rigid-flex printed circuit board

By using a combination of cover film and solder resist ink in the rigid-flex PCB, along with low-flow prepreg and precise window design, the reliability issues of traditional rigid-flex PCBs under temperature cycling and mechanical bending are solved, achieving a balance between performance and cost, and improving product lifespan and electrical performance.

CN225003746UActive Publication Date: 2026-11-20HUIZHOU KING BROTHER CIRCUIT TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522679281.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-17
Publication Date
2026-11-20
Estimated Expiration
2035-12-17

AI Technical Summary

Technical Problem

Traditional rigid-flex panels are prone to interfacial microcracks and delamination under temperature cycling and mechanical bending stress, leading to electrochemical migration or short circuit failures. Furthermore, the full-coverage membrane design is prone to stress concentration and micro-tears during dynamic bending, affecting product reliability and lifespan.

Method used

A hybrid protection scheme is adopted, using a cover film to provide high reliability in critical areas and solder resist ink in non-critical areas. Combined with low-flow prepreg, the layers are fixedly connected. The precise window design prevents the cover adhesive from overflowing the solder pads, ensuring soldering quality and stability.

Benefits of technology

It improves the product's lifespan and reliability in high-frequency bending scenarios, reduces manufacturing costs, decreases the risk of electrical failures, and enhances manufacturing precision and consistency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225003746U_ABST
    Figure CN225003746U_ABST
Patent Text Reader

Abstract

The application relates to the technical field of printed circuit boards, in particular to a rigid-flexible combination board. The rigid-flexible combination board comprises a first rigid plate, a second rigid plate and a flexible plate. The flexible plate is arranged between the first rigid plate and the second rigid plate; a surface layer of the first rigid plate away from the flexible plate is a first surface layer, a surface layer of the first rigid plate close to the flexible plate is a second surface layer, and the first surface layer is provided with a solder resist ink; a surface layer of the second rigid plate close to the flexible plate is a third surface layer, a surface layer of the second rigid plate away from the flexible plate is a fourth surface layer, and the fourth surface layer is provided with a cover film; and the surface layer of the flexible plate close to the first rigid plate and the surface layer of the flexible plate close to the second rigid plate are provided with the cover film. According to actual demands of different surfaces of the circuit board, the first rigid plate is provided with the low-cost solder resist ink, the second rigid plate is provided with the high-performance cover film, and mixed protection is achieved. The cover film is used for providing high reliability in the key area, the solder resist ink is used for controlling the cost in the non-key area, and the performance and the cost are balanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of printed circuit board technology, and more specifically, to rigid-flex boards. Background Technology

[0002] Rigid-flex PCBs, as composite printed circuit boards combining the mechanical support of rigid boards with the bendability of flexible boards, play a crucial role in modern electronic devices. Their unique structural characteristics allow them to adapt to complex spatial layouts and dynamic bending requirements, making them widely used in high-precision fields such as foldable smartphone screen modules, internal connections in wearable devices, precision instruments in spacecraft, and implantable medical devices. Traditional rigid-flex PCB manufacturing processes typically employ a layered protection strategy: the inner flexible circuit board (FPC) layer uses a polyimide coverlay for insulation protection, a material with excellent flexibility and bending resistance; while the outer rigid FR4 layer undergoes surface treatment with photocurable solder resist ink, primarily serving to prevent soldering and oxidation.

[0003] Existing technologies mainly include the following typical protection solutions: The first is the outer rigid plate full solder resist ink process. Although this conventional solution has a low cost, it has obvious defects—the interfacial adhesion between the solder resist ink and the FR4 substrate is limited. Under temperature cycling tests (-55℃ to 125℃) or mechanical bending stress, microcracks are easily generated at the interface and gradually expand into delamination. This failure mode will lead to direct exposure of copper circuits, which will then cause electrochemical migration or short circuit failures, posing a serious hidden danger to high-reliability products such as aerospace electronic equipment that require an MTBF (Mean Time Between Failures) of more than 100,000 hours.

