A device for producing zinc flower size controllable aluminum-zinc plated sheet
By installing a water-cooled roller device in the aluminized zinc production line, and utilizing a water-cooled circulation system with high thermal conductivity materials and low roughness roller surface design, the problem of uneven zinc flower size in aluminized zinc steel sheets is solved, achieving efficient control over zinc flower size and surface uniformity, which is suitable for the production of high-end home appliances and automotive outer panels.
Patent Information
- Application Number
- CN202522499800.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-25
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-11-25
AI Technical Summary
Existing technologies struggle to achieve uniform control of zinc flower size in aluminized zinc-coated steel sheets, especially in thick plates and thick-coated sheets, where zinc flower size is uneven and difficult to precisely control using traditional methods.
A water-cooled roller device is installed at the rear end of the air knife in the continuous hot-dip aluminized zinc production line. Gradual temperature control is achieved by using the cooling roller and water cooling circulation system. The size of the zinc flower is controlled by adjusting the temperature and flow rate of the cooling water. The roller is made of a material with high thermal conductivity and a low roughness roller surface design.
It achieves efficient and controllable zinc flower size of aluminized zinc coated steel sheets, ensuring surface uniformity, which is suitable for the needs of high-end home appliances and automotive exterior panels, reduces the impact of equipment aging on production, and reduces the risk of environmental pollution.
Smart Images

Figure CN224996985U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to a production device for coated plates, and more particularly to a production device for aluminum-zinc coated plates with uniform and controllable zinc flower size. Background Technology
[0002] Aluminized zinc-coated steel sheets are widely used in construction, home appliances, automobiles, and other industries due to their excellent corrosion resistance, heat resistance, and processing performance. During the aluminized zinc coating process, the size and uniformity of the zinc spangle directly affect the product's appearance quality. The size of the zinc spangle on aluminized zinc-coated sheets is easily affected by factors such as air knife pressure and fluctuations in the plating solution composition, leading to poor uniformity.
[0003] In addition, compared with thin plates or thin-coated products, the plating solution of thick plates and thick-coated strips solidifies slowly, and the zinc spangle grains are prone to being too large. Furthermore, the heat dissipation is faster at the edges of the strip and slower at the center, resulting in smaller zinc spangle sizes at the edges and larger zinc spangle sizes in the center.
[0004] Existing technologies typically control zinc spangle by adjusting air knife parameters or plating bath temperature, but these methods suffer from limitations in controllability and a single cooling method, resulting in limited controllability.
[0005] Utility model disclosure CN222935470U discloses a zinc spangle adjustment structure for aluminized zinc-coated steel sheet. This structure adjusts the airflow difference between the two sides and the middle of the steel sheet by changing the shape of the effective air outlet of the sheet cooling device, thereby altering the cooling rate between the middle and the sides of the steel sheet and controlling the size of the zinc spangle in the middle and sides of the steel sheet. However, air cooling is greatly affected by ambient airflow, making it difficult to ensure the temperature uniformity of the steel sheet in both the transverse and longitudinal directions, which can easily lead to fluctuations in the size of the zinc spangle. Furthermore, adjusting the shape of the air outlet can only roughly control the cooling difference between the middle and the sides, and cannot achieve precise temperature control across the entire sheet surface.
[0006] Patent application CN116121682A discloses a method and related equipment for optimizing uneven zinc spangle distribution in aluminized zinc products. This method involves detecting the precision of the production equipment used in the galvanizing process. When the equipment's precision reaches a preset level, the method controls the entry of the strip steel into the galvanizing process to reduce uneven zinc spangle distribution. However, this method is only applicable to production lines with initially good equipment. If the equipment is aging or lacks sufficient precision, it cannot effectively improve zinc spangle uniformity. Utility Model Content
[0007] The technical problem to be solved by this utility model is to provide a production device for aluminum-zinc coated plates with uniform and controllable zinc flower size.
[0008] To solve the above-mentioned technical problems, the technical solution adopted by this utility model is as follows: a water-cooled roller device is set at the rear end of the air knife in the continuous hot-dip aluminum-zinc plating production line; the water-cooled roller device includes a pair of cooling rollers, and the aluminum-zinc plating plate can pass through the cooling rollers; the cooling roller is a cylindrical roller structure with a hollow cavity inside, and the hollow cavity is connected to the cooling water pipeline through a pipeline.
