A scalable method for fabricating wafer-level diamond-based photonic integrated circuits

By depositing diamond nanoparticles on a negative mold and performing thermal annealing, the challenges of optical-grade surface treatment and etching in the manufacturing of diamond-based photonic integrated circuits have been solved, enabling efficient and low-cost D-PIC manufacturing, which is suitable for semiconductor production lines and applications of various optical materials.

CN123165573APending Publication Date: 2026-11-24李嘉旋
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202680002805.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-03-07
Filing Date
2026-03-06
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing technologies are difficult to manufacture diamond-based photonic integrated circuits (D-PIC) efficiently, especially due to the time-consuming, costly, and poorly scalable processes involved in obtaining optical-grade surfaces and etching.

Method used

Diamond nanoparticles are deposited on a negative mold using chemical vapor deposition (CVD) to form a diamond seed layer, and a diamond structure layer is then grown conformally with it. Combined with thermal annealing, an optical-grade surface is obtained by separating the negative mold, avoiding complex polishing and etching steps.

Benefits of technology

It enables efficient and low-cost manufacturing of diamond-based photonic integrated circuits, has good scalability, is suitable for semiconductor production lines, can integrate photonic and electronic devices, and is applicable to a variety of optical materials and manufacturing technologies.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123165573A_ABST
    Figure CN123165573A_ABST
Patent Text Reader

Abstract

A scalable method for fabricating wafer-level diamond-based photonic integrated circuits (D-PICs) is provided. The method includes: preparing a negative model according to a reverse circuit layout of the wafer-level D-PIC; depositing diamond nanoparticles on the negative model to form a diamond seed layer; conformally growing a thin diamond layer with the diamond seed layer to form a diamond structure layer; growing a cladding layer on the diamond structure layer; growing a substrate layer on the cladding layer to form a wafer-level D-PIC assembly on the negative model; performing thermal annealing on the wafer-level D-PIC assembly on the negative model to enhance material crystallinity and interlayer bonding; separating the negative model from the wafer-level D-PIC assembly to obtain the wafer-level D-PIC; and performing post-annealing on the wafer-level D-PIC to release residual stress. The provided method does not involve etching and polishing of the diamond, and is therefore easily scalable.
Need to check novelty before this filing date? Find Prior Art

Description

Cross-references to related applications

[0001] This application claims priority to U.S. Provisional Patent Application No. 63 / 768,185, filed March 7, 2025, the disclosure of which is incorporated herein by reference in its entirety. Technical Field

[0002] This invention generally relates to photonic integrated circuits. More specifically, this invention relates to a scalable method for manufacturing diamond-based photonic integrated circuits (D-PIC). Background Technology

[0003] Photonic integrated circuits (PICs) are an active field of research and technological development. Unlike traditional circuits that use electricity to transmit data, PICs utilize light to transmit data on optical waveguides on the chip, enabling several significant and advanced advantages. Integrating PICs into computer chips results in higher data transfer rates, lower power consumption, and less energy loss as heat. These advantages are particularly valuable as the demand for high-speed and energy-efficient data processing continues to grow in artificial intelligence (AI) server clusters.

[0004] In fact, PICs have already achieved commercial success in advanced optical transceivers and telecommunications mainnets. They help enable fast and reliable data transmission in large-scale networks. Furthermore, the application of PICs is currently expanding to the latest co-packaged optics (CPO) network switches, enabling efficient inter-chip communication for millions of graphics processing units (GPUs) in the age of artificial intelligence.

[0005] Diamond-based photonic integrated circuits (D-PICs) represent a promising direction in the fields of photonics and quantum technology. Integrating photonic devices with diamond substrates allows for the utilization of diamond's unique properties, such as wide bandgap, excellent thermal conductivity, and outstanding optical characteristics, thereby enabling the development of efficient and scalable photonic systems.

[0006] Diamond is widely recognized as an excellent material for a variety of quantum applications, including quantum communication, sensing, and computing. Diamond can accommodate several specific point defects with excellent quantum properties, such as nitrogen-vacancy centers for qubits in quantum computing.

[0007] For photonic circuits, both polycrystalline and single-crystal diamonds possess excellent optical properties for light transmission, such as an extremely wide transmission spectrum from 220 nm to 50 µm and low optical loss. Furthermore, diamond semiconductors can be formed through doping processes to fabricate PICs and electronic devices. For example, p-type diamond semiconductors can be formed by doping a diamond substrate with boron; n-type diamond semiconductors for electron conduction can be formed by doping a diamond substrate with phosphorus. This is commonly used in applications such as high-power electronic devices and radiation detection.

