Pressing strip tooling
By setting through or intermittent grooves on the frame body of the pressure welding strip tooling, it is possible to allow free expansion and contraction under thermal cycling, thus solving the deformation problem caused by thermal cycling and improving the service life of the tooling and the welding quality.
Patent Information
- Application Number
- CN202522564026.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-02
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-12-02
AI Technical Summary
Existing pressure welding strip tooling has a short lifespan due to thermal cycling deformation during the welding process, and there are dynamic thermal stresses and permanent plastic deformations, which affect the uniformity and consistency of the battery cell string welding quality.
Design a pressure welding strip tooling with a frame body and elastically installed pressure pins. The frame body is a hollow frame structure with through or intermittent grooves on the support beams, allowing the frame to expand and contract freely under thermal cycling, reducing the amount of plastic deformation.
It significantly improves the service life of the pressure welding strip tooling. After 100,000 thermal cycles, there is basically no residual deformation, and the flatness stability is excellent, ensuring the uniformity and consistency of welding quality.
Smart Images

Figure CN224992489U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of photovoltaic equipment, specifically a pressure welding strip tooling for a string welding machine. Background Technology
[0002] A string welding machine is a device that welds solar cells and welding strips into a string according to a set pattern. The string welding process can be divided into four stages: preheating, heating, heat preservation, and cooling. To prevent the welding strips from bending and deforming, a welding strip clamping fixture is used to press the welding strips firmly onto the solar cells during the welding process. Since each welding strip clamping fixture is reused on the string welding machine, it undergoes a cycle of heating and cooling during the continuous welding process.
[0003] In this field, pressure welding strip fixtures have various structural forms. During the welding station, the pressure welding strip fixture is located between the welding lamp box and the solar cell to be welded. Therefore, to reduce the impact of heat radiation from the welding lamp box on the solar cell, most pressure welding strip fixtures are typically hollow structures. Under heat radiation heating, the pressure welding strip fixture generates a complex temperature field distribution in the three-dimensional space of the hollow body, especially a large temperature gradient in the thickness direction of the hollow body. According to experimental tests, the working temperature of the upper surface of the hollow body of the pressure welding strip fixture is close to 300°C during operation, while there is a temperature difference between the upper and lower surfaces, ranging from approximately 60°C. This temperature difference causes dynamic thermal deformation and thermal stress in the hollow body during rapid welding. If this thermal cycle deformation is too large, it will directly affect the uniformity and consistency of the solar cell stringing quality. Furthermore, once the thermal stress on the surface of the hollow body exceeds the high-temperature yield limit of the material, permanent plastic deformation will occur on the surface layer of the hollow body. This permanent plastic deformation will accumulate after long-term reciprocating thermal cycling, which will gradually increase the residual stress inside the hollow body, thereby causing fatigue failure of the welding strip tooling and reducing its service life. Utility Model Content
[0004] This application addresses the problem of the short service life of existing pressure welding strip tooling by providing a pressure welding strip tooling with a longer service life.
[0005] This application provides a pressure welding strip tooling, which includes a frame body and pressure pins for pressure welding strips. The frame body is a hollow frame structure composed of several support beams. At least some of the pressure pins are arranged in an array and elastically mounted on the support beams. Several grooves are spaced apart on the upper surface of the support beams, and the grooves extend through the width direction of the support beam.
[0006] The pressure welding strip tooling of this application forms a slotted structure on the upper surface of the support beam of the frame body. Under reciprocating thermal cycling conditions, the shallow layer of the upper surface of the frame body can expand and contract freely, which can reduce the constraint on the expansion of the high-temperature area on its surface, improve the dynamic stress distribution along the thickness direction of the frame body caused by temperature changes, eliminate or effectively reduce the amount of plastic deformation of the shallow surface of the frame body during its heating process, and significantly improve the working life of the pressure welding strip tooling. Experimental verification shows that after 100,000 thermal cycles, the frame body of the pressure welding strip tooling has basically no residual deformation and its flatness stability is excellent.
[0007] In some embodiments, the support beam includes a plurality of transverse beams spaced apart along the length of the frame body and a plurality of longitudinal beams spaced apart along the width of the frame body; wherein: the groove is at least formed on the longitudinal beam and extends through the width of the longitudinal beam.
