Mold for casting with embedded tube and castings thereof

By using cooling blocks and fixing kits in the mold, the problem of thermal deformation of stainless steel pipes inside aluminum alloy castings was solved, achieving high-yield casting production, reducing production costs, and promoting the application of integrated components.

CN224992267UActive Publication Date: 2026-11-20HUZHOU MEIMAI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522686208.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-18
Publication Date
2026-11-20
Estimated Expiration
2035-12-18

AI Technical Summary

Technical Problem

When stainless steel pipes are embedded in aluminum alloy castings, high-temperature casting causes thermal deformation of the stainless steel pipes, resulting in the casting wall thickness not meeting the requirements, which affects the yield and production cost.

Method used

The mold design incorporates cooling blocks and fixing components. The cooling blocks absorb heat to reduce thermal deformation of the pipes, while the fixing components stabilize the pipe positions and ensure precise control of the clearance. Combined with a reasonable coolant channel design, the cooling effect and the fluidity of the molten aluminum are optimized.

Benefits of technology

It has improved the yield of castings, ensured that the wall thickness of the main body of the casting meets the requirements, reduced production costs, and promoted the application of integrated components in industries such as commercial aerospace.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224992267U_ABST
    Figure CN224992267U_ABST
Patent Text Reader

Abstract

The utility model relates to foundry molding technical field, specifically disclose a kind of mould for castings with embedded pipe and its castings.The mould is used to process the castings with embedded pipeline, mould contains sand mould and auxiliary kit embedded in sand mould, auxiliary kit contains two groups of cooling block, cooling chamber formed between two groups of cooling block and the fixing kit for fixing pipeline, which is arranged outside two groups of cooling block;Wherein when pipeline is fixed, the main body of pipeline is placed in cooling chamber;And the wall surface of pipeline and the containing gap between the top and bottom inner wall surface of cooling chamber is 10~15mm.The cooling block in the mould of the utility model can absorb and transfer the heat absorbed by pipeline during aluminum liquid pouring, thereby significantly reducing the thermal deformation of pipeline, avoiding its excessive expansion to occupy the space of aluminum liquid and causing the defects of insufficient wall thickness of castings main body or pipeline exposure, to improve the yield of product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of casting molding technology, specifically to a mold for manufacturing castings containing pre-embedded pipes and the resulting castings. Background Technology

[0002] With the continuous development of industries such as commercial aerospace, the requirements for rapid assembly of components to shorten the assembly cycle are constantly being put forward, and the integration of parts and components has become a major development trend.

[0003] One common requirement for component integration is the pre-embedded installation of pipes within alloy castings. Typically, the main body of such castings is made of aluminum alloy, while the embedded pipes are made of stainless steel. Therefore, during manufacturing, the stainless steel pipes are first placed at the designated locations in the mold, and then the casting process continues to pour the metal to form the main body. During this process, the temperature of the aluminum alloy body during pouring usually reaches 690-730°C. Under these temperatures, the stainless steel pipes are prone to thermal deformation, ultimately resulting in scrap parts. For example, if the aluminum wall thickness near the stainless steel pipe is small, the thermal expansion of the stainless steel pipe during pouring can encroach on the space that the molten aluminum should have filled, potentially leading to a final aluminum wall thickness that does not meet design requirements. This results in parts where the stainless steel pipe protrudes from the main casting, affecting the functionality of the piping and ultimately rendering it scrap.

[0004] Therefore, there is an urgent need for a mold that can achieve high yield production of castings containing embedded pipes, thereby reducing production costs and promoting the use of integrated components. Utility Model Content

[0005] One of the objectives of this utility model is to provide a mold that improves the yield of castings containing embedded pipes;

[0006] The second objective of this utility model is to provide a casting with a pre-embedded pipe that is processed by the above-mentioned mold and gradually has a main body wall thickness that meets the requirements.

[0007] This utility model is achieved through the following technical solution:

[0008] In a first aspect, this utility model provides a mold for casting pre-embedded pipes, used to process castings with pre-embedded pipes. The mold includes a sand mold and an auxiliary kit embedded in the sand mold. The auxiliary kit includes two sets of cooling blocks, a cooling chamber formed between the two sets of cooling blocks, and a fixing kit disposed outside the two sets of cooling blocks for fixing the pipes. When the pipes are fixed, the main body of the pipes is placed in the cooling chamber. The accommodating gap between the wall of the pipes and the top and bottom inner walls of the cooling chamber is 10-15 mm.

