Impact tool

By using carburizing and high-frequency induction hardening processes to form a multi-layer hardened layer on the anvil, combined with the design of a small motor and transmission components, the problems of large weight and length of high-torque wrenches are solved, enabling efficient completion of high-torque fastening tasks and improving the user experience.

CN224993328UActive Publication Date: 2026-11-20JIANGSU DONGCHENG TOOLS TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202522185946.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Priority Date
2025-09-30
Filing Date
2025-10-16
Publication Date
2026-11-20
Estimated Expiration
2035-10-16

AI Technical Summary

Technical Problem

Existing high-torque wrenches are heavy and long, resulting in a poor user experience.

Method used

The anvil is treated with carburizing and high-frequency induction hardening processes to form multiple hardened layers to improve its hardness and toughness. Combined with a smaller motor and transmission component design, it can achieve high-torque fastening tasks.

Benefits of technology

It enables high-torque fastening tasks to be completed with a smaller head size, improving the user experience and the durability of the anvil.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224993328U_ABST
    Figure CN224993328U_ABST
Patent Text Reader

Abstract

The application relates to an impact tool, comprising a housing, a motor, an anvil, an impact assembly, a transmission assembly; wherein the anvil comprises an impact receiving part for receiving an impact force applied by the impact assembly, a head part for receiving a working head, the head part has a minimum cross-sectional width of at least 3 / 4 inch in a plane perpendicular to the length extension direction of the anvil, at least one of the impact receiving part and the head part is formed with a hardened layer after a structural strengthening treatment process, and the hardness value of the hardened layer ranges from HV585 to HV760. The impact tool of the application forms the hardened layer with a hardness value ranging from HV585 to HV760 after a carburizing and quenching process or a carbonitriding and quenching process and a high-frequency induction quenching process, and when the impact tool is applied, a relatively small head size can be adopted to complete a high-torque fastening task beyond the capability of a typical battery-powered impact tool.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field] This application relates to the field of construction equipment technology, and in particular to an impact tool. [Background Technology] Current high-torque wrenches, capable of achieving 2400Nm-3000Nm output torque, typically employ a striking block with an outer diameter of 90mm-95mm, a wrench head with a nominal width of at least 1 inch, and a brushless motor with a diameter of at least 50mm. The striking frequency is at least 1500 strikes per minute. However, high-torque wrenches using this technology offer a poor user experience due to their weight and overall length, making them inconvenient to use.

[0003] Therefore, it is indeed necessary to provide an improved impact tool to overcome the shortcomings of the prior art. [Utility Model Content] To address the shortcomings of existing technologies, the purpose of this application is to provide an impact tool that uses an anvil that has undergone a structurally reinforced process, thereby enabling the use of a relatively small head size to perform high-torque fastening tasks that exceed the capabilities of typical battery-powered impact tools.

[0005] The technical solution adopted by this application to solve the problem of the prior art is: an impact tool, comprising: case; An electric motor, which is housed in the housing, and the outer diameter of the electric motor is at least greater than or equal to 50 mm; An anvil, which is rotatably supported on the housing and protrudes from the front end of the housing; An impact assembly housed in the housing, the impact assembly being capable of applying a circumferential rotational impact force to the anvil, and the impact frequency of the impact force applied by the impact assembly to the anvil being at least 1700 ipm; A transmission assembly, housed in the housing, is connected to the motor and the impact assembly respectively to transmit power from the motor to the impact assembly and generate an operating torque of at least 2400 Nm in the anvil. The anvil includes an impact receiving portion for receiving the impact force applied by the impact assembly and a head for engaging the tool tip, the head having a minimum cross-sectional width of at least 3 / 4 inch in a plane perpendicular to the length extension direction of the anvil.

[0006] A further improvement is that at least one of the impact receiving part and the head of the anvil is formed with a hardened layer after surface treatment.

[0007] A further improvement is as follows: the hardened layer comprises, from the outside to the inside, a first structural layer with a first hardness and a second structural layer with a second hardness; The anvil is formed with a first structural layer after carburizing and quenching or carbonitriding and quenching. The anvil with the first structural layer is further formed with a second structural layer and a third structural layer after a second process. The third structural layer has a third hardness. The hardness values ​​of the first hardness, the second hardness, and the third hardness decrease sequentially.

[0008] A further improvement is as follows: the hardness range of the first structural layer is HV655-HV760, the hardness range of the second structural layer is HV585-HV710, and the hardness range of the third structural layer is HV360-HV560.

[0009] A further improvement is that the diameter of the motor is at least 60mm.

[0010] A further improvement is that the impact frequency at which the impact component applies impact force to the anvil is at least 1800 ipm.

[0011] A further improvement is that the anvil generates a working torque of at least 2500 Nm.

[0012] A further improvement is that the maximum diameter of the shell is less than 110 mm.

[0013] A further improvement is that the weight of the striking block is at least 1500g.

[0014] A further improvement is that the head includes multiple driving surfaces for engaging with the tool tip.

[0015] Another technical solution of this application is: an impact tool, comprising: case; An electric motor, which is housed in the housing, and the outer diameter of the electric motor is at least greater than or equal to 50 mm; An anvil, which is rotatably supported on the housing and protrudes from the front end of the housing; An impact assembly housed in the housing, the impact assembly including a striking block that applies a circumferential rotational impact force to the anvil, the striking block having an outer diameter of at least 100 mm, and the impact frequency at which the impact assembly applies the impact force to the anvil being at least 1700 ipm. A transmission assembly, housed in the housing, is connected to the motor and the impact assembly respectively to transmit power from the motor to the impact assembly and generate an operating torque of at least 2400 Nm in the anvil. The anvil includes an impact receiving portion for receiving the impact force applied by the impact assembly and a head for engaging the tool tip, the head having a minimum cross-sectional width of at least 3 / 4 inch in a plane perpendicular to the length extension direction of the anvil.

