High-temperature preheating device of corrosive medium for high-temperature fatigue test
By designing separate heating high-temperature preheating devices, the problem that corrosion equipment in the prior art cannot effectively preheat gases, high-temperature preheating and stable control of corrosive media is achieved, and the fatigue testing machine is adapted to ensure high-temperature corrosion Test stability and accuracy in atmosphere environment.
Patent Information
- Application Number
- CN202420263076.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-03
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2034-02-03
AI Technical Summary
The existing corrosion equipment devices cannot effectively preheat the gas to 800°C, and the salt spray test chamber is not suitable for the general fatigue testing machine, so the corrosion-fatigue interaction test cannot be achieved, resulting in low experimental efficiency and the inability to ensure gas temperature control.
A high temperature preheating device is designed, including a first-stage tower heater and a second-stage tower heater, by heating the corrosive liquid medium and gas medium separately and mixing in a first dosing pump, the nozzle is located in the high-temperature ambient chamber. Within, high-temperature preheating of corrosive media is realized to ensure stable control of gas flow rate and pressure.
Improve the economy and adaptability of the device, realize high-temperature preheating of different corrosive media, reduce the interference of gas heat exchange on crack propagation data, meet the requirements of high-temperature corrosion atmosphere environment, and ensure the crack propagation potential method Stability and accuracy.
Smart Images

Figure CN221975509U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of engine hot end component material development, in particular to a high-temperature preheating device for corrosive media used in high-temperature fatigue experiments. Background Art
[0002] When studying the environmental adaptability of hot-end components of carrier-based aircraft / gas turbines in a gas-ocean atmosphere coupling environment, it is necessary to combine the gas-ocean atmosphere environment of the actual hot-end component materials and provide the test object with a simulated ocean-going ship platform environment, namely, an acidic salt spray environment. The study of corrosion-fatigue interactive crack propagation in this environment affects the life assessment and safety reliability of hot-end components of aircraft engines. In order to study the corrosion fatigue crack propagation problem, the potential method is generally used to measure crack propagation test data. During the test, in order to ensure the measurement accuracy of the crack propagation test method-potential method, it is necessary to ensure that the error between the ambient gas temperature and the test temperature (≤800℃) is within a controllable range, and the corrosive medium needs to be preheated before entering the test environment chamber.
[0003] The main corrosive environmental media currently under research include gas exhaust (SO2), salt spray, etc. Existing corrosion equipment can already realize the introduction of corrosive gases, but does not consider the preheating of other gases except steam (temperature reaches 800°C); in addition, there are relatively mature heating methods for heating salt spray, such as steam heating, but it requires a long preheating before the experiment, the experiment time is long, the efficiency is low, and the temperature control of the gas at a certain flow rate cannot be guaranteed. In addition, the salt spray test chamber is not compatible with the general fatigue testing machine, and the corrosion-fatigue interactive test cannot be realized.
[0004] Therefore, it is necessary to design a device that is compatible with the high temperature environment chamber of the fatigue testing machine and can control the composition and flow rate of the test corrosive medium and preheat it to solve the above problems. Utility Model Content
[0005] In order to overcome the shortcomings and deficiencies of the prior art, the purpose of the utility model is to provide a high-temperature preheating device for corrosive media used in high-temperature fatigue experiments.