[0008] The support beams are a frame structure composed of spaced horizontal beams and spaced vertical beams. The structure is simple, stable, and easy to form and manufacture. By setting grooves on at least the longer vertical beams, the deformation of the frame body can be significantly reduced.
[0009] In some embodiments, there is at least one slot unit on the frame body along the length direction of the frame body, and each slot unit includes a plurality of slots arranged side by side along the width direction of the frame body.
[0010] In the same slot unit, each slot is opened on a spaced longitudinal beam, or on all longitudinal beams.
[0011] By opening the slots in the same slot unit on all the longitudinal beams, a slot unit can be manufactured in one go, thereby improving production efficiency. By opening the slots in the same slot unit on the longitudinal beams that are spaced apart, the impact on the mechanical strength of the frame body is smaller, and the tooling can also be guaranteed to have a long service life under cyclic heating and cooling conditions.
[0012] In some embodiments, multiple slot units are spaced apart along the length of the frame body, and each slot unit is symmetrically arranged on both sides of the center line of the length direction of the frame body.
[0013] By setting multiple slot units and arranging them symmetrically, the frame body can be guaranteed to expand and contract uniformly.
[0014] In some embodiments, a slot unit is formed on the center line along the length direction of the frame body.
[0015] By creating a slotted unit along the centerline of the frame body's length, it can be ensured that the frame body expands and contracts uniformly on both sides of its length.
[0016] In some embodiments, at least three slot units are provided on the frame body along the length direction of the frame body, wherein the spacing between two adjacent slot units is equal or unequal.
[0017] At least three slot units should be set, and the spacing between the slot units can be equal or unequal, which can be flexibly selected according to the actual situation.
[0018] In some embodiments, at least two slot units are provided on the frame body along the length direction of the frame body, and the depth of the slot increases as the distance between two adjacent slot units increases.
[0019] Setting the groove depth to increase with the increase of the groove unit spacing can ensure that the frame body maintains appropriate expansion and contraction during heating and cooling, thereby reducing the amount of plastic deformation of the frame body.
[0020] In some embodiments, the groove is also formed on the upper surface of at least one crossbeam, and the groove extends through the width of the crossbeam.
[0021] By creating through slots on the upper surface of the crossbeam, the free expansion and contraction performance of the upper surface of the frame body can be further improved, reducing the amount of plastic deformation of the frame body.
[0022] In some embodiments, the groove is a U-shaped groove, a V-shaped groove, a rectangular groove, or an arc-shaped groove with an arc bottom.
[0023] The cross-sectional shape of the groove can be set in various ways, which can be selected according to the actual situation, increasing the flexibility of selection.
[0024] In some embodiments, the depth of the groove is less than or equal to 1 / 3 of the thickness of the supporting beam, and the depths of the grooves may be the same or different; and / or, the upper width of the groove is 0.3mm-0.7mm.
[0025] By limiting the depth of the groove and its upper width to specific parameters, the strength of the frame body can meet the usage requirements while ensuring that the plastic deformation of the frame body is small.
[0026] In some embodiments, the frame body is made of aluminum alloy castings or aluminum alloy profiles.
[0027] The frame body is made of aluminum alloy, which has a low overall cost.
[0028] In some embodiments, the support beam is further provided with a plurality of pressure needle mounting holes that extend along the thickness direction of the support beam. The pressure needle mounting holes are staggered from the grooves. Each pressure needle is elastically mounted in a pressure needle mounting hole by a spring, so that the pressure needle can extend and retract relative to the support beam, and the lower end of the pressure needle extends downward through the support beam.
[0029] By staggering the mounting holes and slots of the pressure pins, the free expansion and contraction of the frame body are independent of the pressure pins, thus avoiding affecting the pressing effect of the pressure pins on the welding strips. Attached Figure Description
[0030] Figure 1 This is a three-dimensional structural schematic diagram of an optional embodiment of the frame body of the pressure welding strip tooling in this application;
[0031] Figure 2 for Figure 1 The main view;
[0032] Figure 3 for Figure 2 Enlarged view of point A in the image;
[0033] Figure 4 for Figure 2 Top view;
[0034] Figure 5 For the pressure needle assembly Figure 1 A sectional view of the frame body in the middle;
[0035] Figure 6 This is a schematic diagram of the various measurement positions during the pressure welding strip tooling experiment;
[0036] Figure 7 This is a schematic diagram of the reference plane used in the test of the pressure welding strip tooling;
[0037] Figure 8 This is a schematic diagram of the measurement method used in the pressure welding strip tooling experiment;
[0038] Figure 9 The distribution of flatness changes on the upper surface of the tooling in four embodiments of the pressure welding strip tooling after 100,000 welding cycles is shown in the diagram.