[0009] Furthermore, the cooling roller includes a roller body, an inlet pipe, an outlet pipe, a bearing, and a sealing gasket; the roller body is cylindrical, and two sealing gaskets are provided, which are respectively fixed to both sides of the roller body to form a hollow cavity inside the roller body; bearings are fixed to the outer sides of the two sealing gaskets, and the inlet pipe and the outlet pipe are respectively rotatably sealed to the bearing on one side, and both the inlet pipe and the outlet pipe are connected to the hollow cavity.
[0010] Furthermore, the roller body is made of a material with a thermal conductivity ≥20W / (m·K).
[0011] Furthermore, the water-cooled roller device is located 0.5m to 1.5m behind the air knife.
[0012] Furthermore, the surface roughness Ra of the cooling roller is ≤0.8μm.
[0013] The beneficial effects of adopting the above technical solution are as follows: This utility model adds a water-cooled roller device after the air knife process, and works in conjunction with a water-cooled circulation system to achieve gradient temperature control, adjust the size of zinc flowers and optimize the size uniformity, thus solving the surface quality problems of large zinc flowers and uneven size of aluminized zinc coated plates; it is suitable for the production of aluminized zinc coated plates with small and uniform zinc flowers.
[0014] This invention produces coated plates with highly efficient and controllable zinc spangle dimensions. Through precise temperature control and adjustable cooling rate of the cooling rollers, it directly intervenes in the coating solidification process, meeting the stringent requirements for surface uniformity in high-end home appliances and automotive exterior panels. This invention exhibits strong process stability during use and is resistant to equipment fluctuations. The cooling rollers provide excellent surface temperature uniformity and are insensitive to changes in air knife pressure and plating solution composition, reducing the need for retrofitting older production lines. This invention utilizes a water-cooling system with zero waste gas emissions, superior to the dust pollution risks of air-cooling processes, and is characterized by environmental friendliness and zero pollution emissions. Attached Figure Description
[0015] The present invention will now be described in further detail with reference to the accompanying drawings and specific embodiments.
[0016] Figure 1 This is a schematic diagram of the structure of this utility model; Figure 2 This is a front view of the cooling roller described in this utility model; Figure 3 This is a left view of the cooling roller described in this utility model; Figure 4 This is a front view of the cooling roller connection structure described in this utility model; Figure 5 This is a left view of the cooling roller connection structure described in this utility model.
[0017] In the diagram: 1. Inlet pipe; 2. Roller body; 3. Hollow cavity; 4. Outlet pipe; 5. Bearing; 6. Metal pipe; 7. Sealing gasket; 11. Plate and strip; 12. Aluminum pot; 13. Submerged roller; 14. Air knife; 15. Cooling roller. Detailed Implementation
[0018] Figure 1-5 As shown, the production apparatus for aluminum-zinc coated sheets with uniform and controllable zinc flower size includes a continuous hot-dip aluminum-zinc coating production line. The continuous hot-dip aluminum-zinc coating production line is equipped with an aluminum pot 12, a submerged roller 13, and an air knife 14. The submerged roller 13 is located inside the aluminum pot 12, and the air knife 14 is located at the rear end of the aluminum pot 12. A water-cooled roller device is installed at the rear end of the air knife 14, preferably 0.5m to 1.5m from the rear end of the air knife 14. Thus, the sheet / strip 11 to be hot-dip coated enters the aluminum pot 12 and, driven by the submerged roller 13, passes through the aluminum-zinc coating solution inside the aluminum pot 12, forming a coating layer on the surface of the sheet / strip 11. After being blown by the air knife 14, the sheet / strip 11 is cooled by the water-cooled roller device, thereby forming the coating.
