Exhaust mechanism for sand mold with iron mold
By designing a stable exhaust assembly, including a multi-stage buffer and purification airflow exhaust mechanism for iron mold sand coating molds, the problem of unstable airflow in traditional iron mold sand coating mold exhaust systems has been solved, improving casting quality and system reliability.
Patent Information
- Application Number
- CN202521960569.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-12
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-09-12
AI Technical Summary
The venting system of traditional iron molds with sand coating has unstable airflow, which leads to unstable negative pressure field in the cavity. This can easily cause molten metal to be drawn back into the venting channel, affecting the quality of the casting.
A stable exhaust assembly is designed, including an air inlet, first and second air collection chambers, first and second pipes, and connectors. It ensures airflow stability by using multi-stage buffering and purification of airflow, adjusting airflow speed with filters and throttling plates, and reducing resistance with high-temperature resistant metal materials.
It has significantly improved the casting yield, avoided the problem of molten metal being sucked back into the exhaust duct, enhanced the system's adaptability and reliability, and reduced the frequency of maintenance.
Smart Images

Figure CN224992239U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of iron mold sand coating mold technology, specifically an air venting mechanism for iron mold sand coating mold. Background Technology
[0002] Iron molds with sand coating are a common type of mold used in casting. They consist of an iron mold and a layer of sand covering the surface of the mold. They are mainly used in the casting process, especially when producing large and complex castings, providing high precision and casting quality. Iron molds with sand coating are widely used in various casting processes, especially when manufacturing large or complex-shaped castings, such as engine parts, mechanical structural parts, and pressure vessels.
[0003] Metal mold bodies are not breathable, and venting relies entirely on a pre-designed venting system and the micropores of an extremely thin sand coating. This places extremely high demands on the stability and reliability of the venting system. Currently, iron molds with sand coating generally use external vacuum pumps for active venting. However, traditional single-stage or straight-through venting structures have certain defects. The venting process is characterized by significant airflow pulsation and poor system stability. The suction effect of the vacuum pump acts directly and without buffering on the mold cavity through the pipe, causing the negative pressure field inside the cavity to be unstable. At the moment of sudden increase in negative pressure, it is very easy to draw the molten metal that has not yet solidified into the venting channel, causing blockage of the venting channel, failure of the venting system, and direct impact on the quality of the casting.
[0004] Therefore, a sand-coated iron mold exhaust mechanism is proposed to solve the aforementioned technical problem of unstable airflow. Utility Model Content
[0005] To address the shortcomings of existing technologies, this utility model provides an exhaust mechanism for iron molds coated with sand, which has the advantage of stable exhaust and solves the problem of poor exhaust stability.
[0006] To achieve the above objectives, this utility model provides the following technical solution: a sand-coated iron mold venting mechanism, comprising an upper mold and a lower mold, wherein the upper mold is located above the lower mold, and a stable venting component is provided on the upper mold; The stable exhaust assembly includes several sets of air inlets, a first gas collecting chamber, a first pipe, a second gas collecting chamber, and a second pipe connected sequentially along the gas flow direction. The volume of the second gas collecting chamber is larger than the volume of the first gas collecting chamber. Several sets of connecting parts are provided on the upper mold, and the connecting parts are connected to the second pipe.
[0007] Furthermore, several sets of the connecting parts are equally spaced on the outside of the upper mold, and the connecting parts are connected to the air inlet of the external vacuum pump.
[0008] Furthermore, the length of the first tube is less than the length of the second tube, and the cross-sectional shape of both the first gas collecting chamber and the second gas collecting chamber is rectangular.
[0009] Furthermore, a filter screen is installed inside the air intake hole, which is used to block impurities such as dust and sand particles.
[0010] Furthermore, a throttling plate is provided inside the first pipe, and a throttling orifice is formed on the throttling plate.
[0011] Furthermore, the first and second tubes are made of high-temperature resistant metals, and their inner walls are smooth to reduce airflow resistance.
[0012] Furthermore, the bottom of the second gas collecting chamber is provided with a slag discharge port for discharging accumulated impurities.
