Low-e coated glass
Patent Information
- Application Number
- CN202522837499.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-31
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-12-31
AI Technical Summary
[0004]本实用新型的主要目的是提出一种低辐射镀膜玻璃,旨在解决在相关技术中镀膜玻璃热加工性能的稳定性不足的技术问题
Smart Images

Figure CN224996791U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of coated glass technology, and in particular to a low-emissivity coated glass. Background Technology
[0002] With the widespread application of glass curtain walls in high-rise buildings, low-emissivity coated glass has attracted much attention as an energy-saving and environmentally friendly material. Its core function is to reduce heat transfer by decreasing the emissivity of the glass, thereby achieving energy-saving effects, while also ensuring good optical and mechanical properties.
[0003] During the tempering process of glass, existing low-emissivity coated glass is prone to problems such as coating oxidation, delamination, and cracking. These problems not only affect the appearance and performance of the product, but also reduce its service life and reliability. Utility Model Content
[0004] The main objective of this invention is to propose a low-emissivity coated glass, which aims to solve the technical problem of insufficient stability in the thermal processing performance of coated glass in related technologies.
[0005] To achieve the above objectives, the present invention proposes a low-emissivity coated glass, comprising a glass substrate, wherein a first dielectric layer, a first protective layer, a functional layer, a second protective layer, and a second dielectric layer are sequentially stacked on the glass substrate; the first dielectric layer comprises a first SiN... x Layers and AlZnO X Layer, the first SiN x A layer covers the glass substrate, the AlZnO X The layer covers the first SiN x The side of the layer that faces away from the glass substrate.
[0006] In one embodiment, the first SiN x Layers and AlZnO X A silicon zirconium oxide layer is disposed between the layers; the thickness of the first dielectric layer is D1, 35nm≤D1≤55nm.
[0007] In one embodiment, the second dielectric layer covers the surface of the second protective layer away from the functional layer; the second dielectric layer comprises sequentially stacked AlZnO X Layer and second SiN x Layer, the AlZnO X A layer covers the surface of the second protective layer away from the functional layer, and the thickness of the second dielectric layer is D2, 30nm≤D2≤50nm.
[0008] In one embodiment, the AlZnO XThe thickness of the layer is 5nm-18nm, the first SiN x Layer or the first SiN x The sum of the thicknesses of the layer and the silicon zirconium oxide layer is 17nm-50nm.
[0009] In one embodiment, the second SiN x The layer is far from the AlZnO X A ZrO2 layer may also be disposed on one side surface of the layer, wherein the thickness of the ZrO2 layer is D3, and 5nm≤D3≤10nm.
[0010] In one embodiment, the first protective layer includes at least one of a NiCr layer and a TiO2 layer. The first protective layer covers the surface of the first dielectric layer away from the glass substrate. The thickness of the first protective layer is D4, where 2nm ≤ D4 ≤ 4nm.
[0011] In one embodiment, the second protective layer includes at least one of a NiCr layer and a TiO2 layer. The second protective layer covers the surface of the functional layer away from the first protective layer. The thickness of the second protective layer is D5, where 3nm ≤ D5 ≤ 5nm.
[0012] In one embodiment, the thickness ratio of the first protective layer to the second protective layer is D4:D5, where 1:1.5 ≤ D4:D5 ≤ 1:2.
[0013] In one embodiment, the functional layer is a metallic material, and the functional layer covers the surface of the first protective layer away from the first dielectric layer. The thickness of the functional layer is D6, where 4nm≤D6≤8nm.
[0014] In one embodiment, the metallic material is silver.
