A double-sided fleece fabric
Patent Information
- Application Number
- CN202521917777.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-05
- Publication Date
- 2026-10-27
- Estimated Expiration
- 2035-09-05
AI Technical Summary
[0003]然而,传统的单面毛纱面料存在毛纱易从底料上脱落的问题,这不仅影响了产品的美观性,还降低了使用寿命
本申请设指导双面毛纱面料能提高布料的使用寿命,并且蓬松效果好,面料柔软度好。
Smart Images

Figure CN224901668U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the technical field of fabrics, and in particular to a double-sided woolen fabric. Background Technology
[0002] In the textile industry, most wool yarn fabrics are single-sided wool. Single-sided wool yarn fabrics are widely used in clothing and home textile products because of their good fluffiness and softness.
[0003] However, traditional single-sided wool fabrics have the problem of the wool fibers easily falling off the base material, which not only affects the appearance of the product but also reduces its service life. Utility Model Content
[0004] In order to improve the service life of the fabric, this application provides a double-sided woolen fabric.
[0005] This application provides a double-sided wool yarn fabric, which adopts the following technical solution: A double-sided woolen fabric includes a base material and a woolen yarn material. The woolen yarn material is disposed on the base material. The woolen yarn material forms a front woolen yarn surface on one side of the base material and a back woolen yarn surface on the other side of the base material. The fibers on both the front and back woolen yarn surfaces form a fluffy, anti-loosening fabric surface.
[0006] By adopting the above technical solution, a raising machine is used to raise the wool yarn, so that a portion of the fibers of the wool yarn form the front wool yarn surface on one side of the base material, and the remaining fibers form the back wool yarn surface on the other side of the base material; finally, the front and back wool yarn surfaces form the fluffy fabric surface, and the anti-shedding fabric fluffy surface in the front and back wool yarn materials reduces the phenomenon of wool shedding and improves the service life of the fabric.
[0007] Optionally, the single fiber on the front yarn surface is bonded together with other fibers through high temperature, and the single fiber on the back yarn surface is bonded together with other fibers through high temperature.
[0008] By adopting the above technical solution, when a single fiber on the front of the yarn is connected with other fibers through high temperature, the fiber will shrink; when the fiber shrinks, it will intertwine and lock together, thereby achieving the effect of fixing the hair and preventing hair loss.
[0009] Optionally, the single fiber on the front yarn surface crosses with other fibers through airflow, and the single fiber on the back yarn surface crosses with other fibers through airflow.
[0010] By adopting the above technical solution, before the single fiber on the front yarn surface is connected with other fibers, the airflow connects the single fiber with other fibers to achieve fiber cross-linking; in this way, when the fibers shrink later, they will be better interwoven and locked, thereby achieving a better effect of fixing the fibers and preventing them from falling out, and also having a good fluffy effect and good fabric softness.
[0011] Optionally, the number of fibers in the front yarn surface accounts for 40%-60% of the total number of fibers in the yarn, and the total number of fibers in the yarn is the number of fibers in the back yarn surface excluding the total number of fibers in the yarn.
[0012] Optionally, the yarn is a fiber between 100D / 144F and 300D / 576F.
[0013] Optionally, the base material is woven from 100D / 48FFDY warp and 100D / 48FDTY weft.
[0014] In summary, this application includes at least one of the following beneficial technical effects: This application provides guidance on how double-sided woolen fabric can improve the fabric's lifespan, and also provides good fluffiness and softness. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the structure in this application embodiment, in which a napping machine is used to form a front napped surface on one side of the base material and a back napped surface on the other side. Figure 2 This is a schematic diagram of the structure of the double-sided woolen fabric in the embodiments of this application.
[0016] Attached labels: 1. Base material; 2. Yarn material; 3. Front yarn side; 4. Back yarn side. Detailed Implementation
[0017] The following is in conjunction with the appendix Figure 1-2 This application will be described in further detail.
[0018] This application discloses a double-sided wool yarn fabric.
[0019] refer to Figure 1 A double-sided woolen fabric, comprising a base material 1, woven from 100D / 48FFDY warp yarns and 100D / 48FDTY weft yarns.
[0020] A wool yarn 2 is woven on the base material 1. The wool yarn 2 is made of fibers between 100D / 144F and 300D / 576F, with the best being 150D / 288F.
[0021] The raising machine raises 55% of the fibers in the yarn 2 to form the front yarn surface 3, and the raising machine pulls the remaining 45% of the fibers in the yarn 2 to the side of the bottom material 1 away from the front yarn surface 3 to form the back yarn surface.
[0022] refer to Figure 1 and Figure 2 The airflow in the air knife crosses the single fiber on the front yarn surface 3 with other fibers; then the high-temperature airflow (temperature ≥150 degrees Celsius) blows onto the cross-linked fibers on the front yarn surface 3, causing the cross-linked fibers to shrink. This allows the fibers on the front yarn surface 3 to lock and fix each other, thus forming a fluffy fabric surface.
[0023] The airflow in the air knife crosses the single fiber on the back yarn surface 4 with other fibers; then a high-temperature airflow (temperature ≥150 degrees Celsius) is blown onto the cross-linked fibers on the back yarn surface 4, causing the cross-linked fibers to shrink. This allows the fibers on the back yarn surface 4 to lock and fix each other, thus forming a fluffy fabric surface.
[0024] In this way, the fibers on both sides of the base material 1 are locked and fixed, and both sides of the base material 1 form a fluffy fabric surface with good pile retention, thereby improving the fabric life.
[0025] The above are all preferred embodiments of this application, and are not intended to limit the scope of protection of this application. Therefore, all equivalent changes made in accordance with the structure, shape and principle of this application should be covered within the scope of protection of this application.
Claims
1. A double-sided woolen fabric, comprising a base material (1), characterized in that, It also includes a wool yarn (2), which is disposed on the base material (1). The wool yarn (2) forms a front wool yarn surface (3) on one side of the base material (1) and a back wool yarn surface (4) on the other side of the base material (1). The fibers on the front wool yarn surface (3) and the fibers on the back wool yarn surface (4) both form a fluffy anti-loosening fabric surface.
2. The double-sided woolen fabric according to claim 1, characterized in that, The single fiber on the front yarn surface (3) is connected to other fibers by high temperature, and the single fiber on the back yarn surface (4) is connected to other fibers by high temperature.
3. The double-sided woolen fabric according to claim 2, characterized in that, The single fiber on the front yarn surface (3) intersects with other fibers through airflow, and the single fiber on the back yarn surface (4) intersects with other fibers through airflow.
4. The double-sided woolen fabric according to claim 1, characterized in that, The number of fibers in the front yarn surface (3) accounts for 40%-60% of the total number of fibers in the yarn material (2), and the total number of fibers in the yarn material (2) is the number of fibers in the back yarn surface (4) excluding the total number of fibers in the yarn material (2).
5. The double-sided woolen fabric according to claim 1, characterized in that, The yarn (2) is a fiber between 100D / 144F and 300D / 576F.
6. The double-sided woolen fabric according to claim 1, characterized in that, The base material (1) is woven from 100D / 48FFDY warp and 100D / 48FDTY weft.