[0016] A further improvement is as follows: at least one of the impact receiving part and the head has a first structural layer, a second structural layer, and a third structural layer from the outside to the inside. The anvil is formed with a first structural layer after carburizing and quenching or carbonitriding and quenching. The first structural layer has a first hardness. The anvil with the first structural layer is formed with a second structural layer and a third structural layer after a second process. The second structural layer has a second hardness, and the third structural layer has a third hardness. The hardness values ​​of the first hardness, the second hardness, and the third hardness decrease sequentially.

[0017] A further improvement is as follows: the first structural layer is composed of mixed martensite and retained austenite, the second structural layer is composed of lath martensite and bainite, and the third structural layer is composed of troostite.

[0018] A further improvement is that the diameter of the motor is at least 50mm.

[0019] Compared with the prior art, this application has the following beneficial effects: The impact tool in this application has an anvil that has been hardened to a hardness range of HV585-HV760 after being subjected to carburizing or carbonitriding hardening or high-frequency induction hardening. When applied to the impact tool, it is possible to perform high-torque fastening tasks that exceed the capabilities of typical battery-powered impact tools with a relatively small head size. [Image Description] The specific embodiments of this application will be described in further detail below with reference to the accompanying drawings: Figure 1 This is a three-dimensional schematic diagram of the impact tool of this application; Figure 2 yes Figure 1 A cross-sectional schematic diagram of the impact tool shown; Figure 3 yes Figure 1 A side view of the impact tool shown; Figure 4 yes Figure 1 An exploded schematic diagram of the power mechanism of the impact tool shown in the figure; Figure 5 yes Figure 1 A three-dimensional schematic diagram of the impact tool anvil shown in the figure; Figure 6 yes Figure 1 A cross-sectional view of an embodiment of the impact tool anvil shown in the figure; Figure 7 yes Figure 6 A cross-sectional view of the impact receiving section in the embodiment of the impact tool anvil shown; Figure 8 yes Figure 1 A cross-sectional view of another embodiment of the impact tool anvil shown; Figure 9 yes Figure 8 A cross-sectional view of the impact receiving section in the embodiment of the impact tool anvil shown; Figure 10 yes Figure 1 A cross-sectional view of another embodiment of the impact tool anvil shown; Figure 11 yes Figure 10 A cross-sectional view of the impact receiving section in the embodiment of the impact tool anvil shown; Figure 12 yes Figure 1 The manufacturing process flow diagram of the impact tool anvil shown in the figure; Figure 13 yes Figure 1 The overall process diagram of the impact tool anvil shown in the figure; Figure 14 yes Figure 1 The diagram shows the carburizing process of the impact tool anvil. Figure 15 yes Figure 1 The high-frequency induction process diagram of the impact tool anvil shown in the figure; Figure 16 yes Figure 1 The diagram shows the post-processing steps of the impact tool anvil.

[0021] Meaning of the reference numerals in the diagram: 100. Impact tools; 10. Housing; 11. Handle housing; 111. Grip; 12. Motor housing; 13. Gearbox housing; 14. Output housing; 20. Motor; 21. Stator; 22. Rotor; 30. Anvil; 30a. First structural layer; 30b. Second structural layer; 30c. Third structural layer; 30e. Fourth structural layer; 31. Handle; 311. First end; 312. Second end; 313. Driving surface; 32. Impact receiving part. 40. Impact assembly; 41. Impact block; 411. Impact protrusion; 42. Steel ball; 43. Elastic element; 44. Intermediate shaft. 50. Transmission assembly; 51. Sun gear; 52. Internal gear ring; 53. Planetary gear; 54. Planet carrier; 60. Battery pack. [Detailed Implementation] To make the technical solution and beneficial effects of this application more apparent and understandable, a detailed description is provided below by listing specific embodiments. Unless otherwise defined, the technical and scientific terms used herein have the same meanings as those in the technical field to which this application pertains.

[0023] The terminology used in this application is for the purpose of describing specific embodiments only and is not intended to limit the application. For example, terms such as "upper," "lower," "front," and "rear" that indicate orientation or positional relationship are based solely on the orientation or positional relationship shown in the accompanying drawings and are used only for the convenience of describing the application and simplifying the description, and are not intended to indicate or imply that the device referred to must have a specific orientation or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the application.

[0024] See Figures 1-2 As shown, the impact tool 100 disclosed in this application can be specifically implemented as an electric wrench, which may include a housing 10 forming its outer contour, a motor 20 housed within the housing 10 to provide a power source, an anvil 30 rotatably supported on the housing 10 and protruding from one end of the housing 10, a power mechanism housed inside the housing 10, and a battery pack 60 for providing electrical energy to the motor 20. The power mechanism may include an impact assembly 40 composed of a striking block and an elastic element, and a transmission assembly 50 composed of a gear train. Alternatively, the power mechanism may be other types of transmission components for transmitting power from the motor 20 to the anvil 30. The battery pack 60 can provide DC power to the motor 20, but it can also be replaced with AC power.

[0025] To facilitate a clear explanation of the specific content of the technical solution of this application, the following definitions are made: the central axis of the anvil 30 and the direction parallel to it are defined as the axial direction; the radial direction of the circumference with the central axis of the anvil 30 as the central axis is defined as the radial direction; the output direction of the anvil 30 is defined as the front; and the direction opposite to the output direction of the anvil 30 is defined as the rear.