[0008] A fundamental requirement for D-PICs is an optical-grade surface with a roughness of 1 nm to 2 nm on a diamond wafer / substrate, which will be used to fabricate optical waveguides for optical transmission and coupling.

[0009] Current industrial methods achieve optical-grade diamond surfaces through polishing. Different polishing techniques, such as mechanical polishing, chemical mechanical polishing (CMP), and non-contact polishing, each have their own advantages and limitations. However, due to the extremely high hardness of diamond, polishing diamond wafers is time-consuming and costly. For specific applications, specialized equipment and materials may be required to achieve the desired surface quality. For polycrystalline diamond substrates, the presence of grain boundaries can easily lead to uneven polishing. Furthermore, polishing can introduce stress, affecting wafer flatness, roughness, and even causing wafer damage.

[0010] Another essential process for obtaining diamond waveguides and photonic devices in D-PICs is etching. However, due to diamond's exceptional hardness and chemical resistance, it is difficult to etch using standard etching methods used in silicon semiconductor foundries. On the other hand, achieving good etching with vertical sidewalls and smooth surface quality is necessary for waveguides and photonic devices. Therefore, diamond etching in the D-PIC manufacturing process remains an industrial challenge, and its scalability issues still need to be addressed. Summary of the Invention

[0011] According to various aspects of the present invention, a scalable method for manufacturing wafer-level diamond-based photonic integrated circuits (D-PICs) is provided. The method includes: preparing a negative model according to a reverse circuit layout of the wafer-level D-PIC; depositing diamond nanoparticles on the negative model to form a diamond seed layer; conformally growing a thin diamond layer with the diamond seed layer to form a diamond structure layer; growing a cladding layer on the diamond structure layer; growing a substrate layer on the cladding layer to form a wafer-level D-PIC assembly on the negative model; performing a thermal annealing treatment on the wafer-level D-PIC assembly on the negative model to enhance material crystallinity and interlayer bonding; separating the negative model from the wafer-level D-PIC assembly to obtain the wafer-level D-PIC; and performing a post-annealing treatment on the wafer-level D-PIC to release residual stress.

[0012] In one embodiment, the negative mold is prepared by patterning the top surface of a semiconductor wafer and depositing a mold protective layer on the patterned top surface.

[0013] In one embodiment, the top surface of the semiconductor wafer has a surface roughness of less than 2 nm.

[0014] In one embodiment, the semiconductor wafer used to prepare the negative mold is a silicon wafer or a silicon carbide wafer; and the mold protective layer is made of aluminum oxide or silicon nitride.

[0015] In one embodiment, the size of the diamond nanoparticles is in the range of 2 nm to 50 nm.

[0016] In one embodiment, the diamond structure layer is formed by a CVD process in which a gas mixture of methane and hydrogen is introduced into the reaction chamber as the reaction gas.

[0017] In one embodiment, the coating layer is made of an optical material with a refractive index lower than that of diamond.

[0018] In one embodiment, the coating layer is a silica coating layer grown by CVD by introducing a gas mixture of silane combined with oxygen or nitrous oxide as a reaction gas in a reaction chamber.

[0019] In one embodiment, the coating layer includes a plurality of sub-coating layers alternately disposed with the adhesion layer; each sub-coating layer is a silicon dioxide layer grown by CVD by introducing a gas mixture of silane combined with oxygen or nitrous oxide as a reaction gas in a reaction chamber; and each adhesion layer is a silicon carbide layer grown by CVD by introducing a gas mixture of silane, methane and hydrogen as a reaction gas in a reaction chamber.

[0020] In one embodiment, the substrate is a silicon nitride substrate grown by CVD by introducing a gas mixture of silane and ammonia as a reaction gas and nitrogen as a carrier gas in a reaction chamber.

[0021] In one embodiment, the substrate is an alumina substrate grown by CVD by introducing a gas mixture of oxygen and trimethylaluminum as a reaction gas and nitrogen as a carrier gas in a reaction chamber.

[0022] In one embodiment, the substrate is a diamond substrate, which is formed by the following steps: depositing diamond nanoparticles on the coating layer to form a second diamond seed layer; and conformally growing a second diamond layer with the second diamond seed layer to form the diamond substrate.

