Fluidized bed boiler for biomass
By setting an anchoring structure composed of multiple pins and an anti-wear coating on the tube bundle of the biomass fluidized bed boiler, the problems of anti-wear cover plate detachment and coating peeling caused by alkali metal corrosion and ash impact are solved, achieving a longer service life and higher safety.
Patent Information
- Application Number
- CN202522571572.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-03
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-12-03
AI Technical Summary
The superheater tube walls of biomass fluidized bed boilers are susceptible to corrosion from alkali metal compounds and wear caused by ash impact. Traditional anti-wear technologies have limited effectiveness in biomass environments, leading to easy detachment of anti-wear covers and easy peeling of sprayed coatings, which affects the safe operation of the boiler.
Multiple anchoring structures are installed on the frontal tube bundle, forming a robust network of pins. An anti-wear coating covers the entire frontal tube bundle and anchoring structure surface, forming a distributed support system that enhances the adhesion between the coating and the tube bundle and prevents localized corrosion failure and peeling.
It significantly extends the service life of the wear-resistant coating, improves the reliability and safety of the structure, reduces maintenance costs, and enhances the operational safety of the boiler.
Smart Images

Figure CN224999634U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of biomass combustion boiler technology, specifically relating to a biomass fluidized bed boiler. Background Technology
[0002] Biomass fluidized bed boilers have been widely used in cogeneration and district heating in recent years due to the environmental friendliness and renewability of their fuels (such as zero-carbon emission fuels like straw and rice husks). However, in actual production and operation, the ash content of conventional biomass fuels (taking typical agricultural waste as an example) is generally as high as 8-20%, far exceeding the 5-10% of bituminous coal. This ash not only contains hard particles such as SiO2 and Al2O3, but more importantly, it contains a large amount of alkali metal compounds—K2O and Na2O can account for 8-15% of the ash by mass, and some rice husk ash can even reach as high as 18%.
[0003] The bed temperature of fluidized bed boilers is generally between 800-950℃. When the boiler operates in a high-temperature environment above 600℃, the aforementioned alkali metals will chemically react with the Fe2O3 oxide layer on the superheater tube wall to generate low-melting-point eutectic phases such as K2Fe2O4 and NaFeO2. The melting points of these compounds are generally below 700℃. This process leads to the formation of a loose corrosion layer on the tube wall surface, exposing the base metal to the high-velocity flue gas. At the same time, the flow velocity of the gas-solid two-phase flow in the fluidized bed is usually maintained at 2-5 m / s, and the ash particles carried by it continuously impact the tube wall, causing a synergistic destructive effect of corrosion and wear. Studies have shown that this synergistic effect can make the wear rate of superheater tubes 3-5 times that of pure mechanical wear, and some power plants have even seen cases where tube bundles need to be replaced in less than 8000 hours of operation.
[0004] More seriously, the anti-wear technology of traditional coal-fired boilers has limited effectiveness in biomass environments. This is especially true for semi-tower biomass fluidized bed boilers, where some of the convective heating surfaces are located above the furnace. Flue gas flows upwards across these surfaces, and when the commonly used anti-wear covers are placed on the tube bundles on the windward side, the gap between the cover and the tube wall is often larger than the gap between the cover and the tail flue heating surface due to production, installation, and inversion. This makes the gap more susceptible to ash blockage, creating localized high-temperature corrosion hotspots. In actual operation, the covers often detach before the normal operating time is reached. If not replaced promptly, tube rupture on the heating surface can occur, affecting the unit's operational safety. Another method used in the industry is to spray a coating onto the highly worn heating surfaces. However, based on practical experience, conventional coatings will generate β-Al₂O₃ (Na₂O·11Al₂O₃) under alkali metal vapor permeation, with a volume expansion rate of up to 12%. This volume expansion accelerates coating peeling.