[0004] The second approach is a full-coverage outer film process. This approach completely abandons the rigid plate structure, using a flexible plate covered with a film for the entire outer layer. While this significantly improves the flexibility of the bending area, the lack of a rigid support structure makes it prone to stress concentration during dynamic bending applications. This can lead to microscopic tears at the interface between the cover film and the substrate, potentially developing into through-fracture after long-term cyclic bending. This failure mode can significantly shorten the product's lifespan, especially in high-frequency bending areas such as the hinge of foldable screen devices. Utility Model Content

[0005] The purpose of this application is to provide a rigid-flex board that uses a mixture of cover film and solder resist ink for protection according to the actual needs of different surfaces of the circuit board, providing high reliability in critical areas and controlling costs in non-critical areas, thereby achieving the best balance between performance and cost.

[0006] To achieve the above objectives, in a first aspect, this application provides a rigid-flexible plate, comprising: First rigid plate and second rigid plate; A flexible plate, wherein the flexible plate is disposed between the first rigid plate and the second rigid plate; The surface layer on the first rigid plate that is away from the flexible plate is the first surface layer, and the surface layer that is close to the flexible plate is the second surface layer. Solder resist ink is provided on the first surface layer. The surface layer of the second rigid plate that is close to the flexible plate is the third surface layer, and the surface layer that is far away from the flexible plate is the fourth surface layer. A covering film is provided on the fourth surface layer. A covering film is provided on the surface layer of the flexible plate near the first rigid plate and the surface layer near the second rigid plate.

[0007] In an optional embodiment, a window is made on the cover film at the fourth surface layer, with the window size at the pad being E and the corresponding pad size being F, where E = F + 4mil.

[0008] In an optional embodiment, the uncovering size at the fourth surface layer is G, and the opening size of the covering film at the uncovering point is H, where G=H.

[0009] In an optional embodiment, the flexible plate is fixedly connected to the first rigid plate and the second rigid plate by a low-flow prepreg.

[0010] In an optional implementation, the number of flexible plates is one.

[0011] In an optional embodiment, the number of flexible plates is two or more, and adjacent flexible plates are connected by a low-flow prepreg.

[0012] In an optional embodiment, the thickness of the cover film on the flexible plate is A, wherein 20μm≤A≤50μm.

[0013] In an optional embodiment, the thickness of the cover film disposed on the fourth surface layer is C, wherein 80μm≤C≤120μm.

[0014] In an optional embodiment, the first rigid plate is arranged parallel to the flexible plate.

[0015] In an optional embodiment, the second rigid plate is arranged parallel to the flexible plate.

[0016] Based on the actual needs of different circuit board surfaces, this application uses low-cost solder resist ink on the first rigid board and a high-performance cover film on the second rigid board, providing hybrid protection. The cover film provides high reliability for critical areas, while the solder resist ink controls costs for non-critical areas, thus balancing performance and cost.

[0017] Other features and advantages of this application will be described in detail in the following detailed description section. Attached Figure Description

[0018] To more clearly illustrate the technical solutions of the embodiments of this application, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of this application and should not be regarded as a limitation of the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.

[0019] Figure 1 A cross-sectional view of one embodiment of the rigid-flexible plate provided in this application; Figure 2 A partial cross-sectional view of one embodiment of the rigid-flexible plate provided in this application; Figure 3 A cross-sectional view of a partial structure of one embodiment of the rigid-flexible plate provided in this application; Figure 4 This is a schematic diagram illustrating the manufacturing process of one embodiment of the rigid-flexible plate provided in this application.

[0020] icon: 100 - First rigid plate; 110 - First surface layer; 120 - Second surface layer; 200 - Second rigid plate; 210 - Third surface layer; 220 - Fourth surface layer; 300-Flexible Board; 410 - Cover film; 420 - Solder resist ink; 430 - Low flow prepreg; 710 - Window opening position; 720 - Cover opening position; 730 - Solder pad position; 810 - Steel plate; 820 - Buffer pad; 830 - Epoxy resin board; 840 - Release film. Detailed Implementation

[0021] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. The components of the embodiments of this application described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.

[0022] In the description of this application, it should be noted that the terms "inner" and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship commonly used when the product is in use. They are used only for the convenience of describing this application and for simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application. Furthermore, the terms "first," "second," etc., are used only to distinguish descriptions and should not be construed as indicating or implying relative importance.

[0023] In the description of this application, it should also be noted that, unless otherwise expressly specified and limited, the terms "setup" and "connection" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.

[0024] Figure 1 The diagram illustrates the relationship between the layers of the rigid-flexible plate provided in the embodiments of this application before the cover is removed.

