A high resistivity silicon carbide single crystal growth apparatus
By dividing the silicon carbide single crystal growth furnace cavity into a transfer chamber and an isolation chamber, and using a crucible insulation cover control device to transfer the crucible between the two chambers, the problem of high nitrogen content in the growth chamber is solved, and the growth of high-quality, high-resistivity silicon carbide crystals is achieved.
Patent Information
- Application Number
- CN202522301778.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-29
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-10-29
AI Technical Summary
Existing silicon carbide single crystal growth equipment has a high nitrogen content in the growth chamber, which makes it difficult to control the nitrogen concentration in the crystal and affects the realization of high resistivity.
The single crystal growth furnace cavity is divided into a transfer chamber and an isolation chamber. A crucible insulation cover control device is used to transfer the crucible between the two chambers before and after growth. The isolation chamber is isolated from the outside air to maintain a low-nitrogen environment.
This effectively reduced nitrogen adsorption, lowered the nitrogen partial pressure in the growth atmosphere, ensured a suitable growth environment for high resistivity silicon carbide crystals, and improved crystal quality.
Smart Images

Figure CN224997102U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of crystal growth technology, and in particular to a high resistivity silicon carbide single crystal growth apparatus. Background Technology
[0002] High-resistivity silicon carbide (SiC) single crystals, with their wide bandgap, have become an ideal material choice for high-end optics and heat dissipation applications. Their high resistivity ensures extremely low intrinsic carrier concentration, laying the physical foundation for excellent optical transmittance and reliable electrical insulation performance. Compared to traditional materials such as glass-ceramic and quartz, SiC's unique advantages lie in its combination of high specific stiffness, high thermal conductivity, and extremely low coefficient of thermal expansion. This combination enables SiC optical components to achieve both lightweight design and high structural stiffness, while overcoming the thermal distortion problems of traditional optical materials through efficient heat dissipation and low thermal expansion. Furthermore, its high hardness, high thermal stability (melting point approximately 2700°C), high critical breakdown electric field, and good radiation resistance have jointly driven the widespread application of SiC in cutting-edge fields such as high-performance optical windows and high-efficiency heat dissipation substrates.
[0003] At the application level, high-resistivity silicon carbide (SiC) single crystals, with their unique thermo-mechanical-optical integrated properties, have become a key material driving development in multiple fields. In high-end optical systems, it is widely used in the manufacture of space telescope primary mirrors, high-energy laser mirrors, and precision optical platforms. Its high stiffness and lightweight characteristics effectively improve the system's natural frequency and reduce load weight, while the perfect combination of high thermal conductivity and low coefficient of thermal expansion ensures that optical components maintain extremely high surface accuracy and dimensional stability under thermal loads. Meanwhile, in the field of efficient thermal management, high-resistivity SiC, as a new generation of heat dissipation substrate and packaging material, directly solves the heat dissipation bottleneck of high-power GaN RF devices, laser diodes, and advanced power modules. Its excellent thermal conductivity ensures efficient heat dissipation, significantly improving system power density and operational reliability.
[0004] In the preparation of silicon carbide (SiC) single crystals, precise control of nitrogen (N) impurity content is crucial for achieving its high-end applications. While nitrogen doping imparts n-type conductivity to silicon carbide, it also imposes multiple limitations on its high-end applications: free electrons not only degrade the material's high resistivity, affecting radio frequency applications, but also reduce optical transmittance through free carrier absorption and weaken its intrinsic high thermal conductivity as phonon scattering centers, thus limiting its applications in fields such as optical windows and efficient heat dissipation. To ensure the performance of silicon carbide single crystals, the nitrogen concentration must be controlled at <1×10¹. 6Below cm⁻³. Achieving low nitrogen concentration through optimized PVT growth processes has become a key technological path to improve the overall performance of SiC. However, current silicon carbide growth processes require a large number of crucibles, heaters, support components made of graphite, and insulation components made of carbon fiber. Due to the inherent porous nature of carbon materials, they easily adsorb large amounts of nitrogen atoms from the air when in contact with air, forming a "nitrogen adsorption pool." These adsorbed nitrogen atoms on the walls are difficult to completely desorb through vacuuming. During the crystal growth stage, these adsorbed nitrogen gases are slowly desorbed and released under the continuous drive of the high-temperature thermal field, continuously polluting the growth atmosphere and becoming an uncontrolled secondary nitrogen source. This makes it difficult for the partial pressure of gaseous nitrogen to quickly drop to the expected target, resulting in a persistently high nitrogen concentration in the crystal, which seriously hinders the achievement of its high resistivity target. In summary, effective improvement measures are urgently needed to reduce nitrogen adsorption in the material, provide a good low-nitrogen environment, and grow high-quality, high-resistivity silicon carbide single crystals. Utility Model Content
[0005] This application provides a high resistivity silicon carbide single crystal growth apparatus to solve the problem of high nitrogen content in the growth chamber of existing silicon carbide single crystal growth apparatuses.