[0006] The utility model is implemented as follows: a high-temperature preheating device for corrosive media used in high-temperature fatigue tests, wherein the corrosive media is composed of corrosive liquid media and corrosive gas media, and the heating device comprises a first heating component for heating and vaporizing the corrosive liquid media, and a second heating component for superheating the corrosive gas media. The heated and vaporized corrosive liquid media and the superheated corrosive gas media are input into a first dosing pump, mixed, and pumped into a nozzle, and the nozzle is located in a high-temperature environment chamber for conducting high-temperature fatigue tests on test specimens; wherein,
[0007] The first heating assembly comprises a first-stage tower heater and a second-stage tower heater having the same structure, wherein a high-temperature resistant ceramic spiral tube is arranged vertically on the axis and spirals downward along the axis, wherein the air inlet of the spiral tube is located at the top of the heater and the air outlet is located at the bottom of the heater, and an electromagnetic heating furnace for heating the spiral tube is arranged on the inner wall of the tower heater;
[0008] The spiral tube air outlet of the first-stage tower heater and the spiral tube air inlet of the second-stage tower heater are connected through an inclined first straight tube. The spiral tube air inlet of the first-stage tower heater is introduced with atomized corrosive liquid medium. The atomized corrosive liquid medium is vaporized to 180° C. by the first-stage tower heater and is overheated to 800° C. by the second-stage tower heater.
[0009] Preferably, the angle between the pipeline in the high-temperature resistant ceramic spiral tube and the horizontal plane is 10°, and the oblique angle between the first straight tube and the horizontal plane is 10°; the spiral tube air outlet of the secondary tower heater is connected to the first metering pump through an inclined second straight tube; and the oblique angle between the second straight tube and the horizontal plane is 10°.
[0010] Preferably, the first straight pipe is provided with a first stop valve for controlling the gas flow rate of the corrosive liquid medium.
[0011] Preferably, the first heating component also includes a brine tank for storing corrosive liquid medium and a gas-liquid booster pump for extracting and atomizing the corrosive liquid medium from the brine tank; the gas-liquid booster pump is connected to the spiral tube air inlet of the first-stage tower heater through an input pipe, and a second stop valve is provided on the input pipe.
[0012] Preferably, the first straight tube and the second straight tube are respectively provided with temperature and pressure sensors.
[0013] Preferably, the second heating component includes a second dosing pump, a gas flow controller, and a tubular gas heating furnace. The corrosive gas medium passes through the second dosing pump and the gas flow controller in sequence through a pipeline and then enters the tubular gas heating furnace for preheating. The preheated corrosive gas medium is connected to the first dosing pump through an output pipeline, and a temperature and pressure sensor is provided on the output pipeline.
[0014] Preferably, the gas flow controller controls the gas flow rate to be no less than 3 L / min.
[0015] Compared with the shortcomings and deficiencies of the prior art, the utility model has the following beneficial effects:
[0016] (1) The device of the utility model heats the corrosive gas medium and the corrosive liquid medium in two ways to form a corrosive gas medium that enters the environmental chamber. The separate heating of the corrosive liquid medium and the corrosive gas medium can improve the economic efficiency of the device, and the flow rate and pressure of the corrosive liquid medium and the corrosive gas medium are stable and controllable; by adjusting the concentration and flow rate of the corrosive gas medium, various extreme special environments (for example: acidic salt spray environment, gas corrosion environment) can be simulated;
[0017] (2) The utility model can realize the preheating of different corrosive medium gases, ensure the stable heat exchange between the flow gas and the environmental equipment, solve the problem of preheating the corrosive atmosphere in the corrosion-fatigue crack growth test process, reduce the interference of gas heat exchange to the potential method (DCPD) monitoring crack growth data, meet the requirements of different high-temperature corrosive atmosphere environments, and ensure the stability and accuracy of crack growth potential method monitoring;
[0018] (3) The device of the utility model can be well adapted to the fatigue testing machine. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a structural schematic diagram of the device of the utility model;
[0020] Figure 2 It is a schematic diagram of the assembly structure of a primary tower heater and a secondary tower heater of a first heating component in the device of the utility model.
