A sulfur trioxide resistant denitration reactor

By using high-temperature resistant alloy coatings, electric heating plates, and turbulence-inducing components in the SCR denitrification reactor, the temperature is controlled and ammonium sulfate formation is prevented, thus solving the problems of catalyst poisoning and corrosion caused by sulfur trioxide and ensuring denitrification efficiency and equipment stability.

CN225006760UActive Publication Date: 2026-11-24JIANGSU YOUSHANG ENVIRONMENTAL ENG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202521869339.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-09-01
Publication Date
2026-11-24
Estimated Expiration
2035-09-01

AI Technical Summary

Technical Problem

In the traditional SCR denitrification process, sulfur trioxide reacts with ammonia to produce ammonium sulfate or ammonium bisulfate, which leads to catalyst poisoning. In addition, high concentrations of SO₃ cause the sulfuric acid dew point temperature to rise, resulting in reactor corrosion and a decrease in denitrification efficiency.

Method used

The reactor body is coated with a high-temperature alloy and is equipped with an electric heating plate and a temperature sensor to control the temperature at 450℃. Combined with a turbulence-inducing component and a honeycomb denitrification catalyst, it prevents the formation of ammonium sulfate and uniforms the airflow temperature, thereby reducing the risk of corrosion.

Benefits of technology

It effectively prevents catalyst poisoning, maintains denitrification efficiency, reduces reactor corrosion, and improves equipment lifespan and operational stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225006760U_ABST
    Figure CN225006760U_ABST
Patent Text Reader

Abstract

This utility model relates to a sulfur trioxide-resistant denitrification reactor, which includes a reactor body. An electric heating plate, a pressure sensor, and a temperature sensor are installed inside the reactor body. The electric heating plate, pressure sensor, and temperature sensor are electrically connected. The electric heating plate is installed at the top of the reactor body along its length. The temperature sensor is located near the electric heating plate, on the side of the electric heating plate closest to the catalytic oxidation combustion chamber. A denitrification catalyst is installed inside the reactor body via an assembly. An inlet pipe and an outlet pipe are respectively installed at both ends of the reactor body along its axial direction. The inlet pipe is connected to the outlet of the catalytic oxidation combustion chamber. The pressure sensor is installed inside the inlet pipe. The outlet pipe is connected to the inlet of the desulfurization tower. This application has the function of ensuring denitrification effect and reducing reactor corrosion.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of waste gas treatment, and in particular to a denitrification reactor resistant to sulfur trioxide. Background Technology

[0002] In VOCs waste gas treatment processes containing sulfur and nitrogen, nitrogen-containing compounds in the waste gas are oxidized into nitrogen oxides after catalytic oxidation. Currently, the denitrification technology used in the market employs traditional denitrification catalysts (vanadium-titanium systems). In the traditional SCR denitrification process, the waste gas first undergoes catalytic oxidation in a combustion chamber, reaching a temperature of approximately 300-400℃. It then enters the denitrification reactor to contact the denitrification catalyst and undergo a denitrification reaction. Afterward, it is cooled by a boiler system and finally passes through a desulfurization tower for desulfurization treatment. If the waste gas contains sulfur, the sulfur will be converted into sulfur dioxide and sulfur trioxide after catalytic oxidation.

[0003] If the exhaust gas after catalytic oxidation contains sulfur trioxide, it will lead to the formation of sulfuric acid in the exhaust gas, which is highly corrosive. When NH3 escapes from the SCR denitrification module, sulfur trioxide will react with ammonia to generate ammonium sulfate or ammonium bisulfate. When the exhaust gas temperature is lower than the dew point temperature of ammonium sulfate or ammonium bisulfate, liquid ammonium sulfate or ammonium bisulfate enters the micropores of the catalyst, covering the active surface and reducing the denitrification effect. The dew point temperatures of ammonium bisulfate and ammonium sulfate depend on the concentrations and partial pressures of ammonia and sulfur trioxide in the exhaust gas. Higher concentrations of NH3 and SO3 in the exhaust gas make ammonium bisulfate and ammonium sulfate more likely to condense at higher temperatures, typically between 280 and 350°C. Under conditions with high SO3 concentrations, this temperature can reach 400°C or higher.