[0005] Therefore, there is an urgent need to provide a biomass fluidized bed boiler with a longer service life. Utility Model Content
[0006] The purpose of this invention is to at least solve the problems of corrosion and subsequent detachment of the wear-resistant cover plates on the heating surfaces of existing biomass fluidized bed boilers, and the easy peeling of the sprayed coating. This objective is achieved through the following technical solution: The first aspect of this utility model discloses a biomass fluidized bed boiler, comprising: Furnace body; Multiple flow-facing tube bundles are disposed inside the furnace body and arranged at intervals along a direction perpendicular to the incoming flow. An anchoring structure, each of the upstream face tube bundles is provided with multiple anchoring structures, the multiple anchoring structures on each of the upstream face tube bundles are spaced apart along the axial direction of the upstream face tube bundles, each anchoring structure includes multiple pins, the multiple pins in each anchoring structure are arranged along the circumference of the upstream face tube bundles; Abrasion-resistant coating is applied to the surfaces of the frontal tube bundle and the anchoring structure.
[0007] Traditional solutions use isolated abrasion-resistant plates or protective tiles, whose weld points to the base pipe wall are easily corroded by high-temperature flue gas and moisture, leading to detachment due to reduced strength. In this solution, multiple anchoring structures are installed on the upstream pipe bundle, forming a robust network of pins. These pins are tightly connected to the upstream pipe bundle itself, forming a distributed, multi-anchor support system. Even if a single connection point corrodes under extreme conditions, the stability of the entire structure remains intact. The impact of dust particles is effectively distributed by other pins, greatly preventing abnormal detachment of the abrasion-resistant coating due to localized corrosion failure and improving structural reliability. Furthermore, in traditional processes, the abrasion-resistant coating is directly applied to the smooth pipe wall, making it prone to peeling off in large sheets due to differences in thermal expansion coefficients and continuous particle impact. This solution covers the entire surface of the upstream pipe bundle and anchoring structures with the abrasion-resistant coating. The pins are embedded within the coating, creating a strong anchoring effect. This significantly increases the bonding strength between the wear-resistant coating and the frontal tube bundle, effectively transferring and dispersing the shear stress and impact force experienced by the coating throughout the rigid structure. Therefore, the wear-resistant coating is no longer an isolated film, but rather integrated with the frontal tube bundle and anchoring structure, resulting in a significant improvement in its peel resistance and a significantly extended service life.
[0008] In addition, the biomass fluidized bed boiler of this utility model may also have the following additional technical features: In some embodiments of this utility model, the pin includes a connecting piece and two arc-shaped pieces. The two arc-shaped pieces are connected side by side to one side of the arc-shaped pieces, and the two arc-shaped pieces are bent in opposite directions. The side of the connecting piece away from the arc-shaped pieces is connected to the tube wall of the frontal tube bundle.
[0009] In some embodiments of this utility model, the connecting piece is welded to the frontal tube bundle.
[0010] In some embodiments of this utility model, in each of the anchoring structures, the included angle α between two adjacent pins is 120°.
[0011] In some embodiments of this utility model, on each of the frontal tube bundles, the pins in two adjacent anchoring structures are staggered, and the stagger angle β is 60°.
[0012] In some embodiments of this utility model, the interval between two adjacent anchoring structures on each of the frontal tube bundles is 80mm to 100mm.
[0013] In some embodiments of this utility model, the pin is made of stainless steel.
[0014] In some embodiments of this utility model, the wear-resistant coating is a corundum plastic coating.
[0015] In some embodiments of this utility model, the wear-resistant coating includes a first wear-resistant coating, a second wear-resistant coating, and a third wear-resistant coating, wherein the first wear-resistant coating, the second wear-resistant coating, and the third wear-resistant coating are sequentially applied to the pipe wall of the frontal tube bundle.
[0016] In some embodiments of this utility model, the thickness of the first anti-wear coating is 10mm to 20mm, the sum of the thicknesses of the second anti-wear coating and the first anti-wear coating is 30mm to 40mm, and the sum of the thicknesses of the first anti-wear coating, the second anti-wear coating and the third anti-wear coating is 50mm to 60mm. Attached Figure Description
[0017] Various other advantages and benefits will become apparent to those skilled in the art upon reading the following detailed description of preferred embodiments. The accompanying drawings are for illustrative purposes only and are not intended to limit the scope of the invention. Furthermore, the same reference numerals denote the same parts throughout the drawings. In the drawings: Figure 1 A schematic cross-sectional view of a partial structure of a biomass fluidized bed boiler according to an embodiment of the present invention is shown. Figure 2 for Figure 1 Schematic diagram of the cross section at point AA; Figure 3 A schematic diagram of the structure of a pin according to an embodiment of the present invention is shown; Figure 4 A schematic diagram of the structure of a pin (unbent) according to an embodiment of the present invention is shown. Figure 5 An assembly diagram of the frontal tube bundle and anchoring structure according to an embodiment of the present invention is shown schematically. Figure 6 for Figure 1 Schematic diagram of the cross section at point BB; Figure 7 for Figure 2 A magnified view of a portion of point A in the middle.
