Hydrogen damage detection on-line sampling device for hydrogen-doped natural gas pipeline

CN224695556UActive Publication Date: 2026-08-28SHANGHAI GAS ENG DESIGN & RES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522410217.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-13
Publication Date
2026-08-28
Estimated Expiration
2035-11-13

AI Technical Summary

Technical Problem

[0002]氢气对管道材料的损伤情况与掺氢比例、输送压力、输送速度、管道材质、天然气组分等有关,理论分析非常复杂,目前只能初步判断损伤趋势无法定量计算,且工程上积累的经验数据也非常有限,导致工程上无法准确评估在役管道的氢损伤情况

Benefits of technology

[0014]本实用新型实现了在运行管道不停输的情况下进行取样,分析结果能够真实可靠的反映在役管道的氢损伤情况。同时可以每隔一定时间多次取样,不断监视管道氢损伤发展情况。解决了在役输氢管道氢损伤情况难以评估的问题。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224695556U_ABST
    Figure CN224695556U_ABST
Patent Text Reader

Abstract

The utility model discloses hydrogen damage detection on -line sampling device of natural gas hydrogen pipeline, including setting in the pry dress, two parallelly arranged sampling pipe, one end of two sampling pipes all stretches out from pry dress, and is connected with the natural gas pipeline to be tested, and the other end all is connected with the manifold, and the position of natural gas pipeline between two sampling pipes is equipped with main cut -off valve, and two sampling pipes from one end with natural gas pipeline to the other end connected with manifold all include sampling pipe cut -off valve, nitrogen replacement mouth, vent pipe connecting mouth, 8 blind plate cut -off mouth in proper order, and same number's multiple sampling section, and the pipeline material and pipe diameter of every sampling section are all completely same with natural gas pipeline, and all are equipped with the same welding seam with the welding process and anticorrosion process of natural gas pipeline, and the length of two sampling sections of two sampling pipes distance manifold same distance is same. The utility model can be under the condition of not stopping gas, and the hydrogen damage condition of hydrogen mixing natural gas pipeline in service is accurately evaluated.