[0039] Figure 10 A surface diagram showing the bending changes of the pressure welding strip tooling after 20,000 welding cycles;
[0040] Figure 11 This is a distribution diagram showing the changes in flatness on the upper surface of the pressure welding strip tooling after 20,000 welding cycles, serving as a comparative example.
[0041] Figures 1-5 The components include: a welding strip fixture 1; a frame body 10, a crossbeam 11, a longitudinal beam 12, a groove unit 13, a groove 131, a pressure pin mounting hole 14; a pressure pin 20, and a spring 21. Detailed Implementation
[0042] To make the above-mentioned objectives, features and advantages of this application more apparent and understandable, the application will be further described in detail below with reference to the accompanying drawings and specific embodiments.
[0043] like Figures 1-5 As shown, this application provides a pressure welding strip tool 1 for pressing the welding strip onto the battery cell during the welding process of a string welding machine.
[0044] The welding strip fixture 1 includes a frame body 10 and pressure pins 20 for welding the strip. The frame body 10 is a hollow frame structure composed of several support beams. The support beams can be a combination of horizontal and vertical beams, or a combination of horizontal and diagonal beams, or a combination of vertical and diagonal beams, etc. At least some of the pressure pins 20 are arranged in an array and elastically mounted on the support beams; that is, some pressure pins 20 are mounted in a horizontal and vertical array on the support beams, while some pressure pins 20 can be mounted irregularly on the support beams without being arranged in an array. Several grooves 131 are spaced apart on the upper surface of the support beams, and the grooves 131 extend along the width direction of the support beam.
[0045] The pressure welding strip tooling 1 of this application forms a slotted structure on the upper surface of the support beam of the frame body 10. Under reciprocating thermal cycling conditions, the shallow layer of the upper surface of the frame body 10 can expand and contract freely, which can reduce the constraint on the expansion of the high-temperature area on its surface, improve the dynamic stress distribution along the thickness direction of the frame body 10 caused by temperature changes, eliminate or effectively reduce the amount of plastic deformation of the shallow surface of the frame body 10 during its heating process, and significantly improve the working life of the pressure welding strip tooling 1. After experimental verification, after 100,000 thermal cycles, the frame body 10 of the pressure welding strip tooling 1 has basically no residual deformation, and its flatness stability is excellent.
[0046] The frame body 10 is typically a rectangular openwork frame structure. In one embodiment, the support beams employ a combination of crisscrossing longitudinal and transverse beams. For example... Figure 1 , Figure 3 As shown, the support beam includes multiple transverse beams 11 spaced apart along the length of the frame body 10 and multiple longitudinal beams 12 spaced apart along the width of the frame body 10. Figure 1 , Figure 3 In the illustrated embodiment, the support beam includes six crossbeams 11 and seven longitudinal beams 12. Of course, the number of crossbeams 11 and longitudinal beams 12 can be determined based on the size of the support beam and actual needs, and is not absolute. When the support beam uses a combination of longitudinal and crossbeams, the groove 131 is at least formed on the longitudinal beam 12, and in this case, the groove 131 extends through the width of the longitudinal beam 12. Alternatively, the groove 131 can be formed on both the longitudinal beam 12 and the crossbeams 11 simultaneously.
[0047] The support beam adopts a frame structure composed of spaced horizontal beams 11 and spaced vertical beams 12. The structure is simple and has good stability, and is easy to form and manufacture. By setting grooves on at least the longer vertical beams 12, the deformation of the frame body 10 can be significantly reduced.
