Atomizing core, atomizer and aerosol generating device
By adding a stronger reinforcing part to the liquid-conducting substrate, the electrical connection part of the heating element is connected to it, which solves the problem of insufficient bonding force between the liquid-conducting substrate and the heating element, and achieves more reliable atomizing core connection and higher compressive strength.
Patent Information
- Application Number
- CN202522151835.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-11
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-10-11
AI Technical Summary
In existing atomizing cores, the bonding force between the liquid-conducting substrate and the heating element is poor, making them prone to separation during assembly and affecting the atomization effect.
A reinforcing section is added to the liquid-conducting substrate, connecting the electrical contact part of the heating element to the reinforcing section. The strength of the reinforcing section is higher than that of the liquid-conducting substrate, thus improving the bonding force.
Without affecting the liquid guiding performance, the bonding force between the liquid guiding matrix and the heating element is significantly improved, ensuring reliable connection and enhancing the compressive strength and atomization efficiency of the atomizing core.
Smart Images

Figure CN225004646U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of atomizer technology, and in particular to an atomizing core, atomizer, and aerosol generating device. Background Technology
[0002] In related technologies, there is an atomizing core for an aerosol generating device that includes a liquid guiding substrate and a heating element. The liquid guiding substrate directs the atomizing liquid to the heating element, which heats the atomizing liquid to atomize it into an aerosol.
[0003] To ensure the transmission of the atomizing liquid, the liquid-conducting substrate generally has a high porosity. However, the bonding force between this liquid-conducting substrate and the heating element is poor. During the assembly process, the liquid-conducting substrate and the heating element are prone to separation under the action of assembly force, which affects the subsequent atomization. Utility Model Content
[0004] In view of this, the embodiments of this application aim to provide an atomizing core, atomizer, and aerosol generating device that can improve the bonding force between the liquid-conducting substrate and the heating element without affecting the liquid-conducting properties.
[0005] To achieve the above objectives, embodiments of this application provide an atomizing core, comprising: A liquid-conducting substrate, the liquid-conducting substrate including a liquid-conducting main body and a reinforcing part disposed on a first side of the liquid-conducting main body along a first direction, the liquid-conducting main body having an atomizing region disposed on the first side, and the reinforcing part avoiding the atomizing region; A heating element having an electrical contact portion and a heating portion electrically connected to the electrical contact portion, the heating element being disposed on the first side, the electrical contact portion being at least connected to the reinforcing portion, and at least a portion of the heating portion being disposed in the atomizing region.
[0006] In one embodiment, the atomizing region is located on one side of the reinforcing portion along a second direction, the second direction intersecting the first direction, and the distance between the heating portion and the reinforcing portion along the second direction is greater than 0.
[0007] In one embodiment, the distance between the heating element and the reinforcing element along the second direction is greater than or equal to 0.3 mm; and / or, a portion of the electrical contact element protrudes from the reinforcing element along the second direction on the side near the atomizing region.
[0008] In one embodiment, the reinforcement includes a connection region and an extended region located around the connection region, and the power receiving part is connected to the connection region.
[0009] In one embodiment, the atomizing region is located on one side of the reinforcing portion along a second direction, which intersects with the first direction; the extended region includes a first sub-region located on one side of the connecting region away from the atomizing region along the second direction; and / or, the extended region includes a second sub-region located on at least one of two opposite sides of the connecting region along a third direction, which intersects with the first direction and the second direction respectively.
[0010] In one embodiment, the extended region includes a second sub-region, a portion of which protrudes from the connecting region along the second direction on the side adjacent to the atomizing region.
[0011] In one embodiment, the liquid guiding body is a porous structure, and the reinforcing part is connected to the structure.
[0012] In one embodiment, a portion of the pores in the porous structure is filled with a reinforcing material such that the portion of the structure not filled with the reinforcing material forms the liquid-conducting body, and the portion of the structure filled with the reinforcing material forms at least a portion of the reinforcing part.
[0013] In one embodiment, the thickness of the portion of the structure filled with the reinforcing material along the first direction is 50 μm to 200 μm.
[0014] In one embodiment, the first side of the liquid-conducting body has a first end face, the reinforcing portion protrudes at least partially from the first end face, and the thickness of the reinforcing portion protruding from the first end face along the first direction is less than or equal to 50 μm; and / or, the reinforcing portion comprises at least an inorganic material with a softening point of 600°C to 1000°C.
[0015] Another embodiment of this application provides an atomizer, including: a housing and the atomizing core described above, the housing having a liquid storage chamber and an air outlet channel, the liquid storage chamber and the air outlet channel being in fluid communication through the atomizing core.