[0021] In the figure, 1. brine tank, 2. gas-liquid booster pump, 3. first-stage tower heater, 4. second-stage tower heater, 5. second temperature and pressure sensor, 6. first metering pump, 7. third temperature and pressure sensor, 8. tubular gas heating furnace, 9. gas flow controller, 10. second metering pump, 11. gas storage tank, 12. nozzle, 13. high-temperature environment chamber, 3.1. second stop valve, 3.2. input pipeline, 3.3. first high-temperature resistant ceramic spiral tube, 3.4. first electromagnetic heating furnace, 3.5. first temperature and pressure sensor, 4.1. first stop valve, 4.2. second high-temperature resistant ceramic spiral tube, 4.3. second electromagnetic heating furnace, 4.4. second straight tube. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described here are only used to explain the utility model and are not used to limit the utility model.
[0023] like Figures 1-2 As shown, Figure 1 It is a structural schematic diagram of the device of the utility model; Figure 2 It is a schematic diagram of the assembly structure of a primary tower heater and a secondary tower heater of a first heating component in the device of the utility model.
[0024] The utility model embodiment discloses a high-temperature preheating device for a corrosive medium used for a high-temperature fatigue test, wherein the corrosive medium is composed of a corrosive liquid medium and a corrosive gas medium, and the heating device comprises a first heating component for heating and vaporizing the corrosive liquid medium, and a second heating component for superheating the corrosive gas medium, wherein the heated and vaporized corrosive liquid medium and the superheated corrosive gas medium are input into a first dosing pump 6 for mixing and pumping into a nozzle 12, and the nozzle 12 is located in a high-temperature environment chamber 13 for conducting a high-temperature fatigue test of a test specimen; wherein the first heating component comprises a first-stage tower heater 3 (i.e., a tower steam generator), a second-stage tower heater 4 (i.e., a tower superheated steam generator), and a first-stage tower heater 5 (i.e., a tower superheated steam generator). The first-stage tower heater 3 is provided with a first high-temperature resistant ceramic spiral tube 3.3 with an axis vertically arranged and spiraling downward along the axis, the air inlet of the first high-temperature resistant ceramic spiral tube 3.3 is located at the top of the heater, and the air outlet is located at the bottom of the heater, and the inner wall of the first-stage tower heater 3 is provided with a first electromagnetic heating furnace 3.4 for heating the first high-temperature resistant ceramic spiral tube 3.3; similarly, the second-stage tower heater 4 is provided with a second high-temperature resistant ceramic spiral tube 4.2 with an axis vertically arranged and spiraling downward along the axis, the air inlet of the second high-temperature resistant ceramic spiral tube 4.2 is located at the top of the heater, and the air outlet is located at the bottom of the heater, and the inner wall of the second-stage tower heater 4 is provided with a second electromagnetic heating furnace 4.3 for heating the second high-temperature resistant ceramic spiral tube 4.2;
[0025] The air outlet of the first high-temperature resistant ceramic spiral tube 3.3 of the first-level tower heater 3 is connected to the air inlet of the second high-temperature resistant ceramic spiral tube 4.2 of the second-level tower heater 4 through an inclined first straight tube. The atomized corrosive liquid medium is introduced into the air inlet of the first high-temperature resistant ceramic spiral tube 3.3 of the first-level tower heater 3. The atomized corrosive liquid medium is heated and vaporized to 180°C by the first-level tower heater 3 and overheated to 800°C by the second-level tower heater 4. The vaporized corrosive liquid medium is input into the first metering pump 6 from the second high-temperature resistant ceramic spiral tube 4.2.
[0026] In the embodiment of the utility model, the first heating component is used to heat and vaporize the corrosive liquid medium in the salt spray state, and the second heating component is used to superheat the corrosive gas medium. The heated and vaporized corrosive liquid medium and the superheated corrosive gas medium are mixed in the first metering pump 6 to obtain the corrosive medium for the experiment, and the corrosive medium for the experiment is sprayed to the test sample in the high temperature environment chamber 13 through the nozzle 12 to form a corrosive medium atmosphere for high temperature fatigue experiment.