[0006] The high resistivity silicon carbide single crystal growth apparatus provided in this application has a single crystal growth furnace chamber divided into a transfer chamber and an isolation chamber, wherein: The isolation chamber is a sealed cavity enclosed by an insulation layer and an insulation cover. A crucible and a heater fitted outside the crucible are installed inside the isolation chamber. The top of the transfer chamber is equipped with a channel gate cover; The single crystal growth apparatus is also equipped with a crucible insulation cover control device. The crucible insulation cover control device is used to open the insulation cover and transfer the crucible from the transfer chamber to the isolation chamber before silicon carbide single crystal growth, when the pressure values in both the transfer chamber and the isolation chamber reach a preset value, and then close the insulation cover; and after silicon carbide single crystal growth is completed, the insulation cover is opened, the crucible is taken from the isolation chamber to the transfer chamber, and then the insulation cover is closed.
[0007] Preferably, the crucible insulation cover control device includes a crucible transport device and an insulation cover lifting arm, wherein: The bottom of the insulation cover lifting arm is equipped with a suction cup, which is used to remove the insulation cover from the insulation layer and to install the insulation cover onto the insulation layer. The crucible transport device is used to transport the crucible between the isolation chamber and the transfer chamber.
[0008] Preferably, the crucible transport device includes a rotating support arm, a tray, and a support rod, wherein: The rotating support arm is disposed in the transfer chamber; The tray is located at one end of the support rod and is used to support the bottom of the crucible, and can push the crucible to move axially.
[0009] Optionally, the insulation layer includes an insulation bucket and an insulation ring disposed on the top of the insulation bucket, wherein the insulation ring and the insulation cover have the same thickness.
[0010] Optionally, the rotating support arm includes a first rotating support arm and a second rotating support arm, wherein: The first rotating support arm and the second rotating support arm are arranged opposite to each other in the transfer chamber; Both the first and second rotating support arms include a rotating shaft and a rotating rod. The rotating shaft is fixed to the inner wall of the transfer chamber, and one end of the rotating rod is rotatably connected to the rotating shaft, while the other end is used to support the bottom of the crucible.
[0011] Optionally, the heater is a resistance heater.
[0012] Optionally, both the transfer chamber and the isolation chamber are equipped with an inert gas introduction module.
[0013] Optionally, a stainless steel metal layer is provided on the top of the insulation layer and the insulation cover.
[0014] This application provides a high-resistivity silicon carbide single crystal growth apparatus. The single crystal growth furnace chamber is divided into a transfer chamber and an isolation chamber. The isolation chamber is a sealed cavity enclosed by an insulation layer and an insulation cover. A crucible and a heater surrounding the crucible are installed inside the isolation chamber. A channel gate cover is installed on the top of the transfer chamber. The single crystal growth apparatus also includes a crucible insulation cover control device. Before silicon carbide single crystal growth, when the pressure values in both the transfer chamber and the isolation chamber reach preset values, the insulation cover is opened using the crucible insulation cover control device, and the crucible is transferred from the transfer chamber to the isolation chamber. The insulation cover is then closed. After silicon carbide single crystal growth is completed, the insulation cover is opened again using the crucible insulation cover control device, and the crucible is transferred from the isolation chamber to the transfer chamber. The insulation cover is then closed. Finally, the channel gate cover is opened to remove the crucible from the transfer chamber, and then the channel gate cover is closed again. Through the above design, the isolation chamber can be isolated from the outside air, thereby keeping the nitrogen content in the isolation chamber at a low level. This reduces the time required to remove nitrogen from the silicon carbide crystal growth device, reduces nitrogen removal costs, and provides a good growth environment for the preparation of optical-grade high resistivity silicon carbide crystals. Attached Figure Description
[0015] To more clearly illustrate the technical solution of this application, the drawings used in the embodiments will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0016] Figure 1 This is a first structural schematic diagram of the high resistivity silicon carbide single crystal growth apparatus in this application.
