Laminate and photovoltaic module using the same

By adding a conductive adhesive layer to the photovoltaic module to prevent sodium ions from migrating to the surface of the solar cells, the PID effect problem of the photovoltaic module is solved, the efficiency and stability of the module are improved, and the service life of the module is extended.

CN225003992UActive Publication Date: 2026-11-20TRINA SOLAR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522073413.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-09-25
Publication Date
2026-11-20
Estimated Expiration
2035-09-25

AI Technical Summary

Technical Problem

Existing technologies are insufficient to effectively improve the PID effect of photovoltaic modules, and traditional improvement methods suffer from sodium ion migration and enrichment problems, which affect module efficiency and lifespan.

Method used

A first conductive adhesive layer and a second conductive adhesive layer are set in the photovoltaic module to prevent sodium ions from migrating to the surface of the cell. Sodium ions are gathered on the conductive adhesive layer to avoid the accumulation of negative charge. The high resistivity adhesive film is used to further improve the module efficiency.

Benefits of technology

It effectively improves the PID effect, enhances the efficiency and stability of photovoltaic modules, reduces resistivity loss, and extends module lifespan.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225003992U_ABST
    Figure CN225003992U_ABST
Patent Text Reader

Abstract

This application provides a laminate and a photovoltaic module applicable thereto, wherein the laminate includes: a battery string, the battery string including a plurality of battery cells, the battery cells including opposing first and second surfaces; a plurality of solder ribbons, the plurality of solder ribbons extending along a first direction, the plurality of solder ribbons being spaced apart on the first and second surfaces of the battery cells in a second direction different from the first direction, the plurality of solder ribbons connecting the plurality of battery cells in series; a first conductive adhesive layer, at least a portion of the surface of the battery cells being covered by the first conductive adhesive layer, at least a portion of the first conductive adhesive layer being located between two adjacent solder ribbons on the same battery cell; a second conductive adhesive layer, the second conductive adhesive layer covering the surface of at least one of the plurality of solder ribbons, at least a portion of the second conductive adhesive layer not in contact with the first conductive adhesive layer; an adhesive film, the adhesive film being located on the side of the first and second conductive adhesive layers away from the battery cells; and glass, the glass being located on the side of the adhesive film away from the first and second conductive adhesive layers.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates primarily to the field of battery technology, and in particular to a laminate and its applicable photovoltaic modules. Background Technology

[0002] Solar energy, with its advantages of safety, reliability, wide distribution, environmental friendliness, and low cost, has become one of the most promising new energy sources. Especially in remote areas with high sunshine levels, solar power generation is gradually becoming a major source of electricity for households. However, solar modules encounter numerous risk factors during actual outdoor operation, seriously threatening their long-term reliability.

[0003] PID, or Potential Induced Degradation, is one of the most common reliability risk factors for photovoltaic modules. It refers to the phenomenon where the performance of a photovoltaic module degrades significantly due to a potential difference under high-voltage operating conditions. Its core hazard is the accumulation of charge on the cell surface, which destroys the passivation effect, leading to a decrease in fill factor (FF), open-circuit voltage (Voc), and short-circuit current (Isc). Power degradation can reach 30% to 50%, severely reducing the module's lifespan. Therefore, some countries and regions have made PID resistance a key requirement for photovoltaic modules.

[0004] The generation of PID (Potential Ingress and Degradation) is related to many factors, such as system voltage and bias, aging of encapsulation materials, and ambient temperature and humidity. Although the exact mechanism is not yet fully understood, numerous studies have shown that it is mainly related to the migration of Na+ ions in the glass. When photovoltaic modules are connected in series, a high system voltage is formed (e.g., the open-circuit voltage of 20 series-connected modules can reach 860–1000V), especially in systems with the negative electrode grounded, where a high negative bias (close to 1000V) is formed between the cells and the metal frame. With prolonged use, the encapsulant film ages and decomposes, producing acetic acid, which reacts with the glass to form freely moving Na+ ions. Under the influence of the high negative bias electric field, Na+ ions migrate towards the cells and accumulate on the cell surface, inducing negative charge accumulation on the cell surface. This attracts photoelectric carriers (holes) to flow towards the surface of the N-type silicon, instead of flowing towards the positive electrode (P-electrode) as in the normal state, thus leading to module power degradation.