[0023] In one embodiment, the thermal annealing process is carried out at an annealing temperature ranging from 100°C to 350°C and an annealing time ranging from 1 hour to 24 hours in a nitrogen atmosphere.

[0024] In one embodiment, the method further includes depositing a protective top layer on the diamond structure layer.

[0025] In one embodiment, the method further includes integrating one or more active photonic / electronic devices into the diamond structure layer by the following steps: forming one or more p-type diamond semiconductor regions on the diamond structure layer by CVD doping or ion implantation; forming one or more n-type diamond semiconductor regions on the diamond structure layer by CVD doping or ion implantation; and depositing metal contact pads on the p-type diamond semiconductor regions and the n-type diamond semiconductor regions, respectively.

[0026] In one embodiment, the method further includes attaching one or more photonic / electronic devices to the top of the diamond structure layer.

[0027] The provided method eliminates challenging manufacturing steps in diamond material processing, such as complex etching or polishing to achieve optical-grade surfaces. It can be integrated into existing semiconductor production lines and offers excellent scalability. It is applicable to a wide range of optical materials in semiconductor photonics, including diamond and sapphire. Furthermore, it is applicable to various manufacturing techniques for growing photonic integrated circuits, such as chemical vapor deposition (CVD) for diamond and sapphire, and physical vapor deposition (PVD) for sapphire. Attached Figure Description

[0028] Embodiments of the present invention will now be described in more detail with reference to the accompanying drawings, wherein:

[0029] Figure 1A process flow for a scalable method for manufacturing wafer-level diamond-based photonic integrated circuits (D-PIC) according to an embodiment of the present invention is shown.

[0030] Figure 2 A wafer-level D-PIC is shown according to an embodiment of the present invention.

[0031] Figure 3 It shows Figure 1 The flowchart of the process flow.

[0032] Figure 4 The process flow for growing diamond substrates is shown.

[0033] Figure 5 It shows Figure 4 Flowchart of the process flow Detailed Implementation

[0034] In the following description, details of the invention are set forth in the form of preferred embodiments. It will be apparent to those skilled in the art that various modifications, including additions and / or substitutions, can be made without departing from the scope and spirit of the invention. Certain specific details may be omitted to avoid unnecessarily obscuring the focus of the invention; however, the content of this disclosure is sufficient to enable those skilled in the art to implement the teachings herein without excessive experimentation.

[0035] According to one embodiment of the present invention, a method for manufacturing wafer-level diamond-based photonic integrated circuits (D-PIC) is provided. Figure 1 It shows the manufacturing process. Figure 2 An exemplary process flow for the wafer-level D-PIC 10 method S100 shown. Figure 3 A flowchart of method S100 is shown. The wafer-level D-PIC 10 includes a diamond structure layer 11, a cladding layer 12 made of an optical material with a refractive index lower than diamond, and a substrate layer 13. Method S100 includes the following steps:

[0036] S101: Prepare a negative model 90 according to the reverse circuit layout of the wafer-level D-PIC;

[0037] S102: Deposit diamond nanoparticles on the negative mold to form a diamond seed layer 51, thereby promoting diamond growth;

[0038] S103: A thin diamond layer is conformally grown with the diamond seed layer to form a diamond structure layer 11;

[0039] S104: A coating layer 12 is grown on the diamond structural layer;

[0040] S105: A substrate layer 13 is grown on the cladding layer to ensure that the D-PIC can work effectively while maintaining mechanical stability, wherein the diamond structure layer 11, the cladding layer 12 and the substrate layer 13 form a wafer-level D-PIC assembly on the negative mold;

[0041] S106: Perform thermal annealing on the wafer-level D-PIC assembly on the negative mold to enhance material crystallinity and interlayer bonding; and

[0042] S107: Separate the negative mold 90 from the wafer-level D-PIC assembly to obtain the wafer-level D-PIC 10.

[0043] In step S101, a reverse circuit layout is obtained by converting the conventional circuit layout of the D-PIC into a "reverse" structure, which is the reverse or opposite structure of the desired final shape of the D-PIC. For example, a ridge waveguide in the conventional circuit layout can be replaced with a trench in the reverse circuit layout. The conventional circuit layout of the D-PIC may include the design of optical waveguides, functional devices, and photonic circuits.

