A multi-layer pole piece and lithium ion battery thereof

By designing a multilayer structure of lithium nickel cobalt manganese aluminum oxide and lithium vanadium iron phosphate on lithium-ion battery electrodes, the low-temperature performance and safety issues of lithium-ion batteries are solved, achieving a balance between high energy density and safety.

CN225002260UActive Publication Date: 2026-11-20YONGKANG HIGH-TECH IND RESEARCH INSTITUTE CO LTD +2
View PDF 0 Cites -1 Cited by

Patent Information

Application Number
CN202522687286.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-18
Publication Date
2026-11-20
Estimated Expiration
2035-12-18

AI Technical Summary

Technical Problem

Lithium-ion batteries experience a sharp decline in charge and discharge efficiency and capacity at low temperatures, and also suffer from low-temperature degradation and safety issues. In particular, the dense lattice structure of phosphate materials leads to a decrease in the lithium-ion diffusion rate, while ternary materials have poor stability and are prone to thermal runaway.

Method used

The electrode adopts a multi-layer electrode structure, with a lithium nickel cobalt manganese aluminum oxide layer and a lithium vanadium iron phosphate layer on the current collector. The lithium nickel cobalt manganese aluminum oxide layer is located in the inner layer to improve low-temperature performance, and the lithium vanadium iron phosphate layer is located in the outer layer to improve safety. The two are prepared by dry process to form a layered structure.

Benefits of technology

It achieves high energy density and safety of lithium-ion batteries in low-temperature environments. The lithium nickel cobalt manganese aluminum oxide layer has low low-temperature degradation, and the lithium vanadium iron phosphate layer has high thermal stability, reducing the risk of thermal runaway and extending cycle life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225002260U_ABST
    Figure CN225002260U_ABST
Patent Text Reader

Abstract

The utility model provides a kind of multilayer pole piece and lithium ion battery thereof, the multilayer pole piece, comprising: current collector, nickel cobalt manganese lithium aluminate layer, vanadium iron lithium phosphate layer, the current collector includes oppositely arranged first surface and second surface;The nickel cobalt manganese lithium aluminate layer is located on the first surface and the second surface;The vanadium iron lithium phosphate layer includes first area;The first area is located on the surface of the nickel cobalt manganese lithium aluminate layer.The multilayer pole piece of the utility model has good low-temperature performance, high energy density, and high safety.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of lithium-ion battery technology, and in particular to a multilayer electrode sheet and its lithium-ion battery. Background Technology

[0002] Lithium-ion batteries boast high energy density and long cycle life, making them widely used in consumer electronics, new energy vehicles, and other fields. However, lithium-ion batteries typically experience significant performance degradation at low temperatures, with charge / discharge efficiency and capacity dropping drastically in low-temperature environments (< -20℃). This deficiency is one of the core pain points faced by lithium-ion batteries in vehicle power applications, directly impacting vehicle range and user experience.

[0003] The rapid degradation of lithium-ion battery performance at low temperatures is primarily due to the fact that low temperatures hinder the migration and reaction of lithium ions. Positive electrode plates using phosphate materials (such as lithium iron phosphate and lithium manganese phosphate) as active materials have a relatively dense crystal structure, causing a sharp decrease in the diffusion rate of lithium ions at low temperatures. This severe low-temperature degradation, coupled with prolonged use in low-temperature environments, can easily lead to lithium dendrite formation, affecting safety. While positive electrode plates using ternary materials or lithium cobalt oxide as active materials are less affected by temperature and exhibit less low-temperature degradation, they suffer from poor stability and are prone to thermal runaway, threatening human safety. Summary of the Invention

[0004] The present invention aims to provide a multilayer electrode to solve the problem that existing electrodes cannot simultaneously meet the requirements of low-temperature performance and safety.

[0005] To solve the above-mentioned technical problems, the technical solution of this utility model is as follows: A multilayer electrode sheet, comprising: A current collector, the current collector comprising a first surface and a second surface disposed opposite to each other; A lithium nickel cobalt manganese aluminum oxide layer is disposed on the first surface and the second surface; A lithium vanadium iron phosphate layer, wherein the lithium vanadium iron phosphate layer includes a first region; the first region is disposed on the surface of the lithium nickel cobalt manganese aluminum oxide layer.

[0006] Preferably, the ratio of the thickness of the lithium nickel cobalt manganese aluminum oxide layer to the thickness of the first region is K, where 0 < K ≤ 0.8. More preferably, 0 < K ≤ 0.15.