[0005] Currently, the main method to improve PID (Potential Influence of Sodium) is to increase the resistivity of the encapsulant film (e.g., replacing conventional EVA films with high volume resistivity films such as POE or EPE), thereby slowing down the migration rate of sodium ions and improving the PID effect. However, this method still results in ion migration and accumulation, and the encapsulant film will age and decompose over long-term use. Modifying the glass with a coating is also a common approach, such as pretreating the glass surface with an ion exchange solution to reduce the sodium ion content and improve the PID effect. However, this method is complex and costly, and most importantly, sodium ion migration and accumulation still exist, making it impossible to fundamentally solve the problem. Summary of the Invention

[0006] The technical problem to be solved by this application is to provide a laminate and a photovoltaic module applicable thereto, which can effectively improve the PID effect and further improve the efficiency of the photovoltaic module.

[0007] To address the aforementioned technical problems, this application provides a laminate suitable for photovoltaic modules. The laminate includes: a battery string comprising a plurality of battery cells, each battery cell having a first surface and a second surface opposite to each other; a plurality of solder ribbons extending along a first direction and spaced apart on the first and second surfaces of the battery cells in a second direction different from the first direction, the solder ribbons connecting the plurality of battery cells in series; a first conductive adhesive layer covering at least a portion of the surface of the battery cells, at least a portion of the first conductive adhesive layer being located between two adjacent solder ribbons on the same battery cell; a second conductive adhesive layer covering the surface of at least one of the solder ribbons, at least a portion of the second conductive adhesive layer not in contact with the first conductive adhesive layer; an adhesive film located on the side of the first and second conductive adhesive layers away from the battery cells; and glass located on the side of the adhesive film away from the first and second conductive adhesive layers.

[0008] Optionally, the material of the first conductive adhesive layer is the same as the material of the second conductive adhesive layer.

[0009] Optionally, the first conductive adhesive layer and the second conductive adhesive layer respectively have the following performance parameters: the viscosity range before curing is 2000 mPa·s to 10000 mPa·s; and / or the thixotropic range before curing is 2 to 3; and / or the softening point temperature is greater than 180℃.

[0010] Optionally, the resistivity of the adhesive film is greater than or equal to 10 times the resistivity of the first conductive adhesive layer or the second conductive adhesive layer. 7 The resistivity of the first conductive adhesive layer or the second conductive adhesive layer is less than or equal to 10. 7The resistivity of the film is greater than or equal to 10 Ω·m. 14 Ω·m.

[0011] Optionally, the refractive index ranges of the first conductive adhesive layer and the second conductive adhesive layer are 1.45 to 1.5, respectively, and the refractive index range of the adhesive film is 1.48 ± 0.05.

[0012] Optionally, the coating area of ​​the first conductive adhesive layer is smaller than the projected area of ​​the battery cell. Optionally, the thickness of the first conductive adhesive layer is smaller than the thickness of the solder strip.

[0013] Optionally, the thickness of the first conductive adhesive layer ranges from 30 μm to 300 μm, and the thickness of the solder strip ranges from 0.2 mm to 0.28 mm.

[0014] Optionally, the basis weight of the adhesive film is in the range of 360 g / m³. 2 ~420G / m 2 .

[0015] Optionally, at least one of the plurality of solder strips is composed of a first region and a second region, wherein the first conductive adhesive layer covers the first region and the second conductive adhesive layer covers 5% to 80% of the second region.

[0016] Compared with the prior art, this application provides a first conductive adhesive layer and a second conductive adhesive layer on the solar cell. When the glass reaction forms freely moving sodium ions, the freely moving sodium ions will not move directly to the solar cell, but will migrate to the conductive adhesive layer. This prevents sodium ions from accumulating on the surface of the solar cell, thereby avoiding the accumulation of negative charges on the surface of the solar cell. This allows the photovoltaic module to improve the PID effect and further improve the efficiency of the photovoltaic module. Attached Figure Description

[0017] The accompanying drawings are included to provide a further understanding of this application; they are incorporated into and constitute a part of this application. The drawings illustrate embodiments of this application and, together with this specification, serve to explain the principles of this application. In the drawings:

[0018] Figure 1 This is a schematic diagram of the structure of a laminate in one embodiment of this application;

[0019] Figure 2 , Figure 3 , Figure 4 and Figure 5 These are schematic diagrams of a laminated component under different working states according to an embodiment of this application;

[0020] Figure 6 This is a partial structural schematic diagram of a laminate in one embodiment of this application. Detailed Implementation

[0021] To more clearly illustrate the technical solutions of the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are merely some examples or embodiments of this application. For those skilled in the art, these drawings can be applied to other similar scenarios without creative effort. Unless obvious from the context or otherwise specified, the same reference numerals in the drawings represent the same structures or operations.

