Semiconductor package
By forming a protective layer with an inclined or stepped surface profile beneath the under-bump metallization layer in a semiconductor package, the interfacial stress problem is solved, the risk of cracking and delamination is reduced, and the resistance and device performance are improved.
Patent Information
- Application Number
- CN202522353026.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Priority Date
- 2024-11-21
- Filing Date
- 2025-11-06
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-11-06
AI Technical Summary
As the integration density of semiconductor devices increases, existing technologies struggle to effectively reduce the interfacial stress between the under-bump metallization layer and the protective layer, leading to an increased risk of cracks and delamination.
A protective layer with an inclined or stepped surface profile is formed under the under-bump metallization layer to reduce interfacial stress by forming grooves in the protective layer and reshaping its surface to match the shape of the under-bump metallization layer.
It reduces the interfacial stress between the metallization layer under the bump and the protective layer, reduces the risk of cracks and delamination, and improves resistance and device performance.
Smart Images

Figure CN225004129U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to a package, and more particularly to a semiconductor package. Background Technology
[0002] The semiconductor industry has experienced rapid growth due to the ever-increasing integration density of various electronic components, such as transistors, diodes, resistors, and capacitors. In most cases, this increase in integration density is due to the continuous shrinking of the smallest feature size, allowing more components to be integrated into a given area. As the demand for miniaturized electronic devices continues to grow, so too does the need for smaller, more innovative semiconductor die packaging technologies. Utility Model Content
[0003] This utility model provides a semiconductor package comprising: a dielectric layer on a conductive component; a polymer layer on the dielectric layer, wherein the polymer layer includes a stepped upper surface; and a bump under-metallization layer on the stepped upper surface of the polymer, wherein the bump under-metallization layer extends through the polymer layer and the dielectric layer to contact the conductive component.
[0004] In one embodiment, the stepped upper surface includes a plurality of horizontal surfaces separated by a plurality of inclined surfaces.
[0005] In one embodiment, the lengths of the plurality of horizontal surfaces are the same.
[0006] In one embodiment, the lengths of the plurality of horizontal surfaces are different from each other.
[0007] In one embodiment, the stepped upper surface includes a plurality of horizontal surfaces separated by a plurality of curved surfaces.
[0008] In one embodiment, the lengths of the plurality of horizontal surfaces are the same.
[0009] In one embodiment, the lengths of the plurality of horizontal surfaces are different from each other.
[0010] In one embodiment, the stepped upper surface laterally surrounds the conductive component.
[0011] In one embodiment, the stepped upper surface includes an inclined top surface.
[0012] In one embodiment, the metallization layer under the bump completely covers the stepped upper surface. Attached Figure Description
[0013] The various aspects of this utility model will be described in detail below with reference to the accompanying drawings. It should be noted that, in accordance with industry standard practice, the various features are not drawn to scale and are for illustrative purposes only. In fact, the dimensions of the units may be arbitrarily enlarged or reduced to clearly demonstrate the features of this utility model.
[0014] According to some embodiments of the present invention, Figures 1 to 16 are cross-sectional views of the under-bump metallization (UBM) structure of a semiconductor device at an intermediate stage of its formation.
[0015] According to some embodiments of the present invention, Figures 17A to 17F are cross-sectional views of the groove surface of the protective layer.
[0016] Explanation of reference numerals in the attached figures: 100: Device 102: Substrate 104: Apparatus 106: Grain 108: Dielectric / ILD 110: Insert plug 112: Interconnection Structure 114: Line 116: Through hole 118: Dielectric layer 120: Metal parts 122: Dielectric layer 124: Passivation layer 126: Opening 128: Seed layer 130: Optical Resistor 132: Opening 134: Conductive materials 136: RDL 140: Passivation layer 142: Passivation layer 144: Opening 146: Protective layer 147: Surface 148: Groove 150: Mask 151: Light Source 152: Seed layer 154: Optical Obscuration 155: Opening 156: Conductive materials 160: Under-bump metallization layer / UBM 162: Conductive connector 170: Region 146': Exposure Zone 146A: District 146B: District 146C: District 147': Sidewall 147A: Surface 147B: Surface 147C: Surface 147D: Surface 147E: Surface 147F: Surface 150A: Opaque Area 150B: Opaque Area 150C: Opaque area A1: Angle A2: Angle A3: Angle D1: Distance H1: Height H2: Height L1: Length L2: Length P1: Point P2: Point T1: Thickness T2: Thickness Detailed Implementation
[0017] The following provides many different embodiments or examples to achieve different features of the present invention. Specific examples of components and configurations are described below to simplify the present invention. Of course, these are merely examples and are not intended to limit the present invention. For example, the following description mentions forming a first component on or above a second component, which may include embodiments where the first and second components are formed in direct contact, and may also include embodiments where an additional component is formed between the first and second components, such that the first and second components do not need to be in direct contact. Furthermore, the present invention may repeat element symbols and / or letters in many examples. These repetitions are for simplification and clarity and do not in themselves represent a specific relationship between the various embodiments and / or configurations discussed.
[0018] Spatially relative terms, such as "below," "under," "lower," "above," and "higher," may be used here to facilitate the description of the relationship between one or more components or features in the accompanying drawings and another component or feature(s). Spatially relative terms are used to include different orientations of the device in use or operation, as well as the orientations described in the accompanying drawings. When the device is turned to different orientations (rotated 90 degrees or other orientations), the spatially relative adjectives used will also be interpreted according to the orientation after the turn.
[0019] Various embodiments provide methods and structures for forming a protective layer beneath an under-bump metallization (UBM) layer. The surface of the protective layer covered by the UBM can be formed with a sloped and / or stepped surface profile, which can reduce interfacial stresses at the protective layer, such as the interfacial stress between the protective layer and the UBM. This can reduce the risk of cracks, delamination, or other stress-related defects.