[0026] See Figure 1 , Figure 2The housing 10 may include a handle housing 11, a motor housing 12, a gearbox housing 13, and an output housing 14. The various parts of the housing 10 are arranged sequentially from back to front, forming a roughly straight line. The handle housing 11 has a grip portion 111 for the operator to hold; this grip portion 111 may be roughly D-shaped, or other shapes convenient for the operator to hold. The motor housing 12 houses the motor 20 that powers the impact tool 100; the motor 20 may be a brushless motor or a brushed motor. The gearbox housing 13 is connected to the front end of the motor housing 12 and houses a transmission assembly 50 to transmit the power of the motor 20 forward to the impact assembly 40. The output housing 13 houses the impact assembly 40 and the anvil 30, from which the motor 20 sequentially passes through the transmission assembly 50 and the impact assembly 40 to drive the anvil 30 for external operation. In some embodiments, the roughly straight housing 10 has a maximum diameter D1 of less than 110 mm.

[0027] See Figure 2 The motor 20, like a conventional internal rotor motor, includes a stator 21 circumferentially fixed to the inner wall of the motor housing 12 and a rotor 22 rotatably supported on the motor housing 12. When the motor 20 is energized, the rotor 22 rotates about its own central axis and transmits power forward to ultimately drive the anvil 30 to perform external operations. In some embodiments, the diameter D2 of the motor 20 is at least 50 mm, meaning the diameter of its stator 21 is at least 50 mm.

[0028] See Figure 2 , Figure 3 , Figure 4 The transmission assembly 50, like commonly used planetary gear systems, includes a planetary gear set driven by the motor 20. The planetary gear set includes a sun gear 51 connected to the rotor shaft of the motor 20, an internal gear ring 52 circumferentially fixed to the inner wall of the gearbox housing 13, planetary gears 53 meshing with both the sun gear 51 and the internal gear ring 52, and a planet carrier 54 for mounting the planetary gears 53. The power from the motor 20 is transmitted sequentially through the sun gear 51, the planetary gears 53, and finally through the planet carrier 54, enabling the anvil 30 to generate an operating torque of at least 2400 Nm. In some embodiments, the transmission assembly 50 transmits the power from the motor 20 to the anvil 30, enabling it to generate an operating torque of 2500 Nm.

[0029] See Figure 2 , Figure 3 , Figure 4The impact assembly 40 may include an impact block 41, a steel ball 42, an elastic element 43, and an intermediate shaft 44. One end of the elastic element 43 abuts against the impact block 41, and the other end abuts against the rear end of the intermediate shaft 44. The shaft of the intermediate shaft 44 is provided with two guide grooves, and the impact block 41 is also provided with guide grooves, in which the steel ball 42 is embedded. The rear end of the anvil 30 is provided with an impact receiving part 32, and the front end of the impact block 41 is provided with opposing impact protrusions 411. In the embodiments of this application, the weight of the impact block 41 is at least 1500g. The operating principle of the impact component 40 of the impact tool 100 is similar to that of a conventional impact wrench (such as the impact mechanism in Japanese Patent Application No. JP1982137905U). The power of the motor 20 is transmitted to the intermediate shaft 44 via the transmission component 50. The intermediate shaft 44 accumulates impact torque through the elastic element 43, and then applies a periodic impact torque with a circumferential impact frequency of at least 1700 ipm to the anvil 30 through the side wall between the impact protrusion 411 at the front end of the impact block 41 and the impact receiving part 32 at the rear end of the anvil 30. In some embodiments, the impact component 40 can also apply an impact force to the anvil 30 with an impact frequency of at least 1800 ipm.

[0030] See Figure 5 In the embodiments of this application, in order to improve the overall performance of the anvil 30, increase its structural strength, increase its structural toughness, improve its wear resistance, and extend its service life, the surface of the anvil 30 can be treated by carburizing process and high-frequency induction heating process, so that it can form a three-layer structure from the inside out.

[0031] like Figure 5 As shown, the cross-section of the anvil 30 is approximately T-shaped, and it includes a handle 31 extending in the front-back direction and an impact receiving portion 32 extending in a first direction, wherein the first direction is perpendicular to the length extension direction of the handle 31. In the embodiments of this application, the handle 31 extends in the axial direction and the impact receiving portion 32 extends in the radial direction.

[0032] like Figure 5As shown, the anvil 30 has a first end 311 at its front end and a second end 312 at its rear end, where the first end 311 is the head, which has multiple drive surfaces 313 for engaging the working head. In some embodiments, the head of the anvil 30 may have four drive surfaces 313 connected end to end, which can form a generally square head for engaging the working head. The nominal width H1 of the head formed by the four drive surfaces 313 can be 3 / 4 inch. The working head may be specifically implemented as a sleeve, drill bit, etc., and has a mounting hole that matches the outline of the head. The head of the anvil 30 is inserted into the mounting hole and detachably connected as one unit. The anvil 30 transmits periodic rotational impacts to the workpiece to be processed through the working head.

[0033] like Figure 5 As shown, in some embodiments, the second end 312 of the anvil 30 may have two impact receiving portions 32 extending in opposite radial directions, which are used to receive the periodic impact torque applied by the striking block 41. The striking block 41 can rotate circumferentially and move axially back and forth under the drive of the impact mechanism 50, and the front end face of the striking block 41 is formed with an impact protrusion 411 for engaging with the aforementioned impact receiving portion 32. When the striking block 41 moves to near the front limit position, the side wall of the impact protrusion 411 abuts against the side wall of the impact receiving portion 32. At this time, the impact protrusion 411 will apply a circumferential impact force to the impact receiving portion 32. This circumferential impact force will pass sequentially through the impact receiving portion 32, the handle 31, the driving surface 313, and the sleeve, and finally be transmitted to the workpiece to be processed to complete the operation. During this process, the sidewall of the impact receiving part 32 of the anvil 30 and the driving surface 313 of the anvil 30 will be subjected to a large impact torque. These two parts of the anvil 30 are also very prone to breakage and failure, which cannot meet the usage requirements of medium and high torque impact wrenches. To address this, the driving surface 313 and the impact receiving part 32 of the anvil 30 can be surface hardened to form at least two structural layers with greater hardness. The anvil 30 retains its internal toughness while its surface hardness is increased, thereby improving the durability and fatigue life of the anvil 30. The depth of the aforementioned at least two structural layers can be determined by the process parameters of the surface hardening treatment. By controlling and adjusting the depth of each structural layer, the optimal structural strength and service life of the anvil 30 can be obtained.