[0016] Another embodiment of this application provides an aerosol generating device, including a power supply component and the atomizer described above, wherein the power supply component is electrically connected to the electrical connection portion of the heating element.
[0017] This application provides an atomizing core, an atomizer, and an aerosol generating device. The atomizing core has a liquid-conducting substrate and a heating element. The liquid-conducting substrate has not only a liquid-conducting main body but also a reinforcing part. The electrical connection part of the heating element is mainly connected to the reinforcing part. Since the strength of the reinforcing part is higher than that of the liquid-conducting substrate, the bonding force between the reinforcing part and the electrical connection part is greater. Therefore, without affecting the liquid conduction, the bonding force between the liquid-conducting substrate and the heating element is significantly improved, thereby enabling the liquid-conducting substrate and the heating element to be reliably connected together. Attached Figure Description
[0018] Figure 1 This is a schematic diagram of the atomizing core according to the first embodiment of this application; Figure 2 This is a schematic diagram of the atomizing core according to the second embodiment of this application; Figure 3 This is a schematic diagram of the atomizing core according to the third embodiment of this application; Figure 4 This is a schematic diagram of the atomizing core with a concealed heating element according to the third embodiment of this application; Figure 5 This is a schematic diagram of the atomizing core according to the fourth embodiment of this application; Figure 6 This is a schematic diagram of the atomizing core according to the fifth embodiment of this application; Figure 7 This is a schematic diagram of the atomizing core according to the sixth embodiment of this application; Figure 8 This is a flowchart illustrating a method for preparing the first atomizing core according to an embodiment of this application; Figure 9 This is a flowchart illustrating a second method for preparing an atomizing core according to an embodiment of this application; Figure 10 This is a strength test diagram of an atomizing core according to an embodiment of this application; Figure 11 Electron microscopy of the atomizing core of the fourth embodiment of this application Figure 1 ; Figure 12 Electron microscopy of the atomizing core of the fourth embodiment of this application Figure 2 ; Figure 13 for Figure 12 Electron micrograph of a cross section along the AA direction.
[0019] Explanation of reference numerals in the attached figures 10. Atomizing core; 11. Liquid guiding substrate; 111. Liquid guiding main body; 111a. Atomizing area; 111b. First end face; 112. Reinforcing part; 112a. Connecting area; 112b. Extended area; 112b1. First sub-area; 112b2. Second sub-area; 12. Heating element; 121. Electrical connection part; 122. Heating part. Detailed Implementation
[0020] In the description of the embodiments in this application, it should be noted that the terms "first direction," "second direction," "third direction," etc., indicate the orientation or positional relationship based on the appendix. Figure 1 To be continued Figure 7 The orientations or positional relationships shown are for the convenience of describing the embodiments of this application and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation on the embodiments of this application.
[0021] This application provides an aerosol generating device, which includes an atomizer and a power supply component.
[0022] Please see Figures 1 to 7 The atomizer includes a housing and an atomizing core 10. The atomizing core 10 includes a liquid-conducting substrate 11 and a heating element 12. The housing has a liquid storage chamber and an air outlet channel, which are fluidly connected through the atomizing core 10.
[0023] The liquid storage chamber is used to store the atomizing liquid and has a liquid outlet. The atomizing core 10 is located at the liquid outlet, and the atomizing liquid flows to the heating element 12 through the liquid guiding substrate 11.
[0024] Please see Figures 1 to 7 The heating element 12 has a grounding portion 121 and a heating element 122 electrically connected to the grounding portion 121. The power supply assembly is electrically connected to the grounding portion 121 of the heating element 12. Specifically, the power supply assembly includes a power source and an electrical connector. The power source is electrically connected to the grounding portion 121 through the electrical connector to supply power to the heating element 12. The electrical connector can be any conductive component; for example, the electrical connector can be a wire, a pin, etc.
[0025] When the heating element 12 is powered on, the heating part 122 can generate heat on its own, thereby heating the atomizing liquid. After the atomizing liquid is heated, it atomizes to form an aerosol, which flows into the user's mouth through the air outlet channel.
[0026] Please see Figures 1 to 7 , Figures 11 to 13The liquid-conducting substrate 11 of the atomizing core 10 in this embodiment includes a liquid-conducting main body 111 and a reinforcing part 112 disposed on a first side of the liquid-conducting main body 111 along a first direction. The liquid-conducting main body 111 has an atomizing region 111a disposed on the first side, and the reinforcing part 112 avoids the atomizing region 111a. A heating element 12 is disposed on the first side, and the electrical connection part 121 of the heating element 12 is at least connected to the reinforcing part 112. At least a portion of the heating part 122 of the heating element 12 is disposed in the atomizing region 111a.