[0020] According to some embodiments of the present invention, Figures 1 to 16 are cross-sectional views of the under-bump metallization (UBM) structure of a semiconductor device at an intermediate stage of formation. It should be understood that although device wafers and device dies are used as examples, embodiments of the present invention can also be applied to the formation of conductive components in other devices (e.g., packaged elements), including but not limited to package substrates, interposers, packages, etc. For example, in some cases, the embodiments described in the present invention can be applied to semiconductor packages.
[0021] Figure 1 This shows a cross-sectional view of a semiconductor device 100. In some embodiments, the semiconductor device 100 is a device wafer including active and / or passive devices, which is represented as an integrated circuit device 104. The semiconductor device 100 can be diced to form a plurality of chips / dies 106 therefrom. Figure 1 The image shows a single die 106. In some embodiments, the semiconductor device 100 is an interposer wafer that has no active devices and may include passive devices. In some embodiments, the semiconductor device 100 is a package substrate strip that includes a coreless package substrate or a cored package substrate having a core therein. In the following discussion, a device wafer is used as an example of the semiconductor device 100, and the semiconductor device 100 may be referred to as a wafer. Embodiments of this invention can also be applied to interposer wafers, package substrates, packages, etc.
[0022] In some embodiments, the die 106 includes logic dies (e.g., central processing units (CPUs), graphics processing units (GPUs), systems-on-chips (SoCs), application processors (APs), microcontrollers, application-specific integrated circuits (ASIC dies, etc.), memory dies (e.g., dynamic random access memory (DRAM) dies, static random access memory (SRAM) dies, high bandwidth memory (HBM) dies, etc.), power management dies (e.g., power management integrated circuit (PMIC) dies), radio frequency (RF) dies, sensor dies, microelectromechanical systems (MEMS) dies, signal processing dies (e.g., digital signal processing (DSP) dies, etc.), front-end dies (e.g., analog front-end (AFE) dies), etc., or combinations thereof. It may also be other types of dies, chips, integrated circuit devices, semiconductor devices, etc.
[0023] In some embodiments, the semiconductor device 100 includes a semiconductor substrate 102 and components formed on the top surface of the semiconductor substrate 102. The semiconductor substrate 102 may be a bulk semiconductor, a semiconductor-on-insulator (SOI) substrate, etc., and may be doped (e.g., with p-type or n-type dopants) or undoped. The semiconductor substrate 102 may be a wafer, such as a silicon wafer. Generally, an SOI substrate is a layer of semiconductor material formed on an insulating layer. The insulating layer may be, for example, a buried oxide (BOX) layer, a silicon oxide layer, etc. The insulating layer is disposed on the substrate, typically a silicon or glass substrate. Other substrates may also be used, such as multilayer or gradient substrates. In some embodiments, the semiconductor material of the semiconductor substrate 102 may include silicon; germanium; compound semiconductors, including silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, including silicon-germanium, gallium arsenide phosphide, aluminum indium arsenide, aluminum gallium arsenide, gallium indium arsenide, gallium indium phosphide, and / or gallium arsenide phosphide; or combinations thereof. Shallow trench isolation (STI) regions (not shown separately) may be formed in the semiconductor substrate 102 to isolate active regions in the semiconductor substrate 102. Vias (not shown separately) may be formed to extend into or through the semiconductor substrate 102 (e.g., vias) and may be used to electrically interconnect components on opposite sides of the semiconductor device 100.
[0024] In some embodiments, the semiconductor device 100 is a stacked device comprising a plurality of semiconductor substrates 102. For example, the semiconductor device 100 may be a memory device, such as a hybrid memory cube (HMC) module, a high-bandwidth memory (HBM) module, etc., which includes a plurality of memory dies. In such embodiments, the semiconductor device 100 includes a plurality of semiconductor substrates 102 interconnected via through-substrate vias (TSVs). Each semiconductor substrate 102 may (or may not) have an interconnect structure (e.g., interconnect structure 112, as described below).
[0025] In some embodiments, the semiconductor device 100 includes an integrated circuit device 104 formed on the top surface of a semiconductor substrate 102. The integrated circuit device 104 may include complementary metal-oxide-semiconductor (CMOS) transistors, FinFETs, nanostructured FETs, resistors, capacitors, diodes, etc. Details of the integrated circuit device 104 are not shown here. In some embodiments, the semiconductor device 100 is used to form an interposer (which does not contain active devices), and the semiconductor substrate 102 may be a semiconductor substrate or a dielectric substrate.
[0026] In some embodiments, an interlayer dielectric (ILD) 108 may be formed on a semiconductor substrate 102 and may fill the space between the gate stacks (not shown separately) of transistors in an integrated circuit device 104. In some embodiments, the ILD 108 is formed of phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), fluorine-doped silicate glass (FSG), silicon oxide, silicon nitride, silicon oxynitride, low-k (dielectric constant) dielectric materials, combinations thereof, or multiples thereof. The ILD 108 may be formed using suitable techniques, such as spin coating, flow chemical vapor deposition (FCVD), etc. In some embodiments, the ILD 108 is formed using deposition methods such as plasma-assisted chemical vapor deposition (PECVD), low-pressure chemical vapor deposition (LPCVD), etc.
[0027] Contact plugs 110 are formed in the ILD 108 and are used to electrically connect the integrated circuit device 104 to the metal lines and / or vias above. In some embodiments, contact plugs 110 are formed of one or more conductive materials, such as tungsten, aluminum, copper, titanium, tantalum, titanium nitride, tantalum nitride, alloys thereof, multilayers thereof, etc. The formation of contact plugs 110 may include forming contact openings in the ILD 108, depositing conductive material into the contact openings, and performing planarization processes (e.g., chemical mechanical polishing (CMP), mechanical polishing, etch-back processes, etc.) to make the top surface of contact plugs 110 flush with the top surface of the ILD 108.
