one of the first to eighteenth aspects, wherein the sulfur concentration of the atomic layer deposition coating is about 100 ppm or lower.
[0111] According to the twentieth aspect, the coated optical component according to any one of the first to nineteenth aspects, wherein the atomic layer deposition coating has an optical absorptivity value of about 1% or less for light at all incident angles (θ) in the wavelength range of 193 nm to 266 nm and in the range of 15 degrees or less.
[0112] According to the twenty-first aspect, the coated optical component according to any one of the first to twentieth aspects, wherein the atomic layer deposition coating has an optical transmittance value of about 94% or greater for light at all incident angles (θ) in the wavelength range of 193 nm to 266 nm and in the range of 15 degrees or less.
[0113] According to the twenty-second aspect, the coated optical component according to any one of the first to twenty-first aspects, wherein the atomic layer deposition coating has an optical reflectivity value of about 5% or less for light at all incident angles (θ) in the wavelength range of 193 nm to 266 nm and in the range of 15 degrees or less.
[0114] According to the twenty-first aspect, and the twenty-second aspect, the coated optical component, wherein the atomic layer deposition coating has an optical reflectivity value of about 0.5% or less for light with a wavelength of 193 nm and at all incident angles (θ) in the range of 15 degrees or less.
[0115] According to the twenty-fourth aspect, a coated optical component according to any one of the first to twenty-third aspects, wherein the substrate is a lens, window, objective lens, prism, beam splitter, filter and / or mirror.
[0116] According to aspect twenty-five, a coated optical component according to any one of aspects one to twenty-four, wherein the substrate comprises calcium fluoride, magnesium fluoride, silicon, or silicate glass.
[0117] According to the twenty-sixth aspect, the coated optical component according to the twenty-fifth aspect, wherein the substrate comprises calcium fluoride.
[0118] According to a twenty-seventh aspect, a method of coating an optical component with an atomic layer deposition coating, the method comprising: converting a fluorine source into a sulfur hexafluoride-based plasma by generating a plasma of a fluorine source while applying a current having a power of about 100 watts to about 400 watts at a temperature of about 5°C to about 20°C; and exposing the surface of a substrate to a cycle of the atomic layer deposition coating process in an atomic layer deposition chamber by: (i) exposing the surface of the substrate to one or more pulses of a lanthanum-based metal precursor while heating the substrate to a temperature of about 100°C to about 400°C; and (ii) exposing the surface of the substrate to one or more pulses of the sulfur hexafluoride-based plasma while heating the substrate to a temperature of about 100°C to about 400°C.
[0119] According to aspect twenty-eight, and according to the method of aspect twenty-seven, the sulfur hexafluoride-based plasma is derived from sulfur hexafluoride and argon.
[0120] According to the twenty-ninth aspect, the method according to the twenty-seventh aspect or the twenty-eighth aspect, the duration of each pulse of the lanthanum-based metal precursor is from about 0.01 seconds to about 10 seconds.
[0121] According to the thirtieth aspect, and the method according to the twenty-ninth aspect, wherein the cycle comprises two or more pulses of the lanthanum-based metal precursor.
[0122] According to the thirty-first aspect, and the method according to any one of the twenty-seventh to thirtieth aspects, the duration of each pulse of the sulfur hexafluoride-based plasma is from about 0.01 seconds to about 30 seconds.
[0123] According to aspect thirty-two, and according to the method of aspect thirty-one, the cycle comprises a pulse of the sulfur hexafluoride-based plasma.
[0124] According to aspect thirty-three, and the method of any one of aspects twenty-seven to thirty-two, the duration of each pulse of the sulfur hexafluoride-based plasma is longer than the duration of each pulse of the lanthanum-based metal precursor.
[0125] According to the thirty-fourth aspect, and the method according to any one of the twenty-seventh to thirty-third aspects, wherein the cycle deposits a first deposited layer of the atomic layer deposition coating on the surface of the substrate, and the method further comprises repeating the cycle to deposit a second deposited layer of the atomic layer deposition coating on the surface of the substrate.
