A preform solder and package having the same
By using prefabricated solder structures and precision deposition technology, the problems of easy solder oxidation and high cost of vacuum coating have been solved, achieving efficient and stable welding results and low-cost production.
Patent Information
- Application Number
- CN202522475328.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-21
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-11-21
AI Technical Summary
Existing solder materials are prone to oxidation and have low purity. Traditional welding processes cannot guarantee welding quality and stability. Vacuum coating equipment is costly and complex to operate, making it difficult to achieve precise welding.
The pre-fabricated solder structure includes a base layer, an adhesive layer, a transition layer, a solder layer, and a protective layer. It is prepared by vapor deposition or magnetron sputtering. The solder layer consists of multiple stacked metal composite layers, which are combined with the tin layer and the transition layer to form an alloy layer. Local deposition is achieved using a masking fixture.
Improve welding efficiency and stability, lower the operational threshold, enhance welding strength, avoid oxidation and contamination, precisely control solder composition and thickness, and reduce production costs.
Smart Images

Figure CN225008804U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of welding materials technology, specifically relating to a pre-made solder and a package having the same. Background Technology
[0002] With the rapid development of electronic technology, the integration and functional requirements of electronic products are constantly increasing. Packaging technology is becoming increasingly important in the manufacturing of electronic components. In the packaging process of electronic products, welding technology is one of the core processes. Its welding quality is directly related to the performance and reliability of the product. Especially under the trend of miniaturization and high-density integration of modern electronic devices, the precision of the welding process and the quality of the solder have become important factors affecting the long-term stability and efficient production of products.
[0003] Solder technology typically uses solder sheets or granular solder. During the soldering process, the solder needs to melt and cool to form a weld joint. However, the composition and thickness of the solder are easily affected by the external environment and operating procedures during manufacturing, resulting in unstable soldering quality. Furthermore, traditional solder materials often have problems such as easy oxidation, low purity, insufficient joint strength, and uneven solder joints after use, which affect the soldering quality and product reliability.
[0004] Compared to soldering technology, vacuum coating technology improves welding quality by evaporating or sputtering materials such as metals, alloys, and ceramics onto the surface of a workpiece in a vacuum environment to form a thin film. However, vacuum coating equipment is usually expensive, with high maintenance and operating costs. The operation process consumes a lot of energy and requires high levels of environmental management and operational skills, as well as high technical capabilities from operators, making it prone to operational errors or equipment failures. Utility Model Content
[0005] To overcome the shortcomings of the prior art, this utility model proposes a pre-made solder, comprising a base layer, an adhesive layer, a transition layer, a solder layer and a protective layer connected in sequence. The base layer includes a copper shell and a nickel layer electroplated on the copper shell. The base layer is connected to the adhesive layer through the nickel layer. The solder layer comprises several stacked metal composite layers, each of the metal composite layers comprising at least two metal layers arranged in the same order, and each metal layer having different structural features from its adjacent metal layer.
[0006] Specifically, at least one of the metal composite layers includes a tin layer, and the metal composite layer adjacent to the transition layer in the solder layer is connected to the transition layer through the tin layer. The transition layer includes one or more of the following: a gold layer, a silver layer, an indium layer, and a zinc layer for forming an alloy layer with the tin layer during the soldering process.
[0007] Optionally, the metal composite layer includes a tin layer and a silver layer; And / or, the metal composite layer includes a tin layer, a silver layer, and a copper layer, and the metal layers in the metal composite layer that includes a tin layer, a silver layer, and a copper layer are arranged in sequence in the order of tin layer, silver layer, and copper layer, or are arranged in sequence in the order of tin layer, copper layer, and silver layer.
[0008] Preferably, in any metal composite layer, the mass percentage of the tin layer ranges from 90% to 99%, the mass percentage of the silver layer ranges from 1% to 6%, and the mass percentage of the copper layer ranges from 0% to 2%.
[0009] Preferably, the solder layer comprises 1-50 stacked metal composite layers, and the thickness of each metal composite layer ranges from 5μm to 100μm.
[0010] Optionally, the adhesive layer includes one or more of titanium, chromium, nickel, and nickel-chromium alloy layers, and the thickness of the adhesive layer ranges from 20 nm to 300 nm.
[0011] Optionally, the protective layer includes a gold layer and / or a silver layer, and the thickness of the protective layer ranges from 20 nm to 500 nm.
[0012] Specifically, the adhesive layer, the transition layer, the solder layer, and the protective layer are prepared by vapor deposition or magnetron sputtering.