[0028] According to some embodiments, an interconnect structure 112 is formed on the ILD 108 and the contact plug 110. The interconnect structure 112 includes metal lines 114 and metal vias 116 formed in a plurality of dielectric layers 118. In some cases, the dielectric layer 118 may be referred to as an intermetallic dielectric (IMD). The metal lines 114 formed at the same level (e.g., on, or within the same dielectric layer 118) may be collectively referred to as a metal layer, a redistribution layer, a metallization pattern, etc. In some embodiments, the interconnect structure 112 includes a plurality of metal layers, the plurality of metal layers including metal lines 114 interconnected through metal vias 116. The metal lines 114 and metal vias 116 may be formed of copper, copper alloys, other metals, etc.
[0029] In some embodiments, dielectric layer 118 is formed of a low-k dielectric material. For example, the dielectric constant (k value) of the low-k dielectric material may be less than about 3.0. Dielectric layer 118 may include carbon-containing low-k dielectric materials, hydrogensilsesquioxane (HSQ), methylsilsesquioxane (MSQ), combinations thereof, or multilayers thereof. In some embodiments, dielectric layer 118 may include PSG, BSG, BPSG, undoped silicate glass (USG), etc. In some embodiments, dielectric layer 118 may include oxides (e.g., silicon oxide), nitrides (e.g., silicon nitride), combinations thereof, etc. In some embodiments, dielectric layer 118 may include polymeric materials such as polyimide, polybenzoxazole (PBO), benzocyclobutene (BCB), etc. Dielectric layer 118 may be formed by suitable techniques such as CVD, FCVD, PECVD, LPCVD, spin coating, etc.
[0030] Forming metal lines 114 and metal vias 116 in the dielectric layer 118 can include a single damascene process and / or a dual damascene process. In a single damascene process, a trench or via opening is formed in one of the dielectric layers 118, and the trench or via opening is filled with a conductive material. A planarization process, such as a CMP process, is then performed to remove excess conductive material, which may be above the top surface of the dielectric layer 118, thereby leaving metal lines 114 or metal vias 116 in the corresponding trench or via opening. In a dual damascene process, both the trench and via opening are formed in the dielectric layer 118, with the via opening located below and connected to the trench. Conductive material is filled into the trench and via opening to form metal lines 114 and metal vias 116, respectively. The conductive material can include a diffusion barrier layer and a copper-containing metal material located on the diffusion barrier layer. The diffusion barrier layer can include titanium, titanium nitride, tantalum, tantalum nitride, etc. In other embodiments, other techniques may be used to form the metal line 114 and the metal via 116.
[0031] Top metal components 120 can be formed in the top dielectric layer 122, such as metal lines, metal vias, metal pads, etc. Top metal components 120 can be formed from the same or similar materials as metal lines 114 and / or metal vias 116 using the same or similar processes. Top dielectric layer 122 can be formed from the same or similar materials as dielectric layer 118 using the same or similar processes. Top metal components 120 can refer to the topmost metal layer in the interconnect structure 112. Although... Figure 1 The interconnect structure 112 is shown as having a specific number of metal layers, but in other embodiments it may include any number of metal layers. The top dielectric layer 122 and the lower dielectric layer 118 immediately below the top dielectric layer 122 may be formed as a single continuous dielectric layer, may be formed as different dielectric layers using different processes, and / or may be formed from different materials.
[0032] A first passivation layer 124 may be formed on the interconnect structure 112 (e.g., on the top dielectric layer 122). The first passivation layer 124 may be formed from a single material layer or may comprise two or more layers of different materials, collectively referred to as the first passivation structure. In some embodiments, the first passivation layer 124 may include PSG, BSG, BPSG, USG, etc. In some embodiments, the first passivation layer 124 may include inorganic dielectric materials such as silicon oxide, silicon nitride, silicon oxynitride, silicon carbide, silicon carbide, low-k dielectric materials, combinations thereof, multilayers thereof, etc. For example, in some embodiments, the first passivation layer 124 may be a passivation structure comprising a USG layer over a silicon nitride layer. Other materials or combinations thereof may also be used. One or more suitable techniques may be used to deposit the first passivation layer 124, such as CVD, physical vapor deposition (PVD), atomic layer deposition (ALD), etc. In some embodiments, the top surface of the top dielectric layer 122 and the top surface of the top metal component 120 are coplanar (e.g., flush with each other). Therefore, the first passivation layer 124 can be a planar layer. In some embodiments, the top metal component 120 protrudes above the top surface of the top dielectric layer 122, and in such embodiments, the first passivation layer 124 may not be planar.
[0033] exist Figure 2 In some embodiments, an opening 126 is formed in the first passivation layer 124. The opening 126 can be formed using a suitable etching process (e.g., a dry etching process). The etching process may include, for example, forming a patterned etch mask (not shown separately), such as a patterned photoresist, on the interconnect structure 112, and then etching the first passivation layer 124 using the patterned etch mask. The patterned etch mask is then removed using a suitable process. The opening 126 may extend completely through the first passivation layer 124 and may expose the top metal component 120.
[0034] exist Figure 3 In some embodiments, a seed layer 128 is formed on the first passivation layer 124, in the opening 126, and on the exposed top metal component 120. The seed layer 128 may include one or more metal layers. For example, in some embodiments, the seed layer 128 may include a titanium layer and a copper layer on the titanium layer. In some embodiments, the seed layer 128 includes a copper layer in contact with the first passivation layer 124 and the top metal component 120. Other materials or combinations of materials may also be used. The seed layer 128 may be formed by a suitable deposition process, such as CVD, PVD, metal-organic chemical vapor deposition (MOCVD), etc.
