A bumper to improve the surface appearance problem of the ultrasonic piercing welding of the bumper

By setting weakening holes and grooves on the ultrasonic puncture welding bracket, the problems of welding marks and top bulges on the bumper surface are solved, improving the appearance quality and meeting the requirements of high-precision processes.

CN224994693UActive Publication Date: 2026-11-20FUWEI DONGYANG AUTO PARTS (SHANGHAI) CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522463840.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-20
Publication Date
2026-11-20
Estimated Expiration
2035-11-20

AI Technical Summary

Technical Problem

Conventional ultrasonic puncture welding can easily leave obvious welding marks or bumps on the surface of car bumpers, affecting their appearance.

Method used

Multiple weakening holes and weakening grooves are set on the ultrasonic puncture welding bracket. The weakening holes are used to release welding stress, and the weakening grooves are used to solve the problem of non-adhesion of the welding surface. The welding structure is improved by designing the weakening part.

Benefits of technology

It effectively solved the problems of welding marks and top bulges, improved the appearance quality of the bumper surface, and met the requirements of high-precision manufacturing processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224994693U_ABST
    Figure CN224994693U_ABST
Patent Text Reader

Abstract

The utility model relates to a bumper for improving bumper ultrasonic penetration welding surface appearance problem, include: bumper body, be located on the ultrasonic penetration welding support of bumper body, open multiple weakening parts on the ultrasonic penetration welding support, multiple weakening parts are uniformly arranged in the welding point welding surface of ultrasonic penetration welding and the position close to welding surface, weakening part includes: the weakening hole of uniform distribution in welding surface and the position close to welding surface, and the weakening groove of opening in the both sides of welding surface, the utility model has the advantages of: through setting weakening hole for releasing welding stress, and then realize the deformation stress of absorbing ultrasonic penetration welding when high temperature fusion bumper and support, through the weakening groove for solving ultrasonic penetration welding support structure is too strong while the welding point surface is not adhered to because of the wall thickness mutation deformation support welding surface and bumper B surface, and the welding top package problem of forming after welding periphery.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of automotive bumper technology, and in particular to a bumper that improves the appearance of the surface after ultrasonic puncture welding. Background Technology

[0002] With the rapid development of the automotive industry, especially the electric vehicle sector, car bumpers are increasingly emphasizing environmental protection and cost control while balancing safety, aerodynamic performance, and aesthetics. Compared to tape application, ultrasonic piercing welding eliminates the need for primer and tape, offering greater environmental advantages and reducing unit production costs, thus leading to its widespread application in the automotive field. However, as OEMs demand increasingly refined product finishes, conventional ultrasonic piercing welding structures are prone to leaving noticeable welding marks or bulges on the surface, a problem that urgently needs to be addressed. Utility Model Content

[0003] In view of the above problems, the purpose of this utility model is to provide a bumper that improves the appearance of the surface of the bumper after ultrasonic puncture welding, thereby overcoming the shortcomings of the prior art.

[0004] This utility model provides a bumper with improved surface appearance issues from ultrasonic puncture welding. It includes: a bumper body, an ultrasonic puncture welding bracket on the bumper body, and multiple weakening portions formed on the ultrasonic puncture welding bracket. The weakening portions are evenly distributed on the ultrasonic puncture welding bracket. Each weakening portion includes: a set of weakening holes evenly distributed on the welding surface and near the welding surface, and weakening grooves formed on both sides of the welding surface. The set of weakening holes is used to release welding stress, thereby absorbing the deformation stress generated during the high-temperature fusion of the bumper and bracket during ultrasonic puncture welding. The weakening grooves on both sides are used to solve the problem of the ultrasonic puncture welding bracket structure being too strong, and the welding surface deforming due to abrupt changes in wall thickness, causing the welding surface of the bracket to not fit properly with the bumper's B-side, resulting in a weld bump around the perimeter after welding.

[0005] As a preferred embodiment of this invention, a set of weakening holes consists of three rows of staggered weakening holes.

[0006] As a preferred embodiment of this invention, the weakening hole is a rectangular hole.