[0048] The multiple slots 131 on the upper surface of the supporting beam can be randomly distributed or regularly distributed. In one embodiment, there is at least one slot unit 13 along the length direction of the frame body 10, that is, the slot unit 13 is located on the longitudinal beam 12. Each slot unit 13 includes a plurality of slots 131 arranged side by side along the width direction of the frame body 10; in the same slot unit 13, each slot 131 is formed on spaced longitudinal beams 12, or on all longitudinal beams 12. Figure 3 As shown, for a slot unit 13, slots can be cut on all seven longitudinal beams 12 (i.e., through slots). These through slots (i.e., slots 131 on all longitudinal beams 12 that extend through the width of the frame body) can be machined in one go using a milling cutter or wire cutting, making processing more convenient and efficient. Alternatively, slots can be cut on alternate longitudinal beams 12 (i.e., intermittent slots), for example, slots can be cut on the 1st, 3rd, 5th, and 7th longitudinal beams 12, while slots can be left uncut on the 2nd, 4th, and 6th longitudinal beams 12. Since the number of slots 12 is less than with through slots, the impact on the mechanical strength of the frame body 10 is smaller. Both intermittent and through slots in the longitudinal beams 12 can reduce the deformation of the frame body.
[0049] In one embodiment, multiple slot units 13 are spaced apart along the length of the frame body 10, and each slot unit 13 is symmetrically arranged on both sides of the center line of the length direction of the frame body 10.
[0050] By setting multiple slot units 13 and arranging each slot unit 13 symmetrically, it can be ensured that the frame body 10 can expand and contract uniformly.
[0051] In one embodiment, a slot unit 13 is formed on the centerline of the length direction of the frame body 10. When there is only one slot unit 13, the slot unit 13 can be formed on the centerline of the length direction of the frame body 10. When there are multiple slot units 13, such as Figure 3 In the illustrated embodiment, there are a total of 5 slot units 13. One slot unit 13 is located on the center line of the length direction of the frame body 10, and the other 4 slot units 13 are symmetrically arranged on both sides of the center line of the length direction of the frame body 10. By opening a slot unit 13 on the center line of the length direction of the frame body 10, it can be ensured that the two sides of the frame body 10 can expand and contract uniformly in the length direction.
[0052] In one embodiment, at least three slot units 13 are provided on the frame body 10 along its length, wherein the spacing between adjacent slot units 13 may be equal or unequal. Figure 3In the illustrated embodiment, there are five slot units 13, designated from left to right as slot unit 1, slot unit 2, slot unit 3, slot unit 4, and slot unit 5. The spacing between adjacent slot units 13 is not entirely equal. Specifically, the spacing between slot unit 1 and slot unit 2 is greater than the spacing between slot unit 2 and slot unit 3; the spacing between slot unit 2 and slot unit 3 is equal to the spacing between slot unit 3 and slot unit 4; and the spacing between slot unit 1 and slot unit 2 is equal to the spacing between slot unit 4 and slot unit 5. Of course, in other embodiments, the spacing between adjacent slot units 13 can be completely equal or varied.
[0053] At least three slot units 13 are provided, and the spacing between the slot units 13 can be equal or unequal, which can be flexibly selected according to the actual situation.
[0054] In one embodiment, at least two slot units 13 are provided on the frame body 10 along the length direction of the frame body 10, and the depth of the slot 131 increases as the distance between two adjacent slot units 13 increases.
[0055] When the spacing of the slot units 13 is equal, the depth of each slot 131 is equal, and the greater the spacing, the greater the depth of the slot 131.
[0056] When the spacing of the slot elements 13 is not equal, the depth of each slot 131 is not equal. The two slot elements 13 with smaller spacing have shallower slots, and the slot elements 13 with larger spacing have deeper slots. For example Figure 3 In the middle, the groove depth in groove unit 1 and groove unit 5 is greater than that in groove unit 2, groove unit 3 and groove unit 4.
[0057] Setting the depth of the groove 131 to increase with the increase of the spacing between the groove units 13 can ensure that the frame body 10 maintains a suitable amount of expansion and contraction when heated and cooled, thereby reducing the amount of plastic deformation of the frame body 10.
[0058] In one embodiment, the groove 131 is also formed on the upper surface of at least one crossbeam 11, and the groove 131 extends through the width of the crossbeam 11.