[0025] Figure 2 The relationship between the layers of the rigid-flexible plate provided in the embodiments of this application is shown after the cover is removed.

[0026] like Figure 1 As shown, in a first aspect, embodiments of this application provide a rigid-flexible plate, including a first rigid plate 100, a second rigid plate 200, and a flexible plate 300.

[0027] like Figure 1 As shown, the flexible plate 300 is disposed between the first rigid plate 100 and the second rigid plate 200.

[0028] like Figure 1 As shown, the surface layer on the first rigid plate 100 that is away from the flexible plate 300 is the first surface layer 110, and the surface layer that is close to the flexible plate 300 is the second surface layer 120. The first surface layer 110 and the second surface layer 120 are in opposite positions.

[0029] like Figure 1 As shown, the first surface layer 110 is provided with solder resist ink 420. The second surface layer 120 is used to connect with the flexible board 300.

[0030] like Figure 1 As shown, the surface layer of the second rigid plate 200 near the flexible plate 300 is the third surface layer 210, and the surface layer away from the flexible plate 300 is the fourth surface layer 220. A cover film 410 is provided on the fourth surface layer 220. The third surface layer 210 is used to connect with the flexible plate 300.

[0031] like Figure 1 As shown, the flexible plate 300 has a cover film 410 on the surface layer near the first rigid plate 100 and the surface layer near the second rigid plate 200.

[0032] Compared to the cover film 410, the solder resist ink 420 is less expensive, while the cover film 410 offers superior performance in certain scenarios. This application, based on the actual needs of different surfaces of the circuit board, applies solder resist ink 420 to the first rigid plate 100 and a cover film 410 to the second rigid plate 200, using a mixture of cover film 410 and solder resist ink 420 for protection on different rigid plates. This approach uses the higher-performance cover film 410 in critical areas (such as areas with high performance requirements and susceptible to external factors) to provide high reliability, while using the less expensive solder resist ink 420 in non-critical areas, effectively controlling costs and thus balancing performance and cost.

[0033] In high-frequency bending areas, the flexible cover film 410 structure is retained. Due to its excellent flexibility and bending resistance, the flexible cover film 410 can adapt to repeated bending actions, avoiding fatigue fracture of the rigid solder resist layer caused by repeated deformation. This improves the service life and reliability of the rigid-flex plate under high-frequency bending scenarios. In ordinary areas, solder resist ink 420 is used. Solder resist ink 420 serves to prevent soldering and oxidation, meeting the protection requirements of ordinary areas. Furthermore, its lower cost reduces the overall manufacturing cost of the rigid-flex plate.

[0034] To prevent the adhesive from flowing onto the solder pads during lamination, such as Figures 1 to 3 As shown, in one embodiment, a window is made on the cover film 410 at the fourth surface layer 220, and the window size at the pad is E, and the corresponding pad size is F, where E = F + 4mil.

[0035] 1mil≈25.4μm, 4mil≈101.6μm.

[0036] For example, Figure 1 and Figure 3 The image shows the window position 710 of the cover film 410 at the fourth surface layer 220, and the pad position 730 corresponds to the window position 710.

[0037] For example, assuming the pads are set as circular pads with a diameter of 4 mil, the cover film 410 will also have corresponding circular openings with a size E = 4 mil + 4 mil = 8 mil. Assuming the pads are set as square pads with a side length of 5 mil, the cover film 410 will also have corresponding square openings with a size E = 5 mil + 4 mil = 9 mil.

[0038] By precisely opening windows in the cover film 410, it is ensured that the cover adhesive does not cover the solder pads, thus avoiding potential short circuits or poor soldering during the soldering process. This improves the electrical performance and reliability of the product.

[0039] The design, with a window size 4 mil larger than the pad size, ensures complete pad exposure, allowing the solder to fully contact the pads during the soldering process, thus improving soldering quality and stability. This helps reduce soldering defects such as cold solder joints and poor solder joints.

[0040] Because the cover adhesive does not leak onto the solder pads, the bond between the pads and the solder is stronger, reducing the risk of electrochemical migration and corrosion caused by the cover adhesive. This significantly improves the long-term reliability and service life of the product.

[0041] In one embodiment, the uncovering size at the fourth surface layer 220 is G, and the opening size of the covering film 410 at the uncovering point is H, where G=H.

[0042] For example, Figure 1 and Figure 3 The image shows the fourth layer, with 220 uncovered locations, 720.