[0009] In the mold of this invention, an auxiliary kit is added. The cooling block in the auxiliary kit can reduce the heat supplied to the pipeline during the pouring of molten aluminum and other casting materials, thereby reducing the thermal deformation of the pipeline. The size of the accommodating gap determines the wall thickness of the casting near the pipeline when the final casting is completed. The cooling block arrangement in this invention is mainly applicable to castings with a wall thickness of 10-15mm. For castings with excessively thin walls, additional cooling blocks in the mold can easily cause premature cooling of the molten aluminum near the cooling blocks, thus affecting the flow of molten aluminum during pouring. For castings with excessively thick walls, the cooling effect of the cooling blocks is poor, making it difficult to achieve the goal of controlling the thermal deformation of the pipeline. Therefore, the arrangement of the cooling blocks and the accommodating gap in this invention takes into account both the need to control the thermal deformation of the pipeline and the smooth progress of the normal pouring of the casting body, thereby enabling the production of castings that meet the requirements.

[0010] As a further improvement of this utility model, the thickness of the cooling block is d1, and the thickness of the casting cavity reserved in the sand mold is d0, where d1 = (0.7~1.5)d0.

[0011] The thickness of the cooling block affects its heat transfer efficiency, directly impacting its cooling capacity; conversely, the thickness of the casting chamber in the sand mold directly controls the thickness of the casting body. Therefore, under these constraints, users can select cooling blocks of different sizes based on the specifications of the casting being processed. This ensures that when the cooling block is in operation, it can control the thermal deformation of the pipes without causing premature solidification of the molten aluminum flowing in the gaps, thus preventing the casting body from failing to meet production requirements.

[0012] As a further improvement of this utility model, a coolant flow port is provided on the outer surface of the cooling block, and a coolant channel connected to the coolant flow port is provided inside the cooling block.

[0013] As a further improvement of this utility model, the coolant channel includes at least two sets of parallel flow channels and a connecting flow channel located at the end of the flow channels and connecting the flow channels.

[0014] As a further improvement of this utility model, the coolant channel is arranged in the middle of the cooling block.

[0015] As a further improvement of this utility model, the auxiliary kit also includes a positioning block. The working end of the positioning block has the same thickness as the receiving gap, which is used to initially define the position of the pipe. When the pipe is not completely fixed, the positioning block can be placed between the cooling block and the pipe to control the positional relationship between the two. After the pipe is fixed, the positioning block can be removed to avoid interfering with the casting of the main body of the casting.

[0016] As a further improvement of this utility model, the fixing kit includes a fixing hole opened on the sand mold and a fixing bolt adapted to the fixing hole. When the pipe is installed, the fixing bolt is placed in the fixing hole and inserted into the connecting parts at both ends of the pipe to fix the position of the pipe through the connecting parts.

[0017] As a further improvement of this utility model, the fixing bolt is provided with a limiting thread, which is adapted to the working thread on the inner wall of the connecting part.

[0018] Secondly, this utility model provides a casting with a pre-embedded pipe, which is made using any of the above-mentioned molds for castings with pre-embedded pipes, and includes a casting body and a pipe embedded in the casting body.

[0019] As a further improvement of this utility model, the wall thickness of the pipe is 1~1.2mm.

[0020] The beneficial effect of this utility model is that by adding an auxiliary kit including a cooling block, a cooling chamber and a fixing kit to the casting mold, the problem of low yield caused by thermal deformation of the pipe due to high temperature casting is effectively solved in the production process of castings containing embedded pipes.

[0021] The cooling block used absorbs and transfers the heat absorbed by the pipe during the pouring of molten aluminum, significantly reducing the thermal deformation of the pipe and preventing defects such as insufficient wall thickness of the casting body or exposed pipe due to excessive expansion encroaching on the space of the molten aluminum. The fixing kit can firmly fix the position of the pipe in the cooling chamber, ensuring that the main body of the pipe is accurately placed in the cooling chamber. Through the initial limitation of the positioning block and the final fixation of the fixing bolt, the required accommodation gap is precisely maintained between the pipe and the inner wall of the cooling block. The precise control of this gap ensures that the wall thickness of the casting body formed near the pipe after pouring meets the design requirements.

[0022] Furthermore, the ratio between the thickness d1 of the cooling block and the thickness d0 of the sand casting chamber, as well as the rational design of the coolant channels inside the cooling block, further optimize the balance between cooling effect and aluminum liquid flowability. This effectively controls the thermal deformation of the pipes and avoids premature solidification of aluminum liquid in the containment gap, which would affect the quality of the casting.

[0023] After using the mold in this utility model, high-quality integrated parts with accurate pipe pre-embedded positions, standard casting wall thickness, and no pipe exposure defects can be stably produced, which greatly improves the yield rate, reduces production costs, and strongly promotes the application of castings with pre-embedded pipes in industries such as commercial aerospace that have high requirements for rapid assembly and integration. Attached Figure Description

[0024] The accompanying drawings are provided below to illustrate the preferred embodiments of this utility model, in order to aid in understanding the purpose and advantages of this utility model, wherein:

[0025] Figure 1 This is a first-person perspective schematic diagram of the casting structure including the embedded pipe.