[0004] Furthermore, in the design and operation of the reactor, the flue gas temperature is one of the important factors affecting the denitrification efficiency and the safe operation of the equipment. The flue gas temperature is constrained by the sulfuric acid dew point in the exhaust gas (the sulfuric acid dew point temperature of the exhaust gas is also related to the concentration of SO3 in the exhaust gas; the higher the concentration of SO3 in the exhaust gas, the higher its sulfuric acid dew point temperature, which can generally be considered as 140~280℃). If the flue gas temperature is too low, a large amount of sulfuric acid vapor will condense on the low-temperature heating surface in the part where the wall temperature is below the dew point, causing severe corrosion of the heating surface metal. In severe cases, the heating surface must be replaced every few months, resulting in huge economic losses.

[0005] To avoid the aforementioned phenomena, the temperature inside the reactor must be maintained above the dew point of ammonium sulfate or ammonium bisulfate and above the dew point of sulfuric acid in the exhaust gas, i.e., 400°C or higher. Therefore, a reactor capable of ensuring denitrification efficiency during the denitrification process is needed. Utility Model Content

[0006] To address the aforementioned technical problems, this application provides a denitrification reactor resistant to sulfur trioxide.

[0007] The sulfur trioxide-resistant denitrification reactor provided in this application adopts the following technical solution: A sulfur trioxide-resistant denitrification reactor includes a reactor body. An electric heating plate, a pressure sensor, and a temperature sensor are installed inside the reactor body. The electric heating plate, the pressure sensor, and the temperature sensor are electrically connected. The electric heating plate is installed at the top of the middle part of the reactor body along its length. The temperature sensor is located near the electric heating plate and on the side of the electric heating plate that is close to the catalytic oxidation reaction combustion chamber. The reactor body is equipped with a denitrification catalyst via an installation assembly. An inlet pipe and an outlet pipe are respectively provided at both ends of the reactor body along the axial direction. The inlet pipe is connected to the outlet end of the catalytic oxidation reaction combustion chamber, and the outlet pipe is connected to the inlet end of the desulfurization tower. The pressure sensor is installed inside the inlet pipe.

[0008] Preferably, a flow-disrupting component is provided inside the reactor body, which is used to uniformly measure the temperature inside the reactor body.

[0009] Preferably, the turbulence-disrupting assembly includes turbulence-disrupting blades, a connecting shaft, and a fixing ring. The turbulence-disrupting blades are inclined and multiple blades are equidistantly arranged along the circumference of the fixing ring. The connecting shaft and the fixing ring are fixedly connected by a connecting rod. The turbulence-disrupting blades are rotatably connected to the connecting shaft via the connecting ring. The outer peripheral wall of the fixing ring is fixedly connected to the inner peripheral wall of the reactor body.

[0010] Preferably, multiple baffles are provided on both sides of the fixed ring in the thickness direction, and the two ends of the connecting shaft are respectively located on both sides of the fixed ring in the thickness direction. The baffles on both sides of the fixed ring are respectively sleeved on the two ends of the connecting shaft through a connecting ring.

[0011] Preferably, at least two connecting rods are provided, one end of the connecting rod is fixedly connected to the connecting shaft, and the other end of the connecting rod is fixedly connected to the fixing ring, and the spacing between the multiple connecting rods is consistent.

[0012] Preferably, the turbulence-disrupting components are respectively disposed at both ends of the reactor body along the axial direction.

[0013] Preferably, the inner peripheral wall of the reactor body is provided with a high-temperature resistant alloy coating, which is a nickel alloy coating.

[0014] Preferably, the installation assembly includes a positioning plate, which is fan-shaped and has uniformly distributed through holes for gas flow; multiple positioning plates are equidistantly arranged along the axial direction of the reactor body, and the denitrification catalyst is disposed between two adjacent positioning plates, wherein the denitrification catalyst is in the form of a honeycomb.

[0015] Preferably, an installation opening is provided on the side wall of the reactor body. The length of the installation opening is greater than the distance between the two furthest surfaces of the two farthest denitrification catalysts, and the width of the installation opening is greater than the width of the denitrification catalyst. A sealing baffle is rotatably installed at the installation opening. The sealing baffle is an arc-shaped plate. The length of the sealing baffle is greater than the length of the installation opening, and the width of the sealing baffle is greater than the width of the installation opening. The inner wall of the sealing baffle abuts against the outer wall of the reactor body, and the top of the sealing baffle is rotatably connected to the outer wall of the reactor body through a rotating shaft. The sealing baffle is fixed to the reactor body by a fixing assembly.