[0035] exist Figure 4In some embodiments, patterned photoresist 130 is formed on seed layer 128. For example, patterned photoresist 130 can be formed by depositing a photosensitive layer on seed layer 128 using spin coating or the like. The photosensitive layer can be a single material layer or can include multiple layers of different materials. The photosensitive layer can then be patterned by exposing it to a patterned energy source (e.g., a patterned light source) and developing it to remove exposed or unexposed portions, thereby forming patterned photoresist 130. Openings 132 exposing seed layer 128 are formed in patterned photoresist 130. Figure 4 As shown, opening 132 may overlap with one or more openings 126. The pattern of the patterned photoresist 130 corresponds to the redistribution layer (RDL) subsequently formed in the patterned photoresist 130, as described below regarding Figure 5 The discussion.
[0036] exist Figure 5 In some embodiments, conductive material 134 is formed on the exposed portion of seed layer 128. Conductive material 134 may fill opening 126 and at least partially fill opening 132. Conductive material 134 may be formed by electroplating, such as electroplating, electroless plating, etc. Conductive material 134 may include metals such as copper, titanium, tungsten, aluminum, aluminum-copper, nickel, cobalt, ruthenium, combinations thereof, alloys thereof, etc. The combination of conductive material 134 and the lower portion of seed layer 128 forms a redistribution layer (e.g., Figure 6 RDL 136).
[0037] exist Figure 6 In this process, the patterned photoresist 130 and the portion of the seed layer 128 on which the conductive material 134 is not formed are removed. The patterned photoresist 130 can be removed by an acceptable ashing or stripping process (e.g., using oxygen plasma). Once the patterned photoresist 130 is removed, the exposed portion of the seed layer 128 is removed using an acceptable etching process (e.g., wet or dry etching). One or more optional cleaning processes may also be performed. According to some embodiments, the remaining portion below the conductive material 134 and the seed layer 128 forms an RDL 136. Each RDL 136 may include a via portion extending through the first passivation layer 124 and a trace / line portion on the first passivation layer 124. The via portions of the RDL 136 are physically and electrically connected to the top metal part 120 of the interconnect structure 112. Although Figure 6 Only one RDL 136 is displayed, but any number of RDL 136 can be formed on each die 106.
[0038] exist Figure 7In this embodiment, a second passivation layer 140 and a third passivation layer 142 are formed over the first passivation layer 124 and over and along the sidewalls and top surface of the RDL 136. The second passivation layer 140 and the third passivation layer 142 may be collectively referred to as the second passivation structure. The second passivation layer 140 and the third passivation layer 142 may be formed of the same or different material as the first passivation layer 124. For example, in some embodiments, the second passivation layer 140 and the third passivation layer 142 may be formed of an inorganic dielectric material, such as silicon oxide, silicon nitride, silicon oxynitride, silicon carbide, silicon carbide, combinations thereof, multilayers thereof, etc. The second passivation layer 140 may be made of a material with high etch selectivity relative to the material of the third passivation layer 142, such that the second passivation layer 140 can serve as an etch stop layer for the process of etching the third passivation layer 142. For example, in some embodiments, the second passivation layer 140 may include silicon oxide, and the third passivation layer 142 may include silicon nitride. Other materials or combinations of materials may also be used. In other embodiments, the second passivation layer 140 may be a single layer, and the third passivation layer 142 may be omitted. Suitable techniques such as CVD, ALD, PECVD, FCVD, spin coating, etc., can be used to deposit the second passivation layer 140 and the third passivation layer 142. In some embodiments, a planarization process (e.g., CMP process, polishing process, etc.) is performed on the second passivation layer 140 before the deposition of the third passivation layer 142. In such embodiments, the planarization process makes the top surface of the second passivation layer 140 flat. Figure 7 As shown, after the planarization process, RDL 136 can remain covered by the second passivation layer 140.
[0039] exist Figure 8 In some embodiments, an opening 144 is formed extending through the second passivation layer 140 and the third passivation layer 142. The opening 144 can be formed using one or more suitable etching processes, such as one or more wet or dry etching processes. In some embodiments, a patterned etch mask (not shown separately), such as a patterned photoresist, is formed on the third passivation layer 142. The patterned etch mask is then used to etch the second passivation layer 140 and the third passivation layer 142. In some embodiments, a first etching step is used to etch the third passivation layer 142, and a second etching step, which may be different from the first etching step, is used to etch the second passivation layer 140. The patterned etch mask is then removed using a suitable process. The opening 144 may extend completely through the second passivation layer 140 and the third passivation layer 142 and may expose the RDL 136. The sidewalls of the opening 144 may be oblique (e.g., oblique, tilted, tapered, etc.) or substantially vertical.
[0040] exist Figure 9 In some embodiments, a protective layer 146 is formed on the third passivation layer 142 and in the opening 144. In some embodiments, the protective layer 146 is formed of a polymeric material (which may be photosensitive), such as polyimide, polybenzoxazole (PBO), benzocyclobutene (BCB), epoxy resin, etc. The protective layer 146 can be formed by CVD, PECVD, spin coating, etc. In some embodiments, the formation of the protective layer 146 includes applying the protective layer 146 in a flowable form and then performing a baking or curing process to harden the protective layer 146. A planarization process, such as a CMP process or a polishing process, can be performed to make the top surface of the protective layer 146 flat. In some embodiments, the protective layer 146 has a thickness T1 of about 2 μm to about 5 μm above the third passivation layer 142, but other thicknesses are also possible.