[0026] Figure 2 This is a top-down view of the structure of the casting containing the embedded pipe and its cross-section at X-X'.

[0027] Figure 3 This is a schematic diagram of a mold structure for castings containing embedded pipes;

[0028] Figure 4 This is a cross-sectional view of the mold structure for casting pre-embedded pipes and its Y-Y' section from a positive viewing angle.

[0029] Figure 5 A schematic diagram of the internal structure of the mold for casting pre-embedded pipes after removing the upper part of the sand mold;

[0030] Figure 6 The image shows the structure of the cooling block and its cross-section at Z-Z' from a positive viewing angle.

[0031] The mold for casting embedded pipes contains two sand molds that are joined together to form a complete sand mold. Figure 5 The upper part of the sand-shaped structure was removed to reveal its interior space. Detailed Implementation

[0032] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments.

[0033] The directional terms such as up, down, left, right, front, back, front, back, top, and bottom mentioned or possibly used in this specification are defined relative to the construction shown in the accompanying drawings. The terms "inner" and "outer" refer to directions toward or away from the geometric center of a specific component, respectively. These are relative concepts and may therefore vary depending on their location and usage. Therefore, these or other directional terms should not be interpreted as restrictive.

[0034] Example 1:

[0035] This embodiment provides a mold for casting pre-embedded pipes, used for processing such as... Figures 1-2 The casting shown contains a pre-embedded pipe A02, where the main body A01 is formed by casting molten aluminum, and the pipe A02 is a stainless steel pipe. Figures 3-5As shown, the mold mainly consists of two parts: a sand mold 1 and an auxiliary kit 2 embedded in the sand mold 1. The sand mold 1 is a conventional casting tool, containing a casting chamber, an aluminum molten metal pouring channel, and other standard structures; the auxiliary kit 2, as shown... Figure 4 As shown, it includes two sets of cooling blocks 201, a cooling chamber 202 formed between the two sets of cooling blocks 201, and a fixing kit 203 disposed outside the two sets of cooling blocks 201 for fixing the pipe A02. After the pipe A02 is fixed and the auxiliary kit 2 and sand mold 1 are assembled, the main body of the pipe A02 is placed in the cooling chamber 202, with both ends exposed. At the same time, the casting chamber in the sand mold 1 and the cooling chamber 202 in the auxiliary kit 2 together constitute the casting space of the casting body A01. When the aluminum liquid fills the casting space and cools, the casting body A01 is formed. In this embodiment, the casting body A01 needs to form a thickness of 10mm at the top and bottom of the pipe A02, thus maintaining a 10mm accommodating gap L1 between the wall of the pipe A02 and the top and bottom inner walls of the cooling chamber 202. Correspondingly, during the casting process, the cooling block 201 can absorb some heat to reduce the thermal deformation of the stainless steel pipe, thereby avoiding too much or too little aluminum liquid filling the accommodating gap L1, thus reducing the possibility that the wall thickness of the casting body A01 does not meet the requirements.

[0036] Preferably, such as Figure 4 As shown, the thickness of the cooling block 201 is d1, the thickness of the casting cavity reserved in the sand mold 1 is d0, which is also the thickness of the casting body A01 formed by casting. In this embodiment, d1=1.2d0. When the thickness of the cooling block 201 and the target casting body A01 form this proportional relationship, it can ensure that the cooling block 201 has a good cooling effect on the pipe A02, and it can also ensure that the aluminum liquid flowing in the receiving gap L1 will not cool and solidify too early, thus affecting the smooth progress of casting.

[0037] Preferably, such as Figure 6 As shown, the cooling block 201 adopts a water-cooled structure, wherein a coolant flow port 201-1 is opened on the outer surface of the cooling block 201, and a coolant channel 201-2 communicating with the coolant flow port 201-1 is arranged inside the cooling block 201; more preferably, as Figure 6 As shown, the coolant channel 201-2 is arranged in the middle of the cooling block 201 and includes two sets of parallel straight channels 201-2-1 and a connecting channel 201-2-2 arranged at the end of the straight channels 201-2-1, which connects the two sets of straight channels 201-2-1. With this channel arrangement, the cooling water can circulate fully in the cooling block 201 and carry away the heat, avoiding uneven distribution of the heat absorption capacity of the cooling block 201.

[0038] Preferably, the auxiliary kit 2 also includes a positioning block. The working end of the positioning block has a thickness consistent with the receiving gap L1, which is 10 mm in this embodiment. Before the pipe A02 is fully fixed, the positioning block can be placed between the wall of the pipe A02 and the cooling chamber 202 to initially define the position of the pipe A02; then the complete fixing of the pipe A02 can be carried out, and the positioning block can be removed after completion to avoid interfering with the casting of the main casting A01.