[0018] The labels in the attached diagram are as follows: 100. Furnace body; 200. Frontal tube bundle; 300. Anchoring structure; 310. Pin; 311. Connecting piece; 312. Arc-shaped piece; 400. Outer contour of the anti-wear coating. Detailed Implementation
[0019] Exemplary embodiments of the present disclosure will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of the present disclosure are shown in the drawings, it should be understood that the present disclosure may be implemented in various forms and should not be limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the disclosure to those skilled in the art.
[0020] It should be understood that the terminology used herein is for the purpose of describing particular exemplary embodiments only and is not intended to be limiting. Unless the context clearly indicates otherwise, the singular forms “a,” “an,” and “described” as used herein may also include the plural forms. The terms “comprising,” “including,” “containing,” and “having” are inclusive and therefore indicate the presence of the stated features, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, steps, operations, elements, components, and / or combinations thereof. The method steps, processes, and operations described herein are not construed as requiring them to be performed in a particular order described or illustrated unless the order of performance is explicitly indicated. It should also be understood that additional or alternative steps may be used.
[0021] Although terms such as first, second, third, etc., may be used in this document to describe multiple elements, components, regions, layers, and / or segments, these elements, components, regions, layers, and / or segments should not be limited by these terms. These terms may be used only to distinguish one element, component, region, layer, or segment from another. Unless the context clearly indicates otherwise, terms such as "first," "second," and other numerical terms used herein do not imply order or sequence. Therefore, the first element, component, region, layer, or segment discussed below may be referred to as the second element, component, region, layer, or segment without departing from the teachings of the exemplary embodiments.
[0022] For ease of description, spatial relative terms may be used in the text to describe the relationship of one element or feature relative to another element or feature, as shown in the figure. These relative terms include, for example, "inside," "outside," "middle," "outer," "below," "below," "above," "over," etc. Such spatial relative terms are intended to include different orientations of the device in use or operation, other than those depicted in the figure. For example, if the device in the figure is flipped, an element described as "below other elements or features" or "below other elements or features" would subsequently be oriented "above other elements or features" or "above other elements or features." Therefore, the example term "below" can include both upper and lower orientations.
[0023] Figure 1 A schematic cross-sectional view of a partial structure of a biomass fluidized bed boiler according to an embodiment of the present invention is shown. Figure 2 for Figure 1 Schematic diagram of the cross section at point AA; Figure 3 A schematic diagram of the structure of a pin according to an embodiment of the present invention is shown; Figure 4 A schematic diagram of the structure of a pin (unbent) according to an embodiment of the present invention is shown. Figure 5 An assembly diagram of the frontal tube bundle and anchoring structure according to an embodiment of the present invention is shown schematically; as follows: Figures 1 to 5As shown, this utility model proposes a biomass fluidized bed boiler, including a furnace body 100, multiple flow-facing tube bundles 200, anchoring structures 300, and an anti-wear coating; the multiple flow-facing tube bundles 200 are disposed inside the furnace body 100 and arranged at intervals along a direction perpendicular to the incoming flow; each flow-facing tube bundle 200 is provided with multiple anchoring structures 300, which are spaced apart along the axial direction of the flow-facing tube bundle 200; each anchoring structure 300 includes multiple pins 310, which are arranged circumferentially along the flow-facing tube bundle 200; the anti-wear coating covers the surfaces of the flow-facing tube bundles 200 and the anchoring structures 300.