[0059] By opening a through groove 131 on the upper surface of the crossbeam 11, the free expansion and contraction performance of the upper surface of the frame body 10 can be further improved, and the amount of plastic deformation of the frame body 10 can be reduced.
[0060] In one embodiment, the groove 131 is a U-shaped groove, a V-shaped groove, a rectangular groove, or an arc-shaped groove with an arc-shaped bottom. When a U-shaped groove or an arc-shaped groove with an arc-shaped bottom is used, there are no sharp corners, which can avoid stress concentration.
[0061] The cross-sectional shape of the groove 131 can be set in multiple ways, which can be selected according to the actual situation, increasing the flexibility of selection.
[0062] In one embodiment, the depth of the groove 131 is less than or equal to one-third of the thickness of the supporting beam, for example, the thickness of the supporting beam can be 10mm, 11mm, 12mm, etc., and the depths of the various grooves 131 may be the same or different; and / or, the upper width of the groove 131 is 0.3mm-0.7mm, for example, 0.3mm, 0.4mm, 0.5mm, 0.6mm, 0.7mm, etc. For V-grooves, the upper width of the groove 131 refers to the width of the widest part of the groove 131. The depths of the various grooves 131 can be the same or different. Generally, when the groove spacing is small, the grooves are shallower, and when the groove spacing is large, the grooves are deeper.
[0063] By limiting the depth of the groove 131 and its upper width to specific parameters, the strength of the frame body 10 can meet the usage requirements while ensuring that the plastic deformation of the frame body 10 is small.
[0064] In one embodiment, the frame body 10 is made of aluminum alloy casting, such as ADC12 aluminum alloy casting, or aluminum alloy profile, such as 2A12 aluminum alloy profile. This grooving method of the present application is also suitable for other materials of the pressure welding strip tooling 1 that are prone to deformation during the welding cycle.
[0065] The frame body 10 is made of aluminum alloy, which has a lower overall cost.
[0066] In one embodiment, the support beam is also provided with a plurality of pressure needle mounting holes 14 extending along the thickness direction of the support beam. The pressure needle mounting holes 14 are offset from the groove 131. Each pressure needle 20 is elastically mounted in a pressure needle mounting hole 14 by a spring 21, so that the pressure needle 20 can extend and retract relative to the support beam, and the lower end of the pressure needle 20 extends downward through the support beam.
[0067] The mounting hole 14 of the pressure needle is staggered from the groove 131, so that the free expansion and contraction of the frame body 10 are independent of the pressure needle 20, thus avoiding affecting the pressing effect of the pressure needle 20 on the welding strip.
[0068] This application also provides a method for preparing a pressure welding strip tooling, the method comprising:
[0069] Grooves are machined on the upper surface of the supporting beams of the frame body;
[0070] The groove is machined using a forming milling cutter or wire EDM.
[0071] Grooves are machined on the upper surface of the support beams of the frame body by forming milling cutter or wire cutting. Under reciprocating thermal cycling conditions, the shallow layer of the upper surface of the frame body can expand and contract freely, which can reduce the residual stress of the pressure welding strip tooling and improve the working life of the pressure welding strip tooling under complex working conditions.
[0072] The following experiments were conducted using the same type of pressure welding strip tooling, specifically four slotted embodiments prepared by the method described in this application for preparing pressure welding strip tooling, and one unslotted comparative embodiment, to measure their respective flatness.
[0073] In this experiment, the welding strip tooling used in the four embodiments and comparative examples has a frame body with a supporting beam consisting of a symmetrical hollow structure composed of 7 longitudinal beams and 6 transverse beams, and the thickness of the supporting beam is 11mm.
[0074] The table below shows the specific parameters for four embodiments and one comparative example.
[0075]
[0076] All embodiments use U-shaped grooves with an upper width of 0.5 mm.
[0077] The test item for the experiment was flatness. The test method was to perform welding cycles on the above five types of pressure welding strip tooling on the string welding machine, and measure after several welding cycles.
[0078] Before the experiment, the welding strips were evenly applied to nine different positions on each welding fixture (e.g., ...). Figure 6 The flatness of each welding strip fixture (numbered 1-9) is measured. Then, each welding strip fixture is put into actual installation test (except for those without battery cells). After each cycle (about 4000 thermal cycles), the flatness of the welding strip fixture is tested again. This process is repeated for multiple cycles to verify the deformation law of the welding strip fixture under working conditions.