[0027] Specifically, the liquid guiding body 111 has pores, and the atomizing liquid flows through the pores of the liquid guiding body 111 located in the atomization region 111a to the heating part 122 of the heating element 12.
[0028] This application does not impose any special limitations on the specific structure of the liquid-conducting substrate 11. Exemplarily, the liquid-conducting substrate 11 can be a cylindrical structure (cylindrical or prismatic structure), a spherical structure, a tubular structure, etc. A tubular structure refers to a cylindrical structure with a channel extending through it. In one embodiment, the liquid-conducting substrate 11 is a cylindrical structure, the first direction can be the radial direction of the cylindrical structure, and the first side can be the inner side of the cylindrical structure.
[0029] The material of the fluid-conducting body 111 includes, but is not limited to, one or more combinations of glass, ceramic, plastic, and metal.
[0030] The average pore size of the pores in the liquid-conducting main body 111 can be adjusted according to design requirements. For example, the average pore size of the pores in the liquid-conducting main body 111 can be 10μm to 40μm (including the endpoint values). For instance, the average pore size of the pores in the liquid-conducting main body 111 can be 10μm, 14μm, 19μm, 25μm, 33μm, 40μm, etc. Preferably, the average pore size of the liquid-conducting main body 111 can be 15μm to 20μm (including the endpoint values).
[0031] The porosity of the liquid-conducting main body 111 can be adjusted according to design requirements. However, in order to reduce energy loss and atomization burst force during the atomization process, it is necessary to improve the liquid-conducting efficiency of the liquid-conducting main body 111. Therefore, it is preferable to use a liquid-conducting main body 111 with high porosity, typically 50% to 75% (including endpoint values). For example, the porosity of the liquid-conducting main body 111 can be 50%, 58%, 66%, 70%, 75%, etc. Preferably, the porosity of the liquid-conducting main body 111 can be 65% to 72% (including endpoint values).
[0032] The reinforcing part 112 is the part of the liquid-conducting substrate 11 that has been reinforced relative to the liquid-conducting main body 111. In other words, the strength of the reinforcing part 112 is higher than that of the liquid-conducting substrate 11.
[0033] The main function of the reinforcing part 112 is to connect to the power receiving part 121.
[0034] In some embodiments, the reinforcing portion 112 may have pores. The average pore diameter of the pores in the reinforcing portion 112 can be adjusted according to design requirements. However, in order to ensure that the strength of the reinforcing portion 112 is greater than the strength of the liquid-conducting main body portion 111, the average pore diameter of the pores in the reinforcing portion 112 should be smaller than the average pore diameter of the pores in the liquid-conducting main body portion 111. For example, the average pore diameter of the pores in the reinforcing portion 112 can be 5μm to 20μm (including endpoint values). For instance, the average pore diameter of the pores in the reinforcing portion 112 can be 5μm, 9μm, 14μm, 18μm, 20μm, etc.
[0035] The porosity of the reinforcing part 112 can be adjusted according to design requirements. However, excessive porosity of the reinforcing part 112 will reduce its strength and bonding ability. Therefore, the porosity of the reinforcing part 112 should be less than the porosity of the liquid-conducting main body 111. Preferably, the porosity of the reinforcing part 112 can be less than or equal to 50%. For example, the porosity of the reinforcing part 112 can be 4%, 11%, 23%, 35%, 41%, 50%, etc.
[0036] In other embodiments, the reinforcement 112 may not have pores, that is, the porosity of the reinforcement 112 is 0%.
[0037] For example, please refer to Figures 1 to 3 The power receiving part 121 and the heating part 122 can be arranged along the second direction. The reinforcing part 112 corresponds to the position of the power receiving part 121, and the atomizing region 111a corresponds to the position of the heating part 122. That is, the atomizing region 111a is located on one side of the reinforcing part 112 along the second direction. The second direction intersects with the first direction. For example, the first direction can be perpendicular to the second direction.
[0038] Please see Figures 1 to 3 , Figures 5 to 7 The number of electrical connection parts 121 can be two, and the heating part 122 is disposed between the two electrical connection parts 121 and electrically connected to the two electrical connection parts 121 respectively. Correspondingly, the number of reinforcing parts 112 is two, and the two reinforcing parts 112 are spaced apart from each other along the second direction, and the atomizing region 111a is located between the two reinforcing parts 112.
[0039] The heating element 122 and the reinforcing element 112 can be staggered so that the entire heating element 122 is located in the atomization area 111a, thereby allowing the atomizing liquid transported in the atomization area 111a to fully contact the heating element 122 and improve atomization efficiency.
[0040] Further, please refer to Figure 1 and Figure 2The distance between the heating part 122 and the reinforcing part 112 along the second direction can be greater than 0.