[0024] Traditional solutions use isolated abrasion-resistant plates or protective tiles, whose weld points to the base pipe wall are easily corroded by high-temperature flue gas and moisture, leading to detachment due to reduced strength. In this solution, multiple anchoring structures 300 are installed on the upstream pipe bundle 200, and each anchoring structure 300 is a robust network composed of multiple pins 310. These pins 310 are tightly connected to the upstream pipe bundle 200 itself, forming a distributed, multi-anchor support system. Even if a single connection point corrodes due to extreme operating conditions, the stability of the entire structure will not be compromised. The impact of dust particles is effectively distributed by other pins 310, greatly avoiding abnormal detachment of the abrasion-resistant coating caused by localized corrosion failure, thus improving the reliability of the structure. Furthermore, in traditional processes, the abrasion-resistant coating is directly applied to the smooth pipe wall, which easily peels off in patches due to differences in thermal expansion coefficients and continuous particle impact. This solution covers the entire surface of the upstream pipe bundle 200 and the anchoring structures 300 with the abrasion-resistant coating. The pin 310 is embedded inside the abrasion-resistant coating, forming a strong anchoring effect. This greatly increases the bonding force between the abrasion-resistant coating and the upstream tube bundle 200, effectively transferring and dispersing the shear stress and impact force on the coating to the entire rigid structure. Therefore, the abrasion-resistant coating is no longer an isolated film, but is integrated with the upstream tube bundle 200 and the anchoring structure 300, significantly improving its peel resistance and extending its service life.
[0025] Further, see Figure 3 The pin 310 includes a connecting piece 311 and two arc-shaped pieces 312. The two arc-shaped pieces 312 are connected side by side to one side of the arc-shaped piece 312, and the two arc-shaped pieces 312 are bent in opposite directions. The side of the connecting piece 311 away from the arc-shaped piece 312 is connected to the pipe wall of the frontal tube bundle 200.
[0026] The pins 310 employ this structural design, where, when the abrasion-resistant coating is applied, the coating fully fills the space between adjacent pins 310 and the grooves formed by the arc-shaped pieces 312. After the abrasion-resistant coating cures, the two opposing arc-shaped pieces 312 act like built-in anchors, forming a robust interlocking structure with the coating. This design significantly enhances the resistance to peeling the abrasion-resistant coating from the pins 310 surface, ensuring that the coating maintains stable adhesion even under prolonged high-speed material flow impact.
[0027] Furthermore, the connecting piece 311 is welded to the frontal tube bundle 200.
[0028] Welding can achieve a high level of structural integrity and connection strength, preventing the anchor structure 300 from loosening or falling off due to long-term vibration or impact, thus ensuring the long-term stability of the anchor structure 300.
[0029] Furthermore, the pin 310 is made of stainless steel.
[0030] Stainless steel structures possess excellent high-temperature resistance and corrosion resistance, effectively preventing corrosion-induced catalytic cracking or breakage during long-term use, and avoiding the peeling of the entire anti-wear coating due to the failure of the anchoring structure 300 itself. Furthermore, stainless steel structures maintain high strength at high temperatures and possess good weldability and processability. Preferably, the pin 310 can be made of 06Cr19Ni10 or austenitic stainless steel, etc. See also Figure 4 During processing, one end of the steel plate is first cut along its centerline, and then the two separated parts are bent into an arc-shaped piece 312.
[0031] Furthermore, Figure 5 This illustrates the distribution of multiple pins 310 within a single anchoring structure 300 on the upstream tube bundle 200. See also... Figure 5 In each anchoring structure 300, the included angle α between two adjacent pins 310 is 120°.
[0032] In each anchoring structure 300, the included angle between two adjacent pins 310 should ensure a balance between anchoring density and material strength. If the included angle α is too small, the pins 310 will be too densely packed, potentially leading to weld points that are too close together and causing the heat-affected zone to overlap. Simultaneously, excessively dense pins 310 will create excessive rigidity locally, limiting the abrasion-resistant coating's ability to withstand minor deformations during thermal expansion and contraction, easily causing internal cracks in the abrasion-resistant coating. If the included angle α is too large, the anchoring points will be too sparse, and the span between the pins 310 will be too large. The abrasion-resistant coating will lack sufficient internal structural support, making it prone to peeling off from the anchoring structure 300 under continuous impact, weakening the overall anchoring effect. Understandably, when the included angle α between two adjacent pins 310 is 120°, each anchoring structure 300 includes three pins 310. In other embodiments, the included angle α between two adjacent pins 310 can be set to 180°, 90° or 60° as needed, and the number of pins 120 can be two, four or six respectively.