[0079] During the experiment, due to potential deformation of the welding strip tooling itself after each experimental cycle, and the difficulty in ensuring consistency in the initial state of the welding strip tooling during each measurement with a 3D coordinate measuring machine, the data analysis of the experimental items in this experiment was conducted using a method that... Figure 6 The plane containing points 1, 3, and 8 is the reference plane (e.g., Figure 7 As shown), the data measured at each other point are mapped to the vertical distance from that point to the reference plane (e.g., ...). Figure 8 As shown, Figure 8 In this context, 'n' represents all points except 1, 3, and 8. Although this method introduces errors, these errors can be temporarily ignored because the deformation of the curved surface is very small compared to the dimensions of the tooling itself.
[0080] The ungrooved pressure welding strip fixture (Series B) was subjected to welding cycles on a string welding machine. The flatness of the pressure welding strip fixture was tested during each cycle. Figure 10 , Figure 11 The experimental data shown are those of the comparative example after 5 welding cycles (i.e., 20,000 welding cycles). Figure 10 This is a 3D image obtained using Minitab software. In the image, X represents the position of the measurement point on the measured plane along the X-axis, and Y represents the position of the measurement point on the measured plane along the Y-axis. X and Y define the specific positions on the plane. 0, 100, and 200 on the X-axis and 0, -25, -50, and -75 on the Y-axis are quantization units, meaning the entire plane of the welding strip fixture is divided into 100×100 cells. Z1 is the deviation value relative to the reference plane, in mm. To clearly show the changes in the Z1 axis... Figure 11 It is Figure 10 The point distribution map is exported in two-dimensional form. Five B-series welding strip fixtures were used in the experiment. Six points (2, 4, 5, 6, 7, and 9) were collected from each fixture, with each point representing one sample data point. Measurements were taken once every 4000 cycles, for a total of five measurements at 20000 cycles, with 30 samples collected each time, for a total of 150 samples. Flatness was measured using a Zeiss coordinate measuring machine, and data in the X, Y, and Z directions were collected for each point. Based on a reference plane established using the least squares method, the tolerance values of the B-series samples were processed using Minitab at a 90% confidence level. The upper bound of the confidence interval for the upper deviation was +0.030 mm, and the lower bound of the confidence interval for the lower deviation was -0.045 mm.
[0081] After nearly 20,000 loading cycles, the overall longitudinal bending deformation of the B series gradually increased, and after approximately 10,000 cycles, the longitudinal bending deformation tended to stabilize (the same was true for the transverse deformation). Figure 10 As shown, after nearly 20,000 thermal cycles, the B series exhibits significant longitudinal bending deformation. Figure 11 As shown, out of 150 sample data, 38 samples exceeded the boundary of the statistical model (i.e., the points exceeding the lower limit in the figure). At this point, the confidence level is only 74.6%, and the original planar hypothesis no longer holds. Looking at the deformation trend of the tooling after welding, the pressure welding strip tooling underwent concave deformation, indicating that the upper surface of the pressure welding strip tooling underwent localized compressive plastic deformation during the welding process. In other words, the ungrooved tooling has undergone severe deformation after 20,000 welding cycles and is no longer usable.
[0082] The slotted welding strip fixtures of Examples 1-4 (G1-G4) were subjected to welding cycles on a string welding machine. The flatness of the welding strip fixtures was tested in each cycle. Figure 9 The figure shows the distribution of flatness changes of the pressure welding strip tooling after 100,000 welding cycles in Examples 1-4 (G1-G4). The meanings of X, Y, and Z1 in the figure are the same as those explained in the B series above, and will not be explained again here.