[0041] According to some embodiments, the protective layer 146 can then be patterned to form a groove 148 (see reference). Figure 11 A groove 148 is formed in the protective layer 146 to expose the RDL 136 for physical and electrical connection to the subsequently formed under-bump metallization (UBM) layer 160 (see reference). Figure 15Therefore, the groove 148 may overlap with one or more openings 144. For embodiments where the protective layer 146 comprises a photosensitive material, a suitable photolithography technique can be used to pattern the protective layer 146. For example, the photosensitive protective layer 146 can be patterned by exposing the protective layer 146 to a patterned energy source (e.g., a patterned light source) and developing the protective layer 146 to remove exposed or unexposed portions of the protective layer 146. In some embodiments, during the formation of the groove 148, the protective layer 146 may be patterned such that the surface of the protective layer 146 subsequently covered by the UBM 160 is reshaped to have a specific profile, such as a sloping profile, a stepped profile, a tapered profile, a curved profile, or a combination thereof. The thickness of the protective layer 146 within the groove 148 is less than the thickness of the protective layer 146 outside the groove 148 (e.g., thickness T1). In some embodiments, the thickness of the protective layer 146 within the groove 148 typically decreases gradually towards the center of the groove 148; however, the profile of the recessed surface 147 of the protective layer 146 within the groove 148 may be inclined, stepped, and / or curved. In some cases, reshaping the protective layer 146 beneath the UBM 160 as described in this invention can reduce the interfacial stress between the UBM 160 and the protective layer 146, or can reduce the interfacial stress between the second passivation structure (e.g., the second passivation layer 140 and / or the third passivation layer 142) and the protective layer 146. In some cases, forming the recessed surface 147 beneath the UBM 160 can reduce the interfacial stress by about 15% or more. According to some embodiments, Figures 17A to 17F described below show non-limiting examples of some surface profiles of the protective layer 146 that can be formed.
[0042] According to some embodiments, Figures 10 and 11 show intermediate steps of forming the recess 148 and reshaping the protective layer 146 to have a sloping surface profile (e.g., at the recessed surface 147). The processes and surface profiles described for Figures 10 and 11 are intended as illustrative examples; other processes or surface profiles are also possible. According to some embodiments, Figures 10 and 11 show the execution of a "grayscale" lithography process. Figure 10 In this process, an exposure region 146' is formed in the protective layer 146 by exposing the protective layer 146 to the energy of the light source 151 using a grayscale lithography mask 150. The grayscale lithography mask 150 is a lithography mask with varying opacity, which allows control over the spatial distribution of exposure received by the protective layer 146. In other words, the amount of exposure received by different locations of the protective layer 146 can be controlled. The portion of the exposure region 146' receiving greater exposure has a greater depth than the portion receiving less exposure. In this way, the depth profile or shape of the exposure region 146' can be controlled by utilizing the corresponding grayscale lithography mask 150.
[0043] refer to Figure 10 As an example, the grayscale photomask 150 shown includes multiple opaque areas 150A-C. Different opaque areas 150A-C allow the underlying areas 146A-C of the protective layer 146 to receive different amounts of exposure from the light source 151. The opaque area 150A of the grayscale photomask 150 is completely opaque, so the underlying area 146A of the protective layer 146 is not exposed to the light source 151. The opaque area 150C of the grayscale photomask 150 is substantially transparent, such that the underlying area 146C of the protective layer 146 is fully exposed to the light source 151, and the depth of the corresponding portion of the exposed area 146' extends completely through the protective layer 146. The opaque area 150B of the grayscale photomask 150 has varying opacities (e.g., different opacities), such that the underlying area 146B of the protective layer 146 receives correspondingly varying exposure, and the corresponding portion of the exposed area 146' has correspondingly varying depth. For example, opaque area 150B is displayed as having an opacity gradient from mostly opaque near opaque area 150A to mostly transparent near opaque area 150C, which gives exposure area 146' a depth gradient from a smaller depth near area 146A to a larger depth near area 146C.
[0044] Figure 10 The grayscale lithography mask 150 shown is an example; other configurations of the grayscale lithography mask 150 with different opacities are possible, which can allow the exposure area 146' to include other depth profiles besides those shown. In other embodiments, multiple exposures using multiple lithography masks can be used to control the depth profile of the exposure area 146'. For example, a relatively transparent lithography mask can be used in an exposure step to form a relatively deep portion of the exposure area 146', and a relatively opaque lithography mask can be used in a separate exposure step to form a relatively shallow portion of the same exposure area 146'. In some embodiments, the use of multiple exposures can be used to form an exposure area 146' with a stepped depth profile. These and other variations and combinations thereof are all covered within the scope of this invention.
[0045] exist Figure 11 In some embodiments, the protective layer 146 is developed to form a groove 148. The protective layer 146 can be developed using a suitable photolithography technique, such as a wet chemical process or other suitable process. In some embodiments, development removes the exposed area 146' of the protective layer 146 to form the groove 148. In this way, controlling the exposure of the protective layer 146 to control the depth profile of the exposed area 146' can control the shape and size of the groove 148. For example, in Figure 11In this recess, the angled depth profile of the exposure area 146' forms a corresponding angled recessed surface 147 of the protective layer 146 within the groove 148. For example, the angled recessed surface 147 extends from the edge of the groove 148 to the sidewall 147' of the protective layer 146 within the groove 148. The recessed surface 147 may surround the opening 144. The sidewall 147' of the protective layer 146 within the groove 148 appears generally vertical, but may be angled in other embodiments. In some embodiments, the top surface of the second passivation structure (e.g., the top surface of the third passivation layer 142) is exposed by the groove 148, but in other embodiments, the second passivation structure remains covered by the protective layer 146. In other words, the sidewall 147' of the protective layer 146 and the second passivation structure may be laterally offset or laterally aligned. Figure 11 As shown, the opening 144 within the recess 148 exposes the underlying RDL 136. In some embodiments, the width of the recess 148 may be greater than the width of the underlying RDL 136. In other words, the recessed surface 147 may protrude laterally beyond the RDL 136. In some embodiments, the recessed surface 147 may laterally surround the RDL 136.