[0007] As a preferred embodiment of this invention, the weakening groove is a rectangular groove.

[0008] As a preferred embodiment of this invention, the width of the weakening hole is 0.8-1mm, and the length of the weakening hole is 3-5mm.

[0009] The beneficial effects of this utility model are as follows:

[0010] 1. This utility model uses weakening holes to release welding stress, thereby absorbing the deformation stress generated during ultrasonic piercing welding due to the high-temperature fusion of the bumper and bracket.

[0011] 2. This utility model solves the problem of the excessive strength of the ultrasonic puncture welding bracket structure and the deformation of the weld point surface due to the sudden change in wall thickness, which causes the bracket welding surface to not fit with the B-side of the bumper and form a weld top after welding. Compared with the existing conventional welding structure, the weakened part can solve the appearance problem of the bumper while meeting the pull-out force of the welding point. Attached Figure Description

[0012] Figure 1 This is a partial structural view of the bumper in this embodiment.

[0013] Figure 2 This is a schematic diagram of the weakening part structure in this embodiment.

[0014] Figure reference numerals: 1. Bumper body; 2. Ultrasonic puncture welding bracket; 3. Weakened part; 4. Weakened hole; 5. Weakened groove. Detailed Implementation

[0015] See Figure 1-2 As shown in the figure, this embodiment provides a bumper that improves the appearance of the surface of the ultrasonic puncture welding of the bumper. It includes: a bumper body 1, an ultrasonic puncture welding bracket 2 located on the bumper body 1, and a plurality of weakening parts 3 opened on the ultrasonic puncture welding bracket 2. The plurality of weakening parts 3 are evenly distributed on the ultrasonic puncture welding bracket 2. The weakening part 3 includes: a set of weakening holes 4 evenly distributed on the welding surface and near the welding surface, and weakening grooves 5 opened on both sides of the welding surface.

[0016] Furthermore, in this embodiment, a set of weakening holes 4 consists of three rows of staggered weakening holes 4, where the weakening holes 4 are rectangular holes and the weakening grooves 5 are rectangular grooves. The width of the weakening holes 4 is 0.8-1mm, and the length of the weakening holes is 3-5mm.

[0017] Working principle: A set of weakening holes 4 is used to release welding stress, thereby absorbing the deformation stress generated by the high temperature fusion of the bumper and bracket during ultrasonic piercing welding. The weakening grooves 5 on both sides are used to solve the problem that the structure of the bracket 2 is too strong and the welding point surface is deformed due to the sudden change in wall thickness, resulting in the bracket welding surface not fitting with the bumper B surface and forming a welding top after welding.

[0018] The above are merely specific embodiments of this utility model, but the protection scope of this utility model is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in this utility model should be included within the protection scope of this utility model. Therefore, the protection scope of this utility model should be determined by the scope of the claims.

Claims

1. A bumper that improves the surface appearance of bumpers after ultrasonic puncture welding, characterized in that, include: The bumper body, the ultrasonic puncture welding bracket located on the bumper body, and multiple weakening parts opened on the ultrasonic puncture welding bracket, wherein the multiple weakening parts are evenly distributed on the ultrasonic puncture welding bracket, and the weakening parts include: a set of weakening holes evenly distributed on the welding surface and near the welding surface, and weakening grooves opened on both sides of the welding surface.

2. The bumper according to claim 1, which improves the surface appearance of the bumper after ultrasonic puncture welding, is characterized in that... A set of weakening holes consists of three rows of staggered weakening holes.

3. A bumper according to claim 1 that improves the surface appearance of bumpers after ultrasonic puncture welding, characterized in that, The weakening hole is a rectangular hole.

4. A bumper for improving the surface appearance of bumpers after ultrasonic puncture welding, as described in claim 1, characterized in that... The weakening groove is a rectangular groove.

5. A bumper according to claim 1 that improves the surface appearance of bumpers after ultrasonic puncture welding, characterized in that, The width of the weakening hole is 0.8-1mm, and the length of the weakening hole is 3-5mm.