[0022] As indicated in this application and claims, unless the context clearly indicates otherwise, the words "a," "an," "an," and / or "the" are not specifically singular and may include plural forms. Generally speaking, the terms "comprising" and "including" only indicate the inclusion of explicitly identified steps and elements, which do not constitute an exclusive list, and the method or apparatus may also include other steps or elements.

[0023] Unless otherwise specifically stated, the relative arrangement, numerical expressions, and values ​​of the components and steps described in these embodiments do not limit the scope of this application. It should also be understood that, for ease of description, the dimensions of the various parts shown in the drawings are not drawn to actual scale. Techniques, methods, and devices known to those skilled in the art may not be discussed in detail, but where appropriate, such techniques, methods, and devices should be considered part of the specification. In all examples shown and discussed herein, any specific values ​​should be interpreted as merely exemplary and not as limitations. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters in the following drawings denote similar items; therefore, once an item is defined in one drawing, it need not be further discussed in subsequent drawings.

[0024] In the description of this application, it should be understood that the orientation or positional relationship indicated by directional terms such as "front, back, up, down, left, right", "horizontal, vertical, horizontal" and "top, bottom" is usually based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of describing this application and simplifying the description. Unless otherwise stated, these directional terms do not indicate or imply that the device or element referred to must have a specific orientation or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation on the scope of protection of this application; the directional terms "inner" and "outer" refer to the inner and outer contours relative to the outline of each component itself.

[0025] For ease of description, spatial relative terms such as "above," "on top of," "on the upper surface of," "above," etc., are used herein to describe the spatial positional relationship of a device or feature as shown in the figures to other devices or features. It should be understood that spatial relative terms are intended to encompass different orientations in use or operation beyond the orientation of the device as described in the figures. For example, if the device in the figures were inverted, a device described as "above" or "on top of" other devices or structures would subsequently be positioned as "below" or "under" other devices or structures. Thus, the exemplary term "above" can include both "above" and "below." The device may also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatial relative descriptions used herein will be interpreted accordingly.

[0026] Furthermore, it should be noted that the use of terms such as "first" and "second" to define components is merely for the purpose of distinguishing the corresponding components. Unless otherwise stated, these terms have no special meaning and therefore should not be construed as limiting the scope of protection of this application. In addition, although the terminology used in this application is selected from commonly known and used terms, some terms mentioned in this application's specification may have been chosen by the applicant according to his or her judgment, and their detailed meanings are explained in the relevant sections of this description. Moreover, this application should be understood not only through the actual terms used, but also through the meaning implied by each term.

[0027] This application refers to Figures 1-6 A laminate 10 is proposed, suitable for photovoltaic modules, which include multiple laminates proposed in any embodiment of this application, such as the laminate 10 described above. (Refer to...) Figure 1 As shown, the laminate 10 mainly includes a battery string 20, multiple solder strips 12, a first conductive adhesive layer 13, a second conductive adhesive layer 14, an adhesive film 15, and glass 16.

[0028] Specifically, the battery string 20 includes multiple battery cells 11, and each battery cell 11 includes a first surface S1 and a second surface S2 (see reference). Figure 1 Multiple solder strips 12 extend along a first direction Y, and are spaced apart on the first surface S1 and the second surface S2 of the battery cell 11 in a second direction X different from the first direction Y. Multiple solder strips 12 are connected in series with multiple battery cells 11 (see reference). Figure 5 In this embodiment, the first direction Y is perpendicular to the second direction X. In other embodiments of this application, the first direction Y and the second direction X may not be perpendicular, and this application does not impose any restrictions on this.