[0013] This utility model also proposes a package, which is provided with the pre-formed solder as described above.
[0014] Specifically, the package includes a non-deposition area and a deposition area for setting the pre-formed solder, wherein the pre-formed solder is pre-masked by a masking fixture to achieve local deposition in the deposition area.
[0015] This utility model has at least the following beneficial effects: The welding material proposed in this utility model can be tightly bonded to the shell, which simplifies the welding operation process, not only improves welding efficiency, but also ensures the stability of welding quality. The metal composite layer effectively improves the strength and stability of welding by stacking different metal layers and having different structural features between adjacent layers. By reducing unnecessary process steps and lowering the operational requirements and technical threshold of the process, production efficiency can be significantly improved. Furthermore, the proposed solution reduces stress concentration during welding and lowers the risk of welding cracks through the alloying reaction of the tin layer and the transition layer. The multi-layer metal composite stack structure increases the total thickness of the solder layer, enhances the mechanical properties of the weld, and effectively disperses thermal stress. At the same time, the metal composite layer has a variety of different combination methods, which can optimize the physical and chemical properties of the welding material to adapt to different usage environments. The bonding layer enhances the bonding force between the welding layer and the substrate, improves the overall strength of the weld, and the protective layer can achieve oxidation resistance. Through vapor deposition and magnetron sputtering methods with precise control of process parameters, the thickness and composition of different layers in the pre-made solder can be guaranteed to meet the design requirements. Furthermore, the packaging component proposed in this utility model achieves precise deposition of pre-made solder on the deposition area by using a shielding fixture, which can avoid the waste of precious metals, reduce production costs, and solve the problem in the prior art that it is difficult to achieve precise local electroplating, and the electroplating area will be much larger than the actual required area, which will increase the cost of using precious metals.
[0016] Therefore, this utility model provides a pre-made solder and a package having therein. The solution proposed by this utility model simplifies the subsequent welding steps and improves welding efficiency by integrating the solder with the shell. It can accurately control the ratio of each component of the solder and the thickness of the solder. Compared with traditional solder sheets, the composition and thickness are more stable and the solder purity is higher. At the same time, it improves the stability of welding and can effectively avoid oxidation or contamination. Attached Figure Description
[0017] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0018] Figure 1 A schematic diagram of the structure of the pre-fabricated solder provided in Example 1; Figure 2 A schematic diagram of another composition of pre-fabricated solder; Figure 3 A schematic diagram of another composition of pre-made solder; Figure 4 This is a structural example diagram of the package provided in Example 2; Figure 5 This is a structural example diagram of another embodiment of the package.
[0019] Figure Labels 1-Base layer; 2-Adhesive layer; 3-Transition layer; 4-Metal composite layer; 5-Protective layer; 6-Encapsulation component; 7-Deposited area; 8-Non-deposited area; 41-Tin layer; 42-Silver layer; 43-Copper layer. Detailed Implementation
[0020] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present utility model, and not all of them. Based on the embodiments of the present utility model, all other embodiments obtained by those skilled in the art without creative effort are within the protection scope of the present utility model.
[0021] Various embodiments of the present invention will be described more fully below. The present invention may have various embodiments, and adjustments and changes may be made therein. However, it should be understood that there is no intention to limit the various embodiments of the present invention to the specific embodiments disclosed herein, but rather the present invention should be understood to cover all adjustments, equivalents, and / or alternatives falling within the spirit and scope of the various embodiments of the present invention.
[0022] In the following, the terms “comprising” or “may include”, which may be used in various embodiments of the present invention, indicate the presence of the disclosed functions, operations, or elements, and do not limit the addition of one or more functions, operations, or elements. Furthermore, as used in various embodiments of the present invention, the terms “comprising,” “having,” and their cognates are intended only to indicate a specific feature, number, step, operation, element, component, or combination of the foregoing, and should not be construed as primarily excluding the presence of one or more other features, numbers, steps, operations, elements, components, or combinations of the foregoing, or the possibility of adding one or more combinations of features, numbers, steps, operations, elements, components, or combinations of the foregoing.
[0023] In various embodiments of this utility model, the expression "or" or "at least one of A and / or B" includes any combination or all combinations of the words listed simultaneously. For example, the expression "A or B" or "at least one of A and / or B" may include A, may include B, or may include both A and B.
[0024] The terms used in the various embodiments of this utility model (such as "first," "second," etc.) may modify various constituent elements in the various embodiments, but do not limit the corresponding constituent elements. For example, the above terms do not limit the order and / or importance of the elements. The above terms are only used for the purpose of distinguishing one element from other elements. For example, a first user device and a second user device refer to different user devices, although both are user devices. For example, without departing from the scope of the various embodiments of this utility model, a first element may be referred to as a second element, and similarly, a second element may be referred to as a first element.