[0044] The negative mold can be fabricated by patterning a semiconductor substrate, such as a silicon wafer, a silicon carbide wafer, or another diamond-compatible semiconductor wafer. Preferably, the semiconductor substrate used to fabricate the negative mold has a surface roughness of less than 2 nm (e.g., about 1 nm), which is optically grade (within 1 / 100 of the wavelength) for devices used in optical communications (e.g., wavelengths of 850 nm and 1260 nm to 1675 nm) and quantum computing (e.g., wavelengths of 455 nm to 800 nm). In some embodiments, a thin protective top layer (e.g., aluminum oxide or silicon nitride) can be deposited on the negative mold to protect the mold surface and facilitate demolding.

[0045] In step S102, diamond nanoparticles with a size ranging from 2 nm to 50 nm are deposited on the negative mold to form a diamond seed layer 51, thereby promoting diamond growth. This step ensures the growth of a uniform and high-quality diamond layer.

[0046] Specifically, the negative mold is first cleaned to remove organic residues, particulate matter, and contaminants that would otherwise inhibit particle adhesion. Cleaning can be performed by rinsing in an organic solvent followed by deionized water, and optionally by plasma or UV-ozone treatment. This activation treatment improves wettability and promotes the interaction between the negative mold and the nanoparticles.

[0047] Diamond nanoparticles are dispersed in a suitable solvent, such as deionized water or an alcohol-based medium, with a concentration and nanoparticle size selected corresponding to the target surface coverage. The diamond nanoparticle dispersion is ultrasonically treated to break up agglomerates and obtain a substantially homogeneous colloidal suspension. The pH and ionic strength of the dispersion can be adjusted to modulate surface charge properties and colloidal stability, thereby promoting electrostatic attraction between the nanoparticles and the negative modulus.

[0048] Then, a measured volume of diamond nanoparticle dispersion is applied to the surface of the negative mold and distributed by spin coating, spraying, or controlled evaporation. During this stage, the nanoparticles adhere to the surface through electrostatic interactions, van der Waals forces, or hydrogen bonding.

[0049] In step S103, a diamond structural layer 11 is grown from the diamond seed layer using a chemical vapor deposition (CVD) process. Specifically, the diamond seed layer is exposed to a gas mixture of methane and hydrogen in a CVD reaction chamber. The gas is typically activated by microwaves or hot filaments to generate plasma, thereby promoting diamond growth on the seed layer. The diamond structural layer can have a thickness ranging from 200 nm to 1,000 nm (e.g., 280 nm) to enable a variety of photonic / quantum devices.

[0050] In step S104, the cladding layer 12 is made of an optical material with a refractive index lower than that of diamond. For example, the cladding layer 12 may be a silicon dioxide (SiO2) cladding layer grown on the diamond structure layer by a chemical vapor deposition (CVD) process. Specifically, the diamond structure layer is exposed to silane-bound oxygen or nitrous oxide in a CVD reaction chamber. The gases are typically activated by radio frequency or thermal energy to generate plasma, thereby promoting the growth of the cladding layer on the diamond layer.

[0051] The thickness of the coating layer can range from 300 nm to 3,000 nm. In some embodiments, the coating layer may include multiple sub-coating layers and an adhesive layer. In one embodiment, the adhesive layer is made of silicon carbide (SiC). Specifically, each SiC adhesive layer can be deposited using a CVD process employing a gas mixture of silane, methane, and hydrogen.

[0052] In step S105, the substrate layer 13 may be a diamond substrate layer grown on the coating layer by performing steps similar to those in steps S102 and S103. Specifically, refer to... Figure 4 and Figure 5 Step S105 may include the following steps:

[0053] S1051: Depositing diamond nanoparticles on the coating layer to form a diamond seed layer 52; and

[0054] S1052: A layer of diamond is conformally grown with the diamond seed layer 52 to form the diamond substrate layer 13.

[0055] Alternatively, the substrate layer 13 may be a silicon nitride substrate layer grown on the cladding layer by a CVD process. Specifically, the silicon nitride substrate layer may be grown by a CVD process using a gas mixture of silane and ammonia as the reaction gas and nitrogen as the carrier gas.

[0056] Alternatively, the substrate layer 13 may be an alumina substrate layer grown on the cladding layer by a CVD process. Specifically, the alumina substrate layer may be grown by a CVD process using oxygen and trimethylaluminum as reaction gases and nitrogen as a carrier gas.

[0057] In one embodiment, by controlling the thickness of the substrate layer 13, the total thickness of the wafer-level D-PIC is made to be in the range of 0.3 µm to 50 µm, preferably in the range of 0.3 µm to 10 µm, thereby making the wafer-level D-PIC a flexible wafer-level D-PIC.