[0041] Due to manufacturing precision issues, if the design spacing between the heating element 122 and the reinforcing element 112 along the second direction is equal to 0, the reinforcing element 112 may partially block the atomization area 111a due to positional deviation. In other words, a portion of the heating element 122 may overlap with the reinforcing element 112, which would reduce the liquid guiding efficiency of the liquid guiding body 111. Therefore, a spacing between the heating element 122 and the reinforcing element 112 along the second direction greater than 0 can better prevent the reinforcing element 112 from blocking the atomization area 111a and reducing the liquid guiding efficiency of the liquid guiding body 111.
[0042] The spacing between the heating element 122 and the reinforcing element 112 along the second direction can be adjusted according to design requirements. Preferably, the distance between the heating element 122 and the reinforcing element 112 along the second direction can be greater than or equal to 0.3 mm. For example, the distance between the heating element 122 and the reinforcing element 112 along the second direction can be 0.3 mm, 0.6 mm, 1 mm, 1.2 mm, etc.
[0043] Further, please refer to Figure 2 and Figure 3 A portion of the electrical connection portion 121 may protrude from the side of the reinforcement portion 112 along the second direction close to the atomization region 111a, thereby ensuring that the distance between the heating portion 122 and the reinforcement portion 112 along the second direction is greater than 0.
[0044] The relationship between the strength of the liquid-conducting main body 111 and its porosity can be approximately expressed as:
[0045] in, For the strength of the liquid-conducting body 111, The strength is corresponding to the density of the material. The porosity of the liquid-conducting body 111 is given by K, which is a constant related to the material type and preparation process conditions.
[0046] The liquid guiding efficiency (i.e., the ability of the atomizing liquid to pass through the liquid guiding body 111) of the liquid guiding body 111 is related to its permeability. Generally speaking, the permeability K of the liquid guiding body 111 is related to... Proportional, i.e., K It can be seen that the liquid conduction efficiency of the liquid-conducting main body 111 depends on the porosity. However, after the porosity increases to a certain stage, the strength of the liquid-conducting main body 111 will be significantly reduced. In other words, the higher the porosity of the liquid-conducting main body 111, the lower its own strength.
[0047] In related technologies, the contact part of the heating element is directly connected to the liquid-conducting substrate. However, since the liquid-conducting substrate generally has a high porosity and low strength, the bonding force between the liquid-conducting substrate and the contact part is poor. During the assembly process, the liquid-conducting substrate and the heating element are prone to separation under the action of assembly force, which affects the subsequent atomization.
[0048] In this embodiment, the liquid-conducting substrate 11 of the atomizing core 10 not only has a liquid-conducting main body 111, but also a reinforcing part 112. The electrical connection part 121 of the heating element 12 is mainly connected to the reinforcing part. Since the strength of the reinforcing part 112 is higher than that of the liquid-conducting substrate 11, the bonding force between the reinforcing part 112 and the electrical connection part 121 is larger. Thus, without affecting the liquid conduction, the bonding force between the liquid-conducting substrate and the heating element is significantly improved, thereby enabling the liquid-conducting substrate 11 and the heating element 12 to be reliably connected together.
[0049] Furthermore, the atomizing core 10 with the reinforcement portion 112 of this application embodiment and the atomizing core without the reinforcement portion 112 of the comparative example were subjected to compressive strength tests. The number of atomizing cores 10 in this application embodiment and 20 in the comparative example were used. The electrical connector used in the test was a cylindrical pin with a diameter of 1 mm. The pin abutted against the electrical contact portion 121 of the heating element 12 of the atomizing core 10 in this application embodiment and the electrical contact portion of the heating element of the comparative example atomizing core. The results obtained are as follows: Figure 10 As shown, Figure 10 The images show the minimum (MIN), maximum (MAN), and average (AVE) values of the failure pin strength of the atomizer core 10 of this application and the atomizer core of the comparative example, respectively. Figure 10 It can be seen that the failure pin strength of the atomizer core 10 of this application is significantly higher than that of the comparative atomizer core, whether it is the minimum value (MIN), the maximum value (MAN), or the average value (AVE). It is evident that the liquid guiding substrate 11 of the atomizer core 10 of this application embodiment can significantly improve the compressive strength of the liquid guiding substrate 11 by providing the reinforcing part 112.
[0050] In addition, generally speaking, the pressure applied by the ejector pin to the liquid-conducting substrate can reach up to 50N, while from... Figure 10 It can be seen that the minimum strength of the failed ejector pin of the atomizing core 10 in this embodiment of the application exceeds 55N. Therefore, the liquid-conducting substrate 11 of the atomizing core 10 in this embodiment of the application can withstand the pressure of the ejector pin well and is not prone to failure due to excessive pressure of the ejector pin.