[0029] Further, clearer reference Figure 1 The laminate 10 further includes a first conductive adhesive layer 13 and a second conductive adhesive layer 14. At least a portion of the surface of the battery cell 11 is covered by the first conductive adhesive layer 13, and at least a portion of the first conductive adhesive layer 13 is located between two adjacent solder strips 12 on the same battery cell 11. The second conductive adhesive layer 14 covers the surface of at least one of the solder strips 12, and at least a portion of the second conductive adhesive layer 14 does not contact the first conductive adhesive layer 13. This embodiment is preferred, and more clearly illustrated, with reference to... Figure 6 At least one of the solder strips 12 has a surface consisting of a first region A1 and a second region A2. A first conductive adhesive layer 13 covers the first region A1, and a second conductive adhesive layer 14 covers 5% to 80% of the second region A2. In other embodiments of this application, the second conductive adhesive layer 14 may cover 20%, 40%, 60%, or 80% of the solder strip area, and this application does not impose any limitation on this.

[0030] In this embodiment, return to reference Figure 1 The laminate 10 also includes an adhesive film 15 and a glass 16. The adhesive film 15 is located on the side of the first conductive adhesive layer 13 and the second conductive adhesive layer 14 away from the battery cell 11, and the glass 16 is located on the side of the adhesive film 15 away from the first conductive adhesive layer 13 and the second conductive adhesive layer 14.

[0031] Generally, as the glass 16 and encapsulant 15 in the laminate 10 age over time, the glass 16 will age and form freely moving sodium ions, thus creating a potential difference between the glass 16 and the solar cell 11 and the solder ribbon 12. At this time, the sodium ions will migrate to the solar cell under the influence of the potential difference, inducing negative charges to accumulate on the surface of the solar cell. However, by setting a first conductive adhesive layer 13 and a second conductive adhesive layer 14 in the laminate 10, when the glass 16 ages and forms freely moving sodium ions, the sodium ions can be gathered on the first conductive adhesive layer 13 or the second conductive adhesive layer 14, thereby preventing the sodium ions from migrating to the surface of the solar cell 11, thus avoiding the PID effect and further improving the efficiency of the photovoltaic module.

[0032] In this preferred embodiment, the first conductive adhesive layer 13 and the second conductive adhesive layer 14 can be cured by UV heating or other methods before the laminate 10 is laminated. Since the first conductive adhesive layer 13 and the second conductive adhesive layer 14 are cured before the laminate 10 is laminated, no overflow of adhesive occurs during the lamination process, avoiding the risk of short circuits caused by overflow. Before curing, the first conductive adhesive layer 13 and the second conductive adhesive layer 14 are in a liquid state and can be coated using a doctor blade coater or a wire rod coater. For example, a wire rod coater is preferred when the thickness of the first conductive adhesive layer 13 or the second conductive adhesive layer 14 is within 150 μm, and a doctor blade coater is preferred when the adhesive thickness is between 150 μm and 300 μm. The doctor blade coater has a thickness adjustment range of 0.1 mm to 10 mm and an accuracy of ±0.003 mm, while the wire rod coater has a thickness adjustment range of 10 μm to 200 μm and an accuracy of ±0.001 mm. The choice of coating machine can be determined based on the actual application, and this application does not impose any restrictions on this.

[0033] In this embodiment, the first conductive adhesive layer 13 and the second conductive adhesive layer 14 are coated on the surface of the battery cell 11 in liquid form, which makes it easier to achieve close contact with the battery surface. After the first conductive adhesive layer 13 and the second conductive adhesive layer 14 are cured, the molecules inside the first conductive adhesive layer 13 and the second conductive adhesive layer 14 cross-link and become solid, and are tightly connected to the battery surface, thereby further improving the stability of the laminate 10.

[0034] In this embodiment, the material of the first conductive adhesive layer 13 is the same as that of the second conductive adhesive layer 14. For example, the first conductive adhesive layer 13 and the second conductive adhesive layer 14 have the following performance parameters: a viscosity range of 2000 mPa·s to 10000 mPa·s before curing; a thixotropic range of 2 to 3 before curing; and / or a softening point temperature greater than 180°C. Through the above-described configuration of the first conductive adhesive layer 13 and the second conductive adhesive layer 14, the viscosity of the first conductive adhesive layer 13 and the second conductive adhesive layer 14 is very high and almost non-flowing. Therefore, when the first conductive adhesive layer 13 and the second conductive adhesive layer 14 are coated onto the battery cell 11 in liquid form, the fluidity is very low, thereby ensuring that the first conductive adhesive layer 13 and the second conductive adhesive layer 14 will not experience overflow or other issues before curing. Furthermore, this application can also control the thickness of the first conductive adhesive layer 13 and the second conductive adhesive layer 14 by changing the viscosity, thixotropy and other process parameters of the first conductive adhesive layer 13 and the second conductive adhesive layer 14, so as to adapt to different battery processes, making the laminate 10 more compatible and further improving the flexibility of the laminate 10 in use.

