Powder metallurgy water cooled die set

CN224854987UActive Publication Date: 2026-10-16SUZHOU NETABHAPE COMPOSITE MATERIALS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522347328.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-05
Publication Date
2026-10-16
Estimated Expiration
2035-11-05

AI Technical Summary

Technical Problem

[0002]粉末冶金传统设计中,水冷中模都会采用在成型中模的底部开进水口和出水口,目的是方便给产品降温,提高产品压制稳定性;此种设计缺陷是遇到产品总高大于50mm以上,水冷中模进水管和出水管很容易因为产品总高高,成型中模行程大,由于水冷中模下面的水管要穿过垫圈,水管被成型模架上下移动压到容易导致水管被垫圈压爆

Benefits of technology

本实用新型将水冷中模的进水口和出水口都设置在了水冷中模上面,防止水管被成型模架压爆裂,提高了粉末冶金成型的稳定性。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224854987U_ABST
    Figure CN224854987U_ABST
Patent Text Reader

Abstract

The utility model relates to a powder metallurgy water -cooling middle die, including water -cooling middle die body, be equipped with water -cooling circulation passageway in water -cooling middle die body, the both ends of water -cooling circulation passageway are equipped with water -cooling middle die water inlet and water -cooling middle die water outlet respectively, water -cooling middle die water inlet and water -cooling middle die water outlet all set up at the upper end surface place of water -cooling middle die body, make water -cooling middle die water inlet and water -cooling middle die water outlet in the upper end of water -cooling middle die body pass through water circulation pipeline intercommunication corresponding water supply mechanism. The utility model sets up the water inlet and water outlet of water -cooling middle die on the water -cooling middle die, prevent the water pipe from being shaped mould frame pressure burst, improved the stability of powder metallurgy forming.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of powder metallurgy technology, specifically to a water-cooled explosion-proof intermediate mold for powder metallurgy. Background Technology

[0002] In traditional powder metallurgy designs, water-cooled intermediate molds typically have inlet and outlet ports at the bottom of the forming die to facilitate product cooling and improve product pressing stability. However, this design has a drawback: when the total product height exceeds 50mm, the water inlet and outlet pipes of the water-cooled intermediate mold are prone to bursting due to the large stroke of the forming die and the fact that the water pipes under the water-cooled intermediate mold must pass through gaskets. The water pipes are easily crushed by the gaskets as the forming die moves up and down. Utility Model Content

[0003] The purpose of this invention is to overcome the problems existing in the prior art and provide a powder metallurgy water-cooling intermediate mold to prevent water pipes from being crushed by the forming mold frame.

[0004] To achieve the above-mentioned technical objectives and effects, this utility model is implemented through the following technical solution: A water-cooled intermediate mold for powder metallurgy includes a water-cooled intermediate mold body. The water-cooled intermediate mold body is provided with a water-cooled circulation channel. The two ends of the water-cooled circulation channel are respectively provided with a water-cooled intermediate mold inlet and a water-cooled intermediate mold outlet. The water-cooled intermediate mold inlet and outlet are both located on the upper end face of the water-cooled intermediate mold body, so that the water-cooled intermediate mold inlet and outlet are connected to the corresponding water supply mechanism at the upper end of the water-cooled intermediate mold body through a water circulation pipeline.

[0005] Furthermore, the diameter of the water-cooled intermediate mold inlet and outlet is larger than the width of the corresponding powder feeder.

[0006] Furthermore, the water-cooled intermediate mold inlet and outlet are flared structures with a smaller bottom and a larger opening.

[0007] Furthermore, the water-cooling circulation channel is spirally arranged from top to bottom along the axial direction of the water-cooling intermediate mold body.

[0008] Furthermore, the outlet of the water-cooled intermediate mold is connected to the upper end of the water-cooling circulation channel, and the inlet of the water-cooled intermediate mold is connected to the lower end of the water-cooling circulation channel through an auxiliary water channel provided in the body of the water-cooled intermediate mold.

[0009] The beneficial effects of this utility model are: This invention places both the water inlet and outlet of the water-cooled intermediate mold on the water-cooled intermediate mold, preventing the water pipe from being crushed by the forming mold frame and improving the stability of powder metallurgy forming. Attached Figure Description

[0010] Figure 1 This is a three-dimensional structural diagram of the present invention; Figure 2 This is a top view of the structure of this utility model; Figure 3 for Figure 2 RR cross-section diagram.