[0017] Figure 2 This is a schematic diagram of the second structure of the high resistivity silicon carbide single crystal growth apparatus in this application. Detailed Implementation
[0018] To enable those skilled in the art to better understand the technical solutions in this application, the technical solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of this application.
[0019] In some technologies, the graphite components in the single crystal growth chamber easily adsorb nitrogen from the air, making it difficult to remove nitrogen during single crystal growth and resulting in high nitrogen content in the grown silicon carbide single crystals. To solve this technical problem, this application provides a high resistivity silicon carbide single crystal growth apparatus. The structure of each part of the high resistivity silicon carbide single crystal growth apparatus is described below.
[0020] like Figure 1 and 2 As shown in the figure of the high resistivity silicon carbide single crystal growth apparatus, in this embodiment of the application, the growth chamber of the silicon carbide single crystal growth furnace is divided into an upper and lower transfer chamber 1 and an isolation chamber 2.
[0021] The transfer chamber 1 can be made of stainless steel shell, and the top of the transfer chamber 1 is provided with a channel gate cover 10. The channel gate cover 10 can also be made of stainless steel, but is not limited to stainless steel. The sealing method can be designed according to actual needs.
[0022] The isolation chamber 2 is a sealed cavity enclosed by an insulation layer 40 and an insulation cover 30. During single crystal growth, a crucible 50 and a heater 60, which is fitted over the crucible 50, are placed inside the isolation chamber 2. The crucible 50 is used to hold silicon carbide powder and a seed crystal; the heater 60 is used to heat the graphite crucible, and the heating method can be induction heating or resistance heating. Therefore, the specific structure and components of the heater 60 can be designed according to its heating method. Since silicon carbide single crystal growth is carried out at high temperatures, the insulation layer 40 and the insulation cover 30 serve both to insulate the crucible 50 and to form a sealed cavity.
[0023] The insulation layer 40 can be a one-piece structure or composed of multiple components. In this embodiment, in order to balance the sealing effect and material cost, the insulation layer 40 is set to be composed of an insulation bucket 42 and an insulation ring 41 set on the top of the insulation bucket. The insulation ring 41 and the insulation cover 30 have the same thickness, that is, the insulation ring 41 and the insulation cover 30 can be made of the same material.
[0024] Since thermal insulation materials are generally made of porous graphite felt and other materials, in order to ensure their sealing effect, other sealing materials, such as stainless steel, can be wrapped around the top of the thermal insulation layer 40 and the thermal insulation cover 30, as well as the outer periphery of the thermal insulation layer 40.
[0025] When the insulation cover 30 is opened, the transfer chamber 1 and the isolation chamber 2 form a connected space; when the insulation cover 30 is fastened onto the insulation layer 40, the transfer chamber 1 and the isolation chamber 2 form two independent sealed chambers. By setting independent vacuum modules in the transfer chamber 1 and the isolation chamber 2, the internal pressure environment can be controlled, and inert gas introduction modules can be set separately to achieve inert gas doping.
[0026] Before silicon carbide single crystal growth, when the pressure values in both transfer chamber 1 and isolation chamber 2 reach preset values, the insulation cover 30 is opened, the crucible 50 is transferred from transfer chamber 1 to isolation chamber 2, and then the insulation cover 30 is closed. After silicon carbide single crystal growth is completed, the insulation cover 30 is opened, the crucible 50 is removed from isolation chamber 2 to transfer chamber 1, and then the insulation cover 30 is closed. In this way, isolation chamber 2 can be isolated from the outside air, thus maintaining a consistently low nitrogen content within it. This reduces the time required for nitrogen removal from the silicon carbide crystal growth apparatus, lowers nitrogen removal costs, and provides a favorable growth environment for the preparation of optical-grade high-resistivity silicon carbide crystals.