[0025] It should be noted that, in this utility model, unless otherwise explicitly specified and defined, terms such as "installation," "connection," and "fixation" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model according to the specific circumstances.
[0026] In this utility model, those skilled in the art should understand that the terms indicating orientation or positional relationship in the text are based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this utility model and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this utility model.
[0027] The terminology used in the various embodiments of this invention is for the purpose of describing particular embodiments only and is not intended to limit the various embodiments of this invention. As used herein, the singular form is intended to include the plural form as well, unless the context clearly indicates otherwise. Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by one of ordinary skill in the art to which the various embodiments of this invention pertain. The terms (such as those defined in a generally used dictionary) are to be interpreted as having the same meaning as in the context of the relevant technical field and are not to be interpreted as having an idealized or overly formal meaning, unless clearly defined in the various embodiments of this invention.
[0028] Example 1 Please see Figures 1-3This embodiment proposes a pre-formed solder, which integrates the solder with the shell, simplifying subsequent welding steps and improving welding efficiency. Furthermore, the solder is deposited through PVD, which allows for precise control of the composition ratio and thickness of the solder. Compared to traditional solder sheets, the composition and thickness are more stable, and the solder purity is higher than that of traditional solders. There is no oxidation or contamination, which also improves the stability of the welding process. The pre-formed solder proposed in this embodiment specifically includes a base layer 1, an adhesive layer 2, a transition layer 3, a solder layer, and a protective layer 5 connected in sequence. The base layer 1 includes a copper shell and a nickel layer electroplated on the copper shell. The base layer 1 is connected to the adhesive layer 2 through the nickel layer. The adhesive layer 2 is used to improve the bonding force between the base layer 1 and other layers. The transition layer 3 is used to form an alloy layer with the solder layer during the welding process, thereby improving the bonding force between the adhesive layer 2 and the solder layer. The protective layer 5 can isolate oxygen in the air to protect the solder layer from oxidation, thereby improving the stability of the pre-formed solder proposed in this embodiment.
[0029] It should be noted that accurately pre-fabricating solder onto the copper shell requires vacuum coating technology, which has a high technical threshold. The pre-fabricated solder proposed in this embodiment lowers the technical threshold while achieving the same welding effect as using vacuum coating technology.
[0030] Specifically, the solder layer includes several sets of stacked metal combination layers 4, each metal combination layer 4 includes at least two metal layers arranged in the same order, and at least one metal layer includes a tin layer 41, and any metal layer has different structural features from its adjacent metal layer. The metal composite layer 4 adjacent to the transition layer 3 in the solder layer is connected to the transition layer 3 through the tin layer 41. The transition layer 3 includes one or more of the following: a gold layer, a silver layer, an indium layer, and a zinc layer, which are used to form an alloy layer with the tin layer 41 during the soldering process.
[0031] It should be noted that the welding temperature between the heat sink and the shell is about 250 degrees. The gold layer, silver layer, indium layer and zinc layer can diffuse with the tin layer 41 to form an alloy transition layer 3 under conditions below 250 degrees, so they can all serve as transition layers 3.
[0032] Optionally, each metal composite layer 4 includes a tin layer 41 and a silver layer 42, please refer again. Figure 3 At this time, the metal composite layer 4 adjacent to the transition layer 3 is connected to the transition layer 3 through the tin layer 41, and the other metal composite layers 4 are connected to the silver layer 42 in the previous metal composite layer 4 through the tin layer 41. The metal composite layer 4 adjacent to the protective layer 5 is connected to the protective layer 5 through the silver layer 42. Alternatively, each metal composite layer 4 may include a tin layer 41, a silver layer 42, and a copper layer 43, with the metal layers in each metal composite layer 4 arranged sequentially in the order of tin layer 41, silver layer 42, and copper layer 43. Please refer again to [the previous section]. Figure 1 At this point, the metal composite layer 4 adjacent to the transition layer 3 is connected to the transition layer 3 through the tin layer 41, and other metal composite layers 4 are connected to the copper layer 43 in the previous metal composite layer 4 through the tin layer 41. The metal composite layer 4 adjacent to the protective layer 5 is connected to the protective layer 5 through the copper layer 43; or they are all arranged in the order of tin layer 41, copper layer 43, and silver layer 42. Please refer again. Figure 2 At this time, the metal composite layer 4 adjacent to the transition layer 3 is connected to the transition layer 3 through the tin layer 41, the other metal composite layers 4 are connected to the silver layer 42 in the previous metal composite layer 4 through the tin layer 41, and the metal composite layer 4 adjacent to the protective layer 5 is connected to the protective layer 5 through the silver layer 42.