[0007] Preferably, the lithium vanadium iron phosphate layer further includes a second region; the second region is disposed on the surface of the current collector and located at the end of the first region.

[0008] Preferably, one end of the second region is the first region, and the other end is provided with a tab.

[0009] Preferably, the thickness of the second region is the sum of the thickness of the first region and the thickness of the lithium nickel cobalt manganese aluminum oxide layer.

[0010] Preferably, both the first and second surfaces of the current collector are provided with an empty foil area and a covering area; an electrode tab is provided in the empty foil area; and the lithium nickel cobalt manganese aluminum oxide layer is disposed on the covering area.

[0011] Preferably, the first surface of the current collector is provided with an empty foil area and a covered area; the second surface is provided with a covered area; an electrode tab is provided in the empty foil area; and the lithium nickel cobalt manganese aluminum oxide layer is provided on the covered area.

[0012] Preferably, the first region of the lithium vanadium iron phosphate layer is two or more; The lithium vanadium iron phosphate layer further includes a third region; the third region is located between two adjacent first regions and covers the tab and / or the empty foil region.

[0013] Preferably, the lithium nickel cobalt manganese aluminum oxide layer and / or the lithium vanadium iron phosphate layer are layered structures formed by dry preparation.

[0014] This utility model also provides a lithium-ion battery comprising the aforementioned multilayer electrode sheets.

[0015] The above-described solution of this utility model has at least the following beneficial effects: The multilayer electrode of this invention comprises: a current collector, a lithium nickel cobalt manganese aluminum oxide layer, and a lithium vanadium iron phosphate layer. The current collector includes a first surface and a second surface disposed opposite to each other. The lithium nickel cobalt manganese aluminum oxide layer is disposed on the first surface and the second surface. The lithium vanadium iron phosphate layer includes a first region, which is disposed on the surface of the lithium nickel cobalt manganese aluminum oxide layer. The multilayer electrode of this invention exhibits good low-temperature performance, high energy density, and high safety.

[0016] The lithium nickel cobalt manganese aluminum oxide layer located between the current collector and the lithium vanadium iron phosphate layer has high energy density, is less affected by temperature, and has less low-temperature decay. The lithium vanadium iron phosphate layer on the surface has poor electronic conductivity and stable thermal performance. In the event of short circuits or punctures, it can effectively control and reduce short-circuit current, allowing heat to be released slowly and reducing the risk of thermal runaway. This results in a multilayer electrode that has good low-temperature performance while having safety comparable to that of lithium iron phosphate electrodes.

[0017] In particular, when the current collector is aluminum foil, lithium nickel cobalt manganese aluminum oxide has better compatibility with aluminum foil, which can improve the electrochemical performance of multilayer electrodes and extend cycle life. Attached Figure Description

[0018] Figure 1This is a schematic cross-sectional view of the multilayer electrode sheet of Embodiment 1 of this utility model; Figure 2 yes Figure 1 A partial structural schematic diagram of the multilayer electrode sheet is shown; Figure 3 This is a cross-sectional structural diagram of the multilayer electrode sheet of Embodiment 2 of this utility model; Figure 4 yes Figure 3 A partial structural schematic diagram of the multilayer electrode sheet is shown; Figure 5 This is a cross-sectional structural diagram of the multilayer electrode sheet of Embodiment 3 of this utility model; Figure 6 yes Figure 5 A schematic diagram of the multilayer electrode sheet as shown in top view; Figure 7 yes Figure 5 The diagram shown illustrates the structure of a multilayer electrode without a lithium iron phosphate vanadium phosphate layer. Figure 8 yes Figure 7 A schematic diagram of the multilayer electrode sheet as shown in top view; Figure 9 This is a cross-sectional structural diagram of the multilayer electrode sheet of Embodiment 4 of this utility model; Figure 10 This is a schematic diagram of the cross-sectional structure of a cylindrical electrode sheet in the prior art; Figure 11 yes Figure 10 A schematic diagram of the cylindrical electrode sheet from a top view. Figure 12 yes Figure 11 The diagram shows the structure of a cylindrical electrode without an active material layer. Among them, 1. Current collector; 11. First surface; 12. Second surface; 13. Empty foil area; 14. Covering area; 2. Lithium nickel cobalt manganese aluminum oxide layer; 3. Lithium vanadium iron phosphate layer; 31. First region; 32. Second region; 33. Third region; 4. Electrode; 5. Active material layer; 6. Adhesive tape. Detailed Implementation

[0019] Exemplary embodiments of the present invention will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of the present invention are shown in the drawings, it should be understood that the present invention may be implemented in various forms and should not be limited to the embodiments set forth herein. Rather, these embodiments are provided so that this invention will be thorough and complete, and will fully convey the scope of the invention to those skilled in the art.