[0126] According to aspect thirty-five, and the method according to any one of aspects twenty-seven to thirty-four, it further comprises heating the atomic layer deposition chamber to a temperature of about 10°C to about 15°C while exposing the surface of the substrate to the pulses of the lanthanum-based metal precursor and the sulfur hexafluoride-based plasma.
[0127] According to the thirty-sixth aspect, and the method according to any one of the twenty-seventh to thirty-fifth aspects, it further comprises converting the fluorine source into the sulfur hexafluoride-based plasma by heating the fluorine source to a temperature of about 10°C to about 15°C and applying the current having a power of about 125 watts to about 375 watts.
[0128] It will be apparent to those skilled in the art that various modifications and variations can be made to the embodiments described herein without departing from the spirit and scope of the claimed subject matter. Therefore, this specification is intended to cover modifications and variations of the various embodiments described herein, provided that such modifications and variations fall within the scope of the appended claims and their equivalents.
Claims
1. A coated optical component comprising: A substrate, the substrate comprising at least one surface; and An atomic layer deposition coating is deposited on at least one surface of the substrate, the atomic layer deposition coating comprising a first layer of lanthanum fluoride. The atomic layer deposition coating has a carbon concentration of about 10,000 ppm or less, an oxygen concentration of about 10,000 ppm or less, and a sulfur concentration of about 500 ppm or less.
2. The coated optical component of claim 1, wherein the atomic layer deposition coating comprises at least a second layer comprising magnesium fluoride or aluminum fluoride.
3. The coated optical component according to claim 1 or claim 2, wherein the atomic layer deposition coating comprises a first layer of two lanthanum fluoride layers and a second layer of magnesium fluoride layer.
4. The coated optical component according to any one of claims 1 to 3, wherein the surface of the substrate has a steepness value in the range of 0.5 to 1.0, the steepness value being equal to the radius of curvature of the surface divided by the aperture of the coated optical component.
5. The coated optical component according to any one of claims 1 to 4, wherein the thickness of the first layer of the atomic layer deposition coating is in the range of about 2 nm to about 50 nm.
6. The coated optical component of claim 5, wherein the thickness of the first layer of the atomic layer deposition coating is in the range of about 10 nm to about 30 nm.
7. The coated optical component of claim 6, wherein the total thickness of the atomic layer deposition coating is in the range of about 20 nm to about 200 nm.
8. The coated optical component of claim 7, wherein the total thickness of the atomic layer deposition coating is in the range of about 40 nm to about 180 nm.
9. The coated optical component according to any one of claims 1 to 8, wherein the atomic layer deposition coating comprises at least a plurality of layers, the plurality of layers including the first layer and the second layer, the first layer comprising a metal fluoride different from the second layer.
10. The coated optical component of claim 9, wherein the refractive index of the second layer is higher than that of the first layer at a wavelength of 193 nm.
11. The coated optical component of claim 10, wherein the refractive index of the second layer is in the range of about 1.65 to about 1.75 at a wavelength of 193 nm.
12. The coated optical component of claim 10, wherein the refractive index of the first layer is in the range of about 1.30 to about 1.60 at a wavelength of 193 nm.
13. The coated optical component according to any one of claims 1 to 12, wherein the atomic layer deposition coating has a surface area (Ra) of about 1.5 nm or less.
14. The coated optical component of claim 13, wherein the surface roughness (Ra) is about 1.00 nm or less.
15. The coated optical component of claim 14, wherein the surface roughness (Ra) is about 0.75 nm or less.
16. The coated optical component according to any one of claims 1 to 15, wherein the thickness of the atomic layer deposition coating varies across the entire surface with respect to the average thickness of the atomic layer deposition coating by about 5% or less.
17. The coated optical component according to any one of claims 1 to 16, wherein the carbon concentration of the atomic layer deposition coating is about 5,000 ppm or less.
18. The coated optical component according to any one of claims 1 to 17, wherein the oxygen concentration of the atomic layer deposition coating is about 5,000 ppm or lower.
19. The coated optical component according to any one of claims 1 to 18, wherein the sulfur concentration of the atomic layer deposition coating is about 100 ppm or less.