[0027] To facilitate the transport of crucible 50 between transfer chamber 1 and isolation chamber 2, a crucible insulation cover control device is also provided within the single crystal growth apparatus. This device may include a crucible transport device and an insulation cover lifting arm 22 that cooperate with each other. The bottom of the insulation cover lifting arm 22 is equipped with a suction cup for removing the insulation cover 30 from the insulation layer 40 and for installing the insulation cover 30 onto the insulation layer 40. The crucible transport device is used to transport crucible 50 between isolation chamber 2 and transfer chamber 1.
[0028] The crucible transport device can be designed using robotic arms or other methods. In this embodiment, to adjust the relative position of the crucible 50 and the heater 60 during the crystal growth process, the crucible transport device includes a rotating support arm 21, a tray 23, and a support rod 24. The rotating support arm 21 is disposed inside the transfer chamber 1. The tray 23 is disposed at one end of the support rod 24 and is used to support the bottom of the crucible 50, and can push the crucible 50 to move axially. The rotating support arm 21 includes a first rotating support arm 211 and a second rotating support arm 222, which are disposed opposite to each other inside the transfer chamber 1. Both the first rotating support arm 211 and the second rotating support arm 222 include a rotating shaft and a rotating rod. The rotating shaft is fixed to the inner wall of the transfer chamber 1, and one end of the rotating rod is rotatably connected to the rotating shaft, while the other end is used to support the bottom of the crucible 50.
[0029] The apparatus provided in this example will be further described below in conjunction with a specific crystal growth process.
[0030] S01: The prepared silicon carbide powder and seed crystal are loaded into the graphite crucible 50.
[0031] S02: Preparing the crucible 50 for loading: Keep the insulation cover 30 closed, control the rotating support arm 21 to rotate to the designated position, that is, adjust the relative position of the first rotating support arm 211 and the second rotating support arm 222 by controlling the rotation angle of the first rotating support arm 211 and the second rotating support arm 222 so that they can support the crucible 50; open the channel gate cover 10, put the crucible 50 on the rotating support arm 21, and close the channel gate cover 10.
[0032] S03: Simultaneously evacuate transfer chamber 1 and isolation chamber 2 until the pressure in both chambers reaches the preset pressure value. The preset pressure in both chambers can be set to be equal, or the pressure in isolation chamber 2 can be slightly higher than that in transfer chamber 1. Then, inert gas is introduced into transfer chamber 1 and isolation chamber 2 to replace the air inside. Specifically, the above air replacement procedure can be set to be executed multiple times to remove nitrogen from the chambers as much as possible.
[0033] S04: Control the lifting arm 22 of the insulation cover to open the insulation cover 30 and move the insulation cover 30 to a position that does not obstruct the crucible 50 from being placed into the isolation chamber 2.
[0034] S05: Control the tray 23 and support rod 24 to move towards the crucible 50 until the tray 3 touches the bottom of the crucible 50, then control the support rod 24 to move downward, driving the crucible 50 to the designated position in the isolation chamber 2, and close the heat preservation cover 30.
[0035] S06: The crucible 50 is heated by the heater 60, allowing the crystal inside the crucible 50 to grow under suitable temperature conditions. During crystal growth, the position of the crucible 50 relative to the resistance heater 5 can be changed to continuously provide a stable temperature gradient. Additionally, before heating the crucible, the isolation chamber 2 can be evacuated and nitrogen removed again as needed.
[0036] S07: After the crystal growth is completed, stop heating and wait for the temperature of the isolation chamber 2 to reach the preset temperature. When the internal pressure of the isolation chamber 2 and the transfer chamber 1 are equal or the internal pressure of the isolation chamber 2 is slightly greater than that of the transfer chamber 1, open the heat preservation cover 30. Control the tray 23 and the support rod 24 to transport the crucible 50 from the isolation chamber 2 to the transfer chamber 1. Control the rotating support arm 21 to support the crucible 50. Then, control the tray 23 and the support rod 24 to move back to the isolation chamber 2, close the heat preservation cover 30, and restore the isolation chamber 2 to a sealed state.
[0037] S08: Open the channel gate cover 10 and remove the crucible 50 from the transfer chamber 1. At this point, the cycle of loading, growing, and opening a silicon carbide crystal is complete.