[0013] Compared with the prior art, the technical solution of this application has the following beneficial effects: 1. The venting mechanism of this iron mold sand-coated mold first buffers and gathers the high-speed, pulsating airflow from the mold cavity in the first gas collection chamber, and then fully expands and slows down in the larger second gas collection chamber. The gas flow rate is significantly reduced. This design greatly smooths the airflow pulsation caused by vacuum pump suction and pouring process, making the entire venting process continuous and stable. It effectively avoids the problem of molten metal being sucked back into the venting channel due to violent fluctuations in negative pressure. It fundamentally solves the technical bottleneck of unstable venting in traditional direct-discharge structure and significantly improves the casting yield.
[0014] 2. The air venting mechanism of this iron mold sand coating mold features throttling orifices on the throttling plate that precisely throttle the airflow, allowing adjustment of the venting speed and back pressure according to different process requirements, thus optimizing the filling process. The filter screen at the air inlet effectively blocks resin sand dust, sand particles, and other impurities from entering the venting system, preventing blockage of subsequent pipes and the air collection chamber. The combination of these two features greatly enhances the system's adaptability, reliability, and anti-clogging capability, reducing maintenance frequency. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the overall structure of this utility model; Figure 2 This is a top view of the structure of this utility model; Figure 3 This is a top view of the connection structure between the connector and the upper mold in this utility model; Figure 4 This is a cross-sectional view of the upper mold in this utility model; Figure 5 This utility model Figure 4 Enlarged schematic diagram of the structure at point A in the middle; Figure 6 This is a schematic diagram of the throttling plate structure in this utility model.
[0016] In the diagram: 100, upper mold; 200, lower mold; 300, stable exhaust assembly; 301, air inlet; 302, first air collection chamber; 303, first pipe; 304, second air collection chamber; 305, second pipe; 306, connector; 307, throttling plate; 308, throttling orifice. Detailed Implementation
[0017] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model. Example
[0018] Please see Figure 1-5 The venting mechanism of the iron mold sand coating mold in this embodiment includes an upper mold 100 and a lower mold 200. The upper mold 100 is located above the lower mold 200, and a stable venting component 300 is provided on the upper mold 100. It should be noted that the upper mold 100 and the lower mold 200 are indispensable components in the existing iron mold sand coating mold, and the usage method and working principle of the upper mold 100 and the lower mold 200 are technologies known to those skilled in the art of iron mold sand coating mold, and will not be described in detail in this application.
[0019] The stable exhaust assembly 300 includes several sets of air inlets 301, a first gas collecting chamber 302, a first pipe 303, a second gas collecting chamber 304, and a second pipe 305 connected sequentially along the gas flow direction. The volume of the second gas collecting chamber 304 is larger than the volume of the first gas collecting chamber 302. Several sets of connectors 306 are provided on the upper mold 100, and the connectors 306 are connected to the second pipe 305.
[0020] During application, in the casting process, the gas generated in the mold cavity is first drawn into the exhaust system through several sets of air inlets 301 set on the upper mold 100 by the external vacuum pump. The high-speed pulsating airflow carrying impurities first enters the first gas collecting chamber 302. Due to the buffering effect of this chamber, the airflow velocity is initially reduced. Some of the larger and heavier particles in the airflow undergo initial settling due to the reduction of kinetic energy and gravity, realizing the initial separation of impurities. The stabilized airflow then enters the second gas collecting chamber 304 with a larger volume. Due to the sudden increase in the cross-sectional area of the chamber, the gas velocity is significantly reduced according to the principle of fluid continuity. The reduction in velocity reduces the carrying capacity of fine dust impurities in the gas, thus allowing them to settle fully at the bottom of the second gas collecting chamber 304, achieving deep purification and impurity collection. After multiple stages of buffering, throttling and purification, the clean and stable gas is finally transported to the connector 306 through the second pipe 305 and smoothly discharged from the system through the connector 306, thereby forming a continuous and stable negative pressure environment in the mold cavity. Example
[0021] The basic content is the same as in Example 1, except that: Please see Figure 3-5 In this embodiment, several sets of connectors 306 are equally spaced on the outside of the upper mold 100, and the connectors 306 are connected to the air inlet of the external vacuum pump.