[0027] In the embodiment of the utility model, a preferred implementation of a second heating component is provided. Specifically, the second heating component includes a second dosing pump 10, a gas flow controller 9, and a tubular gas heating furnace 8. The corrosive gas medium passes through the second dosing pump 10 and the gas flow controller 9 from the gas storage tank 11 through a pipeline and then enters the tubular gas heating furnace 8 for overheating. The overheated corrosive gas medium is connected to the second dosing pump 10 through an output pipeline. The output pipeline is provided with a third temperature and pressure sensor 7. In the embodiment of the utility model, the second dosing pump 10 is used to control the proportion of corrosive gas. Commonly used gases include: air, oxygen, argon, nitrogen, SO 2. Adjust the gas ratio conditions according to the experimental requirements. For example, in a normal atmospheric environment, air is introduced; in a fuel gas environment, SO2 and other gas ratios are introduced; in a low oxygen partial pressure environment, nitrogen / argon is introduced.
[0028] In the embodiments of the present invention, all existing products that can achieve the technical purpose of the present invention can be used to explain the tubular gas heating furnace 8, the second metering pump 10, and the gas flow controller 9 of the present invention.
[0029] In the embodiment of the utility model, the first metering pump 6 is used to proportion the concentration of the corrosive liquid medium and adjust the proportion of the corrosive liquid medium introduced into the nozzle 12. For example, if different concentrations of the corrosive liquid medium need to be adjusted, a certain proportion of air / SO2 / N2 is added to the second metering pump 10 to reduce the concentration of the corrosive liquid medium and provide the oxygen required for oxidation to meet the different concentration conditions of the corrosive liquid medium required by the experiment.
[0030] In the embodiment of the utility model, the corrosive liquid medium is introduced into the first heating component in a salt mist atomization state, because a certain flow rate is required to avoid sedimentation after the salt mist is atomized. In practical applications, the gas flow rate can reach 3L / min, and the increase in flow rate leads to a limited heating time in the first heating component, which makes it unable to reach the temperature required for the experiment before entering the first metering pump 6. Therefore, in the embodiment of the utility model, the first heating component is selected as a two-stage heating method, that is, the first tower heater 3 and the second tower heater 4 are connected in series to increase the heating time so that it is fully heated. Among them, the first tower heater 3 vaporizes the salt mist to 180°, for example, the steam heating component of the thermogravimetric analyzer can realize this function, and the second tower heater 4 is a superheated steam generator, which can superheat the steam to 800°.
[0031] In the embodiment of the utility model, the first high-temperature resistant ceramic spiral tube 3.3 and the second high-temperature resistant ceramic spiral tube 4.2 are arranged in the form of spiral tubes with the axis vertically arranged and spiraling downward along the axis, and the first high-temperature resistant ceramic spiral tube 3.3 and the second high-temperature resistant ceramic spiral tube 4.2 are connected by a first straight tube inclined downward. The design of this pipeline structure can effectively ensure that the temperature of the salt spray gas can be controlled at a certain flow rate, and the heated steam can entrain the precipitated salt particles to pass along the spiral downward pipeline at a certain flow rate, avoiding blockage caused by the precipitation of high-temperature salt particles and reducing the concentration of the corrosive medium in the actual test.
[0032] In the embodiment of the utility model, the first heating component is selected to heat and vaporize the corrosive liquid medium in the salt spray state, and the second heating component is used to overheat the corrosive gas medium, that is, the corrosive liquid medium and the corrosive gas medium are heated separately, which can also effectively improve the economy. The utility model device can be well adapted to the fatigue testing machine, meet the generation requirements of different high-temperature corrosive atmosphere environments, and can also ensure the stability and accuracy of crack extension potential method monitoring.
[0033] In the embodiments of the utility model, it is easy to understand that the components in the device of the utility model that are in contact with corrosive media should have high temperature resistance and corrosion resistance, including high temperature resistant ceramic spiral tubes, the first metering pump 6, the first straight tube, the nozzle 12, etc. For example, the spiral tube is made of high temperature resistant ceramic material, and the nozzle 12 is made of fiberglass.
