TPU artificial leather stripping machine

By preheating the artificial leather during the TPU artificial leather recycling process, and using a heating system and telescopic heating device, the problem of difficult separation between the coating and the base fabric is solved, achieving efficient separation of the coating and the base fabric, and improving the purity and quality of the recycled material.

CN225007992UActive Publication Date: 2026-11-24JIANGXI SHENGXIANG NEW MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522314710.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-10-31
Publication Date
2026-11-24
Estimated Expiration
2035-10-31

AI Technical Summary

Technical Problem

In the current TPU artificial leather recycling process, mechanical blades have difficulty completely separating the coating and base fabric that are too firmly bonded, resulting in residual surface coating on the base fabric or fibers adhering to the coating, which affects the purity of the recycled material.

Method used

Before the separation component comes into contact with the artificial leather, the artificial leather is preheated by the contact roller. The temperature of the contact roller is increased by using a heating tube and a water pump circulation heating system to prevent the adhesion from being too strong. The bonding roller is further preheated by the telescopic tube to ensure effective separation of the coating from the base fabric.

Benefits of technology

This effectively avoids residual surface coatings or fibers adhering to the coating on the base fabric, improving the purity and quality of recycled materials and ensuring the smooth progress of subsequent processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225007992U_ABST
    Figure CN225007992U_ABST
Patent Text Reader

Abstract

This utility model discloses a TPU artificial leather peeling machine, relating to the field of artificial leather recycling technology. It aims to solve the problem that the purity of recycled materials from existing separation devices is affected by the adhesive strength of the artificial leather. The key technical points are: a base plate with two positioning plates fixedly connected to it, and a contact roller rotatably connected between the two positioning plates. The contact roller has a cavity inside. A water tank is fixedly connected to the base plate, and several heating pipes are fixedly connected inside the water tank. Two connecting pipes are rotatably connected to both ends of the contact roller, and the other ends of both connecting pipes are fixedly connected to the water tank and communicate with each other. A water pump is fixedly connected inside the water tank, and the output end of the water pump is fixedly connected to one of its connecting pipes. A separation component for peeling is provided on the positioning plate. This TPU artificial leather peeling machine can preheat the artificial leather via the contact roller before the separation component contacts it, preventing the artificial leather from being too firmly bonded, which could result in residual surface coating or fibers adhering to the surface coating on the base fabric.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of artificial leather recycling technology, and more specifically, it relates to a TPU artificial leather peeling machine. Background Technology

[0002] TPU (thermoplastic polyurethane) artificial leather has excellent wear resistance, flexibility, low temperature resistance, aging resistance, and environmental recyclability. However, the production process generates defective products and waste TPU leather products. When recycling, TPU artificial leather needs to be separated into surface coating and base fabric for separate recycling. Otherwise, it can only be downgraded (such as used as low-grade filler) and has a low value.

[0003] Existing recycling methods typically use purely mechanical stripping. Core components usually include a blade / scraper, a counterweight roller, and a tension control system. First, a tiny stripping point is created at the edge of the material manually or with auxiliary devices. The stripping point is then fed into the gap between the blade and the counterweight roller. Guided by the tensioned material, the sharp blade weds into the interface between the surface coating and the base fabric. The material continues to advance under the traction of the rollers, while the blade maintains a precise angle and position, continuously expanding the stripping interface until the surface coating and base fabric are separated and either wound up or collected separately.

[0004] The separation device in the above scheme does not use water or chemicals in the entire process. The produced TPU film and base fabric are dry and can directly enter the next recycling process without drying or wastewater treatment issues. However, if the artificial leather is too firmly bonded or penetrated too deeply during manufacturing, the mechanical blade may not be able to completely "scrape" it clean, resulting in residual surface coating on the base fabric or fibers adhering to the surface coating, affecting the purity of the recycled material.

[0005] Therefore, a new solution is needed to address this problem. Utility Model Content

[0006] To address the shortcomings of existing technologies, the purpose of this utility model is to provide a TPU artificial leather peeling machine that can preheat the artificial leather with a contact roller before the separation component comes into contact with it, thereby preventing the artificial leather from being too firmly bonded, which could result in residual surface coating on the base fabric or fibers adhering to the surface coating.