[0020] Example 1

[0021] The multilayer electrode sheet in this embodiment, such as Figure 1-2 As shown, it includes: A current collector 1, the current collector 1 including a first surface 11 and a second surface 12 disposed opposite to each other; A lithium nickel cobalt manganese aluminum oxide layer 2 is disposed on the first surface 11 and the second surface 12; The lithium vanadium iron phosphate layer 3 includes a first region 31; the first region 31 is disposed on the surface of the lithium nickel cobalt manganese aluminum oxide layer 2.

[0022] In this embodiment, the lithium nickel cobalt manganese aluminum oxide layer 2 is symmetrically disposed on the first surface 11 and the second surface 12, and the thickness of the lithium nickel cobalt manganese aluminum oxide layer 2 on the first surface 11 and the second surface 12 is equal. The lithium vanadium iron phosphate layer 3 is symmetrically disposed on both sides of the lithium nickel cobalt manganese aluminum oxide layer 2, and the thickness of the lithium vanadium iron phosphate layer 3 on both sides is equal.

[0023] In this preferred design embodiment, the ratio of the thickness d1 of the lithium nickel cobalt manganese aluminum oxide layer 2 to the thickness d2 of the first region 31 is K, where 0 < K ≤ 0.8. When K = 0, the lithium nickel cobalt manganese aluminum oxide layer 2 is absent, and the multilayer electrode consists of the current collector 1 and the lithium vanadium iron phosphate layer 3, resulting in poor low-temperature performance. When K is too large, the lithium vanadium iron phosphate layer 3 cannot fully exert its role in safety protection and structural stability, leading to a deterioration in the safety performance and cycle stability of the multilayer electrode. When 0 < K ≤ 0.8, the resulting multilayer electrode exhibits good performance in both low-temperature performance and safety. In particular, when 0 < K ≤ 0.15, the overall performance of the resulting multilayer electrode is quite ideal.

[0024] In this embodiment, the lithium nickel cobalt manganese aluminum oxide layer 2 and / or the lithium vanadium iron phosphate layer 3 are layered structures formed by dry processing. The preparation process of the multilayer electrode is as follows: Using aluminum foil as the current collector 1, a layer of lithium nickel cobalt manganese aluminum oxide is uniformly prepared on its surface to form the lithium nickel cobalt manganese aluminum oxide layer 2, and then a layer of lithium vanadium iron phosphate is prepared on its surface to form the lithium vanadium iron phosphate layer 3.

[0025] The lithium nickel cobalt manganese aluminum oxide and lithium vanadium iron phosphate can both be known materials in the prior art, or can be obtained by modifying or doping with other elements using known methods. Those skilled in the art can choose according to actual needs.

[0026] It should be noted that the multilayer electrode sheet can be prepared using existing technologies. For example, dry preparation to form a layered structure can be achieved through dry coating, electrostatic deposition, lamination, etc. Those skilled in the art can choose the appropriate method based on actual needs. Furthermore, the current collector 1 includes, but is not limited to, aluminum foil; those skilled in the art can also select other materials and structures based on actual needs.

[0027] The lithium-ion battery of this embodiment includes the multilayer electrode sheet described in this embodiment.

[0028] Example 2

[0029] The multilayer electrode sheet in this embodiment, such as Figure 3-4 As shown, it includes: A current collector 1, the current collector 1 including a first surface 11 and a second surface 12 disposed opposite to each other; A lithium nickel cobalt manganese aluminum oxide layer 2 is disposed on the first surface 11 and the second surface 12; The lithium vanadium iron phosphate layer 3 includes a first region 31; the first region 31 is disposed on the surface of the lithium nickel cobalt manganese aluminum oxide layer 2.

[0030] To improve the conductivity at the distal end of the tab, the lithium vanadium iron phosphate layer 3 further includes a second region 32; the second region 32 is disposed on the surface of the current collector 1 and located at the end of the first region 31. One end of the second region 32 is the first region 31, and the other end is provided with a tab 4.