[0035] Furthermore, the resistivity of the adhesive film 15 is greater than or equal to 10 times the resistivity of the first conductive adhesive layer 13 or the second conductive adhesive layer 14. 7 The resistivity of the first conductive adhesive layer 13 or the second conductive adhesive layer 14 is less than or equal to 10⁻⁶. 7 Ω·m, the resistivity of film 15 is greater than or equal to 10 Ω·m. 14 Ω·m. The above configuration ensures that the first conductive adhesive layer 13 and the second conductive adhesive layer 14, with their lower resistivity, are almost negligible compared to the high-resistivity adhesive film 15, thereby preventing an increase in the offset voltage of sodium ions in either the first conductive adhesive layer 13 or the second conductive adhesive layer 14. Furthermore, the high-resistivity adhesive film 15 can have a larger offset voltage, while the low-resistivity first conductive adhesive layer 13 and the second conductive adhesive layer 14 will have lower offset voltages, thus reducing the risk of positively charged ions (e.g., freely moving sodium ions formed after the glass reaction) shifting within the first and second conductive adhesive layers 13 and 14.

[0036] On the other hand, the refractive index range of the first conductive adhesive layer 13 and the second conductive adhesive layer 14 is 1.45 to 1.5, and the refractive index range of the adhesive film 15 is 1.48 ± 0.05. By setting the refractive index difference between the first conductive adhesive layer 13, the second conductive adhesive layer 14, and the adhesive film to no more than 0.1, the light utilization loss of the laminate 10 can be further reduced, thereby improving the light utilization efficiency of the photovoltaic module and further improving the performance of the photovoltaic module.

[0037] In this embodiment, the coating area of ​​the first conductive adhesive layer 13 is smaller than the area of ​​the battery cell 11. For example, see reference... Figure 3 As shown, Figure 3 This is a schematic diagram of the structure of laminate 10 when only the first conductive adhesive layer 13 is coated during the manufacturing process, as shown below. Figure 3 As shown, the solar cell 11 has four edges c1, c2, c3, and c4. When coating the first conductive adhesive layer 13, the edges of the first conductive adhesive layer 13 are kept at a distance from the four edges c1, c2, c3, and c4 of the solar cell 11, respectively. This distance ranges from 0 to 3 mm, and is preferably 2 mm in this application. By maintaining a sufficient distance between the first conductive adhesive layer 13 and the edges of the solar cell 11 when coating, the risk of adhesive overflow in the laminate 10 can be further reduced, thereby further improving the performance of the photovoltaic module.

[0038] Furthermore, in this embodiment, the thickness of the first conductive adhesive layer 13 is less than the thickness of the solder strip 12. Preferably, the thickness of the first conductive adhesive layer ranges from 30μm to 300μm, such as 30μm, 100μm, 130μm, 200μm, 230μm, and 300μm. The thickness of the solder strip ranges from 0.2mm to 0.28mm, such as 0.2mm, 0.22mm, 0.24mm, 0.26mm, and 0.28mm. By setting the thickness of the first conductive adhesive layer 13 to be less than the thickness of the solder strip 12, the material used for the first conductive adhesive layer 13 can be further saved, thereby further saving the cost of the laminate 10.