[0043] For example, suppose the fourth layer 220 is opened in a circular manner, and the opening size G is the radius of the circle. Suppose G=3mil, then the covering film 410 at the opening is also provided with a circular opening, and the radius of the circular opening is H=3mil.

[0044] By making the opening size G of the cover equal to the opening size H of the cover film 410, precise alignment between the opening area and the opening area of ​​the cover film 410 is ensured. This reduces misalignment problems caused by size mismatch and improves the manufacturing precision and consistency of the product.

[0045] Of course, excess adhesive at the cap opening can be left uncontrolled. If adhesive has flowed to the cap, laser cap removal allows for direct production. Since the inner layer has laser copper lines, minor variations in laser depth due to inconsistent adhesive flow can be ignored. If this area corresponds to tiny solder pads, a thinner cover film 410 (e.g., 27.5μm, 37.5μm) should be prioritized (thin adhesive, less excess adhesive) with a minimum 4mil spacing from the pads, via rings, and IC edges. To minimize the offset between the cover film 410 and the product, and to prevent adhesive overflow onto the solder pads, the cover film must be inspected during the cover film application process. This can include a shrinkage measurement process to ensure a 1:1 shrinkage ratio between the cover film and the product, thereby reducing defects such as offset and adhesive overflow onto the solder pads caused by shrinkage.

[0046] like Figure 1As shown, in one embodiment, the flexible plate 300 is fixedly connected to the first rigid plate 100 and the second rigid plate 200 by a low-flow prepreg sheet 430.

[0047] Low-Flow Prepreg 430, or simply 'Low-Flow PP', is a semi-cured insulating medium material with low epoxy resin content and low flowability during high-temperature and high-pressure lamination. Its low flowability prevents excessive resin outflow during lamination, avoiding voids and other problems, making it suitable for delicate structures; it has high dimensional stability, reducing interlayer displacement and improving alignment accuracy; and it has controllable filling capability, allowing for appropriate filling without overflow in specific structures.

[0048] like Figure 1 As shown, in one embodiment, one flexible plate 300 is provided. One surface layer of the flexible plate 300 is close to the first rigid plate 100, and the flexible plate 300 and the first rigid plate 100 are connected by a low-flow prepreg 430. The other surface layer of the flexible plate 300 is close to the second rigid plate 200, and the flexible plate 300 and the second rigid plate 200 are connected by a low-flow prepreg 430.

[0049] In another embodiment, the number of flexible plates 300 is two or more, and adjacent flexible plates 300 are connected by a low-flow prepreg 430.

[0050] For example, two flexible plates 300 are provided, and the two flexible plates 300 are connected by a low-flow prepreg sheet 430. Of the two flexible plates 300, one flexible plate 300 is fixedly connected to the first rigid plate 100 via the low-flow prepreg sheet 430, and the other flexible plate 300 is fixedly connected to the second rigid plate 200 via the same low-flow prepreg sheet 430. In other embodiments, other numbers of flexible plates 300 may be provided, such as three or four.

[0051] like Figure 1 As shown, in one embodiment, the thickness of the cover film 410 on the flexible plate 300 is A, wherein 20μm≤A≤50μm.

[0052] For example, one of the surfaces of the flexible plate 300 is close to the first rigid plate 100, and the other surface of the flexible plate 300 is close to the second rigid plate 200. A cover film 410 with a thickness of A is respectively provided on the two surfaces of the flexible plate 300.

[0053] For example, the thickness A of the cover film 410 on the flexible plate 300 is 20 μm. In another embodiment, the thickness A of the cover film 410 on the flexible plate 300 is 30 μm. In another embodiment, the thickness A of the cover film 410 on the flexible plate 300 is 40 μm. In yet another embodiment, the thickness A of the cover film 410 on the flexible plate 300 is 50 μm.

[0054] The flexible board 300 has a cover film 410 of thickness A on both sides, which can provide uniform protection and support to the flexible board 300 in both directions. This ensures that the flexible board 300 is subjected to uniform force on both sides during bending, folding and other deformation processes, reduces stress concentration caused by differences between the two sides, thereby reducing the risk of damage to the flexible board 300 and improving the service life and stability of the product.

[0055] If the thickness A of the cover film 410 is less than 20μm, its protective capability will be too low, making it difficult to effectively protect the flexible board 300 from external physical damage (such as scratches and collisions) and chemical corrosion, and it will also fail to provide reliable insulation performance, affecting the normal use and safety of the product.