[0015] The low-emissivity coated glass provided by this invention, through a structure consisting of a first dielectric layer, a first protective layer, a functional layer, a second protective layer, and a second dielectric layer stacked sequentially, solves the problems of high emissivity, insufficient performance stability, poor high-temperature resistance, and short service life of traditional coated glass. In this invention, the first dielectric layer includes a first SiN... x Layers and AlZnO X A layer, which covers the glass substrate. Through the first SiN... X The layer can enhance the bonding strength between the film and the glass substrate, while preventing the migration of alkali metal ions from the glass to subsequent film layers, thus preventing the degradation of the functional layer performance and assisting in optimizing the optical matching performance of the film system; AlZnO X The layer possesses excellent electrical conductivity and transparency, further enhancing the low-emissivity of the glass while improving its surface hardness and abrasion resistance. This is achieved through AlZnO...X The protective functional layer improves the overall oxidation resistance of the glass. This invention utilizes AlZnO... X The magnetron sputtering process enables a denser surface structure, reducing surface defects and porosity, further improving wear resistance and processability. This makes the coated glass less prone to scratches or wear during processing, thus increasing the yield rate. The first and second protective layers effectively protect the functional layers from environmental corrosion, extending the service life of the coated glass and improving its overall performance stability. The second dielectric layer further optimizes the optical properties of the glass. ZrO2 has high hardness and high temperature resistance, directly resisting external dust friction, hard object scratches, and mechanical damage during processing, preventing scratches on the functional film layer. At the same time, its excellent high temperature resistance prevents direct thermal damage to the underlying functional film layer. This allows the coated glass to maintain good light transmittance, processability, mechanical properties, and temperability while possessing low emissivity. Attached Figure Description
[0016] To more clearly illustrate the technical solutions in the embodiments of this utility model or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.
[0017] Figure 1 A schematic diagram of a structure of an embodiment of the low-emissivity coated glass provided by this utility model; Figure 2 A parameter table of the film structure of the first embodiment of the low-emissivity coated glass provided by this utility model; Figure 3 A parameter table of the film structure of the second embodiment of the low-emissivity coated glass provided by this utility model; Figure 4 A parameter table of the film structure of the third embodiment of the low-emissivity coated glass provided by this utility model; Figure 5 The color values of the coated glass before and after tempering in various embodiments provided by this utility model.
[0018] Explanation of icon numbers: 100. Low-emissivity coated glass; 10. Glass substrate; 20. First dielectric layer; 30. First protective layer; 40. Functional layer; 50. Second protective layer; 60. Second dielectric layer.
[0019] The realization of the purpose, functional features and advantages of this utility model will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation
[0020] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present utility model.
[0021] It should be noted that if the embodiments of this utility model involve directional indicators (such as up, down, left, right, front, back, etc.), the directional indicators are only used to explain the relative positional relationship and movement of the components in a specific posture. If the specific posture changes, the directional indicators will also change accordingly.
[0022] Furthermore, if the embodiments of this utility model involve descriptions such as "first" or "second," these descriptions are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features. Additionally, the use of "and / or" or "and / or" throughout the text includes three parallel solutions. For example, "A and / or B" includes solution A, solution B, or a solution where both A and B are satisfied simultaneously. Furthermore, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. When the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this utility model.
[0023] This utility model proposes a low-emissivity coated glass 100.
[0024] Please see Figure 1 In one embodiment of this utility model, the low-emissivity coated glass 100 includes a glass substrate 10, on which a first dielectric layer 20, a first protective layer 30, a functional layer 40, a second protective layer 50, and a second dielectric layer 60 are sequentially stacked; the first dielectric layer 20 includes a first SiN x Layers and AlZnO X Layer, first SiN X A layer of AlZnO is applied to the glass substrate 10. X Layer covering the first SiN x The layer is on the side opposite to the glass substrate 10.