[0039] Preferably, such as Figures 1-2 As shown, in this embodiment, the pipe A02 used in the embedded pipe casting has connecting parts A03 with a tee structure at both ends, and therefore, accordingly, as Figure 4 As shown, a fixing hole 203-1 is provided on the sand mold 1 of the mold, and the mold also contains a fixing bolt 203-2 that matches the fixing hole 203-1. When the pipe A02 is installed, the fixing bolt 203-2 passes through the fixing hole 203-1 and is inserted into the connecting member A03, thereby fixing the position of the pipe A02 through the connecting member A03.

[0040] Preferably, the fixing bolt 203-2 is provided with a limiting thread, which is adapted to the working thread on the inner wall of the connecting member A03. Therefore, the contact relationship between the fixing bolt 203-2 and the connecting member A03 restricts the position of the pipe A02 in the horizontal direction. After the threads are engaged, the depth of the fixing bolt 203-2 in the connecting member A03 can control the position of the pipe A02 in the vertical direction. Thus, the fixing bolt 203-2 under this structure can achieve complete fixation of the pipe A02.

[0041] Example 2:

[0042] like Figures 1-2 As shown, this embodiment provides a casting with a pre-embedded pipe, which is made using the mold in Embodiment 1. It includes a casting body A01 and a pipe A02 embedded therein. The casting body A01 is made of molten aluminum, and the pipe A02 is a stainless steel pipe A02. Both ends of the pipe A02 are connected to a connecting member A03 with a tee structure.

[0043] Preferably, in this embodiment, the wall thickness of pipe A02 is 1.2 mm.

[0044] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this utility model, and not to limit it. Although this utility model has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that they can still modify the technical solutions recorded in the foregoing embodiments, or make equivalent substitutions for some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this utility model.

Claims

1. A mold for casting pre-embedded pipes, used to process castings with pre-embedded pipes (A02), the mold comprising a sand mold (1) and an auxiliary kit (2) embedded in the sand mold (1), characterized in that, The auxiliary kit (2) includes two sets of cooling blocks (201), a cooling chamber (202) formed between the two sets of cooling blocks (201), and a fixing kit (203) disposed outside the two sets of cooling blocks (201) for fixing the pipe (A02). When the pipe (A02) is fixed, the main body of the pipe (A02) is placed inside the cooling chamber (202); and the accommodating gap (L1) between the wall of the pipe (A02) and the top and bottom inner walls of the cooling chamber (202) is 10~15mm.

2. The mold for casting a pre-embedded pipe according to claim 1, characterized in that, The thickness of the cooling block (201) is d1, and the thickness of the casting cavity (101) reserved in the sand mold (1) is d0, where d1 = (0.7~1.5)d0.

3. A mold for casting a pre-embedded pipe according to any one of claims 1 or 2, characterized in that, The outer surface of the cooling block (201) is provided with a coolant flow port (201-1), and the cooling block (201) is provided with a coolant channel (201-2) that is connected to the coolant flow port (201-1).

4. A mold for casting a pre-embedded pipe according to claim 3, characterized in that, The coolant passage (201-2) includes at least two sets of parallel flow channels (201-2-1) and a connecting flow channel (201-2-2) located at the end of the flow channels (201-2-1) and connecting the flow channels (201-2-1).

5. A mold for casting a pre-embedded pipe according to claim 3, characterized in that, The coolant channel (201-2) is located in the middle of the cooling block (201).

6. A mold for casting a pre-embedded pipe according to claim 1, characterized in that, The auxiliary kit (2) also includes a positioning block, the working end of which has a thickness consistent with the accommodating gap (L1) for initially defining the position of the pipe (A02).

7. A mold for casting a pre-embedded pipe according to any one of claims 1 or 6, characterized in that, The fixing kit (203) includes a fixing hole (203-1) opened on the sand mold (1) and a fixing bolt (203-2) adapted to the fixing hole (203-1). When the pipe (A02) is installed, the fixing bolt (203-2) is placed in the fixing hole (203-1) and inserted into the connecting parts (A03) at both ends of the pipe (A02) to fix the position of the pipe (A02) through the connecting parts (A03).

8. A mold for casting a pre-embedded pipe according to claim 7, characterized in that, The fixing bolt (203-2) is provided with a limiting thread, which is adapted to the working thread on the inner wall of the connecting piece (A03).

9. A casting containing a pre-embedded pipe, characterized in that, The casting is made using a mold for a pre-embedded pipe as described in any one of claims 1 to 8, comprising a casting body (A01) and a pipe (A02) embedded in the casting body (A01).

10. A casting with a pre-embedded pipe as described in claim 9, characterized in that, The wall thickness of the pipe (A02) is 1~1.2mm.