[0034] In some embodiments, medium carbon steel can be used as the material for the anvil 30, and the structural properties of the material can be adjusted by changing the carbon content. Of course, in other embodiments, nickel-chromium-molybdenum steel can also be used as the material for the anvil 30, for example, the material of the anvil 30 can be 30CrNi3Mo, 35CrNi3Mo, 30CrNi4Mo, 35Cr2Ni4Mo, 35Cr2Ni3Mo, 35Cr2Ni2Mo, or 35CrNi3Mo.

[0035] like Figure 5 As shown, in this application, to improve the structural strength, increase its structural toughness, improve its wear resistance, and extend its service life of the anvil 30, a structural strengthening process can be applied to the driving surface 313 and the impact receiving part 32 of the anvil 30. In this application, the anvil 30 can be produced using 35Cr2Ni4Mo as raw material. During the production process, the anvil 30 needs to undergo a pre-treatment process to obtain its external structure. This pre-treatment process includes the following steps: Blanking is a process in which the 35Cr2Ni4Mo sheet material is cut or punched to produce a blank with a general shape of an anvil. Hot forging is a process used to perform preliminary forging and plastic deformation on the blanks formed by the above cutting, thereby improving the density and physical and mechanical properties of the blanks. Heat treatment is a process that involves normalizing, tempering, and annealing the hot-forged billet to refine the grains, homogenize the microstructure, eliminate the internal stress generated during the blanking and hot forging processes, improve the machinability of the billet, and prevent the billet from deforming during subsequent processing. Machining is a process in which the blank is mechanically processed to form the shape and outline of the anvil. This includes, but is not limited to, turning, drilling, grinding, etc., until the blank is processed into the final shape and outline of the anvil.

[0036] After the aforementioned pre-processing steps, the anvil blank, which has the final shape and outline of the anvil, needs to be heat-treated. This heat treatment alters the internal microstructure without changing the shape or overall chemical composition of the anvil blank, thereby improving its internal quality and performance. When heat-treating the anvil blank, the specific heat treatment process should be selected based on its actual application scenario. For example, the Chinese patent application CN202080031527.9 uses a high-frequency induction hardening process on the punch lugs and head of the anvil, making the external hardness of these two parts greater than the internal hardness, thus enhancing the durability and wear resistance of the anvil. However, this single high-frequency induction hardening heat treatment method has several drawbacks. First, it only achieves surface martensitic phase transformation through rapid heating and cooling, and the depth of the hardened layer is limited by the high-frequency penetration. Second, it is highly material-dependent and only applicable to medium and high carbon steel materials, and cannot significantly improve the surface hardness of low carbon steel. In addition, it lacks a carbon concentration gradient, and the carbon content of the surface layer is consistent with that of the matrix, which has limited effect on improving the wear resistance of the material.

[0037] In this application, to ensure that the anvil 30 meets the requirements for use with a high-torque wrench, the following heat treatment process is adopted: Carburizing and quenching is a process in which the impact receiving part 32 and the driving surface 313 of the anvil 30, which have undergone the aforementioned pre-treatment process, are infiltrated with carbon atoms in a specific environment. This improves the hardness, wear resistance, and fatigue strength of the impact receiving part 32 and the driving surface 313, while maintaining the toughness of the anvil core. Specifically, carburizing and quenching involves placing the impact receiving part 32 and the driving surface 313 of the anvil 30 in an activated carbon medium, heating it to 900℃-950℃, the temperature at which the raw steel undergoes single-phase austenitization, and holding it at this temperature for a sufficiently long time. This allows the activated carbon atoms decomposed from the carburizing medium to penetrate into the impact receiving part 32 and the driving surface. The surface layer of surface 313 is high carbon, so that the impact receiving part 32 and the driving surface 313 of the anvil are high carbon while the core of the anvil 30 retains its original composition. A surface strengthening layer, namely the first structural layer 30a, is formed on the impact receiving part 32 and the driving surface 313. It has a first hardness (its hardness range can be HV655-HV730). The microstructure of the first structural layer 30a is a combination of mixed martensite and retained austenite. The mixed martensite provides high hardness and wear resistance, while the retained austenite can improve toughness and reduce the risk of quenching cracks. Furthermore, the retained austenite may induce stress-induced mixed martensitic phase transformation under alternating loads, further strengthening the material. High-frequency induction hardening is a process that further induction hardens the impact receiving part 32 and the driving surface 313 of the anvil 30 after carburizing and quenching. Through induction hardening, another surface strengthening layer, namely the second structural layer 30b, is formed between the first structural layer 30a and the core of the anvil 30. It has a second hardness (its hardness range can be HV585-HV710). The microstructure of the second structural layer 30b is a combination of lath martensite and bainite. The lath martensite is mainly strengthened by dislocations, and its comprehensive performance is balanced. The bainite is strengthened by fine grains and carbide dispersion, and its performance is more adjustable. At the same time, the core of the anvil 30 serves as the third structural layer 30c, which has a third hardness (its hardness range can be HV330-HV530). The microstructure of the third structural layer 30c is troostite, which has both high strength and high toughness. The core has excellent comprehensive performance of strength and toughness.