[0056] When the thickness A of the cover film 410 is greater than 50μm, the cover film 410 may be too rigid, which will reduce the flexibility of the flexible plate 300, making it difficult to meet the requirements of some application scenarios that require frequent bending and folding, and may even cause the flexible plate 300 to crack or be damaged during deformation.

[0057] like Figure 1 As shown, in one embodiment, the thickness of the cover film 410 disposed on the fourth surface layer 220 is C, wherein 80μm≤C≤120μm.

[0058] For example, the thickness C of the cover film 410 disposed on the fourth surface layer 220 is 80 μm. In another embodiment, the thickness C of the cover film 410 disposed on the fourth surface layer 220 is 90 μm. In another embodiment, the thickness C of the cover film 410 disposed on the fourth surface layer 220 is 100 μm. In another embodiment, the thickness C of the cover film 410 disposed on the fourth surface layer 220 is 110 μm. In yet another embodiment, the thickness C of the cover film 410 disposed on the fourth surface layer 220 is 120 μm.

[0059] The thickness of the cover film 410 on the fourth layer 220 can be flexibly selected according to factors such as the specific application environment, electrical performance requirements, and mechanical stress resistance of the product. For example, in scenarios where space is limited and weight is sensitive, and the protection requirements are not extremely high, a thinner thickness can be selected; in scenarios where the requirements for protection against mechanical impact and chemical corrosion are strict, or where high insulation performance is required, a thicker thickness can be selected.

[0060] Different thicknesses of cover film offer different performance emphases. Thinner cover films 410 (e.g., 80μm) may improve the flexibility of the product to some extent, making it easier to bend and fold, adapting to installation requirements with special shapes; while thicker cover films 410 (e.g., 120μm) provide stronger mechanical protection, effectively resisting physical damage such as scratches and impacts, while enhancing insulation performance and reducing the risk of electrical faults such as leakage. Cover films 410 with a thickness between 80μm and 120μm have high abrasion resistance and can withstand long-term friction and wear. This is particularly suitable for applications requiring frequent contact or movement, such as electronic device housings and automotive interiors.

[0061] like Figure 1 As shown, in one embodiment, the first rigid plate 100 and the flexible plate 300 are arranged in parallel.

[0062] like Figure 1 As shown, in one embodiment, the second rigid plate 200 is arranged in parallel with the flexible plate 300.

[0063] The first rigid plate 100, the second rigid plate 200, and the flexible plate 300 are parallel to each other.

[0064] Secondly, embodiments of this application also provide a method for manufacturing a rigid-flexible plate, the steps of which include: S100: Fabricate the inner layer circuitry of the first rigid plate 100, the second rigid plate 200, and the flexible plate 300.

[0065] For example, when fabricating the inner layer circuitry of the first rigid board 100 and the second rigid board 200, the inner layer circuitry at the second surface layer 120 of the first rigid board 100 and the third surface layer 210 of the second rigid board 200 are fabricated according to conventional PCB board processes. After the inner layer circuitry of the first rigid board 100 and the second rigid board 200 is fabricated, acid etching and AOI inspection scanning are performed. Then, the first rigid board 100 and the second rigid board 200 are transferred to the lamination process to wait for browning and lamination, thereby completing the fabrication of the first rigid board 100 and the second rigid board 200 components.

[0066] For example, when fabricating the inner layer circuitry of the flexible board 300, the inner layer circuitry of the flexible board 300 is fabricated according to conventional PCB board processes, and then acid etching and AOI inspection scanning are performed. After completion, it is transferred to the lamination process for browning, and then waits for the cover film 410 to be laminated.

[0067] S110: Fabricate the cover film 410 of the flexible board 300; for example, when fabricating the cover film 410, first cut the material to the required size, then obtain the cover film 410 of the required size, and then drill positioning holes on the cover film 410 to complete the cutting of the cover film 410.

[0068] S120: Make a window in the cover film 410 of the flexible panel 300; for example, the cover film 410 with the positioning holes drilled can be made into a window according to the required size and orientation.

[0069] S130: The cover film 410, which has been milled, is precisely positioned with the flexible plate 300 using the preset positioning holes and attached to the surface of the flexible plate 300, which has been browned. Then, a temperature-controlled soldering iron is used to locally heat the edge of the cover film 410 to activate the initial adhesion of its adhesive, achieve temporary fixation, and prevent displacement in subsequent processes, thereby completing the preparation for bonding the cover film 410.