20. The coated optical component according to any one of claims 1 to 19, wherein the atomic layer deposition coating has an optical absorptivity value of about 1% or less for light at all incident angles (θ) within the range of wavelengths from 193 nm to 266 nm and within the range of 15 degrees or less.
21. The coated optical component according to any one of claims 1 to 20, wherein the atomic layer deposition coating has an optical transmittance value of about 94% or greater for light at all incident angles (θ) in the range of wavelengths from 193 nm to 266 nm and in the range of 15 degrees or less.
22. The coated optical component according to any one of claims 1 to 21, wherein the atomic layer deposition coating has an optical reflectivity value of about 5% or less for light at all incident angles (θ) within the range of wavelengths from 193 nm to 266 nm and within the range of 15 degrees or less.
23. The coated optical component of claim 22, wherein the atomic layer deposition coating has an optical reflectivity value of about 0.5% or less for light at all incident angles (θ) with a wavelength of 193 nm and in the range of 15 degrees or less.
24. The coated optical component according to any one of claims 1 to 23, wherein the substrate is a lens, window, objective lens, prism, beam splitter, filter and / or mirror.
25. The coated optical component according to any one of claims 1 to 24, wherein the substrate comprises calcium fluoride, magnesium fluoride, silicon, or silicate glass.
26. The coated optical component of claim 25, wherein the substrate comprises calcium fluoride.
27. A method for coating an optical component with an atomic layer deposition coating, the method comprising: Converting the fluorine source into sulfur hexafluoride-based plasma; and In an atomic layer deposition chamber, the surface of the substrate is exposed to an atomic layer deposition coating process cycle in the following manner: Exposing the surface of the substrate to one or more pulses of a lanthanum-based metal precursor; and The surface of the substrate is exposed to one or more pulses of the sulfur hexafluoride-based plasma.
28. The method of claim 27, further comprising: The fluorine source is converted into a sulfur hexafluoride-based plasma by generating plasma of the fluorine source at a temperature of about 5°C to about 20°C while applying a current with a power of about 100 watts to about 400 watts. While heating the substrate to a temperature of approximately 100°C to approximately 400°C, the surface of the substrate is exposed to one or more pulses from the lanthanum-based metal precursor; and The surface of the substrate is exposed to one or more pulses of the sulfur hexafluoride-based plasma while the substrate is heated to a temperature of approximately 100°C to approximately 400°C.
29. The method of claim 27 or claim 28, wherein the sulfur hexafluoride-based plasma is derived from sulfur hexafluoride and argon.
30. The method according to any one of claims 27 to 29, wherein the duration of each pulse of the lanthanum-based metal precursor is from about 0.01 seconds to about 10 seconds.
31. The method of claim 30, wherein the cycle comprises two or more pulses of the lanthanum-based metal precursor.
32. The method according to any one of claims 27 to 31, wherein the duration of each pulse of the sulfur hexafluoride-based plasma is from about 0.01 seconds to about 30 seconds.
33. The method of claim 32, wherein the cycle comprises a pulse of the sulfur hexafluoride-based plasma.
34. The method according to any one of claims 27 to 33, wherein the duration of each pulse of the sulfur hexafluoride-based plasma is longer than the duration of each pulse of the lanthanum-based metal precursor.
35. The method of any one of claims 27 to 34, wherein the cycle deposits a first deposited layer of the atomic layer deposition coating on the surface of the substrate, and the method further comprises repeating the cycle to deposit a second deposited layer of the atomic layer deposition coating on the surface of the substrate.
36. The method according to any one of claims 27 to 35, further comprising heating the atomic layer deposition chamber to a temperature of about 10°C to about 15°C while exposing the surface of the substrate to the pulses of the lanthanum-based metal precursor and the sulfur hexafluoride-based plasma.
37. The method according to any one of claims 27 to 36, further comprising converting the fluorine source into the sulfur hexafluoride-based plasma by heating the fluorine source to a temperature of about 10°C to about 15°C and applying the current having a power of about 125 watts to about 375 watts.