[0033] Furthermore, Figure 6 for Figure 1 A schematic diagram of the cross-section at point BB. Figure 6 This illustrates the distribution of pins 310 in two adjacent anchoring structures 300 on a certain frontal tube bundle 200. Specifically, on each frontal tube bundle 200, the pins 310 in two adjacent anchoring structures 300 are staggered, and the stagger angle β is 60°.
[0034] When the pins in adjacent anchoring structures are staggered at 60°, they interweave to form a uniform and dense support matrix on the surface of the frontal tube bundle 200, eliminating support blind spots beneath the wear-resistant coating and effectively preventing deformation or tearing of the wear-resistant coating due to insufficient local support. Furthermore, this design significantly optimizes the stress state of the wear-resistant coating. Aligned anchor points easily form penetrating stress concentration lines, along which the wear-resistant coating is prone to overall peeling under impact. The staggered layout forces impact forces and thermal stresses to dissipate and redistribute along more tortuous and complex paths within the wear-resistant coating, thus successfully avoiding the generation of fatal through cracks and mitigating the risk of large-area peeling into controllable localized wear. In other embodiments, the staggered angle β can be set according to the included angle α.
[0035] Furthermore, Figure 7 for Figure 2 A magnified view of a portion at point A. See also... Figure 7 The interval between two adjacent anchoring structures 300 is 80mm to 100mm.
[0036] Understandably, if the gap between two adjacent anchoring structures 300 is too large, the wear-resistant coating, lacking internal support, is prone to cracking and peeling off from the pipe wall. If the gap is too small, it will not only increase material and welding costs, but also cause significant thermal stress within the wear-resistant coating due to uneven expansion and contraction during boiler start-up and shutdown temperature cycles, which will also lead to cracking of the wear-resistant coating. For example, the gap between two adjacent anchoring structures 300 may be 80mm, 85mm, 90mm, 95mm, or 100mm, etc.
[0037] Furthermore, the abrasion-resistant coating is a corundum plastic coating.
[0038] Corundum plastic is an unshaped refractory material constructed by ramming, vibration, or pressing. It is made by mixing refractory aggregates, powders, binders, and additives. Its compressive strength can reach 60 MPa, and its maximum refractory temperature exceeds 1600℃, making it very suitable for industrial equipment parts such as fluidized bed boilers that are subject to high-temperature wear and coal ash impact.
[0039] Furthermore, the abrasion-resistant coating has multiple layers.
[0040] Multi-layer application offers significant advantages over single, thick-layer application. Each layer is more easily compacted, more effectively encapsulating the complex 310 pin structure and preventing defects such as air bubbles or voids. Furthermore, layered application allows for phased quality checks and control of each layer, ensuring the overall density and uniformity of the final coating and guaranteeing the achievement of its designed performance.
[0041] Furthermore, the wear-resistant coating includes a first wear-resistant coating, a second wear-resistant coating, and a third wear-resistant coating, which are sequentially applied to the pipe wall of the flow-facing pipe bundle 200.
[0042] In other words, in this technical solution, the anti-wear coating is applied to the upstream pipe bundle 200 and the anchoring structure 300 in three stages. In other embodiments, the anti-wear coating may also be applied to the upstream pipe bundle 200 and the anchoring structure 300 in two or four stages, depending on the specific application requirements. After the anti-wear coating is applied, the outer contour 400 of the anti-wear coating is as follows: Figure 6 As shown.
[0043] Furthermore, the thickness of the first anti-wear coating is 10mm to 20mm, the sum of the thicknesses of the second and first anti-wear coatings is 30mm to 40mm, and the sum of the thicknesses of the first, second, and third anti-wear coatings is 50mm to 60mm.
[0044] Understandably, the thickness of a single layer should take into account factors such as coating uniformity, curing time, and thermal stress to ensure that the abrasion-resistant coating has sufficient abrasion-resistant thickness, controllable thermal stress, feasible construction technology, and reasonable cost. Optionally, the optimal thickness of each layer can be determined by combining theoretical calculations, simulation analysis, and practical experience.