[0051] In some embodiments, please refer to Figure 4The reinforcing part 112 may include a connecting region 112a and an extended region 112b located around the connecting region 112a. The electrical contact part 121 is connected to the connecting region 112a. That is, the extended region 112b is a region where the shape of the reinforcing part 112 is further enlarged, and the electrical contact part 121 is not connected to the extended region 112b. After the shape of the reinforcing part 112 is enlarged, the structure of the reinforcing part 112 is more stable, which is equivalent to providing a more stable foundation for the electrical contact part 121. Therefore, the reliability of the connection between the liquid-conducting substrate 11 and the heating element 12 can be better improved.
[0052] The extended region 112b may be disposed around at least a portion of the periphery of the connecting region 112a, for example, see [reference needed]. Figures 1 to 4 The extended region 112b may include a first sub-region 112b1, which is located on the side of the connecting region 112a away from the atomizing region 111a along the second direction. That is, the reinforcing part 112 may only extend towards the side away from the atomizing region 111a along the second direction.
[0053] Please continue reading. Figures 1 to 4 The extended region 112b may also include a second sub-region 112b2, which is located on at least one of the opposite sides of the connecting region 112a along a third direction. This third direction intersects the first and second directions, respectively; for example, the third direction may be perpendicular to both the first and second directions. In other words, the reinforcement 112 may also extend outward from at least one of the opposite sides along the third direction. To further increase the area of the extended region 112b, please refer to some embodiments. Figure 3 and Figure 4 A portion of the second sub-region 112b2 may also protrude from the connecting region 112a along the second direction on the side close to the atomizing region 111a.
[0054] Figures 1 to 4 The extended region 112b of the reinforcement 112 shown has both a first sub-region 112b1 and a second sub-region 112b2. In other embodiments, the extended region 112b may have only the first sub-region 112b1 and no second sub-region 112b2, or it may have only the second sub-region 112b2 and no first sub-region 112b1.
[0055] Please continue reading. Figures 5 to 7The first side of the liquid guiding body 111 has a first end face 111b. In some embodiments, the reinforcing part 112 may at least partially protrude from the first end face 111b. That is, at least a portion of the reinforcing part 112 is higher than the first end face 111b. Thus, the reinforcing part 112 can block the atomized liquid flowing from the atomization region 111a to the first end face 111b, thereby minimizing the flow of the atomized liquid to the relatively low-temperature contact part 121, and thus better preventing the atomized liquid from being ineffectively atomized in the contact part 121.
[0056] The thickness of the reinforcing portion 112 protruding from the first end face 111b along the first direction can be adjusted according to design requirements. However, if the thickness of the reinforcing portion 112 protruding from the first end face 111b along the first direction is too thick, it will be detrimental to the contact between the heating element 12 and the liquid guiding body portion 111, affecting the liquid guiding efficiency. Therefore, preferably, the thickness of the reinforcing portion 112 protruding from the first end face 111b along the first direction can be less than or equal to 50 μm (including the endpoint value). For example, the thickness of the reinforcing portion 112 protruding from the first end face 111b along the first direction can be 5 μm, 10 μm, 22 μm, 30 μm, 44 μm, 50 μm, etc.
[0057] In other embodiments, the reinforcement 112 may not protrude from the first end face 111b, for example, see [link to relevant documentation]. Figure 5 The reinforcing part 112 can also be flush with the first end face 111b. The fact that the reinforcing part 112 is flush with the first end face 111b allows the outer surface of the reinforcing part 112 and the first end face 111b to form a flat surface together, which is also beneficial for the installation of the heating element 12.
[0058] In some embodiments, please refer to Figure 5 and Figure 7 , Figures 11 to 13 The liquid-conducting matrix 11 can be formed by filling some of the pores of a porous structure with a reinforcing material, so that the part of the structure not filled with the reinforcing material forms the liquid-conducting main body 111, and the part of the structure filled with the reinforcing material forms at least a part of the reinforcing part 112.
[0059] The reinforcing material is the main material used in manufacturing the reinforcing section 112. Please refer to... Figure 5 , Figures 11 to 13 If the reinforcing material is completely absorbed into the pores of the structure, then the part of the structure filled with the reinforcing material forms the reinforcing part 112.
[0060] In other embodiments, only a portion of the reinforcing material may penetrate into the pores of the structure, while the other portion may be located on the surface of the structure. In this case, the portion of the structure filled with the reinforcing material and the reinforcing material located on the surface of the structure together form the reinforcing portion 112.