[0039] In this embodiment, in fact, the thinner the first conductive adhesive layer 13, the higher the efficiency of the photovoltaic module. This can be seen in Table 1 below, which shows the specific experimental data on the transmittance and external quantum efficiency (EQE) of the first conductive adhesive layer 13 with different thicknesses:

[0040] Example 1 Example 2 Example 3 The first conductive adhesive layer has a thickness of 13 μm. 30 60 150 <![CDATA[15 g weight per square meter of adhesive film G / m 2 > 380 380 380 280nm~380nm transmittance % 48.28 46.36 39.19 380nm~1100nm transmittance % 92.91 92.74 92.42 <![CDATA[EQE1100nm mA / cm 2 ]]> 38.979 38.973 38.954 PID 96h Appearance normal normal normal

[0041] Table 1

[0042] In the table above:

[0043] Examples 1, 2, and 3 are identical in structure except for the thickness of the first conductive adhesive layer 13. The battery cell 11 in Examples 1, 2, and 3 is TOPCon, 210 specification; the solder ribbon 12 is a standard room-temperature solder ribbon with a thickness of 0.28 mm; and the adhesive film 15 is a standard high-transparency EVA film with a basis weight of 380 g / m³. 2 Glass 16 is conventional high-transmittance glass. As shown in Table 1, firstly, when the thickness of the first conductive adhesive layer 13 changes, the photovoltaic module composed of the laminate 10 maintains a normal appearance after PID96h, indicating that changing the thickness of the first conductive adhesive layer 13 does not alter the anti-PID effect of the laminate 10. Furthermore, the smaller the thickness of the first conductive adhesive layer 13, the higher the transmittance in the spectral ranges of 280nm–380nm and 380nm–1100nm, thereby improving the light utilization rate of the photovoltaic module composed of the laminate 10. Additionally, the smaller the thickness of the first conductive adhesive layer 13, the larger the EQE of the photovoltaic module composed of the laminate 10, further improving the efficiency of the photovoltaic module.

[0044] In this embodiment, the basis weight of the adhesive film 15 is in the range of 360 g / m³. 2 ~420G / m 2 For example, 360G / m 2 380G / m 2 400G / m2 and 420G / m 2 For example, film 15 can be an EVA film.

[0045] The preparation process of laminate 10 will now be briefly described, referring to... Figures 2-5 As shown, the fabrication process of the laminate 10 includes steps S1 to S5. (Refer to...) Figure 3 Step S1 includes coating a first conductive adhesive layer 13 onto a portion of the surface of the battery cell 11, and leaving a space on the surface of the battery cell 11 for placing the solder ribbon 12, maintaining a distance h between the edge of the first conductive adhesive layer 13 and the edge of the battery cell 11, wherein h ranges from 0 mm to 3 mm; (Refer to...) Figure 4 Step S2 includes placing the solder ribbon 12 and coating a portion of the solder ribbon 12 with a second conductive adhesive layer 14, such that the second conductive adhesive layer 14 occupies 5% to 80% of the solder ribbon area; Step S3 includes curing the first conductive adhesive layer 13 and the second conductive adhesive layer 14; Refer to Figure 5 Step S4 includes sequentially stacking the adhesive film 15 and the glass 16; step S5 includes laminating the adhesive film 15 and the glass 16.

[0046] In this application, the first conductive adhesive layer 13 and the second conductive adhesive layer 14 are respectively covered on the surface of the solar cell 11 and the surface of the solder ribbon 12. The total resistance of the solar cell 11 can be reduced by the parallel connection of the first conductive adhesive layer 13, the second conductive adhesive layer 14, the solar cell 11 and the solder ribbon 12. Since the photovoltaic module provided in this application usually contains multiple parallel laminates 10, the above arrangement can effectively improve the series resistance of the photovoltaic module and enhance the electrical performance of the photovoltaic module.

[0047] The basic concepts have been described above. Obviously, for those skilled in the art, the above disclosure is merely illustrative and does not constitute a limitation of this application. Although not explicitly stated herein, those skilled in the art may make various modifications, improvements, and corrections to this application. Such modifications, improvements, and corrections are suggested in this application, and therefore remain within the spirit and scope of the exemplary embodiments of this application.

[0048] Furthermore, this application uses specific terms to describe embodiments of the application. For example, "an embodiment," "one embodiment," and / or "some embodiments" refer to a particular feature, structure, or characteristic related to at least one embodiment of the application. Therefore, it should be emphasized and noted that "an embodiment," "one embodiment," or "an alternative embodiment" mentioned twice or more in different locations in this specification do not necessarily refer to the same embodiment. In addition, certain features, structures, or characteristics in one or more embodiments of the application can be appropriately combined.