[0083] The flatness of the upper surface of the welding strip fixture was tested using a Zeiss coordinate measuring machine. Based on a reference plane established by the least squares method, confidence intervals for the deviation values of Examples 1-4 were constructed with a 90% confidence level using Minitab software. The upper bound of the confidence interval for the upper deviation was +0.100 mm, and the lower bound of the confidence interval for the lower deviation was -0.090 mm. During the experiment, for each of the four welding strip fixtures in Examples 1-4, six points (2, 4, 5, 6, 7, and 9) were collected, with each point representing one sample data point, resulting in 24 sample data points each time. Figure 9 As shown, after 100,000 welding cycles, a total of 25 samples were collected, totaling 600 sample data. Among them, the total number of samples exceeding the statistical model boundary was 53 (i.e., the points exceeding the lower line in the figure). At this point, the confidence level was 91.0%. In summary, the flatness of the pressure welding strip tooling with the slotted structure meets the expectations, that is, the pressure welding strip tooling is basically unchanged after the 100,000 welding cycle experiment.
[0084] Compared with the pressure welding strip tooling of the above-mentioned comparative example, the pressure welding strip tooling with the slotted structure of this application can still perform well after 100,000 welding cycles. The slotted structure can reduce the residual stress along the thickness direction caused by temperature changes, thereby reducing the amount of plastic deformation on the shallow surface of the pressure welding strip tooling body and significantly improving the service life of the pressure welding strip tooling.
[0085] The foregoing has provided a sufficiently detailed and specific description of this application. Those skilled in the art should understand that the descriptions in the embodiments are merely exemplary, and all changes made without departing from the true spirit and scope of this application should fall within the protection scope of this application. The scope of protection claimed in this application is defined by the claims, and not by the above descriptions in the embodiments.
Claims
1. A tooling for pressure welding strips, characterized in that, The welding strip fixture includes a frame body and pressure pins for welding strips. The frame body is a hollow frame structure composed of several support beams. At least some of the pressure pins are arranged in an array and elastically mounted on the support beams. Several grooves are spaced apart on the upper surface of the support beams, and the grooves extend through the width direction of the support beam.
2. The pressure welding strip tooling according to claim 1, characterized in that, The support beam includes a plurality of horizontal beams spaced apart along the length of the frame body and a plurality of longitudinal beams spaced apart along the width of the frame body; wherein: the groove is at least formed on the longitudinal beam, and the groove extends through the width of the longitudinal beam in which it is located.
3. The pressure welding strip tooling according to claim 2, characterized in that, The frame body has at least one slot unit along the length direction of the frame body, and each slot unit includes a plurality of slots arranged side by side along the width direction of the frame body; In the same slot unit, each slot is formed on the longitudinal beams that are spaced apart, or on all the longitudinal beams.
4. The pressure welding strip tooling according to claim 3, characterized in that, The slot units are spaced apart along the length of the frame body, and each slot unit is symmetrically arranged on both sides of the center line of the length direction of the frame body.
5. The pressure welding strip tooling according to claim 3, characterized in that, One of the slot units is formed on the center line of the length direction of the frame body.
6. The pressure welding strip tooling according to claim 3, characterized in that, At least three slot units are provided on the frame body along the length direction of the frame body, wherein the spacing between two adjacent slot units is equal or unequal.
7. The pressure welding strip tooling according to claim 3, characterized in that, At least two slot units are provided on the frame body along the length direction of the frame body, and the depth of the slot increases as the distance between two adjacent slot units increases.
8. The pressure welding strip tooling according to claim 2, characterized in that, The groove is also formed on the upper surface of at least one of the crossbeams, and the groove extends through the width of the crossbeam.
9. The pressure welding strip tooling according to any one of claims 1-8, characterized in that, The groove is a U-shaped groove, a V-shaped groove, a rectangular groove, or an arc-shaped groove with an arc bottom.
10. The pressure welding strip tooling according to any one of claims 1-8, characterized in that, The depth of the groove is less than or equal to one-third of the thickness of the supporting beam in which it is located, and the depths of the various grooves may be the same or different; and / or, The upper width of the groove is 0.3mm-0.7mm.
11. The pressure welding strip tooling according to any one of claims 1-8, characterized in that, The frame body is made of aluminum alloy castings or aluminum alloy profiles.
12. The pressure welding strip tooling according to any one of claims 1-8, characterized in that, The support beam is also provided with a plurality of pressure pin mounting holes that extend along the thickness direction of the support beam. The pressure pin mounting holes are offset from the groove. Each pressure pin is elastically mounted in a pressure pin mounting hole by a spring, so that the pressure pin can extend and retract relative to the support beam. The lower end of the pressure pin extends downward through the support beam.