[0031] like Figure 4 The diagram shown is a partial structural schematic from a top view after the contact surface between the first region 31 and the lithium nickel cobalt manganese aluminum oxide layer 2 is cut open.

[0032] In this embodiment, the lithium nickel cobalt manganese aluminum oxide layer 2 is symmetrically disposed on the first surface 11 and the second surface 12, and the thickness of the lithium nickel cobalt manganese aluminum oxide layer 2 on the first surface 11 and the second surface 12 is equal. The lithium vanadium iron phosphate layer 3 is symmetrically disposed on both sides of the lithium nickel cobalt manganese aluminum oxide layer 2, and the thickness of the lithium vanadium iron phosphate layer 3 on both sides is equal.

[0033] In a preferred design of this embodiment, the ratio of the thickness of the lithium nickel cobalt manganese aluminum oxide layer 2 to the thickness of the first region 31 is K, where 0 < K ≤ 0.8. The thickness of the second region 32 is the sum of the thicknesses of the first region 31 and the lithium nickel cobalt manganese aluminum oxide layer 2.

[0034] The multilayer electrode sheet described in this embodiment can be prepared using the same method as in Example 1.

[0035] The lithium-ion battery of this embodiment includes the multilayer electrode sheet described in this embodiment.

[0036] It should be noted that the multilayer electrode sheet described in this embodiment is a pouch electrode sheet, which can be used in flexible-packaged lithium-ion batteries.

[0037] Example 3

[0038] The multilayer electrode sheet in this embodiment, such as Figure 5-6 As shown, it includes: A current collector 1, the current collector 1 including a first surface 11 and a second surface 12 disposed opposite to each other; A lithium nickel cobalt manganese aluminum oxide layer 2 is disposed on the first surface 11 and the second surface 12; The lithium vanadium iron phosphate layer 3 includes a first region 31; the first region 31 is disposed on the surface of the lithium nickel cobalt manganese aluminum oxide layer 2.

[0039] In this embodiment, the lithium nickel cobalt manganese aluminum oxide layer 2 is symmetrically disposed on the first surface 11 and the second surface 12, and the thickness of the lithium nickel cobalt manganese aluminum oxide layer 2 on the first surface 11 and the second surface 12 is equal. The lithium vanadium iron phosphate layer 3 is symmetrically disposed on both sides of the lithium nickel cobalt manganese aluminum oxide layer 2, and the thickness of the lithium vanadium iron phosphate layer 3 on both sides is equal.

[0040] As a preferred design in this embodiment, the ratio of the thickness of the lithium nickel cobalt manganese aluminum oxide layer 2 to the thickness of the first region 31 is K, where 0 < K ≤ 0.8.

[0041] To facilitate fixing the tab 4, the first surface 11 and the second surface 12 of the current collector 1 are provided with an empty foil area 13 and a covering area 14; the tab 4 is provided at the empty foil area 13; the lithium nickel cobalt manganese aluminum oxide layer 2 is provided on the covering area 14.

[0042] To provide battery capacity, the first region 31 of the lithium vanadium iron phosphate layer 3 is two or more; the lithium vanadium iron phosphate layer 3 also includes a third region 33; the third region 33 is located between two adjacent first regions 31 and covers the tab 4 and / or the empty foil region 13.

[0043] In this embodiment, the lithium nickel cobalt manganese aluminum oxide layer 2 and / or the lithium vanadium iron phosphate layer 3 are layered structures formed by dry processing. The preparation process of the multilayer electrode is as follows: Using aluminum foil as the current collector 1, a layer of lithium nickel cobalt manganese aluminum oxide is uniformly prepared on its surface to form the lithium nickel cobalt manganese aluminum oxide layer 2. During the preparation of the lithium nickel cobalt manganese aluminum oxide layer 2, the empty foil region 13 can be constructed on the current collector 1 using methods such as masking. Then, electrode tabs 4 are welded to the empty foil region 13, resulting in the structure shown below. Figure 7-8As shown. Then, a layered material containing lithium vanadium iron phosphate is prepared on its surface to form the lithium vanadium iron phosphate layer 3.

