Mold insert for preventing aluminum chip residue
By setting an inclined gap between the mold insert and the mold core and combining it with a snap-fit positioning connection, the problems of aluminum shavings residue and ejector pin jamming caused by the gap of the mold insert are solved, achieving efficient aluminum shavings removal and improved product quality.
Patent Information
- Application Number
- CN202522646181.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-15
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-15
AI Technical Summary
In existing technologies, the gap between the mold insert and the ejector pin can easily form a channel for aluminum liquid to penetrate, resulting in aluminum shavings residue, obstructed ejector pin movement, burrs on the product surface, and frequent shutdowns, which reduces production efficiency. Furthermore, traditional solutions increase manufacturing costs.
The design incorporates an inclined gap between the insert and the mold core, combined with snap-fit positioning and high-precision gap to form a three-level seal. Elastic pre-tightening and nano-coating are used to block the aluminum melt penetration path, and aluminum chips are automatically discharged through a spiral chip removal channel.
It effectively blocks the penetration path of molten aluminum, reduces burr formation, shortens downtime, reduces maintenance costs, and improves product qualification rate and production efficiency.
Smart Images

Figure CN225008435U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to a mold insert for preventing aluminum shavings residue, belonging to the technical field of mold components. Background Technology
[0002] Due to the requirements for surface and internal quality of products, die-casting molds often use inserts in many places. The burrs formed by the gaps between these inserts and the mold core or slide block require cleaning. In existing technology, the clearance (0.02-0.05mm) between the mold inserts and the ejector pins easily forms channels for molten aluminum to penetrate, leading to: (1) During the die casting process, aluminum chips accumulate in the gaps between the inserts. (2) Obstruction of ejector pin movement causes mold jamming failure (the industry average failure rate is 12%) (3) The product surface has burrs and flash (defect rate exceeds 8%) (4) Frequent machine shutdowns for cleaning (every 2 hours / time) reduce production efficiency. Traditional solutions involve increasing the hardness of the ejector pin (HRC58-62) or applying a DLC coating to the surface, but these methods cannot fundamentally solve the problem of aluminum molten metal penetration and increase manufacturing costs by more than 30%. Utility Model Content
[0003] The present invention addresses the above-mentioned defects by providing a mold insert with a reasonable structure that reduces burr generation and prevents aluminum shavings residue.
[0004] Therefore, the technical solution adopted by this utility model is as follows: a mold insert for preventing aluminum shavings residue, comprising the following structural form: including an insert, wherein the gap formed between the insert and the slider is perpendicular to the workpiece ejection direction, and the gap formed between the insert and the mold core is inclined at a certain angle to the workpiece ejection direction.
[0005] Furthermore, the gap formed between the insert and the mold core and the tilt angle of the workpiece ejection direction are set to be greater than or equal to 10 degrees.
[0006] Furthermore, the gap formed between the insert and the slider is maintained at 0.01~0.02mm on one side.
[0007] Furthermore, the gap between the insert and the mold core is maintained at 0.01~0.02mm on one side.
[0008] Furthermore, the insert and the slider are positioned and connected by snap-fit locating pins.
[0009] Furthermore, the insert and the mold core are positioned and connected by snap-fit locating pins.
[0010] The advantages of this utility model are: 1) It establishes a physical isolation barrier to block the penetration path of molten aluminum; 2) It designs a quick maintenance structure to shorten downtime; 3) It reduces mold maintenance costs by more than 40%; 4) It increases the product qualification rate to 99.5%. Attached Figure Description
[0011] Figure 1 This is a schematic diagram of the structure between the insert and the slider of this utility model.
[0012] Figure 2 This is a schematic diagram of the structure between the insert and the mold core of this utility model. Detailed Implementation
[0013] A mold insert for preventing aluminum shavings residue includes the following structure: it includes an insert, the gap between the insert and the slider is perpendicular to the workpiece ejection direction, and the gap between the insert and the mold core is inclined at a certain angle to the workpiece ejection direction.
[0014] Furthermore, the gap formed between the insert and the mold core and the tilt angle of the workpiece ejection direction are set to be greater than or equal to 10 degrees.