[0016] Preferably, the fixing component includes a fixing screw and a fixing nut. The fixing screw is fixedly connected to both sides of the installation port along its length. The sealing baffle has fixing holes on both sides along its length for the fixing screw to pass through. The fixing holes are oblong in shape. The fixing nut is threaded to the part of the fixing screw that passes through the fixing hole. The fixing nut is abutted against the side of the sealing baffle away from the reactor body.

[0017] In summary, this application includes the following beneficial technical effects: By installing an electric heating plate inside the reactor body, the electric heating plate is activated when the pressure sensor detects that the exhaust gas has just entered the inlet pipe. The temperature sensor detects that the electric heating plate has heated the temperature inside the reactor body to 450℃ and then controls the electric heating plate to stop heating. In a temperature environment of 400℃-450℃, the possibility of sulfur trioxide reacting with ammonia to form ammonium sulfate or ammonium bisulfate is reduced. This reduces the possibility of liquid ammonium sulfate or ammonium bisulfate entering the micropores of the catalyst and blocking the active surface, ensuring the effectiveness of the catalyst and the denitrification effect. It also reduces the possibility of sulfuric acid vapor condensation on the low-temperature heating surfaces inside the reactor where the wall temperature is below the dew point, thereby reducing the corrosion of the metal reactor. When the exhaust gas passes through the baffle blades, the baffle blades rotate, and the turbulent airflow makes the gas temperature rise more uniformly and quickly, resulting in better performance. Attached Figure Description

[0018] Figure 1 This is a schematic diagram of the overall structure of a sulfur trioxide-resistant denitrification reactor in an embodiment of this application.

[0019] Figure 2 This is a schematic diagram illustrating the structure of the sealing baffle after it is opened, as shown in the embodiments of this application.

[0020] Figure 3 This is a cross-sectional structural diagram used in the embodiments of this application to show the internal structure of the reactor body.

[0021] Explanation of reference numerals in the attached drawings: 1. Reactor body; 11. Inlet pipe; 12. Outlet pipe; 13. Mounting port; 14. Sealing baffle; 141. Fixing hole; 2. Electric heating plate; 3. Pressure sensor; 4. Temperature sensor; 5. Mounting assembly; 51. Positioning plate; 511. Through hole; 6. Fixing assembly; 61. Fixing screw; 62. Fixing nut; 7. Turbulence assembly; 71. Turbulence blade; 72. Connecting shaft; 73. Fixing ring; 74. Connecting rod; 75. Connecting ring. Detailed Implementation

[0022] The following is in conjunction with the appendix Figure 1-3 This application will be described in further detail.

[0023] This application discloses a sulfur trioxide-resistant denitrification reactor.

[0024] Reference Figure 1-3 The sulfur trioxide-resistant denitrification reactor includes a reactor body 1. The inner peripheral wall of the reactor body is provided with a high-temperature resistant alloy coating. The high-temperature resistant alloy coating is a nickel alloy coating. Nickel alloy has extremely high corrosion resistance and can withstand temperatures up to 1300℃. By setting the nickel alloy coating, the high-temperature resistance and corrosion resistance of the reactor body 1 can be greatly improved, thereby increasing the service life of the reactor body 1.

[0025] The reactor body 1 is equipped with an electric heating plate 2, a pressure sensor 3 and a temperature sensor 4. The electric heating plate 2, the pressure sensor 3 and the temperature sensor 4 are electrically connected. The electric heating plate 2 is installed at the top of the middle part of the reactor body 1 in the length direction. The temperature sensor 4 is located near the electric heating plate 2 and is located on the side of the electric heating plate 2 that is close to the catalytic oxidation reaction combustion chamber.

[0026] An inlet pipe 11 and an outlet pipe 12 are respectively provided at both ends of the reactor body 1 along the axial direction. The inlet pipe 11 is connected to the outlet end of the catalytic oxidation reaction combustion chamber, and the outlet pipe 12 is connected to the inlet end of the desulfurization tower. The pressure sensor 3 is installed inside the inlet pipe 11.

[0027] A denitrification catalyst is installed inside the reactor body 1 via an installation assembly 5. The installation assembly 5 includes a positioning plate 51, which is fan-shaped and whose outer wall is fixedly connected to the inner wall of the reactor body 1. The positioning plate 51 has uniformly distributed through holes 511 for gas flow. Multiple positioning plates 51 are equidistantly arranged along the axial direction of the reactor body 1. The denitrification catalyst is positioned between adjacent positioning plates 51. In this embodiment, there are five positioning plates 51 and four denitrification catalysts, which are arranged in a honeycomb structure.