[0058] In another embodiment, by controlling the thickness of the substrate layer 13, the total thickness of the wafer-level D-PIC is made to be in the range of 50 µm to 1000 µm, thereby making the wafer-level D-PIC a non-flexible wafer-level D-PIC.

[0059] In step S106, the thermal annealing process is carried out for 1 hour to 24 hours under conditions of, for example, 100°C to 350°C (preferably 200°C to 300°C) and a nitrogen atmosphere.

[0060] The bonding between CVD deposited layers can be enhanced by thermal annealing. This process can also improve the crystallinity of the material in the CVD layers by forming a more ordered crystal structure.

[0061] In step S107, the negative mold 90 is separated (or released) from the wafer-level D-PIC 10 using various techniques (e.g., mechanical methods and wafer bonding). For example, in adhesive wafer bonding, an adhesive (e.g., epoxy resin, polyimide, benzocyclobutene BCB, or SU-8) is spin-coated onto a silicon wafer, aligning the silicon wafer with the wafer-level D-PIC. The silicon wafer and the wafer-level D-PIC are then bonded together by applying pressure and thermosetting the adhesive at 150°C to 300°C. After wafer bonding, mechanical peeling is performed to separate the wafer-level D-PIC from the negative mold.

[0062] The released D-PIC wafers have optical-grade surfaces with the required flatness, surface quality, and roughness of less than 1 / 100 of a wavelength, which is crucial for photonic waveguide applications that require ultra-smooth surfaces.

[0063] In some embodiments, to eliminate residual stress on the wafer-level D-PIC, a post-annealing process may be performed after releasing the negative mold, with annealing conditions such as 100°C to 350°C (preferably 200°C to 300°C), 1 hour to 24 hours, and an ambient nitrogen atmosphere.

[0064] To protect the optical waveguides and photonic devices on the D-PIC surface from environmental factors (such as mechanical shock and dust) and improve their reliability, a protective top layer (such as silicon dioxide) can be deposited on the diamond structure layer by a CVD process.

[0065] The method S100 for manufacturing the wafer-level D-PIC is compatible with conventional semiconductor wafer processing, thereby allowing photonic devices and electronic devices to be manufactured together on the same chip with the D-PIC to provide hybrid functionality.

[0066] To integrate active photonic devices (such as electrically pumped single-photon sources and diamond photodiodes) onto D-PICs, p-type diamond semiconductors, n-type diamond semiconductors, and metal contact pads can be fabricated on the diamond structure layer using standard CMOS manufacturing processes.

[0067] p-type and n-type dopants can be introduced into the diamond structure layer by CVD doping during growth or by ion implantation after the formation of the diamond layer. The p-type dopants may include, but are not limited to, boron and aluminum, and the n-type dopants may include, but are not limited to, phosphorus and nitrogen.

[0068] Subsequently, metal contact pads (e.g., titanium and gold) are deposited on the p-type and n-type regions by sputtering or electron beam evaporation to establish electrical connections with the doped semiconductor regions. The metal contact pads may include, but are not limited to, titanium, gold, platinum, and aluminum.

[0069] In addition, other active devices, such as light sources and photodetectors formed from semiconductor materials other than diamond, can be heterogeneously integrated onto the diamond structure layer via flip-chip bonding or wafer bonding.

[0070] The CVD processes performed in manufacturing the wafer-level D-PIC and integrating active photonic devices on the wafer-level D-PIC may include, but are not limited to, microwave plasma-assisted chemical vapor deposition (MPCVD), radio frequency chemical vapor deposition (RFCVD), plasma-enhanced chemical vapor deposition (PECVD), direct current plasma-enhanced chemical vapor deposition (DC-CVD), and hot filament chemical vapor deposition (HFCVD).

[0071] Although this disclosure has been described and illustrated with reference to specific embodiments thereof, such descriptions and illustrations are not limiting. The drawings are not necessarily drawn to scale. Due to manufacturing processes and tolerances, there may be differences between the drawings of this disclosure and actual apparatus. Other embodiments not specifically shown may also exist in this disclosure. Modifications may be made to adapt particular circumstances, materials, compositions, methods, or processes to the purpose and scope of this disclosure. All such modifications are intended to fall within the scope of the appended claims. Although the methods disclosed herein have been described with reference to specific operations performed in a particular order, it should be understood that these operations may be combined, subdivided, or reordered to form equivalent methods without departing from the teachings of this disclosure. Therefore, unless specifically indicated herein, the order and grouping of operations are not limiting.