[0038] The heat treatment process of first carburizing and quenching followed by composite high-frequency induction hardening used in the embodiments of this application can significantly improve the overall performance of the anvil 30 compared to the above-mentioned single high-frequency hardening process. Its implementation principle can include the following aspects: (1) First, the carbon concentration gradient formed on the surface of the anvil 30 after the carburizing and quenching process has a synergistic optimization effect with the hardened layer depth of the high-frequency induction quenching process: In the carburizing stage, the anvil 30 is in a carbon-rich environment, and carbon atoms diffuse to 0.3mm-2.5mm below the surface of the anvil 30, forming a high carbon concentration gradient (the carbon content on the surface of the anvil can be increased to 0.45%-0.75%), which can provide sufficient carbon source for the subsequent high-frequency induction quenching process; In the high-frequency quenching process stage, the high-frequency current rapidly heats the surface of the anvil 30 to a depth of 1.2mm-2.2mm to the preset temperature and quenches it, and the high solubility of carbon atoms in austenite promotes the formation of martensite; The depth between the carburized layer and the high-frequency induction quenching layer is matched, avoiding the problem of the hardened layer being too shallow and the carbon distribution being uneven caused by the above-mentioned single high-frequency quenching process.

[0039] (2) Secondly, the carburized layer formed by the carburizing and quenching process and the hardened layer formed by the high-frequency induction hardening process have a synergistic strengthening effect in terms of microstructure: the microstructure of the carburized layer formed on the surface of the anvil 30 is a combination of mixed martensite and retained austenite, which can improve the surface hardness and wear resistance of the anvil 30; the hardened layer formed by the high-frequency induction hardening process is located inside the carburized layer, and its microstructure is a combination of lath martensite and bainite, which can improve the fatigue strength of the anvil 30; the temperature gradient between the two processes during the carburizing and quenching process and the high-frequency induction hardening process can keep the core of the anvil 30 tough, so that the anvil 30 can form a structure with a hard outer surface and a tough inner core, which can improve the impact resistance of the anvil 30.

[0040] (3) Furthermore, the carburizing and quenching process and the high-frequency induction hardening process have a synergistic optimization effect on deformation control: the high-frequency induction hardening process locally heats the impact receiving part 32 and the driving surface 313 of the anvil 30, which can reduce the heat-affected zone of the anvil 30. Combined with the low-temperature tempering after the carburizing and quenching process, the deformation of the anvil 30 caused by heat can be controlled to the minimum.

[0041] The heat treatment process of first carburizing and quenching followed by composite high-frequency induction hardening adopted in the embodiments of this application is more necessary for the rationality of the entire heat treatment process of the anvil 30 compared with the above-mentioned single high-frequency induction hardening process. This necessity is mainly reflected in the following aspects: (1) First, the composite heat treatment process of carburizing and quenching followed by high frequency induction hardening can avoid the hardness fluctuation of the anvil 30: after the anvil 30 is first subjected to carburizing and quenching, the carbon content on its surface can be increased to 0.45%-0.75%, forming a high carbon gradient layer. The subsequent high frequency induction hardening and rapid cooling can refine the martensite grains. This process can avoid the hardness fluctuation of the anvil 30 caused by uneven carbon distribution in the single high frequency induction hardening process.

[0042] (2) Secondly, the composite heat treatment process of first carburizing and quenching and then high frequency induction hardening can further strengthen the microstructure of the carburized layer of the anvil 30: the single high frequency induction hardening process can only obtain coarse martensite structure, while the composite heat treatment process of first carburizing and quenching and then high frequency induction hardening can make the carburized layer form a composite structure of mixed martensite and retained austenite after the high frequency induction hardening process, the latter having a higher hardness than the former.

[0043] (3) Furthermore, the composite heat treatment process of first carburizing and quenching and then high frequency induction hardening can balance the surface hardness and core toughness of the anvil 30: the single high frequency induction hardening process will cause the core of the anvil 30 to not be completely austenitized due to rapid heating, while the composite heat treatment process of first carburizing and quenching and then high frequency induction hardening can pre-set the carbon source by carburizing, thereby ensuring the toughness of the core during quenching, so that the surface hardness and core toughness of the anvil 30 can reach a certain balance, and improve the tensile strength of the anvil 30.

[0044] The composite heat treatment process of carburizing and quenching followed by high-frequency induction hardening used in the embodiments of this application has lower requirements for the adaptability of the raw materials and shape contour of the anvil 30 compared with the single high-frequency induction hardening process mentioned above. This is reflected in the following aspects: (1) First, the single high-frequency induction hardening process is more suitable for surface hardening of medium carbon steel materials. When quenching low carbon steel materials, there will be a defect of insufficient hardening due to lack of carbon source. The composite heat treatment process of carburizing and quenching followed by high-frequency induction hardening can be applied to both low carbon steel materials and medium carbon steel materials. This composite heat treatment process has higher adaptability to raw materials.

[0045] (2) Secondly, for a single high-frequency induction hardening process, it is more suitable for heat treatment of parts with relatively simple external structure; while for a composite heat treatment process of first carburizing and then high-frequency induction hardening, it can be used to locally strengthen the parts by first carburizing and then high-frequency induction hardening. It is suitable for parts with relatively simple external structure as well as irregular parts with complex external structure.

[0046] The composite heat treatment process of carburizing and quenching followed by high-frequency induction hardening used in the embodiments of this application can complement the single high-frequency induction hardening process described above, thereby improving the overall performance of the anvil 30. Specifically, this is reflected in the following aspects: (1) First, after the anvil 30 is subjected to carburizing and quenching process, the carbon content of its surface layer is increased. The higher carbon content can improve the heating efficiency of the subsequent high frequency induction quenching process. That is, the steel material with higher carbon content has higher resistivity and can generate more significant eddy current effect. When the anvil 30 is subjected to high frequency induction heating, the temperature rises faster. Furthermore, the carburized layer formed after the anvil 30 is subjected to carburizing and quenching process has a gentle gradient of carbon concentration. When the anvil 30 is subjected to high frequency induction quenching, it can effectively avoid local overheating of the anvil 30, thereby making the hardened layer formed by the high frequency induction quenching process transition more uniformly.