[0028] An installation port 13 is provided on the side wall of the reactor body 1. The length of the installation port 13 is greater than the distance between the two furthest surfaces of the two farthest denitrification catalysts. The width of the installation port 13 is greater than the width of the denitrification catalyst. A sealing baffle 14 is rotatably installed at the installation port 13. The sealing baffle 14 is an arc-shaped plate. The length of the sealing baffle 14 is greater than the length of the installation port 13. The width of the sealing baffle 14 is greater than the width of the installation port 13. The inner wall of the sealing baffle 14 abuts against the outer wall of the reactor body 1. The top of the sealing baffle 14 is rotatably connected to the outer wall of the reactor body 1 through a rotating shaft. The sealing baffle 14 is fixed to the reactor body 1 by a fixing component 6.

[0029] The fixing component 6 includes a fixing screw 61 and a fixing nut 62. The fixing screw 61 is fixedly connected to both sides of the mounting port 13 along its length. The sealing baffle 14 has fixing holes 141 on both sides along its length for the fixing screw 61 to pass through. The fixing holes 141 are oblong in shape to allow the fixing screw 61 to pass through. The fixing nut 62 is threaded to the part of the fixing screw 61 that extends out of the fixing hole 141. The fixing nut 62 abuts against the side of the sealing baffle 14 away from the reactor body 1, locking the sealing baffle 14 to the reactor body 1. When the denitrification catalyst needs to be replaced, the fixing nut 62 is unscrewed, the sealing baffle 14 is opened, and the denitrification catalyst can be replaced, making the operation convenient.

[0030] A flow disturbance component 7 is provided inside the reactor body 1. The flow disturbance component 7 is respectively located at both ends of the reactor body 1 along the axial direction to improve the flow disturbance effect. The flow disturbance component 7 is used to uniformly measure the temperature inside the reactor body 1.

[0031] The turbulence-inducing assembly 7 includes turbulence-inducing blades 71, a connecting shaft 72, and a fixing ring 73. The turbulence-inducing blades 71 are inclined and multiple blades are equidistantly arranged along the circumference of the fixing ring 73. The connecting shaft 72 and the fixing ring 73 are fixedly connected by connecting rods 74. At least two connecting rods 74 are provided, one end of which is fixedly connected to the connecting shaft 72, and the other end of which is fixedly connected to the fixing ring 73. The spacing between the multiple connecting rods 74 is consistent. The turbulence-inducing blades 71 are rotatably connected to the connecting shaft 72 via connecting rings 75. The outer circumferential wall of the fixing ring 73 is fixedly connected to the inner circumferential wall of the reactor body 1. Multiple turbulence-inducing blades 71 are arranged on both sides of the fixing ring 73 in the thickness direction. The two ends of the connecting shaft 72 are located on both sides of the fixing ring 73 in the thickness direction. The turbulence-inducing blades 71 on both sides of the fixing ring 73 are respectively fitted onto the two ends of the connecting shaft 72 via a connecting ring 75, thereby improving the turbulence-inducing effect.

[0032] By installing an electric heating plate 2 inside the reactor body 1, the electric heating plate 2 is activated when the pressure sensor 3 detects that the exhaust gas has just entered the inlet pipe 11. The temperature sensor 4 detects that the electric heating plate 2 has heated the temperature inside the reactor body 1 to 450℃ and then controls the electric heating plate 2 to stop heating. In a temperature environment of 400℃-450℃, the possibility of sulfur trioxide reacting with ammonia to produce ammonium sulfate or ammonium bisulfate is reduced, thereby reducing the possibility of liquid ammonium sulfate or ammonium bisulfate entering the micropores of the catalyst and blocking the active surface, ensuring the effect of the catalyst and the denitrification effect. It also reduces the possibility of sulfuric acid vapor condensation on the low-temperature heating surface inside the reactor where the wall temperature is below the dew point, thereby reducing the corrosion of the metal reactor. When the exhaust gas passes through the baffle blades 71, the baffle blades 71 rotate, and the turbulent airflow makes the gas temperature rise more uniformly and quickly, resulting in better effect.