[0034] In the further implementation process, according to the actual parameters such as flow rate and temperature, in order to facilitate the conduction of the pipeline and avoid the accumulation of salt particles, preferably, the angle between the pipeline and the horizontal plane in the first high-temperature resistant ceramic spiral tube 3.3 and the second high-temperature resistant ceramic spiral tube 4.2 is 10°, and the oblique angle between the first straight tube and the horizontal plane is 10°; the air outlet of the second high-temperature resistant ceramic spiral tube 4.2 is connected to the first metering pump 6 through the oblique second straight tube 4.4; and the oblique angle between the second straight tube 4.4 and the horizontal plane is 10°. It is easy to understand that the purpose of the oblique placement of the first straight tube and the second straight tube 4.4 is also to reduce the precipitation of salt at the bottom of the pipeline. The first high-temperature resistant ceramic spiral tube 3.3, the second high-temperature resistant ceramic spiral tube 4.2, the first straight tube, and the second straight tube 4.4 are all given a certain inclination and the flow rate of the gas is flushed, which can well avoid precipitation and precipitation, avoid the enrichment of salt particles inside the pipeline, and ensure the concentration of salt mist entering the cabin while protecting the pipeline from being blocked.
[0035] In the further implementation process, in order to facilitate the control of the gas flow rate of the corrosive liquid medium, preferably, the first straight pipe is provided with a first stop valve 4.1 for controlling the gas flow rate of the corrosive liquid medium and preventing gas backflow. In the embodiment of the utility model, it is determined based on actual experience that the first stop valve 4.1 should control the gas flow rate of the corrosive liquid medium to be no less than 3L / min.
[0036] In the further implementation process, in order to facilitate the provision of salt-atomized corrosive liquid medium, preferably, the first heating component also includes a brine tank 1 for storing the corrosive liquid medium and a gas-liquid booster pump 2 for extracting and atomizing the corrosive liquid medium from the brine tank 1; the gas-liquid booster pump 2 is connected to the first high-temperature resistant ceramic spiral tube 3.3 air inlet of the first-level tower heater 3 through an input pipe 3.2, and a second stop valve 3.1 is provided on the input pipe 3.2 to prevent gas backflow.
[0037] In the further implementation process, a first temperature and pressure sensor 3.5 is provided on the first straight pipe, and a second temperature and pressure sensor 5 is provided on the second straight pipe 4.4. In the embodiment of the utility model, the first temperature and pressure sensor 3.5 and the second temperature and pressure sensor 5 are used to confirm the state after the salt vapor is heated, and can timely judge whether the salt spray gas reaches the experimental temperature and whether the gas pressure has a safety hazard, and can make adjustments after monitoring before entering the cabin.
[0038] In the practical application process of the utility model, the corrosive liquid medium (salt solution) is pumped out from the salt water tank 1 by the gas-liquid booster pump 2, and the gas-liquid booster pump 2 atomizes the salt solution and enters the first-stage tower heater 3, after being fully heated to the set 180°C, enters the second-stage tower heater 4 through the inclined first straight pipe, and then is fully heated to the set 800°C to form salt mist gas and enter the first metering pump 6. The first temperature and pressure sensor 3.5 and the second temperature and pressure sensor 5 are used to ensure that the heating process is safe and controllable; in addition, the corrosive gas medium is connected to the second metering pump 10 for metering and mixing multiple atmospheres, and is connected to the gas flow controller 9 for controlling the gas flow rate. The gas is fully heated in the tubular gas heating furnace 8 and then enters the first metering pump 6. At this time, the two gas paths are combined and adjusted by the first metering pump 6 to enter the experimental high temperature environment chamber 13, and are sprayed through the nozzle 12 to allow the corrosive medium to fully contact the test sample.