[0061] For example, the reinforcing material may include at least an inorganic material. For instance, the reinforcing part 112 may include at least an inorganic material with a softening point of 600°C to 1000°C (inclusive). For example, the inorganic material may be a silicate (e.g., at least one of silicon oxide, sodium oxide, calcium oxide, and magnesium oxide). The reinforcing material is sintered so that the inorganic material can at least partially penetrate into the pores of the structure.
[0062] Please see Figure 13 The thickness of the portion of the structure filled with reinforcing material along the first direction can be adjusted according to design requirements. However, in order to form a structurally stable reinforcing part 112, it is preferable that the thickness of the portion of the structure filled with reinforcing material along the first direction can be 50μm to 200μm (including endpoint values). For example, the thickness of the portion of the structure filled with reinforcing material along the first direction can be 50μm, 77μm, 100μm, 136μm, 150μm, 178μm, 200μm, etc.
[0063] In other embodiments, the liquid-conducting body 111 may also be a porous structure, with the reinforcing part 112 connected to the structure. That is, the reinforcing part 112 is mainly formed on the surface of the structure, and the reinforcing material of the reinforcing part 112 hardly penetrates into the pores of the structure (in some cases, a small amount of reinforcing material may penetrate into the pores of the structure).
[0064] Exemplarily, the material used to manufacture the reinforcement 112 may include reinforcing material and aggregate, wherein the aggregate may be one or more of ceramics, alumina, and zirconium oxide. The reinforcing material may also include at least an inorganic material with a softening point of 600°C to 1000°C (inclusive). The reinforcing material can be bonded to the structure by sintering, and the aggregate will not penetrate into the pores of the structure during sintering, thereby allowing the reinforcement 112 to be mainly formed on the surface of the structure.
[0065] This application also provides a method for preparing an atomizing core 10. This method can be used to prepare the atomizing core 10 with reinforcing material infiltrating the structure described in the above embodiments. Please refer to [link to relevant documentation]. Figure 8 The preparation method includes the following steps: Step S1: Apply a reinforcing slurry containing reinforcing material to a porous structure so that at least part of the reinforcing slurry penetrates into some of the pores of the structure.
[0066] The reinforcing material is mainly in powder form. In addition to the reinforcing material, the reinforcing slurry may also contain organic solvents and resins. The reinforcing material, organic solvents, and resins can be premixed to ensure that the powdered reinforcing material is evenly dispersed. Then, the reinforcing slurry is repeatedly rolled using a mill to achieve a submicron fineness (typically less than 10 μm) in the powder particles of the reinforcing material. This allows at least a portion of the reinforcing slurry to penetrate into some of the pores of the structure.
[0067] Step S2: Dry the reinforcing slurry so that the parts of the structure not filled with reinforcing material form a liquid-conducting body, and the parts of the structure filled with reinforcing material form at least a portion of the reinforcing part.
[0068] Since at least a portion of the reinforcing slurry penetrates into some of the pores of the structure before the reinforcing slurry is dried, after the reinforcing slurry is dried, at least a portion of the reinforcing material can fill some of the pores of the structure, thereby forming at least a portion of the reinforcing part in the area of the structure filled with the reinforcing material.
[0069] Step S3: Connect the electrical connection part of the heating element to the reinforcement part.
[0070] For example, an adhesive paste or a screen-printed adhesive layer can be applied to the contact portion 121 of the heating element 12, and the contact portion 121 can be bonded to the reinforcing portion 112 through the adhesive paste or adhesive layer. After the bonding is completed, a drying process is performed again to dry the adhesive paste or adhesive layer.
[0071] Step S4: Sinter the structure.
[0072] For some reinforcing slurries, before sintering, only a portion of the slurry penetrates into some of the pores of the structure, while the remaining portion remains outside the structure. Therefore, during the sintering process, at least some of the reinforcing material outside the structure can soften and penetrate into some of the pores. This effectively increases the thickness of the portion of the structure filled with reinforcing material after sintering.
[0073] In one specific embodiment, the structure may be made of ceramic material, the porosity of the structure is 68%, the average pore size of the structure is 20 μm, and the thickness of the structure along the first direction is 2 mm.
[0074] Reinforcing materials may include 72% 11% 11% 3% MgO and 3% The softening point of the reinforcing material is 750℃, and the reinforcing material is a powder with a particle size of 3mm~8mm (inclusive). Then, organic solvents and resins are added. The organic solvents include terpineol and butylcarbohydrate, which are mixed in a 7:3 ratio. The final formulation is a reinforcing slurry with a solid content of 55%, meaning that in 100 parts by weight, the reinforcing slurry comprises 55 parts of reinforcing material, 42 parts of organic solvent, and 3 parts of resin. The reinforcing slurry is then ground and rolled, resulting in a viscosity of approximately 60 Pa·s-120 Pa·s (inclusive).