[0033] The above are all preferred embodiments of this application, and are not intended to limit the scope of protection of this application. Therefore, all equivalent changes made in accordance with the structure, shape and principle of this application should be covered within the scope of protection of this application.

Claims

1. A sulfur trioxide resistant denitration reactor characterized by: The reactor includes a reactor body, within which an electric heating plate, a pressure sensor, and a temperature sensor are installed. The electric heating plate, pressure sensor, and temperature sensor are electrically connected. The electric heating plate is installed at the top of the reactor body in the middle of its length direction, and the temperature sensor is located near the electric heating plate and on the side of the electric heating plate that is close to the catalytic oxidation reaction combustion chamber. The reactor body is equipped with a denitrification catalyst via an installation assembly. An inlet pipe and an outlet pipe are respectively provided at both ends of the reactor body along the axial direction. The inlet pipe is connected to the outlet end of the catalytic oxidation reaction combustion chamber, and the outlet pipe is connected to the inlet end of the desulfurization tower. The pressure sensor is installed inside the inlet pipe.

2. The sulfur trioxide tolerant deNOx reactor of claim 1, wherein: The reactor body is equipped with a flow-dispersing component, which is used to uniformly measure the temperature within the reactor body.

3. The sulfur trioxide-resistant denitrification reactor according to claim 2, characterized in that: The turbulence-disrupting assembly includes turbulence-disrupting blades, a connecting shaft, and a fixing ring. The turbulence-disrupting blades are inclined and multiple blades are equidistantly arranged along the circumference of the fixing ring. The connecting shaft and the fixing ring are fixedly connected by a connecting rod. The turbulence-disrupting blades are rotatably connected to the connecting shaft through the connecting ring. The outer peripheral wall of the fixing ring is fixedly connected to the inner peripheral wall of the reactor body.

4. The sulfur trioxide-resistant denitrification reactor according to claim 3, characterized in that: Multiple aerodynamic blades are provided on both sides of the fixed ring in the thickness direction. The two ends of the connecting shaft are located on both sides of the fixed ring in the thickness direction. The aerodynamic blades on both sides of the fixed ring are respectively sleeved on both ends of the connecting shaft through a connecting ring.

5. The sulfur trioxide-resistant denitrification reactor according to claim 3, characterized in that: The connecting rod is provided with at least two rods. One end of the connecting rod is fixedly connected to the connecting shaft, and the other end of the connecting rod is fixedly connected to the fixing ring. The spacing between the multiple connecting rods is consistent.

6. The sulfur trioxide-resistant denitrification reactor according to claim 2, characterized in that: The turbulence-inducing components are respectively located at both ends of the reactor body along its axial direction.

7. The sulfur trioxide-resistant denitrification reactor according to claim 1, characterized in that: The inner peripheral wall of the reactor body is provided with a high-temperature resistant alloy coating, which is a nickel alloy coating.

8. The sulfur trioxide-resistant denitrification reactor according to claim 1, characterized in that: The installation assembly includes a positioning plate, which is fan-shaped and has uniformly spaced through holes for gas flow. Multiple positioning plates are equidistantly arranged along the axial direction of the reactor body, and a denitrification catalyst is placed between two adjacent positioning plates. The denitrification catalyst is in the form of a honeycomb.

9. The sulfur trioxide-resistant denitrification reactor according to claim 8, characterized in that: An installation opening is provided on the side wall of the reactor body. The length of the installation opening is greater than the distance between the two furthest surfaces of the two farthest denitrification catalysts, and the width of the installation opening is greater than the width of the denitrification catalyst. A sealing baffle is rotatably installed at the installation opening. The sealing baffle is an arc-shaped plate. The length of the sealing baffle is greater than the length of the installation opening, and the width of the sealing baffle is greater than the width of the installation opening. The inner wall of the sealing baffle abuts against the outer wall of the reactor body, and the top of the sealing baffle is rotatably connected to the outer wall of the reactor body through a rotating shaft. The sealing baffle is fixed to the reactor body by a fixing assembly.

10. The sulfur trioxide-resistant denitrification reactor according to claim 9, characterized in that: The fixing assembly includes a fixing screw and a fixing nut. The fixing screw is fixedly connected to both sides of the installation port along its length. The sealing baffle has fixing holes on both sides along its length for the fixing screw to pass through. The fixing holes are oblong in shape. The fixing nut is threaded to the part of the fixing screw that passes through the fixing hole. The fixing nut is pressed against the side of the sealing baffle away from the reactor body.