[0033] Preferably, in the metal composite layer 4, the mass percentage of tin layer 41 ranges from 90% to 99%, the mass percentage of silver layer 42 ranges from 1% to 6%, and the mass percentage of copper layer 43 ranges from 0% to 2%. That is, when a group of metal composite layers 4 includes only tin layer 41 and silver layer 42, the mass percentage of tin layer 41 in the group of metal composite layers 4 ranges from 90% to 99%, and the mass percentage of silver layer 42 ranges from 1% to 6%; while when a group of metal composite layers 4 includes tin layer 41, silver layer 42 and copper layer 43, the mass percentage of tin layer 41 in the group of metal composite layers 4 ranges from 90% to 99%, the mass percentage of silver layer 42 ranges from 1% to 6%, and the mass percentage of copper layer 43 ranges from greater than 0% to not greater than 2%.
[0034] Preferably, the solder layer comprises 1-50 stacked metal combination layers 4, and the thickness of each metal combination layer 4 ranges from 5μm to 100μm.
[0035] Optionally, the adhesive layer 2 includes one or more of titanium, chromium, nickel, and nickel-chromium alloy layers, and the thickness of the adhesive layer 2 ranges from 20nm to 300nm. In this embodiment, the bonding force between the substrate layer 1 and other layers based on the adhesive layer is greater than 80kg.
[0036] Optionally, the protective layer 5 includes a gold layer and / or a silver layer, and the thickness of the protective layer 5 ranges from 20 nm to 500 nm.
[0037] Specifically, the adhesive layer 2, transition layer 3, solder layer and protective layer 5 are prepared by vapor deposition or magnetron sputtering.
[0038] In one specific embodiment, the base layer in the preformed solder includes a nickel layer with a thickness of 1 μm deposited on the copper shell by electroplating. The bonding layer includes a nickel layer, which is deposited on the substrate layer with a thickness of 100 nm by plasma cleaning of the nickel-plated shell for 6 minutes and then by magnetron sputtering. The transition layer includes a 300 nm thick silver layer deposited on the binder layer using magnetron sputtering; The solder layer consists of five metal composite layers arranged in a tin, silver, and copper configuration. Each tin layer is 4000 nm thick, each silver layer is 86.2 nm thick, and each copper layer is 16.8 nm thick. The mass percentages of the tin, silver, and copper layers are 96.5%, 3%, and 0.5%, respectively. The protective layer consists of a 200nm thick silver layer deposited on the solder layer.
[0039] By soldering the heat sink onto the shell of the tin-silver-copper solder prepared in the above manner using eutectic reflow soldering, and observing the soldering effect around the heat sink under a microscope, it can be confirmed that there is solder around the heat sink, which indicates that the soldering effect is good and there is no cold solder joint. The heat sink soldered on the pre-made tin-silver-copper solder was subjected to a push force test to push the heat sink off the pre-made solder. The push force value was greater than 100 kg, which is comparable to that of the tin-silver-copper solder sheet. Observation from the pushed-off heat sink surface can confirm that the solder fully wets the back of the heat sink, which indicates that the welding effect is good. The heat sink was soldered to the prefabricated tin-silver-copper shell using eutectic reflow soldering. The reliability of the soldering was evaluated by thermal shock testing. The thermal shock test conditions were -50~150℃, with 200 cycles. It was confirmed that there was no detachment or delamination between the heat sink and the shell, indicating that the reliability test was qualified.
[0040] It should be noted that having the same thickness of the same metal layer in different metal combination layers facilitates mass production. In actual production, the pre-made solder proposed in this embodiment can make the same metal layer in different metal combination layers have different thicknesses according to requirements.
[0041] In another embodiment, the base layer in the preformed solder includes a 2 μm thick nickel layer deposited on the copper shell by electroplating. The bonding layer includes a nickel layer, which is deposited on the substrate layer with a thickness of 200 nm by plasma cleaning of the nickel-plated shell for 6 minutes and then by vapor deposition. The transition layer includes a 200 nm thick gold layer deposited on the bonding layer by vapor deposition; The solder layer consists of eight metal composite layers arranged in a tin, copper, and silver configuration. Each tin layer is 4000 nm thick, each silver layer is 86.2 nm thick, and each copper layer is 16.8 nm thick. The mass percentages of the tin, silver, and copper layers are 96.5%, 3%, and 0.5%, respectively. The protective layer consists of a 200nm thick silver layer deposited on the solder layer.