[0025] In this embodiment, the surface film layer on the glass substrate 10 of the low-emissivity coated glass 100 provided by this invention has good heat resistance and stable hot processing performance, making it suitable for both flat and curved glass tempering processes. After the tempering process, the film layer is stable and free from defects such as cracking, oxidation, delamination, and scratches. It should be noted that the first dielectric layer 20 is made of first SiN... x As a base layer, it enhances the bonding strength between the film layer and the glass substrate 10, while simultaneously preventing the migration of alkali metal ions from the glass to subsequent film layers, thus preventing performance degradation of the functional layers and assisting in optimizing the optical matching performance of the film system. Meanwhile, the first SiN... x It has higher hardness and stronger wear resistance by using the first SiN x The formation of the first dielectric layer 20 can improve the scratch resistance of the top layer of the coating layer and further improve the mechanical properties of the coating layer. The AlZnO in the first dielectric layer 20... X The first protective layer (hereinafter referred to as AZO) has good transparency, high visible light transmittance, and good infrared light reflectivity. The second dielectric layer 60 is located on the top layer of the film layer on the entire glass substrate 10 surface. It improves the mechanical properties and scratch resistance of the film layer on the entire glass substrate 10 surface, making the coated product less susceptible to scratches. Both the first protective layer 30 and the second protective layer 50 protect the functional layer 40, preventing it from oxidizing under the high temperatures of the thermal processing. The functional layer 40 utilizes the low emissivity of the metallic material in the functional layer 40 to reduce the emissivity of the coated glass, filtering sunlight into a cold light source and improving transmittance.
[0026] The low-emissivity coated glass 100 provided by this invention, through a structure consisting of a first dielectric layer 20, a first protective layer 30, a functional layer 40, a second protective layer 50, and a second dielectric layer 60 stacked sequentially, can solve the problems of high emissivity, insufficient performance stability, poor high-temperature resistance, and short service life of traditional coated glass. In this invention, the first dielectric layer 20 includes a first SiN... x Layers and AlZnO X A layer that covers the glass substrate 10. Through the first SiN... x The layer can enhance the bonding strength between the film and the glass substrate, while preventing the migration of alkali metal ions from the glass to subsequent film layers, thus preventing the degradation of the functional layer performance and assisting in optimizing the optical matching performance of the film system; AlZnO X The layer possesses excellent electrical conductivity and transparency, further enhancing the low-emissivity of the glass while improving its surface hardness and abrasion resistance. This invention utilizes AlZnO... XThe magnetron sputtering process enables a denser surface structure, reducing surface defects and porosity, further improving wear resistance and processability. This makes the coated glass less prone to scratches or wear during processing, thereby increasing the yield rate. The first protective layer 30 and the second protective layer 50 effectively protect the functional layer 40 from external environmental corrosion, extending the service life of the coated glass and improving its overall performance stability. The second dielectric layer 60 further optimizes the optical properties of the glass. ZrO2 has high hardness and high temperature resistance, directly resisting external dust friction, hard object scratches, and mechanical damage during processing, preventing scratches on the functional film layer. At the same time, its excellent high temperature resistance prevents direct thermal damage to the underlying functional film layer. This allows the coated glass to maintain good light transmittance, processability, temperability, and high temperature resistance while possessing low emissivity.
[0027] In one embodiment of this utility model, the first SiN x Layers and AlZnO X A silicon zirconium oxide layer is disposed between the layers; the thickness of the first dielectric layer 20 is D1, 35nm≤D1≤55nm.
[0028] In this embodiment, the thickness D1 of the first dielectric layer 20 is in the range of 35 to 55 nm. D1 can be 35 nm, 40 nm, 45 nm, 55 nm, etc., and can be set as needed. No limitation is made here.
[0029] In one embodiment of this invention, the second dielectric layer 60 covers the surface of the second protective layer 50 away from the functional layer 40; the second dielectric layer 60 comprises AlZnO layers stacked sequentially. X Layer and second SiN x Layer, AlZnO X The second protective layer 50 is covered on the side of the second protective layer 50 away from the functional layer 40, and the thickness of the second dielectric layer 60 is D2, 30nm≤D2≤50nm.