[0046] According to some embodiments, Figures 12 to 15 show the formation of UBM 160 (reference). Figure 15 This is an intermediate step in the process. UBM 160 is a conductive component formed in the recess 148, which makes physical and electrical contact with RDL 136 and allows the structure to be connected to the outside. A portion of UBM 160 extends along the recessed surface 147 of the protective layer 146. By forming the recessed surface 147 under UBM 160 as described in this invention, the interfacial stress between UBM 160 and the protective layer 146 can be reduced, which can reduce the risk of delamination or cracking and can improve resistance, device performance, or yield. The process described below with reference to Figures 12 to 15 is an example, and other materials or techniques may be used to form the UBM in the recess 148 in other embodiments.
[0047] exist Figure 12 In some embodiments, a seed layer 152 is formed on a protective layer 146, on an RDL 136, on a second passivation layer 140, on a third passivation layer 142, within a groove 148, and within an opening 144. In some embodiments, the seed layer 152 may include a titanium layer and a copper layer on the titanium layer. In other embodiments, the seed layer 152 includes a copper layer in contact with the RDL 136, the second passivation layer 140, the third passivation layer 142, and the protective layer 146. The seed layer 152 can be formed by deposition processes such as PVD, CVD, MOCVD, etc. The seed layer 152 can be deposited compliantly.
[0048] exist Figure 13In some embodiments, a patterned photoresist 154 is formed on a seed layer 152. The patterned photoresist 154 can be formed by depositing a photosensitive layer (e.g., photoresist, etc.) on the seed layer 152 using spin coating or the like. The photosensitive layer can then be patterned by exposing it to a patterned energy source (e.g., a patterned light source) and developing it to remove exposed or unexposed portions, thereby forming an opening 155 in the patterned photoresist 154. The opening 155 exposes a portion of the seed layer 152 within a recess 148. The opening 155 is aligned with and at least partially overlaps with the recess 148. In some embodiments, the opening 155 and the recess 148 may have similar widths, and the edge of the recess 148 may be substantially aligned with the sidewall of the opening 155. In other embodiments, the opening 155 may have a width greater than or smaller than the width of the recess 148. The opening 155 in the patterned photoresist 154 corresponds to the subsequently formed UBM 160 (described below).
[0049] exist Figure 14 In some embodiments, conductive material 156 is deposited in opening 155. Conductive material 156 can be deposited using an electroplating process, such as electroplating, electroless plating, etc. Conductive material 156 may include metals, such as copper, nickel, silver, combinations thereof, etc. In some embodiments, the metal of conductive material 156 may be similar to the metal previously described with respect to conductive material 134. Other conductive materials may also be used. The combination of conductive material 156 and the lower portion of seed layer 152 forms UBM 160 (see reference). Figure 15 ).
[0050] exist Figure 15In some embodiments, the portion of the patterned photoresist 154 and the seed layer 152 on which the conductive material 156 is not formed is removed. The patterned photoresist 154 can be removed by an acceptable ashing or stripping process, such as using oxygen plasma. Once the patterned photoresist 154 is removed, the exposed portion of the seed layer 152 is removed using an acceptable etching process (e.g., wet or dry etching). The remaining portion below the conductive material 156 and the seed layer 152 forms a UBM 160. The UBM 160 may include bump portions extending on the recessed surface 147 of the protective layer 146. The UBM 160 may also include via portions in and extending through the first opening 144 of the second passivation layer 140, the third passivation layer 142, and / or the protective layer 146, the via portions being physically and electrically coupled to the RDL 136. Thus, the UBM 160 is electrically coupled to a device (e.g., integrated circuit device 104). In some embodiments, the first bottom surface of the bump portion of UBM 160 that is closer to the via portion of UBM 160 may be closer to the semiconductor substrate 102 than the second bottom surface of the bump portion of UBM 160 that is farther away from the via portion of UBM 160.
[0051] In some embodiments, UBM 160 completely covers the recessed surface 147 of the protective layer 146. For example, the sidewalls of UBM 160 may be aligned with the edge of the recessed surface 147 (e.g., perpendicularly positioned on the edge of the recessed surface 147). In other embodiments, the sidewalls of UBM 160 may be laterally offset from the edge of the recessed surface 147. For example, the sidewalls of UBM 160 may protrude beyond the edge of the recessed surface 147, such as protruding beyond the horizontal surface of the protective layer 146. In other embodiments, UBM 160 may not completely cover the recessed surface 147, such that a portion of the recessed surface 147 may be exposed.
[0052] exist Figure 16In some embodiments, a conductive connector 162 is formed on a UBM 160. The conductive connector 162 may be a ball grid array (BGA) connector, solder balls, metal pillars, controlled collapse chip connection (C4) bumps, microbumps, bumps formed using an electroless nickel-electroless palladium-immersion gold technique (ENEPIG), etc. The conductive connector 162 may include conductive materials such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, etc., or combinations thereof. In some embodiments, the conductive connector 162 is initially formed by forming a solder layer through vapor deposition, electroplating, printing, solder transfer, ball placement, etc. Once the solder layer is structurally formed, reflow soldering can be performed to shape the material into the desired bump shape. In other embodiments, the conductive material of the conductive connector 162 is deposited on the UBM 160 before the patterned photoresist 154 is removed.
[0053] According to some embodiments, Figures 17A to 17F show example recessed surfaces 147A-F of the protective layer 146 with different surface profiles. Figures 17A to 17F show... Figure 16 The diagram shows an enlarged cross-sectional view of a structure similar to region 170. For clarity, the seed layer 152 of UBM 160 is not shown in Figures 17A to 17F. The recessed surfaces 147A-F described for Figures 17A-17F are intended as non-limiting examples, and other profiles, dimensions, shapes, constructions, or configurations are possible. The recessed surfaces 147A-F can be formed using techniques similar to those described in Figures 10 and 11 for forming the recessed surfaces 147. For example, grayscale lithography and / or multiple exposures can be used to form the recessed surfaces 147A-F in the protective layer 146. Forming the protective layer 146 with the recessed surfaces 147 under UBM 160 can reduce interfacial stress and can reduce the chance of delamination or other defects. The specific surface profile of the recessed surfaces 147 under UBM 160 can depend on the specific arrangement or configuration of the structure.