Claims

1. A scalable method for manufacturing wafer-level diamond-based photonic integrated circuits (D-PIC), comprising: A negative model is prepared based on the reverse circuit layout of the wafer-level D-PIC; Diamond nanoparticles are deposited on the negative mold to form a diamond seed layer; A thin diamond layer is conformally grown with the diamond seed layer to form a diamond structural layer; A coating layer is grown on the diamond structural layer; A substrate layer is grown on the coating layer to form a wafer-level D-PIC assembly on the negative mold; The wafer-level D-PIC assembly on the negative mold is subjected to thermal annealing to enhance the crystallinity of the material and the bonding between layers; as well as The negative mold is separated from the wafer-level D-PIC assembly to obtain the wafer-level D-PIC.

2. The method according to claim 1, wherein, The negative mold is prepared by patterning the top surface of a semiconductor wafer and depositing a mold protective layer on the patterned top surface.

3. The method according to claim 1 or 2, wherein, The top surface of the semiconductor wafer has a surface roughness of less than 2 nm.

4. The method according to any one of claims 1 to 3, wherein, The semiconductor wafer used to prepare the negative mold is a silicon wafer or a silicon carbide wafer; and the mold protective layer is made of aluminum oxide or silicon nitride.

5. The method according to any one of claims 1 to 4, wherein, The size of the diamond nanoparticles is in the range of 2 nm to 50 nm.

6. The method according to any one of claims 1 to 5, wherein, The diamond structure layer is formed by chemical vapor deposition (CVD) in which a gas mixture of methane and hydrogen is introduced into the reaction chamber as the reaction gas.

7. The method according to any one of claims 1 to 6, wherein, The coating layer is made of an optical material with a refractive index lower than that of diamond.

8. The method according to any one of claims 1 to 7, wherein, The coating layer is a silica coating layer grown by CVD by introducing a gas mixture of silane combined with oxygen or nitrous oxide as a reaction gas in a reaction chamber.

9. The method according to any one of claims 1 to 8, wherein, The coating layer includes a plurality of sub-coating layers that are alternately arranged with the adhesion layer; Each sub-coating layer is a silica layer grown by CVD using a gas mixture of silane combined with oxygen or nitrous oxide as the reaction gas in the reaction chamber; and Each adhesion layer is a silicon carbide layer grown by CVD by introducing a gas mixture of silane, methane and hydrogen as the reaction gas in the reaction chamber.

10. The method according to any one of claims 1 to 9, wherein, The substrate is a silicon nitride substrate grown by CVD by introducing a gas mixture of silane and ammonia as the reaction gas and nitrogen as the carrier gas in the reaction chamber.

11. The method according to any one of claims 1 to 9, wherein, The substrate is an alumina substrate grown by CVD by introducing a gas mixture of oxygen and trimethylaluminum as the reaction gas and nitrogen as the carrier gas in the reaction chamber.

12. The method according to any one of claims 1 to 9, wherein, The substrate layer is a diamond substrate layer, which is formed through the following steps: Diamond nanoparticles are deposited on the coating layer to form a second diamond seed layer; and a second diamond layer is conformally grown with the second diamond seed layer to form the diamond substrate layer.

13. The method according to any one of claims 1 to 11, wherein, The thermal annealing process is carried out in a nitrogen atmosphere at an annealing temperature ranging from 100°C to 350°C for an annealing time ranging from 1 hour to 24 hours.

14. The method according to any one of claims 1 to 12, further comprising depositing a protective top layer on the diamond structure layer.

15. The method according to any one of claims 1 to 13, further comprising: One or more active photonic / electronic devices are integrated into the diamond structure layer through the following steps: One or more p-type diamond semiconductor regions are formed on the diamond structure layer by CVD doping or ion implantation. One or more n-type diamond semiconductor regions are formed on the diamond structure layer by CVD doping or ion implantation; and Metal contact pads are deposited on the p-type diamond semiconductor region and the n-type diamond semiconductor region, respectively.

16. The method according to any one of claims 1 to 15, further comprising attaching one or more photonic / electronic devices to the top of the diamond structure layer.

17. The method according to any one of claims 1 to 16, further comprising performing a post-annealing process on the wafer-level D-PIC after separating the negative mold from the wafer-level D-PIC assembly to release residual stress.