[0015] Furthermore, the gap formed between the insert and the slider is maintained at 0.01~0.02mm on one side.
[0016] Furthermore, the gap between the insert and the mold core is maintained at 0.01~0.02mm on one side.
[0017] Furthermore, the insert and the slider are positioned and connected by snap-fit locating pins.
[0018] Furthermore, the insert and the mold core are positioned and connected by snap-fit locating pins.
[0019] The present invention will be further described below to provide a better understanding of it: Design principles: 1. Mounting: Position the gap where the insert might form burrs perpendicular to the product's ejection direction to avoid burr formation (see...). Figure 1 ).
[0020] 2. Angled Inlay: The gaps between the inserts that may form burrs are designed at a certain angle to the product's ejection direction. This angle should be greater than or equal to 10° to effectively avoid burr formation (see...). Figure 2 ).
[0021] 3. High-precision mold processing: Minimize the size of the gap, keep the splicing gap at 0.01~0.02mm on one side to prevent the formation of burrs.
[0022] The working process of this utility model is as follows: 1. When the mold is closed, the elastic clamping mechanism generates a pre-tightening force of 8-12kN, so that the insert and the mold core fit tightly together; 2. During the die-casting process, the micro-convex guide platform guides the molten aluminum to flow towards the chip removal groove; 3. During mold opening, the spiral chip removal channel generates centrifugal force (>200N) during the ejection process, discharging aluminum chips along a 45° guide angle; 4. The nano-coating reduces the surface friction coefficient (μ < 0.1) and prevents secondary adhesion.
[0023] The aforementioned structures, such as spiral chip conveyor channels and flow guiding platforms, are all conventional structures and will not be described in detail here.
[0024] This utility model: 1) Composite seepage-proof structure: stepped inserts + elastic pre-tightening form a three-level seal (gap < 0.005mm).
[0025] 2) Dynamic chip removal mechanism: The spiral groove is coupled with the ejector pin to realize the automatic discharge of aluminum chips. This feature is a conventional structure and will not be described further here.
[0026] 3) Quick disassembly and assembly design: adopts snap-on positioning pins (disassembly time < 30 seconds).
[0027] 4) Thermal expansion compensation: The insert and the mold core are designed with different coefficients of thermal expansion (Δα=2.3×10⁻). 6 / ℃), determined by rationally selecting existing materials.
[0028] Using the above-mentioned technical features, the experimental data of this utility model in a certain instance is as follows: index Before improvement Improved Increase Single-use residue (g) 3.2 0.08 97.5% Frequency of pin jamming 8 times / shift 0 times 100% Product flash rate 8.7% 0.3% 96.6% Mold maintenance cycle (h) 2 24 1100% Total cost (RMB / unit) 4.5 3.2 28.9% (Note: Test conditions: 280T die casting machine, ADC12 aluminum alloy, mold temperature 220±10℃) This solution has been verified through 720 hours of continuous production and meets the requirements of GB / T 15114-2020 aluminum alloy die casting standard.
Claims
1. A mold insert for preventing aluminum shavings residue, characterized in that, The structure includes the following forms: it includes an insert, the gap between the insert and the slider is perpendicular to the workpiece ejection direction, and the gap between the insert and the mold core is inclined at a certain angle to the workpiece ejection direction.
2. A mold insert for preventing aluminum shavings residue according to claim 1, characterized in that, The gap between the insert and the mold core and the tilt angle of the workpiece ejection direction are set to be greater than or equal to 10 degrees.
3. A mold insert for preventing aluminum shavings residue according to claim 1, characterized in that, The gap between the insert and the slider is maintained at 0.01~0.02mm on one side.
4. A mold insert for preventing aluminum shavings residue according to claim 1, characterized in that, The gap between the insert and the mold core is maintained at 0.01~0.02mm on one side.
5. A mold insert for preventing aluminum shavings residue according to claim 1, characterized in that, The insert and slider are positioned and connected by snap-fit locating pins.
6. A mold insert for preventing aluminum shavings residue according to claim 1, characterized in that, The insert and the mold core are connected by snap-fit positioning pins.