[0030] In this embodiment, it should be noted that the second dielectric layer 60 is located on the top layer of the film layer on the entire glass substrate 10 surface. It is used to improve the mechanical properties and scratch resistance of the film layer on the entire glass substrate 10 surface, making the coated product less susceptible to scratches. The second dielectric layer 60 includes AlZnO. X Layer (hereinafter referred to as AZO) and second SiN x The second protective layer 50, with an AZO layer covering the surface of the second protective layer 50 away from the functional layer 40, and the second SiN layer... xA layer covers the surface of the AZO layer away from the second protective layer 50. The AZO layer serves as a protective layer, preventing the functional layer 40 from oxidation or physical damage, and improving the durability and stability of the surface film on the glass substrate 10. The thickness of the AZO layer is 10 nm. The thickness D2 of the second dielectric layer 60 can be 30 nm, 35 nm, 40 nm, 45 nm, 50 nm, etc., and can be set according to specific needs.
[0031] In one embodiment of this utility model, AlZnO in the first dielectric layer X The thickness of the layer is 5nm-18nm, the first SiN x Layer or first SiN x The sum of the thicknesses of the layer and the silicon zirconium oxide layer is 17nm-50nm.
[0032] In this embodiment, it can be understood that a first SiNx layer is first sputtered on the glass substrate 10, followed by a silicon zirconium oxide layer sputtered on its surface, with the sum of the thicknesses of the two layers precisely controlled to be 17nm-50nm. Subsequently, AlZnO layers of 5nm-18nm are deposited sequentially. X The introduction of the silicon zirconium oxide layer, along with other films, can further enhance the scratch resistance and UV aging resistance of the first dielectric layer 20. When the first SiN... x When the combined thickness of the AlZnO layer and its silicon zirconium oxide layer is 17nm-50nm, this composite structure can form a stable optical resonant cavity. It utilizes the destructive interference effect of light to cancel reflected waves in the visible light band, thereby improving the light transmittance of the glass. X The thickness of the layer is 5nm-18nm, and can be 5nm, 10nm, 15nm, 18nm, etc.; the first SiN x Layer or first SiN x The sum of the thicknesses of the layer and the silicon zirconium oxide layer is 17nm-50nm, which can be 17nm, 20nm, 30nm, 40nm, 50nm, etc., and can be set according to specific needs.
[0033] In one embodiment of this utility model, the second SiN x Layers far from AlZnO X A ZrO2 layer can also be disposed on one side of the layer, with a thickness of D3, where 5nm≤D3≤10nm.
[0034] In this embodiment, it can be understood that the ZrO2 layer is actually a zirconium dioxide layer. The ZrO2 layer possesses high hardness and high-temperature resistance. As the top layer, it can directly resist external dust friction, hard object scratches, and mechanical damage during processing, preventing scratches on the underlying functional film layer. Simultaneously, its excellent high-temperature resistance prevents direct thermal damage to the underlying functional film layer, significantly extending the service life of the coated glass. The value of D3 ranges from 5 to 10 nm; D3 can be 5 nm, 6 nm, 7 nm, 8 nm, 9 nm, etc., and can be set according to specific needs.
[0035] In one embodiment of the present invention, the first protective layer 30 includes at least one of a NiCr layer and a TiO2 layer. The first protective layer 30 covers the surface of the first dielectric layer 20 away from the glass substrate 10. The thickness of the first protective layer 30 is D4, where 2nm≤D4≤4nm.
[0036] In this embodiment, it should be noted that the NiCr layer can form a dense oxide layer under high temperature conditions, effectively preventing oxygen diffusion and thus significantly improving the oxidation resistance of the film layer on the upper surface of the glass substrate 10. The TiO2 layer can effectively block the diffusion of external water vapor, oxygen, and corrosive ions to the functional layer, ensuring the long-term stability of the low-emissivity performance of the coated glass. The thickness D4 of the first protective layer 30 can be 2nm, 2.5nm, 3nm, 3.1nm, 3.3nm, 3.5nm, 4nm, etc., and can be set according to specific needs, without limitation here.