[0019] Figure 1-5 As shown, this production apparatus for aluminum-zinc coated sheets with uniform and controllable zinc flower size includes a water-cooled roller device comprising a pair of cooling rollers 15 through which the aluminum-zinc coated sheet can pass. Each cooling roller 15 includes a roller body 2, an inlet pipe 1, an outlet pipe 4, bearings 5, and sealing gaskets 7. The roller body 2 is cylindrical, and two sealing gaskets 7 are fixedly attached to both sides of the roller body 2, thus forming a hollow cavity 3 within the roller body 2. A bearing 5 is fixedly attached to the outer side of each of the two sealing gaskets 7. The inlet pipe 1 is rotatably and sealingly connected to one of the bearings 5, and the outlet pipe 4 is rotatably and sealingly connected to the other bearing 5. Furthermore, the inlet pipe 1 connects to one side of the hollow cavity 3, and the outlet pipe 4 connects to the other side of the hollow cavity 3. The inlet pipe 1 and the outlet pipe 4 connect to a cooling water pipeline, forming a cooling water circulation pipeline. The surface roughness of the cooling roller, i.e. the surface roughness of the roller body 2, is Ra≤0.8μm. The roller body 2 is made of a material with a thermal conductivity ≥20W / (m·K), preferably one of titanium copper, manganese copper and stainless steel.
[0020] With this structure, the aluminum-zinc coated sheet passes through the rollers 2. As the rollers 2 rotate with the movement of the aluminum-zinc coated sheet, the inlet pipe 1 and outlet pipe 4 do not rotate due to the bearing 5. Cooling water from the cooling water pipeline is fed into the hollow cavity 3 inside the roller 2 through the inlet pipe 1 and flows back into the cooling water pipeline through the outlet pipe 4. Thus, the cooling water circulates through the rollers 2, cooling the aluminum-zinc coated sheet. The temperature of the cooling roller surface is controlled within the range of 150–300°C by adjusting the temperature and flow rate of the circulating cooling water. When the coating of the aluminum-zinc coated sheet contacts the roller surface, the coating is rapidly cooled, significantly increasing the supercooling at the solidification front and improving the crystal nucleation rate, thereby effectively refining the zinc flowers. Simultaneously, because the roller surface temperature is extremely uniformly distributed laterally, the problem of uneven cooling at the edges and center caused by traditional air cooling is overcome, ultimately resulting in a high-quality aluminum-zinc coated steel sheet surface with fine and uniform zinc flowers.
Claims
1. A production apparatus for aluminum-zinc coated plates with uniform and controllable zinc flower size, characterized in that: In a continuous hot-dip aluminum-zinc galvanizing production line, a water-cooled roller device is provided at the rear end of the air knife (14); the water-cooled roller device includes a pair of cooling rollers, and the aluminum-zinc galvanized plate can pass through the cooling rollers; the cooling roller is a cylindrical roller structure with a hollow cavity (3) inside, and the hollow cavity is connected to the cooling water pipeline through a pipeline.
2. The production apparatus for aluminum-zinc coated plates with uniform and controllable zinc flower size according to claim 1, characterized in that: The cooling roller includes a roller body (2), an inlet pipe (1), an outlet pipe (4), a bearing (5), and a sealing gasket (7). The roller body (2) is cylindrical, and two sealing gaskets (7) are provided, which are fixedly connected to both sides of the roller body (2) to form a hollow cavity (3) inside the roller body (2). The outer sides of the two sealing gaskets (7) are fixedly connected to the bearings (5). The inlet pipe (1) and the outlet pipe (4) are rotatably and sealingly connected to the bearings (5) on one side, and the inlet pipe (1) and the outlet pipe (4) are connected to the hollow cavity (3).
3. The production apparatus for aluminum-zinc coated plates with uniform and controllable zinc flower size according to claim 2, characterized in that: The roller body (2) is made of a material with a thermal conductivity of ≥20W / (m·K).
4. The production apparatus for aluminum-zinc coated plates with uniform and controllable zinc flower size according to claim 1, characterized in that: The water-cooled roller device is located 0.5m to 1.5m behind the air knife (14).
5. A production apparatus for aluminum-zinc coated plates with uniform and controllable zinc flower size according to any one of claims 1-4, characterized in that: The surface roughness Ra of the cooling roller is ≤0.8μm.
Citation Information
Patent Citations
Method for optimizing non-uniform spangles of aluminum and zinc plated product and related equipment
CN116121682A
Zinc spangle adjusting structure of aluminum-zinc plated steel plate
CN222935470U