[0047] (2) Secondly, after the carburizing and quenching process, the anvil 30 needs to be pre-cooled to 800℃-850℃ before the subsequent high-frequency induction quenching process. This heat treatment method of first carburizing and then high-frequency induction heating can reduce the coarsening of austenite grains and also shorten the time required for the high-frequency induction quenching process.

[0048] (3) Furthermore, in conventional heat treatment processes, a cryogenic treatment process is required after carburizing and quenching to allow the retained austenite to continue transforming into martensite, thereby reducing the amount of retained austenite and increasing the amount of martensite, thus improving hardness. However, in the composite heat treatment process adopted in this application, the anvil 30 can be subjected to high-frequency induction rapid heating after the carburizing and quenching process. This composite heat treatment method can not only reduce the amount of retained austenite and avoid the high cost of cryogenic treatment, but also avoid quenching cracks caused by excessive thermal stress due to excessive cooling rate.

[0049] (4) Furthermore, when steel parts achieve the same physical properties after heat treatment, the composite heat treatment process of carburizing and quenching followed by high-frequency induction hardening consumes less energy and takes less time.

[0050] The composite heat treatment process of carburizing and quenching followed by high-frequency induction hardening used in the embodiments of this application, compared with the above-mentioned single high-frequency induction hardening process, suppresses the uneven diffusion of carbon atoms from both thermodynamic and kinetic perspectives. This avoids the phenomenon of carbon segregation in the anvil 30 and ensures that the carbon diffusion in the anvil 30 is uniform after the composite heat treatment process. Specifically, this is reflected in the following aspects: (1) First, in the composite heat treatment process, a controllable carbon gradient can be established on the anvil 30 during the carburizing stage. At this stage, whether a gas carburizing process such as propane or natural gas is used or a solid carburizing process such as charcoal mixed with carbonate is used, carbon atoms can diffuse to 0.4mm-2.2mm below the surface of the anvil 30 in an environment of 900℃-950℃, and a high carbon concentration gradient of 0.45%-0.75% on the surface and 0.32%-0.38% in the core is formed, so as to achieve precise control of carbon potential. At the same time, a segmented process of strong carburizing + diffusion can be used to carburize the anvil 30, so as to avoid the phenomenon of excessively high local carbon concentration at the connection or inflection point of the impact receiving part 32 and the handle 31 of the anvil 30, so as to improve the uniformity of the diffusion layer in the anvil 30.

[0051] (2) Secondly, in the composite heat treatment process, the transfer of carbon atoms that have penetrated into the anvil 30 through the carburizing and quenching process can be suppressed through the high frequency induction quenching stage. When the high frequency current heats the anvil 30, the surface of the anvil 30 can reach the austenitizing temperature within a few seconds. Then, rapid quenching is required by oil cooling or water cooling. During this high frequency induction quenching process, due to rapid heating and cooling, carbon atoms do not have time to diffuse over long distances and are "frozen" in the martensite. In addition, high frequency induction quenching can form lath martensite with a lamellar spacing of less than 0.2 μm, which makes the penetrated carbon atoms dispersed and thus reduces carbon segregation caused by slow cooling.

[0052] (3) Furthermore, in the composite heat treatment process, the anvil 30 can be directly subjected to high frequency induction quenching after carburizing and quenching, which can avoid the redistribution of carbon atoms caused by intermediate cooling; in addition, the low temperature tempering of the carburizing and quenching process and the local heating method of high frequency induction quenching can control the deformation of the anvil 30 to within 0.1 mm, thereby avoiding the uneven stress of the carbon layer caused by the deformation of the anvil 30.

[0053] In this application, in order to achieve a composite heat treatment process that synergizes and promotes the aforementioned carburizing and quenching process and high-frequency induction hardening process, the anvil 30 after the pretreatment process can be subjected to the following treatment process: S10, Carburizing process: The entire anvil 30 is placed in a controlled atmosphere carburizing furnace and kept at a temperature in a carbon-containing medium, so that carbon atoms can diffuse into the surface of the anvil 30 to form a carburized layer. S20, High-frequency induction hardening process: After cleaning the surface of the anvil 30 with the carburized layer, the heating induction coil is sleeved on the outer periphery of the impact receiving part 32 and the driving surface 313 of the anvil 30 to perform local induction heating on the anvil 30. S30. Post-processing: The anvil 30, which has a hardened layer after high-frequency induction hardening, is subjected to quenching and tempering.

[0054] For example, the S10 carburizing process described above may include the following specific steps: S11. After the entire anvil 30 is placed in a controlled atmosphere carburizing furnace, the furnace temperature is raised to 910℃-940℃, and propane, natural gas or other carbon-containing gases are injected into it to perform gas carburizing on the anvil 30. S12. The carbon potential in the controlled atmosphere carburizing furnace is controlled between 1.0% and 1.2%, and monitored and controlled by an infrared analyzer or other sensors, so that the anvil 30 enters the strong carburizing period and continues for 2-3 hours. S13. The carbon potential in the controlled atmosphere carburizing furnace is controlled between 0.8% and 0.9%, and monitored and controlled by an infrared analyzer or other sensors, so that the anvil 30 enters the carburizing diffusion period and lasts for 3.5h-4.5h. S14. Subsequently, the furnace temperature in the controlled atmosphere carburizing furnace is pre-cooled to 800℃-850℃ in preparation for subsequent high-frequency induction heating.

[0055] In the specific steps of the S10 carburizing process described above, the carbon potential in the controlled atmosphere carburizing furnace can be controlled between 1.0% and 1.2% for the strong carburizing period of carbon atom diffusion, and then the carbon potential can be controlled between 0.8% and 0.9% for the diffusion period of carbon atom diffusion. This segmented carbon potential control method in the anvil 30 makes the carbon concentration gradient smoother, effectively eliminating carbon concentration gradient peaks and preventing the formation of a network of carbides on the anvil 30.