[0011] The labels in the diagram are as follows: 1. Water-cooled intermediate mold body; 2. Water-cooled circulation channel; 3. Water-cooled intermediate mold inlet; 4. Water-cooled intermediate mold outlet; 5. Auxiliary water channel. Detailed Implementation

[0012] The present invention will now be described in detail with reference to the accompanying drawings and embodiments.

[0013] like Figures 1 to 3 As shown, a water-cooled intermediate mold for powder metallurgy includes a water-cooled intermediate mold body 1. The water-cooled intermediate mold body 1 is provided with a water-cooled circulation channel 2. The two ends of the water-cooled circulation channel 2 are respectively provided with a water-cooled intermediate mold inlet 3 and a water-cooled intermediate mold outlet 4. The water-cooled intermediate mold inlet 3 and the water-cooled intermediate mold outlet 4 are both located at the upper end surface of the water-cooled intermediate mold body 1, so that the water-cooled intermediate mold inlet 3 and the water-cooled intermediate mold outlet 4 are connected to the corresponding water supply mechanism at the upper end of the water-cooled intermediate mold body 1 through a water circulation pipeline.

[0014] The diameter of the water-cooled intermediate mold inlet 3 and the water-cooled intermediate mold outlet 4 is larger than the width of the corresponding powder feeder.

[0015] The water-cooled intermediate mold inlet 3 and water-cooled intermediate mold outlet 4 are flared structures with a small bottom and a large opening.

[0016] The water-cooled circulation channel 2 is spirally arranged from top to bottom along the axial direction of the water-cooled intermediate mold body 1.

[0017] The water outlet 4 of the water-cooled intermediate mold is connected to the upper end of the water-cooled circulation channel 2, and the water inlet 3 of the water-cooled intermediate mold is connected to the lower end of the water-cooled circulation channel 2 through the auxiliary water channel 5 set in the water-cooled intermediate mold body 1. The holes on the side of the water-cooled intermediate mold body 1 are manufacturing process holes, which are sealed when in use and do not affect the water circulation in the channel.

[0018] The above description is merely a preferred embodiment of this utility model and is not intended to limit the utility model. Various modifications and variations can be made to this utility model by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this utility model should be included within the protection scope of this utility model.

Claims

1. A water-cooled intermediate mold for powder metallurgy, characterized in that, The system includes a water-cooled intermediate mold body (1), which has a water-cooled circulation channel (2) inside. The two ends of the water-cooled circulation channel (2) are respectively provided with a water-cooled intermediate mold inlet (3) and a water-cooled intermediate mold outlet (4). The water-cooled intermediate mold inlet (3) and the water-cooled intermediate mold outlet (4) are both located on the upper end face of the water-cooled intermediate mold body (1), so that the water-cooled intermediate mold inlet (3) and the water-cooled intermediate mold outlet (4) are connected to the corresponding water supply mechanism through a water circulation pipeline at the upper end of the water-cooled intermediate mold body (1).

2. The powder metallurgy water-cooled intermediate mold according to claim 1, characterized in that, The diameter of the water-cooled intermediate mold inlet (3) and the water-cooled intermediate mold outlet (4) is greater than the width of the corresponding powder feeder.

3. The powder metallurgy water-cooled intermediate mold according to claim 1 or 2, characterized in that, The water-cooled intermediate mold inlet (3) and water-cooled intermediate mold outlet (4) are flared structures with a small bottom and a large opening.

4. The powder metallurgy water-cooled intermediate mold according to claim 1, characterized in that, The water-cooled circulation channel (2) is spirally arranged from top to bottom along the axial direction of the water-cooled intermediate mold body (1).

5. The powder metallurgy water-cooled intermediate mold according to claim 4, characterized in that, The water outlet (4) of the water-cooled intermediate mold is connected to the upper end of the water-cooled circulation channel (2), and the water inlet (3) of the water-cooled intermediate mold is connected to the lower end of the water-cooled circulation channel (2) through the auxiliary water channel (5) set in the water-cooled intermediate mold body (1).