[0037] In one embodiment of the present invention, the second protective layer 50 includes at least one of a NiCr layer and a TiO2 layer. The second protective layer 50 covers the surface of the functional layer 40 away from the first protective layer 30. The thickness of the second protective layer 50 is D5, where 3nm≤D5≤5nm.
[0038] In this embodiment, it should be noted that the NiCr layer in the second protective layer 50 can form a dense oxide layer under high temperature conditions, effectively preventing oxygen diffusion. The TiO2 layer can effectively block the diffusion of external water vapor, oxygen, and corrosive ions to the functional layer, ensuring the long-term stability of the low-emissivity performance of the coated glass. The thickness D5 of the second protective layer 50 can be 3nm, 3.5nm, 4nm, 4.5nm, 5nm, etc., and can be set according to specific needs, without limitation.
[0039] In one embodiment of this utility model, the thickness ratio of the first protective layer 30 to the second protective layer 50 is D4:D5, where 1:1.5≤D4:D5≤1:2.
[0040] In this embodiment, it is understood that the thickness ratio of the first protective layer 30 to the second protective layer 50 can be selected within the range of 1:1.5 to 1:2. D4:D5 can be 1:1.5, 1:1.6, 1:1.7, 1:1.8, 1:1.9, or 1:2.
[0041] In one embodiment of this utility model, the functional layer 40 is made of metal material and covers the surface of the first protective layer 30 away from the first dielectric layer 20. The thickness of the functional layer 40 is D6, where 4nm≤D6≤8nm, and D6 can be 4nm, 5nm, 6nm, 7nm, 8nm, etc.
[0042] In this embodiment, it should be noted that the metal material used is single-silver material. The low emissivity of single-silver material reduces the emissivity of the coated glass, filtering sunlight into a cold light source and improving light transmittance. Simultaneously, using single-silver material as the functional layer 40 gives the coated glass a bright silver appearance, which is clear, beautiful, and blends seamlessly with the surrounding architecture, effectively enhancing the overall aesthetics.
[0043] This application designs the types and thicknesses of the film layers, and coordinates the layers to produce coated glass with high light transmittance, excellent mechanical properties, and temperability. The low-emissivity coated glass 100 produced by this invention has a surface transmittance T of 68%–73%, a* of 1.8–2.0, and b* of -9 to -11. After tempering, the surface transmittance T of the low-emissivity coated glass 100 produced by this invention is 71%–74%, a* of -2.5 to -4.5, and b* of -2.1 to -4.
[0044] The transmittance of low-emissivity coated glass 100 in related technologies is about 60%. The low-emissivity glass provided by this utility model not only has a transmittance of more than 70% after tempering, but also has excellent thermal processing performance and mechanical properties. It solves the problem of high transmittance single-silver low-emissivity glass being difficult to process, and improves the versatility and adaptability of high transmittance temperable single-silver low-emissivity coated glass 100.
[0045] Based on the above, the present invention discloses the following embodiment, wherein the glass thickness is 6mm.
[0046] In the first embodiment, the film structure on the glass substrate is as follows: Figure 2 As shown: The first dielectric layer has a thickness of 46.1 nm, the first protective NiCr layer has a thickness of 2 nm, the functional Ag layer has a thickness of 4.8 nm, the second protective NiCr layer has a thickness of 3 nm, and the second dielectric layer has a thickness of 46 nm. The thickness ratio of the first protective layer to the second protective NiCr layer is 1:1.5.
[0047] In the second embodiment, the film structure on the glass substrate is referenced Figure 3 As shown: The first dielectric layer has a thickness of 41.8 nm, the first protective NiCr layer has a thickness of 2 nm, the functional Ag layer has a thickness of 6.5 nm, the second protective NiCr layer has a thickness of 4 nm, and the second dielectric layer has a thickness of 48 nm. The thickness ratio of the first protective layer to the second protective NiCr layer is 1:2.