[0039] The utility model device heats the corrosive gas medium and the corrosive liquid medium in two ways to form a corrosive gas medium that enters the environmental chamber, wherein the separate heating of the corrosive liquid medium and the corrosive gas medium can improve the economy of the device, and the flow rate and pressure of the corrosive liquid medium and the corrosive gas medium are stable and controllable; by adjusting the concentration and flow rate of the corrosive gas medium, various extreme special environments (for example, acidic salt spray environment, gas corrosion environment) can be simulated; in addition, the utility model can realize the preheating of different corrosive medium gases, can ensure the stable heat exchange between the flow gas and the environmental equipment, can solve the problem of preheating the corrosive atmosphere in the corrosion-fatigue crack extension test process, reduce the interference of gas heat exchange on the crack extension data monitored by the potential method, meet the requirements of different high-temperature corrosion atmosphere environments, and can also ensure the stability and accuracy of crack extension potential method monitoring; in addition, the utility model device can be well adapted to the fatigue testing machine.
[0040] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A high temperature preheating device for corrosive medium used in high temperature fatigue test, wherein the corrosive medium is composed of corrosive liquid medium and corrosive gas medium. It is characterized in that The heating device comprises a first heating component for heating and vaporizing a corrosive liquid medium, and a second heating component for superheating a corrosive gas medium. The heated and vaporized corrosive liquid medium and the superheated corrosive gas medium are input into a first dosing pump for mixing and pumping into a nozzle, and the nozzle is located in a high temperature environment chamber for conducting a high temperature fatigue test of a test specimen; wherein, The first heating assembly comprises a first-stage tower heater and a second-stage tower heater having the same structure, wherein a high-temperature resistant ceramic spiral tube is arranged vertically on the axis and spirals downward along the axis, wherein the air inlet of the spiral tube is located at the top of the heater and the air outlet is located at the bottom of the heater, and an electromagnetic heating furnace for heating the spiral tube is arranged on the inner wall of the tower heater; The spiral tube air outlet of the first-stage tower heater and the spiral tube air inlet of the second-stage tower heater are connected through an inclined first straight tube. The spiral tube air inlet of the first-stage tower heater is introduced with atomized corrosive liquid medium. The atomized corrosive liquid medium is vaporized to 180° C. by the first-stage tower heater and is overheated to 800° C. by the second-stage tower heater.
2. The device according to claim 1, It is characterized in that The angle between the pipeline in the high-temperature resistant ceramic spiral tube and the horizontal plane is 10°, and the inclined angle between the first straight tube and the horizontal plane is 10°; the spiral tube air outlet of the secondary tower heater is connected to the first metering pump through the inclined second straight tube; and the inclined angle between the second straight tube and the horizontal plane is 10°.
3. The device according to claim 1, It is characterized in that The first straight pipe is provided with a first stop valve for controlling the gas flow rate of the corrosive liquid medium.
4. The device according to claim 1, It is characterized in that The first heating component also includes a brine tank for storing corrosive liquid medium and a gas-liquid booster pump for extracting and atomizing the corrosive liquid medium from the brine tank; the gas-liquid booster pump is connected to the spiral tube air inlet of the first-stage tower heater through an input pipeline, and a second stop valve is provided on the input pipeline.
5. The device according to claim 1, It is characterized in that The first straight tube and the second straight tube are respectively provided with temperature and pressure sensors.
6. The device according to claim 1, It is characterized in that The second heating component includes a second dosing pump, a gas flow controller, and a tubular gas heating furnace. The corrosive gas medium passes through a pipeline and sequentially passes through the second dosing pump and the gas flow controller before entering the tubular gas heating furnace for preheating. The preheated corrosive gas medium is connected to the first dosing pump through an output pipeline, and a temperature and pressure sensor is provided on the output pipeline.
7. The device according to claim 6, It is characterized in that The gas flow controller controls the gas flow rate to be no less than 3 L / min.