[0022] The length of the first tube 303 is less than the length of the second tube 305. The cross-sectional shape of the first gas collecting chamber 302 and the second gas collecting chamber 304 is rectangular. Compared with the circular cross-section of the gas collecting chamber with the throttling effect of the throttling hole 308, the rectangular cross-section is easier to process and manufacture. Moreover, its flat bottom is more conducive to the accumulation of sedimented impurities towards the slag discharge port, avoiding the accumulation of impurities in the corners of the chamber and making it easier to clean.
[0023] The air inlet 301 is equipped with a filter screen, which is used to block impurities such as dust and sand.
[0024] A throttling plate 307 is provided inside the first tube 303. A throttling orifice 308 is provided on the throttling plate 307. The throttling orifice 308 can effectively suppress the airflow pulsation from the cavity, making the airflow entering the second-stage gas collection cavity more stable and further avoiding pressure fluctuations.
[0025] The first pipe 303 and the second pipe 305 are made of high-temperature resistant metal. Their inner walls are smooth to reduce airflow resistance, ensuring that the pipes can work for a long time in a high-temperature gas environment without deformation, oxidation or performance degradation, thus guaranteeing the durability of the system. They significantly reduce the friction resistance of gas flow, reduce pressure loss, and improve exhaust efficiency. At the same time, they also help prevent dust from adhering to the pipe walls and have a certain self-cleaning effect.
[0026] The bottom of the second air chamber 304 is equipped with a slag discharge port for discharging accumulated impurities.
[0027] It should be noted that the slag discharge port at the bottom of the second gas collection chamber 304 facilitates the regular cleaning of impurities accumulated there, ensuring the long-term stability and maintenance-free nature of the system.
[0028] During application, in the pouring process, the connector 306 connected to the external vacuum pump is activated. Because several sets of connectors 306 are evenly spaced on the outside of the upper mold 100, the negative pressure distribution in each area of the mold cavity is ensured to be uniform, avoiding localized poor venting. Under the uniform negative pressure, the gas generated in the cavity first enters the exhaust system through the air inlet 301. The filter screen installed in the air inlet 301 immediately plays its role, effectively blocking large particles such as dust and sand, preventing them from entering the system, thus achieving preliminary gas purification. The filtered airflow, carrying a small amount of fine impurities, enters the first gas collecting chamber 302. This rectangular chamber provides initial buffering for the high-speed pulsating airflow, causing the flow rate to decrease. Some particles with greater inertia or under gravity undergo initial settling here, achieving initial separation of impurities. The airflow then enters the first pipe 303, which is made of high-temperature resistant metal with a smooth inner wall, effectively reducing flow resistance. More importantly, the throttling plate 307 and its throttling orifice 308 inside the pipe constitute a key control unit. The throttling effect of the throttling orifice 308 allows for precise adjustment and control of the airflow velocity, thereby optimizing the system back pressure and exhaust flow according to different casting process requirements. This greatly enhances process adaptability and control precision, further stabilizing the airflow. The throttled and stabilized airflow then enters the larger, rectangular cross-section of the second gas collecting chamber 304. Here, the cross-sectional area of the airflow channel increases significantly. According to fluid mechanics principles, the gas velocity drops sharply. This rapid decrease in velocity greatly weakens the gas's ability to carry fine dust particles, causing these fine impurities to settle fully at the bottom of the second gas collecting chamber 304, achieving deep purification of the gas. Finally, the clean gas, after thorough purification and pressure stabilization, is smoothly delivered to the connector 306 through the longer second pipe 305. The second pipe 305 also uses a high-temperature resistant material with a smooth inner wall, ensuring reliability during long-term operation in high-temperature environments and low resistance and high efficiency in airflow transmission. The gas is then smoothly extracted by the vacuum pump, thus maintaining a uniform and stable negative pressure environment within the mold cavity.