[0048] In the third embodiment, the film structure on the glass substrate is referenced. Figure 4 As shown: The first dielectric layer has a thickness of 40.2 nm, the first protective NiCr layer has a thickness of 2.5 nm, the functional Ag layer has a thickness of 7 nm, the second protective NiCr layer has a thickness of 4.5 nm, and the second dielectric layer has a thickness of 41 nm. The thickness ratio of the first protective layer to the second protective NiCr layer is 1:1.8.
[0049] Reference values for the coating color of the glass before and after tempering in each embodiment Figure 5 As shown.
[0050] In summary, the low-emissivity coated glass 100 produced by this invention has good heat resistance and stable thermal processing performance. After tempering, the coating is stable and does not exhibit defects such as cracking, oxidation, delamination, or scratches.
[0051] The above description is merely an exemplary embodiment of the present utility model and does not limit the patent scope of the present utility model. Any equivalent structural transformations made based on the technical concept of the present utility model and the contents of the present utility model specification and drawings, or direct / indirect applications in other related technical fields, are included within the patent protection scope of the present utility model.
Claims
1. A low-emissivity coated glass, comprising a glass substrate, characterized in that, The glass substrate is provided with a first dielectric layer, a first protective layer, a functional layer, a second protective layer, and a second dielectric layer stacked sequentially; the first dielectric layer includes a first SiN X Layers and AlZnO X Layer, the first SiN X A layer covers the glass substrate, the AlZnO X The layer covers the first SiN X The side of the layer that faces away from the glass substrate.
2. The low-emissivity coated glass as described in claim 1, characterized in that, The first SiN x Layers and AlZnO X A silicon zirconium oxide layer is disposed between the layers; the thickness of the first dielectric layer is D1, 35nm≤D1≤55nm.
3. The low-emissivity coated glass as described in claim 1, characterized in that, The second dielectric layer covers the surface of the second protective layer away from the functional layer; the second dielectric layer comprises sequentially stacked AlZnO X Layer and second SiN x Layer, the AlZnO X A layer covers the surface of the second protective layer away from the functional layer, and the thickness of the second dielectric layer is D2, 30nm≤D2≤50nm.
4. The low-emissivity coated glass as described in claim 1, characterized in that, The AlZnO X The thickness of the layer is 5nm-18nm, the first SiN x Layer or the first SiN x The sum of the thicknesses of the layer and the silicon zirconium oxide layer is 17nm-50nm.
5. The low-emissivity coated glass as described in claim 3, characterized in that, The second SiN x The layer is far from the AlZnO X A ZrO2 layer may also be disposed on one side surface of the layer, wherein the thickness of the ZrO2 layer is D3, and 5nm≤D3≤10nm.
6. The low-emissivity coated glass as described in claim 1, characterized in that, The first protective layer includes at least one of NiCr layer and TiO2 layer. The first protective layer covers the surface of the first dielectric layer away from the glass substrate. The thickness of the first protective layer is D4, where 2nm≤D4≤4nm.
7. The low-emissivity coated glass as described in claim 1, characterized in that, The second protective layer includes at least one of a NiCr layer and a TiO2 layer. The second protective layer covers the surface of the functional layer away from the first protective layer. The thickness of the second protective layer is D5, where 3nm ≤ D5 ≤ 5nm.
8. The low-emissivity coated glass as described in any one of claims 6 or 7, characterized in that, The thickness ratio of the first protective layer to the second protective layer is D4:D5, where 1:1.5 ≤ D4:D5 ≤ 1:
2.
9. The low-emissivity coated glass as described in claim 1, characterized in that, The functional layer is made of a metallic material and covers the surface of the first protective layer away from the first dielectric layer. The thickness of the functional layer is D6, and 4nm≤D6≤8nm.
10. The low-emissivity coated glass as described in claim 9, characterized in that, The metallic material is silver.