[0045] Optionally, pneumatic tamping equipment is used to evenly apply the prepared corundum plastic in three layers to the outer surface of the air-facing tube bundle 200. The first layer is 10mm to 20mm thick and covers the root area of the pins 310. High-frequency vibration (28Hz to 32Hz) ensures a tight fit between the material and the tube wall and the pins 310. When the second layer is 30mm to 40mm thick, the compaction of the 120° arc area on the windward side is strengthened, and a cross-tamping process is used to eliminate internal voids. After the final layer reaches the designed thickness of 50mm to 60mm, an arc-shaped scraper is used to streamline the surface and reduce the airflow stripping effect during operation. The entire construction process requires maintaining an ambient temperature ≥10℃, and far-infrared heating is used immediately after the material initially sets for stepped curing treatment, ultimately forming a seamless continuous protective body. This body, together with the pre-embedded pins 310, constitutes a three-dimensional anchoring system, achieving mechanical-thermal dual coupling between the refractory layer and the air-facing tube bundle 200. For example, the thickness of the first anti-wear coating is 15mm, the anti-wear thickness of the second anti-wear coating is 20mm, and the thickness of the third anti-wear coating is 20mm.
[0046] The biomass fluidized bed boiler provided by this technical solution adopts a modular design, which improves maintenance efficiency by 60% and significantly reduces the intensity of maintenance work; the anchoring structure 300 and the anti-wear coating reduce the wear of the heat-receiving frontal tube bundle 200 by more than 80%, effectively eliminating the risk of steam leakage caused by tube wall thinning; while improving the safety of unit operation, this technical solution can reduce annual maintenance costs and provide a more reliable superheater protection solution for biomass power plants.
[0047] The above are merely preferred embodiments of this utility model, but the scope of protection of this utility model is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in this utility model should be included within the scope of protection of this utility model. Therefore, the scope of protection of this utility model should be determined by the scope of the claims.
Claims
1. A biomass fluidized bed boiler, characterized in that, include: Furnace body (100); Multiple flow-facing tube bundles (200) are disposed inside the furnace body (100) and spaced apart in a direction perpendicular to the incoming flow. An anchoring structure (300) is provided on each of the frontal tube bundles (200). The multiple anchoring structures (300) on each of the frontal tube bundles (200) are spaced apart along the axial direction of the frontal tube bundles (200). Each anchoring structure (300) includes multiple pins (310). The multiple pins (310) in each anchoring structure (300) are arranged along the circumferential direction of the frontal tube bundles (200). Abrasion-resistant coating is applied to the surfaces of the frontal tube bundle (200) and the anchoring structure (300).
2. The biomass fluidized bed boiler according to claim 1, characterized in that, The pin (310) includes a connecting piece (311) and two arc-shaped pieces (312). The two arc-shaped pieces (312) are connected side by side to one side of the arc-shaped piece (312), and the two arc-shaped pieces (312) are bent in opposite directions. The side of the connecting piece (311) away from the arc-shaped piece (312) is connected to the tube wall of the frontal tube bundle (200).
3. The biomass fluidized bed boiler according to claim 2, characterized in that, The connecting piece (311) is welded to the frontal tube bundle (200).
4. The biomass fluidized bed boiler according to claim 1, characterized in that, In each of the anchoring structures (300), the included angle α between two adjacent pins (310) is 120°.
5. The biomass fluidized bed boiler according to claim 1, characterized in that, On each of the frontal tube bundles (200), the pins (310) in two adjacent anchoring structures (300) are staggered, and the stagger angle β is 60°.
6. The biomass fluidized bed boiler according to claim 1, characterized in that, On each of the aforementioned frontal tube bundles (200), the interval between two adjacent anchoring structures (300) is 80mm to 100mm.
7. The biomass fluidized bed boiler according to claim 1, characterized in that, The pin (310) is made of stainless steel.
8. The biomass fluidized bed boiler according to claim 1, characterized in that, The wear-resistant coating is a corundum plastic coating.
9. The biomass fluidized bed boiler according to claim 1, characterized in that, The wear-resistant coating includes a first wear-resistant coating, a second wear-resistant coating, and a third wear-resistant coating, which are sequentially applied to the pipe wall of the frontal tube bundle (200).
10. The biomass fluidized bed boiler according to claim 9, characterized in that, The thickness of the first anti-wear coating is 10mm to 20mm, the sum of the thicknesses of the second anti-wear coating and the first anti-wear coating is 30mm to 40mm, and the sum of the thicknesses of the first anti-wear coating, the second anti-wear coating and the third anti-wear coating is 50mm to 60mm.