[0075] A layer of reinforcing paste is coated onto the structure using a screen printing process and then dried at 80℃~120℃.
[0076] A layer of adhesive paste is applied to the electrical contact portion 121 of the heating element 12 using a screen printing process. The electrical contact portion 121 of the heating element 12 is aligned with the position on the structure where the reinforcing paste is applied, and the conductive portion is aligned with the atomization area 111a. The heating element 12 and the structure are bonded together using the adhesive paste, and then dried at a temperature of 80°C to 120°C (including the endpoint value).
[0077] After drying, sintering is performed. The sintering temperature can be adjusted according to the bonding slurry, but is generally 900℃. The sintering process takes 60 minutes.
[0078] After sintering, the atomizing core 10 is formed.
[0079] In addition, to improve production efficiency during industrial production, a larger structure can be used. For example, the surface of the structure perpendicular to the first direction can be quadrilateral, with dimensions of (60mm~100mm) × (60mm~100mm). Multiple reinforcing portions 112 of atomizing cores 10 are simultaneously formed on the structure. Each reinforcing portion 112 is connected to the corresponding electrical connection portion 121 of the heating element 12. After sintering, the structure is cut to a preset size to form multiple atomizing cores 10.
[0080] This application also provides a method for preparing the atomizing core 10. Please refer to [link to relevant documentation]. Figure 9 This preparation method can be used to prepare the atomizing core 10 described in the above embodiments, in which the reinforcing material hardly penetrates into the pores of the structure. The preparation method includes the following steps: Step S5: Apply a reinforcing slurry containing aggregates and reinforcing materials to a porous structure.
[0081] The reinforcing slurry includes aggregates and reinforcing materials. The aggregates can be materials similar to or the same as those in the structure, and the particle size of the aggregates is larger than the pore diameter of the structure. The reinforcing slurry may also include a pore-forming agent, and by controlling the ratio of aggregates to pore-forming agent, the porosity of the reinforcing part 112 is pre-controlled to below 50%.
[0082] Step S6: Dry the reinforcing slurry so that the structure forms a liquid-conducting body, and the aggregate and reinforcing material form a reinforcing part on the outer surface of the liquid-conducting body.
[0083] If the particle size of the reinforcing material is larger than the pore diameter of the structure, the reinforcing material is located outside the structure during coating and drying. If the particle size of the reinforcing material is less than or equal to the pore diameter of the structure, some of the reinforcing material will penetrate into some of the pores of the structure after coating. However, for this type of atomizing core 10, the main structure of the reinforcing part 112 is formed by aggregate, so the reinforcing part 112 is mainly formed on the outer surface of the liquid guiding body.
[0084] Step S7: Connect the electrical connection part of the heating element to the reinforcement part.
[0085] This step is largely the same as step S3 in the previous embodiment, and will not be described again here. Step S8: Perform sintering treatment on the structure.
[0086] During the sintering process of the structure, the reinforcing material mainly softens and penetrates into the aggregate, thus bonding with the aggregate as a whole.
[0087] In one specific embodiment, the structure may be made of ceramic material, the structure has a porosity of 68%, an average pore size of 20 μm, and a thickness of 2 mm along the first direction.
[0088] In 100 parts by weight, the reinforcing slurry comprises 30 parts diatomaceous earth, 10 parts reinforcing material, 15 parts pore-forming agent, 42 parts organic solvent, and 3 parts resin. The diatomaceous earth is the aggregate, with a particle size of 30 μm. The reinforcing material comprises 72%... 11% 11% 3% MgO and 3% The softening point of the reinforcing material is 750℃, and the reinforcing material is in powder form with a particle size of 3mm~8mm (inclusive). The organic solvents include terpineol and butylcarbohydrate, which are mixed in a 7:3 ratio. The pore-forming agent and diatomaceous earth are mixed in a 1:2.5 ratio.
[0089] A layer of reinforcing paste is coated onto the structure using a screen printing process. The thickness of the reinforcing paste along the first direction is 30μm~50μm (including the endpoint value), and then dried at 80℃~120℃.
[0090] A layer of adhesive paste is applied to the contact portion 121 of the heating element 12 using a screen printing process. The contact portion 121 of the heating element 12 is aligned with the position on the structure coated with reinforcing paste, and the conductive portion is aligned with the atomization area 111a. The heating element 12 and the structure are bonded together using the adhesive paste, and then dried at 80℃~120℃ (including the endpoint value). In industrial production, multiple heating elements 12 can be bonded to the liquid-conducting body portion 111.