[0056] In addition, in the specific steps of the S10 carburizing process, after the anvil 30 completes the final carburizing diffusion period, the furnace temperature in the controlled atmosphere carburizing furnace can be reduced to 800℃-850℃ to pre-cool the anvil 30, which can suppress the formation of residual austenite and reduce quenching deformation.

[0057] For example, the above-described S20 high-frequency induction hardening process may include the following specific steps: S21. After cleaning the surface of the anvil 30 with the carburized layer, multiple heating induction coils are sleeved on the outer periphery of the impact receiving part 32 and the driving surface 313 of the anvil 30. S22. Adjust the frequency of the high-frequency AC power to 10-50kHz and perform deep hardening on the impact receiving part 32 and the driving surface 313. The hardening depth can be 1.5mm-2mm. S23. Adjust the frequency of the high-frequency AC power to 100-300kHz, and perform surface hardening on the impact receiving part 32 and the driving surface 313. The hardening depth can be 0.5mm-1.0mm.

[0058] In the aforementioned S20 high-frequency induction hardening process, the anvil 30 undergoes deep through-heating at a frequency of 10-50 kHz and surface fine heating at a frequency of 100-300 kHz. This reduces the austenitization time inside the anvil 30 to 1.5-3 seconds, and the grain size can be controlled to above ASTM grade 12. This not only shortens the high-frequency induction hardening time but also yields an ultrafine microstructure.

[0059] For example, the post-processing step S30 described above may include the following specific steps: S31. Cool and quench the anvil 30 using a 5%-10% water-based polymer solution, and control the temperature cooling rate to be greater than 50℃ / s. S32. Subsequently, the anvil 30 is tempered at a temperature of 130℃-200℃ for 2-4 hours.

[0060] In the S30 post-processing step described above, controlling the cooling rate of the anvil 30 ensures martensitic transformation. Alternatively, the anvil 30 can be quenched using a self-cooling method.

[0061] In the above-mentioned S30 post-treatment process, the tempering temperature is controlled at 130℃-200℃, which can eliminate the internal stress of the anvil 30 and stabilize its internal structure.

[0062] Of course, in the embodiments of this application, the above-mentioned carburizing and quenching process can also be replaced by a carbonitriding and quenching process. The principle and purpose are basically the same as carburizing and quenching, both forming a surface strengthening layer, i.e., the first structural layer 30a, on the impact receiving part 32 and the driving surface 313. In this application, the durability and fatigue resistance of the anvil 30 can be determined according to the following test criteria: Anvil 30 was fitted onto an electric wrench capable of outputting 1000 Nm of torque (2400-2630 bpm). An M24 bolt was continuously loosened using a cyclical process of 2 seconds of operation followed by a 2-second pause. The durability and fatigue resistance of the anvil were assessed by counting the number of fully charged battery packs consumed before it fractured. The final test results showed that anvils treated only with high-frequency induction heating fractured after consuming 30-130 fully charged battery packs; anvils treated with carburizing and high-frequency induction heating did not fracture after consuming 180-195 fully charged battery packs.

[0063] For steel, carbon is an important element for ensuring its strength, especially for forming a surface strengthening layer. Therefore, in this application, the carbon content of the three structural layers (30a, 30b, 30c) of the anvil varies. For example, in the carburizing and quenching process or the carbonitriding and quenching process, the carbon content in the first structural layer 30a can be controlled to a weight percentage range of 0.45%-0.75%. In the high-frequency induction hardening process, the carbon content in the second structural layer 30b can be controlled to a weight percentage range of 0.32%-0.38%. When selecting the steel raw material, a carbon content weight percentage range of 0.32%-0.38% can be chosen, thereby ensuring that the carbon content weight percentage of the third structural layer 30c is also within the range of 0.32%-0.38%. By controlling the carbon content as described above, the durability and fatigue resistance of the three different structural layers of the anvil 30 can be distinguished and controlled, thereby forming at least two structural layers with greater hardness on its surface, while the interior of the anvil 30 maintains toughness, enabling it to meet the usage requirements of high torque wrenches.

[0064] See appendix Figure 6 The impact receiving part 32 and the driving surface 313 of the anvil 30, after undergoing carburizing and quenching processes and high-frequency induction hardening processes, form three structural layers of a certain depth. From the outside to the inside, these layers are defined as a first structural layer 30a with a depth of H1, a second structural layer 30b with a depth of H2, and a third structural layer 30c with a depth of H3. The depth H1 of the first structural layer 30a is defined as the distance from the outer surface of the impact receiving part 32 or the driving surface 313 to the interface between the first structural layer 30a and the second structural layer 30b; the depth H2 of the second structural layer 30b is defined as the distance from the interface between the first structural layer 30a and the second structural layer 30b to the interface between the second structural layer 30b and the third structural layer 30c; and the depth H3 of the third structural layer 30c is defined as the distance from the interface between the second structural layer 30b and the third structural layer 30c to the central axis of the anvil 30.

[0065] In this application, the depth of each structural layer can be determined based on a comprehensive balance between the strength requirements of the structural layer and the negative impact of the resulting reduction in material toughness. In this application, the depth H1 of the first structural layer 30a can range from 0.4 mm to 1.2 mm, the depth H2 of the second structural layer 30b can range from 1.2 mm to 2.2 mm, and the depth H3 of the third structural layer 30c can range from 5 mm to 10 mm.

[0066] For example, in the first embodiment of this application, the depth H1 of the first structural layer 30a can be 0.4 mm, the depth H2 of the second structural layer 30b can be 2.2 mm, and the depth H3 of the third structural layer 30c can be 5 mm.