[0029] In summary, the working principle of the air venting mechanism of this iron mold with sand coating is as follows: During the casting process, the connector 306, which connects to the external vacuum pump, is activated. Because several sets of connectors 306 are evenly spaced on the outside of the upper mold 100, the negative pressure distribution in each area of the mold cavity is ensured to be uniform, avoiding localized poor venting. Under the uniform negative pressure, the gas generated in the cavity first enters the exhaust system through the air inlet 301. The filter screen installed inside the air inlet 301 immediately functions, effectively blocking large particles such as dust and sand, preventing them from entering the system and achieving preliminary gas purification. The filtered airflow, carrying a small amount of fine impurities, enters the first gas collecting chamber 302. This rectangular chamber provides initial buffering for the high-speed pulsating airflow, causing the flow rate to decrease. Some particles with high inertia or under gravity undergo initial settling here, achieving initial impurity separation. The airflow then enters the first pipe 303, which is made of high-temperature resistant metal with a smooth inner wall, effectively reducing flow resistance. More importantly, the throttling plate 307 and its throttling orifice 308 inside the pipe constitute a key control unit. The throttling effect of the orifice 308 allows for precise adjustment and control of the airflow velocity, thereby optimizing the system back pressure and exhaust flow according to different casting process requirements. This greatly enhances process adaptability and control precision, further stabilizing the airflow. The throttled and stabilized airflow then enters the larger, rectangular second gas collecting chamber 304. Here, the cross-sectional area of the airflow channel increases significantly. According to fluid mechanics principles, the gas velocity drops sharply. This rapid decrease in velocity greatly weakens the gas's ability to carry fine dust particles, causing these fine impurities to settle fully at the bottom of the second gas collecting chamber 304, achieving deep purification of the gas. Finally, the clean gas, after thorough purification and pressure stabilization, is smoothly delivered to the connector 306 through the longer second pipe 305. The second pipe 305 also uses a high-temperature resistant material with a smooth inner wall, ensuring reliability during long-term operation in high-temperature environments and low resistance and high efficiency in airflow transmission. The gas is then smoothly extracted by the vacuum pump, thus maintaining a uniform and stable negative pressure environment within the mold cavity.
[0030] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.
[0031] Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the present invention.
Claims
1. A venting mechanism for a sand-coated iron mold, characterized in that: It includes an upper mold (100) and a lower mold (200), the upper mold (100) being located above the lower mold (200), and a stable venting assembly (300) being provided on the upper mold (100). The stable exhaust assembly (300) includes several sets of air inlets (301), a first gas collection chamber (302), a first pipe (303), a second gas collection chamber (304), and a second pipe (305) connected sequentially along the gas flow direction. The volume of the second gas collection chamber (304) is larger than the volume of the first gas collection chamber (302). Several sets of connectors (306) are provided on the upper mold (100). The connectors (306) are connected to the second pipe (305).
2. The air venting mechanism for a sand-coated iron mold according to claim 1, characterized in that: Several sets of the connecting parts (306) are equally spaced on the outside of the upper mold (100), and the connecting parts (306) are connected to the air inlet of the external vacuum pump.
3. The air venting mechanism for a sand-coated iron mold according to claim 1, characterized in that: The length of the first tube (303) is less than the length of the second tube (305), and the cross-sectional shape of the first gas collecting chamber (302) and the second gas collecting chamber (304) is rectangular.
4. The air venting mechanism for a sand-coated iron mold according to claim 1, characterized in that: The air inlet (301) is equipped with a filter screen, which is used to block dust and sand impurities.
5. The air venting mechanism for a sand-coated iron mold according to claim 1, characterized in that: A throttling plate (307) is provided inside the first tube (303), and a throttling hole (308) is provided on the throttling plate (307).
6. The air venting mechanism for a sand-coated iron mold according to claim 1, characterized in that: The first tube (303) and the second tube (305) are made of high-temperature resistant metal, and their inner walls are smooth to reduce airflow resistance.