[0044] like Figure 10-11 As shown, this is a common cylindrical electrode structure with a fixed tab 4 in existing technology, used in wound batteries. It includes a current collector 1 and an active material layer 5. The active material layer 5 is disposed on the upper and lower surfaces of the current collector 1, and the tab 4 is usually fixed to the empty foil area 13 of the current collector 1 by welding, resulting in the structure shown. Figure 12 As shown, to prevent the current collector 1 from being exposed and causing an internal short circuit, tape 6 needs to be installed at the empty foil area 13, i.e. Figure 10-11 The structure shown.

[0045] In this embodiment, the structure does not require the installation of tape 6 after welding the tab 4 to prevent the current collector 1 from being exposed. Instead, the third region 33 is used to cover the empty foil area 13, which not only simplifies the preparation process and eliminates the step of setting tape, but also improves the battery capacity.

[0046] The lithium-ion battery of this embodiment includes the multilayer electrode sheet described in this embodiment.

[0047] It should be noted that the multilayer electrode sheet described in this embodiment is a cylindrical electrode sheet, which can be used in wound batteries.

[0048] Example 4

[0049] The multilayer electrode sheet in this embodiment, such as Figure 9 As shown, the structure is the same as that in Example 3, with the only difference being: The current collector 1 has an empty foil area 13 and a covering area 14 on its first surface 11; the second surface 12 has a covering area 14; the empty foil area 13 has an electrode tab 4; and the covering area 14 has a lithium nickel cobalt manganese aluminum oxide layer 2.

[0050] The first region 31 of the lithium vanadium iron phosphate layer 3 is two; the lithium vanadium iron phosphate layer 3 also includes a third region 33; the third region 33 is located between two adjacent first regions 31 and covers the tab 4 and the empty foil region 13.

[0051] It should be noted that the multilayer electrode sheet described in this embodiment is a cylindrical electrode sheet, which can be used in wound batteries.

[0052] The above description is the preferred embodiment of this utility model. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of this utility model, and these improvements and modifications should also be considered within the protection scope of this utility model.

Claims

1. A multilayer electrode sheet, characterized in that, include: A current collector (1) includes a first surface (11) and a second surface (12) disposed opposite to each other. A lithium nickel cobalt manganese aluminum oxide layer (2) is disposed on the first surface (11) and the second surface (12); The lithium vanadium iron phosphate layer (3) includes a first region (31); the first region (31) is disposed on the surface of the lithium nickel cobalt manganese aluminum oxide layer (2).

2. The multilayer electrode sheet according to claim 1, characterized in that, The ratio of the thickness of the nickel cobalt manganese aluminum oxide lithium layer (2) to the thickness of the first region (31) is K, where 0 < K ≤ 0.

8.

3. The multilayer electrode sheet according to claim 2, characterized in that, The lithium vanadium iron phosphate layer (3) further includes a second region (32); the second region (32) is disposed on the surface of the current collector (1) and located at the end of the first region (31).

4. The multilayer electrode sheet according to claim 3, characterized in that, One end of the second region (32) is the first region (31), and the other end is provided with a tab (4).

5. The multilayer electrode sheet according to claim 4, characterized in that, The thickness of the second region (32) is the sum of the thickness of the first region (31) and the thickness of the lithium nickel cobalt manganese aluminum oxide layer (2).

6. The multilayer electrode sheet according to claim 2, characterized in that, The current collector (1) has an empty foil area (13) and a covering area (14) on its first surface (11) and second surface (12); the empty foil area (13) is provided with a tab (4); the covering area (14) is provided with the lithium nickel cobalt manganese aluminum oxide layer (2).

7. The multilayer electrode sheet according to claim 2, characterized in that, The current collector (1) has an empty foil area (13) and a covering area (14) on its first surface (11); the second surface (12) has a covering area (14); the empty foil area (13) has a tab (4); and the covering area (14) has a lithium nickel cobalt manganese aluminum oxide layer (2).

8. The multilayer electrode sheet according to claim 6 or 7, characterized in that, The first region (31) of the lithium iron phosphate layer (3) is two or more; The lithium vanadium iron phosphate layer (3) further includes a third region (33); the third region (33) is located between two adjacent first regions (31) and covers the tab (4) and / or the empty foil region (13).

9. The multilayer electrode sheet according to claim 1, characterized in that, The lithium nickel cobalt manganese aluminum oxide layer (2) and / or the lithium vanadium iron phosphate layer (3) are layered structures formed by dry preparation.

10. A lithium-ion battery comprising the multilayer electrode sheet as described in any one of claims 1-9.