[0038] As can be seen from the above crystal growth process, by setting up the transfer chamber 1 and the corresponding crucible transport components, the isolation chamber 2 is not in direct contact with the outside atmosphere, which can greatly reduce the amount of nitrogen adsorption in the cavity of the isolation chamber 2, thus providing a guarantee for the growth of high resistivity silicon carbide crystals, especially optical grade silicon carbide crystals.
[0039] The above detailed embodiments further illustrate the purpose, technical solution, and beneficial effects of the embodiments of this application. It should be understood that the above are merely specific embodiments of the embodiments of this application and are not intended to limit the protection scope of the embodiments of this application. Any modifications, equivalent substitutions, improvements, etc., made on the basis of the technical solutions of the embodiments of this application should be included within the protection scope of the embodiments of this application.
Claims
1. A high-resistivity silicon carbide single crystal growth apparatus, characterized in that, The single crystal growth furnace cavity is divided into a transfer chamber (1) and an isolation chamber (2), wherein: The isolation chamber (2) is a sealed cavity formed by the insulation layer (40) and the insulation cover (30). The isolation chamber (2) is used to set up the crucible (50) and the heater (60) sleeved on the outside of the crucible (50). The top of the transfer chamber (1) is provided with a channel gate cover (10). The single crystal growth apparatus is also equipped with a crucible insulation cover control device. The crucible insulation cover control device is used to open the insulation cover (30) and send the crucible (50) from the transfer chamber (1) to the isolation chamber (2) before silicon carbide single crystal growth, when the pressure values in the transfer chamber (1) and the isolation chamber (2) both reach the preset value, and then close the insulation cover (30); and after the silicon carbide single crystal growth is completed, to open the insulation cover (30), send the crucible (50) from the isolation chamber (2) to the transfer chamber (1), and then close the insulation cover (30).
2. The high resistivity silicon carbide single crystal growth apparatus according to claim 1, characterized in that, The crucible insulation cover control device includes a crucible transport device and an insulation cover lifting arm (22), wherein: The bottom of the heat preservation cover lifting arm (22) is provided with a suction cup, which is used to remove the heat preservation cover (30) from the heat preservation layer (40) by means of the suction cup, and to install the heat preservation cover (30) on the heat preservation layer (40) by means of the suction cup; The crucible transport device is used to transport the crucible (50) between the isolation chamber (2) and the transfer chamber (1).
3. The high resistivity silicon carbide single crystal growth apparatus according to claim 2, characterized in that, The crucible transport device includes a rotating support arm (21), a tray (23), and a support rod (24), wherein: The rotating support arm (21) is disposed inside the transfer chamber (1); The tray (23) is disposed at one end of the support rod (24) for supporting the bottom of the crucible (50) and for pushing the crucible (50) to move axially.
4. The high resistivity silicon carbide single crystal growth apparatus according to claim 1, characterized in that, The insulation layer (40) includes an insulation bucket (42) and an insulation ring (41) disposed on the top of the insulation bucket. The insulation ring (41) and the insulation cover (30) have the same thickness.
5. The high resistivity silicon carbide single crystal growth apparatus according to claim 3, characterized in that, The rotating support arm (21) includes a first rotating support arm (211) and a second rotating support arm (222), wherein: The first rotating support arm (211) and the second rotating support arm (222) are arranged opposite to each other in the transfer chamber (1); The first rotating support arm (211) and the second rotating support arm (222) both include a rotating shaft and a rotating rod. The rotating shaft is fixed to the inner wall of the transfer chamber (1). One end of the rotating rod is rotatably connected to the rotating shaft, and the other end is used to support the bottom of the crucible (50).
6. The high resistivity silicon carbide single crystal growth apparatus according to claim 1, characterized in that, The heater (60) is a resistance heater.
7. The high resistivity silicon carbide single crystal growth apparatus according to claim 1, characterized in that, Both the transfer chamber (1) and the isolation chamber (2) are equipped with inert gas inlet modules.
8. The high resistivity silicon carbide single crystal growth apparatus according to claim 1, characterized in that, The top of the insulation layer (40) and the insulation cover (30) are provided with a stainless steel metal layer.