[0007] The above-mentioned technical objective of this utility model is achieved through the following technical solution: A TPU artificial leather peeling machine includes a base plate, two positioning plates are fixedly connected to the base plate, and a contact roller is rotatably connected between the two positioning plates. A cavity is opened in the contact roller. A water tank is fixedly connected to the base plate, and several heating tubes are fixedly connected to the water tank. Two connecting pipes are rotatably connected to both ends of the contact roller. The other ends of the two connecting pipes are fixedly connected to the water tank and communicate with each other. A water pump is fixedly connected to the water tank. The output end of the water pump is fixedly connected to one of the connecting pipes. A separation component for peeling leather is provided on the positioning plate.

[0008] The present invention is further configured such that: the separation component includes a positioning frame fixedly connected to the positioning plate, a positioning roller rotatably connected to the positioning frame, a bonding roller connected to the positioning frame, two positioning rings connected to the bonding roller, and a cutter fixedly connected between the two positioning rings; the positioning frame is provided with a driving component for driving the bonding roller to slide.

[0009] The present invention is further configured such that: the bonding roller is rotatably connected to the positioning frame, the positioning ring is rotatably connected to the bonding roller, the driving component includes an extension rod fixedly connected to the positioning frame and a spring telescopic rod fixedly connected to the extension rod, the telescopic end of the spring telescopic rod is fixedly connected to the adjacent positioning ring, and when the spring telescopic rod is in the normal state, the bonding roller and the positioning roller are in contact with each other.

[0010] The present invention is further configured such that: a telescopic tube is rotatably connected to the connecting tube, and the telescopic ends of the two telescopic tubes are respectively rotatably connected to the two ends of the bonding roller and communicate with each other.

[0011] The present invention is further configured such that a guide plate is fixedly connected to the cutter.

[0012] The present invention is further configured such that: a water pump is fixedly connected to the input end of the water pump, and the other end of the water pump is in contact with the bottom side of the water tank.

[0013] In summary, the present invention has the following beneficial effects: the artificial leather can be preheated by the contact roller before the separation component comes into contact with the artificial leather, so as to avoid the artificial leather being too firmly bonded, resulting in residual surface coating on the base fabric or fibers adhering to the surface coating. The artificial leather can also be further preheated by heating the bonding roller through the telescopic tube. Attached Figure Description

[0014] Figure 1 This is a schematic diagram of the structure of this utility model; Figure 2 A cross-sectional view of this utility model Figure 1 ; Figure 3 A cross-sectional view of this utility model Figure 2 .

[0015] In the diagram: 1. Base plate; 2. Positioning plate; 3. Contact roller; 4. Cavity; 5. Water tank; 6. Heating tube; 7. Connecting tube; 8. Water pump; 9. Positioning frame; 10. Positioning roller; 11. Bonding roller; 12. Positioning ring; 13. Cutter; 14. Extension rod; 15. Spring telescopic rod; 16. Telescopic tube; 17. Guide plate; 18. Pumping pipe. Detailed Implementation

[0016] The present invention will now be described in detail with reference to the accompanying drawings and embodiments.