[0070] S200: A cover film 410 is provided on the surface layer of the flexible plate 300.

[0071] Place the uncured flexible board 300, which has been covered with the cover film 410, into the high-pressure press. Cover both the top and bottom surfaces with a layer of auxiliary release film 840 (to prevent the hot press plate from directly contacting the product and causing contamination or tearing). Perform high-pressure pressing: apply a certain temperature (usually 150℃-180℃) and pressure (approximately 10 kg / cm²). 2 -30kg / cm 2 The pressing process lasts 30-200 seconds; the purpose is to allow the adhesive on the back of the cover film 410 to flow and initially cure under heat, thus firmly adhering to the circuit surface. After pressing, the cover film 410 is no longer loosely attached, but forms a stable and continuous protective layer, which can proceed to subsequent processes (such as plasma treatment, lamination, etc.) without wrinkling, bubbling, or shifting.

[0072] S300: Pressing together the first rigid plate 100, the flexible plate 300, and the second rigid plate 200. Exemplarily, the first rigid plate 100, the flexible plate 300, and the second rigid plate 200 can be pressed together using conventional processes.

[0073] S310: Fabricate the cover film 410 for the second rigid plate 200. Exemplarily, as needed, cut the material and drill positioning holes to obtain the cover film 410 required for the second rigid plate 200.

[0074] S320: Open a window in the cover film 410; for example, open the window in the cover film 410 using a UV laser machine.

[0075] S330: Attach the cover film 410 to the fourth surface layer 220 of the second rigid plate 200, and use a soldering iron to spot weld it in the blank position, waiting for the cover film 410 to be pressed.

[0076] S400: A cover film 410 is provided on the fourth surface layer 220 of the second rigid plate 200.

[0077] For example, such as Figure 4 As shown, when implementing S400, the third layer 210 of the second rigid plate 200 without the cover film 410 is filled with a buffer pad 820 and pressed with a steel plate 810; the fourth layer 220 with the cover film 410 is filled with a release film 840, an epoxy resin board 830 and a buffer pad 820, and pressed with a steel plate 810 to prevent excessive glue flow from the cover film 410, which could cover the solder pads and lead to poor product quality.

[0078] Steel plate 810 is used to provide rigid support, prevent plate deformation, improve surface flatness, and avoid uneven stress that could lead to thickness differences or slippage.

[0079] The 820 cushioning pad is used to absorb impact, balance pressure, and buffer heat conduction, thus achieving uniform pressure distribution.

[0080] Release film 840 is used to prevent the adhesive of cover film 410 from sticking back to cushioning pad 820 or steel plate 810.

[0081] The epoxy resin board 830 surface can still maintain a certain hardness under high temperature and high pressure environment. Based on this characteristic, its flat surface can support the second rigid plate 200 during the pressing process, thereby effectively preventing the second rigid plate 200 from warping after pressing.

[0082] After the cover film 410 is pressed onto the fourth surface layer 220, it awaits plasma fabrication.

[0083] S410: Perform plasma degumming using the required parameters to remove excess impurities from the first surface layer 110 of the first rigid plate 100, while increasing the bonding strength between the first rigid plate 100 and the solder resist.

[0084] S500: Solder resist ink 420 is applied to the first surface layer 110 of the first rigid plate 100.

[0085] For example, the solder resist ink 420 is printed on one side: the solder resist process is performed on the first surface layer 110.

[0086] The rigid-flex PCB manufacturing method provided in this application overcomes, to some extent, the technical biases inherent in traditional manufacturing methods. For example, traditional methods often consider the poor compatibility between solder resist ink and cover film, frequently employing either full solder resist ink or full cover film manufacturing schemes. However, PCBs made with full solder resist ink exhibit poor performance, while PCBs made with full cover film are more expensive. In the rigid-flex PCB manufacturing method provided in this application, the solder resist ink on the first rigid board is not printed before the cover film on the second rigid board is laminated. The solder resist ink is printed on the first rigid board only after the cover film on the second rigid board is laminated. This avoids the solder resist ink being affected by the cover film lamination process, preventing problems such as peeling, bubbling, or deterioration and whitening. This manufacturing sequence is adopted because the cover film has a certain degree of corrosion resistance. If the solder resist ink is printed on the first rigid board first, and then the cover film on the second rigid board is laminated, the solder resist ink will be affected, potentially leading to peeling, bubbling, or deterioration and whitening.