[0054] According to some embodiments, Figure 17A Showing a recessed surface 147A with a sloping surface profile. Figure 17AThe recessed surface 147A may be similar to the recessed surface 147 in Figures 11 to 16. For example, the protective layer 146 may have an inclined recessed surface 147A below the UBM 160, such that the thickness of the protective layer 146 gradually decreases toward the via portion of the UBM 160. For example, the protective layer 146 may gradually decrease from thickness T1 to a smaller thickness T2 at or near the sidewall 147' of the protective layer 146. In some embodiments, the thickness T2 is between about 10% and about 90% of the thickness T1. In some embodiments, the thickness T2 may be about 1 μm to about 2 μm. Other thicknesses are also possible. The recessed surface 147A may be generally flat or contoured. The recessed surface 147A may have an angle A1 of about 1 degree to about 45 degrees relative to the top surface of the protective layer 146, but other angles are also possible. The sidewall 147' of the protective layer 146 can be laterally offset from the edge (e.g., sidewall) of the second passivation structure by a distance D1 of approximately 0 μm to approximately 20 μm, but other distances are also possible. In some embodiments where the distance D1 is non-zero, the recessed surface 147A can form a single "step" from the protective layer 146 to the third passivation layer 142. The sidewall 147' can be substantially vertical, such as... Figure 17A As shown, it can be tilted or curved.
[0055] According to some embodiments, Figure 17B The recessed surface 147B displays a stepped surface profile. The recessed surface 147B includes a first “step” with a sidewall height H1 and a length L1 above the second passivation structure, and a second “step” with a sidewall height H2 and a length L2 above the second passivation structure. In some embodiments, the total height H1+H2 may be approximately the same as the thickness T1 of the protective layer 146. Heights H1 and H2 may be similar or different. In some embodiments, the total length L1+L2 may be approximately the same as the length of the recessed surface 147B below the UBM 160. Lengths L1 and L2 may be similar or different. In some cases, the top surface of the protective layer 146 covered by the UBM 160 may be considered part of the recessed surface 147B, even if it may be approximately flush with the top surface of the protective layer 146 not covered by the UBM 160. In other cases, only the surface of the portion of the protective layer 146 thinner than the thickness T1 is considered part of the recessed surface 147B. The surfaces of the recessed surface 147B can be approximately horizontal or approximately vertical, such as... Figure 17B As shown, or it can be tilted (e.g., tilted relative to the horizontal or vertical).
[0056] In any stepped embodiment, the recessed surface 147 can have any suitable number of steps. For example, according to some embodiments, Figure 17CA recessed surface 147C is shown as a stepped surface with three steps. The lengths of the top surfaces of the steps of the recessed surface 147C may be similar or different, and the heights of the sidewalls of the steps of the recessed surface 147C may be similar or different. In other embodiments, the recessed surface 147 may have more than three steps.
[0057] According to some embodiments, Figure 17D A recessed surface 147D is shown, having a surface profile comprising a combination of inclined surfaces and steps. Recessed surface 147D is similar to recessed surface 147B, except that the steps of recessed surface 147D have inclined sidewalls instead of vertical sidewalls. For example, the first (e.g., the lowest) step of recessed surface 147D has a sidewall inclined at angle A1, and the second step of recessed surface 147D has a sidewall inclined at angle A2. Angles A1 and A2 can each be from about 1° to about 90°. The top surface of the steps can be generally horizontal or can be inclined, and can have similar or different lengths. The heights of the steps can be similar or different. In other embodiments, other numbers of steps may be present.
[0058] According to some embodiments, Figure 17E A recessed surface 147E is shown, having a surface profile comprising a combination of inclined surfaces and steps. Recessed surface 147E is similar to recessed surface 147D, except that the top surface of the first (e.g., lowest) step of recessed surface 147E is inclined. For example, the first step of recessed surface 147E has sidewalls inclined at angle A1, the second step of recessed surface 147E has sidewalls inclined at angle A2, and the top surface of the first step has an angle A3 relative to the sidewall of the second step. In other words, the angle between the sidewall of the second step and the top surface of the second step is A2, the angle between the top surface of the first step and the sidewall of the second step is A3, and the angle between the sidewall of the first step and the top surface of the first step is A1. Angles A1, A2, and A3 can all be in the range of about 1° to about 90°. In some embodiments, the sum of all relative angles of recessed surface 147E (e.g., A1+A2+A3) can be greater than 90°. In other words, along the first edge of recessed surface 147E (e.g., ... Figure 17E From point P1) to the second edge of the concave surface 147E (e.g., Figure 17E The total rotation of the continuous path from point P2 can be greater than 90°. In other embodiments, more than one step may have a sloping top surface. In such embodiments, the sum of the relative angles between the sidewalls and the top surface of the step can be greater than 90°. In some cases, making the sum of all relative angles of the steps on the recessed surface 147 greater than about 90° can reduce interfacial stress and reduce the risk of defects. In other embodiments, other numbers of steps or sloping surfaces may be present.
[0059] According to some embodiments, Figure 17F The recessed surface 147F is shown to have a curved surface profile. Although the recessed surfaces 147A-E are shown to have a generally straight (e.g., flat) surface, in other embodiments, some or all of the recessed surfaces 147 may be curved. Figure 17F The example curved recessed surface 147F is shown as an illustrative example, but any suitable curved surface profile can be formed in other embodiments. In some embodiments, the recessed surface 147 may have a generally stepped shape with one or more curved portions. In some embodiments, the recessed surface 147 may include generally straight surfaces separated by curved surfaces. For example, in some embodiments, the top surface of the steps of the recessed surface 147 may be straight (e.g., horizontal or inclined), and the sidewalls between the steps may be curved. Other surface profiles are also possible.