[0091] After bonding, sintering is performed. The sintering temperature can be adjusted according to the bonding slurry, generally 900℃. Sintering takes 60 minutes. During sintering, a pore-forming agent acts on the diatomaceous earth, creating pores. The porosity of the diatomaceous earth is 50%. The reinforcing material softens and flows, penetrating into the pores of the structure and the pores of the diatomaceous earth, forming the reinforcing part 112. The remaining portion forms the liquid-conducting main body 111. The thickness of the reinforcing part 112 along the first direction is 20μm~30μm (including the endpoints).
[0092] After sintering, the atomizing core 10 is formed.
[0093] In addition, to improve production efficiency during industrial production, a larger structure can be used. For example, the surface of the structure perpendicular to the first direction can be quadrilateral, with dimensions of (60mm~100mm) × (60mm~100mm). Multiple reinforcing portions 112 of atomizing cores 10 are simultaneously formed on the structure. Each reinforcing portion 112 is connected to the corresponding electrical connection portion 121 of the heating element 12. After sintering, the structure is cut to a preset size to form multiple atomizing cores 10.
[0094] In the description of this application, the references to terms such as "in one embodiment," "in some embodiments," "in other embodiments," "in yet another embodiment," or "exemplary," etc., refer to specific features, structures, materials, or characteristics described in connection with that embodiment or example, which are included in at least one embodiment or example of the embodiments of this application. In this application, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in a suitable manner in any one or more embodiments or examples. Furthermore, without contradiction, those skilled in the art can combine the different embodiments or examples described in this application, as well as the features of the different embodiments or examples.
[0095] The above description is merely a preferred embodiment of this application and is not intended to limit the application. Various modifications and variations can be made to this application by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application are included within the scope of protection of this application.
Claims
1. An atomizing core, characterized in that, include: A liquid-conducting substrate, the liquid-conducting substrate including a liquid-conducting main body and a reinforcing part disposed on a first side of the liquid-conducting main body along a first direction, the liquid-conducting main body having an atomizing region disposed on the first side, and the reinforcing part avoiding the atomizing region; A heating element having an electrical contact portion and a heating portion electrically connected to the electrical contact portion, the heating element being disposed on the first side, the electrical contact portion being at least connected to the reinforcing portion, and at least a portion of the heating portion being disposed in the atomizing region.
2. The atomizing core according to claim 1, characterized in that, The atomizing region is located on one side of the reinforcing part along the second direction, which intersects with the first direction, and the distance between the heating part and the reinforcing part along the second direction is greater than 0.
3. The atomizing core according to claim 2, characterized in that, The distance between the heating element and the reinforcing element along the second direction is greater than or equal to 0.3 mm; and / or, A portion of the electrical contact portion protrudes from the reinforcing portion along the second direction on the side near the atomizing region.
4. The atomizing core according to any one of claims 1 to 3, characterized in that, The reinforcement includes a connection region and an extended region located around the connection region, and the power receiving part is connected to the connection region.
5. The atomizing core according to claim 4, characterized in that, The atomizing region is located on one side of the reinforcing portion along the second direction, which intersects with the first direction; The extended region includes a first sub-region, which is located on the side of the connecting region opposite to the atomizing region along the second direction; and / or The extended region includes a second sub-region, which is located on at least one side of the connecting region along a third direction, the third direction intersecting the first direction and the second direction respectively.
6. The atomizing core according to claim 5, characterized in that, The extended region includes the second sub-region, a portion of which protrudes from the connecting region along the second direction on the side close to the atomizing region.
7. The atomizing core according to any one of claims 1 to 3, characterized in that, The liquid guiding body is a porous structure, and the reinforcing part is connected to the structure.
8. The atomizing core according to any one of claims 1 to 3, characterized in that, A portion of the porous structure is filled with a reinforcing material such that the unfilled portions of the structure form the fluid-conducting body, and the portions of the structure filled with the reinforcing material form at least a portion of the reinforcing part.
9. The atomizing core according to claim 8, characterized in that, The thickness of the portion of the structure filled with the reinforcing material along the first direction is 50 μm to 200 μm.
10. The atomizing core according to any one of claims 1 to 3, characterized in that, The first side of the liquid-conducting body has a first end face, and the reinforcing portion at least partially protrudes from the first end face, wherein the thickness of the reinforcing portion protruding from the first end face along the first direction is less than or equal to 50 μm; and / or, The reinforcing part includes at least an inorganic material with a softening point of 600℃ to 1000℃.
11. An atomizer, characterized in that, include: The housing and the atomizing core according to any one of claims 1 to 10, wherein the housing has a liquid storage chamber and an air outlet channel, and the liquid storage chamber and the air outlet channel are in fluid communication through the atomizing core.
12. An aerosol generating device, characterized in that, include: The power supply assembly and the atomizer of claim 11, wherein the power supply assembly is electrically connected to the electrical connection portion of the heating element.