[0067] In the second embodiment of this application, the depth H1 of the first structural layer 30a can be 1.2 mm, the depth H2 of the second structural layer 30b can be 1.2 mm, and the depth H3 of the third structural layer 30c can be 10 mm.

[0068] In the third embodiment of this application, the depth H1 of the first structural layer 30a can be 0.8 mm, the depth H2 of the second structural layer 30b can be 1.7 mm, and the depth H3 of the third structural layer 30c can be 7.5 mm.

[0069] In the fourth embodiment of this application, the depth H1 of the first structural layer 30a can be 0.8 mm, the depth H2 of the second structural layer 30b can be 2.2 mm, and the depth H3 of the third structural layer 30c can be 10 mm.

[0070] In the fifth embodiment of this application, the depth H1 of the first structural layer 30a can be 1.2 mm, the depth H2 of the second structural layer 30b can be 1.5 mm, and the depth H3 of the third structural layer 30c can be 5 mm.

[0071] In addition, the anvil 30 formed above can be shot blasted to generate residual compressive stress on the outer surface of the first structural layer 30a, thereby changing the metal mechanical properties of the surface of the anvil 30 and forming a fourth structural layer 30e on the outer surface of the first structural layer 30a. The fourth structural layer 30e has a fourth hardness, and the hardness value of the fourth hardness is greater than the hardness value of the first hardness.

[0072] In some embodiments, the impact tool 100 may employ an anvil 30 with a nominal width of at least 3 / 4 inch after the aforementioned structural reinforcement process. This enables the use of a relatively small head size to perform high-torque fastening tasks beyond the capabilities of typical battery-powered impact tools.

[0073] It should be understood that the above embodiments are exemplary and are not intended to encompass all possible implementations included in the claims. Various modifications and changes can be made to the above embodiments without departing from the scope of this disclosure. Similarly, the various technical features of the above embodiments can be arbitrarily combined to form other embodiments of this application that may not be explicitly described. Therefore, the above embodiments only illustrate several implementations of this application and do not limit the scope of protection of this patent application.

Claims

1. An impact tool, characterized in that, include: case; An electric motor, which is housed in the housing, and the outer diameter of the electric motor is at least greater than or equal to 50 mm; An anvil, which is rotatably supported on the housing and protrudes from the front end of the housing; An impact assembly housed in the housing, the impact assembly being capable of applying a circumferential rotational impact force to the anvil, and the impact frequency of the impact force applied by the impact assembly to the anvil being at least 1700 ipm; A transmission assembly, housed in the housing, is connected to the motor and the impact assembly respectively to transmit power from the motor to the impact assembly and generate an operating torque of at least 2400 Nm in the anvil. The anvil includes an impact receiving portion for receiving the impact force applied by the impact assembly and a head for engaging the tool tip, the head having a minimum cross-sectional width of at least 3 / 4 inch in a plane perpendicular to the length extension direction of the anvil.

2. The impact tool according to claim 1, characterized in that: At least one of the impact receiving part and the head of the anvil is formed with a hardened layer after surface treatment.

3. The impact tool according to claim 2, characterized in that: The hardened layer, from the outside to the inside, includes a first structural layer with a first hardness and a second structural layer with a second hardness. The anvil is formed with a first structural layer after carburizing and quenching or carbonitriding and quenching. The anvil with the first structural layer is further formed with a second structural layer and a third structural layer after a second process. The third structural layer has a third hardness. The hardness values ​​of the first hardness, the second hardness, and the third hardness decrease sequentially.

4. The impact tool according to claim 3, characterized in that: The hardness range of the first structural layer is HV655-HV760, the hardness range of the second structural layer is HV585-HV710, and the hardness range of the third structural layer is HV360-HV560.

5. The impact tool according to claim 1, characterized in that: The diameter of the motor is at least 60 mm.

6. The impact tool according to claim 1, characterized in that: The impact frequency at which the impact component applies an impact force to the anvil is at least 1800 ipm.

7. The impact tool according to claim 1, characterized in that: The anvil generates a working torque of at least 2500 Nm.

8. The impact tool according to claim 1, characterized in that: The maximum diameter of the shell is less than 110 mm.

9. The impact tool according to claim 1, characterized in that: The impact assembly includes an impact block, the impact block weighing at least 1500g.

10. The impact tool according to claim 1, characterized in that: The head includes multiple drive surfaces for engaging with the tool tip.

11. An impact tool, characterized in that, include: case; An electric motor, which is housed in the housing, and the outer diameter of the electric motor is at least greater than or equal to 50 mm; An anvil, which is rotatably supported on the housing and protrudes from the front end of the housing; An impact assembly housed in the housing, the impact assembly including a striking block that applies a circumferential rotational impact force to the anvil, the striking block having an outer diameter of at least 100 mm, and the impact frequency at which the impact assembly applies the impact force to the anvil being at least 1700 ipm. A transmission assembly, housed in the housing, is connected to the motor and the impact assembly respectively to transmit power from the motor to the impact assembly and generate an operating torque of at least 2400 Nm in the anvil. The anvil includes an impact receiving portion for receiving the impact force applied by the impact assembly and a head for engaging the tool tip, the head having a minimum cross-sectional width of at least 3 / 4 inch in a plane perpendicular to the length extension direction of the anvil.

12. The impact tool according to claim 10, characterized in that: At least one of the impact receiving part and the head has a first structural layer, a second structural layer and a third structural layer from the outside to the inside. The anvil is formed with a first structural layer after carburizing and quenching or carbonitriding and quenching. The first structural layer has a first hardness. The anvil with the first structural layer is formed with a second structural layer and a third structural layer after a second process. The second structural layer has a second hardness and the third structural layer has a third hardness. The hardness values ​​of the first hardness, the second hardness and the third hardness decrease sequentially.

13. The impact tool according to claim 11, characterized in that: The diameter of the motor is at least 50 mm.

Citation Information

Patent Citations