[0087] S550: The shape of the rigid-flexible plate can be made using a spiral cutter to avoid burrs or other defects on the surface of the membrane 410 covering the second rigid plate 200.

[0088] S600: Laser-assisted opening; for example, such as Figure 2 As shown, the first rigid plate 100 and the second rigid plate 200 are laser-coated according to production requirements. Figure 1 and Figure 3 The image shows the opening position 720.

[0089] like Figure 3 As shown, in one embodiment, a window is made in the cover film 410 on the fourth surface layer 220, and the window size at the pad is E, the corresponding pad size is F, and E=F+4mil.

[0090] When the pad is round, elliptical or polygonal, the window size at the pad is E=F+4mil.

[0091] like Figure 3 As shown, in one embodiment, the cover is removed at the fourth surface layer 220, the size of the removal is G, and the opening size of the cover film 410 at the removal point is H, where G=H.

[0092] When the fourth layer 220 is peeled off, the peeling dimension G is consistent with the size of the target copper surface (such as the gold fingers). When making the cover film 410, the opening dimension H of the area to be peeled off should be exactly the same as the peeling dimension G, neither enlarged nor reduced—because the exposure is achieved by physical peeling, there is no problem of glue overflow and obstruction. For example, if the length of the gold fingers is 5mm, then G=H=5mm; and if the length of the gold fingers is 10mm, then G=H=10mm.

[0093] The table below shows the stable performance of rigid-flex plates fabricated using the rigid-flex plate fabrication method of this application under reflow soldering process:

[0094] It should be noted that, where there is no conflict, the features in the embodiments of this application can be combined with each other.

[0095] The above description is merely a preferred embodiment of this application and is not intended to limit this application. Various modifications and variations can be made to this application by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application should be included within the protection scope of this application.

Claims

1. A rigid-flexible composite plate, characterized in that, include: First rigid plate (100) and second rigid plate (200); A flexible plate (300) is disposed between the first rigid plate (100) and the second rigid plate (200); The surface layer on the first rigid plate (100) that is away from the flexible plate (300) is the first surface layer (110), and the surface layer that is close to the flexible plate (300) is the second surface layer (120). Solder resist ink (420) is provided on the first surface layer (110). The surface layer of the second rigid plate (200) near the flexible plate (300) is the third surface layer (210), and the surface layer away from the flexible plate (300) is the fourth surface layer (220). A covering film (410) is provided on the fourth surface layer (220). A covering film (410) is provided on the surface layer of the flexible plate (300) near the first rigid plate (100) and the surface layer near the second rigid plate (200).

2. The rigid-flexible composite plate according to claim 1, characterized in that, A window is made on the cover film (410) at the fourth surface layer (220), with the window size at the pad being E and the corresponding pad size being F, where E = F + 4mil.

3. The rigid-flexible composite plate according to claim 2, characterized in that, The uncovering size at the fourth surface layer (220) is G, and the opening size of the covering film (410) at the uncovering point is H, where G=H.

4. The rigid-flexible plate according to claim 1, characterized in that, The flexible plate (300) is fixedly connected to the first rigid plate (100) and the second rigid plate (200) by a low-flow adhesive semi-cured sheet (430).

5. The rigid-flexible composite plate according to claim 1, characterized in that, The number of flexible plates (300) is one.

6. The rigid-flexible composite plate according to claim 1, characterized in that, The number of flexible plates (300) is two or more, and adjacent flexible plates (300) are connected by a low-flow prepreg (430).

7. The rigid-flexible plate according to claim 1, characterized in that, The thickness of the cover film (410) on the flexible plate (300) is A, wherein 20μm≤A≤50μm.

8. The rigid-flexible composite plate according to claim 1, characterized in that, The thickness of the cover film (410) disposed on the fourth surface layer (220) is C, wherein 80μm≤C≤120μm.

9. The rigid-flexible composite plate according to claim 1, characterized in that, The first rigid plate (100) is arranged in parallel with the flexible plate (300).

10. The rigid-flexible plate according to claim 1, characterized in that, The second rigid plate (200) is arranged in parallel with the flexible plate (300).