[0060] Various advantages can be achieved through several embodiments of this invention. Forming a protective layer (e.g., a polymer layer, etc.) such that the portion covered by the under-bump metallization (UBM) is sloped and / or stepped can reduce interfacial stress. For example, interfacial stress between the protective layer and the underlying passivation layer, or between the protective layer and the upper UBM, can be reduced. In some cases, interfacial stress can be reduced by about 15% or more. Reducing stress in this way can reduce the risk of defects such as delamination, cracking, or warping. Therefore, the yield, reliability, and performance of the package can be improved. The recessed portions of the protective layer can be formed with a specific surface profile suitable for a particular application or structure. The surface profile of the protective layer can be controlled using the techniques described in this invention, such as grayscale lithography or multiple exposure lithography.
[0061] According to some embodiments, the present invention provides a method for forming a semiconductor package, comprising: forming a passivation structure on a first conductive component; forming an opening in the passivation structure to expose the first conductive component; forming a protective layer on the passivation structure and in the opening, wherein the protective layer on the passivation structure has a first thickness; etching a portion of the protective layer to form a groove, wherein the groove exposes the first conductive component, wherein a second thickness of the protective layer on the sidewall of the groove is less than the first thickness; and forming a second conductive component on the protective layer and in the groove.
[0062] In some embodiments, the top surface of the etched portion of the protective layer is inclined.
[0063] In some embodiments, the sloping top surface extends from the edge of the second conductive component on the protective layer to the sidewall of the groove.
[0064] In some embodiments, the groove exposes the top surface of the passivated structure.
[0065] In some embodiments, the passivation structure includes a silicon nitride layer on a silicon oxide layer.
[0066] In some embodiments, the width of the groove is greater than the width of the first conductive structure.
[0067] In some embodiments, a portion of the etched protective layer includes performing a grayscale lithography process.
[0068] In some embodiments, the protective layer comprises polyimide.
[0069] In some embodiments, the top surface of the etched portion of the protective layer has a stepped profile.
[0070] According to other embodiments, the present invention provides a method for forming a semiconductor package, comprising: forming a first passivation layer on a redistribution line; patterning the first passivation layer to form a first opening, the first opening exposing a first surface of the redistribution line; depositing a polymer layer on the first passivation layer and the first surface of the redistribution line; patterning the polymer layer to form a second opening, the second opening exposing the first surface of the redistribution line, wherein the patterning reshapes the top surface of the polymer layer adjacent to the second opening; and forming a bump under-metallization layer that covers the first surface of the redistribution line and the reshaped top surface of the polymer layer.
[0071] In other embodiments, the reshaped top surface of the polymer layer surrounds the second opening.
[0072] In other embodiments, the reshaped top surface of the polymer layer includes multiple stepped surfaces.
[0073] In other embodiments, at least one of the stepped surfaces is inclined.
[0074] In other embodiments, at least two of the stepped surfaces have different lengths.
[0075] In other embodiments, the sidewall of the polymer layer at the second opening has a first height, wherein the polymer layer adjacent to the metallization layer under the bump has a first thickness, wherein the first height is less than the first thickness.
[0076] According to some other embodiments, the present invention provides a semiconductor package comprising: a dielectric layer on a conductive component; a polymer layer on the dielectric layer, wherein the polymer layer includes a stepped upper surface; and a bump under-metallization layer on the stepped upper surface of the polymer, wherein the bump under-metallization layer extends through the polymer layer and the dielectric layer to contact the conductive component.
[0077] In some other embodiments, the stepped upper surface includes a plurality of horizontal surfaces separated by inclined surfaces.
[0078] In some other embodiments, the stepped upper surface includes a plurality of horizontal surfaces separated by curved surfaces.
[0079] In yet another embodiment, the stepped upper surface laterally surrounds the conductive component.
[0080] In some other embodiments, the stepped upper surface includes an inclined top surface.
[0081] The foregoing outlines the features of several embodiments to enable those skilled in the art to better understand the viewpoints of the present invention. Those skilled in the art should understand that other processes and structures can be easily designed or modified based on the embodiments of the present invention to achieve the same purpose and / or advantages as the embodiments described herein. Those skilled in the art should also understand that such equivalent structures do not depart from the concept and scope of the present invention, and various changes, substitutions, and replacements can be made without departing from the concept and scope of the present invention. Therefore, the scope of protection of the present invention shall be determined by the claims.
Claims
1. A semiconductor package, characterized in that, include: A dielectric layer on a conductive component; A polymer layer on the dielectric layer, wherein the polymer layer includes a stepped upper surface; as well as A bump under-metallization layer is provided on the stepped upper surface of the polymer, wherein the bump under-metallization layer extends through the polymer layer and the dielectric layer to contact the conductive component.
2. The semiconductor package as claimed in claim 1, characterized in that, The stepped upper surface comprises multiple horizontal surfaces, which are separated by multiple inclined surfaces.
3. The semiconductor package as described in claim 2, characterized in that, The lengths of these multiple horizontal surfaces are the same.
4. The semiconductor package as claimed in claim 2, characterized in that, The lengths of these multiple horizontal surfaces are different from each other.
5. The semiconductor package as claimed in claim 1, characterized in that, The stepped upper surface comprises multiple horizontal surfaces, which are separated by multiple curved surfaces.
6. The semiconductor package as claimed in claim 5, characterized in that, The lengths of these multiple horizontal surfaces are the same.
7. The semiconductor package as claimed in claim 5, characterized in that, The lengths of these multiple horizontal surfaces are different from each other.
8. The semiconductor package as claimed in any one of claims 1 to 7, characterized in that, The stepped upper surface surrounds the conductive component laterally.
9. The semiconductor package as claimed in any one of claims 1 to 7, characterized in that, The stepped upper surface includes a sloping top surface.
10. The semiconductor package according to any one of claims 1 to 7, characterized in that, The metallization layer under the bump completely covers the stepped upper surface.