[0049] Similarly, it should be noted that, in order to simplify the description of the present application and thus aid in the understanding of one or more embodiments, the foregoing description of the embodiments of the present application sometimes combines multiple features into a single embodiment, drawing, or description thereof. However, this disclosure method does not imply that the subject matter of the present application requires more features than those mentioned in the claims. In fact, the embodiments contain fewer features than all the features of the single embodiments disclosed above.

[0050] In some embodiments, numbers describing the quantity of components and attributes are used. It should be understood that such numbers used in the description of embodiments are modified in some examples with the terms "approximately," "approximately," or "generally." Unless otherwise stated, "approximately," "approximately," or "generally" indicates that the numbers are allowed to vary by ±20%. Accordingly, in some embodiments, the numerical parameters used in the specification and claims are approximate values, which may be changed depending on the characteristics required by individual embodiments. In some embodiments, numerical parameters should take into account specified significant digits and employ a general method of digit reservation. Although the numerical ranges and parameters used to confirm their breadth of scope in some embodiments of this application are approximate values, in specific embodiments, such values ​​are set as precisely as feasible.

[0051] Although this application has been described with reference to specific embodiments, those skilled in the art should recognize that the above embodiments are only used to illustrate this application, and various equivalent changes or substitutions can be made without departing from the spirit of this application. Therefore, any changes or modifications to the above embodiments within the essential spirit of this application will fall within the scope of the claims of this application.

Claims

1. A laminate suitable for photovoltaic modules, characterized in that, The laminate includes: A battery string, the battery string comprising a plurality of battery cells, the battery cells comprising opposing first and second surfaces; Multiple solder strips extend along a first direction and are spaced apart on the first and second surfaces of the battery cell in a second direction different from the first direction, and the multiple solder strips connect the multiple battery cells in series; A first conductive adhesive layer is provided, at least a portion of the surface of the battery cell is covered by the first conductive adhesive layer, and at least a portion of the first conductive adhesive layer is located between two adjacent solder strips on the same battery cell. A second conductive adhesive layer covers the surface of at least one of the plurality of solder strips, and at least a portion of the second conductive adhesive layer does not contact the first conductive adhesive layer. An adhesive film, the adhesive film being located on the side of the first conductive adhesive layer and the second conductive adhesive layer away from the battery cell; and Glass, the glass being located on the side of the adhesive film away from the first conductive adhesive layer and the second conductive adhesive layer.

2. The laminate as described in claim 1, characterized in that, The material of the first conductive adhesive layer is the same as that of the second conductive adhesive layer.

3. The laminate as described in claim 2, characterized in that, The first conductive adhesive layer and the second conductive adhesive layer each have the following performance parameters: The viscosity range before curing is 2000 mPa·s to 10000 mPa·s; and / or The thixotropic range before curing is 2–3; and / or The softening point temperature is greater than 180℃.

4. The laminate as described in claim 3, characterized in that, The resistivity of the adhesive film is greater than or equal to 10% of the resistivity of the first conductive adhesive layer or the second conductive adhesive layer. 7 The resistivity of the first conductive adhesive layer or the second conductive adhesive layer is less than or equal to 10. 7 The resistivity of the film is greater than or equal to 10 Ω·m. 14 Ω·m.

5. The laminate as claimed in claim 1, characterized in that, The refractive index ranges of the first conductive adhesive layer and the second conductive adhesive layer are 1.45 to 1.5, respectively, and the refractive index range of the adhesive film is 1.48 ± 0.

05.

6. The laminate as claimed in claim 1, characterized in that, The coating area of ​​the first conductive adhesive layer is smaller than the area on the battery cell.

7. The laminate as claimed in claim 1, characterized in that, The thickness of the first conductive adhesive layer is less than the thickness of the solder strip.

8. The laminate as claimed in claim 7, characterized in that, The thickness of the first conductive adhesive layer ranges from 30μm to 300μm, and the thickness of the solder strip ranges from 0.2mm to 0.28mm.

9. The laminate as claimed in claim 1, characterized in that, The basis weight of the adhesive film is in the range of 360 g / m³. 2 ~420G / m 2 .

10. The laminate according to any one of claims 1 to 9, characterized in that, The surface of at least one of the plurality of solder strips is composed of a first region and a second region, wherein the first conductive adhesive layer covers the first region and the second conductive adhesive layer covers 5% to 80% of the second region.

11. A photovoltaic module, characterized in that, Includes the laminate as described in any one of claims 1 to 9.