[0042] In another embodiment, the base layer in the preformed solder includes a 2 μm thick nickel layer deposited on the copper shell by electroplating. The bonding layer includes a nickel layer. After plasma cleaning the nickel-plated shell for 6 minutes, a titanium layer with a thickness of 100 nm is deposited on the substrate by magnetron sputtering. The transition layer includes a 300 nm thick silver layer deposited on the binder layer using magnetron sputtering; The solder layer consists of eight metal composite layers arranged in a tin, copper, and silver configuration. Each tin layer is 5000 nm thick, each silver layer is 146.1 nm thick, and each copper layer is 42.8 nm thick. The mass percentages of the tin, silver, and copper layers are 95%, 4%, and 1%, respectively. The protective layer consists of a 200nm thick gold layer deposited on the solder layer.
[0043] Example 2 Please see Figures 4-5 This embodiment proposes a package 6, which is provided with pre-formed solder as proposed in Embodiment 1.
[0044] Specifically, the package 6 includes a non-deposition area 8 and a deposition area 7 for setting pre-formed solder. The pre-formed solder is pre-masked in the non-deposition area 8 by a masking fixture to achieve local deposition in the deposition area 7. By using a masking fixture to accurately deposit the pre-formed solder on the deposition area 7, the waste of precious metals can be avoided, thereby reducing production costs.
[0045] In summary, this utility model provides a pre-made solder and a package having the same. The proposed solution simplifies the subsequent welding steps and improves welding efficiency by integrating the solder with the shell. It can accurately control the ratio of each component of the solder and the solder thickness. Compared with traditional solder sheets, the composition and thickness are more stable and the solder purity is higher. At the same time, it improves the stability of welding and can effectively avoid oxidation or contamination.
[0046] The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present utility model should be included within the protection scope of the present utility model.
Claims
1. A preform solder, characterized by, It includes a base layer, an adhesive layer, a transition layer, a solder layer and a protective layer connected in sequence. The base layer includes a copper shell and a nickel layer electroplated on the copper shell. The base layer is connected to the adhesive layer through the nickel layer. The solder layer comprises several stacked metal composite layers, each of the metal composite layers comprising at least two metal layers arranged in the same order, and each metal layer having different structural features from its adjacent metal layer.
2. The preform solder of claim 1, wherein, At least one of the metal composite layers includes a tin layer, and the metal composite layer adjacent to the transition layer in the solder layer is connected to the transition layer through the tin layer. The transition layer includes one or more of the following: a gold layer, a silver layer, an indium layer, and a zinc layer for forming an alloy layer with the tin layer during the soldering process.
3. The preform solder of claim 2, wherein, The metal composite layer includes a tin layer and a silver layer; And / or, the metal composite layer includes a tin layer, a silver layer, and a copper layer, and the metal layers in the metal composite layer that includes a tin layer, a silver layer, and a copper layer are arranged in sequence in the order of tin layer, silver layer, and copper layer, or are arranged in sequence in the order of tin layer, copper layer, and silver layer.
4. The preform of claim 3 wherein the preform has a wall thickness of 0.5 to 1.5 mm. In any metal composite layer, the mass percentage of the tin layer ranges from 90% to 99%, the mass percentage of the silver layer ranges from 1% to 6%, and the mass percentage of the copper layer ranges from 0% to 2%.
5. The pre-formed solder according to any one of claims 1-4, characterized in that, The solder layer comprises 1-50 stacked metal composite layers, each of which has a thickness ranging from 5μm to 100μm.
6. The pre-formed solder according to claim 1, characterized in that, The adhesive layer includes one or more of titanium, chromium, nickel, and nickel-chromium alloy layers, and the thickness of the adhesive layer ranges from 20 nm to 300 nm.
7. The pre-made solder according to claim 1, characterized in that, The protective layer includes a gold layer and / or a silver layer, and the thickness of the protective layer ranges from 20 nm to 500 nm.
8. The pre-formed solder according to claim 1, characterized in that, The adhesive layer, the transition layer, the solder layer, and the protective layer are prepared by vapor deposition or magnetron sputtering.
9. A package, characterized in that, It is provided with the pre-formed solder as described in any one of claims 1-8.
10. The package according to claim 9, characterized in that, It includes a non-deposition area and a deposition area for setting the pre-formed solder, wherein the pre-formed solder is pre-masked by a masking fixture to achieve local deposition in the deposition area.