[0017] A TPU artificial leather peeling machine, such as Figures 1-3 As shown, the system includes a base plate 1, two positioning plates 2 fixedly connected to the base plate 1, a contact roller 3 rotatably connected between the two positioning plates 2, a cavity 4 inside the contact roller 3, a water tank 5 fixedly connected to the base plate 1, several heating tubes 6 fixedly connected inside the water tank 5, two connecting pipes 7 rotatably connected to both ends of the contact roller 3, the other ends of the two connecting pipes 7 being fixedly connected to the water tank 5 and communicating with each other, a water pump 8 fixedly connected inside the water tank 5, the output end of the water pump 8 being fixedly connected to one of its connecting pipes 7, and a separation component for peeling leather on the positioning plates 2, the separation component including a positioning frame 9 fixedly connected to the positioning plates 2, and a fixed frame 9 rotatably connected to the positioning frame 9. The positioning roller 10, the bonding roller 11 connected to the positioning frame 9, the two positioning rings 12 connected to the bonding roller 11, and the cutter 13 fixedly connected between the two positioning rings 12 are provided on the positioning frame 9. The positioning frame 9 is provided with a driving component for driving the bonding roller 11 to slide. The bonding roller 11 is rotatably connected to the positioning frame 9, and the positioning rings 12 are rotatably connected to the bonding roller 11. The driving component includes an extension rod 14 fixedly connected to the positioning frame 9 and a spring telescopic rod 15 fixedly connected to the extension rod 14. The telescopic end of the spring telescopic rod 15 is fixedly connected to the adjacent positioning ring 12. When the spring telescopic rod 15 is in the normal state, the bonding roller 11 and the positioning roller 10 are in contact with each other.

[0018] like Figures 1-3As shown, when peeling is required, liquid can be poured into water tank 5 first, and then heating pipe 6 can be turned on to heat the liquid. When the liquid reaches the set temperature, water pump 8 can be turned on. Water pump 8 will draw liquid from water tank 5 and guide it into contact roller 3 through connecting pipe 7. Then, it will enter another connecting pipe 7 through contact roller 3 and finally return to water tank 5. This cycle will continuously heat contact roller 3. This heating method can greatly improve the temperature uniformity of contact roller 3, thereby avoiding residual surface coating or fibers adhering to the surface coating on the base fabric. Then, take one end of artificial leather and preheat the base fabric side against contact roller 3. Then, insert artificial leather into positioning roller 10 and bonding roller. Between 11, the bonding roller 11 will move towards the base plate 1, and the spring telescopic rod 15 will be in a contracted state, constantly pushing the artificial leather, so that the coating side and the positioning roller 10 are in contact with each other, and the base fabric side and the bonding roller 11 are in contact with each other. Then the artificial leather is separated by the cutter 13, so that the artificial leather is separated into the surface coating and the base fabric. Then the surface coating and the base fabric can be fixedly connected to the external coating winding roller and the external base fabric winding roller respectively (the external coating winding roller is located on the upper side of the external base fabric winding roller). Then the external coating winding roller and the external base fabric winding roller are started to rotate synchronously to peel the leather. If there is still adhesion in some parts of the artificial leather, the cutter 13 can cut the adhesion to ensure that the peeling can be carried out smoothly.

[0019] like Figure 1 , Figure 3 As shown, the bonding roller 11 is a hollow roller, and a telescopic tube 16 is rotatably connected to the connecting pipe 7. The telescopic ends of the two telescopic tubes 16 are rotatably connected to both ends of the bonding roller 11 and communicate with each other. When the water pump 8 draws liquid from the water tank 5, some liquid will enter the bonding roller 11 through the telescopic tube 16 and circulate to heat the bonding roller 11, thereby further preheating it so that the base fabric can be better peeled off from the coating, avoiding the presence of residual surface coating or fibers on the surface coating on the base fabric. When the artificial leather is inserted between the positioning roller 10 and the bonding roller 11, causing the bonding roller 11 to move towards the base plate 1, the telescopic tube 16 will also be driven to rotate and extend on the connecting pipe 7 and the bonding roller 11 to ensure that heated liquid can be transported into the bonding roller 11.

[0020] like Figure 1 As shown, a guide plate 17 is fixedly connected to the cutter 13. When the base fabric take-up roller is in a horizontal position above the cutter 13, the base fabric will come into contact with the guide plate 17, thereby preventing the tail end of the cutter 13 from scratching the base fabric.

[0021] like Figure 2 As shown, a water pump 8 is fixedly connected to a water pump pipe 18 at its input end. The other end of the water pump pipe 18 is in contact with the bottom side of the water tank 5, which can extend the interval between replenishing liquid into the water tank 5 and make full use of the liquid in the water tank 5.

[0022] Working principle: When peeling is required, liquid is first poured into water tank 5, and then heating pipe 6 is turned on to heat the liquid. When the liquid reaches the set temperature, water pump 8 is turned on. Water pump 8 draws liquid from water tank 5 and guides it into contact roller 3 through connecting pipe 7. Then, it enters another connecting pipe 7 through contact roller 3 and finally returns to water tank 5, thus circulating and continuously heating contact roller 3. At this time, some liquid enters bonding roller 11 through telescopic pipe 16 and circulates to heat bonding roller 11. Then, one end of artificial leather is removed, and the base fabric side of bonding contact roller 3 is preheated. Then, artificial leather is inserted between positioning roller 10 and bonding roller 11. At this time, bonding roller 11 will move towards the base plate 1 and... At this time, the spring telescopic rod 15 will be in a contracted state and will continue to push the artificial leather, so that the coating side and the positioning roller 10 are in contact with each other, and the base fabric side is in contact with the bonding roller 11. At the same time, the telescopic tube 16 will also be driven by the bonding roller 11 to rotate and extend on the connecting tube 7 and the bonding roller 11 to ensure that the heating liquid can be transported into the bonding roller 11. Then, the artificial leather is separated by the cutter 13, so that the artificial leather is separated into the surface coating and the base fabric. Then, the surface coating and the base fabric can be fixedly connected to the external coating winding roller and the external base fabric winding roller respectively. Then, the external coating winding roller and the external base fabric winding roller are started to rotate synchronously to peel the leather. If there is still adhesion in some parts of the artificial leather, the cutter 13 can cut the adhesion to ensure that the leather can be peeled smoothly.

[0023] The above description is merely a preferred embodiment of this utility model. The protection scope of this utility model is not limited to the above embodiments. All technical solutions falling within the scope of this utility model's concept are protected. It should be noted that for those skilled in the art, any improvements and modifications made without departing from the principle of this utility model should also be considered within the protection scope of this utility model.

Claims

1. A TPU artificial leather peeling machine, comprising a base plate (1), characterized in that: Two positioning plates (2) are fixedly connected to the base plate (1), and a contact roller (3) is rotatably connected between the two positioning plates (2). A cavity (4) is opened in the contact roller (3). A water tank (5) is fixedly connected to the base plate (1). Several heating tubes (6) are fixedly connected in the water tank (5). Two connecting pipes (7) are rotatably connected to both ends of the contact roller (3). The other ends of the two connecting pipes (7) are fixedly connected to the water tank (5) and communicate with each other. A water pump (8) is fixedly connected in the water tank (5). The output end of the water pump (8) is fixedly connected to one of the connecting pipes (7). A separation component for peeling leather is provided on the positioning plate (2).

2. The TPU artificial leather peeling machine according to claim 1, characterized in that: The separation assembly includes a positioning frame (9) fixedly connected to the positioning plate (2), a positioning roller (10) rotatably connected to the positioning frame (9), a bonding roller (11) connected to the positioning frame (9), two positioning rings (12) connected to the bonding roller (11), and a cutter (13) fixedly connected between the two positioning rings (12). The positioning frame (9) is provided with a driving component for driving the bonding roller (11) to slide.

3. A TPU artificial leather peeling machine according to claim 2, characterized in that: The bonding roller (11) is rotatably connected to the positioning frame (9), and the positioning ring (12) is rotatably connected to the bonding roller (11). The driving component includes an extension rod (14) fixedly connected to the positioning frame (9) and a spring telescopic rod (15) fixedly connected to the extension rod (14). The telescopic end of the spring telescopic rod (15) is fixedly connected to the adjacent positioning ring (12). When the spring telescopic rod (15) is in the normal state, the bonding roller (11) and the positioning roller (10) are in contact with each other.

4. A TPU artificial leather peeling machine according to claim 2, characterized in that: The connecting pipe (7) is rotatably connected to a telescopic pipe (16), and the telescopic ends of the two telescopic pipes (16) are rotatably connected to both ends of the bonding roller (11) and communicate with each other.

5. A TPU artificial leather peeling machine according to claim 2, characterized in that: A guide plate (17) is fixedly connected to the cutter (13).